Elapsed Time, Volts/Count, Torch On, Arc Good, Voltage Control, THC Up, THC Down, Set Point, Current Voltage
17063, V, 0, 0, 0, 0, 0, 704, 52
17063, V, 0, 0, 0, 0, 0, 704, 52
17320, V, 0, 0, 0, 0, 0, 704, 52
17320, V, 0, 0, 0, 0, 0, 704, 52
17577, V, 0, 0, 0, 0, 0, 704, 52
17577, V, 0, 0, 0, 0, 0, 704, 52
17835, V, 0, 0, 0, 0, 0, 704, 52
17835, V, 0, 0, 0, 0, 0, 704, 52
18092, V, 0, 0, 0, 0, 0, 704, 52
18092, V, 0, 0, 0, 0, 0, 704, 52
18349, V, 0, 0, 0, 0, 0, 704, 52
18349, V, 0, 0, 0, 0, 0, 704, 52
18606, V, 0, 0, 0, 0, 0, 704, 52
18606, V, 0, 0, 0, 0, 0, 704, 52
18863, V, 0, 0, 0, 0, 0, 704, 52
18863, V, 0, 0, 0, 0, 0, 704, 52
19120, V, 0, 0, 0, 0, 0, 704, 52
19120, V, 0, 0, 0, 0, 0, 704, 52
19377, V, 0, 0, 0, 0, 0, 704, 52
19377, V, 0, 0, 0, 0, 0, 704, 52
19634, V, 0, 0, 0, 0, 0, 704, 52
19634, V, 0, 0, 0, 0, 0, 704, 52
19891, V, 0, 0, 0, 0, 0, 704, 52
19891, V, 0, 0, 0, 0, 0, 704, 52
20148, V, 0, 0, 0, 0, 0, 704, 52
20148, V, 0, 0, 0, 0, 0, 704, 52
20405, V, 0, 0, 0, 0, 0, 704, 52
20405, V, 0, 0, 0, 0, 0, 704, 52
20662, V, 0, 0, 0, 0, 0, 704, 52
20662, V, 0, 0, 0, 0, 0, 704, 52
20919, V, 0, 0, 0, 0, 0, 704, 52
20919, V, 0, 0, 0, 0, 0, 704, 52
21176, V, 0, 0, 0, 0, 0, 704, 52
21176, V, 0, 0, 0, 0, 0, 704, 52
21433, V, 0, 0, 0, 0, 0, 704, 52
21433, V, 0, 0, 0, 0, 0, 704, 52
21690, V, 0, 0, 0, 0, 0, 704, 52
21690, V, 0, 0, 0, 0, 0, 704, 52
21947, V, 0, 0, 0, 0, 0, 704, 52
21947, V, 0, 0, 0, 0, 0, 704, 52
22204, V, 0, 0, 0, 0, 0, 704, 52
22204, V, 0, 0, 0, 0, 0, 704, 52
22461, V, 0, 0, 0, 0, 0, 704, 52
22461, V, 0, 0, 0, 0, 0, 704, 52
22718, V, 0, 0, 0, 0, 0, 704, 52
22718, V, 0, 0, 0, 0, 0, 704, 52
22975, V, 0, 0, 0, 0, 0, 704, 52
22975, V, 0, 0, 0, 0, 0, 704, 52
23232, V, 0, 0, 0, 0, 0, 704, 52
23232, V, 0, 0, 0, 0, 0, 704, 52
23489, V, 0, 0, 0, 0, 0, 704, 51
23489, V, 0, 0, 0, 0, 0, 704, 51
23746, V, 0, 0, 0, 0, 0, 704, 51
23746, V, 0, 0, 0, 0, 0, 704, 51
24003, V, 0, 0, 0, 0, 0, 704, 51
24003, V, 0, 0, 0, 0, 0, 704, 51
24260, V, 0, 0, 0, 0, 0, 704, 51
24260, V, 0, 0, 0, 0, 0, 704, 51
24517, V, 0, 0, 0, 0, 0, 704, 51
24517, V, 0, 0, 0, 0, 0, 704, 51
24774, V, 0, 0, 0, 0, 0, 704, 51
24774, V, 0, 0, 0, 0, 0, 704, 51
25031, V, 0, 0, 0, 0, 0, 704, 51
25031, V, 0, 0, 0, 0, 0, 704, 51
25288, V, 0, 0, 0, 0, 0, 704, 51
25288, V, 0, 0, 0, 0, 0, 704, 51
25545, V, 0, 0, 0, 0, 0, 704, 51
25545, V, 0, 0, 0, 0, 0, 704, 51
25802, V, 0, 0, 0, 0, 0, 704, 13
25802, V, 0, 0, 0, 0, 0, 704, 13
26059, V, 0, 0, 0, 0, 0, 704, 48
26059, V, 0, 0, 0, 0, 0, 704, 48
26316, V, 0, 0, 0, 0, 0, 704, 52
26316, V, 0, 0, 0, 0, 0, 704, 52
26486, V, 1, 0, 0, 0, 0, 704, 52
26487, V, 1, 0, 0, 0, 0, 704, 52
26488, V, 1, 0, 0, 0, 0, 704, 52
26489, V, 1, 0, 0, 0, 0, 704, 52
26490, V, 1, 0, 0, 0, 0, 704, 52
26491, V, 1, 0, 0, 0, 0, 704, 52
26492, V, 1, 0, 0, 0, 0, 704, 52
26493, V, 1, 0, 0, 0, 0, 704, 52
26494, V, 1, 0, 0, 0, 0, 704, 52
26496, V, 1, 0, 0, 0, 0, 704, 52
26497, V, 1, 0, 0, 0, 0, 704, 52
26498, V, 1, 0, 0, 0, 0, 704, 52
26499, V, 1, 0, 0, 0, 0, 704, 52
26500, V, 1, 0, 0, 0, 0, 704, 52
26501, V, 1, 0, 0, 0, 0, 704, 52
26502, V, 1, 0, 0, 0, 0, 704, 52
26503, V, 1, 0, 0, 0, 0, 704, 52
26504, V, 1, 0, 0, 0, 0, 704, 52
26505, V, 1, 0, 0, 0, 0, 704, 52
26506, V, 1, 0, 0, 0, 0, 704, 52
26507, V, 1, 0, 0, 0, 0, 704, 52
26508, V, 1, 0, 0, 0, 0, 704, 52
26509, V, 1, 0, 0, 0, 0, 704, 52
26510, V, 1, 0, 0, 0, 0, 704, 52
26511, V, 1, 0, 0, 0, 0, 704, 52
26512, V, 1, 0, 0, 0, 0, 704, 52
26513, V, 1, 0, 0, 0, 0, 704, 52
26514, V, 1, 0, 0, 0, 0, 704, 52
26515, V, 1, 0, 0, 0, 0, 704, 52
26516, V, 1, 0, 0, 0, 0, 704, 52
26517, V, 1, 0, 0, 0, 0, 704, 52
26518, V, 1, 0, 0, 0, 0, 704, 52
26519, V, 1, 0, 0, 0, 0, 704, 52
26520, V, 1, 0, 0, 0, 0, 704, 52
26521, V, 1, 0, 0, 0, 0, 704, 52
26522, V, 1, 0, 0, 0, 0, 704, 52
26523, V, 1, 0, 0, 0, 0, 704, 52
26524, V, 1, 0, 0, 0, 0, 704, 52
26525, V, 1, 0, 0, 0, 0, 704, 52
26526, V, 1, 0, 0, 0, 0, 704, 52
26527, V, 1, 0, 0, 0, 0, 704, 52
26528, V, 1, 0, 0, 0, 0, 704, 52
26529, V, 1, 0, 0, 0, 0, 704, 52
26530, V, 1, 0, 0, 0, 0, 704, 52
26531, V, 1, 0, 0, 0, 0, 704, 52
26532, V, 1, 0, 0, 0, 0, 704, 52
26533, V, 1, 0, 0, 0, 0, 704, 52
26534, V, 1, 0, 0, 0, 0, 704, 52
26535, V, 1, 0, 0, 0, 0, 704, 52
26536, V, 1, 0, 0, 0, 0, 704, 52
26537, V, 1, 0, 0, 0, 0, 704, 52
26539, V, 1, 0, 0, 0, 0, 704, 52
26540, V, 1, 0, 0, 0, 0, 704, 52
26541, V, 1, 0, 0, 0, 0, 704, 52
26542, V, 1, 0, 0, 0, 0, 704, 52
26543, V, 1, 0, 0, 0, 0, 704, 52
26544, V, 1, 0, 0, 0, 0, 704, 52
26545, V, 1, 0, 0, 0, 0, 704, 52
26546, V, 1, 0, 0, 0, 0, 704, 52
26547, V, 1, 0, 0, 0, 0, 704, 52
26548, V, 1, 0, 0, 0, 0, 704, 52
26549, V, 1, 0, 0, 0, 0, 704, 52
26550, V, 1, 0, 0, 0, 0, 704, 52
26551, V, 1, 0, 0, 0, 0, 704, 52
26552, V, 1, 0, 0, 0, 0, 704, 52
26553, V, 1, 0, 0, 0, 0, 704, 52
26554, V, 1, 0, 0, 0, 0, 704, 52
26555, V, 1, 0, 0, 0, 0, 704, 52
26556, V, 1, 0, 0, 0, 0, 704, 52
26557, V, 1, 0, 0, 0, 0, 704, 52
26558, V, 1, 0, 0, 0, 0, 704, 52
26559, V, 1, 0, 0, 0, 0, 704, 52
26560, V, 1, 0, 0, 0, 0, 704, 52
26561, V, 1, 0, 0, 0, 0, 704, 52
26562, V, 1, 0, 0, 0, 0, 704, 52
26563, V, 1, 0, 0, 0, 0, 704, 52
26564, V, 1, 0, 0, 0, 0, 704, 52
26565, V, 1, 0, 0, 0, 0, 704, 52
26566, V, 1, 0, 0, 0, 0, 704, 52
26567, V, 1, 0, 0, 0, 0, 704, 52
26568, V, 1, 0, 0, 0, 0, 704, 52
26569, V, 1, 0, 0, 0, 0, 704, 52
26570, V, 1, 0, 0, 0, 0, 704, 52
26571, V, 1, 0, 0, 0, 0, 704, 52
26572, V, 1, 0, 0, 0, 0, 704, 52
26573, V, 1, 0, 0, 0, 0, 704, 52
26574, V, 1, 0, 0, 0, 0, 704, 52
26575, V, 1, 0, 0, 0, 0, 704, 52
26576, V, 1, 0, 0, 0, 0, 704, 52
26577, V, 1, 0, 0, 0, 0, 704, 52
26578, V, 1, 0, 0, 0, 0, 704, 52
26579, V, 1, 0, 0, 0, 0, 704, 52
26580, V, 1, 0, 0, 0, 0, 704, 52
26582, V, 1, 0, 0, 0, 0, 704, 52
26583, V, 1, 0, 0, 0, 0, 704, 52
26584, V, 1, 0, 0, 0, 0, 704, 52
26585, V, 1, 0, 0, 0, 0, 704, 52
26586, V, 1, 0, 0, 0, 0, 704, 52
26587, V, 1, 0, 0, 0, 0, 704, 52
26588, V, 1, 0, 0, 0, 0, 704, 52
26589, V, 1, 0, 0, 0, 0, 704, 52
26590, V, 1, 0, 0, 0, 0, 704, 52
26591, V, 1, 0, 0, 0, 0, 704, 52
26592, V, 1, 0, 0, 0, 0, 704, 52
26593, V, 1, 0, 0, 0, 0, 704, 52
26594, V, 1, 0, 0, 0, 0, 704, 52
26595, V, 1, 0, 0, 0, 0, 704, 52
26596, V, 1, 0, 0, 0, 0, 704, 52
26597, V, 1, 0, 0, 0, 0, 704, 52
26598, V, 1, 0, 0, 0, 0, 704, 52
26599, V, 1, 0, 0, 0, 0, 704, 52
26600, V, 1, 0, 0, 0, 0, 704, 52
26601, V, 1, 0, 0, 0, 0, 704, 52
26602, V, 1, 0, 0, 0, 0, 704, 52
26603, V, 1, 0, 0, 0, 0, 704, 52
26604, V, 1, 0, 0, 0, 0, 704, 52
26605, V, 1, 0, 0, 0, 0, 704, 52
26606, V, 1, 0, 0, 0, 0, 704, 52
26607, V, 1, 0, 0, 0, 0, 704, 52
26608, V, 1, 0, 0, 0, 0, 704, 52
26609, V, 1, 0, 0, 0, 0, 704, 52
26610, V, 1, 0, 0, 0, 0, 704, 52
26611, V, 1, 0, 0, 0, 0, 704, 52
26612, V, 1, 0, 0, 0, 0, 704, 52
26613, V, 1, 0, 0, 0, 0, 704, 52
26614, V, 1, 0, 0, 0, 0, 704, 52
26615, V, 1, 0, 0, 0, 0, 704, 52
26616, V, 1, 0, 0, 0, 0, 704, 52
26617, V, 1, 0, 0, 0, 0, 704, 52
26618, V, 1, 0, 0, 0, 0, 704, 52
26619, V, 1, 0, 0, 0, 0, 704, 52
26620, V, 1, 0, 0, 0, 0, 704, 52
26621, V, 1, 0, 0, 0, 0, 704, 52
26622, V, 1, 0, 0, 0, 0, 704, 52
26624, V, 1, 0, 0, 0, 0, 704, 52
26625, V, 1, 0, 0, 0, 0, 704, 52
26626, V, 1, 0, 0, 0, 0, 704, 52
26627, V, 1, 0, 0, 0, 0, 704, 52
26628, V, 1, 0, 0, 0, 0, 704, 52
26629, V, 1, 0, 0, 0, 0, 704, 52
26630, V, 1, 0, 0, 0, 0, 704, 52
26631, V, 1, 0, 0, 0, 0, 704, 52
26632, V, 1, 0, 0, 0, 0, 704, 52
26633, V, 1, 0, 0, 0, 0, 704, 52
26634, V, 1, 0, 0, 0, 0, 704, 52
26635, V, 1, 0, 0, 0, 0, 704, 52
26636, V, 1, 0, 0, 0, 0, 704, 52
26637, V, 1, 0, 0, 0, 0, 704, 52
26638, V, 1, 0, 0, 0, 0, 704, 52
26639, V, 1, 0, 0, 0, 0, 704, 52
26640, V, 1, 0, 0, 0, 0, 704, 52
26641, V, 1, 0, 0, 0, 0, 704, 52
26642, V, 1, 0, 0, 0, 0, 704, 52
26643, V, 1, 0, 0, 0, 0, 704, 52
26644, V, 1, 0, 0, 0, 0, 704, 52
26645, V, 1, 0, 0, 0, 0, 704, 52
26646, V, 1, 0, 0, 0, 0, 704, 52
26647, V, 1, 0, 0, 0, 0, 704, 52
26648, V, 1, 0, 0, 0, 0, 704, 52
26649, V, 1, 0, 0, 0, 0, 704, 52
26650, V, 1, 0, 0, 0, 0, 704, 52
26651, V, 1, 0, 0, 0, 0, 704, 52
26652, V, 1, 0, 0, 0, 0, 704, 52
26653, V, 1, 0, 0, 0, 0, 704, 52
26654, V, 1, 0, 0, 0, 0, 704, 52
26655, V, 1, 0, 0, 0, 0, 704, 52
26656, V, 1, 0, 0, 0, 0, 704, 52
26657, V, 1, 0, 0, 0, 0, 704, 52
26658, V, 1, 0, 0, 0, 0, 704, 53
26659, V, 1, 0, 0, 0, 0, 704, 52
26660, V, 1, 0, 0, 0, 0, 704, 53
26661, V, 1, 0, 0, 0, 0, 704, 52
26662, V, 1, 0, 0, 0, 0, 704, 52
26663, V, 1, 0, 0, 0, 0, 704, 52
26664, V, 1, 0, 0, 0, 0, 704, 52
26665, V, 1, 0, 0, 0, 0, 704, 52
26667, V, 1, 0, 0, 0, 0, 704, 52
26668, V, 1, 0, 0, 0, 0, 704, 52
26669, V, 1, 0, 0, 0, 0, 704, 52
26670, V, 1, 0, 0, 0, 0, 704, 52
26671, V, 1, 0, 0, 0, 0, 704, 52
26672, V, 1, 0, 0, 0, 0, 704, 52
26673, V, 1, 0, 0, 0, 0, 704, 52
26674, V, 1, 0, 0, 0, 0, 704, 52
26675, V, 1, 0, 0, 0, 0, 704, 52
26676, V, 1, 0, 0, 0, 0, 704, 52
26677, V, 1, 0, 0, 0, 0, 704, 52
26678, V, 1, 0, 0, 0, 0, 704, 52
26679, V, 1, 0, 0, 0, 0, 704, 52
26680, V, 1, 0, 0, 0, 0, 704, 52
26681, V, 1, 0, 0, 0, 0, 704, 53
26682, V, 1, 0, 0, 0, 0, 704, 52
26683, V, 1, 0, 0, 0, 0, 704, 52
26684, V, 1, 0, 0, 0, 0, 704, 52
26685, V, 1, 0, 0, 0, 0, 704, 52
26686, V, 1, 0, 0, 0, 0, 704, 53
26687, V, 1, 0, 0, 0, 0, 704, 53
26688, V, 1, 0, 0, 0, 0, 704, 52
26689, V, 1, 0, 0, 0, 0, 704, 52
26690, V, 1, 0, 0, 0, 0, 704, 52
26691, V, 1, 0, 0, 0, 0, 704, 52
26692, V, 1, 0, 0, 0, 0, 704, 52
26693, V, 1, 0, 0, 0, 0, 704, 52
26694, V, 1, 0, 0, 0, 0, 704, 52
26695, V, 1, 0, 0, 0, 0, 704, 52
26696, V, 1, 0, 0, 0, 0, 704, 52
26697, V, 1, 0, 0, 0, 0, 704, 52
26698, V, 1, 0, 0, 0, 0, 704, 52
26699, V, 1, 0, 0, 0, 0, 704, 52
26700, V, 1, 0, 0, 0, 0, 704, 53
26701, V, 1, 0, 0, 0, 0, 704, 53
26702, V, 1, 0, 0, 0, 0, 704, 52
26703, V, 1, 0, 0, 0, 0, 704, 52
26704, V, 1, 0, 0, 0, 0, 704, 52
26705, V, 1, 0, 0, 0, 0, 704, 53
26706, V, 1, 0, 0, 0, 0, 704, 53
26707, V, 1, 0, 0, 0, 0, 704, 52
26708, V, 1, 0, 0, 0, 0, 704, 52
26710, V, 1, 0, 0, 0, 0, 704, 53
26711, V, 1, 0, 0, 0, 0, 704, 53
26712, V, 1, 0, 0, 0, 0, 704, 52
26713, V, 1, 0, 0, 0, 0, 704, 52
26714, V, 1, 0, 0, 0, 0, 704, 52
26715, V, 1, 0, 0, 0, 0, 704, 52
26716, V, 1, 0, 0, 0, 0, 704, 52
26717, V, 1, 0, 0, 0, 0, 704, 52
26718, V, 1, 0, 0, 0, 0, 704, 52
26719, V, 1, 0, 0, 0, 0, 704, 52
26720, V, 1, 0, 0, 0, 0, 704, 52
26721, V, 1, 0, 0, 0, 0, 704, 53
26722, V, 1, 0, 0, 0, 0, 704, 53
26723, V, 1, 0, 0, 0, 0, 704, 52
26724, V, 1, 0, 0, 0, 0, 704, 52
26725, V, 1, 0, 0, 0, 0, 704, 53
26726, V, 1, 0, 0, 0, 0, 704, 52
26727, V, 1, 0, 0, 0, 0, 704, 52
26728, V, 1, 0, 0, 0, 0, 704, 52
26729, V, 1, 0, 0, 0, 0, 704, 52
26730, V, 1, 0, 0, 0, 0, 704, 53
26731, V, 1, 0, 0, 0, 0, 704, 52
26732, V, 1, 0, 0, 0, 0, 704, 53
26733, V, 1, 0, 0, 0, 0, 704, 52
26734, V, 1, 0, 0, 0, 0, 704, 52
26735, V, 1, 0, 0, 0, 0, 704, 52
26736, V, 1, 0, 0, 0, 0, 704, 52
26737, V, 1, 0, 0, 0, 0, 704, 52
26738, V, 1, 0, 0, 0, 0, 704, 52
26739, V, 1, 0, 0, 0, 0, 704, 52
26740, V, 1, 0, 0, 0, 0, 704, 53
26741, V, 1, 0, 0, 0, 0, 704, 52
26742, V, 1, 0, 0, 0, 0, 704, 52
26743, V, 1, 0, 0, 0, 0, 704, 53
26744, V, 1, 0, 0, 0, 0, 704, 52
26745, V, 1, 0, 0, 0, 0, 704, 53
26746, V, 1, 0, 0, 0, 0, 704, 53
26747, V, 1, 0, 0, 0, 0, 704, 52
26748, V, 1, 0, 0, 0, 0, 704, 52
26749, V, 1, 0, 0, 0, 0, 704, 52
26750, V, 1, 0, 0, 0, 0, 704, 53
26752, V, 1, 0, 0, 0, 0, 704, 52
26753, V, 1, 0, 0, 0, 0, 704, 52
26754, V, 1, 0, 0, 0, 0, 704, 52
26755, V, 1, 0, 0, 0, 0, 704, 52
26756, V, 1, 0, 0, 0, 0, 704, 52
26757, V, 1, 0, 0, 0, 0, 704, 52
26758, V, 1, 0, 0, 0, 0, 704, 52
26759, V, 1, 0, 0, 0, 0, 704, 52
26760, V, 1, 0, 0, 0, 0, 704, 52
26761, V, 1, 0, 0, 0, 0, 704, 53
26762, V, 1, 0, 0, 0, 0, 704, 52
26763, V, 1, 0, 0, 0, 0, 704, 52
26764, V, 1, 0, 0, 0, 0, 704, 53
26765, V, 1, 0, 0, 0, 0, 704, 53
26766, V, 1, 0, 0, 0, 0, 704, 53
26767, V, 1, 0, 0, 0, 0, 704, 52
26768, V, 1, 0, 0, 0, 0, 704, 52
26769, V, 1, 0, 0, 0, 0, 704, 53
26770, V, 1, 0, 0, 0, 0, 704, 53
26771, V, 1, 0, 0, 0, 0, 704, 52
26772, V, 1, 0, 0, 0, 0, 704, 53
26773, V, 1, 0, 0, 0, 0, 704, 52
26774, V, 1, 0, 0, 0, 0, 704, 52
26775, V, 1, 0, 0, 0, 0, 704, 52
26776, V, 1, 0, 0, 0, 0, 704, 52
26777, V, 1, 0, 0, 0, 0, 704, 52
26778, V, 1, 0, 0, 0, 0, 704, 52
26779, V, 1, 0, 0, 0, 0, 704, 52
26780, V, 1, 0, 0, 0, 0, 704, 53
26781, V, 1, 0, 0, 0, 0, 704, 53
26782, V, 1, 0, 0, 0, 0, 704, 52
26783, V, 1, 0, 0, 0, 0, 704, 52
26784, V, 1, 0, 0, 0, 0, 704, 53
26785, V, 1, 0, 0, 0, 0, 704, 53
26786, V, 1, 0, 0, 0, 0, 704, 53
26787, V, 1, 0, 0, 0, 0, 704, 53
26788, V, 1, 0, 0, 0, 0, 704, 52
26789, V, 1, 0, 0, 0, 0, 704, 53
26790, V, 1, 0, 0, 0, 0, 704, 53
26791, V, 1, 0, 0, 0, 0, 704, 52
26792, V, 1, 0, 0, 0, 0, 704, 52
26793, V, 1, 0, 0, 0, 0, 704, 52
26795, V, 1, 0, 0, 0, 0, 704, 52
26796, V, 1, 0, 0, 0, 0, 704, 53
26797, V, 1, 0, 0, 0, 0, 704, 52
26798, V, 1, 0, 0, 0, 0, 704, 52
26799, V, 1, 0, 0, 0, 0, 704, 52
26800, V, 1, 0, 0, 0, 0, 704, 53
26801, V, 1, 0, 0, 0, 0, 704, 53
26802, V, 1, 0, 0, 0, 0, 704, 53
26803, V, 1, 0, 0, 0, 0, 704, 52
26804, V, 1, 0, 0, 0, 0, 704, 53
26805, V, 1, 0, 0, 0, 0, 704, 53
26806, V, 1, 0, 0, 0, 0, 704, 53
26807, V, 1, 0, 0, 0, 0, 704, 52
26808, V, 1, 0, 0, 0, 0, 704, 53
26809, V, 1, 0, 0, 0, 0, 704, 53
26810, V, 1, 0, 0, 0, 0, 704, 52
26811, V, 1, 0, 0, 0, 0, 704, 52
26812, V, 1, 0, 0, 0, 0, 704, 53
26813, V, 1, 0, 0, 0, 0, 704, 52
26814, V, 1, 0, 0, 0, 0, 704, 53
26815, V, 1, 0, 0, 0, 0, 704, 53
26816, V, 1, 0, 0, 0, 0, 704, 52
26817, V, 1, 0, 0, 0, 0, 704, 53
26818, V, 1, 0, 0, 0, 0, 704, 52
26819, V, 1, 0, 0, 0, 0, 704, 53
26820, V, 1, 0, 0, 0, 0, 704, 52
26821, V, 1, 0, 0, 0, 0, 704, 52
26822, V, 1, 0, 0, 0, 0, 704, 52
26823, V, 1, 0, 0, 0, 0, 704, 53
26824, V, 1, 0, 0, 0, 0, 704, 53
26825, V, 1, 0, 0, 0, 0, 704, 53
26826, V, 1, 0, 0, 0, 0, 704, 53
26827, V, 1, 0, 0, 0, 0, 704, 53
26828, V, 1, 0, 0, 0, 0, 704, 52
26829, V, 1, 0, 0, 0, 0, 704, 53
26830, V, 1, 0, 0, 0, 0, 704, 52
26831, V, 1, 0, 0, 0, 0, 704, 53
26832, V, 1, 0, 0, 0, 0, 704, 52
26833, V, 1, 0, 0, 0, 0, 704, 52
26834, V, 1, 0, 0, 0, 0, 704, 52
26835, V, 1, 0, 0, 0, 0, 704, 52
26836, V, 1, 0, 0, 0, 0, 704, 53
26838, V, 1, 0, 0, 0, 0, 704, 52
26839, V, 1, 0, 0, 0, 0, 704, 52
26840, V, 1, 0, 0, 0, 0, 704, 53
26841, V, 1, 0, 0, 0, 0, 704, 52
26842, V, 1, 0, 0, 0, 0, 704, 52
26843, V, 1, 0, 0, 0, 0, 704, 52
26844, V, 1, 0, 0, 0, 0, 704, 53
26845, V, 1, 0, 0, 0, 0, 704, 53
26846, V, 1, 0, 0, 0, 0, 704, 52
26847, V, 1, 0, 0, 0, 0, 704, 53
26848, V, 1, 0, 0, 0, 0, 704, 53
26849, V, 1, 0, 0, 0, 0, 704, 53
26850, V, 1, 0, 0, 0, 0, 704, 53
26851, V, 1, 0, 0, 0, 0, 704, 53
26852, V, 1, 0, 0, 0, 0, 704, 52
26853, V, 1, 0, 0, 0, 0, 704, 52
26854, V, 1, 0, 0, 0, 0, 704, 52
26855, V, 1, 0, 0, 0, 0, 704, 53
26856, V, 1, 0, 0, 0, 0, 704, 53
26857, V, 1, 0, 0, 0, 0, 704, 53
26858, V, 1, 0, 0, 0, 0, 704, 53
26859, V, 1, 0, 0, 0, 0, 704, 52
26860, V, 1, 0, 0, 0, 0, 704, 52
26861, V, 1, 0, 0, 0, 0, 704, 53
26862, V, 1, 0, 0, 0, 0, 704, 53
26863, V, 1, 0, 0, 0, 0, 704, 52
26864, V, 1, 0, 0, 0, 0, 704, 53
26865, V, 1, 0, 0, 0, 0, 704, 53
26866, V, 1, 0, 0, 0, 0, 704, 53
26867, V, 1, 0, 0, 0, 0, 704, 53
26868, V, 1, 0, 0, 0, 0, 704, 53
26869, V, 1, 0, 0, 0, 0, 704, 52
26870, V, 1, 0, 0, 0, 0, 704, 53
26871, V, 1, 0, 0, 0, 0, 704, 53
26872, V, 1, 0, 0, 0, 0, 704, 52
26873, V, 1, 0, 0, 0, 0, 704, 52
26874, V, 1, 0, 0, 0, 0, 704, 53
26875, V, 1, 0, 0, 0, 0, 704, 52
26876, V, 1, 0, 0, 0, 0, 704, 53
26877, V, 1, 0, 0, 0, 0, 704, 52
26878, V, 1, 0, 0, 0, 0, 704, 52
26880, V, 1, 0, 0, 0, 0, 704, 53
26881, V, 1, 0, 0, 0, 0, 704, 53
26882, V, 1, 0, 0, 0, 0, 704, 53
26883, V, 1, 0, 0, 0, 0, 704, 53
26884, V, 1, 0, 0, 0, 0, 704, 53
26885, V, 1, 0, 0, 0, 0, 704, 53
26886, V, 1, 0, 0, 0, 0, 704, 53
26887, V, 1, 0, 0, 0, 0, 704, 52
26888, V, 1, 0, 0, 0, 0, 704, 53
26889, V, 1, 0, 0, 0, 0, 704, 52
26890, V, 1, 0, 0, 0, 0, 704, 53
26891, V, 1, 0, 0, 0, 0, 704, 53
26892, V, 1, 0, 0, 0, 0, 704, 53
26893, V, 1, 0, 0, 0, 0, 704, 52
26894, V, 1, 0, 0, 0, 0, 704, 52
26895, V, 1, 0, 0, 0, 0, 704, 52
26896, V, 1, 0, 0, 0, 0, 704, 53
26897, V, 1, 0, 0, 0, 0, 704, 53
26898, V, 1, 0, 0, 0, 0, 704, 52
26899, V, 1, 0, 0, 0, 0, 704, 52
26900, V, 1, 0, 0, 0, 0, 704, 52
26901, V, 1, 0, 0, 0, 0, 704, 52
26902, V, 1, 0, 0, 0, 0, 704, 53
26903, V, 1, 0, 0, 0, 0, 704, 53
26904, V, 1, 0, 0, 0, 0, 704, 52
26905, V, 1, 0, 0, 0, 0, 704, 53
26906, V, 1, 0, 0, 0, 0, 704, 53
26907, V, 1, 0, 0, 0, 0, 704, 53
26908, V, 1, 0, 0, 0, 0, 704, 52
26909, V, 1, 0, 0, 0, 0, 704, 53
26910, V, 1, 0, 0, 0, 0, 704, 53
26911, V, 1, 0, 0, 0, 0, 704, 52
26912, V, 1, 0, 0, 0, 0, 704, 52
26913, V, 1, 0, 0, 0, 0, 704, 52
26914, V, 1, 0, 0, 0, 0, 704, 52
26915, V, 1, 0, 0, 0, 0, 704, 53
26916, V, 1, 0, 0, 0, 0, 704, 53
26917, V, 1, 0, 0, 0, 0, 704, 52
26918, V, 1, 0, 0, 0, 0, 704, 53
26919, V, 1, 0, 0, 0, 0, 704, 53
26920, V, 1, 0, 0, 0, 0, 704, 52
26921, V, 1, 0, 0, 0, 0, 704, 53
26923, V, 1, 0, 0, 0, 0, 704, 53
26924, V, 1, 0, 0, 0, 0, 704, 53
26925, V, 1, 0, 0, 0, 0, 704, 53
26926, V, 1, 0, 0, 0, 0, 704, 53
26927, V, 1, 0, 0, 0, 0, 704, 53
26928, V, 1, 0, 0, 0, 0, 704, 53
26929, V, 1, 0, 0, 0, 0, 704, 53
26930, V, 1, 0, 0, 0, 0, 704, 53
26931, V, 1, 0, 0, 0, 0, 704, 52
26932, V, 1, 0, 0, 0, 0, 704, 52
26933, V, 1, 0, 0, 0, 0, 704, 52
26934, V, 1, 0, 0, 0, 0, 704, 52
26935, V, 1, 0, 0, 0, 0, 704, 53
26936, V, 1, 0, 0, 0, 0, 704, 53
26937, V, 1, 0, 0, 0, 0, 704, 52
26938, V, 1, 0, 0, 0, 0, 704, 52
26939, V, 1, 0, 0, 0, 0, 704, 52
26940, V, 1, 0, 0, 0, 0, 704, 53
26941, V, 1, 0, 0, 0, 0, 704, 53
26942, V, 1, 0, 0, 0, 0, 704, 53
26943, V, 1, 0, 0, 0, 0, 704, 53
26944, V, 1, 0, 0, 0, 0, 704, 53
26945, V, 1, 0, 0, 0, 0, 704, 53
26946, V, 1, 0, 0, 0, 0, 704, 53
26947, V, 1, 0, 0, 0, 0, 704, 53
26948, V, 1, 0, 0, 0, 0, 704, 53
26949, V, 1, 0, 0, 0, 0, 704, 52
26950, V, 1, 0, 0, 0, 0, 704, 52
26951, V, 1, 0, 0, 0, 0, 704, 53
26952, V, 1, 0, 0, 0, 0, 704, 53
26953, V, 1, 0, 0, 0, 0, 704, 52
26954, V, 1, 0, 0, 0, 0, 704, 53
26955, V, 1, 0, 0, 0, 0, 704, 53
26956, V, 1, 0, 0, 0, 0, 704, 52
26957, V, 1, 0, 0, 0, 0, 704, 52
26958, V, 1, 0, 0, 0, 0, 704, 53
26959, V, 1, 0, 0, 0, 0, 704, 53
26960, V, 1, 0, 0, 0, 0, 704, 53
26961, V, 1, 0, 0, 0, 0, 704, 53
26962, V, 1, 0, 0, 0, 0, 704, 53
26963, V, 1, 0, 0, 0, 0, 704, 53
26964, V, 1, 0, 0, 0, 0, 704, 53
26966, V, 1, 0, 0, 0, 0, 704, 53
26967, V, 1, 0, 0, 0, 0, 704, 53
26968, V, 1, 0, 0, 0, 0, 704, 53
26969, V, 1, 0, 0, 0, 0, 704, 53
26970, V, 1, 0, 0, 0, 0, 704, 53
26971, V, 1, 0, 0, 0, 0, 704, 53
26972, V, 1, 0, 0, 0, 0, 704, 53
26973, V, 1, 0, 0, 0, 0, 704, 52
26974, V, 1, 0, 0, 0, 0, 704, 53
26975, V, 1, 0, 0, 0, 0, 704, 53
26976, V, 1, 0, 0, 0, 0, 704, 53
26977, V, 1, 0, 0, 0, 0, 704, 52
26978, V, 1, 0, 0, 0, 0, 704, 52
26979, V, 1, 0, 0, 0, 0, 704, 52
26980, V, 1, 0, 0, 0, 0, 704, 53
26981, V, 1, 0, 0, 0, 0, 704, 53
26982, V, 1, 0, 0, 0, 0, 704, 52
26983, V, 1, 0, 0, 0, 0, 704, 53
26984, V, 1, 0, 0, 0, 0, 704, 53
26985, V, 1, 0, 0, 0, 0, 704, 53
26986, V, 1, 0, 0, 0, 0, 704, 53
26987, V, 1, 0, 0, 0, 0, 704, 53
26988, V, 1, 0, 0, 0, 0, 704, 52
26989, V, 1, 0, 0, 0, 0, 704, 53
26990, V, 1, 0, 0, 0, 0, 704, 53
26991, V, 1, 0, 0, 0, 0, 704, 53
26992, V, 1, 0, 0, 0, 0, 704, 52
26993, V, 1, 0, 0, 0, 0, 704, 52
26994, V, 1, 0, 0, 0, 0, 704, 53
26995, V, 1, 0, 0, 0, 0, 704, 52
26996, V, 1, 0, 0, 0, 0, 704, 53
26997, V, 1, 0, 0, 0, 0, 704, 53
26998, V, 1, 0, 0, 0, 0, 704, 52
26999, V, 1, 0, 0, 0, 0, 704, 53
27000, V, 1, 0, 0, 0, 0, 704, 53
27001, V, 1, 0, 0, 0, 0, 704, 53
27002, V, 1, 0, 0, 0, 0, 704, 53
27003, V, 1, 0, 0, 0, 0, 704, 53
27004, V, 1, 0, 0, 0, 0, 704, 52
27005, V, 1, 0, 0, 0, 0, 704, 53
27006, V, 1, 0, 0, 0, 0, 704, 53
27008, V, 1, 0, 0, 0, 0, 704, 53
27009, V, 1, 0, 0, 0, 0, 704, 52
27010, V, 1, 0, 0, 0, 0, 704, 53
27011, V, 1, 0, 0, 0, 0, 704, 53
27012, V, 1, 0, 0, 0, 0, 704, 52
27013, V, 1, 0, 0, 0, 0, 704, 52
27014, V, 1, 0, 0, 0, 0, 704, 53
27015, V, 1, 0, 0, 0, 0, 704, 52
27016, V, 1, 0, 0, 0, 0, 704, 53
27017, V, 1, 0, 0, 0, 0, 704, 52
27018, V, 1, 0, 0, 0, 0, 704, 52
27019, V, 1, 0, 0, 0, 0, 704, 52
27020, V, 1, 0, 0, 0, 0, 704, 53
27021, V, 1, 0, 0, 0, 0, 704, 53
27022, V, 1, 0, 0, 0, 0, 704, 53
27023, V, 1, 0, 0, 0, 0, 704, 53
27024, V, 1, 0, 0, 0, 0, 704, 52
27025, V, 1, 0, 0, 0, 0, 704, 53
27026, V, 1, 0, 0, 0, 0, 704, 53
27027, V, 1, 0, 0, 0, 0, 704, 53
27028, V, 1, 0, 0, 0, 0, 704, 52
27029, V, 1, 0, 0, 0, 0, 704, 52
27030, V, 1, 0, 0, 0, 0, 704, 53
27031, V, 1, 0, 0, 0, 0, 704, 53
27032, V, 1, 0, 0, 0, 0, 704, 53
27033, V, 1, 0, 0, 0, 0, 704, 52
27034, V, 1, 0, 0, 0, 0, 704, 53
27035, V, 1, 0, 0, 0, 0, 704, 52
27036, V, 1, 0, 0, 0, 0, 704, 52
27037, V, 1, 0, 0, 0, 0, 704, 53
27038, V, 1, 0, 0, 0, 0, 704, 53
27039, V, 1, 0, 0, 0, 0, 704, 53
27040, V, 1, 0, 0, 0, 0, 704, 53
27041, V, 1, 0, 0, 0, 0, 704, 53
27042, V, 1, 0, 0, 0, 0, 704, 53
27043, V, 1, 0, 0, 0, 0, 704, 53
27044, V, 1, 0, 0, 0, 0, 704, 53
27045, V, 1, 0, 0, 0, 0, 704, 53
27046, V, 1, 0, 0, 0, 0, 704, 53
27047, V, 1, 0, 0, 0, 0, 704, 53
27048, V, 1, 0, 0, 0, 0, 704, 53
27049, V, 1, 0, 0, 0, 0, 704, 53
27051, V, 1, 0, 0, 0, 0, 704, 53
27052, V, 1, 0, 0, 0, 0, 704, 53
27053, V, 1, 0, 0, 0, 0, 704, 53
27054, V, 1, 0, 0, 0, 0, 704, 53
27055, V, 1, 0, 0, 0, 0, 704, 53
27056, V, 1, 0, 0, 0, 0, 704, 53
27057, V, 1, 0, 0, 0, 0, 704, 53
27058, V, 1, 0, 0, 0, 0, 704, 53
27059, V, 1, 0, 0, 0, 0, 704, 53
27060, V, 1, 0, 0, 0, 0, 704, 53
27061, V, 1, 0, 0, 0, 0, 704, 53
27062, V, 1, 0, 0, 0, 0, 704, 53
27063, V, 1, 0, 0, 0, 0, 704, 54
27064, V, 1, 0, 0, 0, 0, 704, 54
27065, V, 1, 0, 0, 0, 0, 704, 54
27066, V, 1, 0, 0, 0, 0, 704, 54
27067, V, 1, 0, 0, 0, 0, 704, 54
27068, V, 1, 0, 0, 0, 0, 704, 54
27069, V, 1, 0, 0, 0, 0, 704, 54
27070, V, 1, 0, 0, 0, 0, 704, 54
27071, V, 1, 0, 0, 0, 0, 704, 54
27072, V, 1, 0, 0, 0, 0, 704, 54
27073, V, 1, 0, 0, 0, 0, 704, 54
27074, V, 1, 0, 0, 0, 0, 704, 54
27075, V, 1, 0, 0, 0, 0, 704, 54
27076, V, 1, 0, 0, 0, 0, 704, 54
27077, V, 1, 0, 0, 0, 0, 704, 54
27078, V, 1, 0, 0, 0, 0, 704, 54
27079, V, 1, 0, 0, 0, 0, 704, 54
27080, V, 1, 0, 0, 0, 0, 704, 54
27081, V, 1, 0, 0, 0, 0, 704, 54
27082, V, 1, 0, 0, 0, 0, 704, 54
27083, V, 1, 0, 0, 0, 0, 704, 54
27084, V, 1, 0, 0, 0, 0, 704, 54
27085, V, 1, 0, 0, 0, 0, 704, 54
27086, V, 1, 0, 0, 0, 0, 704, 54
27087, V, 1, 0, 0, 0, 0, 704, 54
27088, V, 1, 0, 0, 0, 0, 704, 54
27089, V, 1, 0, 0, 0, 0, 704, 54
27090, V, 1, 0, 0, 0, 0, 704, 54
27091, V, 1, 0, 0, 0, 0, 704, 54
27092, V, 1, 0, 0, 0, 0, 704, 54
27094, V, 1, 0, 0, 0, 0, 704, 54
27095, V, 1, 0, 0, 0, 0, 704, 54
27096, V, 1, 0, 0, 0, 0, 704, 54
27097, V, 1, 0, 0, 0, 0, 704, 54
27098, V, 1, 0, 0, 0, 0, 704, 54
27099, V, 1, 0, 0, 0, 0, 704, 54
27100, V, 1, 0, 0, 0, 0, 704, 54
27101, V, 1, 0, 0, 0, 0, 704, 54
27102, V, 1, 0, 0, 0, 0, 704, 54
27103, V, 1, 0, 0, 0, 0, 704, 54
27104, V, 1, 0, 0, 0, 0, 704, 54
27105, V, 1, 0, 0, 0, 0, 704, 54
27106, V, 1, 0, 0, 0, 0, 704, 54
27107, V, 1, 0, 0, 0, 0, 704, 54
27108, V, 1, 0, 0, 0, 0, 704, 54
27109, V, 1, 0, 0, 0, 0, 704, 54
27110, V, 1, 0, 0, 0, 0, 704, 54
27111, V, 1, 0, 0, 0, 0, 704, 54
27112, V, 1, 0, 0, 0, 0, 704, 54
27113, V, 1, 0, 0, 0, 0, 704, 54
27114, V, 1, 0, 0, 0, 0, 704, 54
27115, V, 1, 0, 0, 0, 0, 704, 54
27116, V, 1, 0, 0, 0, 0, 704, 54
27117, V, 1, 0, 0, 0, 0, 704, 54
27118, V, 1, 0, 0, 0, 0, 704, 54
27119, V, 1, 0, 0, 0, 0, 704, 54
27120, V, 1, 0, 0, 0, 0, 704, 54
27121, V, 1, 0, 0, 0, 0, 704, 54
27122, V, 1, 0, 0, 0, 0, 704, 54
27123, V, 1, 0, 0, 0, 0, 704, 54
27124, V, 1, 0, 0, 0, 0, 704, 54
27125, V, 1, 0, 0, 0, 0, 704, 54
27126, V, 1, 0, 0, 0, 0, 704, 54
27127, V, 1, 0, 0, 0, 0, 704, 54
27128, V, 1, 0, 0, 0, 0, 704, 54
27129, V, 1, 0, 0, 0, 0, 704, 54
27130, V, 1, 0, 0, 0, 0, 704, 54
27131, V, 1, 0, 0, 0, 0, 704, 54
27132, V, 1, 0, 0, 0, 0, 704, 54
27133, V, 1, 0, 0, 0, 0, 704, 54
27134, V, 1, 0, 0, 0, 0, 704, 54
27136, V, 1, 0, 0, 0, 0, 704, 54
27137, V, 1, 0, 0, 0, 0, 704, 54
27138, V, 1, 0, 0, 0, 0, 704, 54
27139, V, 1, 0, 0, 0, 0, 704, 54
27140, V, 1, 0, 0, 0, 0, 704, 54
27141, V, 1, 0, 0, 0, 0, 704, 54
27142, V, 1, 0, 0, 0, 0, 704, 54
27143, V, 1, 0, 0, 0, 0, 704, 54
27144, V, 1, 0, 0, 0, 0, 704, 54
27145, V, 1, 0, 0, 0, 0, 704, 54
27146, V, 1, 0, 0, 0, 0, 704, 54
27147, V, 1, 0, 0, 0, 0, 704, 54
27148, V, 1, 0, 0, 0, 0, 704, 54
27149, V, 1, 0, 0, 0, 0, 704, 54
27150, V, 1, 0, 0, 0, 0, 704, 54
27151, V, 1, 0, 0, 0, 0, 704, 54
27152, V, 1, 0, 0, 0, 0, 704, 54
27153, V, 1, 0, 0, 0, 0, 704, 54
27154, V, 1, 0, 0, 0, 0, 704, 54
27155, V, 1, 0, 0, 0, 0, 704, 55
27156, V, 1, 0, 0, 0, 0, 704, 54
27157, V, 1, 0, 0, 0, 0, 704, 54
27158, V, 1, 0, 0, 0, 0, 704, 54
27159, V, 1, 0, 0, 0, 0, 704, 55
27160, V, 1, 0, 0, 0, 0, 704, 54
27161, V, 1, 0, 0, 0, 0, 704, 55
27162, V, 1, 0, 0, 0, 0, 704, 55
27163, V, 1, 0, 0, 0, 0, 704, 55
27164, V, 1, 0, 0, 0, 0, 704, 55
27165, V, 1, 0, 0, 0, 0, 704, 55
27166, V, 1, 0, 0, 0, 0, 704, 55
27167, V, 1, 0, 0, 0, 0, 704, 55
27168, V, 1, 0, 0, 0, 0, 704, 55
27169, V, 1, 0, 0, 0, 0, 704, 55
27170, V, 1, 0, 0, 0, 0, 704, 55
27171, V, 1, 0, 0, 0, 0, 704, 55
27172, V, 1, 0, 0, 0, 0, 704, 55
27173, V, 1, 0, 0, 0, 0, 704, 55
27174, V, 1, 0, 0, 0, 0, 704, 55
27175, V, 1, 0, 0, 0, 0, 704, 55
27176, V, 1, 0, 0, 0, 0, 704, 55
27177, V, 1, 0, 0, 0, 0, 704, 55
27179, V, 1, 0, 0, 0, 0, 704, 55
27180, V, 1, 0, 0, 0, 0, 704, 55
27181, V, 1, 0, 0, 0, 0, 704, 55
27182, V, 1, 0, 0, 0, 0, 704, 55
27183, V, 1, 0, 0, 0, 0, 704, 55
27184, V, 1, 0, 0, 0, 0, 704, 55
27185, V, 1, 0, 0, 0, 0, 704, 55
27186, V, 1, 0, 0, 0, 0, 704, 55
27187, V, 1, 0, 0, 0, 0, 704, 55
27188, V, 1, 0, 0, 0, 0, 704, 55
27189, V, 1, 0, 0, 0, 0, 704, 55
27190, V, 1, 0, 0, 0, 0, 704, 55
27191, V, 1, 0, 0, 0, 0, 704, 55
27192, V, 1, 0, 0, 0, 0, 704, 55
27193, V, 1, 0, 0, 0, 0, 704, 55
27194, V, 1, 0, 0, 0, 0, 704, 55
27195, V, 1, 0, 0, 0, 0, 704, 55
27196, V, 1, 0, 0, 0, 0, 704, 55
27197, V, 1, 0, 0, 0, 0, 704, 55
27198, V, 1, 0, 0, 0, 0, 704, 55
27199, V, 1, 0, 0, 0, 0, 704, 55
27200, V, 1, 0, 0, 0, 0, 704, 55
27201, V, 1, 0, 0, 0, 0, 704, 55
27202, V, 1, 0, 0, 0, 0, 704, 55
27203, V, 1, 0, 0, 0, 0, 704, 55
27204, V, 1, 0, 0, 0, 0, 704, 55
27205, V, 1, 0, 0, 0, 0, 704, 55
27206, V, 1, 0, 0, 0, 0, 704, 55
27207, V, 1, 0, 0, 0, 0, 704, 55
27208, V, 1, 0, 0, 0, 0, 704, 55
27209, V, 1, 0, 0, 0, 0, 704, 55
27210, V, 1, 0, 0, 0, 0, 704, 55
27211, V, 1, 0, 0, 0, 0, 704, 55
27212, V, 1, 0, 0, 0, 0, 704, 55
27213, V, 1, 0, 0, 0, 0, 704, 55
27214, V, 1, 0, 0, 0, 0, 704, 55
27215, V, 1, 0, 0, 0, 0, 704, 55
27216, V, 1, 0, 0, 0, 0, 704, 56
27217, V, 1, 0, 0, 0, 0, 704, 56
27218, V, 1, 0, 0, 0, 0, 704, 56
27219, V, 1, 0, 0, 0, 0, 704, 56
27220, V, 1, 0, 0, 0, 0, 704, 56
27222, V, 1, 0, 0, 0, 0, 704, 56
27223, V, 1, 0, 0, 0, 0, 704, 56
27224, V, 1, 0, 0, 0, 0, 704, 56
27225, V, 1, 0, 0, 0, 0, 704, 57
27226, V, 1, 0, 0, 0, 0, 704, 57
27227, V, 1, 0, 0, 0, 0, 704, 57
27228, V, 1, 0, 0, 0, 0, 704, 57
27229, V, 1, 0, 0, 0, 0, 704, 57
27230, V, 1, 0, 0, 0, 0, 704, 58
27231, V, 1, 0, 0, 0, 0, 704, 58
27232, V, 1, 0, 0, 0, 0, 704, 58
27233, V, 1, 0, 0, 0, 0, 704, 58
27234, V, 1, 0, 0, 0, 0, 704, 58
27235, V, 1, 0, 0, 0, 0, 704, 58
27236, V, 1, 0, 0, 0, 0, 704, 59
27237, V, 1, 0, 0, 0, 0, 704, 59
27238, V, 1, 0, 0, 0, 0, 704, 59
27239, V, 1, 0, 0, 0, 0, 704, 59
27240, V, 1, 0, 0, 0, 0, 704, 59
27241, V, 1, 0, 0, 0, 0, 704, 60
27242, V, 1, 0, 0, 0, 0, 704, 60
27243, V, 1, 0, 0, 0, 0, 704, 60
27244, V, 1, 0, 0, 0, 0, 704, 60
27245, V, 1, 0, 0, 0, 0, 704, 60
27246, V, 1, 0, 0, 0, 0, 704, 60
27247, V, 1, 0, 0, 0, 0, 704, 60
27248, V, 1, 0, 0, 0, 0, 704, 61
27249, V, 1, 0, 0, 0, 0, 704, 61
27250, V, 1, 0, 0, 0, 0, 704, 61
27251, V, 1, 0, 0, 0, 0, 704, 61
27252, V, 1, 0, 0, 0, 0, 704, 61
27253, V, 1, 0, 0, 0, 0, 704, 61
27254, V, 1, 0, 0, 0, 0, 704, 61
27255, V, 1, 0, 0, 0, 0, 704, 61
27256, V, 1, 0, 0, 0, 0, 704, 61
27257, V, 1, 0, 0, 0, 0, 704, 62
27258, V, 1, 0, 0, 0, 0, 704, 62
27259, V, 1, 0, 0, 0, 0, 704, 62
27260, V, 1, 0, 0, 0, 0, 704, 62
27261, V, 1, 0, 0, 0, 0, 704, 62
27262, V, 1, 0, 0, 0, 0, 704, 62
27264, V, 1, 0, 0, 0, 0, 704, 62
27265, V, 1, 0, 0, 0, 0, 704, 62
27266, V, 1, 0, 0, 0, 0, 704, 62
27267, V, 1, 0, 0, 0, 0, 704, 63
27268, V, 1, 0, 0, 0, 0, 704, 63
27269, V, 1, 0, 0, 0, 0, 704, 63
27270, V, 1, 0, 0, 0, 0, 704, 63
27271, V, 1, 0, 0, 0, 0, 704, 63
27272, V, 1, 0, 0, 0, 0, 704, 63
27273, V, 1, 0, 0, 0, 0, 704, 63
27274, V, 1, 0, 0, 0, 0, 704, 63
27275, V, 1, 0, 0, 0, 0, 704, 63
27276, V, 1, 0, 0, 0, 0, 704, 63
27277, V, 1, 0, 0, 0, 0, 704, 64
27278, V, 1, 0, 0, 0, 0, 704, 64
27279, V, 1, 0, 0, 0, 0, 704, 64
27280, V, 1, 0, 0, 0, 0, 704, 64
27281, V, 1, 0, 0, 0, 0, 704, 64
27282, V, 1, 0, 0, 0, 0, 704, 64
27283, V, 1, 0, 0, 0, 0, 704, 64
27284, V, 1, 0, 0, 0, 0, 704, 64
27285, V, 1, 0, 0, 0, 0, 704, 64
27286, V, 1, 0, 0, 0, 0, 704, 64
27287, V, 1, 0, 0, 0, 0, 704, 64
27288, V, 1, 0, 0, 0, 0, 704, 64
27289, V, 1, 0, 0, 0, 0, 704, 65
27290, V, 1, 0, 0, 0, 0, 704, 65
27291, V, 1, 0, 0, 0, 0, 704, 65
27292, V, 1, 0, 0, 0, 0, 704, 65
27293, V, 1, 0, 0, 0, 0, 704, 65
27294, V, 1, 0, 0, 0, 0, 704, 65
27295, V, 1, 0, 0, 0, 0, 704, 65
27296, V, 1, 0, 0, 0, 0, 704, 65
27297, V, 1, 0, 0, 0, 0, 704, 65
27298, V, 1, 0, 0, 0, 0, 704, 65
27299, V, 1, 0, 0, 0, 0, 704, 65
27300, V, 1, 0, 0, 0, 0, 704, 66
27301, V, 1, 0, 0, 0, 0, 704, 66
27302, V, 1, 0, 0, 0, 0, 704, 66
27303, V, 1, 0, 0, 0, 0, 704, 66
27304, V, 1, 0, 0, 0, 0, 704, 66
27305, V, 1, 0, 0, 0, 0, 704, 66
27307, V, 1, 0, 0, 0, 0, 704, 66
27308, V, 1, 0, 0, 0, 0, 704, 66
27309, V, 1, 0, 0, 0, 0, 704, 66
27310, V, 1, 0, 0, 0, 0, 704, 66
27311, V, 1, 0, 0, 0, 0, 704, 66
27312, V, 1, 0, 0, 0, 0, 704, 66
27313, V, 1, 0, 0, 0, 0, 704, 66
27314, V, 1, 0, 0, 0, 0, 704, 67
27315, V, 1, 0, 0, 0, 0, 704, 67
27316, V, 1, 0, 0, 0, 0, 704, 67
27317, V, 1, 0, 0, 0, 0, 704, 67
27318, V, 1, 0, 0, 0, 0, 704, 67
27319, V, 1, 0, 0, 0, 0, 704, 67
27320, V, 1, 0, 0, 0, 0, 704, 67
27321, V, 1, 0, 0, 0, 0, 704, 67
27322, V, 1, 0, 0, 0, 0, 704, 67
27323, V, 1, 0, 0, 0, 0, 704, 67
27324, V, 1, 0, 0, 0, 0, 704, 67
27325, V, 1, 0, 0, 0, 0, 704, 67
27326, V, 1, 0, 0, 0, 0, 704, 67
27327, V, 1, 0, 0, 0, 0, 704, 68
27328, V, 1, 0, 0, 0, 0, 704, 68
27329, V, 1, 0, 0, 0, 0, 704, 68
27330, V, 1, 0, 0, 0, 0, 704, 68
27331, V, 1, 0, 0, 0, 0, 704, 68
27332, V, 1, 0, 0, 0, 0, 704, 68
27333, V, 1, 0, 0, 0, 0, 704, 68
27334, V, 1, 0, 0, 0, 0, 704, 68
27335, V, 1, 0, 0, 0, 0, 704, 68
27336, V, 1, 0, 0, 0, 0, 704, 68
27337, V, 1, 0, 0, 0, 0, 704, 68
27338, V, 1, 0, 0, 0, 0, 704, 68
27339, V, 1, 0, 0, 0, 0, 704, 68
27340, V, 1, 0, 0, 0, 0, 704, 68
27341, V, 1, 0, 0, 0, 0, 704, 68
27342, V, 1, 0, 0, 0, 0, 704, 68
27343, V, 1, 0, 0, 0, 0, 704, 68
27344, V, 1, 0, 0, 0, 0, 704, 68
27345, V, 1, 0, 0, 0, 0, 704, 68
27346, V, 1, 0, 0, 0, 0, 704, 69
27347, V, 1, 0, 0, 0, 0, 704, 69
27348, V, 1, 0, 0, 0, 0, 704, 69
27350, V, 1, 0, 0, 0, 0, 704, 69
27351, V, 1, 0, 0, 0, 0, 704, 69
27352, V, 1, 0, 0, 0, 0, 704, 69
27353, V, 1, 0, 0, 0, 0, 704, 69
27354, V, 1, 0, 0, 0, 0, 704, 69
27355, V, 1, 0, 0, 0, 0, 704, 69
27356, V, 1, 0, 0, 0, 0, 704, 69
27357, V, 1, 0, 0, 0, 0, 704, 69
27358, V, 1, 0, 0, 0, 0, 704, 69
27359, V, 1, 1, 0, 0, 0, 704, 69
27359, V, 1, 1, 0, 0, 0, 704, 69
27360, V, 1, 0, 0, 0, 0, 704, 69
27360, V, 1, 0, 0, 0, 0, 704, 69
27361, V, 1, 0, 0, 0, 0, 704, 69
27362, V, 1, 0, 0, 0, 0, 704, 69
27363, V, 1, 0, 0, 0, 0, 704, 69
27364, V, 1, 0, 0, 0, 0, 704, 69
27365, V, 1, 0, 0, 0, 0, 704, 70
27366, V, 1, 0, 0, 0, 0, 704, 70
27367, V, 1, 0, 0, 0, 0, 704, 70
27368, V, 1, 0, 0, 0, 0, 704, 70
27369, V, 1, 0, 0, 0, 0, 704, 70
27370, V, 1, 0, 0, 0, 0, 704, 70
27371, V, 1, 0, 0, 0, 0, 704, 70
27372, V, 1, 0, 0, 0, 0, 704, 70
27373, V, 1, 0, 0, 0, 0, 704, 70
27374, V, 1, 0, 0, 0, 0, 704, 70
27375, V, 1, 0, 0, 0, 0, 704, 69
27376, V, 1, 0, 0, 0, 0, 704, 69
27377, V, 1, 1, 0, 0, 0, 704, 69
27377, V, 1, 1, 0, 0, 0, 704, 69
27378, V, 1, 0, 0, 0, 0, 704, 70
27378, V, 1, 0, 0, 0, 0, 704, 70
27379, V, 1, 0, 0, 0, 0, 704, 69
27380, V, 1, 0, 0, 0, 0, 704, 69
27381, V, 1, 0, 0, 0, 0, 704, 70
27382, V, 1, 0, 0, 0, 0, 704, 70
27383, V, 1, 0, 0, 0, 0, 704, 70
27384, V, 1, 0, 0, 0, 0, 704, 70
27385, V, 1, 0, 0, 0, 0, 704, 70
27386, V, 1, 0, 0, 0, 0, 704, 70
27387, V, 1, 0, 0, 0, 0, 704, 70
27388, V, 1, 0, 0, 0, 0, 704, 70
27389, V, 1, 0, 0, 0, 0, 704, 70
27390, V, 1, 0, 0, 0, 0, 704, 70
27392, V, 1, 0, 0, 0, 0, 704, 70
27393, V, 1, 1, 0, 0, 0, 704, 70
27393, V, 1, 1, 0, 0, 0, 704, 70
27394, V, 1, 0, 0, 0, 0, 704, 70
27394, V, 1, 0, 0, 0, 0, 704, 70
27395, V, 1, 0, 0, 0, 0, 704, 70
27396, V, 1, 0, 0, 0, 0, 704, 70
27397, V, 1, 0, 0, 0, 0, 704, 70
27398, V, 1, 0, 0, 0, 0, 704, 70
27399, V, 1, 0, 0, 0, 0, 704, 70
27400, V, 1, 0, 0, 0, 0, 704, 70
27401, V, 1, 0, 0, 0, 0, 704, 70
27402, V, 1, 0, 0, 0, 0, 704, 70
27403, V, 1, 0, 0, 0, 0, 704, 70
27404, V, 1, 0, 0, 0, 0, 704, 70
27405, V, 1, 0, 0, 0, 0, 704, 70
27406, V, 1, 0, 0, 0, 0, 704, 70
27407, V, 1, 0, 0, 0, 0, 704, 70
27408, V, 1, 0, 0, 0, 0, 704, 70
27409, V, 1, 0, 0, 0, 0, 704, 70
27410, V, 1, 0, 0, 0, 0, 704, 70
27411, V, 1, 0, 0, 0, 0, 704, 70
27412, V, 1, 0, 0, 0, 0, 704, 70
27413, V, 1, 0, 0, 0, 0, 704, 70
27414, V, 1, 0, 0, 0, 0, 704, 70
27415, V, 1, 0, 0, 0, 0, 704, 70
27416, V, 1, 0, 0, 0, 0, 704, 70
27417, V, 1, 0, 0, 0, 0, 704, 70
27418, V, 1, 0, 0, 0, 0, 704, 70
27419, V, 1, 0, 0, 0, 0, 704, 70
27420, V, 1, 0, 0, 0, 0, 704, 70
27421, V, 1, 0, 0, 0, 0, 704, 70
27422, V, 1, 0, 0, 0, 0, 704, 70
27423, V, 1, 0, 0, 0, 0, 704, 70
27424, V, 1, 0, 0, 0, 0, 704, 70
27425, V, 1, 0, 0, 0, 0, 704, 70
27426, V, 1, 0, 0, 0, 0, 704, 70
27427, V, 1, 0, 0, 0, 0, 704, 70
27428, V, 1, 0, 0, 0, 0, 704, 70
27429, V, 1, 0, 0, 0, 0, 704, 70
27430, V, 1, 1, 0, 0, 0, 704, 70
27430, V, 1, 1, 0, 0, 0, 704, 70
27431, V, 1, 0, 0, 0, 0, 704, 70
27431, V, 1, 0, 0, 0, 0, 704, 70
27432, V, 1, 0, 0, 0, 0, 704, 70
27433, V, 1, 0, 0, 0, 0, 704, 70
27435, V, 1, 0, 0, 0, 0, 704, 70
27436, V, 1, 0, 0, 0, 0, 704, 70
27437, V, 1, 0, 0, 0, 0, 704, 70
27438, V, 1, 0, 0, 0, 0, 704, 70
27439, V, 1, 0, 0, 0, 0, 704, 70
27440, V, 1, 0, 0, 0, 0, 704, 70
27441, V, 1, 0, 0, 0, 0, 704, 70
27442, V, 1, 0, 0, 0, 0, 704, 70
27443, V, 1, 0, 0, 0, 0, 704, 70
27444, V, 1, 0, 0, 0, 0, 704, 70
27445, V, 1, 0, 0, 0, 0, 704, 70
27446, V, 1, 0, 0, 0, 0, 704, 70
27447, V, 1, 0, 0, 0, 0, 704, 70
27448, V, 1, 0, 0, 0, 0, 704, 70
27449, V, 1, 0, 0, 0, 0, 704, 70
27450, V, 1, 0, 0, 0, 0, 704, 70
27451, V, 1, 0, 0, 0, 0, 704, 70
27452, V, 1, 0, 0, 0, 0, 704, 70
27453, V, 1, 0, 0, 0, 0, 704, 70
27454, V, 1, 0, 0, 0, 0, 704, 70
27455, V, 1, 0, 0, 0, 0, 704, 70
27456, V, 1, 0, 0, 0, 0, 704, 70
27457, V, 1, 0, 0, 0, 0, 704, 70
27458, V, 1, 0, 0, 0, 0, 704, 70
27459, V, 1, 0, 0, 0, 0, 704, 70
27460, V, 1, 0, 0, 0, 0, 704, 70
27461, V, 1, 0, 0, 0, 0, 704, 70
27462, V, 1, 0, 0, 0, 0, 704, 70
27463, V, 1, 0, 0, 0, 0, 704, 70
27464, V, 1, 0, 0, 0, 0, 704, 70
27465, V, 1, 0, 0, 0, 0, 704, 70
27466, V, 1, 0, 0, 0, 0, 704, 70
27467, V, 1, 0, 0, 0, 0, 704, 70
27468, V, 1, 0, 0, 0, 0, 704, 70
27469, V, 1, 0, 0, 0, 0, 704, 70
27470, V, 1, 0, 0, 0, 0, 704, 70
27471, V, 1, 0, 0, 0, 0, 704, 70
27472, V, 1, 0, 0, 0, 0, 704, 70
27473, V, 1, 0, 0, 0, 0, 704, 70
27474, V, 1, 0, 0, 0, 0, 704, 70
27475, V, 1, 0, 0, 0, 0, 704, 70
27476, V, 1, 0, 0, 0, 0, 704, 70
27478, V, 1, 0, 0, 0, 0, 704, 70
27479, V, 1, 0, 0, 0, 0, 704, 70
27480, V, 1, 0, 0, 0, 0, 704, 69
27481, V, 1, 1, 0, 0, 0, 704, 70
27481, V, 1, 1, 0, 0, 0, 704, 70
27482, V, 1, 0, 0, 0, 0, 704, 70
27482, V, 1, 0, 0, 0, 0, 704, 70
27483, V, 1, 0, 0, 0, 0, 704, 69
27484, V, 1, 0, 0, 0, 0, 704, 70
27485, V, 1, 0, 0, 0, 0, 704, 70
27486, V, 1, 0, 0, 0, 0, 704, 70
27487, V, 1, 0, 0, 0, 0, 704, 70
27488, V, 1, 0, 0, 0, 0, 704, 70
27489, V, 1, 0, 0, 0, 0, 704, 70
27490, V, 1, 0, 0, 0, 0, 704, 70
27491, V, 1, 0, 0, 0, 0, 704, 70
27492, V, 1, 0, 0, 0, 0, 704, 70
27493, V, 1, 0, 0, 0, 0, 704, 70
27494, V, 1, 0, 0, 0, 0, 704, 70
27495, V, 1, 0, 0, 0, 0, 704, 70
27496, V, 1, 0, 0, 0, 0, 704, 70
27497, V, 1, 0, 0, 0, 0, 704, 70
27498, V, 1, 0, 0, 0, 0, 704, 70
27499, V, 1, 0, 0, 0, 0, 704, 70
27500, V, 1, 0, 0, 0, 0, 704, 70
27501, V, 1, 0, 0, 0, 0, 704, 70
27502, V, 1, 0, 0, 0, 0, 704, 70
27503, V, 1, 0, 0, 0, 0, 704, 70
27504, V, 1, 0, 0, 0, 0, 704, 70
27505, V, 1, 0, 0, 0, 0, 704, 69
27506, V, 1, 0, 0, 0, 0, 704, 69
27507, V, 1, 0, 0, 0, 0, 704, 69
27508, V, 1, 0, 0, 0, 0, 704, 69
27509, V, 1, 0, 0, 0, 0, 704, 69
27510, V, 1, 0, 0, 0, 0, 704, 69
27511, V, 1, 0, 0, 0, 0, 704, 69
27512, V, 1, 0, 0, 0, 0, 704, 69
27513, V, 1, 0, 0, 0, 0, 704, 69
27514, V, 1, 0, 0, 0, 0, 704, 69
27515, V, 1, 0, 0, 0, 0, 704, 69
27516, V, 1, 0, 0, 0, 0, 704, 69
27517, V, 1, 0, 0, 0, 0, 704, 69
27518, V, 1, 0, 0, 0, 0, 704, 69
27520, V, 1, 0, 0, 0, 0, 704, 69
27521, V, 1, 0, 0, 0, 0, 704, 69
27522, V, 1, 0, 0, 0, 0, 704, 69
27523, V, 1, 0, 0, 0, 0, 704, 69
27524, V, 1, 0, 0, 0, 0, 704, 69
27525, V, 1, 0, 0, 0, 0, 704, 69
27526, V, 1, 0, 0, 0, 0, 704, 69
27527, V, 1, 0, 0, 0, 0, 704, 69
27528, V, 1, 0, 0, 0, 0, 704, 69
27529, V, 1, 0, 0, 0, 0, 704, 69
27530, V, 1, 0, 0, 0, 0, 704, 69
27531, V, 1, 0, 0, 0, 0, 704, 69
27532, V, 1, 0, 0, 0, 0, 704, 69
27533, V, 1, 0, 0, 0, 0, 704, 69
27534, V, 1, 1, 0, 0, 0, 704, 69
27534, V, 1, 1, 0, 0, 0, 704, 69
27535, V, 1, 0, 0, 0, 0, 704, 69
27535, V, 1, 0, 0, 0, 0, 704, 69
27536, V, 1, 0, 0, 0, 0, 704, 69
27537, V, 1, 0, 0, 0, 0, 704, 69
27538, V, 1, 0, 0, 0, 0, 704, 69
27539, V, 1, 0, 0, 0, 0, 704, 69
27540, V, 1, 0, 0, 0, 0, 704, 69
27541, V, 1, 0, 0, 0, 0, 704, 69
27542, V, 1, 0, 0, 0, 0, 704, 69
27543, V, 1, 0, 0, 0, 0, 704, 70
27544, V, 1, 0, 0, 0, 0, 704, 70
27545, V, 1, 0, 0, 0, 0, 704, 69
27546, V, 1, 0, 0, 0, 0, 704, 70
27547, V, 1, 0, 0, 0, 0, 704, 70
27548, V, 1, 0, 0, 0, 0, 704, 69
27549, V, 1, 0, 0, 0, 0, 704, 69
27550, V, 1, 0, 0, 0, 0, 704, 69
27551, V, 1, 0, 0, 0, 0, 704, 69
27552, V, 1, 0, 0, 0, 0, 704, 69
27553, V, 1, 0, 0, 0, 0, 704, 69
27554, V, 1, 0, 0, 0, 0, 704, 69
27555, V, 1, 0, 0, 0, 0, 704, 69
27556, V, 1, 0, 0, 0, 0, 704, 69
27557, V, 1, 0, 0, 0, 0, 704, 69
27558, V, 1, 0, 0, 0, 0, 704, 69
27559, V, 1, 0, 0, 0, 0, 704, 69
27560, V, 1, 0, 0, 0, 0, 704, 69
27561, V, 1, 0, 0, 0, 0, 704, 69
27563, V, 1, 0, 0, 0, 0, 704, 69
27564, V, 1, 0, 0, 0, 0, 704, 69
27565, V, 1, 0, 0, 0, 0, 704, 69
27566, V, 1, 1, 0, 0, 0, 704, 69
27566, V, 1, 1, 0, 0, 0, 704, 69
27567, V, 1, 0, 0, 0, 0, 704, 69
27567, V, 1, 0, 0, 0, 0, 704, 69
27568, V, 1, 0, 0, 0, 0, 704, 69
27569, V, 1, 0, 0, 0, 0, 704, 69
27570, V, 1, 0, 0, 0, 0, 704, 69
27571, V, 1, 0, 0, 0, 0, 704, 70
27572, V, 1, 0, 0, 0, 0, 704, 70
27573, V, 1, 0, 0, 0, 0, 704, 70
27574, V, 1, 0, 0, 0, 0, 704, 70
27575, V, 1, 0, 0, 0, 0, 704, 70
27576, V, 1, 0, 0, 0, 0, 704, 70
27577, V, 1, 0, 0, 0, 0, 704, 70
27578, V, 1, 0, 0, 0, 0, 704, 70
27579, V, 1, 0, 0, 0, 0, 704, 70
27580, V, 1, 0, 0, 0, 0, 704, 70
27581, V, 1, 0, 0, 0, 0, 704, 70
27582, V, 1, 0, 0, 0, 0, 704, 70
27583, V, 1, 0, 0, 0, 0, 704, 70
27584, V, 1, 0, 0, 0, 0, 704, 70
27585, V, 1, 0, 0, 0, 0, 704, 70
27586, V, 1, 0, 0, 0, 0, 704, 70
27587, V, 1, 0, 0, 0, 0, 704, 70
27588, V, 1, 0, 0, 0, 0, 704, 70
27589, V, 1, 0, 0, 0, 0, 704, 70
27590, V, 1, 0, 0, 0, 0, 704, 70
27591, V, 1, 0, 0, 0, 0, 704, 70
27592, V, 1, 0, 0, 0, 0, 704, 70
27593, V, 1, 0, 0, 0, 0, 704, 70
27594, V, 1, 0, 0, 0, 0, 704, 70
27595, V, 1, 0, 0, 0, 0, 704, 70
27596, V, 1, 0, 0, 0, 0, 704, 70
27597, V, 1, 0, 0, 0, 0, 704, 70
27598, V, 1, 0, 0, 0, 0, 704, 70
27599, V, 1, 0, 0, 0, 0, 704, 70
27600, V, 1, 1, 0, 0, 0, 704, 70
27600, V, 1, 1, 0, 0, 0, 704, 70
27601, V, 1, 0, 0, 0, 0, 704, 70
27601, V, 1, 0, 0, 0, 0, 704, 70
27602, V, 1, 0, 0, 0, 0, 704, 70
27603, V, 1, 0, 0, 0, 0, 704, 70
27604, V, 1, 0, 0, 0, 0, 704, 70
27606, V, 1, 0, 0, 0, 0, 704, 70
27607, V, 1, 0, 0, 0, 0, 704, 70
27608, V, 1, 0, 0, 0, 0, 704, 70
27609, V, 1, 0, 0, 0, 0, 704, 70
27610, V, 1, 0, 0, 0, 0, 704, 70
27611, V, 1, 0, 0, 0, 0, 704, 70
27612, V, 1, 0, 0, 0, 0, 704, 70
27613, V, 1, 0, 0, 0, 0, 704, 70
27614, V, 1, 0, 0, 0, 0, 704, 70
27615, V, 1, 0, 0, 0, 0, 704, 70
27616, V, 1, 0, 0, 0, 0, 704, 70
27617, V, 1, 0, 0, 0, 0, 704, 70
27618, V, 1, 0, 0, 0, 0, 704, 70
27619, V, 1, 0, 0, 0, 0, 704, 70
27620, V, 1, 0, 0, 0, 0, 704, 70
27621, V, 1, 0, 0, 0, 0, 704, 70
27622, V, 1, 0, 0, 0, 0, 704, 70
27623, V, 1, 0, 0, 0, 0, 704, 70
27624, V, 1, 0, 0, 0, 0, 704, 70
27625, V, 1, 0, 0, 0, 0, 704, 70
27626, V, 1, 0, 0, 0, 0, 704, 70
27627, V, 1, 0, 0, 0, 0, 704, 70
27628, V, 1, 0, 0, 0, 0, 704, 70
27629, V, 1, 0, 0, 0, 0, 704, 70
27630, V, 1, 0, 0, 0, 0, 704, 70
27631, V, 1, 0, 0, 0, 0, 704, 70
27632, V, 1, 0, 0, 0, 0, 704, 70
27633, V, 1, 0, 0, 0, 0, 704, 70
27634, V, 1, 0, 0, 0, 0, 704, 70
27635, V, 1, 0, 0, 0, 0, 704, 70
27636, V, 1, 0, 0, 0, 0, 704, 70
27637, V, 1, 0, 0, 0, 0, 704, 70
27638, V, 1, 0, 0, 0, 0, 704, 70
27639, V, 1, 0, 0, 0, 0, 704, 70
27640, V, 1, 0, 0, 0, 0, 704, 70
27641, V, 1, 0, 0, 0, 0, 704, 70
27642, V, 1, 0, 0, 0, 0, 704, 70
27643, V, 1, 0, 0, 0, 0, 704, 70
27644, V, 1, 1, 0, 0, 0, 704, 70
27644, V, 1, 1, 0, 0, 0, 704, 70
27645, V, 1, 0, 0, 0, 0, 704, 70
27645, V, 1, 0, 0, 0, 0, 704, 70
27646, V, 1, 0, 0, 0, 0, 704, 70
27648, V, 1, 0, 0, 0, 0, 704, 70
27649, V, 1, 0, 0, 0, 0, 704, 70
27650, V, 1, 0, 0, 0, 0, 704, 70
27651, V, 1, 0, 0, 0, 0, 704, 70
27652, V, 1, 0, 0, 0, 0, 704, 70
27653, V, 1, 0, 0, 0, 0, 704, 70
27654, V, 1, 0, 0, 0, 0, 704, 70
27655, V, 1, 0, 0, 0, 0, 704, 70
27656, V, 1, 0, 0, 0, 0, 704, 70
27657, V, 1, 0, 0, 0, 0, 704, 70
27658, V, 1, 0, 0, 0, 0, 704, 70
27659, V, 1, 0, 0, 0, 0, 704, 70
27660, V, 1, 0, 0, 0, 0, 704, 70
27661, V, 1, 0, 0, 0, 0, 704, 70
27662, V, 1, 0, 0, 0, 0, 704, 70
27663, V, 1, 0, 0, 0, 0, 704, 70
27664, V, 1, 0, 0, 0, 0, 704, 70
27665, V, 1, 0, 0, 0, 0, 704, 70
27666, V, 1, 0, 0, 0, 0, 704, 70
27667, V, 1, 0, 0, 0, 0, 704, 70
27668, V, 1, 0, 0, 0, 0, 704, 70
27669, V, 1, 0, 0, 0, 0, 704, 70
27670, V, 1, 0, 0, 0, 0, 704, 70
27671, V, 1, 0, 0, 0, 0, 704, 70
27672, V, 1, 0, 0, 0, 0, 704, 70
27673, V, 1, 0, 0, 0, 0, 704, 70
27674, V, 1, 0, 0, 0, 0, 704, 70
27675, V, 1, 0, 0, 0, 0, 704, 70
27676, V, 1, 0, 0, 0, 0, 704, 70
27677, V, 1, 0, 0, 0, 0, 704, 70
27678, V, 1, 0, 0, 0, 0, 704, 70
27679, V, 1, 0, 0, 0, 0, 704, 70
27680, V, 1, 0, 0, 0, 0, 704, 70
27681, V, 1, 0, 0, 0, 0, 704, 70
27682, V, 1, 0, 0, 0, 0, 704, 70
27683, V, 1, 0, 0, 0, 0, 704, 70
27684, V, 1, 0, 0, 0, 0, 704, 70
27685, V, 1, 0, 0, 0, 0, 704, 70
27686, V, 1, 0, 0, 0, 0, 704, 70
27687, V, 1, 0, 0, 0, 0, 704, 70
27688, V, 1, 0, 0, 0, 0, 704, 70
27689, V, 1, 0, 0, 0, 0, 704, 70
27691, V, 1, 0, 0, 0, 0, 704, 70
27692, V, 1, 0, 0, 0, 0, 704, 69
27693, V, 1, 0, 0, 0, 0, 704, 69
27694, V, 1, 0, 0, 0, 0, 704, 69
27695, V, 1, 0, 0, 0, 0, 704, 69
27696, V, 1, 0, 0, 0, 0, 704, 69
27697, V, 1, 0, 0, 0, 0, 704, 69
27698, V, 1, 0, 0, 0, 0, 704, 69
27699, V, 1, 0, 0, 0, 0, 704, 69
27700, V, 1, 0, 0, 0, 0, 704, 69
27701, V, 1, 0, 0, 0, 0, 704, 69
27702, V, 1, 0, 0, 0, 0, 704, 69
27703, V, 1, 0, 0, 0, 0, 704, 69
27704, V, 1, 0, 0, 0, 0, 704, 69
27705, V, 1, 0, 0, 0, 0, 704, 69
27706, V, 1, 0, 0, 0, 0, 704, 69
27707, V, 1, 0, 0, 0, 0, 704, 69
27708, V, 1, 0, 0, 0, 0, 704, 69
27709, V, 1, 0, 0, 0, 0, 704, 69
27710, V, 1, 0, 0, 0, 0, 704, 69
27711, V, 1, 0, 0, 0, 0, 704, 69
27712, V, 1, 0, 0, 0, 0, 704, 69
27713, V, 1, 0, 0, 0, 0, 704, 68
27714, V, 1, 0, 0, 0, 0, 704, 68
27715, V, 1, 0, 0, 0, 0, 704, 68
27716, V, 1, 0, 0, 0, 0, 704, 68
27717, V, 1, 0, 0, 0, 0, 704, 68
27718, V, 1, 0, 0, 0, 0, 704, 68
27719, V, 1, 0, 0, 0, 0, 704, 68
27720, V, 1, 0, 0, 0, 0, 704, 68
27721, V, 1, 0, 0, 0, 0, 704, 68
27722, V, 1, 0, 0, 0, 0, 704, 68
27723, V, 1, 0, 0, 0, 0, 704, 68
27724, V, 1, 0, 0, 0, 0, 704, 68
27725, V, 1, 0, 0, 0, 0, 704, 68
27726, V, 1, 0, 0, 0, 0, 704, 68
27727, V, 1, 0, 0, 0, 0, 704, 68
27728, V, 1, 0, 0, 0, 0, 704, 68
27729, V, 1, 0, 0, 0, 0, 704, 68
27730, V, 1, 0, 0, 0, 0, 704, 68
27731, V, 1, 0, 0, 0, 0, 704, 68
27732, V, 1, 0, 0, 0, 0, 704, 68
27734, V, 1, 0, 0, 0, 0, 704, 68
27735, V, 1, 0, 0, 0, 0, 704, 68
27736, V, 1, 0, 0, 0, 0, 704, 68
27737, V, 1, 0, 0, 0, 0, 704, 68
27738, V, 1, 0, 0, 0, 0, 704, 68
27739, V, 1, 0, 0, 0, 0, 704, 68
27740, V, 1, 0, 0, 0, 0, 704, 68
27741, V, 1, 0, 0, 0, 0, 704, 67
27742, V, 1, 0, 0, 0, 0, 704, 67
27743, V, 1, 0, 0, 0, 0, 704, 67
27744, V, 1, 0, 0, 0, 0, 704, 67
27745, V, 1, 0, 0, 0, 0, 704, 67
27746, V, 1, 0, 0, 0, 0, 704, 67
27747, V, 1, 0, 0, 0, 0, 704, 67
27748, V, 1, 0, 0, 0, 0, 704, 67
27749, V, 1, 0, 0, 0, 0, 704, 67
27750, V, 1, 0, 0, 0, 0, 704, 67
27751, V, 1, 0, 0, 0, 0, 704, 67
27752, V, 1, 0, 0, 0, 0, 704, 67
27753, V, 1, 0, 0, 0, 0, 704, 67
27754, V, 1, 0, 0, 0, 0, 704, 67
27755, V, 1, 0, 0, 0, 0, 704, 67
27756, V, 1, 0, 0, 0, 0, 704, 67
27757, V, 1, 0, 0, 0, 0, 704, 67
27758, V, 1, 1, 0, 0, 0, 704, 67
27758, V, 1, 1, 0, 0, 0, 704, 67
27759, V, 1, 0, 0, 0, 0, 704, 67
27759, V, 1, 0, 0, 0, 0, 704, 67
27760, V, 1, 0, 0, 0, 0, 704, 67
27761, V, 1, 0, 0, 0, 0, 704, 67
27762, V, 1, 0, 0, 0, 0, 704, 67
27763, V, 1, 0, 0, 0, 0, 704, 67
27764, V, 1, 0, 0, 0, 0, 704, 67
27765, V, 1, 0, 0, 0, 0, 704, 67
27766, V, 1, 0, 0, 0, 0, 704, 67
27767, V, 1, 0, 0, 0, 0, 704, 67
27768, V, 1, 0, 0, 0, 0, 704, 67
27769, V, 1, 0, 0, 0, 0, 704, 67
27770, V, 1, 0, 0, 0, 0, 704, 67
27771, V, 1, 0, 0, 0, 0, 704, 67
27772, V, 1, 0, 0, 0, 0, 704, 67
27773, V, 1, 0, 0, 0, 0, 704, 67
27774, V, 1, 0, 0, 0, 0, 704, 67
27776, V, 1, 0, 0, 0, 0, 704, 67
27777, V, 1, 0, 0, 0, 0, 704, 67
27778, V, 1, 0, 0, 0, 0, 704, 67
27779, V, 1, 0, 0, 0, 0, 704, 67
27780, V, 1, 0, 0, 0, 0, 704, 67
27781, V, 1, 0, 0, 0, 0, 704, 67
27782, V, 1, 0, 0, 0, 0, 704, 67
27783, V, 1, 0, 0, 0, 0, 704, 67
27784, V, 1, 0, 0, 0, 0, 704, 67
27785, V, 1, 0, 0, 0, 0, 704, 67
27786, V, 1, 0, 0, 0, 0, 704, 67
27787, V, 1, 0, 0, 0, 0, 704, 67
27788, V, 1, 0, 0, 0, 0, 704, 67
27789, V, 1, 0, 0, 0, 0, 704, 67
27790, V, 1, 0, 0, 0, 0, 704, 67
27791, V, 1, 0, 0, 0, 0, 704, 67
27792, V, 1, 0, 0, 0, 0, 704, 67
27793, V, 1, 0, 0, 0, 0, 704, 67
27794, V, 1, 0, 0, 0, 0, 704, 67
27795, V, 1, 0, 0, 0, 0, 704, 67
27796, V, 1, 0, 0, 0, 0, 704, 67
27797, V, 1, 0, 0, 0, 0, 704, 67
27798, V, 1, 0, 0, 0, 0, 704, 67
27799, V, 1, 0, 0, 0, 0, 704, 67
27800, V, 1, 0, 0, 0, 0, 704, 67
27801, V, 1, 0, 0, 0, 0, 704, 67
27802, V, 1, 0, 0, 0, 0, 704, 67
27803, V, 1, 0, 0, 0, 0, 704, 67
27804, V, 1, 0, 0, 0, 0, 704, 67
27805, V, 1, 0, 0, 0, 0, 704, 67
27806, V, 1, 0, 0, 0, 0, 704, 67
27807, V, 1, 0, 0, 0, 0, 704, 67
27808, V, 1, 0, 0, 0, 0, 704, 67
27809, V, 1, 0, 0, 0, 0, 704, 66
27810, V, 1, 0, 0, 0, 0, 704, 66
27811, V, 1, 0, 0, 0, 0, 704, 66
27812, V, 1, 0, 0, 0, 0, 704, 66
27813, V, 1, 0, 0, 0, 0, 704, 66
27814, V, 1, 0, 0, 0, 0, 704, 66
27815, V, 1, 0, 0, 0, 0, 704, 66
27816, V, 1, 0, 0, 0, 0, 704, 66
27817, V, 1, 0, 0, 0, 0, 704, 66
27819, V, 1, 0, 0, 0, 0, 704, 66
27820, V, 1, 0, 0, 0, 0, 704, 66
27821, V, 1, 0, 0, 0, 0, 704, 66
27822, V, 1, 0, 0, 0, 0, 704, 66
27823, V, 1, 0, 0, 0, 0, 704, 66
27824, V, 1, 0, 0, 0, 0, 704, 66
27825, V, 1, 0, 0, 0, 0, 704, 66
27826, V, 1, 0, 0, 0, 0, 704, 66
27827, V, 1, 0, 0, 0, 0, 704, 66
27828, V, 1, 1, 0, 0, 0, 704, 66
27828, V, 1, 1, 0, 0, 0, 704, 66
27829, V, 1, 0, 0, 0, 0, 704, 66
27829, V, 1, 0, 0, 0, 0, 704, 66
27830, V, 1, 0, 0, 0, 0, 704, 66
27831, V, 1, 0, 0, 0, 0, 704, 66
27832, V, 1, 0, 0, 0, 0, 704, 66
27833, V, 1, 0, 0, 0, 0, 704, 66
27834, V, 1, 0, 0, 0, 0, 704, 66
27835, V, 1, 0, 0, 0, 0, 704, 67
27836, V, 1, 0, 0, 0, 0, 704, 67
27837, V, 1, 0, 0, 0, 0, 704, 67
27838, V, 1, 0, 0, 0, 0, 704, 67
27839, V, 1, 0, 0, 0, 0, 704, 67
27840, V, 1, 0, 0, 0, 0, 704, 67
27841, V, 1, 0, 0, 0, 0, 704, 67
27842, V, 1, 0, 0, 0, 0, 704, 67
27843, V, 1, 0, 0, 0, 0, 704, 67
27844, V, 1, 0, 0, 0, 0, 704, 67
27845, V, 1, 0, 0, 0, 0, 704, 67
27846, V, 1, 0, 0, 0, 0, 704, 67
27847, V, 1, 0, 0, 0, 0, 704, 67
27848, V, 1, 0, 0, 0, 0, 704, 67
27849, V, 1, 0, 0, 0, 0, 704, 67
27850, V, 1, 0, 0, 0, 0, 704, 67
27851, V, 1, 0, 0, 0, 0, 704, 66
27852, V, 1, 0, 0, 0, 0, 704, 66
27853, V, 1, 0, 0, 0, 0, 704, 66
27854, V, 1, 0, 0, 0, 0, 704, 66
27855, V, 1, 0, 0, 0, 0, 704, 66
27856, V, 1, 0, 0, 0, 0, 704, 66
27857, V, 1, 0, 0, 0, 0, 704, 66
27858, V, 1, 0, 0, 0, 0, 704, 66
27859, V, 1, 0, 0, 0, 0, 704, 66
27860, V, 1, 0, 0, 0, 0, 704, 66
27862, V, 1, 0, 0, 0, 0, 704, 66
27863, V, 1, 0, 0, 0, 0, 704, 66
27864, V, 1, 0, 0, 0, 0, 704, 66
27865, V, 1, 0, 0, 0, 0, 704, 66
27866, V, 1, 0, 0, 0, 0, 704, 66
27867, V, 1, 0, 0, 0, 0, 704, 66
27868, V, 1, 0, 0, 0, 0, 704, 66
27869, V, 1, 0, 0, 0, 0, 704, 66
27870, V, 1, 0, 0, 0, 0, 704, 66
27871, V, 1, 0, 0, 0, 0, 704, 66
27872, V, 1, 0, 0, 0, 0, 704, 66
27873, V, 1, 0, 0, 0, 0, 704, 66
27874, V, 1, 0, 0, 0, 0, 704, 66
27875, V, 1, 0, 0, 0, 0, 704, 66
27876, V, 1, 0, 0, 0, 0, 704, 66
27877, V, 1, 0, 0, 0, 0, 704, 66
27878, V, 1, 1, 0, 0, 0, 704, 66
27878, V, 1, 1, 0, 0, 0, 704, 66
27879, V, 1, 0, 0, 0, 0, 704, 66
27879, V, 1, 0, 0, 0, 0, 704, 66
27880, V, 1, 0, 0, 0, 0, 704, 66
27881, V, 1, 0, 0, 0, 0, 704, 66
27882, V, 1, 0, 0, 0, 0, 704, 66
27883, V, 1, 0, 0, 0, 0, 704, 66
27884, V, 1, 0, 0, 0, 0, 704, 66
27885, V, 1, 0, 0, 0, 0, 704, 67
27886, V, 1, 0, 0, 0, 0, 704, 67
27887, V, 1, 0, 0, 0, 0, 704, 67
27888, V, 1, 0, 0, 0, 0, 704, 67
27889, V, 1, 0, 0, 0, 0, 704, 67
27890, V, 1, 0, 0, 0, 0, 704, 67
27891, V, 1, 0, 0, 0, 0, 704, 67
27892, V, 1, 0, 0, 0, 0, 704, 67
27893, V, 1, 0, 0, 0, 0, 704, 67
27894, V, 1, 0, 0, 0, 0, 704, 67
27895, V, 1, 0, 0, 0, 0, 704, 67
27896, V, 1, 0, 0, 0, 0, 704, 66
27897, V, 1, 0, 0, 0, 0, 704, 66
27898, V, 1, 0, 0, 0, 0, 704, 67
27899, V, 1, 0, 0, 0, 0, 704, 67
27900, V, 1, 0, 0, 0, 0, 704, 66
27901, V, 1, 0, 0, 0, 0, 704, 66
27902, V, 1, 0, 0, 0, 0, 704, 67
27904, V, 1, 0, 0, 0, 0, 704, 67
27905, V, 1, 0, 0, 0, 0, 704, 67
27906, V, 1, 0, 0, 0, 0, 704, 67
27907, V, 1, 0, 0, 0, 0, 704, 67
27908, V, 1, 0, 0, 0, 0, 704, 66
27909, V, 1, 0, 0, 0, 0, 704, 67
27910, V, 1, 0, 0, 0, 0, 704, 67
27911, V, 1, 0, 0, 0, 0, 704, 67
27912, V, 1, 0, 0, 0, 0, 704, 67
27913, V, 1, 0, 0, 0, 0, 704, 67
27914, V, 1, 0, 0, 0, 0, 704, 67
27915, V, 1, 0, 0, 0, 0, 704, 67
27916, V, 1, 0, 0, 0, 0, 704, 67
27917, V, 1, 0, 0, 0, 0, 704, 67
27918, V, 1, 0, 0, 0, 0, 704, 67
27919, V, 1, 0, 0, 0, 0, 704, 67
27920, V, 1, 0, 0, 0, 0, 704, 67
27921, V, 1, 0, 0, 0, 0, 704, 67
27922, V, 1, 0, 0, 0, 0, 704, 67
27923, V, 1, 0, 0, 0, 0, 704, 67
27924, V, 1, 0, 0, 0, 0, 704, 67
27925, V, 1, 0, 0, 0, 0, 704, 67
27926, V, 1, 0, 0, 0, 0, 704, 67
27927, V, 1, 0, 0, 0, 0, 704, 67
27928, V, 1, 0, 0, 0, 0, 704, 67
27929, V, 1, 0, 0, 0, 0, 704, 67
27930, V, 1, 0, 0, 0, 0, 704, 67
27931, V, 1, 0, 0, 0, 0, 704, 68
27932, V, 1, 0, 0, 0, 0, 704, 68
27933, V, 1, 0, 0, 0, 0, 704, 68
27934, V, 1, 0, 0, 0, 0, 704, 68
27935, V, 1, 0, 0, 0, 0, 704, 68
27936, V, 1, 0, 0, 0, 0, 704, 68
27937, V, 1, 0, 0, 0, 0, 704, 68
27938, V, 1, 0, 0, 0, 0, 704, 68
27939, V, 1, 0, 0, 0, 0, 704, 68
27940, V, 1, 0, 0, 0, 0, 704, 68
27941, V, 1, 0, 0, 0, 0, 704, 68
27942, V, 1, 0, 0, 0, 0, 704, 68
27943, V, 1, 0, 0, 0, 0, 704, 68
27944, V, 1, 0, 0, 0, 0, 704, 68
27945, V, 1, 0, 0, 0, 0, 704, 68
27947, V, 1, 0, 0, 0, 0, 704, 68
27948, V, 1, 0, 0, 0, 0, 704, 68
27949, V, 1, 0, 0, 0, 0, 704, 68
27950, V, 1, 0, 0, 0, 0, 704, 68
27951, V, 1, 0, 0, 0, 0, 704, 68
27952, V, 1, 0, 0, 0, 0, 704, 68
27953, V, 1, 0, 0, 0, 0, 704, 68
27954, V, 1, 0, 0, 0, 0, 704, 68
27955, V, 1, 0, 0, 0, 0, 704, 68
27956, V, 1, 0, 0, 0, 0, 704, 68
27957, V, 1, 0, 0, 0, 0, 704, 68
27958, V, 1, 0, 0, 0, 0, 704, 69
27959, V, 1, 0, 0, 0, 0, 704, 69
27960, V, 1, 0, 0, 0, 0, 704, 69
27961, V, 1, 1, 0, 0, 0, 704, 69
27961, V, 1, 1, 0, 0, 0, 704, 69
27962, V, 1, 0, 0, 0, 0, 704, 69
27962, V, 1, 0, 0, 0, 0, 704, 69
27963, V, 1, 0, 0, 0, 0, 704, 69
27964, V, 1, 0, 0, 0, 0, 704, 69
27965, V, 1, 0, 0, 0, 0, 704, 69
27966, V, 1, 0, 0, 0, 0, 704, 69
27967, V, 1, 0, 0, 0, 0, 704, 69
27968, V, 1, 0, 0, 0, 0, 704, 70
27969, V, 1, 0, 0, 0, 0, 704, 70
27970, V, 1, 0, 0, 0, 0, 704, 70
27971, V, 1, 0, 0, 0, 0, 704, 70
27972, V, 1, 0, 0, 0, 0, 704, 70
27973, V, 1, 0, 0, 0, 0, 704, 70
27974, V, 1, 0, 0, 0, 0, 704, 70
27975, V, 1, 0, 0, 0, 0, 704, 70
27976, V, 1, 0, 0, 0, 0, 704, 70
27977, V, 1, 0, 0, 0, 0, 704, 70
27978, V, 1, 0, 0, 0, 0, 704, 70
27979, V, 1, 0, 0, 0, 0, 704, 70
27980, V, 1, 0, 0, 0, 0, 704, 70
27981, V, 1, 0, 0, 0, 0, 704, 70
27982, V, 1, 0, 0, 0, 0, 704, 70
27983, V, 1, 0, 0, 0, 0, 704, 70
27984, V, 1, 0, 0, 0, 0, 704, 70
27985, V, 1, 0, 0, 0, 0, 704, 70
27986, V, 1, 0, 0, 0, 0, 704, 70
27987, V, 1, 1, 0, 0, 0, 704, 70
27987, V, 1, 1, 0, 0, 0, 704, 70
27988, V, 1, 0, 0, 0, 0, 704, 70
27988, V, 1, 0, 0, 0, 0, 704, 70
27990, V, 1, 0, 0, 0, 0, 704, 70
27991, V, 1, 0, 0, 0, 0, 704, 70
27992, V, 1, 0, 0, 0, 0, 704, 70
27993, V, 1, 0, 0, 0, 0, 704, 70
27994, V, 1, 0, 0, 0, 0, 704, 70
27995, V, 1, 0, 0, 0, 0, 704, 71
27996, V, 1, 0, 0, 0, 0, 704, 71
27997, V, 1, 0, 0, 0, 0, 704, 71
27998, V, 1, 0, 0, 0, 0, 704, 71
27999, V, 1, 0, 0, 0, 0, 704, 71
28000, V, 1, 0, 0, 0, 0, 704, 71
28001, V, 1, 0, 0, 0, 0, 704, 71
28002, V, 1, 0, 0, 0, 0, 704, 71
28003, V, 1, 0, 0, 0, 0, 704, 71
28004, V, 1, 1, 0, 0, 0, 704, 71
28004, V, 1, 1, 0, 0, 0, 704, 71
28005, V, 1, 1, 1, 1, 0, 704, 72
28006, V, 1, 1, 1, 1, 0, 704, 72
28007, V, 1, 1, 1, 1, 0, 704, 72
28008, V, 1, 1, 1, 1, 0, 704, 72
28009, V, 1, 1, 1, 1, 0, 704, 73
28010, V, 1, 1, 1, 1, 0, 704, 73
28011, V, 1, 1, 1, 1, 0, 704, 74
28012, V, 1, 1, 1, 1, 0, 704, 75
28013, V, 1, 1, 1, 1, 0, 704, 75
28014, V, 1, 1, 1, 1, 0, 704, 76
28015, V, 1, 1, 1, 1, 0, 704, 77
28016, V, 1, 1, 1, 1, 0, 704, 78
28017, V, 1, 1, 1, 1, 0, 704, 78
28018, V, 1, 1, 1, 1, 0, 704, 79
28019, V, 1, 1, 1, 1, 0, 704, 80
28020, V, 1, 1, 1, 1, 0, 704, 80
28021, V, 1, 1, 1, 1, 0, 704, 81
28022, V, 1, 1, 1, 1, 0, 704, 81
28023, V, 1, 1, 1, 1, 0, 704, 82
28024, V, 1, 1, 1, 1, 0, 704, 82
28025, V, 1, 1, 1, 1, 0, 704, 83
28026, V, 1, 1, 1, 1, 0, 704, 83
28027, V, 1, 1, 1, 1, 0, 704, 84
28028, V, 1, 1, 1, 1, 0, 704, 84
28029, V, 1, 1, 1, 1, 0, 704, 85
28030, V, 1, 1, 1, 1, 0, 704, 85
28032, V, 1, 1, 1, 1, 0, 704, 86
28033, V, 1, 1, 1, 1, 0, 704, 86
28034, V, 1, 1, 1, 1, 0, 704, 87
28035, V, 1, 1, 1, 1, 0, 704, 87
28036, V, 1, 1, 1, 1, 0, 704, 88
28037, V, 1, 1, 1, 1, 0, 704, 88
28038, V, 1, 1, 1, 1, 0, 704, 88
28039, V, 1, 1, 1, 1, 0, 704, 89
28040, V, 1, 1, 1, 1, 0, 704, 89
28041, V, 1, 1, 1, 1, 0, 704, 89
28042, V, 1, 1, 1, 1, 0, 704, 90
28043, V, 1, 1, 1, 1, 0, 704, 90
28044, V, 1, 1, 1, 1, 0, 704, 90
28045, V, 1, 1, 1, 1, 0, 704, 91
28046, V, 1, 1, 1, 1, 0, 704, 91
28047, V, 1, 1, 1, 1, 0, 704, 91
28048, V, 1, 1, 1, 1, 0, 704, 91
28049, V, 1, 1, 1, 1, 0, 704, 92
28050, V, 1, 1, 1, 1, 0, 704, 92
28051, V, 1, 1, 1, 1, 0, 704, 92
28052, V, 1, 1, 1, 1, 0, 704, 92
28053, V, 1, 1, 1, 1, 0, 704, 93
28054, V, 1, 1, 1, 1, 0, 704, 93
28055, V, 1, 1, 1, 1, 0, 704, 93
28056, V, 1, 1, 1, 1, 0, 704, 93
28057, V, 1, 1, 1, 1, 0, 704, 93
28058, V, 1, 1, 1, 1, 0, 704, 94
28059, V, 1, 1, 1, 1, 0, 704, 94
28060, V, 1, 1, 1, 1, 0, 704, 94
28061, V, 1, 1, 1, 1, 0, 704, 94
28062, V, 1, 1, 1, 1, 0, 704, 94
28063, V, 1, 1, 1, 1, 0, 704, 94
28064, V, 1, 1, 1, 1, 0, 704, 95
28065, V, 1, 1, 1, 1, 0, 704, 95
28066, V, 1, 1, 1, 1, 0, 704, 95
28067, V, 1, 1, 1, 1, 0, 704, 95
28068, V, 1, 1, 1, 1, 0, 704, 95
28069, V, 1, 1, 1, 1, 0, 704, 95
28070, V, 1, 1, 1, 1, 0, 704, 96
28071, V, 1, 1, 1, 1, 0, 704, 96
28072, V, 1, 1, 1, 1, 0, 704, 96
28073, V, 1, 1, 1, 1, 0, 704, 96
28075, V, 1, 1, 1, 1, 0, 704, 96
28076, V, 1, 1, 1, 1, 0, 704, 96
28077, V, 1, 1, 1, 1, 0, 704, 96
28078, V, 1, 1, 1, 1, 0, 704, 96
28079, V, 1, 1, 1, 1, 0, 704, 96
28080, V, 1, 1, 1, 1, 0, 704, 97
28081, V, 1, 1, 1, 1, 0, 704, 97
28082, V, 1, 1, 1, 1, 0, 704, 97
28083, V, 1, 1, 1, 1, 0, 704, 97
28084, V, 1, 1, 1, 1, 0, 704, 97
28085, V, 1, 1, 1, 1, 0, 704, 97
28086, V, 1, 1, 1, 1, 0, 704, 97
28087, V, 1, 1, 1, 1, 0, 704, 97
28088, V, 1, 1, 1, 1, 0, 704, 97
28089, V, 1, 1, 1, 1, 0, 704, 97
28090, V, 1, 1, 1, 1, 0, 704, 97
28091, V, 1, 1, 1, 1, 0, 704, 98
28092, V, 1, 1, 1, 1, 0, 704, 98
28093, V, 1, 1, 1, 1, 0, 704, 98
28094, V, 1, 1, 1, 1, 0, 704, 98
28095, V, 1, 1, 1, 1, 0, 704, 98
28096, V, 1, 1, 1, 1, 0, 704, 98
28097, V, 1, 1, 1, 1, 0, 704, 98
28098, V, 1, 1, 1, 1, 0, 704, 98
28099, V, 1, 1, 1, 1, 0, 704, 98
28100, V, 1, 1, 1, 1, 0, 704, 98
28101, V, 1, 1, 1, 1, 0, 704, 98
28102, V, 1, 1, 1, 1, 0, 704, 98
28103, V, 1, 1, 1, 1, 0, 704, 98
28104, V, 1, 1, 1, 1, 0, 704, 98
28105, V, 1, 1, 1, 1, 0, 704, 98
28106, V, 1, 1, 1, 1, 0, 704, 98
28107, V, 1, 1, 1, 1, 0, 704, 99
28108, V, 1, 1, 1, 1, 0, 704, 99
28109, V, 1, 1, 1, 1, 0, 704, 99
28110, V, 1, 1, 1, 1, 0, 704, 99
28111, V, 1, 1, 1, 1, 0, 704, 99
28112, V, 1, 1, 1, 1, 0, 704, 99
28113, V, 1, 1, 1, 1, 0, 704, 99
28114, V, 1, 1, 1, 1, 0, 704, 99
28115, V, 1, 1, 1, 1, 0, 704, 99
28116, V, 1, 1, 1, 1, 0, 704, 99
28118, V, 1, 1, 1, 1, 0, 704, 99
28119, V, 1, 1, 1, 1, 0, 704, 99
28120, V, 1, 1, 1, 1, 0, 704, 99
28121, V, 1, 1, 1, 1, 0, 704, 99
28122, V, 1, 1, 1, 1, 0, 704, 99
28123, V, 1, 1, 1, 1, 0, 704, 99
28124, V, 1, 1, 1, 1, 0, 704, 99
28125, V, 1, 1, 1, 1, 0, 704, 99
28126, V, 1, 1, 1, 1, 0, 704, 99
28127, V, 1, 1, 1, 1, 0, 704, 99
28128, V, 1, 1, 1, 1, 0, 704, 99
28129, V, 1, 1, 1, 1, 0, 704, 99
28130, V, 1, 1, 1, 1, 0, 704, 100
28131, V, 1, 1, 1, 1, 0, 704, 100
28132, V, 1, 1, 1, 1, 0, 704, 100
28133, V, 1, 1, 1, 1, 0, 704, 100
28134, V, 1, 1, 1, 1, 0, 704, 100
28135, V, 1, 1, 1, 1, 0, 704, 100
28136, V, 1, 1, 1, 1, 0, 704, 100
28137, V, 1, 1, 1, 1, 0, 704, 100
28138, V, 1, 1, 1, 1, 0, 704, 100
28139, V, 1, 1, 1, 1, 0, 704, 100
28140, V, 1, 1, 1, 1, 0, 704, 100
28141, V, 1, 1, 1, 1, 0, 704, 100
28142, V, 1, 1, 1, 1, 0, 704, 100
28143, V, 1, 1, 1, 1, 0, 704, 100
28144, V, 1, 1, 1, 1, 0, 704, 100
28145, V, 1, 1, 1, 1, 0, 704, 100
28146, V, 1, 1, 1, 1, 0, 704, 100
28147, V, 1, 1, 1, 1, 0, 704, 100
28148, V, 1, 1, 1, 1, 0, 704, 100
28149, V, 1, 1, 1, 1, 0, 704, 100
28150, V, 1, 1, 1, 1, 0, 704, 100
28151, V, 1, 1, 1, 1, 0, 704, 100
28152, V, 1, 1, 1, 1, 0, 704, 100
28153, V, 1, 1, 1, 1, 0, 704, 100
28154, V, 1, 1, 1, 1, 0, 704, 100
28155, V, 1, 1, 1, 1, 0, 704, 100
28156, V, 1, 1, 1, 1, 0, 704, 100
28157, V, 1, 1, 1, 1, 0, 704, 100
28158, V, 1, 1, 1, 1, 0, 704, 100
28160, V, 1, 1, 1, 1, 0, 704, 100
28161, V, 1, 1, 1, 1, 0, 704, 100
28162, V, 1, 1, 1, 1, 0, 704, 100
28163, V, 1, 1, 1, 1, 0, 704, 100
28164, V, 1, 1, 1, 1, 0, 704, 100
28165, V, 1, 1, 1, 1, 0, 704, 100
28166, V, 1, 1, 1, 1, 0, 704, 100
28167, V, 1, 1, 1, 1, 0, 704, 100
28168, V, 1, 1, 1, 1, 0, 704, 100
28169, V, 1, 1, 1, 1, 0, 704, 100
28170, V, 1, 1, 1, 1, 0, 704, 100
28171, V, 1, 1, 1, 1, 0, 704, 100
28172, V, 1, 1, 1, 1, 0, 704, 100
28173, V, 1, 1, 1, 1, 0, 704, 100
28174, V, 1, 1, 1, 1, 0, 704, 100
28175, V, 1, 1, 1, 1, 0, 704, 100
28176, V, 1, 1, 1, 1, 0, 704, 100
28177, V, 1, 1, 1, 1, 0, 704, 100
28178, V, 1, 1, 1, 1, 0, 704, 100
28179, V, 1, 1, 1, 1, 0, 704, 100
28180, V, 1, 1, 1, 1, 0, 704, 100
28181, V, 1, 1, 1, 1, 0, 704, 100
28182, V, 1, 1, 1, 1, 0, 704, 100
28183, V, 1, 1, 1, 1, 0, 704, 100
28184, V, 1, 1, 1, 1, 0, 704, 100
28185, V, 1, 1, 1, 1, 0, 704, 100
28186, V, 1, 1, 1, 1, 0, 704, 100
28187, V, 1, 1, 1, 1, 0, 704, 100
28188, V, 1, 1, 1, 1, 0, 704, 100
28189, V, 1, 1, 1, 1, 0, 704, 100
28190, V, 1, 1, 1, 1, 0, 704, 100
28191, V, 1, 1, 1, 1, 0, 704, 100
28192, V, 1, 1, 1, 1, 0, 704, 100
28193, V, 1, 1, 1, 1, 0, 704, 100
28194, V, 1, 1, 1, 1, 0, 704, 100
28195, V, 1, 1, 1, 1, 0, 704, 100
28196, V, 1, 1, 1, 1, 0, 704, 100
28197, V, 1, 1, 1, 1, 0, 704, 100
28198, V, 1, 1, 1, 1, 0, 704, 100
28199, V, 1, 1, 1, 1, 0, 704, 100
28200, V, 1, 1, 1, 1, 0, 704, 100
28201, V, 1, 1, 1, 1, 0, 704, 100
28203, V, 1, 1, 1, 1, 0, 704, 100
28204, V, 1, 1, 1, 1, 0, 704, 100
28205, V, 1, 1, 1, 1, 0, 704, 100
28206, V, 1, 1, 1, 1, 0, 704, 100
28207, V, 1, 1, 1, 1, 0, 704, 100
28208, V, 1, 1, 1, 1, 0, 704, 100
28209, V, 1, 1, 1, 1, 0, 704, 100
28210, V, 1, 1, 1, 1, 0, 704, 100
28211, V, 1, 1, 1, 1, 0, 704, 100
28212, V, 1, 1, 1, 1, 0, 704, 100
28213, V, 1, 1, 1, 1, 0, 704, 100
28214, V, 1, 1, 1, 1, 0, 704, 100
28215, V, 1, 1, 1, 1, 0, 704, 100
28216, V, 1, 1, 1, 1, 0, 704, 100
28217, V, 1, 1, 1, 1, 0, 704, 100
28218, V, 1, 1, 1, 1, 0, 704, 100
28219, V, 1, 1, 1, 1, 0, 704, 100
28220, V, 1, 1, 1, 1, 0, 704, 100
28221, V, 1, 1, 1, 1, 0, 704, 100
28222, V, 1, 1, 1, 1, 0, 704, 100
28223, V, 1, 1, 1, 1, 0, 704, 100
28224, V, 1, 1, 1, 1, 0, 704, 100
28225, V, 1, 1, 1, 1, 0, 704, 100
28226, V, 1, 1, 1, 1, 0, 704, 100
28227, V, 1, 1, 1, 1, 0, 704, 100
28228, V, 1, 1, 1, 1, 0, 704, 100
28229, V, 1, 1, 1, 1, 0, 704, 100
28230, V, 1, 1, 1, 1, 0, 704, 100
28231, V, 1, 1, 1, 1, 0, 704, 100
28232, V, 1, 1, 1, 1, 0, 704, 100
28233, V, 1, 1, 1, 1, 0, 704, 100
28234, V, 1, 1, 1, 1, 0, 704, 100
28235, V, 1, 1, 1, 1, 0, 704, 100
28236, V, 1, 1, 1, 1, 0, 704, 100
28237, V, 1, 1, 1, 1, 0, 704, 100
28238, V, 1, 1, 1, 1, 0, 704, 100
28239, V, 1, 1, 1, 1, 0, 704, 100
28240, V, 1, 1, 1, 1, 0, 704, 100
28241, V, 1, 1, 1, 1, 0, 704, 100
28242, V, 1, 1, 1, 1, 0, 704, 100
28243, V, 1, 1, 1, 1, 0, 704, 100
28244, V, 1, 1, 1, 1, 0, 704, 100
28246, V, 1, 1, 1, 1, 0, 704, 100
28247, V, 1, 1, 1, 1, 0, 704, 100
28248, V, 1, 1, 1, 1, 0, 704, 100
28249, V, 1, 1, 1, 1, 0, 704, 100
28250, V, 1, 1, 1, 1, 0, 704, 100
28251, V, 1, 1, 1, 1, 0, 704, 100
28252, V, 1, 1, 1, 1, 0, 704, 100
28253, V, 1, 1, 1, 1, 0, 704, 100
28254, V, 1, 1, 1, 1, 0, 704, 100
28255, V, 1, 1, 1, 1, 0, 704, 100
28256, V, 1, 1, 1, 1, 0, 704, 100
28257, V, 1, 1, 1, 1, 0, 704, 100
28258, V, 1, 1, 1, 1, 0, 704, 100
28259, V, 1, 1, 1, 1, 0, 704, 100
28260, V, 1, 1, 1, 1, 0, 704, 100
28261, V, 1, 1, 1, 1, 0, 704, 100
28262, V, 1, 1, 1, 1, 0, 704, 100
28263, V, 1, 1, 1, 1, 0, 704, 100
28264, V, 1, 1, 1, 1, 0, 704, 101
28265, V, 1, 1, 1, 1, 0, 704, 100
28266, V, 1, 1, 1, 1, 0, 704, 101
28267, V, 1, 1, 1, 1, 0, 704, 101
28268, V, 1, 1, 1, 1, 0, 704, 100
28269, V, 1, 1, 1, 1, 0, 704, 101
28270, V, 1, 1, 1, 1, 0, 704, 100
28271, V, 1, 1, 1, 1, 0, 704, 100
28272, V, 1, 1, 1, 1, 0, 704, 101
28273, V, 1, 1, 1, 1, 0, 704, 101
28274, V, 1, 1, 1, 1, 0, 704, 101
28275, V, 1, 1, 1, 1, 0, 704, 101
28276, V, 1, 1, 1, 1, 0, 704, 101
28277, V, 1, 1, 1, 1, 0, 704, 101
28278, V, 1, 1, 1, 1, 0, 704, 101
28279, V, 1, 1, 1, 1, 0, 704, 101
28280, V, 1, 1, 1, 1, 0, 704, 101
28281, V, 1, 1, 1, 1, 0, 704, 101
28282, V, 1, 1, 1, 1, 0, 704, 101
28283, V, 1, 1, 1, 1, 0, 704, 101
28284, V, 1, 1, 1, 1, 0, 704, 101
28285, V, 1, 1, 1, 1, 0, 704, 101
28286, V, 1, 1, 1, 1, 0, 704, 101
28288, V, 1, 1, 1, 1, 0, 704, 101
28289, V, 1, 1, 1, 1, 0, 704, 101
28290, V, 1, 1, 1, 1, 0, 704, 101
28291, V, 1, 1, 1, 1, 0, 704, 101
28292, V, 1, 1, 1, 1, 0, 704, 101
28293, V, 1, 1, 1, 1, 0, 704, 101
28294, V, 1, 1, 1, 1, 0, 704, 101
28295, V, 1, 1, 1, 1, 0, 704, 101
28296, V, 1, 1, 1, 1, 0, 704, 101
28297, V, 1, 1, 1, 1, 0, 704, 101
28298, V, 1, 1, 1, 1, 0, 704, 101
28299, V, 1, 1, 1, 1, 0, 704, 101
28300, V, 1, 1, 1, 1, 0, 704, 101
28301, V, 1, 1, 1, 1, 0, 704, 101
28302, V, 1, 1, 1, 1, 0, 704, 101
28303, V, 1, 1, 1, 1, 0, 704, 101
28304, V, 1, 1, 1, 1, 0, 704, 100
28305, V, 1, 1, 1, 1, 0, 704, 101
28306, V, 1, 1, 1, 1, 0, 704, 101
28307, V, 1, 1, 1, 1, 0, 704, 101
28308, V, 1, 1, 1, 1, 0, 704, 100
28309, V, 1, 1, 1, 1, 0, 704, 100
28310, V, 1, 1, 1, 1, 0, 704, 101
28311, V, 1, 1, 1, 1, 0, 704, 100
28312, V, 1, 1, 1, 1, 0, 704, 101
28313, V, 1, 1, 1, 1, 0, 704, 100
28314, V, 1, 1, 1, 1, 0, 704, 100
28315, V, 1, 1, 1, 1, 0, 704, 100
28316, V, 1, 1, 1, 1, 0, 704, 100
28317, V, 1, 1, 1, 1, 0, 704, 101
28318, V, 1, 1, 1, 1, 0, 704, 100
28319, V, 1, 1, 1, 1, 0, 704, 100
28320, V, 1, 1, 1, 1, 0, 704, 100
28321, V, 1, 1, 1, 1, 0, 704, 100
28322, V, 1, 1, 1, 1, 0, 704, 100
28323, V, 1, 1, 1, 1, 0, 704, 100
28324, V, 1, 1, 1, 1, 0, 704, 100
28325, V, 1, 1, 1, 1, 0, 704, 100
28326, V, 1, 1, 1, 1, 0, 704, 100
28327, V, 1, 1, 1, 1, 0, 704, 100
28328, V, 1, 1, 1, 1, 0, 704, 100
28329, V, 1, 1, 1, 1, 0, 704, 100
28331, V, 1, 1, 1, 1, 0, 704, 100
28332, V, 1, 1, 1, 1, 0, 704, 100
28333, V, 1, 1, 1, 1, 0, 704, 100
28334, V, 1, 1, 1, 1, 0, 704, 100
28335, V, 1, 1, 1, 1, 0, 704, 100
28336, V, 1, 1, 1, 1, 0, 704, 100
28337, V, 1, 1, 1, 1, 0, 704, 100
28338, V, 1, 1, 1, 1, 0, 704, 100
28339, V, 1, 1, 1, 1, 0, 704, 100
28340, V, 1, 1, 1, 1, 0, 704, 100
28341, V, 1, 1, 1, 1, 0, 704, 100
28342, V, 1, 1, 1, 1, 0, 704, 100
28343, V, 1, 1, 1, 1, 0, 704, 101
28344, V, 1, 1, 1, 1, 0, 704, 101
28345, V, 1, 1, 1, 1, 0, 704, 101
28346, V, 1, 1, 1, 1, 0, 704, 101
28347, V, 1, 1, 1, 1, 0, 704, 101
28348, V, 1, 1, 1, 1, 0, 704, 101
28349, V, 1, 1, 1, 1, 0, 704, 100
28350, V, 1, 1, 1, 1, 0, 704, 101
28351, V, 1, 1, 1, 1, 0, 704, 101
28352, V, 1, 1, 1, 1, 0, 704, 101
28353, V, 1, 1, 1, 1, 0, 704, 101
28354, V, 1, 1, 1, 1, 0, 704, 101
28355, V, 1, 1, 1, 1, 0, 704, 101
28356, V, 1, 1, 1, 1, 0, 704, 101
28357, V, 1, 1, 1, 1, 0, 704, 101
28358, V, 1, 1, 1, 1, 0, 704, 101
28359, V, 1, 1, 1, 1, 0, 704, 101
28360, V, 1, 1, 1, 1, 0, 704, 101
28361, V, 1, 1, 1, 1, 0, 704, 101
28362, V, 1, 1, 1, 1, 0, 704, 101
28363, V, 1, 1, 1, 1, 0, 704, 101
28364, V, 1, 1, 1, 1, 0, 704, 101
28365, V, 1, 1, 1, 1, 0, 704, 101
28366, V, 1, 1, 1, 1, 0, 704, 101
28367, V, 1, 1, 1, 1, 0, 704, 101
28368, V, 1, 1, 1, 1, 0, 704, 101
28369, V, 1, 1, 1, 1, 0, 704, 101
28370, V, 1, 1, 1, 1, 0, 704, 101
28371, V, 1, 1, 1, 1, 0, 704, 101
28372, V, 1, 1, 1, 1, 0, 704, 101
28374, V, 1, 1, 1, 1, 0, 704, 101
28375, V, 1, 1, 1, 1, 0, 704, 101
28376, V, 1, 1, 1, 1, 0, 704, 101
28377, V, 1, 1, 1, 1, 0, 704, 101
28378, V, 1, 1, 1, 1, 0, 704, 101
28379, V, 1, 1, 1, 1, 0, 704, 101
28380, V, 1, 1, 1, 1, 0, 704, 101
28381, V, 1, 1, 1, 1, 0, 704, 101
28382, V, 1, 1, 1, 1, 0, 704, 100
28383, V, 1, 1, 1, 1, 0, 704, 101
28384, V, 1, 1, 1, 1, 0, 704, 101
28385, V, 1, 1, 1, 1, 0, 704, 101
28386, V, 1, 1, 1, 1, 0, 704, 101
28387, V, 1, 1, 1, 1, 0, 704, 101
28388, V, 1, 1, 1, 1, 0, 704, 101
28389, V, 1, 1, 1, 1, 0, 704, 101
28390, V, 1, 1, 1, 1, 0, 704, 100
28391, V, 1, 1, 1, 1, 0, 704, 100
28392, V, 1, 1, 1, 1, 0, 704, 100
28393, V, 1, 1, 1, 1, 0, 704, 100
28394, V, 1, 1, 1, 1, 0, 704, 100
28395, V, 1, 1, 1, 1, 0, 704, 100
28396, V, 1, 1, 1, 1, 0, 704, 100
28397, V, 1, 1, 1, 1, 0, 704, 100
28398, V, 1, 1, 1, 1, 0, 704, 100
28399, V, 1, 1, 1, 1, 0, 704, 100
28400, V, 1, 1, 1, 1, 0, 704, 100
28401, V, 1, 1, 1, 1, 0, 704, 100
28402, V, 1, 1, 1, 1, 0, 704, 100
28403, V, 1, 1, 1, 1, 0, 704, 101
28404, V, 1, 1, 1, 1, 0, 704, 100
28405, V, 1, 1, 1, 1, 0, 704, 100
28406, V, 1, 1, 1, 1, 0, 704, 100
28407, V, 1, 1, 1, 1, 0, 704, 100
28408, V, 1, 1, 1, 1, 0, 704, 100
28409, V, 1, 1, 1, 1, 0, 704, 100
28410, V, 1, 1, 1, 1, 0, 704, 100
28411, V, 1, 1, 1, 1, 0, 704, 100
28412, V, 1, 1, 1, 1, 0, 704, 100
28413, V, 1, 1, 1, 1, 0, 704, 100
28414, V, 1, 1, 1, 1, 0, 704, 101
28416, V, 1, 1, 1, 1, 0, 704, 101
28417, V, 1, 1, 1, 1, 0, 704, 100
28418, V, 1, 1, 1, 1, 0, 704, 101
28419, V, 1, 1, 1, 1, 0, 704, 100
28420, V, 1, 1, 1, 1, 0, 704, 100
28421, V, 1, 1, 1, 1, 0, 704, 101
28422, V, 1, 1, 1, 1, 0, 704, 101
28423, V, 1, 1, 1, 1, 0, 704, 101
28424, V, 1, 1, 1, 1, 0, 704, 101
28425, V, 1, 1, 1, 1, 0, 704, 101
28426, V, 1, 1, 1, 1, 0, 704, 101
28427, V, 1, 1, 1, 1, 0, 704, 101
28428, V, 1, 1, 1, 1, 0, 704, 101
28429, V, 1, 1, 1, 1, 0, 704, 101
28430, V, 1, 1, 1, 1, 0, 704, 101
28431, V, 1, 1, 1, 1, 0, 704, 100
28432, V, 1, 1, 1, 1, 0, 704, 101
28433, V, 1, 1, 1, 1, 0, 704, 101
28434, V, 1, 1, 1, 1, 0, 704, 101
28435, V, 1, 1, 1, 1, 0, 704, 101
28436, V, 1, 1, 1, 1, 0, 704, 101
28437, V, 1, 1, 1, 1, 0, 704, 100
28438, V, 1, 1, 1, 1, 0, 704, 101
28439, V, 1, 1, 1, 1, 0, 704, 101
28440, V, 1, 1, 1, 1, 0, 704, 101
28441, V, 1, 1, 1, 1, 0, 704, 101
28442, V, 1, 1, 1, 1, 0, 704, 101
28443, V, 1, 1, 1, 1, 0, 704, 101
28444, V, 1, 1, 1, 1, 0, 704, 101
28445, V, 1, 1, 1, 1, 0, 704, 101
28446, V, 1, 1, 1, 1, 0, 704, 101
28447, V, 1, 1, 1, 1, 0, 704, 101
28448, V, 1, 1, 1, 1, 0, 704, 101
28449, V, 1, 1, 1, 1, 0, 704, 101
28450, V, 1, 1, 1, 1, 0, 704, 101
28451, V, 1, 1, 1, 1, 0, 704, 101
28452, V, 1, 1, 1, 1, 0, 704, 101
28453, V, 1, 1, 1, 1, 0, 704, 101
28454, V, 1, 1, 1, 1, 0, 704, 101
28455, V, 1, 1, 1, 1, 0, 704, 101
28456, V, 1, 1, 1, 1, 0, 704, 101
28457, V, 1, 1, 1, 1, 0, 704, 100
28459, V, 1, 1, 1, 1, 0, 704, 101
28460, V, 1, 1, 1, 1, 0, 704, 100
28461, V, 1, 1, 1, 1, 0, 704, 100
28462, V, 1, 1, 1, 1, 0, 704, 101
28463, V, 1, 1, 1, 1, 0, 704, 100
28464, V, 1, 1, 1, 1, 0, 704, 100
28465, V, 1, 1, 1, 1, 0, 704, 100
28466, V, 1, 1, 1, 1, 0, 704, 100
28467, V, 1, 1, 1, 1, 0, 704, 100
28468, V, 1, 1, 1, 1, 0, 704, 100
28469, V, 1, 1, 1, 1, 0, 704, 100
28470, V, 1, 1, 1, 1, 0, 704, 100
28471, V, 1, 1, 1, 1, 0, 704, 100
28472, V, 1, 1, 1, 1, 0, 704, 100
28473, V, 1, 1, 1, 1, 0, 704, 100
28474, V, 1, 1, 1, 1, 0, 704, 100
28475, V, 1, 1, 1, 1, 0, 704, 100
28476, V, 1, 1, 1, 1, 0, 704, 100
28477, V, 1, 1, 1, 1, 0, 704, 100
28478, V, 1, 1, 1, 1, 0, 704, 100
28479, V, 1, 1, 1, 1, 0, 704, 101
28480, V, 1, 1, 1, 1, 0, 704, 100
28481, V, 1, 1, 1, 1, 0, 704, 100
28482, V, 1, 1, 1, 1, 0, 704, 100
28483, V, 1, 1, 1, 1, 0, 704, 100
28484, V, 1, 1, 1, 1, 0, 704, 100
28485, V, 1, 1, 1, 1, 0, 704, 100
28486, V, 1, 1, 1, 1, 0, 704, 100
28487, V, 1, 1, 1, 1, 0, 704, 100
28488, V, 1, 1, 1, 1, 0, 704, 100
28489, V, 1, 1, 1, 1, 0, 704, 101
28490, V, 1, 1, 1, 1, 0, 704, 100
28491, V, 1, 1, 1, 1, 0, 704, 100
28492, V, 1, 1, 1, 1, 0, 704, 100
28493, V, 1, 1, 1, 1, 0, 704, 100
28494, V, 1, 1, 1, 1, 0, 704, 100
28495, V, 1, 1, 1, 1, 0, 704, 100
28496, V, 1, 1, 1, 1, 0, 704, 100
28497, V, 1, 1, 1, 1, 0, 704, 100
28498, V, 1, 1, 1, 1, 0, 704, 101
28499, V, 1, 1, 1, 1, 0, 704, 101
28500, V, 1, 1, 1, 1, 0, 704, 101
28502, V, 1, 1, 1, 1, 0, 704, 101
28503, V, 1, 1, 1, 1, 0, 704, 101
28504, V, 1, 1, 1, 1, 0, 704, 101
28505, V, 1, 1, 1, 1, 0, 704, 101
28506, V, 1, 1, 1, 1, 0, 704, 101
28507, V, 1, 1, 1, 1, 0, 704, 101
28508, V, 1, 1, 1, 1, 0, 704, 101
28509, V, 1, 1, 1, 1, 0, 704, 101
28510, V, 1, 1, 1, 1, 0, 704, 101
28511, V, 1, 1, 1, 1, 0, 704, 100
28512, V, 1, 1, 1, 1, 0, 704, 101
28513, V, 1, 1, 1, 1, 0, 704, 101
28514, V, 1, 1, 1, 1, 0, 704, 101
28515, V, 1, 1, 1, 1, 0, 704, 101
28516, V, 1, 1, 1, 1, 0, 704, 100
28517, V, 1, 1, 1, 1, 0, 704, 100
28518, V, 1, 1, 1, 1, 0, 704, 100
28519, V, 1, 1, 1, 1, 0, 704, 101
28520, V, 1, 1, 1, 1, 0, 704, 101
28521, V, 1, 1, 1, 1, 0, 704, 101
28522, V, 1, 1, 1, 1, 0, 704, 101
28523, V, 1, 1, 1, 1, 0, 704, 100
28524, V, 1, 1, 1, 1, 0, 704, 101
28525, V, 1, 1, 1, 1, 0, 704, 101
28526, V, 1, 1, 1, 1, 0, 704, 100
28527, V, 1, 1, 1, 1, 0, 704, 100
28528, V, 1, 1, 1, 1, 0, 704, 100
28529, V, 1, 1, 1, 1, 0, 704, 100
28530, V, 1, 1, 1, 1, 0, 704, 100
28531, V, 1, 1, 1, 1, 0, 704, 100
28532, V, 1, 1, 1, 1, 0, 704, 100
28533, V, 1, 1, 1, 1, 0, 704, 100
28534, V, 1, 1, 1, 1, 0, 704, 100
28535, V, 1, 1, 1, 1, 0, 704, 100
28536, V, 1, 1, 1, 1, 0, 704, 100
28537, V, 1, 1, 1, 1, 0, 704, 100
28538, V, 1, 1, 1, 1, 0, 704, 100
28539, V, 1, 1, 1, 1, 0, 704, 100
28540, V, 1, 1, 1, 1, 0, 704, 100
28541, V, 1, 1, 1, 1, 0, 704, 100
28542, V, 1, 1, 1, 1, 0, 704, 100
28544, V, 1, 1, 1, 1, 0, 704, 100
28545, V, 1, 1, 1, 1, 0, 704, 100
28546, V, 1, 1, 1, 1, 0, 704, 100
28547, V, 1, 1, 1, 1, 0, 704, 100
28548, V, 1, 1, 1, 1, 0, 704, 100
28549, V, 1, 1, 1, 1, 0, 704, 100
28550, V, 1, 1, 1, 1, 0, 704, 100
28551, V, 1, 1, 1, 1, 0, 704, 100
28552, V, 1, 1, 1, 1, 0, 704, 100
28553, V, 1, 1, 1, 1, 0, 704, 100
28554, V, 1, 1, 1, 1, 0, 704, 100
28555, V, 1, 1, 1, 1, 0, 704, 100
28556, V, 1, 1, 1, 1, 0, 704, 100
28557, V, 1, 1, 1, 1, 0, 704, 100
28558, V, 1, 1, 1, 1, 0, 704, 100
28559, V, 1, 1, 1, 1, 0, 704, 100
28560, V, 1, 1, 1, 1, 0, 704, 100
28561, V, 1, 1, 1, 1, 0, 704, 100
28562, V, 1, 1, 1, 1, 0, 704, 100
28563, V, 1, 0, 0, 1, 0, 704, 100
28563, V, 1, 0, 0, 0, 0, 704, 100
28564, V, 1, 1, 0, 0, 0, 704, 101
28564, V, 1, 1, 0, 0, 0, 704, 101
28565, V, 1, 1, 1, 1, 0, 704, 101
28566, V, 1, 1, 1, 1, 0, 704, 100
28567, V, 1, 1, 1, 1, 0, 704, 100
28568, V, 1, 1, 1, 1, 0, 704, 100
28569, V, 1, 1, 1, 1, 0, 704, 100
28570, V, 1, 1, 1, 1, 0, 704, 100
28571, V, 1, 1, 1, 1, 0, 704, 100
28572, V, 1, 1, 1, 1, 0, 704, 100
28573, V, 1, 1, 1, 1, 0, 704, 100
28574, V, 1, 1, 1, 1, 0, 704, 100
28575, V, 1, 1, 1, 1, 0, 704, 100
28576, V, 1, 1, 1, 1, 0, 704, 100
28577, V, 1, 1, 1, 1, 0, 704, 100
28578, V, 1, 1, 1, 1, 0, 704, 100
28579, V, 1, 1, 1, 1, 0, 704, 100
28580, V, 1, 1, 1, 1, 0, 704, 100
28581, V, 1, 1, 1, 1, 0, 704, 100
28582, V, 1, 1, 1, 1, 0, 704, 100
28583, V, 1, 1, 1, 1, 0, 704, 100
28584, V, 1, 1, 1, 1, 0, 704, 100
28585, V, 1, 1, 1, 1, 0, 704, 100
28587, V, 1, 1, 1, 1, 0, 704, 100
28588, V, 1, 1, 1, 1, 0, 704, 100
28589, V, 1, 1, 1, 1, 0, 704, 100
28590, V, 1, 1, 1, 1, 0, 704, 100
28591, V, 1, 1, 1, 1, 0, 704, 100
28592, V, 1, 1, 1, 1, 0, 704, 100
28593, V, 1, 1, 1, 1, 0, 704, 100
28594, V, 1, 1, 1, 1, 0, 704, 100
28595, V, 1, 1, 1, 1, 0, 704, 100
28596, V, 1, 1, 1, 1, 0, 704, 100
28597, V, 1, 1, 1, 1, 0, 704, 100
28598, V, 1, 1, 1, 1, 0, 704, 100
28599, V, 1, 1, 1, 1, 0, 704, 100
28600, V, 1, 1, 1, 1, 0, 704, 100
28601, V, 1, 1, 1, 1, 0, 704, 100
28602, V, 1, 1, 1, 1, 0, 704, 100
28603, V, 1, 1, 1, 1, 0, 704, 100
28604, V, 1, 1, 1, 1, 0, 704, 100
28605, V, 1, 1, 1, 1, 0, 704, 100
28606, V, 1, 1, 1, 1, 0, 704, 100
28607, V, 1, 1, 1, 1, 0, 704, 100
28608, V, 1, 1, 1, 1, 0, 704, 100
28609, V, 1, 1, 1, 1, 0, 704, 100
28610, V, 1, 1, 1, 1, 0, 704, 100
28611, V, 1, 1, 1, 1, 0, 704, 100
28612, V, 1, 1, 1, 1, 0, 704, 100
28613, V, 1, 1, 1, 1, 0, 704, 100
28614, V, 1, 1, 1, 1, 0, 704, 100
28615, V, 1, 1, 1, 1, 0, 704, 100
28616, V, 1, 1, 1, 1, 0, 704, 100
28617, V, 1, 1, 1, 1, 0, 704, 100
28618, V, 1, 1, 1, 1, 0, 704, 100
28619, V, 1, 1, 1, 1, 0, 704, 100
28620, V, 1, 1, 1, 1, 0, 704, 100
28621, V, 1, 1, 1, 1, 0, 704, 100
28622, V, 1, 1, 1, 1, 0, 704, 100
28623, V, 1, 1, 1, 1, 0, 704, 100
28624, V, 1, 1, 1, 1, 0, 704, 100
28625, V, 1, 1, 1, 1, 0, 704, 100
28626, V, 1, 1, 1, 1, 0, 704, 100
28627, V, 1, 1, 1, 1, 0, 704, 100
28628, V, 1, 1, 1, 1, 0, 704, 100
28630, V, 1, 1, 1, 1, 0, 704, 100
28631, V, 1, 1, 1, 1, 0, 704, 100
28632, V, 1, 1, 1, 1, 0, 704, 100
28633, V, 1, 1, 1, 1, 0, 704, 100
28634, V, 1, 1, 1, 1, 0, 704, 100
28635, V, 1, 1, 1, 1, 0, 704, 100
28636, V, 1, 1, 1, 1, 0, 704, 100
28637, V, 1, 1, 1, 1, 0, 704, 100
28638, V, 1, 1, 1, 1, 0, 704, 100
28639, V, 1, 1, 1, 1, 0, 704, 100
28640, V, 1, 1, 1, 1, 0, 704, 100
28641, V, 1, 1, 1, 1, 0, 704, 100
28642, V, 1, 1, 1, 1, 0, 704, 100
28643, V, 1, 1, 1, 1, 0, 704, 100
28644, V, 1, 1, 1, 1, 0, 704, 100
28645, V, 1, 1, 1, 1, 0, 704, 100
28646, V, 1, 1, 1, 1, 0, 704, 100
28647, V, 1, 1, 1, 1, 0, 704, 100
28648, V, 1, 1, 1, 1, 0, 704, 100
28649, V, 1, 1, 1, 1, 0, 704, 100
28650, V, 1, 1, 1, 1, 0, 704, 100
28651, V, 1, 1, 1, 1, 0, 704, 100
28652, V, 1, 1, 1, 1, 0, 704, 100
28653, V, 1, 1, 1, 1, 0, 704, 100
28654, V, 1, 1, 1, 1, 0, 704, 100
28655, V, 1, 1, 1, 1, 0, 704, 100
28656, V, 1, 1, 1, 1, 0, 704, 100
28657, V, 1, 1, 1, 1, 0, 704, 100
28658, V, 1, 1, 1, 1, 0, 704, 100
28659, V, 1, 1, 1, 1, 0, 704, 100
28660, V, 1, 1, 1, 1, 0, 704, 100
28661, V, 1, 1, 1, 1, 0, 704, 100
28662, V, 1, 1, 1, 1, 0, 704, 100
28663, V, 1, 1, 1, 1, 0, 704, 100
28664, V, 1, 1, 1, 1, 0, 704, 100
28665, V, 1, 1, 1, 1, 0, 704, 100
28666, V, 1, 1, 1, 1, 0, 704, 100
28667, V, 1, 1, 1, 1, 0, 704, 100
28668, V, 1, 1, 1, 1, 0, 704, 100
28669, V, 1, 1, 1, 1, 0, 704, 100
28670, V, 1, 1, 1, 1, 0, 704, 100
28672, V, 1, 1, 1, 1, 0, 704, 100
28673, V, 1, 1, 1, 1, 0, 704, 100
28674, V, 1, 1, 1, 1, 0, 704, 100
28675, V, 1, 1, 1, 1, 0, 704, 100
28676, V, 1, 1, 1, 1, 0, 704, 100
28677, V, 1, 1, 1, 1, 0, 704, 100
28678, V, 1, 1, 1, 1, 0, 704, 100
28679, V, 1, 1, 1, 1, 0, 704, 100
28680, V, 1, 1, 1, 1, 0, 704, 100
28681, V, 1, 1, 1, 1, 0, 704, 100
28682, V, 1, 1, 1, 1, 0, 704, 100
28683, V, 1, 1, 1, 1, 0, 704, 100
28684, V, 1, 1, 1, 1, 0, 704, 100
28685, V, 1, 1, 1, 1, 0, 704, 100
28686, V, 1, 1, 1, 1, 0, 704, 100
28687, V, 1, 1, 1, 1, 0, 704, 100
28688, V, 1, 1, 1, 1, 0, 704, 100
28689, V, 1, 1, 1, 1, 0, 704, 100
28690, V, 1, 1, 1, 1, 0, 704, 100
28691, V, 1, 1, 1, 1, 0, 704, 100
28692, V, 1, 1, 1, 1, 0, 704, 100
28693, V, 1, 1, 1, 1, 0, 704, 100
28694, V, 1, 1, 1, 1, 0, 704, 100
28695, V, 1, 1, 1, 1, 0, 704, 100
28696, V, 1, 1, 1, 1, 0, 704, 100
28697, V, 1, 1, 1, 1, 0, 704, 100
28698, V, 1, 1, 1, 1, 0, 704, 100
28699, V, 1, 1, 1, 1, 0, 704, 100
28700, V, 1, 1, 1, 1, 0, 704, 100
28701, V, 1, 1, 1, 1, 0, 704, 100
28702, V, 1, 1, 1, 1, 0, 704, 100
28703, V, 1, 1, 1, 1, 0, 704, 100
28704, V, 1, 1, 1, 1, 0, 704, 100
28705, V, 1, 1, 1, 1, 0, 704, 100
28706, V, 1, 1, 1, 1, 0, 704, 100
28707, V, 1, 1, 1, 1, 0, 704, 100
28708, V, 1, 1, 1, 1, 0, 704, 100
28709, V, 1, 1, 1, 1, 0, 704, 100
28710, V, 1, 1, 1, 1, 0, 704, 100
28711, V, 1, 1, 1, 1, 0, 704, 100
28712, V, 1, 1, 1, 1, 0, 704, 100
28713, V, 1, 1, 1, 1, 0, 704, 100
28715, V, 1, 1, 1, 1, 0, 704, 100
28716, V, 1, 1, 1, 1, 0, 704, 100
28717, V, 1, 1, 1, 1, 0, 704, 100
28718, V, 1, 1, 1, 1, 0, 704, 100
28719, V, 1, 1, 1, 1, 0, 704, 100
28720, V, 1, 1, 1, 1, 0, 704, 100
28721, V, 1, 1, 1, 1, 0, 704, 100
28722, V, 1, 1, 1, 1, 0, 704, 100
28723, V, 1, 1, 1, 1, 0, 704, 100
28724, V, 1, 1, 1, 1, 0, 704, 100
28725, V, 1, 1, 1, 1, 0, 704, 100
28726, V, 1, 1, 1, 1, 0, 704, 100
28727, V, 1, 1, 1, 1, 0, 704, 100
28728, V, 1, 1, 1, 1, 0, 704, 100
28729, V, 1, 1, 1, 1, 0, 704, 100
28730, V, 1, 1, 1, 1, 0, 704, 100
28731, V, 1, 1, 1, 1, 0, 704, 101
28732, V, 1, 1, 1, 1, 0, 704, 100
28733, V, 1, 1, 1, 1, 0, 704, 100
28734, V, 1, 1, 1, 1, 0, 704, 101
28735, V, 1, 1, 1, 1, 0, 704, 100
28736, V, 1, 1, 1, 1, 0, 704, 100
28737, V, 1, 1, 1, 1, 0, 704, 100
28738, V, 1, 1, 1, 1, 0, 704, 101
28739, V, 1, 1, 1, 1, 0, 704, 100
28740, V, 1, 1, 1, 1, 0, 704, 101
28741, V, 1, 1, 1, 1, 0, 704, 100
28742, V, 1, 1, 1, 1, 0, 704, 101
28743, V, 1, 1, 1, 1, 0, 704, 100
28744, V, 1, 1, 1, 1, 0, 704, 101
28745, V, 1, 1, 1, 1, 0, 704, 100
28746, V, 1, 1, 1, 1, 0, 704, 100
28747, V, 1, 1, 1, 1, 0, 704, 101
28748, V, 1, 1, 1, 1, 0, 704, 100
28749, V, 1, 1, 1, 1, 0, 704, 100
28750, V, 1, 1, 1, 1, 0, 704, 100
28751, V, 1, 1, 1, 1, 0, 704, 100
28752, V, 1, 1, 1, 1, 0, 704, 100
28753, V, 1, 1, 1, 1, 0, 704, 100
28754, V, 1, 1, 1, 1, 0, 704, 100
28755, V, 1, 1, 1, 1, 0, 704, 100
28756, V, 1, 1, 1, 1, 0, 704, 100
28758, V, 1, 1, 1, 1, 0, 704, 100
28759, V, 1, 1, 1, 1, 0, 704, 100
28760, V, 1, 1, 1, 1, 0, 704, 100
28761, V, 1, 1, 1, 1, 0, 704, 100
28762, V, 1, 1, 1, 1, 0, 704, 100
28763, V, 1, 1, 1, 1, 0, 704, 100
28764, V, 1, 1, 1, 1, 0, 704, 100
28765, V, 1, 1, 1, 1, 0, 704, 100
28766, V, 1, 1, 1, 1, 0, 704, 100
28767, V, 1, 1, 1, 1, 0, 704, 100
28768, V, 1, 1, 1, 1, 0, 704, 100
28769, V, 1, 1, 1, 1, 0, 704, 100
28770, V, 1, 1, 1, 1, 0, 704, 100
28771, V, 1, 1, 1, 1, 0, 704, 100
28772, V, 1, 1, 1, 1, 0, 704, 100
28773, V, 1, 1, 1, 1, 0, 704, 100
28774, V, 1, 1, 1, 1, 0, 704, 100
28775, V, 1, 1, 1, 1, 0, 704, 100
28776, V, 1, 1, 1, 1, 0, 704, 100
28777, V, 1, 1, 1, 1, 0, 704, 100
28778, V, 1, 1, 1, 1, 0, 704, 100
28779, V, 1, 1, 1, 1, 0, 704, 100
28780, V, 1, 1, 1, 1, 0, 704, 100
28781, V, 1, 1, 1, 1, 0, 704, 100
28782, V, 1, 1, 1, 1, 0, 704, 100
28783, V, 1, 1, 1, 1, 0, 704, 100
28784, V, 1, 1, 1, 1, 0, 704, 100
28785, V, 1, 1, 1, 1, 0, 704, 100
28786, V, 1, 1, 1, 1, 0, 704, 100
28787, V, 1, 1, 1, 1, 0, 704, 100
28788, V, 1, 1, 1, 1, 0, 704, 100
28789, V, 1, 1, 1, 1, 0, 704, 100
28790, V, 1, 1, 1, 1, 0, 704, 100
28791, V, 1, 1, 1, 1, 0, 704, 100
28792, V, 1, 1, 1, 1, 0, 704, 100
28793, V, 1, 1, 1, 1, 0, 704, 100
28794, V, 1, 1, 1, 1, 0, 704, 100
28795, V, 1, 1, 1, 1, 0, 704, 100
28796, V, 1, 1, 1, 1, 0, 704, 100
28797, V, 1, 1, 1, 1, 0, 704, 100
28798, V, 1, 1, 1, 1, 0, 704, 100
28800, V, 1, 1, 1, 1, 0, 704, 100
28801, V, 1, 1, 1, 1, 0, 704, 100
28802, V, 1, 1, 1, 1, 0, 704, 100
28803, V, 1, 1, 1, 1, 0, 704, 100
28804, V, 1, 1, 1, 1, 0, 704, 100
28805, V, 1, 1, 1, 1, 0, 704, 100
28806, V, 1, 1, 1, 1, 0, 704, 100
28807, V, 1, 1, 1, 1, 0, 704, 100
28808, V, 1, 1, 1, 1, 0, 704, 100
28809, V, 1, 1, 1, 1, 0, 704, 100
28810, V, 1, 1, 1, 1, 0, 704, 100
28811, V, 1, 1, 1, 1, 0, 704, 100
28812, V, 1, 1, 1, 1, 0, 704, 100
28813, V, 1, 1, 1, 1, 0, 704, 100
28814, V, 1, 1, 1, 1, 0, 704, 100
28815, V, 1, 1, 1, 1, 0, 704, 100
28816, V, 1, 1, 1, 1, 0, 704, 100
28817, V, 1, 1, 1, 1, 0, 704, 100
28818, V, 1, 1, 1, 1, 0, 704, 100
28819, V, 1, 1, 1, 1, 0, 704, 100
28820, V, 1, 1, 1, 1, 0, 704, 100
28821, V, 1, 1, 1, 1, 0, 704, 100
28822, V, 1, 1, 1, 1, 0, 704, 100
28823, V, 1, 1, 1, 1, 0, 704, 100
28824, V, 1, 1, 1, 1, 0, 704, 100
28825, V, 1, 1, 1, 1, 0, 704, 100
28826, V, 1, 1, 1, 1, 0, 704, 100
28827, V, 1, 1, 1, 1, 0, 704, 100
28828, V, 1, 1, 1, 1, 0, 704, 100
28829, V, 1, 1, 1, 1, 0, 704, 100
28830, V, 1, 1, 1, 1, 0, 704, 100
28831, V, 1, 1, 1, 1, 0, 704, 100
28832, V, 1, 1, 1, 1, 0, 704, 100
28833, V, 1, 1, 1, 1, 0, 704, 100
28834, V, 1, 1, 1, 1, 0, 704, 100
28835, V, 1, 1, 1, 1, 0, 704, 100
28836, V, 1, 1, 1, 1, 0, 704, 100
28837, V, 1, 1, 1, 1, 0, 704, 100
28838, V, 1, 1, 1, 1, 0, 704, 100
28839, V, 1, 1, 1, 1, 0, 704, 100
28840, V, 1, 1, 1, 1, 0, 704, 100
28841, V, 1, 1, 1, 1, 0, 704, 100
28843, V, 1, 1, 1, 1, 0, 704, 100
28844, V, 1, 1, 1, 1, 0, 704, 100
28845, V, 1, 1, 1, 1, 0, 704, 100
28846, V, 1, 1, 1, 1, 0, 704, 100
28847, V, 1, 1, 1, 1, 0, 704, 100
28848, V, 1, 1, 1, 1, 0, 704, 100
28849, V, 1, 1, 1, 1, 0, 704, 100
28850, V, 1, 1, 1, 1, 0, 704, 100
28851, V, 1, 1, 1, 1, 0, 704, 100
28852, V, 1, 1, 1, 1, 0, 704, 100
28853, V, 1, 1, 1, 1, 0, 704, 100
28854, V, 1, 1, 1, 1, 0, 704, 100
28855, V, 1, 1, 1, 1, 0, 704, 100
28856, V, 1, 1, 1, 1, 0, 704, 100
28857, V, 1, 1, 1, 1, 0, 704, 100
28858, V, 1, 1, 1, 1, 0, 704, 100
28859, V, 1, 1, 1, 1, 0, 704, 100
28860, V, 1, 1, 1, 1, 0, 704, 100
28861, V, 1, 1, 1, 1, 0, 704, 100
28862, V, 1, 1, 1, 1, 0, 704, 100
28863, V, 1, 1, 1, 1, 0, 704, 100
28864, V, 1, 1, 1, 1, 0, 704, 100
28865, V, 1, 1, 1, 1, 0, 704, 100
28866, V, 1, 1, 1, 1, 0, 704, 100
28867, V, 1, 1, 1, 1, 0, 704, 100
28868, V, 1, 1, 1, 1, 0, 704, 100
28869, V, 1, 1, 1, 1, 0, 704, 100
28870, V, 1, 1, 1, 1, 0, 704, 100
28871, V, 1, 1, 1, 1, 0, 704, 100
28872, V, 1, 1, 1, 1, 0, 704, 100
28873, V, 1, 1, 1, 1, 0, 704, 100
28874, V, 1, 1, 1, 1, 0, 704, 100
28875, V, 1, 1, 1, 1, 0, 704, 100
28876, V, 1, 1, 1, 1, 0, 704, 100
28877, V, 1, 1, 1, 1, 0, 704, 100
28878, V, 1, 1, 1, 1, 0, 704, 100
28879, V, 1, 1, 1, 1, 0, 704, 100
28880, V, 1, 1, 1, 1, 0, 704, 100
28881, V, 1, 1, 1, 1, 0, 704, 100
28882, V, 1, 1, 1, 1, 0, 704, 100
28883, V, 1, 1, 1, 1, 0, 704, 100
28884, V, 1, 1, 1, 1, 0, 704, 100
28886, V, 1, 1, 1, 1, 0, 704, 100
28887, V, 1, 1, 1, 1, 0, 704, 100
28888, V, 1, 1, 1, 1, 0, 704, 100
28889, V, 1, 1, 1, 1, 0, 704, 100
28890, V, 1, 1, 1, 1, 0, 704, 100
28891, V, 1, 1, 1, 1, 0, 704, 100
28892, V, 1, 1, 1, 1, 0, 704, 100
28893, V, 1, 1, 1, 1, 0, 704, 100
28894, V, 1, 1, 1, 1, 0, 704, 100
28895, V, 1, 1, 1, 1, 0, 704, 100
28896, V, 1, 1, 1, 1, 0, 704, 100
28897, V, 1, 1, 1, 1, 0, 704, 100
28898, V, 1, 1, 1, 1, 0, 704, 100
28899, V, 1, 1, 1, 1, 0, 704, 100
28900, V, 1, 1, 1, 1, 0, 704, 100
28901, V, 1, 1, 1, 1, 0, 704, 100
28902, V, 1, 1, 1, 1, 0, 704, 100
28903, V, 1, 1, 1, 1, 0, 704, 100
28904, V, 1, 1, 1, 1, 0, 704, 101
28905, V, 1, 1, 1, 1, 0, 704, 100
28906, V, 1, 1, 1, 1, 0, 704, 100
28907, V, 1, 1, 1, 1, 0, 704, 100
28908, V, 1, 1, 1, 1, 0, 704, 100
28909, V, 1, 1, 1, 1, 0, 704, 100
28910, V, 1, 1, 1, 1, 0, 704, 100
28911, V, 1, 1, 1, 1, 0, 704, 100
28912, V, 1, 1, 1, 1, 0, 704, 100
28913, V, 1, 1, 1, 1, 0, 704, 100
28914, V, 1, 1, 1, 1, 0, 704, 100
28915, V, 1, 1, 1, 1, 0, 704, 100
28916, V, 1, 1, 1, 1, 0, 704, 100
28917, V, 1, 1, 1, 1, 0, 704, 100
28918, V, 1, 1, 1, 1, 0, 704, 100
28919, V, 1, 1, 1, 1, 0, 704, 100
28920, V, 1, 1, 1, 1, 0, 704, 100
28921, V, 1, 1, 1, 1, 0, 704, 100
28922, V, 1, 1, 1, 1, 0, 704, 100
28923, V, 1, 1, 1, 1, 0, 704, 100
28924, V, 1, 1, 1, 1, 0, 704, 100
28925, V, 1, 1, 1, 1, 0, 704, 100
28926, V, 1, 1, 1, 1, 0, 704, 100
28928, V, 1, 1, 1, 1, 0, 704, 100
28929, V, 1, 1, 1, 1, 0, 704, 100
28930, V, 1, 1, 1, 1, 0, 704, 100
28931, V, 1, 1, 1, 1, 0, 704, 100
28932, V, 1, 1, 1, 1, 0, 704, 100
28933, V, 1, 1, 1, 1, 0, 704, 100
28934, V, 1, 1, 1, 1, 0, 704, 100
28935, V, 1, 1, 1, 1, 0, 704, 100
28936, V, 1, 1, 1, 1, 0, 704, 100
28937, V, 1, 1, 1, 1, 0, 704, 100
28938, V, 1, 1, 1, 1, 0, 704, 100
28939, V, 1, 1, 1, 1, 0, 704, 100
28940, V, 1, 1, 1, 1, 0, 704, 100
28941, V, 1, 1, 1, 1, 0, 704, 100
28942, V, 1, 1, 1, 1, 0, 704, 100
28943, V, 1, 1, 1, 1, 0, 704, 100
28944, V, 1, 1, 1, 1, 0, 704, 100
28945, V, 1, 1, 1, 1, 0, 704, 100
28946, V, 1, 1, 1, 1, 0, 704, 100
28947, V, 1, 1, 1, 1, 0, 704, 100
28948, V, 1, 1, 1, 1, 0, 704, 100
28949, V, 1, 1, 1, 1, 0, 704, 100
28950, V, 1, 1, 1, 1, 0, 704, 100
28951, V, 1, 1, 1, 1, 0, 704, 100
28952, V, 1, 1, 1, 1, 0, 704, 100
28953, V, 1, 1, 1, 1, 0, 704, 100
28954, V, 1, 1, 1, 1, 0, 704, 100
28955, V, 1, 1, 1, 1, 0, 704, 100
28956, V, 1, 1, 1, 1, 0, 704, 100
28957, V, 1, 1, 1, 1, 0, 704, 100
28958, V, 1, 1, 1, 1, 0, 704, 100
28959, V, 1, 1, 1, 1, 0, 704, 100
28960, V, 1, 1, 1, 1, 0, 704, 100
28961, V, 1, 1, 1, 1, 0, 704, 100
28962, V, 1, 1, 1, 1, 0, 704, 100
28963, V, 1, 1, 1, 1, 0, 704, 100
28964, V, 1, 1, 1, 1, 0, 704, 100
28965, V, 1, 1, 1, 1, 0, 704, 100
28966, V, 1, 1, 1, 1, 0, 704, 100
28967, V, 1, 1, 1, 1, 0, 704, 100
28968, V, 1, 1, 1, 1, 0, 704, 100
28969, V, 1, 1, 1, 1, 0, 704, 100
28971, V, 1, 1, 1, 1, 0, 704, 100
28972, V, 1, 1, 1, 1, 0, 704, 100
28973, V, 1, 1, 1, 1, 0, 704, 100
28974, V, 1, 1, 1, 1, 0, 704, 100
28975, V, 1, 1, 1, 1, 0, 704, 100
28976, V, 1, 1, 1, 1, 0, 704, 100
28977, V, 1, 1, 1, 1, 0, 704, 100
28978, V, 1, 1, 1, 1, 0, 704, 100
28979, V, 1, 1, 1, 1, 0, 704, 100
28980, V, 1, 1, 1, 1, 0, 704, 100
28981, V, 1, 1, 1, 1, 0, 704, 100
28982, V, 1, 1, 1, 1, 0, 704, 100
28983, V, 1, 1, 1, 1, 0, 704, 100
28984, V, 1, 1, 1, 1, 0, 704, 100
28985, V, 1, 1, 1, 1, 0, 704, 100
28986, V, 1, 1, 1, 1, 0, 704, 100
28987, V, 1, 1, 1, 1, 0, 704, 100
28988, V, 1, 1, 1, 1, 0, 704, 100
28989, V, 1, 1, 1, 1, 0, 704, 100
28990, V, 1, 1, 1, 1, 0, 704, 100
28991, V, 1, 1, 1, 1, 0, 704, 100
28992, V, 1, 1, 1, 1, 0, 704, 100
28993, V, 1, 0, 0, 1, 0, 704, 100
28993, V, 1, 0, 0, 0, 0, 704, 100
28994, V, 1, 1, 0, 0, 0, 704, 100
28994, V, 1, 1, 0, 0, 0, 704, 100
28995, V, 1, 1, 1, 1, 0, 704, 100
28996, V, 1, 1, 1, 1, 0, 704, 100
28997, V, 1, 1, 1, 1, 0, 704, 100
28998, V, 1, 1, 1, 1, 0, 704, 100
28999, V, 1, 1, 1, 1, 0, 704, 100
29000, V, 1, 1, 1, 1, 0, 704, 100
29001, V, 1, 1, 1, 1, 0, 704, 100
29002, V, 1, 1, 1, 1, 0, 704, 100
29003, V, 1, 1, 1, 1, 0, 704, 100
29004, V, 1, 1, 1, 1, 0, 704, 100
29005, V, 1, 1, 1, 1, 0, 704, 100
29006, V, 1, 1, 1, 1, 0, 704, 100
29007, V, 1, 1, 1, 1, 0, 704, 100
29008, V, 1, 1, 1, 1, 0, 704, 100
29009, V, 1, 1, 1, 1, 0, 704, 100
29010, V, 1, 1, 1, 1, 0, 704, 100
29011, V, 1, 1, 1, 1, 0, 704, 100
29012, V, 1, 1, 1, 1, 0, 704, 100
29014, V, 1, 1, 1, 1, 0, 704, 100
29015, V, 1, 1, 1, 1, 0, 704, 100
29016, V, 1, 1, 1, 1, 0, 704, 100
29017, V, 1, 1, 1, 1, 0, 704, 100
29018, V, 1, 1, 1, 1, 0, 704, 100
29019, V, 1, 1, 1, 1, 0, 704, 100
29020, V, 1, 1, 1, 1, 0, 704, 100
29021, V, 1, 1, 1, 1, 0, 704, 100
29022, V, 1, 1, 1, 1, 0, 704, 100
29023, V, 1, 1, 1, 1, 0, 704, 100
29024, V, 1, 1, 1, 1, 0, 704, 100
29025, V, 1, 1, 1, 1, 0, 704, 100
29026, V, 1, 1, 1, 1, 0, 704, 100
29027, V, 1, 1, 1, 1, 0, 704, 100
29028, V, 1, 1, 1, 1, 0, 704, 100
29029, V, 1, 1, 1, 1, 0, 704, 100
29030, V, 1, 1, 1, 1, 0, 704, 100
29031, V, 1, 1, 1, 1, 0, 704, 100
29032, V, 1, 1, 1, 1, 0, 704, 100
29033, V, 1, 1, 1, 1, 0, 704, 100
29034, V, 1, 1, 1, 1, 0, 704, 100
29035, V, 1, 1, 1, 1, 0, 704, 100
29036, V, 1, 1, 1, 1, 0, 704, 100
29037, V, 1, 1, 1, 1, 0, 704, 100
29038, V, 1, 1, 1, 1, 0, 704, 100
29039, V, 1, 1, 1, 1, 0, 704, 100
29040, V, 1, 1, 1, 1, 0, 704, 100
29041, V, 1, 1, 1, 1, 0, 704, 100
29042, V, 1, 1, 1, 1, 0, 704, 100
29043, V, 1, 1, 1, 1, 0, 704, 100
29044, V, 1, 1, 1, 1, 0, 704, 100
29045, V, 1, 1, 1, 1, 0, 704, 100
29046, V, 1, 1, 1, 1, 0, 704, 100
29047, V, 1, 1, 1, 1, 0, 704, 100
29048, V, 1, 1, 1, 1, 0, 704, 100
29049, V, 1, 1, 1, 1, 0, 704, 100
29050, V, 1, 1, 1, 1, 0, 704, 100
29051, V, 1, 1, 1, 1, 0, 704, 100
29052, V, 1, 1, 1, 1, 0, 704, 100
29053, V, 1, 1, 1, 1, 0, 704, 100
29054, V, 1, 1, 1, 1, 0, 704, 100
29056, V, 1, 1, 1, 1, 0, 704, 100
29057, V, 1, 1, 1, 1, 0, 704, 100
29058, V, 1, 1, 1, 1, 0, 704, 100
29059, V, 1, 1, 1, 1, 0, 704, 100
29060, V, 1, 1, 1, 1, 0, 704, 100
29061, V, 1, 1, 1, 1, 0, 704, 100
29062, V, 1, 1, 1, 1, 0, 704, 100
29063, V, 1, 1, 1, 1, 0, 704, 100
29064, V, 1, 1, 1, 1, 0, 704, 100
29065, V, 1, 1, 1, 1, 0, 704, 100
29066, V, 1, 1, 1, 1, 0, 704, 100
29067, V, 1, 1, 1, 1, 0, 704, 100
29068, V, 1, 1, 1, 1, 0, 704, 100
29069, V, 1, 1, 1, 1, 0, 704, 100
29070, V, 1, 1, 1, 1, 0, 704, 100
29071, V, 1, 1, 1, 1, 0, 704, 100
29072, V, 1, 1, 1, 1, 0, 704, 100
29073, V, 1, 1, 1, 1, 0, 704, 100
29074, V, 1, 1, 1, 1, 0, 704, 100
29075, V, 1, 1, 1, 1, 0, 704, 100
29076, V, 1, 1, 1, 1, 0, 704, 100
29077, V, 1, 1, 1, 1, 0, 704, 100
29078, V, 1, 1, 1, 1, 0, 704, 100
29079, V, 1, 1, 1, 1, 0, 704, 100
29080, V, 1, 1, 1, 1, 0, 704, 100
29081, V, 1, 1, 1, 1, 0, 704, 100
29082, V, 1, 1, 1, 1, 0, 704, 100
29083, V, 1, 1, 1, 1, 0, 704, 100
29084, V, 1, 1, 1, 1, 0, 704, 100
29085, V, 1, 1, 1, 1, 0, 704, 100
29086, V, 1, 1, 1, 1, 0, 704, 100
29087, V, 1, 1, 1, 1, 0, 704, 100
29088, V, 1, 1, 1, 1, 0, 704, 100
29089, V, 1, 1, 1, 1, 0, 704, 100
29090, V, 1, 1, 1, 1, 0, 704, 100
29091, V, 1, 1, 1, 1, 0, 704, 100
29092, V, 1, 1, 1, 1, 0, 704, 100
29093, V, 1, 1, 1, 1, 0, 704, 100
29094, V, 1, 1, 1, 1, 0, 704, 100
29095, V, 1, 1, 1, 1, 0, 704, 100
29096, V, 1, 1, 1, 1, 0, 704, 100
29097, V, 1, 1, 1, 1, 0, 704, 100
29099, V, 1, 1, 1, 1, 0, 704, 100
29100, V, 1, 1, 1, 1, 0, 704, 100
29101, V, 1, 1, 1, 1, 0, 704, 100
29102, V, 1, 1, 1, 1, 0, 704, 100
29103, V, 1, 1, 1, 1, 0, 704, 100
29104, V, 1, 1, 1, 1, 0, 704, 100
29105, V, 1, 1, 1, 1, 0, 704, 100
29106, V, 1, 1, 1, 1, 0, 704, 100
29107, V, 1, 1, 1, 1, 0, 704, 100
29108, V, 1, 1, 1, 1, 0, 704, 100
29109, V, 1, 1, 1, 1, 0, 704, 100
29110, V, 1, 1, 1, 1, 0, 704, 100
29111, V, 1, 1, 1, 1, 0, 704, 100
29112, V, 1, 1, 1, 1, 0, 704, 100
29113, V, 1, 1, 1, 1, 0, 704, 100
29114, V, 1, 1, 1, 1, 0, 704, 100
29115, V, 1, 1, 1, 1, 0, 704, 100
29116, V, 1, 1, 1, 1, 0, 704, 100
29117, V, 1, 1, 1, 1, 0, 704, 100
29118, V, 1, 1, 1, 1, 0, 704, 100
29119, V, 1, 1, 1, 1, 0, 704, 100
29120, V, 1, 1, 1, 1, 0, 704, 100
29121, V, 1, 1, 1, 1, 0, 704, 100
29122, V, 1, 1, 1, 1, 0, 704, 100
29123, V, 1, 1, 1, 1, 0, 704, 100
29124, V, 1, 1, 1, 1, 0, 704, 100
29125, V, 1, 1, 1, 1, 0, 704, 100
29126, V, 1, 1, 1, 1, 0, 704, 100
29127, V, 1, 1, 1, 1, 0, 704, 100
29128, V, 1, 1, 1, 1, 0, 704, 100
29129, V, 1, 1, 1, 1, 0, 704, 100
29130, V, 1, 1, 1, 1, 0, 704, 100
29131, V, 1, 1, 1, 1, 0, 704, 100
29132, V, 1, 1, 1, 1, 0, 704, 100
29133, V, 1, 1, 1, 1, 0, 704, 100
29134, V, 1, 1, 1, 1, 0, 704, 100
29135, V, 1, 1, 1, 1, 0, 704, 100
29136, V, 1, 1, 1, 1, 0, 704, 100
29137, V, 1, 1, 1, 1, 0, 704, 100
29138, V, 1, 1, 1, 1, 0, 704, 100
29139, V, 1, 1, 1, 1, 0, 704, 100
29140, V, 1, 1, 1, 1, 0, 704, 100
29142, V, 1, 1, 1, 1, 0, 704, 100
29143, V, 1, 1, 1, 1, 0, 704, 100
29144, V, 1, 1, 1, 1, 0, 704, 100
29145, V, 1, 1, 1, 1, 0, 704, 100
29146, V, 1, 1, 1, 1, 0, 704, 100
29147, V, 1, 1, 1, 1, 0, 704, 100
29148, V, 1, 1, 1, 1, 0, 704, 100
29149, V, 1, 1, 1, 1, 0, 704, 100
29150, V, 1, 1, 1, 1, 0, 704, 100
29151, V, 1, 1, 1, 1, 0, 704, 100
29152, V, 1, 1, 1, 1, 0, 704, 100
29153, V, 1, 1, 1, 1, 0, 704, 100
29154, V, 1, 1, 1, 1, 0, 704, 100
29155, V, 1, 1, 1, 1, 0, 704, 100
29156, V, 1, 1, 1, 1, 0, 704, 100
29157, V, 1, 1, 1, 1, 0, 704, 100
29158, V, 1, 1, 1, 1, 0, 704, 100
29159, V, 1, 1, 1, 1, 0, 704, 100
29160, V, 1, 1, 1, 1, 0, 704, 100
29161, V, 1, 1, 1, 1, 0, 704, 100
29162, V, 1, 1, 1, 1, 0, 704, 100
29163, V, 1, 1, 1, 1, 0, 704, 100
29164, V, 1, 1, 1, 1, 0, 704, 100
29165, V, 1, 1, 1, 1, 0, 704, 100
29166, V, 1, 1, 1, 1, 0, 704, 100
29167, V, 1, 1, 1, 1, 0, 704, 100
29168, V, 1, 1, 1, 1, 0, 704, 100
29169, V, 1, 1, 1, 1, 0, 704, 100
29170, V, 1, 1, 1, 1, 0, 704, 100
29171, V, 1, 1, 1, 1, 0, 704, 100
29172, V, 1, 1, 1, 1, 0, 704, 100
29173, V, 1, 1, 1, 1, 0, 704, 100
29174, V, 1, 1, 1, 1, 0, 704, 100
29175, V, 1, 1, 1, 1, 0, 704, 100
29176, V, 1, 1, 1, 1, 0, 704, 100
29177, V, 1, 1, 1, 1, 0, 704, 100
29178, V, 1, 1, 1, 1, 0, 704, 100
29179, V, 1, 1, 1, 1, 0, 704, 100
29180, V, 1, 1, 1, 1, 0, 704, 100
29181, V, 1, 1, 1, 1, 0, 704, 100
29182, V, 1, 1, 1, 1, 0, 704, 100
29184, V, 1, 1, 1, 1, 0, 704, 100
29185, V, 1, 1, 1, 1, 0, 704, 100
29186, V, 1, 1, 1, 1, 0, 704, 100
29187, V, 1, 1, 1, 1, 0, 704, 100
29188, V, 1, 1, 1, 1, 0, 704, 100
29189, V, 1, 1, 1, 1, 0, 704, 100
29190, V, 1, 1, 1, 1, 0, 704, 100
29191, V, 1, 1, 1, 1, 0, 704, 100
29192, V, 1, 1, 1, 1, 0, 704, 100
29193, V, 1, 1, 1, 1, 0, 704, 100
29194, V, 1, 1, 1, 1, 0, 704, 100
29195, V, 1, 1, 1, 1, 0, 704, 100
29196, V, 1, 1, 1, 1, 0, 704, 100
29197, V, 1, 1, 1, 1, 0, 704, 100
29198, V, 1, 1, 1, 1, 0, 704, 100
29199, V, 1, 1, 1, 1, 0, 704, 100
29200, V, 1, 1, 1, 1, 0, 704, 100
29201, V, 1, 1, 1, 1, 0, 704, 100
29202, V, 1, 1, 1, 1, 0, 704, 100
29203, V, 1, 1, 1, 1, 0, 704, 100
29204, V, 1, 1, 1, 1, 0, 704, 100
29205, V, 1, 1, 1, 1, 0, 704, 100
29206, V, 1, 1, 1, 1, 0, 704, 100
29207, V, 1, 1, 1, 1, 0, 704, 100
29208, V, 1, 1, 1, 1, 0, 704, 100
29209, V, 1, 1, 1, 1, 0, 704, 100
29210, V, 1, 1, 1, 1, 0, 704, 100
29211, V, 1, 1, 1, 1, 0, 704, 100
29212, V, 1, 1, 1, 1, 0, 704, 100
29213, V, 1, 1, 1, 1, 0, 704, 100
29214, V, 1, 1, 1, 1, 0, 704, 100
29215, V, 1, 1, 1, 1, 0, 704, 100
29216, V, 1, 1, 1, 1, 0, 704, 100
29217, V, 1, 1, 1, 1, 0, 704, 100
29218, V, 1, 1, 1, 1, 0, 704, 100
29219, V, 1, 1, 1, 1, 0, 704, 100
29220, V, 1, 1, 1, 1, 0, 704, 100
29221, V, 1, 1, 1, 1, 0, 704, 100
29222, V, 1, 1, 1, 1, 0, 704, 100
29223, V, 1, 1, 1, 1, 0, 704, 100
29224, V, 1, 1, 1, 1, 0, 704, 100
29225, V, 1, 1, 1, 1, 0, 704, 100
29227, V, 1, 1, 1, 1, 0, 704, 100
29228, V, 1, 1, 1, 1, 0, 704, 100
29229, V, 1, 1, 1, 1, 0, 704, 100
29230, V, 1, 1, 1, 1, 0, 704, 100
29231, V, 1, 1, 1, 1, 0, 704, 100
29232, V, 1, 1, 1, 1, 0, 704, 100
29233, V, 1, 1, 1, 1, 0, 704, 100
29234, V, 1, 1, 1, 1, 0, 704, 100
29235, V, 1, 1, 1, 1, 0, 704, 100
29236, V, 1, 1, 1, 1, 0, 704, 100
29237, V, 1, 1, 1, 1, 0, 704, 100
29238, V, 1, 1, 1, 1, 0, 704, 100
29239, V, 1, 1, 1, 1, 0, 704, 100
29240, V, 1, 1, 1, 1, 0, 704, 100
29241, V, 1, 1, 1, 1, 0, 704, 100
29242, V, 1, 1, 1, 1, 0, 704, 100
29243, V, 1, 1, 1, 1, 0, 704, 100
29244, V, 1, 1, 1, 1, 0, 704, 100
29245, V, 1, 1, 1, 1, 0, 704, 100
29246, V, 1, 1, 1, 1, 0, 704, 100
29247, V, 1, 1, 1, 1, 0, 704, 100
29248, V, 1, 1, 1, 1, 0, 704, 100
29249, V, 1, 1, 1, 1, 0, 704, 100
29250, V, 1, 1, 1, 1, 0, 704, 100
29251, V, 1, 1, 1, 1, 0, 704, 100
29252, V, 1, 1, 1, 1, 0, 704, 100
29253, V, 1, 1, 1, 1, 0, 704, 100
29254, V, 1, 1, 1, 1, 0, 704, 100
29255, V, 1, 1, 1, 1, 0, 704, 100
29256, V, 1, 1, 1, 1, 0, 704, 100
29257, V, 1, 1, 1, 1, 0, 704, 100
29258, V, 1, 1, 1, 1, 0, 704, 100
29259, V, 1, 1, 1, 1, 0, 704, 100
29260, V, 1, 1, 1, 1, 0, 704, 100
29261, V, 1, 1, 1, 1, 0, 704, 100
29262, V, 1, 1, 1, 1, 0, 704, 100
29263, V, 1, 1, 1, 1, 0, 704, 100
29264, V, 1, 1, 1, 1, 0, 704, 100
29265, V, 1, 1, 1, 1, 0, 704, 100
29266, V, 1, 1, 1, 1, 0, 704, 100
29267, V, 1, 1, 1, 1, 0, 704, 100
29268, V, 1, 1, 1, 1, 0, 704, 100
29270, V, 1, 1, 1, 1, 0, 704, 100
29271, V, 1, 1, 1, 1, 0, 704, 100
29272, V, 1, 1, 1, 1, 0, 704, 100
29273, V, 1, 1, 1, 1, 0, 704, 100
29274, V, 1, 1, 1, 1, 0, 704, 100
29275, V, 1, 1, 1, 1, 0, 704, 100
29276, V, 1, 1, 1, 1, 0, 704, 100
29277, V, 1, 1, 1, 1, 0, 704, 100
29278, V, 1, 1, 1, 1, 0, 704, 100
29279, V, 1, 1, 1, 1, 0, 704, 100
29280, V, 1, 1, 1, 1, 0, 704, 100
29281, V, 1, 1, 1, 1, 0, 704, 100
29282, V, 1, 1, 1, 1, 0, 704, 100
29283, V, 1, 1, 1, 1, 0, 704, 100
29284, V, 1, 1, 1, 1, 0, 704, 100
29285, V, 1, 1, 1, 1, 0, 704, 100
29286, V, 1, 1, 1, 1, 0, 704, 100
29287, V, 1, 1, 1, 1, 0, 704, 100
29288, V, 1, 1, 1, 1, 0, 704, 100
29289, V, 1, 1, 1, 1, 0, 704, 100
29290, V, 1, 1, 1, 1, 0, 704, 100
29291, V, 1, 1, 1, 1, 0, 704, 100
29292, V, 1, 1, 1, 1, 0, 704, 100
29293, V, 1, 1, 1, 1, 0, 704, 100
29294, V, 1, 1, 1, 1, 0, 704, 100
29295, V, 1, 1, 1, 1, 0, 704, 100
29296, V, 1, 1, 1, 1, 0, 704, 100
29297, V, 1, 1, 1, 1, 0, 704, 100
29298, V, 1, 1, 1, 1, 0, 704, 100
29299, V, 1, 1, 1, 1, 0, 704, 100
29300, V, 1, 1, 1, 1, 0, 704, 100
29301, V, 1, 1, 1, 1, 0, 704, 100
29302, V, 1, 1, 1, 1, 0, 704, 100
29303, V, 1, 1, 1, 1, 0, 704, 100
29304, V, 1, 1, 1, 1, 0, 704, 100
29305, V, 1, 1, 1, 1, 0, 704, 100
29306, V, 1, 1, 1, 1, 0, 704, 100
29307, V, 1, 1, 1, 1, 0, 704, 100
29308, V, 1, 1, 1, 1, 0, 704, 100
29309, V, 1, 1, 1, 1, 0, 704, 100
29310, V, 1, 1, 1, 1, 0, 704, 100
29312, V, 1, 1, 1, 1, 0, 704, 100
29313, V, 1, 1, 1, 1, 0, 704, 100
29314, V, 1, 1, 1, 1, 0, 704, 100
29315, V, 1, 1, 1, 1, 0, 704, 100
29316, V, 1, 1, 1, 1, 0, 704, 100
29317, V, 1, 1, 1, 1, 0, 704, 100
29318, V, 1, 1, 1, 1, 0, 704, 100
29319, V, 1, 1, 1, 1, 0, 704, 100
29320, V, 1, 1, 1, 1, 0, 704, 100
29321, V, 1, 1, 1, 1, 0, 704, 100
29322, V, 1, 1, 1, 1, 0, 704, 100
29323, V, 1, 1, 1, 1, 0, 704, 100
29324, V, 1, 1, 1, 1, 0, 704, 100
29325, V, 1, 1, 1, 1, 0, 704, 100
29326, V, 1, 1, 1, 1, 0, 704, 100
29327, V, 1, 1, 1, 1, 0, 704, 100
29328, V, 1, 1, 1, 1, 0, 704, 100
29329, V, 1, 1, 1, 1, 0, 704, 100
29330, V, 1, 1, 1, 1, 0, 704, 100
29331, V, 1, 1, 1, 1, 0, 704, 100
29332, V, 1, 1, 1, 1, 0, 704, 100
29333, V, 1, 1, 1, 1, 0, 704, 100
29334, V, 1, 1, 1, 1, 0, 704, 100
29335, V, 1, 1, 1, 1, 0, 704, 100
29336, V, 1, 1, 1, 1, 0, 704, 100
29337, V, 1, 1, 1, 1, 0, 704, 100
29338, V, 1, 1, 1, 1, 0, 704, 100
29339, V, 1, 1, 1, 1, 0, 704, 100
29340, V, 1, 1, 1, 1, 0, 704, 100
29341, V, 1, 1, 1, 1, 0, 704, 100
29342, V, 1, 1, 1, 1, 0, 704, 100
29343, V, 1, 1, 1, 1, 0, 704, 100
29344, V, 1, 1, 1, 1, 0, 704, 100
29345, V, 1, 1, 1, 1, 0, 704, 100
29346, V, 1, 1, 1, 1, 0, 704, 100
29347, V, 1, 1, 1, 1, 0, 704, 100
29348, V, 1, 1, 1, 1, 0, 704, 100
29349, V, 1, 1, 1, 1, 0, 704, 100
29350, V, 1, 1, 1, 1, 0, 704, 100
29351, V, 1, 1, 1, 1, 0, 704, 100
29352, V, 1, 1, 1, 1, 0, 704, 100
29353, V, 1, 1, 1, 1, 0, 704, 100
29355, V, 1, 1, 1, 1, 0, 704, 100
29356, V, 1, 1, 1, 1, 0, 704, 100
29357, V, 1, 1, 1, 1, 0, 704, 100
29358, V, 1, 1, 1, 1, 0, 704, 100
29359, V, 1, 1, 1, 1, 0, 704, 100
29360, V, 1, 1, 1, 1, 0, 704, 100
29361, V, 1, 1, 1, 1, 0, 704, 100
29362, V, 1, 1, 1, 1, 0, 704, 100
29363, V, 1, 1, 1, 1, 0, 704, 100
29364, V, 1, 1, 1, 1, 0, 704, 100
29365, V, 1, 1, 1, 1, 0, 704, 100
29366, V, 1, 1, 1, 1, 0, 704, 100
29367, V, 1, 1, 1, 1, 0, 704, 100
29368, V, 1, 1, 1, 1, 0, 704, 100
29369, V, 1, 1, 1, 1, 0, 704, 100
29370, V, 1, 1, 1, 1, 0, 704, 100
29371, V, 1, 1, 1, 1, 0, 704, 100
29372, V, 1, 1, 1, 1, 0, 704, 100
29373, V, 1, 1, 1, 1, 0, 704, 100
29374, V, 1, 1, 1, 1, 0, 704, 100
29375, V, 1, 1, 1, 1, 0, 704, 100
29376, V, 1, 1, 1, 1, 0, 704, 100
29377, V, 1, 1, 1, 1, 0, 704, 100
29378, V, 1, 1, 1, 1, 0, 704, 100
29379, V, 1, 1, 1, 1, 0, 704, 100
29380, V, 1, 1, 1, 1, 0, 704, 100
29381, V, 1, 1, 1, 1, 0, 704, 100
29382, V, 1, 1, 1, 1, 0, 704, 100
29383, V, 1, 1, 1, 1, 0, 704, 100
29384, V, 1, 1, 1, 1, 0, 704, 100
29385, V, 1, 1, 1, 1, 0, 704, 100
29386, V, 1, 1, 1, 1, 0, 704, 100
29387, V, 1, 1, 1, 1, 0, 704, 100
29388, V, 1, 1, 1, 1, 0, 704, 100
29389, V, 1, 1, 1, 1, 0, 704, 100
29390, V, 1, 1, 1, 1, 0, 704, 100
29391, V, 1, 1, 1, 1, 0, 704, 100
29392, V, 1, 1, 1, 1, 0, 704, 100
29393, V, 1, 1, 1, 1, 0, 704, 100
29394, V, 1, 1, 1, 1, 0, 704, 100
29395, V, 1, 1, 1, 1, 0, 704, 100
29396, V, 1, 1, 1, 1, 0, 704, 100
29398, V, 1, 1, 1, 1, 0, 704, 100
29399, V, 1, 1, 1, 1, 0, 704, 100
29400, V, 1, 1, 1, 1, 0, 704, 100
29401, V, 1, 1, 1, 1, 0, 704, 100
29402, V, 1, 1, 1, 1, 0, 704, 100
29403, V, 1, 1, 1, 1, 0, 704, 100
29404, V, 1, 1, 1, 1, 0, 704, 100
29405, V, 1, 1, 1, 1, 0, 704, 100
29406, V, 1, 1, 1, 1, 0, 704, 100
29407, V, 1, 1, 1, 1, 0, 704, 100
29408, V, 1, 1, 1, 1, 0, 704, 100
29409, V, 1, 1, 1, 1, 0, 704, 100
29410, V, 1, 1, 1, 1, 0, 704, 100
29411, V, 1, 1, 1, 1, 0, 704, 100
29412, V, 1, 1, 1, 1, 0, 704, 100
29413, V, 1, 1, 1, 1, 0, 704, 100
29414, V, 1, 1, 1, 1, 0, 704, 100
29415, V, 1, 1, 1, 1, 0, 704, 100
29416, V, 1, 1, 1, 1, 0, 704, 100
29417, V, 1, 1, 1, 1, 0, 704, 100
29418, V, 1, 1, 1, 1, 0, 704, 100
29419, V, 1, 1, 1, 1, 0, 704, 100
29420, V, 1, 1, 1, 1, 0, 704, 100
29421, V, 1, 1, 1, 1, 0, 704, 100
29422, V, 1, 1, 1, 1, 0, 704, 100
29423, V, 1, 1, 1, 1, 0, 704, 100
29424, V, 1, 1, 1, 1, 0, 704, 100
29425, V, 1, 1, 1, 1, 0, 704, 100
29426, V, 1, 1, 1, 1, 0, 704, 100
29427, V, 1, 1, 1, 1, 0, 704, 100
29428, V, 1, 1, 1, 1, 0, 704, 100
29429, V, 1, 1, 1, 1, 0, 704, 100
29430, V, 1, 1, 1, 1, 0, 704, 100
29431, V, 1, 1, 1, 1, 0, 704, 100
29432, V, 1, 1, 1, 1, 0, 704, 100
29433, V, 1, 1, 1, 1, 0, 704, 100
29434, V, 1, 1, 1, 1, 0, 704, 100
29435, V, 1, 1, 1, 1, 0, 704, 100
29436, V, 1, 1, 1, 1, 0, 704, 100
29437, V, 1, 1, 1, 1, 0, 704, 100
29438, V, 1, 1, 1, 1, 0, 704, 100
29440, V, 1, 1, 1, 1, 0, 704, 100
29441, V, 1, 1, 1, 1, 0, 704, 100
29442, V, 1, 1, 1, 1, 0, 704, 100
29443, V, 1, 1, 1, 1, 0, 704, 100
29444, V, 1, 1, 1, 1, 0, 704, 100
29445, V, 1, 1, 1, 1, 0, 704, 100
29446, V, 1, 1, 1, 1, 0, 704, 100
29447, V, 1, 1, 1, 1, 0, 704, 100
29448, V, 1, 1, 1, 1, 0, 704, 100
29449, V, 1, 1, 1, 1, 0, 704, 100
29450, V, 1, 1, 1, 1, 0, 704, 100
29451, V, 1, 1, 1, 1, 0, 704, 100
29452, V, 1, 1, 1, 1, 0, 704, 100
29453, V, 1, 1, 1, 1, 0, 704, 100
29454, V, 1, 1, 1, 1, 0, 704, 100
29455, V, 1, 1, 1, 1, 0, 704, 100
29456, V, 1, 1, 1, 1, 0, 704, 100
29457, V, 1, 1, 1, 1, 0, 704, 100
29458, V, 1, 1, 1, 1, 0, 704, 100
29459, V, 1, 1, 1, 1, 0, 704, 100
29460, V, 1, 1, 1, 1, 0, 704, 100
29461, V, 1, 1, 1, 1, 0, 704, 100
29462, V, 1, 1, 1, 1, 0, 704, 100
29463, V, 1, 1, 1, 1, 0, 704, 100
29464, V, 1, 1, 1, 1, 0, 704, 100
29465, V, 1, 1, 1, 1, 0, 704, 100
29466, V, 1, 1, 1, 1, 0, 704, 100
29467, V, 1, 1, 1, 1, 0, 704, 100
29468, V, 1, 1, 1, 1, 0, 704, 100
29469, V, 1, 1, 1, 1, 0, 704, 100
29470, V, 1, 1, 1, 1, 0, 704, 100
29471, V, 1, 1, 1, 1, 0, 704, 100
29472, V, 1, 1, 1, 1, 0, 704, 100
29473, V, 1, 1, 1, 1, 0, 704, 100
29474, V, 1, 1, 1, 1, 0, 704, 100
29475, V, 1, 1, 1, 1, 0, 704, 100
29476, V, 1, 1, 1, 1, 0, 704, 100
29477, V, 1, 1, 1, 1, 0, 704, 100
29478, V, 1, 1, 1, 1, 0, 704, 100
29479, V, 1, 1, 1, 1, 0, 704, 100
29480, V, 1, 1, 1, 1, 0, 704, 100
29481, V, 1, 1, 1, 1, 0, 704, 100
29483, V, 1, 1, 1, 1, 0, 704, 100
29484, V, 1, 1, 1, 1, 0, 704, 100
29485, V, 1, 1, 1, 1, 0, 704, 100
29486, V, 1, 1, 1, 1, 0, 704, 100
29487, V, 1, 1, 1, 1, 0, 704, 100
29488, V, 1, 1, 1, 1, 0, 704, 100
29489, V, 1, 1, 1, 1, 0, 704, 100
29490, V, 1, 1, 1, 1, 0, 704, 100
29491, V, 1, 1, 1, 1, 0, 704, 100
29492, V, 1, 1, 1, 1, 0, 704, 100
29493, V, 1, 1, 1, 1, 0, 704, 100
29494, V, 1, 1, 1, 1, 0, 704, 100
29495, V, 1, 1, 1, 1, 0, 704, 100
29496, V, 1, 1, 1, 1, 0, 704, 100
29497, V, 1, 1, 1, 1, 0, 704, 100
29498, V, 1, 1, 1, 1, 0, 704, 100
29499, V, 1, 1, 1, 1, 0, 704, 100
29500, V, 1, 1, 1, 1, 0, 704, 100
29501, V, 1, 1, 1, 1, 0, 704, 100
29502, V, 1, 1, 1, 1, 0, 704, 100
29503, V, 1, 1, 1, 1, 0, 704, 100
29504, V, 1, 1, 1, 1, 0, 704, 100
29505, V, 1, 1, 1, 1, 0, 704, 100
29506, V, 1, 1, 1, 1, 0, 704, 100
29507, V, 1, 1, 1, 1, 0, 704, 100
29508, V, 1, 1, 1, 1, 0, 704, 100
29509, V, 1, 1, 1, 1, 0, 704, 100
29510, V, 1, 1, 1, 1, 0, 704, 100
29511, V, 1, 1, 1, 1, 0, 704, 100
29512, V, 1, 1, 1, 1, 0, 704, 100
29513, V, 1, 1, 1, 1, 0, 704, 100
29514, V, 1, 1, 1, 1, 0, 704, 100
29515, V, 1, 1, 1, 1, 0, 704, 100
29516, V, 1, 1, 1, 1, 0, 704, 100
29517, V, 1, 1, 1, 1, 0, 704, 100
29518, V, 1, 1, 1, 1, 0, 704, 100
29519, V, 1, 1, 1, 1, 0, 704, 100
29520, V, 1, 1, 1, 1, 0, 704, 100
29521, V, 1, 1, 1, 1, 0, 704, 100
29522, V, 1, 1, 1, 1, 0, 704, 100
29523, V, 1, 1, 1, 1, 0, 704, 100
29524, V, 1, 1, 1, 1, 0, 704, 100
29526, V, 1, 1, 1, 1, 0, 704, 100
29527, V, 1, 1, 1, 1, 0, 704, 100
29528, V, 1, 1, 1, 1, 0, 704, 100
29529, V, 1, 1, 1, 1, 0, 704, 100
29530, V, 1, 1, 1, 1, 0, 704, 100
29531, V, 1, 1, 1, 1, 0, 704, 100
29532, V, 1, 1, 1, 1, 0, 704, 100
29533, V, 1, 1, 1, 1, 0, 704, 100
29534, V, 1, 1, 1, 1, 0, 704, 100
29535, V, 1, 1, 1, 1, 0, 704, 100
29536, V, 1, 1, 1, 1, 0, 704, 100
29537, V, 1, 1, 1, 1, 0, 704, 100
29538, V, 1, 1, 1, 1, 0, 704, 100
29539, V, 1, 1, 1, 1, 0, 704, 100
29540, V, 1, 1, 1, 1, 0, 704, 100
29541, V, 1, 1, 1, 1, 0, 704, 100
29542, V, 1, 1, 1, 1, 0, 704, 100
29543, V, 1, 1, 1, 1, 0, 704, 100
29544, V, 1, 1, 1, 1, 0, 704, 100
29545, V, 1, 1, 1, 1, 0, 704, 100
29546, V, 1, 1, 1, 1, 0, 704, 100
29547, V, 1, 1, 1, 1, 0, 704, 100
29548, V, 1, 1, 1, 1, 0, 704, 100
29549, V, 1, 1, 1, 1, 0, 704, 100
29550, V, 1, 1, 1, 1, 0, 704, 100
29551, V, 1, 1, 1, 1, 0, 704, 100
29552, V, 1, 1, 1, 1, 0, 704, 100
29553, V, 1, 1, 1, 1, 0, 704, 100
29554, V, 1, 1, 1, 1, 0, 704, 100
29555, V, 1, 1, 1, 1, 0, 704, 100
29556, V, 1, 1, 1, 1, 0, 704, 100
29557, V, 1, 1, 1, 1, 0, 704, 100
29558, V, 1, 1, 1, 1, 0, 704, 100
29559, V, 1, 1, 1, 1, 0, 704, 100
29560, V, 1, 1, 1, 1, 0, 704, 100
29561, V, 1, 1, 1, 1, 0, 704, 100
29562, V, 1, 1, 1, 1, 0, 704, 100
29563, V, 1, 1, 1, 1, 0, 704, 100
29564, V, 1, 1, 1, 1, 0, 704, 100
29565, V, 1, 1, 1, 1, 0, 704, 100
29566, V, 1, 1, 1, 1, 0, 704, 100
29568, V, 1, 1, 1, 1, 0, 704, 100
29569, V, 1, 1, 1, 1, 0, 704, 100
29570, V, 1, 1, 1, 1, 0, 704, 100
29571, V, 1, 1, 1, 1, 0, 704, 100
29572, V, 1, 1, 1, 1, 0, 704, 100
29573, V, 1, 1, 1, 1, 0, 704, 100
29574, V, 1, 1, 1, 1, 0, 704, 100
29575, V, 1, 1, 1, 1, 0, 704, 100
29576, V, 1, 1, 1, 1, 0, 704, 100
29577, V, 1, 1, 1, 1, 0, 704, 100
29578, V, 1, 1, 1, 1, 0, 704, 100
29579, V, 1, 1, 1, 1, 0, 704, 100
29580, V, 1, 1, 1, 1, 0, 704, 100
29581, V, 1, 1, 1, 1, 0, 704, 100
29582, V, 1, 1, 1, 1, 0, 704, 100
29583, V, 1, 1, 1, 1, 0, 704, 100
29584, V, 1, 1, 1, 1, 0, 704, 100
29585, V, 1, 1, 1, 1, 0, 704, 100
29586, V, 1, 1, 1, 1, 0, 704, 100
29587, V, 1, 1, 1, 1, 0, 704, 100
29588, V, 1, 1, 1, 1, 0, 704, 100
29589, V, 1, 1, 1, 1, 0, 704, 100
29590, V, 1, 1, 1, 1, 0, 704, 100
29591, V, 1, 1, 1, 1, 0, 704, 100
29592, V, 1, 1, 1, 1, 0, 704, 100
29593, V, 1, 1, 1, 1, 0, 704, 100
29594, V, 1, 1, 1, 1, 0, 704, 100
29595, V, 1, 1, 1, 1, 0, 704, 100
29596, V, 1, 1, 1, 1, 0, 704, 100
29597, V, 1, 1, 1, 1, 0, 704, 100
29598, V, 1, 1, 1, 1, 0, 704, 100
29599, V, 1, 1, 1, 1, 0, 704, 100
29600, V, 1, 1, 1, 1, 0, 704, 100
29601, V, 1, 1, 1, 1, 0, 704, 100
29602, V, 1, 1, 1, 1, 0, 704, 100
29603, V, 1, 1, 1, 1, 0, 704, 100
29604, V, 1, 1, 1, 1, 0, 704, 100
29605, V, 1, 1, 1, 1, 0, 704, 100
29606, V, 1, 1, 1, 1, 0, 704, 100
29607, V, 1, 1, 1, 1, 0, 704, 100
29608, V, 1, 1, 1, 1, 0, 704, 100
29609, V, 1, 1, 1, 1, 0, 704, 100
29611, V, 1, 1, 1, 1, 0, 704, 100
29612, V, 1, 1, 1, 1, 0, 704, 100
29613, V, 1, 1, 1, 1, 0, 704, 100
29614, V, 1, 1, 1, 1, 0, 704, 100
29615, V, 1, 1, 1, 1, 0, 704, 100
29616, V, 1, 1, 1, 1, 0, 704, 100
29617, V, 1, 1, 1, 1, 0, 704, 100
29618, V, 1, 1, 1, 1, 0, 704, 100
29619, V, 1, 1, 1, 1, 0, 704, 100
29620, V, 1, 1, 1, 1, 0, 704, 100
29621, V, 1, 1, 1, 1, 0, 704, 100
29622, V, 1, 1, 1, 1, 0, 704, 100
29623, V, 1, 1, 1, 1, 0, 704, 100
29624, V, 1, 1, 1, 1, 0, 704, 100
29625, V, 1, 1, 1, 1, 0, 704, 100
29626, V, 1, 1, 1, 1, 0, 704, 100
29627, V, 1, 1, 1, 1, 0, 704, 100
29628, V, 1, 1, 1, 1, 0, 704, 100
29629, V, 1, 1, 1, 1, 0, 704, 100
29630, V, 1, 1, 1, 1, 0, 704, 100
29631, V, 1, 1, 1, 1, 0, 704, 100
29632, V, 1, 1, 1, 1, 0, 704, 100
29633, V, 1, 1, 1, 1, 0, 704, 100
29634, V, 1, 1, 1, 1, 0, 704, 100
29635, V, 1, 1, 1, 1, 0, 704, 100
29636, V, 1, 1, 1, 1, 0, 704, 100
29637, V, 1, 1, 1, 1, 0, 704, 100
29638, V, 1, 1, 1, 1, 0, 704, 100
29639, V, 1, 1, 1, 1, 0, 704, 100
29640, V, 1, 1, 1, 1, 0, 704, 100
29641, V, 1, 1, 1, 1, 0, 704, 100
29642, V, 1, 1, 1, 1, 0, 704, 100
29643, V, 1, 1, 1, 1, 0, 704, 100
29644, V, 1, 1, 1, 1, 0, 704, 100
29645, V, 1, 1, 1, 1, 0, 704, 100
29646, V, 1, 1, 1, 1, 0, 704, 100
29647, V, 1, 1, 1, 1, 0, 704, 100
29648, V, 1, 1, 1, 1, 0, 704, 100
29649, V, 1, 1, 1, 1, 0, 704, 100
29650, V, 1, 1, 1, 1, 0, 704, 100
29651, V, 1, 1, 1, 1, 0, 704, 100
29652, V, 1, 1, 1, 1, 0, 704, 100
29654, V, 1, 1, 1, 1, 0, 704, 100
29655, V, 1, 1, 1, 1, 0, 704, 100
29656, V, 1, 1, 1, 1, 0, 704, 100
29657, V, 1, 1, 1, 1, 0, 704, 100
29658, V, 1, 1, 1, 1, 0, 704, 100
29659, V, 1, 1, 1, 1, 0, 704, 100
29660, V, 1, 1, 1, 1, 0, 704, 100
29661, V, 1, 1, 1, 1, 0, 704, 100
29662, V, 1, 1, 1, 1, 0, 704, 100
29663, V, 1, 1, 1, 1, 0, 704, 100
29664, V, 1, 1, 1, 1, 0, 704, 100
29665, V, 1, 1, 1, 1, 0, 704, 100
29666, V, 1, 1, 1, 1, 0, 704, 100
29667, V, 1, 1, 1, 1, 0, 704, 100
29668, V, 1, 1, 1, 1, 0, 704, 100
29669, V, 1, 1, 1, 1, 0, 704, 100
29670, V, 1, 1, 1, 1, 0, 704, 100
29671, V, 1, 1, 1, 1, 0, 704, 100
29672, V, 1, 1, 1, 1, 0, 704, 100
29673, V, 1, 1, 1, 1, 0, 704, 100
29674, V, 1, 1, 1, 1, 0, 704, 100
29675, V, 1, 1, 1, 1, 0, 704, 100
29676, V, 1, 1, 1, 1, 0, 704, 100
29677, V, 1, 1, 1, 1, 0, 704, 100
29678, V, 1, 1, 1, 1, 0, 704, 100
29679, V, 1, 1, 1, 1, 0, 704, 100
29680, V, 1, 1, 1, 1, 0, 704, 100
29681, V, 1, 1, 1, 1, 0, 704, 100
29682, V, 1, 1, 1, 1, 0, 704, 100
29683, V, 1, 1, 1, 1, 0, 704, 100
29684, V, 1, 1, 1, 1, 0, 704, 100
29685, V, 1, 1, 1, 1, 0, 704, 100
29686, V, 1, 1, 1, 1, 0, 704, 100
29687, V, 1, 1, 1, 1, 0, 704, 100
29688, V, 1, 1, 1, 1, 0, 704, 100
29689, V, 1, 1, 1, 1, 0, 704, 100
29690, V, 1, 1, 1, 1, 0, 704, 100
29691, V, 1, 1, 1, 1, 0, 704, 100
29692, V, 1, 1, 1, 1, 0, 704, 100
29693, V, 1, 1, 1, 1, 0, 704, 100
29694, V, 1, 1, 1, 1, 0, 704, 100
29696, V, 1, 1, 1, 1, 0, 704, 100
29697, V, 1, 1, 1, 1, 0, 704, 100
29698, V, 1, 1, 1, 1, 0, 704, 100
29699, V, 1, 1, 1, 1, 0, 704, 100
29700, V, 1, 1, 1, 1, 0, 704, 100
29701, V, 1, 1, 1, 1, 0, 704, 100
29702, V, 1, 1, 1, 1, 0, 704, 100
29703, V, 1, 1, 1, 1, 0, 704, 100
29704, V, 1, 1, 1, 1, 0, 704, 100
29705, V, 1, 1, 1, 1, 0, 704, 100
29706, V, 1, 1, 1, 1, 0, 704, 100
29707, V, 1, 1, 1, 1, 0, 704, 100
29708, V, 1, 1, 1, 1, 0, 704, 100
29709, V, 1, 1, 1, 1, 0, 704, 100
29710, V, 1, 1, 1, 1, 0, 704, 100
29711, V, 1, 1, 1, 1, 0, 704, 100
29712, V, 1, 1, 1, 1, 0, 704, 100
29713, V, 1, 1, 1, 1, 0, 704, 100
29714, V, 1, 1, 1, 1, 0, 704, 100
29715, V, 1, 1, 1, 1, 0, 704, 100
29716, V, 1, 1, 1, 1, 0, 704, 100
29717, V, 1, 1, 1, 1, 0, 704, 100
29718, V, 1, 1, 1, 1, 0, 704, 100
29719, V, 1, 1, 1, 1, 0, 704, 100
29720, V, 1, 1, 1, 1, 0, 704, 100
29721, V, 1, 1, 1, 1, 0, 704, 100
29722, V, 1, 1, 1, 1, 0, 704, 100
29723, V, 1, 1, 1, 1, 0, 704, 100
29724, V, 1, 1, 1, 1, 0, 704, 100
29725, V, 1, 1, 1, 1, 0, 704, 100
29726, V, 1, 1, 1, 1, 0, 704, 100
29727, V, 1, 1, 1, 1, 0, 704, 100
29728, V, 1, 1, 1, 1, 0, 704, 100
29729, V, 1, 1, 1, 1, 0, 704, 100
29730, V, 1, 1, 1, 1, 0, 704, 100
29731, V, 1, 1, 1, 1, 0, 704, 100
29732, V, 1, 1, 1, 1, 0, 704, 100
29733, V, 1, 1, 1, 1, 0, 704, 100
29734, V, 1, 1, 1, 1, 0, 704, 100
29735, V, 1, 1, 1, 1, 0, 704, 100
29736, V, 1, 1, 1, 1, 0, 704, 100
29737, V, 1, 1, 1, 1, 0, 704, 100
29739, V, 1, 1, 1, 1, 0, 704, 100
29740, V, 1, 1, 1, 1, 0, 704, 100
29741, V, 1, 1, 1, 1, 0, 704, 100
29742, V, 1, 1, 1, 1, 0, 704, 100
29743, V, 1, 1, 1, 1, 0, 704, 100
29744, V, 1, 1, 1, 1, 0, 704, 100
29745, V, 1, 1, 1, 1, 0, 704, 100
29746, V, 1, 1, 1, 1, 0, 704, 100
29747, V, 1, 1, 1, 1, 0, 704, 100
29748, V, 1, 1, 1, 1, 0, 704, 100
29749, V, 1, 1, 1, 1, 0, 704, 100
29750, V, 1, 1, 1, 1, 0, 704, 100
29751, V, 1, 1, 1, 1, 0, 704, 100
29752, V, 1, 1, 1, 1, 0, 704, 100
29753, V, 1, 1, 1, 1, 0, 704, 100
29754, V, 1, 1, 1, 1, 0, 704, 100
29755, V, 1, 1, 1, 1, 0, 704, 100
29756, V, 1, 1, 1, 1, 0, 704, 100
29757, V, 1, 1, 1, 1, 0, 704, 100
29758, V, 1, 1, 1, 1, 0, 704, 100
29759, V, 1, 1, 1, 1, 0, 704, 100
29760, V, 1, 1, 1, 1, 0, 704, 100
29761, V, 1, 1, 1, 1, 0, 704, 100
29762, V, 1, 1, 1, 1, 0, 704, 100
29763, V, 1, 1, 1, 1, 0, 704, 100
29764, V, 1, 1, 1, 1, 0, 704, 100
29765, V, 1, 1, 1, 1, 0, 704, 100
29766, V, 1, 1, 1, 1, 0, 704, 100
29767, V, 1, 1, 1, 1, 0, 704, 100
29768, V, 1, 1, 1, 1, 0, 704, 100
29769, V, 1, 1, 1, 1, 0, 704, 100
29770, V, 1, 1, 1, 1, 0, 704, 100
29771, V, 1, 1, 1, 1, 0, 704, 100
29772, V, 1, 1, 1, 1, 0, 704, 100
29773, V, 1, 1, 1, 1, 0, 704, 100
29774, V, 1, 1, 1, 1, 0, 704, 100
29775, V, 1, 1, 1, 1, 0, 704, 100
29776, V, 1, 1, 1, 1, 0, 704, 100
29777, V, 1, 1, 1, 1, 0, 704, 100
29778, V, 1, 1, 1, 1, 0, 704, 100
29779, V, 1, 1, 1, 1, 0, 704, 100
29780, V, 1, 1, 1, 1, 0, 704, 100
29782, V, 1, 1, 1, 1, 0, 704, 100
29783, V, 1, 1, 1, 1, 0, 704, 100
29784, V, 1, 1, 1, 1, 0, 704, 100
29785, V, 1, 1, 1, 1, 0, 704, 100
29786, V, 1, 1, 1, 1, 0, 704, 100
29787, V, 1, 1, 1, 1, 0, 704, 100
29788, V, 1, 1, 1, 1, 0, 704, 100
29789, V, 1, 1, 1, 1, 0, 704, 100
29790, V, 1, 1, 1, 1, 0, 704, 100
29791, V, 1, 1, 1, 1, 0, 704, 100
29792, V, 1, 1, 1, 1, 0, 704, 100
29793, V, 1, 1, 1, 1, 0, 704, 100
29794, V, 1, 1, 1, 1, 0, 704, 100
29795, V, 1, 1, 1, 1, 0, 704, 100
29796, V, 1, 1, 1, 1, 0, 704, 100
29797, V, 1, 1, 1, 1, 0, 704, 100
29798, V, 1, 1, 1, 1, 0, 704, 100
29799, V, 1, 1, 1, 1, 0, 704, 100
29800, V, 1, 1, 1, 1, 0, 704, 100
29801, V, 1, 1, 1, 1, 0, 704, 100
29802, V, 1, 1, 1, 1, 0, 704, 100
29803, V, 1, 1, 1, 1, 0, 704, 100
29804, V, 1, 1, 1, 1, 0, 704, 100
29805, V, 1, 1, 1, 1, 0, 704, 100
29806, V, 1, 1, 1, 1, 0, 704, 100
29807, V, 1, 1, 1, 1, 0, 704, 100
29808, V, 1, 1, 1, 1, 0, 704, 100
29809, V, 1, 1, 1, 1, 0, 704, 100
29810, V, 1, 1, 1, 1, 0, 704, 100
29811, V, 1, 1, 1, 1, 0, 704, 100
29812, V, 1, 1, 1, 1, 0, 704, 100
29813, V, 1, 1, 1, 1, 0, 704, 100
29814, V, 1, 1, 1, 1, 0, 704, 100
29815, V, 1, 1, 1, 1, 0, 704, 100
29816, V, 1, 1, 1, 1, 0, 704, 100
29817, V, 1, 1, 1, 1, 0, 704, 100
29818, V, 1, 1, 1, 1, 0, 704, 100
29819, V, 1, 1, 1, 1, 0, 704, 100
29820, V, 1, 1, 1, 1, 0, 704, 100
29821, V, 1, 1, 1, 1, 0, 704, 100
29822, V, 1, 1, 1, 1, 0, 704, 100
29824, V, 1, 1, 1, 1, 0, 704, 100
29825, V, 1, 1, 1, 1, 0, 704, 100
29826, V, 1, 1, 1, 1, 0, 704, 100
29827, V, 1, 1, 1, 1, 0, 704, 100
29828, V, 1, 1, 1, 1, 0, 704, 100
29829, V, 1, 1, 1, 1, 0, 704, 100
29830, V, 1, 1, 1, 1, 0, 704, 100
29831, V, 1, 1, 1, 1, 0, 704, 100
29832, V, 1, 1, 1, 1, 0, 704, 100
29833, V, 1, 1, 1, 1, 0, 704, 100
29834, V, 1, 1, 1, 1, 0, 704, 100
29835, V, 1, 1, 1, 1, 0, 704, 100
29836, V, 1, 1, 1, 1, 0, 704, 100
29837, V, 1, 1, 1, 1, 0, 704, 100
29838, V, 1, 1, 1, 1, 0, 704, 100
29839, V, 1, 1, 1, 1, 0, 704, 100
29840, V, 1, 1, 1, 1, 0, 704, 100
29841, V, 1, 1, 1, 1, 0, 704, 100
29842, V, 1, 1, 1, 1, 0, 704, 100
29843, V, 1, 1, 1, 1, 0, 704, 100
29844, V, 1, 1, 1, 1, 0, 704, 100
29845, V, 1, 1, 1, 1, 0, 704, 100
29846, V, 1, 1, 1, 1, 0, 704, 100
29847, V, 1, 1, 1, 1, 0, 704, 100
29848, V, 1, 1, 1, 1, 0, 704, 100
29849, V, 1, 1, 1, 1, 0, 704, 100
29850, V, 1, 1, 1, 1, 0, 704, 100
29851, V, 1, 1, 1, 1, 0, 704, 100
29852, V, 1, 1, 1, 1, 0, 704, 100
29853, V, 1, 1, 1, 1, 0, 704, 100
29854, V, 1, 1, 1, 1, 0, 704, 100
29855, V, 1, 1, 1, 1, 0, 704, 100
29856, V, 1, 1, 1, 1, 0, 704, 100
29857, V, 1, 1, 1, 1, 0, 704, 100
29858, V, 1, 1, 1, 1, 0, 704, 100
29859, V, 1, 1, 1, 1, 0, 704, 100
29860, V, 1, 1, 1, 1, 0, 704, 100
29861, V, 1, 1, 1, 1, 0, 704, 100
29862, V, 1, 1, 1, 1, 0, 704, 100
29863, V, 1, 1, 1, 1, 0, 704, 100
29864, V, 1, 1, 1, 1, 0, 704, 100
29865, V, 1, 1, 1, 1, 0, 704, 100
29867, V, 1, 1, 1, 1, 0, 704, 100
29868, V, 1, 1, 1, 1, 0, 704, 100
29869, V, 1, 1, 1, 1, 0, 704, 100
29870, V, 1, 1, 1, 1, 0, 704, 100
29871, V, 1, 1, 1, 1, 0, 704, 100
29872, V, 1, 1, 1, 1, 0, 704, 100
29873, V, 1, 1, 1, 1, 0, 704, 100
29874, V, 1, 1, 1, 1, 0, 704, 100
29875, V, 1, 1, 1, 1, 0, 704, 100
29876, V, 1, 1, 1, 1, 0, 704, 100
29877, V, 1, 1, 1, 1, 0, 704, 100
29878, V, 1, 1, 1, 1, 0, 704, 100
29879, V, 1, 1, 1, 1, 0, 704, 100
29880, V, 1, 1, 1, 1, 0, 704, 100
29881, V, 1, 1, 1, 1, 0, 704, 100
29882, V, 1, 1, 1, 1, 0, 704, 100
29883, V, 1, 1, 1, 1, 0, 704, 100
29884, V, 1, 1, 1, 1, 0, 704, 100
29885, V, 1, 1, 1, 1, 0, 704, 100
29886, V, 1, 1, 1, 1, 0, 704, 100
29887, V, 1, 1, 1, 1, 0, 704, 100
29888, V, 1, 1, 1, 1, 0, 704, 100
29889, V, 1, 1, 1, 1, 0, 704, 100
29890, V, 1, 1, 1, 1, 0, 704, 100
29891, V, 1, 1, 1, 1, 0, 704, 100
29892, V, 1, 1, 1, 1, 0, 704, 100
29893, V, 1, 1, 1, 1, 0, 704, 100
29894, V, 1, 1, 1, 1, 0, 704, 100
29895, V, 1, 1, 1, 1, 0, 704, 100
29896, V, 1, 1, 1, 1, 0, 704, 100
29897, V, 1, 1, 1, 1, 0, 704, 100
29898, V, 1, 1, 1, 1, 0, 704, 100
29899, V, 1, 1, 1, 1, 0, 704, 100
29900, V, 1, 1, 1, 1, 0, 704, 100
29901, V, 1, 1, 1, 1, 0, 704, 100
29902, V, 1, 1, 1, 1, 0, 704, 100
29903, V, 1, 1, 1, 1, 0, 704, 100
29904, V, 1, 1, 1, 1, 0, 704, 100
29905, V, 1, 1, 1, 1, 0, 704, 100
29906, V, 1, 1, 1, 1, 0, 704, 100
29907, V, 1, 1, 1, 1, 0, 704, 100
29908, V, 1, 1, 1, 1, 0, 704, 100
29910, V, 1, 1, 1, 1, 0, 704, 100
29911, V, 1, 1, 1, 1, 0, 704, 100
29912, V, 1, 1, 1, 1, 0, 704, 100
29913, V, 1, 1, 1, 1, 0, 704, 100
29914, V, 1, 1, 1, 1, 0, 704, 100
29915, V, 1, 1, 1, 1, 0, 704, 100
29916, V, 1, 1, 1, 1, 0, 704, 100
29917, V, 1, 1, 1, 1, 0, 704, 100
29918, V, 1, 1, 1, 1, 0, 704, 100
29919, V, 1, 1, 1, 1, 0, 704, 100
29920, V, 1, 1, 1, 1, 0, 704, 100
29921, V, 1, 1, 1, 1, 0, 704, 100
29922, V, 1, 1, 1, 1, 0, 704, 100
29923, V, 1, 1, 1, 1, 0, 704, 100
29924, V, 1, 1, 1, 1, 0, 704, 100
29925, V, 1, 1, 1, 1, 0, 704, 100
29926, V, 1, 1, 1, 1, 0, 704, 100
29927, V, 1, 1, 1, 1, 0, 704, 100
29928, V, 1, 1, 1, 1, 0, 704, 100
29929, V, 1, 1, 1, 1, 0, 704, 100
29930, V, 1, 1, 1, 1, 0, 704, 100
29931, V, 1, 1, 1, 1, 0, 704, 100
29932, V, 1, 1, 1, 1, 0, 704, 100
29933, V, 1, 1, 1, 1, 0, 704, 100
29934, V, 1, 1, 1, 1, 0, 704, 100
29935, V, 1, 1, 1, 1, 0, 704, 100
29936, V, 1, 1, 1, 1, 0, 704, 100
29937, V, 1, 1, 1, 1, 0, 704, 100
29938, V, 1, 1, 1, 1, 0, 704, 100
29939, V, 1, 1, 1, 1, 0, 704, 100
29940, V, 1, 1, 1, 1, 0, 704, 100
29941, V, 1, 1, 1, 1, 0, 704, 100
29942, V, 1, 1, 1, 1, 0, 704, 100
29943, V, 1, 1, 1, 1, 0, 704, 100
29944, V, 1, 1, 1, 1, 0, 704, 100
29945, V, 1, 1, 1, 1, 0, 704, 100
29946, V, 1, 1, 1, 1, 0, 704, 100
29947, V, 1, 1, 1, 1, 0, 704, 100
29948, V, 1, 1, 1, 1, 0, 704, 100
29949, V, 1, 1, 1, 1, 0, 704, 100
29950, V, 1, 1, 1, 1, 0, 704, 100
29952, V, 1, 1, 1, 1, 0, 704, 100
29953, V, 1, 1, 1, 1, 0, 704, 100
29954, V, 1, 1, 1, 1, 0, 704, 100
29955, V, 1, 1, 1, 1, 0, 704, 100
29956, V, 1, 1, 1, 1, 0, 704, 100
29957, V, 1, 1, 1, 1, 0, 704, 100
29958, V, 1, 1, 1, 1, 0, 704, 100
29959, V, 1, 1, 1, 1, 0, 704, 100
29960, V, 1, 1, 1, 1, 0, 704, 100
29961, V, 1, 1, 1, 1, 0, 704, 100
29962, V, 1, 1, 1, 1, 0, 704, 100
29963, V, 1, 1, 1, 1, 0, 704, 100
29964, V, 1, 1, 1, 1, 0, 704, 100
29965, V, 1, 1, 1, 1, 0, 704, 100
29966, V, 1, 1, 1, 1, 0, 704, 100
29967, V, 1, 1, 1, 1, 0, 704, 100
29968, V, 1, 1, 1, 1, 0, 704, 100
29969, V, 1, 1, 1, 1, 0, 704, 100
29970, V, 1, 1, 1, 1, 0, 704, 100
29971, V, 1, 1, 1, 1, 0, 704, 100
29972, V, 1, 1, 1, 1, 0, 704, 100
29973, V, 1, 1, 1, 1, 0, 704, 100
29974, V, 1, 1, 1, 1, 0, 704, 100
29975, V, 1, 1, 1, 1, 0, 704, 100
29976, V, 1, 1, 1, 1, 0, 704, 100
29977, V, 1, 1, 1, 1, 0, 704, 100
29978, V, 1, 1, 1, 1, 0, 704, 100
29979, V, 1, 1, 1, 1, 0, 704, 100
29980, V, 1, 1, 1, 1, 0, 704, 100
29981, V, 1, 1, 1, 1, 0, 704, 100
29982, V, 1, 1, 1, 1, 0, 704, 100
29983, V, 1, 1, 1, 1, 0, 704, 100
29984, V, 1, 1, 1, 1, 0, 704, 100
29985, V, 1, 1, 1, 1, 0, 704, 100
29986, V, 1, 1, 1, 1, 0, 704, 100
29987, V, 1, 1, 1, 1, 0, 704, 100
29988, V, 1, 1, 1, 1, 0, 704, 100
29989, V, 1, 1, 1, 1, 0, 704, 100
29990, V, 1, 1, 1, 1, 0, 704, 100
29991, V, 1, 1, 1, 1, 0, 704, 100
29992, V, 1, 1, 1, 1, 0, 704, 100
29993, V, 1, 1, 1, 1, 0, 704, 100
29995, V, 1, 1, 1, 1, 0, 704, 100
29996, V, 1, 1, 1, 1, 0, 704, 100
29997, V, 1, 1, 1, 1, 0, 704, 100
29998, V, 1, 1, 1, 1, 0, 704, 100
29999, V, 1, 1, 1, 1, 0, 704, 100
30000, V, 1, 1, 1, 1, 0, 704, 100
30001, V, 1, 1, 1, 1, 0, 704, 100
30002, V, 1, 1, 1, 1, 0, 704, 100
30003, V, 1, 1, 1, 1, 0, 704, 100
30004, V, 1, 1, 1, 1, 0, 704, 100
30005, V, 1, 1, 1, 1, 0, 704, 100
30006, V, 1, 1, 1, 1, 0, 704, 100
30007, V, 1, 1, 1, 1, 0, 704, 100
30008, V, 1, 1, 1, 1, 0, 704, 100
30009, V, 1, 1, 1, 1, 0, 704, 100
30010, V, 1, 1, 1, 1, 0, 704, 100
30011, V, 1, 1, 1, 1, 0, 704, 100
30012, V, 1, 1, 1, 1, 0, 704, 100
30013, V, 1, 1, 1, 1, 0, 704, 100
30014, V, 1, 1, 1, 1, 0, 704, 100
30015, V, 1, 1, 1, 1, 0, 704, 100
30016, V, 1, 1, 1, 1, 0, 704, 100
30017, V, 1, 1, 1, 1, 0, 704, 100
30018, V, 1, 1, 1, 1, 0, 704, 100
30019, V, 1, 1, 1, 1, 0, 704, 100
30020, V, 1, 1, 1, 1, 0, 704, 100
30021, V, 1, 1, 1, 1, 0, 704, 100
30022, V, 1, 1, 1, 1, 0, 704, 100
30023, V, 1, 1, 1, 1, 0, 704, 100
30024, V, 1, 1, 1, 1, 0, 704, 100
30025, V, 1, 1, 1, 1, 0, 704, 100
30026, V, 1, 1, 1, 1, 0, 704, 100
30027, V, 1, 1, 1, 1, 0, 704, 100
30028, V, 1, 1, 1, 1, 0, 704, 100
30029, V, 1, 1, 1, 1, 0, 704, 100
30030, V, 1, 1, 1, 1, 0, 704, 100
30031, V, 1, 1, 1, 1, 0, 704, 100
30032, V, 1, 1, 1, 1, 0, 704, 100
30033, V, 1, 1, 1, 1, 0, 704, 100
30034, V, 1, 1, 1, 1, 0, 704, 100
30035, V, 1, 1, 1, 1, 0, 704, 100
30036, V, 1, 1, 1, 1, 0, 704, 100
30038, V, 1, 1, 1, 1, 0, 704, 100
30039, V, 1, 1, 1, 1, 0, 704, 100
30040, V, 1, 1, 1, 1, 0, 704, 100
30041, V, 1, 1, 1, 1, 0, 704, 100
30042, V, 1, 1, 1, 1, 0, 704, 100
30043, V, 1, 1, 1, 1, 0, 704, 100
30044, V, 1, 1, 1, 1, 0, 704, 100
30045, V, 1, 1, 1, 1, 0, 704, 100
30046, V, 1, 1, 1, 1, 0, 704, 100
30047, V, 1, 1, 1, 1, 0, 704, 100
30048, V, 1, 1, 1, 1, 0, 704, 100
30049, V, 1, 1, 1, 1, 0, 704, 100
30050, V, 1, 1, 1, 1, 0, 704, 100
30051, V, 1, 1, 1, 1, 0, 704, 100
30052, V, 1, 1, 1, 1, 0, 704, 100
30053, V, 1, 1, 1, 1, 0, 704, 100
30054, V, 1, 1, 1, 1, 0, 704, 100
30055, V, 1, 1, 1, 1, 0, 704, 100
30056, V, 1, 1, 1, 1, 0, 704, 100
30057, V, 1, 1, 1, 1, 0, 704, 100
30058, V, 1, 1, 1, 1, 0, 704, 100
30059, V, 1, 1, 1, 1, 0, 704, 100
30060, V, 1, 1, 1, 1, 0, 704, 100
30061, V, 1, 1, 1, 1, 0, 704, 100
30062, V, 1, 1, 1, 1, 0, 704, 100
30063, V, 1, 1, 1, 1, 0, 704, 100
30064, V, 1, 1, 1, 1, 0, 704, 100
30065, V, 1, 1, 1, 1, 0, 704, 100
30066, V, 1, 1, 1, 1, 0, 704, 100
30067, V, 1, 1, 1, 1, 0, 704, 100
30068, V, 1, 1, 1, 1, 0, 704, 100
30069, V, 1, 1, 1, 1, 0, 704, 100
30070, V, 1, 1, 1, 1, 0, 704, 100
30071, V, 1, 1, 1, 1, 0, 704, 100
30072, V, 1, 1, 1, 1, 0, 704, 100
30073, V, 1, 1, 1, 1, 0, 704, 100
30074, V, 1, 1, 1, 1, 0, 704, 100
30075, V, 1, 1, 1, 1, 0, 704, 100
30076, V, 1, 1, 1, 1, 0, 704, 100
30077, V, 1, 1, 1, 1, 0, 704, 100
30078, V, 1, 1, 1, 1, 0, 704, 100
30080, V, 1, 1, 1, 1, 0, 704, 100
30081, V, 1, 1, 1, 1, 0, 704, 100
30082, V, 1, 1, 1, 1, 0, 704, 100
30083, V, 1, 1, 1, 1, 0, 704, 100
30084, V, 1, 1, 1, 1, 0, 704, 100
30085, V, 1, 1, 1, 1, 0, 704, 100
30086, V, 1, 1, 1, 1, 0, 704, 100
30087, V, 1, 1, 1, 1, 0, 704, 100
30088, V, 1, 1, 1, 1, 0, 704, 100
30089, V, 1, 1, 1, 1, 0, 704, 100
30090, V, 1, 1, 1, 1, 0, 704, 100
30091, V, 1, 1, 1, 1, 0, 704, 100
30092, V, 1, 1, 1, 1, 0, 704, 100
30093, V, 1, 1, 1, 1, 0, 704, 100
30094, V, 1, 1, 1, 1, 0, 704, 100
30095, V, 1, 1, 1, 1, 0, 704, 100
30096, V, 1, 1, 1, 1, 0, 704, 100
30097, V, 1, 1, 1, 1, 0, 704, 100
30098, V, 1, 1, 1, 1, 0, 704, 100
30099, V, 1, 1, 1, 1, 0, 704, 100
30100, V, 1, 1, 1, 1, 0, 704, 100
30101, V, 1, 1, 1, 1, 0, 704, 100
30102, V, 1, 1, 1, 1, 0, 704, 100
30103, V, 1, 1, 1, 1, 0, 704, 100
30104, V, 1, 1, 1, 1, 0, 704, 100
30105, V, 1, 1, 1, 1, 0, 704, 100
30106, V, 1, 1, 1, 1, 0, 704, 100
30107, V, 1, 1, 1, 1, 0, 704, 100
30108, V, 1, 1, 1, 1, 0, 704, 100
30109, V, 1, 1, 1, 1, 0, 704, 100
30110, V, 1, 1, 1, 1, 0, 704, 100
30111, V, 1, 1, 1, 1, 0, 704, 100
30112, V, 1, 1, 1, 1, 0, 704, 100
30113, V, 1, 1, 1, 1, 0, 704, 100
30114, V, 1, 1, 1, 1, 0, 704, 100
30115, V, 1, 1, 1, 1, 0, 704, 100
30116, V, 1, 1, 1, 1, 0, 704, 100
30117, V, 1, 1, 1, 1, 0, 704, 100
30118, V, 1, 1, 1, 1, 0, 704, 100
30119, V, 1, 1, 1, 1, 0, 704, 100
30120, V, 1, 1, 1, 1, 0, 704, 100
30121, V, 1, 1, 1, 1, 0, 704, 100
30123, V, 1, 1, 1, 1, 0, 704, 100
30124, V, 1, 1, 1, 1, 0, 704, 100
30125, V, 1, 1, 1, 1, 0, 704, 100
30126, V, 1, 1, 1, 1, 0, 704, 100
30127, V, 1, 1, 1, 1, 0, 704, 100
30128, V, 1, 1, 1, 1, 0, 704, 100
30129, V, 1, 1, 1, 1, 0, 704, 100
30130, V, 1, 1, 1, 1, 0, 704, 100
30131, V, 1, 1, 1, 1, 0, 704, 100
30132, V, 1, 1, 1, 1, 0, 704, 100
30133, V, 1, 1, 1, 1, 0, 704, 100
30134, V, 1, 1, 1, 1, 0, 704, 100
30135, V, 1, 1, 1, 1, 0, 704, 100
30136, V, 1, 1, 1, 1, 0, 704, 100
30137, V, 1, 1, 1, 1, 0, 704, 100
30138, V, 1, 1, 1, 1, 0, 704, 100
30139, V, 1, 1, 1, 1, 0, 704, 100
30140, V, 1, 1, 1, 1, 0, 704, 100
30141, V, 1, 1, 1, 1, 0, 704, 100
30142, V, 1, 1, 1, 1, 0, 704, 100
30143, V, 1, 1, 1, 1, 0, 704, 100
30144, V, 1, 1, 1, 1, 0, 704, 100
30145, V, 1, 1, 1, 1, 0, 704, 100
30146, V, 1, 1, 1, 1, 0, 704, 100
30147, V, 1, 1, 1, 1, 0, 704, 100
30148, V, 1, 1, 1, 1, 0, 704, 100
30149, V, 1, 1, 1, 1, 0, 704, 100
30150, V, 1, 1, 1, 1, 0, 704, 100
30151, V, 1, 1, 1, 1, 0, 704, 100
30152, V, 1, 1, 1, 1, 0, 704, 100
30153, V, 1, 1, 1, 1, 0, 704, 100
30154, V, 1, 1, 1, 1, 0, 704, 100
30155, V, 1, 1, 1, 1, 0, 704, 100
30156, V, 1, 1, 1, 1, 0, 704, 100
30157, V, 1, 1, 1, 1, 0, 704, 100
30158, V, 1, 1, 1, 1, 0, 704, 100
30159, V, 1, 1, 1, 1, 0, 704, 100
30160, V, 1, 1, 1, 1, 0, 704, 100
30161, V, 1, 1, 1, 1, 0, 704, 100
30162, V, 1, 1, 1, 1, 0, 704, 100
30163, V, 1, 1, 1, 1, 0, 704, 100
30164, V, 1, 1, 1, 1, 0, 704, 100
30166, V, 1, 1, 1, 1, 0, 704, 100
30167, V, 1, 1, 1, 1, 0, 704, 100
30168, V, 1, 1, 1, 1, 0, 704, 100
30169, V, 1, 1, 1, 1, 0, 704, 100
30170, V, 1, 1, 1, 1, 0, 704, 100
30171, V, 1, 1, 1, 1, 0, 704, 100
30172, V, 1, 1, 1, 1, 0, 704, 100
30173, V, 1, 1, 1, 1, 0, 704, 100
30174, V, 1, 1, 1, 1, 0, 704, 100
30175, V, 1, 1, 1, 1, 0, 704, 100
30176, V, 1, 1, 1, 1, 0, 704, 100
30177, V, 1, 1, 1, 1, 0, 704, 100
30178, V, 1, 1, 1, 1, 0, 704, 100
30179, V, 1, 1, 1, 1, 0, 704, 100
30180, V, 1, 1, 1, 1, 0, 704, 100
30181, V, 1, 1, 1, 1, 0, 704, 100
30182, V, 1, 1, 1, 1, 0, 704, 100
30183, V, 1, 1, 1, 1, 0, 704, 100
30184, V, 1, 1, 1, 1, 0, 704, 100
30185, V, 1, 1, 1, 1, 0, 704, 100
30186, V, 1, 1, 1, 1, 0, 704, 100
30187, V, 1, 1, 1, 1, 0, 704, 100
30188, V, 1, 1, 1, 1, 0, 704, 100
30189, V, 1, 1, 1, 1, 0, 704, 100
30190, V, 1, 1, 1, 1, 0, 704, 100
30191, V, 1, 1, 1, 1, 0, 704, 100
30192, V, 1, 1, 1, 1, 0, 704, 100
30193, V, 1, 1, 1, 1, 0, 704, 100
30194, V, 1, 1, 1, 1, 0, 704, 100
30195, V, 1, 1, 1, 1, 0, 704, 100
30196, V, 1, 1, 1, 1, 0, 704, 100
30197, V, 1, 1, 1, 1, 0, 704, 100
30198, V, 1, 1, 1, 1, 0, 704, 100
30199, V, 1, 1, 1, 1, 0, 704, 100
30200, V, 1, 1, 1, 1, 0, 704, 100
30201, V, 1, 1, 1, 1, 0, 704, 100
30202, V, 1, 1, 1, 1, 0, 704, 100
30203, V, 1, 1, 1, 1, 0, 704, 100
30204, V, 1, 1, 1, 1, 0, 704, 100
30205, V, 1, 1, 1, 1, 0, 704, 100
30206, V, 1, 1, 1, 1, 0, 704, 100
30208, V, 1, 1, 1, 1, 0, 704, 100
30209, V, 1, 1, 1, 1, 0, 704, 100
30210, V, 1, 1, 1, 1, 0, 704, 100
30211, V, 1, 1, 1, 1, 0, 704, 100
30212, V, 1, 1, 1, 1, 0, 704, 100
30213, V, 1, 1, 1, 1, 0, 704, 100
30214, V, 1, 1, 1, 1, 0, 704, 100
30215, V, 1, 1, 1, 1, 0, 704, 100
30216, V, 1, 1, 1, 1, 0, 704, 100
30217, V, 1, 1, 1, 1, 0, 704, 100
30218, V, 1, 1, 1, 1, 0, 704, 100
30219, V, 1, 1, 1, 1, 0, 704, 100
30220, V, 1, 1, 1, 1, 0, 704, 100
30221, V, 1, 1, 1, 1, 0, 704, 100
30222, V, 1, 1, 1, 1, 0, 704, 100
30223, V, 1, 1, 1, 1, 0, 704, 100
30224, V, 1, 1, 1, 1, 0, 704, 100
30225, V, 1, 1, 1, 1, 0, 704, 100
30226, V, 1, 1, 1, 1, 0, 704, 100
30227, V, 1, 1, 1, 1, 0, 704, 100
30228, V, 1, 1, 1, 1, 0, 704, 100
30229, V, 1, 1, 1, 1, 0, 704, 100
30230, V, 1, 1, 1, 1, 0, 704, 100
30231, V, 1, 1, 1, 1, 0, 704, 100
30232, V, 1, 1, 1, 1, 0, 704, 100
30233, V, 1, 1, 1, 1, 0, 704, 100
30234, V, 1, 1, 1, 1, 0, 704, 100
30235, V, 1, 1, 1, 1, 0, 704, 100
30236, V, 1, 1, 1, 1, 0, 704, 100
30237, V, 1, 1, 1, 1, 0, 704, 100
30238, V, 1, 1, 1, 1, 0, 704, 100
30239, V, 1, 1, 1, 1, 0, 704, 100
30240, V, 1, 1, 1, 1, 0, 704, 100
30241, V, 1, 1, 1, 1, 0, 704, 100
30242, V, 1, 1, 1, 1, 0, 704, 100
30243, V, 1, 1, 1, 1, 0, 704, 100
30244, V, 1, 1, 1, 1, 0, 704, 100
30245, V, 1, 1, 1, 1, 0, 704, 100
30246, V, 1, 1, 1, 1, 0, 704, 100
30247, V, 1, 1, 1, 1, 0, 704, 100
30248, V, 1, 1, 1, 1, 0, 704, 100
30249, V, 1, 1, 1, 1, 0, 704, 100
30251, V, 1, 1, 1, 1, 0, 704, 100
30252, V, 1, 1, 1, 1, 0, 704, 100
30253, V, 1, 1, 1, 1, 0, 704, 100
30254, V, 1, 1, 1, 1, 0, 704, 100
30255, V, 1, 1, 1, 1, 0, 704, 100
30256, V, 1, 1, 1, 1, 0, 704, 100
30257, V, 1, 1, 1, 1, 0, 704, 100
30258, V, 1, 1, 1, 1, 0, 704, 100
30259, V, 1, 1, 1, 1, 0, 704, 100
30260, V, 1, 1, 1, 1, 0, 704, 100
30261, V, 1, 1, 1, 1, 0, 704, 100
30262, V, 1, 1, 1, 1, 0, 704, 100
30263, V, 1, 1, 1, 1, 0, 704, 100
30264, V, 1, 1, 1, 1, 0, 704, 100
30265, V, 1, 1, 1, 1, 0, 704, 100
30266, V, 1, 1, 1, 1, 0, 704, 100
30267, V, 1, 1, 1, 1, 0, 704, 100
30268, V, 1, 1, 1, 1, 0, 704, 100
30269, V, 1, 1, 1, 1, 0, 704, 100
30270, V, 1, 1, 1, 1, 0, 704, 100
30271, V, 1, 1, 1, 1, 0, 704, 100
30272, V, 1, 1, 1, 1, 0, 704, 100
30273, V, 1, 1, 1, 1, 0, 704, 100
30274, V, 1, 1, 1, 1, 0, 704, 100
30275, V, 1, 1, 1, 1, 0, 704, 100
30276, V, 1, 1, 1, 1, 0, 704, 100
30277, V, 1, 1, 1, 1, 0, 704, 100
30278, V, 1, 1, 1, 1, 0, 704, 100
30279, V, 1, 1, 1, 1, 0, 704, 100
30280, V, 1, 1, 1, 1, 0, 704, 100
30281, V, 1, 1, 1, 1, 0, 704, 100
30282, V, 1, 1, 1, 1, 0, 704, 100
30283, V, 1, 1, 1, 1, 0, 704, 100
30284, V, 1, 1, 1, 1, 0, 704, 100
30285, V, 1, 1, 1, 1, 0, 704, 100
30286, V, 1, 1, 1, 1, 0, 704, 100
30287, V, 1, 1, 1, 1, 0, 704, 100
30288, V, 1, 1, 1, 1, 0, 704, 100
30289, V, 1, 1, 1, 1, 0, 704, 100
30290, V, 1, 1, 1, 1, 0, 704, 100
30291, V, 1, 1, 1, 1, 0, 704, 100
30292, V, 1, 0, 0, 1, 0, 704, 100
30292, V, 1, 0, 0, 0, 0, 704, 100
30294, V, 1, 1, 0, 0, 0, 704, 100
30294, V, 1, 1, 0, 0, 0, 704, 100
30295, V, 1, 1, 1, 1, 0, 704, 100
30296, V, 1, 1, 1, 1, 0, 704, 100
30297, V, 1, 1, 1, 1, 0, 704, 100
30298, V, 1, 1, 1, 1, 0, 704, 100
30299, V, 1, 1, 1, 1, 0, 704, 100
30300, V, 1, 1, 1, 1, 0, 704, 100
30301, V, 1, 1, 1, 1, 0, 704, 100
30302, V, 1, 1, 1, 1, 0, 704, 99
30303, V, 1, 1, 1, 1, 0, 704, 99
30304, V, 1, 1, 1, 1, 0, 704, 99
30305, V, 1, 1, 1, 1, 0, 704, 99
30306, V, 1, 1, 1, 1, 0, 704, 99
30307, V, 1, 1, 1, 1, 0, 704, 100
30308, V, 1, 1, 1, 1, 0, 704, 100
30309, V, 1, 1, 1, 1, 0, 704, 100
30310, V, 1, 1, 1, 1, 0, 704, 100
30311, V, 1, 1, 1, 1, 0, 704, 100
30312, V, 1, 1, 1, 1, 0, 704, 100
30313, V, 1, 1, 1, 1, 0, 704, 100
30314, V, 1, 1, 1, 1, 0, 704, 100
30315, V, 1, 1, 1, 1, 0, 704, 100
30316, V, 1, 1, 1, 1, 0, 704, 100
30317, V, 1, 1, 1, 1, 0, 704, 100
30318, V, 1, 1, 1, 1, 0, 704, 100
30319, V, 1, 1, 1, 1, 0, 704, 100
30320, V, 1, 1, 1, 1, 0, 704, 100
30321, V, 1, 1, 1, 1, 0, 704, 100
30322, V, 1, 1, 1, 1, 0, 704, 100
30323, V, 1, 1, 1, 1, 0, 704, 100
30324, V, 1, 1, 1, 1, 0, 704, 100
30325, V, 1, 1, 1, 1, 0, 704, 100
30326, V, 1, 1, 1, 1, 0, 704, 100
30327, V, 1, 1, 1, 1, 0, 704, 100
30328, V, 1, 1, 1, 1, 0, 704, 100
30329, V, 1, 1, 1, 1, 0, 704, 100
30330, V, 1, 1, 1, 1, 0, 704, 100
30331, V, 1, 1, 1, 1, 0, 704, 100
30332, V, 1, 1, 1, 1, 0, 704, 100
30333, V, 1, 1, 1, 1, 0, 704, 100
30334, V, 1, 1, 1, 1, 0, 704, 100
30336, V, 1, 1, 1, 1, 0, 704, 100
30337, V, 1, 1, 1, 1, 0, 704, 100
30338, V, 1, 1, 1, 1, 0, 704, 100
30339, V, 1, 1, 1, 1, 0, 704, 100
30340, V, 1, 1, 1, 1, 0, 704, 100
30341, V, 1, 1, 1, 1, 0, 704, 100
30342, V, 1, 1, 1, 1, 0, 704, 100
30343, V, 1, 1, 1, 1, 0, 704, 100
30344, V, 1, 1, 1, 1, 0, 704, 100
30345, V, 1, 1, 1, 1, 0, 704, 100
30346, V, 1, 1, 1, 1, 0, 704, 100
30347, V, 1, 1, 1, 1, 0, 704, 100
30348, V, 1, 1, 1, 1, 0, 704, 100
30349, V, 1, 1, 1, 1, 0, 704, 100
30350, V, 1, 1, 1, 1, 0, 704, 100
30351, V, 1, 1, 1, 1, 0, 704, 100
30352, V, 1, 1, 1, 1, 0, 704, 100
30353, V, 1, 1, 1, 1, 0, 704, 100
30354, V, 1, 1, 1, 1, 0, 704, 100
30355, V, 1, 1, 1, 1, 0, 704, 100
30356, V, 1, 1, 1, 1, 0, 704, 100
30357, V, 1, 1, 1, 1, 0, 704, 100
30358, V, 1, 1, 1, 1, 0, 704, 100
30359, V, 1, 1, 1, 1, 0, 704, 100
30360, V, 1, 1, 1, 1, 0, 704, 100
30361, V, 1, 1, 1, 1, 0, 704, 100
30362, V, 1, 1, 1, 1, 0, 704, 100
30363, V, 1, 1, 1, 1, 0, 704, 100
30364, V, 1, 1, 1, 1, 0, 704, 100
30365, V, 1, 1, 1, 1, 0, 704, 100
30366, V, 1, 1, 1, 1, 0, 704, 100
30367, V, 1, 1, 1, 1, 0, 704, 100
30368, V, 1, 1, 1, 1, 0, 704, 100
30369, V, 1, 1, 1, 1, 0, 704, 100
30370, V, 1, 1, 1, 1, 0, 704, 100
30371, V, 1, 1, 1, 1, 0, 704, 100
30372, V, 1, 1, 1, 1, 0, 704, 100
30373, V, 1, 1, 1, 1, 0, 704, 100
30374, V, 1, 1, 1, 1, 0, 704, 100
30375, V, 1, 1, 1, 1, 0, 704, 100
30376, V, 1, 1, 1, 1, 0, 704, 100
30377, V, 1, 1, 1, 1, 0, 704, 100
30379, V, 1, 1, 1, 1, 0, 704, 100
30380, V, 1, 1, 1, 1, 0, 704, 100
30381, V, 1, 1, 1, 1, 0, 704, 100
30382, V, 1, 1, 1, 1, 0, 704, 100
30383, V, 1, 1, 1, 1, 0, 704, 100
30384, V, 1, 1, 1, 1, 0, 704, 100
30385, V, 1, 1, 1, 1, 0, 704, 100
30386, V, 1, 1, 1, 1, 0, 704, 100
30387, V, 1, 1, 1, 1, 0, 704, 100
30388, V, 1, 1, 1, 1, 0, 704, 100
30389, V, 1, 1, 1, 1, 0, 704, 100
30390, V, 1, 1, 1, 1, 0, 704, 100
30391, V, 1, 1, 1, 1, 0, 704, 100
30392, V, 1, 1, 1, 1, 0, 704, 100
30393, V, 1, 1, 1, 1, 0, 704, 100
30394, V, 1, 1, 1, 1, 0, 704, 100
30395, V, 1, 1, 1, 1, 0, 704, 100
30396, V, 1, 1, 1, 1, 0, 704, 100
30397, V, 1, 1, 1, 1, 0, 704, 100
30398, V, 1, 1, 1, 1, 0, 704, 100
30399, V, 1, 1, 1, 1, 0, 704, 100
30400, V, 1, 1, 1, 1, 0, 704, 100
30401, V, 1, 1, 1, 1, 0, 704, 100
30402, V, 1, 1, 1, 1, 0, 704, 100
30403, V, 1, 1, 1, 1, 0, 704, 100
30404, V, 1, 1, 1, 1, 0, 704, 100
30405, V, 1, 1, 1, 1, 0, 704, 100
30406, V, 1, 1, 1, 1, 0, 704, 100
30407, V, 1, 1, 1, 1, 0, 704, 100
30408, V, 1, 1, 1, 1, 0, 704, 100
30409, V, 1, 1, 1, 1, 0, 704, 100
30410, V, 1, 1, 1, 1, 0, 704, 100
30411, V, 1, 1, 1, 1, 0, 704, 100
30412, V, 1, 1, 1, 1, 0, 704, 100
30413, V, 1, 1, 1, 1, 0, 704, 100
30414, V, 1, 1, 1, 1, 0, 704, 100
30415, V, 1, 1, 1, 1, 0, 704, 100
30416, V, 1, 1, 1, 1, 0, 704, 100
30417, V, 1, 1, 1, 1, 0, 704, 100
30418, V, 1, 1, 1, 1, 0, 704, 100
30419, V, 1, 1, 1, 1, 0, 704, 100
30420, V, 1, 1, 1, 1, 0, 704, 100
30422, V, 1, 1, 1, 1, 0, 704, 100
30423, V, 1, 1, 1, 1, 0, 704, 100
30424, V, 1, 1, 1, 1, 0, 704, 100
30425, V, 1, 1, 1, 1, 0, 704, 100
30426, V, 1, 1, 1, 1, 0, 704, 100
30427, V, 1, 1, 1, 1, 0, 704, 100
30428, V, 1, 1, 1, 1, 0, 704, 100
30429, V, 1, 1, 1, 1, 0, 704, 100
30430, V, 1, 1, 1, 1, 0, 704, 100
30431, V, 1, 1, 1, 1, 0, 704, 100
30432, V, 1, 1, 1, 1, 0, 704, 100
30433, V, 1, 1, 1, 1, 0, 704, 100
30434, V, 1, 1, 1, 1, 0, 704, 100
30435, V, 1, 1, 1, 1, 0, 704, 100
30436, V, 1, 1, 1, 1, 0, 704, 100
30437, V, 1, 1, 1, 1, 0, 704, 100
30438, V, 1, 1, 1, 1, 0, 704, 100
30439, V, 1, 1, 1, 1, 0, 704, 100
30440, V, 1, 1, 1, 1, 0, 704, 100
30441, V, 1, 1, 1, 1, 0, 704, 100
30442, V, 1, 1, 1, 1, 0, 704, 100
30443, V, 1, 1, 1, 1, 0, 704, 100
30444, V, 1, 1, 1, 1, 0, 704, 100
30445, V, 1, 1, 1, 1, 0, 704, 100
30446, V, 1, 1, 1, 1, 0, 704, 100
30447, V, 1, 1, 1, 1, 0, 704, 100
30448, V, 1, 1, 1, 1, 0, 704, 100
30449, V, 1, 1, 1, 1, 0, 704, 100
30450, V, 1, 1, 1, 1, 0, 704, 100
30451, V, 1, 1, 1, 1, 0, 704, 100
30452, V, 1, 1, 1, 1, 0, 704, 100
30453, V, 1, 1, 1, 1, 0, 704, 100
30454, V, 1, 1, 1, 1, 0, 704, 100
30455, V, 1, 1, 1, 1, 0, 704, 100
30456, V, 1, 1, 1, 1, 0, 704, 100
30457, V, 1, 1, 1, 1, 0, 704, 100
30458, V, 1, 1, 1, 1, 0, 704, 100
30459, V, 1, 1, 1, 1, 0, 704, 100
30460, V, 1, 1, 1, 1, 0, 704, 100
30461, V, 1, 1, 1, 1, 0, 704, 100
30462, V, 1, 1, 1, 1, 0, 704, 100
30464, V, 1, 1, 1, 1, 0, 704, 100
30465, V, 1, 1, 1, 1, 0, 704, 100
30466, V, 1, 1, 1, 1, 0, 704, 100
30467, V, 1, 1, 1, 1, 0, 704, 100
30468, V, 1, 0, 0, 1, 0, 704, 100
30468, V, 1, 0, 0, 0, 0, 704, 100
30469, V, 1, 1, 0, 0, 0, 704, 100
30469, V, 1, 1, 0, 0, 0, 704, 100
30470, V, 1, 1, 1, 1, 0, 704, 100
30471, V, 1, 1, 1, 1, 0, 704, 100
30472, V, 1, 1, 1, 1, 0, 704, 100
30473, V, 1, 1, 1, 1, 0, 704, 100
30474, V, 1, 1, 1, 1, 0, 704, 100
30475, V, 1, 1, 1, 1, 0, 704, 100
30476, V, 1, 1, 1, 1, 0, 704, 100
30477, V, 1, 1, 1, 1, 0, 704, 99
30478, V, 1, 1, 1, 1, 0, 704, 99
30479, V, 1, 1, 1, 1, 0, 704, 100
30480, V, 1, 1, 1, 1, 0, 704, 100
30481, V, 1, 1, 1, 1, 0, 704, 100
30482, V, 1, 1, 1, 1, 0, 704, 100
30483, V, 1, 1, 1, 1, 0, 704, 100
30484, V, 1, 1, 1, 1, 0, 704, 100
30485, V, 1, 1, 1, 1, 0, 704, 100
30486, V, 1, 1, 1, 1, 0, 704, 100
30487, V, 1, 1, 1, 1, 0, 704, 100
30488, V, 1, 1, 1, 1, 0, 704, 100
30489, V, 1, 1, 1, 1, 0, 704, 100
30490, V, 1, 1, 1, 1, 0, 704, 100
30491, V, 1, 1, 1, 1, 0, 704, 100
30492, V, 1, 1, 1, 1, 0, 704, 100
30493, V, 1, 1, 1, 1, 0, 704, 100
30494, V, 1, 1, 1, 1, 0, 704, 100
30495, V, 1, 1, 1, 1, 0, 704, 100
30496, V, 1, 1, 1, 1, 0, 704, 100
30497, V, 1, 1, 1, 1, 0, 704, 100
30498, V, 1, 1, 1, 1, 0, 704, 100
30499, V, 1, 1, 1, 1, 0, 704, 100
30500, V, 1, 1, 1, 1, 0, 704, 100
30501, V, 1, 1, 1, 1, 0, 704, 100
30502, V, 1, 1, 1, 1, 0, 704, 100
30503, V, 1, 1, 1, 1, 0, 704, 100
30504, V, 1, 1, 1, 1, 0, 704, 100
30505, V, 1, 1, 1, 1, 0, 704, 100
30507, V, 1, 1, 1, 1, 0, 704, 100
30508, V, 1, 1, 1, 1, 0, 704, 100
30509, V, 1, 1, 1, 1, 0, 704, 100
30510, V, 1, 1, 1, 1, 0, 704, 100
30511, V, 1, 1, 1, 1, 0, 704, 100
30512, V, 1, 1, 1, 1, 0, 704, 100
30513, V, 1, 1, 1, 1, 0, 704, 100
30514, V, 1, 1, 1, 1, 0, 704, 100
30515, V, 1, 1, 1, 1, 0, 704, 100
30516, V, 1, 1, 1, 1, 0, 704, 100
30517, V, 1, 1, 1, 1, 0, 704, 100
30518, V, 1, 1, 1, 1, 0, 704, 100
30519, V, 1, 1, 1, 1, 0, 704, 100
30520, V, 1, 1, 1, 1, 0, 704, 100
30521, V, 1, 1, 1, 1, 0, 704, 100
30522, V, 1, 1, 1, 1, 0, 704, 100
30523, V, 1, 1, 1, 1, 0, 704, 100
30524, V, 1, 1, 1, 1, 0, 704, 100
30525, V, 1, 1, 1, 1, 0, 704, 100
30526, V, 1, 1, 1, 1, 0, 704, 100
30527, V, 1, 1, 1, 1, 0, 704, 100
30528, V, 1, 1, 1, 1, 0, 704, 100
30529, V, 1, 1, 1, 1, 0, 704, 100
30530, V, 1, 1, 1, 1, 0, 704, 100
30531, V, 1, 1, 1, 1, 0, 704, 100
30532, V, 1, 1, 1, 1, 0, 704, 100
30533, V, 1, 1, 1, 1, 0, 704, 100
30534, V, 1, 1, 1, 1, 0, 704, 100
30535, V, 1, 1, 1, 1, 0, 704, 100
30536, V, 1, 1, 1, 1, 0, 704, 100
30537, V, 1, 1, 1, 1, 0, 704, 100
30538, V, 1, 1, 1, 1, 0, 704, 100
30539, V, 1, 1, 1, 1, 0, 704, 100
30540, V, 1, 1, 1, 1, 0, 704, 100
30541, V, 1, 1, 1, 1, 0, 704, 100
30542, V, 1, 1, 1, 1, 0, 704, 100
30543, V, 1, 1, 1, 1, 0, 704, 100
30544, V, 1, 1, 1, 1, 0, 704, 100
30545, V, 1, 1, 1, 1, 0, 704, 100
30546, V, 1, 1, 1, 1, 0, 704, 100
30547, V, 1, 1, 1, 1, 0, 704, 100
30548, V, 1, 1, 1, 1, 0, 704, 100
30550, V, 1, 1, 1, 1, 0, 704, 100
30551, V, 1, 1, 1, 1, 0, 704, 100
30552, V, 1, 1, 1, 1, 0, 704, 100
30553, V, 1, 1, 1, 1, 0, 704, 100
30554, V, 1, 1, 1, 1, 0, 704, 100
30555, V, 1, 1, 1, 1, 0, 704, 100
30556, V, 1, 1, 1, 1, 0, 704, 100
30557, V, 1, 1, 1, 1, 0, 704, 100
30558, V, 1, 1, 1, 1, 0, 704, 100
30559, V, 1, 1, 1, 1, 0, 704, 100
30560, V, 1, 1, 1, 1, 0, 704, 100
30561, V, 1, 1, 1, 1, 0, 704, 100
30562, V, 1, 1, 1, 1, 0, 704, 100
30563, V, 1, 1, 1, 1, 0, 704, 100
30564, V, 1, 1, 1, 1, 0, 704, 100
30565, V, 1, 1, 1, 1, 0, 704, 100
30566, V, 1, 1, 1, 1, 0, 704, 100
30567, V, 1, 1, 1, 1, 0, 704, 100
30568, V, 1, 1, 1, 1, 0, 704, 100
30569, V, 1, 1, 1, 1, 0, 704, 100
30570, V, 1, 1, 1, 1, 0, 704, 100
30571, V, 1, 1, 1, 1, 0, 704, 100
30572, V, 1, 1, 1, 1, 0, 704, 100
30573, V, 1, 1, 1, 1, 0, 704, 100
30574, V, 1, 1, 1, 1, 0, 704, 100
30575, V, 1, 1, 1, 1, 0, 704, 100
30576, V, 1, 1, 1, 1, 0, 704, 100
30577, V, 1, 1, 1, 1, 0, 704, 100
30578, V, 1, 1, 1, 1, 0, 704, 100
30579, V, 1, 1, 1, 1, 0, 704, 100
30580, V, 1, 1, 1, 1, 0, 704, 100
30581, V, 1, 1, 1, 1, 0, 704, 100
30582, V, 1, 1, 1, 1, 0, 704, 100
30583, V, 1, 1, 1, 1, 0, 704, 100
30584, V, 1, 1, 1, 1, 0, 704, 100
30585, V, 1, 1, 1, 1, 0, 704, 100
30586, V, 1, 1, 1, 1, 0, 704, 100
30587, V, 1, 1, 1, 1, 0, 704, 100
30588, V, 1, 1, 1, 1, 0, 704, 100
30589, V, 1, 1, 1, 1, 0, 704, 100
30590, V, 1, 1, 1, 1, 0, 704, 100
30592, V, 1, 1, 1, 1, 0, 704, 100
30593, V, 1, 1, 1, 1, 0, 704, 100
30594, V, 1, 1, 1, 1, 0, 704, 100
30595, V, 1, 1, 1, 1, 0, 704, 100
30596, V, 1, 1, 1, 1, 0, 704, 100
30597, V, 1, 1, 1, 1, 0, 704, 100
30598, V, 1, 1, 1, 1, 0, 704, 100
30599, V, 1, 1, 1, 1, 0, 704, 100
30600, V, 1, 1, 1, 1, 0, 704, 100
30601, V, 1, 1, 1, 1, 0, 704, 100
30602, V, 1, 1, 1, 1, 0, 704, 100
30603, V, 1, 1, 1, 1, 0, 704, 100
30604, V, 1, 1, 1, 1, 0, 704, 100
30605, V, 1, 1, 1, 1, 0, 704, 100
30606, V, 1, 1, 1, 1, 0, 704, 100
30607, V, 1, 1, 1, 1, 0, 704, 100
30608, V, 1, 1, 1, 1, 0, 704, 100
30609, V, 1, 1, 1, 1, 0, 704, 100
30610, V, 1, 1, 1, 1, 0, 704, 100
30611, V, 1, 1, 1, 1, 0, 704, 100
30612, V, 1, 1, 1, 1, 0, 704, 100
30613, V, 1, 1, 1, 1, 0, 704, 100
30614, V, 1, 1, 1, 1, 0, 704, 100
30615, V, 1, 1, 1, 1, 0, 704, 100
30616, V, 1, 1, 1, 1, 0, 704, 100
30617, V, 1, 1, 1, 1, 0, 704, 100
30618, V, 1, 1, 1, 1, 0, 704, 100
30619, V, 1, 1, 1, 1, 0, 704, 100
30620, V, 1, 1, 1, 1, 0, 704, 100
30621, V, 1, 1, 1, 1, 0, 704, 100
30622, V, 1, 1, 1, 1, 0, 704, 100
30623, V, 1, 1, 1, 1, 0, 704, 100
30624, V, 1, 1, 1, 1, 0, 704, 100
30625, V, 1, 1, 1, 1, 0, 704, 100
30626, V, 1, 1, 1, 1, 0, 704, 100
30627, V, 1, 1, 1, 1, 0, 704, 100
30628, V, 1, 1, 1, 1, 0, 704, 100
30629, V, 1, 1, 1, 1, 0, 704, 100
30630, V, 1, 1, 1, 1, 0, 704, 100
30631, V, 1, 1, 1, 1, 0, 704, 100
30632, V, 1, 1, 1, 1, 0, 704, 100
30633, V, 1, 1, 1, 1, 0, 704, 100
30635, V, 1, 1, 1, 1, 0, 704, 100
30636, V, 1, 1, 1, 1, 0, 704, 100
30637, V, 1, 1, 1, 1, 0, 704, 100
30638, V, 1, 1, 1, 1, 0, 704, 100
30639, V, 1, 1, 1, 1, 0, 704, 100
30640, V, 1, 1, 1, 1, 0, 704, 100
30641, V, 1, 1, 1, 1, 0, 704, 100
30642, V, 1, 1, 1, 1, 0, 704, 100
30643, V, 1, 1, 1, 1, 0, 704, 100
30644, V, 1, 1, 1, 1, 0, 704, 100
30645, V, 1, 1, 1, 1, 0, 704, 100
30646, V, 1, 1, 1, 1, 0, 704, 100
30647, V, 1, 1, 1, 1, 0, 704, 100
30648, V, 1, 1, 1, 1, 0, 704, 100
30649, V, 1, 1, 1, 1, 0, 704, 100
30650, V, 1, 1, 1, 1, 0, 704, 100
30651, V, 1, 1, 1, 1, 0, 704, 100
30652, V, 1, 1, 1, 1, 0, 704, 100
30653, V, 1, 1, 1, 1, 0, 704, 100
30654, V, 1, 1, 1, 1, 0, 704, 100
30655, V, 1, 1, 1, 1, 0, 704, 100
30656, V, 1, 1, 1, 1, 0, 704, 100
30657, V, 1, 1, 1, 1, 0, 704, 100
30658, V, 1, 1, 1, 1, 0, 704, 100
30659, V, 1, 1, 1, 1, 0, 704, 100
30660, V, 1, 1, 1, 1, 0, 704, 100
30661, V, 1, 1, 1, 1, 0, 704, 100
30662, V, 1, 1, 1, 1, 0, 704, 100
30663, V, 1, 1, 1, 1, 0, 704, 100
30664, V, 1, 1, 1, 1, 0, 704, 100
30665, V, 1, 1, 1, 1, 0, 704, 100
30666, V, 1, 1, 1, 1, 0, 704, 100
30667, V, 1, 1, 1, 1, 0, 704, 100
30668, V, 1, 1, 1, 1, 0, 704, 100
30669, V, 1, 1, 1, 1, 0, 704, 100
30670, V, 1, 1, 1, 1, 0, 704, 100
30671, V, 1, 1, 1, 1, 0, 704, 100
30672, V, 1, 1, 1, 1, 0, 704, 100
30673, V, 1, 1, 1, 1, 0, 704, 100
30674, V, 1, 1, 1, 1, 0, 704, 100
30675, V, 1, 1, 1, 1, 0, 704, 100
30676, V, 1, 1, 1, 1, 0, 704, 100
30678, V, 1, 1, 1, 1, 0, 704, 100
30679, V, 1, 1, 1, 1, 0, 704, 100
30680, V, 1, 1, 1, 1, 0, 704, 100
30681, V, 1, 1, 1, 1, 0, 704, 100
30682, V, 1, 1, 1, 1, 0, 704, 100
30683, V, 1, 1, 1, 1, 0, 704, 100
30684, V, 1, 1, 1, 1, 0, 704, 100
30685, V, 1, 1, 1, 1, 0, 704, 100
30686, V, 1, 1, 1, 1, 0, 704, 100
30687, V, 1, 1, 1, 1, 0, 704, 100
30688, V, 1, 1, 1, 1, 0, 704, 100
30689, V, 1, 1, 1, 1, 0, 704, 100
30690, V, 1, 1, 1, 1, 0, 704, 100
30691, V, 1, 1, 1, 1, 0, 704, 100
30692, V, 1, 1, 1, 1, 0, 704, 100
30693, V, 1, 1, 1, 1, 0, 704, 100
30694, V, 1, 1, 1, 1, 0, 704, 100
30695, V, 1, 1, 1, 1, 0, 704, 100
30696, V, 1, 1, 1, 1, 0, 704, 100
30697, V, 1, 1, 1, 1, 0, 704, 100
30698, V, 1, 1, 1, 1, 0, 704, 100
30699, V, 1, 1, 1, 1, 0, 704, 100
30700, V, 1, 1, 1, 1, 0, 704, 100
30701, V, 1, 1, 1, 1, 0, 704, 100
30702, V, 1, 1, 1, 1, 0, 704, 100
30703, V, 1, 1, 1, 1, 0, 704, 100
30704, V, 1, 1, 1, 1, 0, 704, 100
30705, V, 1, 1, 1, 1, 0, 704, 100
30706, V, 1, 1, 1, 1, 0, 704, 100
30707, V, 1, 1, 1, 1, 0, 704, 100
30708, V, 1, 1, 1, 1, 0, 704, 100
30709, V, 1, 1, 1, 1, 0, 704, 100
30710, V, 1, 1, 1, 1, 0, 704, 100
30711, V, 1, 1, 1, 1, 0, 704, 100
30712, V, 1, 1, 1, 1, 0, 704, 100
30713, V, 1, 1, 1, 1, 0, 704, 100
30714, V, 1, 1, 1, 1, 0, 704, 100
30715, V, 1, 1, 1, 1, 0, 704, 100
30716, V, 1, 1, 1, 1, 0, 704, 100
30717, V, 1, 1, 1, 1, 0, 704, 100
30718, V, 1, 1, 1, 1, 0, 704, 100
30720, V, 1, 1, 1, 1, 0, 704, 100
30721, V, 1, 1, 1, 1, 0, 704, 100
30722, V, 1, 1, 1, 1, 0, 704, 100
30723, V, 1, 1, 1, 1, 0, 704, 100
30724, V, 1, 1, 1, 1, 0, 704, 100
30725, V, 1, 1, 1, 1, 0, 704, 100
30726, V, 1, 1, 1, 1, 0, 704, 100
30727, V, 1, 1, 1, 1, 0, 704, 100
30728, V, 1, 1, 1, 1, 0, 704, 100
30729, V, 1, 1, 1, 1, 0, 704, 100
30730, V, 1, 1, 1, 1, 0, 704, 100
30731, V, 1, 1, 1, 1, 0, 704, 100
30732, V, 1, 1, 1, 1, 0, 704, 100
30733, V, 1, 1, 1, 1, 0, 704, 100
30734, V, 1, 1, 1, 1, 0, 704, 100
30735, V, 1, 1, 1, 1, 0, 704, 100
30736, V, 1, 1, 1, 1, 0, 704, 100
30737, V, 1, 1, 1, 1, 0, 704, 100
30738, V, 1, 1, 1, 1, 0, 704, 100
30739, V, 1, 1, 1, 1, 0, 704, 100
30740, V, 1, 1, 1, 1, 0, 704, 100
30741, V, 1, 1, 1, 1, 0, 704, 100
30742, V, 1, 1, 1, 1, 0, 704, 100
30743, V, 1, 1, 1, 1, 0, 704, 100
30744, V, 1, 1, 1, 1, 0, 704, 100
30745, V, 1, 1, 1, 1, 0, 704, 100
30746, V, 1, 1, 1, 1, 0, 704, 100
30747, V, 1, 1, 1, 1, 0, 704, 100
30748, V, 1, 1, 1, 1, 0, 704, 100
30749, V, 1, 1, 1, 1, 0, 704, 100
30750, V, 1, 1, 1, 1, 0, 704, 100
30751, V, 1, 1, 1, 1, 0, 704, 100
30752, V, 1, 1, 1, 1, 0, 704, 100
30753, V, 1, 1, 1, 1, 0, 704, 100
30754, V, 1, 1, 1, 1, 0, 704, 100
30755, V, 1, 1, 1, 1, 0, 704, 100
30756, V, 1, 1, 1, 1, 0, 704, 100
30757, V, 1, 1, 1, 1, 0, 704, 100
30758, V, 1, 1, 1, 1, 0, 704, 100
30759, V, 1, 1, 1, 1, 0, 704, 100
30760, V, 1, 1, 1, 1, 0, 704, 100
30761, V, 1, 1, 1, 1, 0, 704, 100
30763, V, 1, 1, 1, 1, 0, 704, 100
30764, V, 1, 1, 1, 1, 0, 704, 100
30765, V, 1, 1, 1, 1, 0, 704, 100
30766, V, 1, 1, 1, 1, 0, 704, 100
30767, V, 1, 1, 1, 1, 0, 704, 100
30768, V, 1, 1, 1, 1, 0, 704, 100
30769, V, 1, 1, 1, 1, 0, 704, 100
30770, V, 1, 1, 1, 1, 0, 704, 100
30771, V, 1, 1, 1, 1, 0, 704, 100
30772, V, 1, 1, 1, 1, 0, 704, 100
30773, V, 1, 1, 1, 1, 0, 704, 100
30774, V, 1, 1, 1, 1, 0, 704, 100
30775, V, 1, 1, 1, 1, 0, 704, 100
30776, V, 1, 1, 1, 1, 0, 704, 100
30777, V, 1, 1, 1, 1, 0, 704, 100
30778, V, 1, 1, 1, 1, 0, 704, 100
30779, V, 1, 1, 1, 1, 0, 704, 100
30780, V, 1, 1, 1, 1, 0, 704, 100
30781, V, 1, 1, 1, 1, 0, 704, 100
30782, V, 1, 1, 1, 1, 0, 704, 100
30783, V, 1, 1, 1, 1, 0, 704, 100
30784, V, 1, 1, 1, 1, 0, 704, 100
30785, V, 1, 1, 1, 1, 0, 704, 100
30786, V, 1, 1, 1, 1, 0, 704, 100
30787, V, 1, 1, 1, 1, 0, 704, 100
30788, V, 1, 1, 1, 1, 0, 704, 100
30789, V, 1, 1, 1, 1, 0, 704, 100
30790, V, 1, 1, 1, 1, 0, 704, 100
30791, V, 1, 1, 1, 1, 0, 704, 100
30792, V, 1, 1, 1, 1, 0, 704, 100
30793, V, 1, 1, 1, 1, 0, 704, 100
30794, V, 1, 1, 1, 1, 0, 704, 100
30795, V, 1, 1, 1, 1, 0, 704, 100
30796, V, 1, 1, 1, 1, 0, 704, 100
30797, V, 1, 1, 1, 1, 0, 704, 100
30798, V, 1, 1, 1, 1, 0, 704, 100
30799, V, 1, 1, 1, 1, 0, 704, 100
30800, V, 1, 1, 1, 1, 0, 704, 100
30801, V, 1, 1, 1, 1, 0, 704, 100
30802, V, 1, 1, 1, 1, 0, 704, 100
30803, V, 1, 1, 1, 1, 0, 704, 100
30804, V, 1, 1, 1, 1, 0, 704, 100
30806, V, 1, 1, 1, 1, 0, 704, 100
30807, V, 1, 1, 1, 1, 0, 704, 100
30808, V, 1, 1, 1, 1, 0, 704, 100
30809, V, 1, 1, 1, 1, 0, 704, 100
30810, V, 1, 1, 1, 1, 0, 704, 100
30811, V, 1, 1, 1, 1, 0, 704, 100
30812, V, 1, 1, 1, 1, 0, 704, 100
30813, V, 1, 1, 1, 1, 0, 704, 100
30814, V, 1, 1, 1, 1, 0, 704, 100
30815, V, 1, 1, 1, 1, 0, 704, 100
30816, V, 1, 1, 1, 1, 0, 704, 100
30817, V, 1, 1, 1, 1, 0, 704, 100
30818, V, 1, 1, 1, 1, 0, 704, 100
30819, V, 1, 1, 1, 1, 0, 704, 100
30820, V, 1, 1, 1, 1, 0, 704, 100
30821, V, 1, 1, 1, 1, 0, 704, 100
30822, V, 1, 1, 1, 1, 0, 704, 100
30823, V, 1, 1, 1, 1, 0, 704, 100
30824, V, 1, 1, 1, 1, 0, 704, 100
30825, V, 1, 1, 1, 1, 0, 704, 100
30826, V, 1, 1, 1, 1, 0, 704, 100
30827, V, 1, 1, 1, 1, 0, 704, 100
30828, V, 1, 1, 1, 1, 0, 704, 100
30829, V, 1, 1, 1, 1, 0, 704, 100
30830, V, 1, 1, 1, 1, 0, 704, 100
30831, V, 1, 1, 1, 1, 0, 704, 100
30832, V, 1, 1, 1, 1, 0, 704, 100
30833, V, 1, 1, 1, 1, 0, 704, 100
30834, V, 1, 1, 1, 1, 0, 704, 100
30835, V, 1, 1, 1, 1, 0, 704, 100
30836, V, 1, 1, 1, 1, 0, 704, 100
30837, V, 1, 1, 1, 1, 0, 704, 100
30838, V, 1, 1, 1, 1, 0, 704, 100
30839, V, 1, 1, 1, 1, 0, 704, 100
30840, V, 1, 1, 1, 1, 0, 704, 100
30841, V, 1, 1, 1, 1, 0, 704, 100
30842, V, 1, 1, 1, 1, 0, 704, 100
30843, V, 1, 1, 1, 1, 0, 704, 100
30844, V, 1, 1, 1, 1, 0, 704, 100
30845, V, 1, 1, 1, 1, 0, 704, 100
30846, V, 1, 1, 1, 1, 0, 704, 100
30848, V, 1, 1, 1, 1, 0, 704, 100
30849, V, 1, 1, 1, 1, 0, 704, 100
30850, V, 1, 1, 1, 1, 0, 704, 100
30851, V, 1, 1, 1, 1, 0, 704, 100
30852, V, 1, 1, 1, 1, 0, 704, 100
30853, V, 1, 1, 1, 1, 0, 704, 100
30854, V, 1, 1, 1, 1, 0, 704, 100
30855, V, 1, 1, 1, 1, 0, 704, 100
30856, V, 1, 1, 1, 1, 0, 704, 100
30857, V, 1, 1, 1, 1, 0, 704, 100
30858, V, 1, 1, 1, 1, 0, 704, 100
30859, V, 1, 1, 1, 1, 0, 704, 100
30860, V, 1, 1, 1, 1, 0, 704, 100
30861, V, 1, 1, 1, 1, 0, 704, 100
30862, V, 1, 1, 1, 1, 0, 704, 100
30863, V, 1, 1, 1, 1, 0, 704, 100
30864, V, 1, 1, 1, 1, 0, 704, 100
30865, V, 1, 1, 1, 1, 0, 704, 100
30866, V, 1, 1, 1, 1, 0, 704, 100
30867, V, 1, 1, 1, 1, 0, 704, 100
30868, V, 1, 1, 1, 1, 0, 704, 100
30869, V, 1, 1, 1, 1, 0, 704, 100
30870, V, 1, 1, 1, 1, 0, 704, 100
30871, V, 1, 1, 1, 1, 0, 704, 100
30872, V, 1, 1, 1, 1, 0, 704, 100
30873, V, 1, 1, 1, 1, 0, 704, 100
30874, V, 1, 1, 1, 1, 0, 704, 100
30875, V, 1, 1, 1, 1, 0, 704, 100
30876, V, 1, 1, 1, 1, 0, 704, 100
30877, V, 1, 1, 1, 1, 0, 704, 100
30878, V, 1, 1, 1, 1, 0, 704, 100
30879, V, 1, 1, 1, 1, 0, 704, 100
30880, V, 1, 1, 1, 1, 0, 704, 100
30881, V, 1, 1, 1, 1, 0, 704, 100
30882, V, 1, 1, 1, 1, 0, 704, 100
30883, V, 1, 1, 1, 1, 0, 704, 100
30884, V, 1, 1, 1, 1, 0, 704, 100
30885, V, 1, 1, 1, 1, 0, 704, 100
30886, V, 1, 1, 1, 1, 0, 704, 100
30887, V, 1, 1, 1, 1, 0, 704, 100
30888, V, 1, 1, 1, 1, 0, 704, 100
30889, V, 1, 1, 1, 1, 0, 704, 100
30891, V, 1, 1, 1, 1, 0, 704, 100
30892, V, 1, 1, 1, 1, 0, 704, 100
30893, V, 1, 1, 1, 1, 0, 704, 100
30894, V, 1, 1, 1, 1, 0, 704, 100
30895, V, 1, 1, 1, 1, 0, 704, 100
30896, V, 1, 1, 1, 1, 0, 704, 100
30897, V, 1, 1, 1, 1, 0, 704, 100
30898, V, 1, 1, 1, 1, 0, 704, 100
30899, V, 1, 1, 1, 1, 0, 704, 100
30900, V, 1, 1, 1, 1, 0, 704, 100
30901, V, 1, 1, 1, 1, 0, 704, 100
30902, V, 1, 1, 1, 1, 0, 704, 100
30903, V, 1, 1, 1, 1, 0, 704, 100
30904, V, 1, 1, 1, 1, 0, 704, 100
30905, V, 1, 1, 1, 1, 0, 704, 100
30906, V, 1, 1, 1, 1, 0, 704, 100
30907, V, 1, 1, 1, 1, 0, 704, 100
30908, V, 1, 1, 1, 1, 0, 704, 100
30909, V, 1, 1, 1, 1, 0, 704, 100
30910, V, 1, 1, 1, 1, 0, 704, 100
30911, V, 1, 1, 1, 1, 0, 704, 100
30912, V, 1, 1, 1, 1, 0, 704, 100
30913, V, 1, 1, 1, 1, 0, 704, 100
30914, V, 1, 1, 1, 1, 0, 704, 100
30915, V, 1, 1, 1, 1, 0, 704, 100
30916, V, 1, 1, 1, 1, 0, 704, 100
30917, V, 1, 1, 1, 1, 0, 704, 100
30918, V, 1, 1, 1, 1, 0, 704, 100
30919, V, 1, 1, 1, 1, 0, 704, 100
30920, V, 1, 1, 1, 1, 0, 704, 100
30921, V, 1, 1, 1, 1, 0, 704, 100
30922, V, 1, 1, 1, 1, 0, 704, 100
30923, V, 1, 1, 1, 1, 0, 704, 100
30924, V, 1, 1, 1, 1, 0, 704, 100
30925, V, 1, 1, 1, 1, 0, 704, 100
30926, V, 1, 1, 1, 1, 0, 704, 100
30927, V, 1, 1, 1, 1, 0, 704, 100
30928, V, 1, 1, 1, 1, 0, 704, 100
30929, V, 1, 1, 1, 1, 0, 704, 100
30930, V, 1, 1, 1, 1, 0, 704, 100
30931, V, 1, 1, 1, 1, 0, 704, 100
30932, V, 1, 1, 1, 1, 0, 704, 100
30934, V, 1, 1, 1, 1, 0, 704, 100
30935, V, 1, 1, 1, 1, 0, 704, 100
30936, V, 1, 1, 1, 1, 0, 704, 100
30937, V, 1, 1, 1, 1, 0, 704, 100
30938, V, 1, 1, 1, 1, 0, 704, 100
30939, V, 1, 1, 1, 1, 0, 704, 100
30940, V, 1, 1, 1, 1, 0, 704, 100
30941, V, 1, 1, 1, 1, 0, 704, 100
30942, V, 1, 1, 1, 1, 0, 704, 100
30943, V, 1, 1, 1, 1, 0, 704, 100
30944, V, 1, 1, 1, 1, 0, 704, 100
30945, V, 1, 1, 1, 1, 0, 704, 100
30946, V, 1, 1, 1, 1, 0, 704, 100
30947, V, 1, 1, 1, 1, 0, 704, 100
30948, V, 1, 1, 1, 1, 0, 704, 100
30949, V, 1, 1, 1, 1, 0, 704, 100
30950, V, 1, 1, 1, 1, 0, 704, 100
30951, V, 1, 1, 1, 1, 0, 704, 100
30952, V, 1, 1, 1, 1, 0, 704, 100
30953, V, 1, 1, 1, 1, 0, 704, 100
30954, V, 1, 1, 1, 1, 0, 704, 100
30955, V, 1, 1, 1, 1, 0, 704, 100
30956, V, 1, 1, 1, 1, 0, 704, 100
30957, V, 1, 1, 1, 1, 0, 704, 100
30958, V, 1, 1, 1, 1, 0, 704, 100
30959, V, 1, 1, 1, 1, 0, 704, 100
30960, V, 1, 1, 1, 1, 0, 704, 100
30961, V, 1, 1, 1, 1, 0, 704, 100
30962, V, 1, 1, 1, 1, 0, 704, 100
30963, V, 1, 1, 1, 1, 0, 704, 100
30964, V, 1, 1, 1, 1, 0, 704, 100
30965, V, 1, 1, 1, 1, 0, 704, 100
30966, V, 1, 1, 1, 1, 0, 704, 100
30967, V, 1, 1, 1, 1, 0, 704, 100
30968, V, 1, 1, 1, 1, 0, 704, 100
30969, V, 1, 1, 1, 1, 0, 704, 100
30970, V, 1, 1, 1, 1, 0, 704, 100
30971, V, 1, 1, 1, 1, 0, 704, 100
30972, V, 1, 1, 1, 1, 0, 704, 100
30973, V, 1, 1, 1, 1, 0, 704, 100
30974, V, 1, 1, 1, 1, 0, 704, 100
30976, V, 1, 1, 1, 1, 0, 704, 100
30977, V, 1, 1, 1, 1, 0, 704, 100
30978, V, 1, 1, 1, 1, 0, 704, 100
30979, V, 1, 1, 1, 1, 0, 704, 100
30980, V, 1, 1, 1, 1, 0, 704, 100
30981, V, 1, 1, 1, 1, 0, 704, 100
30982, V, 1, 1, 1, 1, 0, 704, 100
30983, V, 1, 1, 1, 1, 0, 704, 100
30984, V, 1, 1, 1, 1, 0, 704, 100
30985, V, 1, 1, 1, 1, 0, 704, 100
30986, V, 1, 1, 1, 1, 0, 704, 100
30987, V, 1, 1, 1, 1, 0, 704, 100
30988, V, 1, 1, 1, 1, 0, 704, 100
30989, V, 1, 1, 1, 1, 0, 704, 100
30990, V, 1, 1, 1, 1, 0, 704, 100
30991, V, 1, 1, 1, 1, 0, 704, 100
30992, V, 1, 1, 1, 1, 0, 704, 100
30993, V, 1, 1, 1, 1, 0, 704, 100
30994, V, 1, 1, 1, 1, 0, 704, 100
30995, V, 1, 1, 1, 1, 0, 704, 100
30996, V, 1, 1, 1, 1, 0, 704, 100
30997, V, 1, 1, 1, 1, 0, 704, 100
30998, V, 1, 1, 1, 1, 0, 704, 100
30999, V, 1, 1, 1, 1, 0, 704, 100
31000, V, 1, 1, 1, 1, 0, 704, 100
31001, V, 1, 1, 1, 1, 0, 704, 100
31002, V, 1, 1, 1, 1, 0, 704, 100
31003, V, 1, 1, 1, 1, 0, 704, 100
31004, V, 1, 1, 1, 1, 0, 704, 100
31005, V, 1, 1, 1, 1, 0, 704, 100
31006, V, 1, 1, 1, 1, 0, 704, 100
31007, V, 1, 1, 1, 1, 0, 704, 100
31008, V, 1, 1, 1, 1, 0, 704, 100
31009, V, 1, 1, 1, 1, 0, 704, 100
31010, V, 1, 1, 1, 1, 0, 704, 100
31011, V, 1, 1, 1, 1, 0, 704, 100
31012, V, 1, 1, 1, 1, 0, 704, 100
31013, V, 1, 1, 1, 1, 0, 704, 100
31014, V, 1, 1, 1, 1, 0, 704, 100
31015, V, 1, 1, 1, 1, 0, 704, 100
31016, V, 1, 1, 1, 1, 0, 704, 100
31017, V, 1, 1, 1, 1, 0, 704, 100
31019, V, 1, 1, 1, 1, 0, 704, 100
31020, V, 1, 1, 1, 1, 0, 704, 100
31021, V, 1, 1, 1, 1, 0, 704, 100
31022, V, 1, 1, 1, 1, 0, 704, 100
31023, V, 1, 1, 1, 1, 0, 704, 100
31024, V, 1, 1, 1, 1, 0, 704, 100
31025, V, 1, 1, 1, 1, 0, 704, 100
31026, V, 1, 1, 1, 1, 0, 704, 100
31027, V, 1, 1, 1, 1, 0, 704, 100
31028, V, 1, 1, 1, 1, 0, 704, 100
31029, V, 1, 1, 1, 1, 0, 704, 100
31030, V, 1, 1, 1, 1, 0, 704, 100
31031, V, 1, 1, 1, 1, 0, 704, 100
31032, V, 1, 1, 1, 1, 0, 704, 100
31033, V, 1, 1, 1, 1, 0, 704, 100
31034, V, 1, 1, 1, 1, 0, 704, 100
31035, V, 1, 1, 1, 1, 0, 704, 100
31036, V, 1, 1, 1, 1, 0, 704, 100
31037, V, 1, 1, 1, 1, 0, 704, 100
31038, V, 1, 1, 1, 1, 0, 704, 100
31039, V, 1, 1, 1, 1, 0, 704, 100
31040, V, 1, 1, 1, 1, 0, 704, 100
31041, V, 1, 1, 1, 1, 0, 704, 100
31042, V, 1, 1, 1, 1, 0, 704, 100
31043, V, 1, 1, 1, 1, 0, 704, 100
31044, V, 1, 1, 1, 1, 0, 704, 100
31045, V, 1, 1, 1, 1, 0, 704, 100
31046, V, 1, 1, 1, 1, 0, 704, 100
31047, V, 1, 1, 1, 1, 0, 704, 100
31048, V, 1, 1, 1, 1, 0, 704, 100
31049, V, 1, 1, 1, 1, 0, 704, 100
31050, V, 1, 1, 1, 1, 0, 704, 100
31051, V, 1, 1, 1, 1, 0, 704, 100
31052, V, 1, 1, 1, 1, 0, 704, 100
31053, V, 1, 1, 1, 1, 0, 704, 100
31054, V, 1, 1, 1, 1, 0, 704, 100
31055, V, 1, 1, 1, 1, 0, 704, 100
31056, V, 1, 1, 1, 1, 0, 704, 100
31057, V, 1, 1, 1, 1, 0, 704, 100
31058, V, 1, 1, 1, 1, 0, 704, 100
31059, V, 1, 1, 1, 1, 0, 704, 100
31060, V, 1, 1, 1, 1, 0, 704, 100
31062, V, 1, 1, 1, 1, 0, 704, 100
31063, V, 1, 1, 1, 1, 0, 704, 100
31064, V, 1, 1, 1, 1, 0, 704, 100
31065, V, 1, 1, 1, 1, 0, 704, 100
31066, V, 1, 1, 1, 1, 0, 704, 100
31067, V, 1, 1, 1, 1, 0, 704, 100
31068, V, 1, 1, 1, 1, 0, 704, 100
31069, V, 1, 1, 1, 1, 0, 704, 100
31070, V, 1, 1, 1, 1, 0, 704, 100
31071, V, 1, 1, 1, 1, 0, 704, 100
31072, V, 1, 1, 1, 1, 0, 704, 100
31073, V, 1, 1, 1, 1, 0, 704, 100
31074, V, 1, 1, 1, 1, 0, 704, 100
31075, V, 1, 1, 1, 1, 0, 704, 100
31076, V, 1, 1, 1, 1, 0, 704, 100
31077, V, 1, 1, 1, 1, 0, 704, 100
31078, V, 1, 1, 1, 1, 0, 704, 100
31079, V, 1, 1, 1, 1, 0, 704, 100
31080, V, 1, 1, 1, 1, 0, 704, 100
31081, V, 1, 1, 1, 1, 0, 704, 100
31082, V, 1, 1, 1, 1, 0, 704, 100
31083, V, 1, 1, 1, 1, 0, 704, 100
31084, V, 1, 1, 1, 1, 0, 704, 100
31085, V, 1, 1, 1, 1, 0, 704, 100
31086, V, 1, 1, 1, 1, 0, 704, 100
31087, V, 1, 1, 1, 1, 0, 704, 100
31088, V, 1, 1, 1, 1, 0, 704, 100
31089, V, 1, 1, 1, 1, 0, 704, 100
31090, V, 1, 1, 1, 1, 0, 704, 100
31091, V, 1, 1, 1, 1, 0, 704, 100
31092, V, 1, 1, 1, 1, 0, 704, 100
31093, V, 1, 1, 1, 1, 0, 704, 100
31094, V, 1, 1, 1, 1, 0, 704, 100
31095, V, 1, 1, 1, 1, 0, 704, 100
31096, V, 1, 1, 1, 1, 0, 704, 100
31097, V, 1, 1, 1, 1, 0, 704, 100
31098, V, 1, 1, 1, 1, 0, 704, 100
31099, V, 1, 1, 1, 1, 0, 704, 100
31100, V, 1, 1, 1, 1, 0, 704, 100
31101, V, 1, 1, 1, 1, 0, 704, 100
31102, V, 1, 1, 1, 1, 0, 704, 100
31104, V, 1, 1, 1, 1, 0, 704, 100
31105, V, 1, 1, 1, 1, 0, 704, 100
31106, V, 1, 1, 1, 1, 0, 704, 100
31107, V, 1, 1, 1, 1, 0, 704, 100
31108, V, 1, 1, 1, 1, 0, 704, 100
31109, V, 1, 1, 1, 1, 0, 704, 100
31110, V, 1, 1, 1, 1, 0, 704, 100
31111, V, 1, 1, 1, 1, 0, 704, 100
31112, V, 1, 1, 1, 1, 0, 704, 100
31113, V, 1, 1, 1, 1, 0, 704, 100
31114, V, 1, 1, 1, 1, 0, 704, 100
31115, V, 1, 0, 0, 1, 0, 704, 100
31115, V, 1, 0, 0, 0, 0, 704, 100
31116, V, 1, 1, 0, 0, 0, 704, 100
31116, V, 1, 1, 0, 0, 0, 704, 100
31117, V, 1, 1, 1, 1, 0, 704, 100
31118, V, 1, 1, 1, 1, 0, 704, 100
31119, V, 1, 1, 1, 1, 0, 704, 100
31120, V, 1, 1, 1, 1, 0, 704, 100
31121, V, 1, 1, 1, 1, 0, 704, 100
31122, V, 1, 1, 1, 1, 0, 704, 99
31123, V, 1, 1, 1, 1, 0, 704, 99
31124, V, 1, 1, 1, 1, 0, 704, 99
31125, V, 1, 1, 1, 1, 0, 704, 99
31126, V, 1, 1, 1, 1, 0, 704, 99
31127, V, 1, 1, 1, 1, 0, 704, 99
31128, V, 1, 1, 1, 1, 0, 704, 99
31129, V, 1, 1, 1, 1, 0, 704, 99
31130, V, 1, 1, 1, 1, 0, 704, 99
31131, V, 1, 1, 1, 1, 0, 704, 99
31132, V, 1, 1, 1, 1, 0, 704, 99
31133, V, 1, 1, 1, 1, 0, 704, 99
31134, V, 1, 1, 1, 1, 0, 704, 99
31135, V, 1, 1, 1, 1, 0, 704, 99
31136, V, 1, 1, 1, 1, 0, 704, 100
31137, V, 1, 1, 1, 1, 0, 704, 99
31138, V, 1, 1, 1, 1, 0, 704, 100
31139, V, 1, 1, 1, 1, 0, 704, 100
31140, V, 1, 1, 1, 1, 0, 704, 100
31141, V, 1, 1, 1, 1, 0, 704, 100
31142, V, 1, 1, 1, 1, 0, 704, 100
31143, V, 1, 1, 1, 1, 0, 704, 100
31144, V, 1, 1, 1, 1, 0, 704, 100
31145, V, 1, 1, 1, 1, 0, 704, 100
31147, V, 1, 1, 1, 1, 0, 704, 100
31148, V, 1, 1, 1, 1, 0, 704, 100
31149, V, 1, 1, 1, 1, 0, 704, 100
31150, V, 1, 1, 1, 1, 0, 704, 100
31151, V, 1, 1, 1, 1, 0, 704, 100
31152, V, 1, 1, 1, 1, 0, 704, 100
31153, V, 1, 1, 1, 1, 0, 704, 100
31154, V, 1, 1, 1, 1, 0, 704, 100
31155, V, 1, 1, 1, 1, 0, 704, 100
31156, V, 1, 1, 1, 1, 0, 704, 100
31157, V, 1, 1, 1, 1, 0, 704, 100
31158, V, 1, 1, 1, 1, 0, 704, 100
31159, V, 1, 1, 1, 1, 0, 704, 100
31160, V, 1, 1, 1, 1, 0, 704, 100
31161, V, 1, 1, 1, 1, 0, 704, 100
31162, V, 1, 1, 1, 1, 0, 704, 100
31163, V, 1, 1, 1, 1, 0, 704, 100
31164, V, 1, 1, 1, 1, 0, 704, 100
31165, V, 1, 1, 1, 1, 0, 704, 100
31166, V, 1, 1, 1, 1, 0, 704, 100
31167, V, 1, 1, 1, 1, 0, 704, 100
31168, V, 1, 1, 1, 1, 0, 704, 100
31169, V, 1, 1, 1, 1, 0, 704, 100
31170, V, 1, 1, 1, 1, 0, 704, 100
31171, V, 1, 1, 1, 1, 0, 704, 100
31172, V, 1, 1, 1, 1, 0, 704, 100
31173, V, 1, 1, 1, 1, 0, 704, 100
31174, V, 1, 1, 1, 1, 0, 704, 100
31175, V, 1, 1, 1, 1, 0, 704, 100
31176, V, 1, 1, 1, 1, 0, 704, 100
31177, V, 1, 1, 1, 1, 0, 704, 100
31178, V, 1, 1, 1, 1, 0, 704, 100
31179, V, 1, 1, 1, 1, 0, 704, 100
31180, V, 1, 1, 1, 1, 0, 704, 100
31181, V, 1, 1, 1, 1, 0, 704, 100
31182, V, 1, 1, 1, 1, 0, 704, 100
31183, V, 1, 1, 1, 1, 0, 704, 100
31184, V, 1, 1, 1, 1, 0, 704, 100
31185, V, 1, 1, 1, 1, 0, 704, 100
31186, V, 1, 1, 1, 1, 0, 704, 100
31187, V, 1, 1, 1, 1, 0, 704, 100
31188, V, 1, 1, 1, 1, 0, 704, 100
31190, V, 1, 1, 1, 1, 0, 704, 100
31191, V, 1, 1, 1, 1, 0, 704, 100
31192, V, 1, 1, 1, 1, 0, 704, 100
31193, V, 1, 1, 1, 1, 0, 704, 100
31194, V, 1, 1, 1, 1, 0, 704, 100
31195, V, 1, 1, 1, 1, 0, 704, 100
31196, V, 1, 1, 1, 1, 0, 704, 100
31197, V, 1, 1, 1, 1, 0, 704, 100
31198, V, 1, 1, 1, 1, 0, 704, 100
31199, V, 1, 1, 1, 1, 0, 704, 100
31200, V, 1, 1, 1, 1, 0, 704, 100
31201, V, 1, 1, 1, 1, 0, 704, 100
31202, V, 1, 1, 1, 1, 0, 704, 100
31203, V, 1, 1, 1, 1, 0, 704, 100
31204, V, 1, 1, 1, 1, 0, 704, 100
31205, V, 1, 1, 1, 1, 0, 704, 100
31206, V, 1, 1, 1, 1, 0, 704, 100
31207, V, 1, 1, 1, 1, 0, 704, 100
31208, V, 1, 1, 1, 1, 0, 704, 100
31209, V, 1, 1, 1, 1, 0, 704, 100
31210, V, 1, 1, 1, 1, 0, 704, 100
31211, V, 1, 1, 1, 1, 0, 704, 100
31212, V, 1, 1, 1, 1, 0, 704, 100
31213, V, 1, 1, 1, 1, 0, 704, 100
31214, V, 1, 1, 1, 1, 0, 704, 100
31215, V, 1, 1, 1, 1, 0, 704, 100
31216, V, 1, 1, 1, 1, 0, 704, 100
31217, V, 1, 1, 1, 1, 0, 704, 100
31218, V, 1, 1, 1, 1, 0, 704, 100
31219, V, 1, 1, 1, 1, 0, 704, 100
31220, V, 1, 1, 1, 1, 0, 704, 100
31221, V, 1, 1, 1, 1, 0, 704, 100
31222, V, 1, 0, 0, 1, 0, 704, 100
31222, V, 1, 0, 0, 0, 0, 704, 100
31223, V, 1, 1, 0, 0, 0, 704, 100
31223, V, 1, 1, 0, 0, 0, 704, 100
31224, V, 1, 1, 1, 1, 0, 704, 100
31225, V, 1, 1, 1, 1, 0, 704, 100
31226, V, 1, 1, 1, 1, 0, 704, 100
31227, V, 1, 1, 1, 1, 0, 704, 100
31228, V, 1, 1, 1, 1, 0, 704, 99
31229, V, 1, 1, 1, 1, 0, 704, 99
31230, V, 1, 1, 1, 1, 0, 704, 99
31232, V, 1, 1, 1, 1, 0, 704, 99
31233, V, 1, 1, 1, 1, 0, 704, 99
31234, V, 1, 1, 1, 1, 0, 704, 99
31235, V, 1, 1, 1, 1, 0, 704, 99
31236, V, 1, 1, 1, 1, 0, 704, 99
31237, V, 1, 1, 1, 1, 0, 704, 99
31238, V, 1, 1, 1, 1, 0, 704, 99
31239, V, 1, 1, 1, 1, 0, 704, 99
31240, V, 1, 1, 1, 1, 0, 704, 99
31241, V, 1, 1, 1, 1, 0, 704, 99
31242, V, 1, 1, 1, 1, 0, 704, 99
31243, V, 1, 1, 1, 1, 0, 704, 99
31244, V, 1, 1, 1, 1, 0, 704, 100
31245, V, 1, 1, 1, 1, 0, 704, 100
31246, V, 1, 1, 1, 1, 0, 704, 100
31247, V, 1, 1, 1, 1, 0, 704, 100
31248, V, 1, 1, 1, 1, 0, 704, 100
31249, V, 1, 1, 1, 1, 0, 704, 100
31250, V, 1, 1, 1, 1, 0, 704, 100
31251, V, 1, 1, 1, 1, 0, 704, 100
31252, V, 1, 1, 1, 1, 0, 704, 100
31253, V, 1, 1, 1, 1, 0, 704, 100
31254, V, 1, 1, 1, 1, 0, 704, 100
31255, V, 1, 1, 1, 1, 0, 704, 100
31256, V, 1, 1, 1, 1, 0, 704, 100
31257, V, 1, 1, 1, 1, 0, 704, 100
31258, V, 1, 1, 1, 1, 0, 704, 100
31259, V, 1, 1, 1, 1, 0, 704, 100
31260, V, 1, 1, 1, 1, 0, 704, 100
31261, V, 1, 1, 1, 1, 0, 704, 100
31262, V, 1, 1, 1, 1, 0, 704, 100
31263, V, 1, 1, 1, 1, 0, 704, 100
31264, V, 1, 1, 1, 1, 0, 704, 100
31265, V, 1, 1, 1, 1, 0, 704, 100
31266, V, 1, 1, 1, 1, 0, 704, 100
31267, V, 1, 1, 1, 1, 0, 704, 100
31268, V, 1, 1, 1, 1, 0, 704, 100
31269, V, 1, 1, 1, 1, 0, 704, 100
31270, V, 1, 1, 1, 1, 0, 704, 100
31271, V, 1, 1, 1, 1, 0, 704, 100
31272, V, 1, 1, 1, 1, 0, 704, 100
31273, V, 1, 1, 1, 1, 0, 704, 100
31275, V, 1, 1, 1, 1, 0, 704, 100
31276, V, 1, 1, 1, 1, 0, 704, 100
31277, V, 1, 1, 1, 1, 0, 704, 100
31278, V, 1, 1, 1, 1, 0, 704, 100
31279, V, 1, 1, 1, 1, 0, 704, 100
31280, V, 1, 1, 1, 1, 0, 704, 100
31281, V, 1, 1, 1, 1, 0, 704, 100
31282, V, 1, 1, 1, 1, 0, 704, 100
31283, V, 1, 1, 1, 1, 0, 704, 100
31284, V, 1, 1, 1, 1, 0, 704, 100
31285, V, 1, 1, 1, 1, 0, 704, 100
31286, V, 1, 1, 1, 1, 0, 704, 100
31287, V, 1, 1, 1, 1, 0, 704, 100
31288, V, 1, 1, 1, 1, 0, 704, 100
31289, V, 1, 1, 1, 1, 0, 704, 100
31290, V, 1, 1, 1, 1, 0, 704, 100
31291, V, 1, 1, 1, 1, 0, 704, 100
31292, V, 1, 1, 1, 1, 0, 704, 100
31293, V, 1, 1, 1, 1, 0, 704, 100
31294, V, 1, 1, 1, 1, 0, 704, 100
31295, V, 1, 1, 1, 1, 0, 704, 100
31296, V, 1, 1, 1, 1, 0, 704, 100
31297, V, 1, 1, 1, 1, 0, 704, 100
31298, V, 1, 1, 1, 1, 0, 704, 100
31299, V, 1, 1, 1, 1, 0, 704, 100
31300, V, 1, 1, 1, 1, 0, 704, 100
31301, V, 1, 1, 1, 1, 0, 704, 100
31302, V, 1, 1, 1, 1, 0, 704, 100
31303, V, 1, 1, 1, 1, 0, 704, 100
31304, V, 1, 1, 1, 1, 0, 704, 100
31305, V, 1, 1, 1, 1, 0, 704, 100
31306, V, 1, 1, 1, 1, 0, 704, 100
31307, V, 1, 1, 1, 1, 0, 704, 100
31308, V, 1, 1, 1, 1, 0, 704, 100
31309, V, 1, 1, 1, 1, 0, 704, 100
31310, V, 1, 1, 1, 1, 0, 704, 100
31311, V, 1, 1, 1, 1, 0, 704, 100
31312, V, 1, 1, 1, 1, 0, 704, 100
31313, V, 1, 1, 1, 1, 0, 704, 100
31314, V, 1, 1, 1, 1, 0, 704, 100
31315, V, 1, 1, 1, 1, 0, 704, 100
31316, V, 1, 1, 1, 1, 0, 704, 100
31318, V, 1, 1, 1, 1, 0, 704, 100
31319, V, 1, 1, 1, 1, 0, 704, 100
31320, V, 1, 1, 1, 1, 0, 704, 100
31321, V, 1, 1, 1, 1, 0, 704, 100
31322, V, 1, 1, 1, 1, 0, 704, 100
31323, V, 1, 1, 1, 1, 0, 704, 100
31324, V, 1, 1, 1, 1, 0, 704, 100
31325, V, 1, 1, 1, 1, 0, 704, 100
31326, V, 1, 1, 1, 1, 0, 704, 100
31327, V, 1, 1, 1, 1, 0, 704, 100
31328, V, 1, 1, 1, 1, 0, 704, 100
31329, V, 1, 1, 1, 1, 0, 704, 100
31330, V, 1, 1, 1, 1, 0, 704, 100
31331, V, 1, 1, 1, 1, 0, 704, 100
31332, V, 1, 1, 1, 1, 0, 704, 100
31333, V, 1, 1, 1, 1, 0, 704, 100
31334, V, 1, 1, 1, 1, 0, 704, 100
31335, V, 1, 1, 1, 1, 0, 704, 100
31336, V, 1, 1, 1, 1, 0, 704, 100
31337, V, 1, 1, 1, 1, 0, 704, 100
31338, V, 1, 1, 1, 1, 0, 704, 100
31339, V, 1, 1, 1, 1, 0, 704, 100
31340, V, 1, 1, 1, 1, 0, 704, 100
31341, V, 1, 1, 1, 1, 0, 704, 100
31342, V, 1, 1, 1, 1, 0, 704, 100
31343, V, 1, 1, 1, 1, 0, 704, 100
31344, V, 1, 1, 1, 1, 0, 704, 100
31345, V, 1, 1, 1, 1, 0, 704, 100
31346, V, 1, 1, 1, 1, 0, 704, 100
31347, V, 1, 1, 1, 1, 0, 704, 100
31348, V, 1, 1, 1, 1, 0, 704, 100
31349, V, 1, 1, 1, 1, 0, 704, 100
31350, V, 1, 1, 1, 1, 0, 704, 100
31351, V, 1, 1, 1, 1, 0, 704, 100
31352, V, 1, 1, 1, 1, 0, 704, 100
31353, V, 1, 1, 1, 1, 0, 704, 100
31354, V, 1, 1, 1, 1, 0, 704, 100
31355, V, 1, 1, 1, 1, 0, 704, 100
31356, V, 1, 1, 1, 1, 0, 704, 100
31357, V, 1, 1, 1, 1, 0, 704, 100
31358, V, 1, 1, 1, 1, 0, 704, 100
31360, V, 1, 1, 1, 1, 0, 704, 100
31361, V, 1, 1, 1, 1, 0, 704, 100
31362, V, 1, 1, 1, 1, 0, 704, 100
31363, V, 1, 1, 1, 1, 0, 704, 100
31364, V, 1, 1, 1, 1, 0, 704, 100
31365, V, 1, 1, 1, 1, 0, 704, 100
31366, V, 1, 1, 1, 1, 0, 704, 100
31367, V, 1, 1, 1, 1, 0, 704, 100
31368, V, 1, 1, 1, 1, 0, 704, 100
31369, V, 1, 1, 1, 1, 0, 704, 100
31370, V, 1, 1, 1, 1, 0, 704, 100
31371, V, 1, 1, 1, 1, 0, 704, 100
31372, V, 1, 1, 1, 1, 0, 704, 100
31373, V, 1, 1, 1, 1, 0, 704, 100
31374, V, 1, 1, 1, 1, 0, 704, 100
31375, V, 1, 1, 1, 1, 0, 704, 100
31376, V, 1, 1, 1, 1, 0, 704, 100
31377, V, 1, 1, 1, 1, 0, 704, 100
31378, V, 1, 1, 1, 1, 0, 704, 100
31379, V, 1, 1, 1, 1, 0, 704, 100
31380, V, 1, 1, 1, 1, 0, 704, 100
31381, V, 1, 1, 1, 1, 0, 704, 100
31382, V, 1, 1, 1, 1, 0, 704, 100
31383, V, 1, 1, 1, 1, 0, 704, 100
31384, V, 1, 1, 1, 1, 0, 704, 100
31385, V, 1, 1, 1, 1, 0, 704, 100
31386, V, 1, 1, 1, 1, 0, 704, 100
31387, V, 1, 1, 1, 1, 0, 704, 100
31388, V, 1, 1, 1, 1, 0, 704, 100
31389, V, 1, 1, 1, 1, 0, 704, 100
31390, V, 1, 1, 1, 1, 0, 704, 100
31391, V, 1, 1, 1, 1, 0, 704, 100
31392, V, 1, 1, 1, 1, 0, 704, 100
31393, V, 1, 1, 1, 1, 0, 704, 100
31394, V, 1, 1, 1, 1, 0, 704, 100
31395, V, 1, 1, 1, 1, 0, 704, 100
31396, V, 1, 1, 1, 1, 0, 704, 100
31397, V, 1, 1, 1, 1, 0, 704, 100
31398, V, 1, 1, 1, 1, 0, 704, 100
31399, V, 1, 1, 1, 1, 0, 704, 100
31400, V, 1, 1, 1, 1, 0, 704, 100
31401, V, 1, 1, 1, 1, 0, 704, 100
31403, V, 1, 1, 1, 1, 0, 704, 100
31404, V, 1, 1, 1, 1, 0, 704, 100
31405, V, 1, 1, 1, 1, 0, 704, 100
31406, V, 1, 1, 1, 1, 0, 704, 100
31407, V, 1, 1, 1, 1, 0, 704, 100
31408, V, 1, 1, 1, 1, 0, 704, 100
31409, V, 1, 1, 1, 1, 0, 704, 100
31410, V, 1, 1, 1, 1, 0, 704, 100
31411, V, 1, 1, 1, 1, 0, 704, 100
31412, V, 1, 1, 1, 1, 0, 704, 100
31413, V, 1, 1, 1, 1, 0, 704, 100
31414, V, 1, 1, 1, 1, 0, 704, 100
31415, V, 1, 1, 1, 1, 0, 704, 100
31416, V, 1, 1, 1, 1, 0, 704, 100
31417, V, 1, 1, 1, 1, 0, 704, 100
31418, V, 1, 1, 1, 1, 0, 704, 100
31419, V, 1, 1, 1, 1, 0, 704, 100
31420, V, 1, 1, 1, 1, 0, 704, 100
31421, V, 1, 1, 1, 1, 0, 704, 100
31422, V, 1, 1, 1, 1, 0, 704, 100
31423, V, 1, 1, 1, 1, 0, 704, 100
31424, V, 1, 1, 1, 1, 0, 704, 100
31425, V, 1, 1, 1, 1, 0, 704, 100
31426, V, 1, 1, 1, 1, 0, 704, 100
31427, V, 1, 1, 1, 1, 0, 704, 100
31428, V, 1, 1, 1, 1, 0, 704, 100
31429, V, 1, 1, 1, 1, 0, 704, 100
31430, V, 1, 1, 1, 1, 0, 704, 100
31431, V, 1, 1, 1, 1, 0, 704, 100
31432, V, 1, 1, 1, 1, 0, 704, 100
31433, V, 1, 1, 1, 1, 0, 704, 100
31434, V, 1, 1, 1, 1, 0, 704, 100
31435, V, 1, 1, 1, 1, 0, 704, 100
31436, V, 1, 1, 1, 1, 0, 704, 100
31437, V, 1, 1, 1, 1, 0, 704, 100
31438, V, 1, 1, 1, 1, 0, 704, 100
31439, V, 1, 1, 1, 1, 0, 704, 100
31440, V, 1, 1, 1, 1, 0, 704, 100
31441, V, 1, 1, 1, 1, 0, 704, 100
31442, V, 1, 1, 1, 1, 0, 704, 100
31443, V, 1, 1, 1, 1, 0, 704, 100
31444, V, 1, 1, 1, 1, 0, 704, 100
31446, V, 1, 1, 1, 1, 0, 704, 100
31447, V, 1, 1, 1, 1, 0, 704, 100
31448, V, 1, 1, 1, 1, 0, 704, 100
31449, V, 1, 1, 1, 1, 0, 704, 100
31450, V, 1, 1, 1, 1, 0, 704, 100
31451, V, 1, 1, 1, 1, 0, 704, 100
31452, V, 1, 1, 1, 1, 0, 704, 100
31453, V, 1, 1, 1, 1, 0, 704, 100
31454, V, 1, 1, 1, 1, 0, 704, 100
31455, V, 1, 1, 1, 1, 0, 704, 100
31456, V, 1, 1, 1, 1, 0, 704, 100
31457, V, 1, 1, 1, 1, 0, 704, 100
31458, V, 1, 1, 1, 1, 0, 704, 100
31459, V, 1, 1, 1, 1, 0, 704, 100
31460, V, 1, 1, 1, 1, 0, 704, 100
31461, V, 1, 1, 1, 1, 0, 704, 100
31462, V, 1, 1, 1, 1, 0, 704, 100
31463, V, 1, 1, 1, 1, 0, 704, 100
31464, V, 1, 1, 1, 1, 0, 704, 100
31465, V, 1, 1, 1, 1, 0, 704, 100
31466, V, 1, 1, 1, 1, 0, 704, 100
31467, V, 1, 1, 1, 1, 0, 704, 100
31468, V, 1, 1, 1, 1, 0, 704, 100
31469, V, 1, 1, 1, 1, 0, 704, 100
31470, V, 1, 0, 0, 1, 0, 704, 100
31470, V, 1, 0, 0, 0, 0, 704, 100
31471, V, 1, 1, 0, 0, 0, 704, 100
31471, V, 1, 1, 0, 0, 0, 704, 100
31472, V, 1, 1, 1, 1, 0, 704, 100
31473, V, 1, 1, 1, 1, 0, 704, 100
31474, V, 1, 1, 1, 1, 0, 704, 100
31475, V, 1, 1, 1, 1, 0, 704, 100
31476, V, 1, 1, 1, 1, 0, 704, 100
31477, V, 1, 1, 1, 1, 0, 704, 100
31478, V, 1, 1, 1, 1, 0, 704, 99
31479, V, 1, 1, 1, 1, 0, 704, 99
31480, V, 1, 1, 1, 1, 0, 704, 99
31481, V, 1, 1, 1, 1, 0, 704, 99
31482, V, 1, 1, 1, 1, 0, 704, 99
31483, V, 1, 1, 1, 1, 0, 704, 99
31484, V, 1, 1, 1, 1, 0, 704, 99
31485, V, 1, 1, 1, 1, 0, 704, 99
31486, V, 1, 1, 1, 1, 0, 704, 99
31488, V, 1, 1, 1, 1, 0, 704, 99
31489, V, 1, 1, 1, 1, 0, 704, 99
31490, V, 1, 1, 1, 1, 0, 704, 99
31491, V, 1, 1, 1, 1, 0, 704, 99
31492, V, 1, 1, 1, 1, 0, 704, 99
31493, V, 1, 1, 1, 1, 0, 704, 99
31494, V, 1, 1, 1, 1, 0, 704, 100
31495, V, 1, 1, 1, 1, 0, 704, 100
31496, V, 1, 1, 1, 1, 0, 704, 100
31497, V, 1, 1, 1, 1, 0, 704, 100
31498, V, 1, 1, 1, 1, 0, 704, 100
31499, V, 1, 1, 1, 1, 0, 704, 100
31500, V, 1, 1, 1, 1, 0, 704, 100
31501, V, 1, 1, 1, 1, 0, 704, 100
31502, V, 1, 1, 1, 1, 0, 704, 100
31503, V, 1, 1, 1, 1, 0, 704, 100
31504, V, 1, 1, 1, 1, 0, 704, 100
31505, V, 1, 1, 1, 1, 0, 704, 100
31506, V, 1, 1, 1, 1, 0, 704, 100
31507, V, 1, 1, 1, 1, 0, 704, 100
31508, V, 1, 1, 1, 1, 0, 704, 100
31509, V, 1, 1, 1, 1, 0, 704, 100
31510, V, 1, 1, 1, 1, 0, 704, 100
31511, V, 1, 1, 1, 1, 0, 704, 100
31512, V, 1, 1, 1, 1, 0, 704, 100
31513, V, 1, 1, 1, 1, 0, 704, 100
31514, V, 1, 1, 1, 1, 0, 704, 100
31515, V, 1, 1, 1, 1, 0, 704, 100
31516, V, 1, 1, 1, 1, 0, 704, 100
31517, V, 1, 1, 1, 1, 0, 704, 100
31518, V, 1, 1, 1, 1, 0, 704, 100
31519, V, 1, 1, 1, 1, 0, 704, 100
31520, V, 1, 1, 1, 1, 0, 704, 100
31521, V, 1, 1, 1, 1, 0, 704, 100
31522, V, 1, 1, 1, 1, 0, 704, 100
31523, V, 1, 1, 1, 1, 0, 704, 100
31524, V, 1, 1, 1, 1, 0, 704, 100
31525, V, 1, 1, 1, 1, 0, 704, 100
31526, V, 1, 1, 1, 1, 0, 704, 100
31527, V, 1, 1, 1, 1, 0, 704, 100
31528, V, 1, 1, 1, 1, 0, 704, 100
31529, V, 1, 1, 1, 1, 0, 704, 100
31531, V, 1, 1, 1, 1, 0, 704, 100
31532, V, 1, 1, 1, 1, 0, 704, 100
31533, V, 1, 1, 1, 1, 0, 704, 100
31534, V, 1, 1, 1, 1, 0, 704, 100
31535, V, 1, 1, 1, 1, 0, 704, 100
31536, V, 1, 1, 1, 1, 0, 704, 100
31537, V, 1, 1, 1, 1, 0, 704, 100
31538, V, 1, 1, 1, 1, 0, 704, 100
31539, V, 1, 1, 1, 1, 0, 704, 100
31540, V, 1, 1, 1, 1, 0, 704, 100
31541, V, 1, 1, 1, 1, 0, 704, 100
31542, V, 1, 1, 1, 1, 0, 704, 100
31543, V, 1, 1, 1, 1, 0, 704, 100
31544, V, 1, 1, 1, 1, 0, 704, 100
31545, V, 1, 1, 1, 1, 0, 704, 100
31546, V, 1, 1, 1, 1, 0, 704, 100
31547, V, 1, 1, 1, 1, 0, 704, 100
31548, V, 1, 1, 1, 1, 0, 704, 100
31549, V, 1, 1, 1, 1, 0, 704, 100
31550, V, 1, 1, 1, 1, 0, 704, 100
31551, V, 1, 1, 1, 1, 0, 704, 100
31552, V, 1, 1, 1, 1, 0, 704, 100
31553, V, 1, 1, 1, 1, 0, 704, 100
31554, V, 1, 1, 1, 1, 0, 704, 100
31555, V, 1, 1, 1, 1, 0, 704, 100
31556, V, 1, 1, 1, 1, 0, 704, 100
31557, V, 1, 1, 1, 1, 0, 704, 100
31558, V, 1, 1, 1, 1, 0, 704, 100
31559, V, 1, 1, 1, 1, 0, 704, 100
31560, V, 1, 1, 1, 1, 0, 704, 100
31561, V, 1, 1, 1, 1, 0, 704, 100
31562, V, 1, 1, 1, 1, 0, 704, 100
31563, V, 1, 1, 1, 1, 0, 704, 100
31564, V, 1, 1, 1, 1, 0, 704, 100
31565, V, 1, 1, 1, 1, 0, 704, 100
31566, V, 1, 1, 1, 1, 0, 704, 100
31567, V, 1, 1, 1, 1, 0, 704, 100
31568, V, 1, 1, 1, 1, 0, 704, 100
31569, V, 1, 1, 1, 1, 0, 704, 100
31570, V, 1, 1, 1, 1, 0, 704, 100
31571, V, 1, 1, 1, 1, 0, 704, 100
31572, V, 1, 1, 1, 1, 0, 704, 100
31574, V, 1, 1, 1, 1, 0, 704, 100
31575, V, 1, 1, 1, 1, 0, 704, 100
31576, V, 1, 1, 1, 1, 0, 704, 100
31577, V, 1, 1, 1, 1, 0, 704, 100
31578, V, 1, 1, 1, 1, 0, 704, 100
31579, V, 1, 1, 1, 1, 0, 704, 100
31580, V, 1, 1, 1, 1, 0, 704, 100
31581, V, 1, 1, 1, 1, 0, 704, 100
31582, V, 1, 1, 1, 1, 0, 704, 100
31583, V, 1, 1, 1, 1, 0, 704, 100
31584, V, 1, 1, 1, 1, 0, 704, 100
31585, V, 1, 1, 1, 1, 0, 704, 100
31586, V, 1, 1, 1, 1, 0, 704, 100
31587, V, 1, 1, 1, 1, 0, 704, 100
31588, V, 1, 1, 1, 1, 0, 704, 100
31589, V, 1, 1, 1, 1, 0, 704, 100
31590, V, 1, 1, 1, 1, 0, 704, 100
31591, V, 1, 1, 1, 1, 0, 704, 100
31592, V, 1, 1, 1, 1, 0, 704, 100
31593, V, 1, 1, 1, 1, 0, 704, 100
31594, V, 1, 1, 1, 1, 0, 704, 100
31595, V, 1, 1, 1, 1, 0, 704, 100
31596, V, 1, 1, 1, 1, 0, 704, 100
31597, V, 1, 1, 1, 1, 0, 704, 100
31598, V, 1, 1, 1, 1, 0, 704, 100
31599, V, 1, 1, 1, 1, 0, 704, 100
31600, V, 1, 1, 1, 1, 0, 704, 100
31601, V, 1, 1, 1, 1, 0, 704, 100
31602, V, 1, 1, 1, 1, 0, 704, 100
31603, V, 1, 1, 1, 1, 0, 704, 100
31604, V, 1, 1, 1, 1, 0, 704, 100
31605, V, 1, 1, 1, 1, 0, 704, 100
31606, V, 1, 1, 1, 1, 0, 704, 100
31607, V, 1, 1, 1, 1, 0, 704, 100
31608, V, 1, 1, 1, 1, 0, 704, 100
31609, V, 1, 1, 1, 1, 0, 704, 100
31610, V, 1, 1, 1, 1, 0, 704, 100
31611, V, 1, 1, 1, 1, 0, 704, 100
31612, V, 1, 1, 1, 1, 0, 704, 100
31613, V, 1, 1, 1, 1, 0, 704, 100
31614, V, 1, 1, 1, 1, 0, 704, 100
31616, V, 1, 1, 1, 1, 0, 704, 100
31617, V, 1, 1, 1, 1, 0, 704, 100
31618, V, 1, 1, 1, 1, 0, 704, 100
31619, V, 1, 1, 1, 1, 0, 704, 100
31620, V, 1, 1, 1, 1, 0, 704, 100
31621, V, 1, 1, 1, 1, 0, 704, 100
31622, V, 1, 1, 1, 1, 0, 704, 100
31623, V, 1, 1, 1, 1, 0, 704, 100
31624, V, 1, 1, 1, 1, 0, 704, 100
31625, V, 1, 1, 1, 1, 0, 704, 100
31626, V, 1, 1, 1, 1, 0, 704, 100
31627, V, 1, 1, 1, 1, 0, 704, 100
31628, V, 1, 1, 1, 1, 0, 704, 100
31629, V, 1, 1, 1, 1, 0, 704, 100
31630, V, 1, 1, 1, 1, 0, 704, 100
31631, V, 1, 1, 1, 1, 0, 704, 100
31632, V, 1, 1, 1, 1, 0, 704, 100
31633, V, 1, 1, 1, 1, 0, 704, 100
31634, V, 1, 1, 1, 1, 0, 704, 100
31635, V, 1, 1, 1, 1, 0, 704, 100
31636, V, 1, 1, 1, 1, 0, 704, 100
31637, V, 1, 1, 1, 1, 0, 704, 100
31638, V, 1, 1, 1, 1, 0, 704, 100
31639, V, 1, 1, 1, 1, 0, 704, 100
31640, V, 1, 1, 1, 1, 0, 704, 100
31641, V, 1, 1, 1, 1, 0, 704, 100
31642, V, 1, 1, 1, 1, 0, 704, 100
31643, V, 1, 1, 1, 1, 0, 704, 100
31644, V, 1, 1, 1, 1, 0, 704, 100
31645, V, 1, 1, 1, 1, 0, 704, 100
31646, V, 1, 1, 1, 1, 0, 704, 100
31647, V, 1, 1, 1, 1, 0, 704, 100
31648, V, 1, 1, 1, 1, 0, 704, 100
31649, V, 1, 1, 1, 1, 0, 704, 100
31650, V, 1, 1, 1, 1, 0, 704, 100
31651, V, 1, 1, 1, 1, 0, 704, 100
31652, V, 1, 1, 1, 1, 0, 704, 100
31653, V, 1, 1, 1, 1, 0, 704, 100
31654, V, 1, 1, 1, 1, 0, 704, 100
31655, V, 1, 1, 1, 1, 0, 704, 100
31656, V, 1, 1, 1, 1, 0, 704, 100
31657, V, 1, 1, 1, 1, 0, 704, 100
31659, V, 1, 1, 1, 1, 0, 704, 100
31660, V, 1, 1, 1, 1, 0, 704, 100
31661, V, 1, 1, 1, 1, 0, 704, 100
31662, V, 1, 1, 1, 1, 0, 704, 100
31663, V, 1, 1, 1, 1, 0, 704, 100
31664, V, 1, 1, 1, 1, 0, 704, 100
31665, V, 1, 1, 1, 1, 0, 704, 100
31666, V, 1, 1, 1, 1, 0, 704, 100
31667, V, 1, 1, 1, 1, 0, 704, 100
31668, V, 1, 1, 1, 1, 0, 704, 100
31669, V, 1, 1, 1, 1, 0, 704, 100
31670, V, 1, 1, 1, 1, 0, 704, 100
31671, V, 1, 1, 1, 1, 0, 704, 100
31672, V, 1, 1, 1, 1, 0, 704, 100
31673, V, 1, 1, 1, 1, 0, 704, 100
31674, V, 1, 1, 1, 1, 0, 704, 100
31675, V, 1, 1, 1, 1, 0, 704, 100
31676, V, 1, 1, 1, 1, 0, 704, 100
31677, V, 1, 1, 1, 1, 0, 704, 100
31678, V, 1, 1, 1, 1, 0, 704, 100
31679, V, 1, 1, 1, 1, 0, 704, 100
31680, V, 1, 1, 1, 1, 0, 704, 100
31681, V, 1, 1, 1, 1, 0, 704, 100
31682, V, 1, 1, 1, 1, 0, 704, 100
31683, V, 1, 1, 1, 1, 0, 704, 100
31684, V, 1, 1, 1, 1, 0, 704, 100
31685, V, 1, 1, 1, 1, 0, 704, 100
31686, V, 1, 1, 1, 1, 0, 704, 100
31687, V, 1, 1, 1, 1, 0, 704, 100
31688, V, 1, 1, 1, 1, 0, 704, 100
31689, V, 1, 1, 1, 1, 0, 704, 100
31690, V, 1, 1, 1, 1, 0, 704, 100
31691, V, 1, 1, 1, 1, 0, 704, 100
31692, V, 1, 1, 1, 1, 0, 704, 100
31693, V, 1, 1, 1, 1, 0, 704, 100
31694, V, 1, 1, 1, 1, 0, 704, 100
31695, V, 1, 1, 1, 1, 0, 704, 100
31696, V, 1, 1, 1, 1, 0, 704, 100
31697, V, 1, 1, 1, 1, 0, 704, 100
31698, V, 1, 1, 1, 1, 0, 704, 100
31699, V, 1, 1, 1, 1, 0, 704, 100
31700, V, 1, 1, 1, 1, 0, 704, 100
31702, V, 1, 1, 1, 1, 0, 704, 100
31703, V, 1, 1, 1, 1, 0, 704, 100
31704, V, 1, 1, 1, 1, 0, 704, 100
31705, V, 1, 1, 1, 1, 0, 704, 100
31706, V, 1, 1, 1, 1, 0, 704, 100
31707, V, 1, 1, 1, 1, 0, 704, 100
31708, V, 1, 1, 1, 1, 0, 704, 100
31709, V, 1, 1, 1, 1, 0, 704, 100
31710, V, 1, 1, 1, 1, 0, 704, 100
31711, V, 1, 1, 1, 1, 0, 704, 100
31712, V, 1, 1, 1, 1, 0, 704, 100
31713, V, 1, 1, 1, 1, 0, 704, 100
31714, V, 1, 1, 1, 1, 0, 704, 100
31715, V, 1, 1, 1, 1, 0, 704, 100
31716, V, 1, 1, 1, 1, 0, 704, 100
31717, V, 1, 1, 1, 1, 0, 704, 100
31718, V, 1, 1, 1, 1, 0, 704, 100
31719, V, 1, 1, 1, 1, 0, 704, 100
31720, V, 1, 1, 1, 1, 0, 704, 100
31721, V, 1, 1, 1, 1, 0, 704, 100
31722, V, 1, 1, 1, 1, 0, 704, 100
31723, V, 1, 1, 1, 1, 0, 704, 100
31724, V, 1, 1, 1, 1, 0, 704, 100
31725, V, 1, 1, 1, 1, 0, 704, 100
31726, V, 1, 1, 1, 1, 0, 704, 100
31727, V, 1, 1, 1, 1, 0, 704, 100
31728, V, 1, 1, 1, 1, 0, 704, 100
31729, V, 1, 1, 1, 1, 0, 704, 100
31730, V, 1, 1, 1, 1, 0, 704, 100
31731, V, 1, 1, 1, 1, 0, 704, 100
31732, V, 1, 1, 1, 1, 0, 704, 100
31733, V, 1, 1, 1, 1, 0, 704, 100
31734, V, 1, 1, 1, 1, 0, 704, 100
31735, V, 1, 1, 1, 1, 0, 704, 100
31736, V, 1, 1, 1, 1, 0, 704, 100
31737, V, 1, 1, 1, 1, 0, 704, 100
31738, V, 1, 1, 1, 1, 0, 704, 100
31739, V, 1, 1, 1, 1, 0, 704, 100
31740, V, 1, 1, 1, 1, 0, 704, 100
31741, V, 1, 1, 1, 1, 0, 704, 100
31742, V, 1, 1, 1, 1, 0, 704, 100
31744, V, 1, 1, 1, 1, 0, 704, 100
31745, V, 1, 1, 1, 1, 0, 704, 100
31746, V, 1, 1, 1, 1, 0, 704, 100
31747, V, 1, 1, 1, 1, 0, 704, 100
31748, V, 1, 1, 1, 1, 0, 704, 100
31749, V, 1, 1, 1, 1, 0, 704, 100
31750, V, 1, 1, 1, 1, 0, 704, 100
31751, V, 1, 1, 1, 1, 0, 704, 100
31752, V, 1, 1, 1, 1, 0, 704, 100
31753, V, 1, 1, 1, 1, 0, 704, 100
31754, V, 1, 1, 1, 1, 0, 704, 100
31755, V, 1, 1, 1, 1, 0, 704, 100
31756, V, 1, 1, 1, 1, 0, 704, 100
31757, V, 1, 1, 1, 1, 0, 704, 100
31758, V, 1, 1, 1, 1, 0, 704, 100
31759, V, 1, 1, 1, 1, 0, 704, 100
31760, V, 1, 1, 1, 1, 0, 704, 100
31761, V, 1, 1, 1, 1, 0, 704, 100
31762, V, 1, 1, 1, 1, 0, 704, 100
31763, V, 1, 1, 1, 1, 0, 704, 100
31764, V, 1, 1, 1, 1, 0, 704, 100
31765, V, 1, 1, 1, 1, 0, 704, 100
31766, V, 1, 1, 1, 1, 0, 704, 100
31767, V, 1, 1, 1, 1, 0, 704, 100
31768, V, 1, 1, 1, 1, 0, 704, 100
31769, V, 1, 1, 1, 1, 0, 704, 100
31770, V, 1, 1, 1, 1, 0, 704, 100
31771, V, 1, 1, 1, 1, 0, 704, 100
31772, V, 1, 1, 1, 1, 0, 704, 100
31773, V, 1, 1, 1, 1, 0, 704, 100
31774, V, 1, 1, 1, 1, 0, 704, 100
31775, V, 1, 1, 1, 1, 0, 704, 100
31776, V, 1, 1, 1, 1, 0, 704, 100
31777, V, 1, 1, 1, 1, 0, 704, 100
31778, V, 1, 1, 1, 1, 0, 704, 100
31779, V, 1, 1, 1, 1, 0, 704, 100
31780, V, 1, 1, 1, 1, 0, 704, 100
31781, V, 1, 1, 1, 1, 0, 704, 100
31782, V, 1, 1, 1, 1, 0, 704, 100
31783, V, 1, 1, 1, 1, 0, 704, 100
31784, V, 1, 1, 1, 1, 0, 704, 100
31785, V, 1, 1, 1, 1, 0, 704, 100
31787, V, 1, 1, 1, 1, 0, 704, 100
31788, V, 1, 1, 1, 1, 0, 704, 100
31789, V, 1, 1, 1, 1, 0, 704, 100
31790, V, 1, 1, 1, 1, 0, 704, 100
31791, V, 1, 1, 1, 1, 0, 704, 100
31792, V, 1, 1, 1, 1, 0, 704, 100
31793, V, 1, 1, 1, 1, 0, 704, 100
31794, V, 1, 1, 1, 1, 0, 704, 100
31795, V, 1, 1, 1, 1, 0, 704, 100
31796, V, 1, 1, 1, 1, 0, 704, 100
31797, V, 1, 1, 1, 1, 0, 704, 100
31798, V, 1, 1, 1, 1, 0, 704, 100
31799, V, 1, 1, 1, 1, 0, 704, 100
31800, V, 1, 1, 1, 1, 0, 704, 100
31801, V, 1, 1, 1, 1, 0, 704, 100
31802, V, 1, 1, 1, 1, 0, 704, 100
31803, V, 1, 1, 1, 1, 0, 704, 100
31804, V, 1, 1, 1, 1, 0, 704, 100
31805, V, 1, 1, 1, 1, 0, 704, 100
31806, V, 1, 1, 1, 1, 0, 704, 100
31807, V, 1, 1, 1, 1, 0, 704, 100
31808, V, 1, 1, 1, 1, 0, 704, 100
31809, V, 1, 1, 1, 1, 0, 704, 100
31810, V, 1, 1, 1, 1, 0, 704, 100
31811, V, 1, 1, 1, 1, 0, 704, 100
31812, V, 1, 1, 1, 1, 0, 704, 100
31813, V, 1, 1, 1, 1, 0, 704, 100
31814, V, 1, 1, 1, 1, 0, 704, 100
31815, V, 1, 1, 1, 1, 0, 704, 100
31816, V, 1, 1, 1, 1, 0, 704, 100
31817, V, 1, 1, 1, 1, 0, 704, 100
31818, V, 1, 1, 1, 1, 0, 704, 100
31819, V, 1, 1, 1, 1, 0, 704, 100
31820, V, 1, 1, 1, 1, 0, 704, 100
31821, V, 1, 1, 1, 1, 0, 704, 100
31822, V, 1, 1, 1, 1, 0, 704, 100
31823, V, 1, 1, 1, 1, 0, 704, 100
31824, V, 1, 1, 1, 1, 0, 704, 100
31825, V, 1, 1, 1, 1, 0, 704, 100
31826, V, 1, 1, 1, 1, 0, 704, 100
31827, V, 1, 1, 1, 1, 0, 704, 100
31828, V, 1, 1, 1, 1, 0, 704, 100
31830, V, 1, 1, 1, 1, 0, 704, 100
31831, V, 1, 1, 1, 1, 0, 704, 100
31832, V, 1, 1, 1, 1, 0, 704, 100
31833, V, 1, 1, 1, 1, 0, 704, 100
31834, V, 1, 1, 1, 1, 0, 704, 100
31835, V, 1, 1, 1, 1, 0, 704, 100
31836, V, 1, 1, 1, 1, 0, 704, 100
31837, V, 1, 1, 1, 1, 0, 704, 100
31838, V, 1, 1, 1, 1, 0, 704, 100
31839, V, 1, 1, 1, 1, 0, 704, 100
31840, V, 1, 1, 1, 1, 0, 704, 100
31841, V, 1, 1, 1, 1, 0, 704, 100
31842, V, 1, 1, 1, 1, 0, 704, 100
31843, V, 1, 1, 1, 1, 0, 704, 100
31844, V, 1, 1, 1, 1, 0, 704, 100
31845, V, 1, 1, 1, 1, 0, 704, 100
31846, V, 1, 1, 1, 1, 0, 704, 100
31847, V, 1, 1, 1, 1, 0, 704, 100
31848, V, 1, 1, 1, 1, 0, 704, 100
31849, V, 1, 1, 1, 1, 0, 704, 100
31850, V, 1, 1, 1, 1, 0, 704, 100
31851, V, 1, 1, 1, 1, 0, 704, 100
31852, V, 1, 1, 1, 1, 0, 704, 100
31853, V, 1, 1, 1, 1, 0, 704, 100
31854, V, 1, 1, 1, 1, 0, 704, 100
31855, V, 1, 1, 1, 1, 0, 704, 100
31856, V, 1, 1, 1, 1, 0, 704, 100
31857, V, 1, 1, 1, 1, 0, 704, 100
31858, V, 1, 1, 1, 1, 0, 704, 100
31859, V, 1, 1, 1, 1, 0, 704, 100
31860, V, 1, 1, 1, 1, 0, 704, 100
31861, V, 1, 1, 1, 1, 0, 704, 100
31862, V, 1, 1, 1, 1, 0, 704, 100
31863, V, 1, 1, 1, 1, 0, 704, 100
31864, V, 1, 1, 1, 1, 0, 704, 100
31865, V, 1, 1, 1, 1, 0, 704, 100
31866, V, 1, 1, 1, 1, 0, 704, 100
31867, V, 1, 1, 1, 1, 0, 704, 100
31868, V, 1, 1, 1, 1, 0, 704, 100
31869, V, 1, 1, 1, 1, 0, 704, 100
31870, V, 1, 1, 1, 1, 0, 704, 100
31872, V, 1, 1, 1, 1, 0, 704, 100
31873, V, 1, 1, 1, 1, 0, 704, 100
31874, V, 1, 1, 1, 1, 0, 704, 100
31875, V, 1, 1, 1, 1, 0, 704, 100
31876, V, 1, 1, 1, 1, 0, 704, 100
31877, V, 1, 1, 1, 1, 0, 704, 100
31878, V, 1, 1, 1, 1, 0, 704, 100
31879, V, 1, 1, 1, 1, 0, 704, 100
31880, V, 1, 1, 1, 1, 0, 704, 100
31881, V, 1, 1, 1, 1, 0, 704, 100
31882, V, 1, 1, 1, 1, 0, 704, 100
31883, V, 1, 1, 1, 1, 0, 704, 100
31884, V, 1, 1, 1, 1, 0, 704, 100
31885, V, 1, 1, 1, 1, 0, 704, 100
31886, V, 1, 1, 1, 1, 0, 704, 100
31887, V, 1, 1, 1, 1, 0, 704, 100
31888, V, 1, 1, 1, 1, 0, 704, 100
31889, V, 1, 1, 1, 1, 0, 704, 100
31890, V, 1, 1, 1, 1, 0, 704, 100
31891, V, 1, 1, 1, 1, 0, 704, 100
31892, V, 1, 1, 1, 1, 0, 704, 100
31893, V, 1, 1, 1, 1, 0, 704, 100
31894, V, 1, 1, 1, 1, 0, 704, 100
31895, V, 1, 1, 1, 1, 0, 704, 100
31896, V, 1, 1, 1, 1, 0, 704, 100
31897, V, 1, 1, 1, 1, 0, 704, 100
31898, V, 1, 1, 1, 1, 0, 704, 100
31899, V, 1, 1, 1, 1, 0, 704, 100
31900, V, 1, 1, 1, 1, 0, 704, 100
31901, V, 1, 1, 1, 1, 0, 704, 100
31902, V, 1, 1, 1, 1, 0, 704, 100
31903, V, 1, 1, 1, 1, 0, 704, 100
31904, V, 1, 1, 1, 1, 0, 704, 100
31905, V, 1, 1, 1, 1, 0, 704, 100
31906, V, 1, 1, 1, 1, 0, 704, 100
31907, V, 1, 1, 1, 1, 0, 704, 100
31908, V, 1, 1, 1, 1, 0, 704, 100
31909, V, 1, 1, 1, 1, 0, 704, 100
31910, V, 1, 1, 1, 1, 0, 704, 100
31911, V, 1, 1, 1, 1, 0, 704, 100
31912, V, 1, 1, 1, 1, 0, 704, 100
31913, V, 1, 1, 1, 1, 0, 704, 100
31915, V, 1, 1, 1, 1, 0, 704, 100
31916, V, 1, 1, 1, 1, 0, 704, 100
31917, V, 1, 1, 1, 1, 0, 704, 100
31918, V, 1, 1, 1, 1, 0, 704, 100
31919, V, 1, 1, 1, 1, 0, 704, 100
31920, V, 1, 1, 1, 1, 0, 704, 100
31921, V, 1, 1, 1, 1, 0, 704, 100
31922, V, 1, 1, 1, 1, 0, 704, 100
31923, V, 1, 1, 1, 1, 0, 704, 100
31924, V, 1, 1, 1, 1, 0, 704, 100
31925, V, 1, 1, 1, 1, 0, 704, 100
31926, V, 1, 1, 1, 1, 0, 704, 100
31927, V, 1, 1, 1, 1, 0, 704, 100
31928, V, 1, 1, 1, 1, 0, 704, 100
31929, V, 1, 1, 1, 1, 0, 704, 100
31930, V, 1, 1, 1, 1, 0, 704, 100
31931, V, 1, 1, 1, 1, 0, 704, 100
31932, V, 1, 1, 1, 1, 0, 704, 100
31933, V, 1, 1, 1, 1, 0, 704, 100
31934, V, 1, 1, 1, 1, 0, 704, 100
31935, V, 1, 1, 1, 1, 0, 704, 100
31936, V, 1, 1, 1, 1, 0, 704, 100
31937, V, 1, 1, 1, 1, 0, 704, 100
31938, V, 1, 1, 1, 1, 0, 704, 100
31939, V, 1, 1, 1, 1, 0, 704, 100
31940, V, 1, 1, 1, 1, 0, 704, 100
31941, V, 1, 1, 1, 1, 0, 704, 100
31942, V, 1, 1, 1, 1, 0, 704, 100
31943, V, 1, 1, 1, 1, 0, 704, 100
31944, V, 1, 1, 1, 1, 0, 704, 100
31945, V, 1, 1, 1, 1, 0, 704, 100
31946, V, 1, 1, 1, 1, 0, 704, 100
31947, V, 1, 1, 1, 1, 0, 704, 100
31948, V, 1, 1, 1, 1, 0, 704, 100
31949, V, 1, 1, 1, 1, 0, 704, 100
31950, V, 1, 1, 1, 1, 0, 704, 100
31951, V, 1, 1, 1, 1, 0, 704, 100
31952, V, 1, 1, 1, 1, 0, 704, 100
31953, V, 1, 1, 1, 1, 0, 704, 100
31954, V, 1, 1, 1, 1, 0, 704, 100
31955, V, 1, 1, 1, 1, 0, 704, 100
31956, V, 1, 1, 1, 1, 0, 704, 100
31958, V, 1, 1, 1, 1, 0, 704, 100
31959, V, 1, 1, 1, 1, 0, 704, 100
31960, V, 1, 1, 1, 1, 0, 704, 100
31961, V, 1, 1, 1, 1, 0, 704, 100
31962, V, 1, 1, 1, 1, 0, 704, 100
31963, V, 1, 1, 1, 1, 0, 704, 100
31964, V, 1, 1, 1, 1, 0, 704, 100
31965, V, 1, 1, 1, 1, 0, 704, 100
31966, V, 1, 1, 1, 1, 0, 704, 100
31967, V, 1, 1, 1, 1, 0, 704, 100
31968, V, 1, 1, 1, 1, 0, 704, 100
31969, V, 1, 1, 1, 1, 0, 704, 100
31970, V, 1, 1, 1, 1, 0, 704, 100
31971, V, 1, 1, 1, 1, 0, 704, 100
31972, V, 1, 1, 1, 1, 0, 704, 100
31973, V, 1, 1, 1, 1, 0, 704, 100
31974, V, 1, 1, 1, 1, 0, 704, 100
31975, V, 1, 1, 1, 1, 0, 704, 100
31976, V, 1, 1, 1, 1, 0, 704, 100
31977, V, 1, 1, 1, 1, 0, 704, 100
31978, V, 1, 1, 1, 1, 0, 704, 100
31979, V, 1, 1, 1, 1, 0, 704, 100
31980, V, 1, 1, 1, 1, 0, 704, 100
31981, V, 1, 1, 1, 1, 0, 704, 100
31982, V, 1, 1, 1, 1, 0, 704, 100
31983, V, 1, 1, 1, 1, 0, 704, 100
31984, V, 1, 1, 1, 1, 0, 704, 100
31985, V, 1, 1, 1, 1, 0, 704, 100
31986, V, 1, 1, 1, 1, 0, 704, 100
31987, V, 1, 1, 1, 1, 0, 704, 100
31988, V, 1, 1, 1, 1, 0, 704, 100
31989, V, 1, 1, 1, 1, 0, 704, 100
31990, V, 1, 1, 1, 1, 0, 704, 100
31991, V, 1, 1, 1, 1, 0, 704, 100
31992, V, 1, 1, 1, 1, 0, 704, 100
31993, V, 1, 1, 1, 1, 0, 704, 100
31994, V, 1, 1, 1, 1, 0, 704, 100
31995, V, 1, 1, 1, 1, 0, 704, 100
31996, V, 1, 1, 1, 1, 0, 704, 100
31997, V, 1, 1, 1, 1, 0, 704, 100
31998, V, 1, 1, 1, 1, 0, 704, 100
32000, V, 1, 1, 1, 1, 0, 704, 100
32001, V, 1, 1, 1, 1, 0, 704, 100
32002, V, 1, 1, 1, 1, 0, 704, 100
32003, V, 1, 1, 1, 1, 0, 704, 100
32004, V, 1, 1, 1, 1, 0, 704, 100
32005, V, 1, 1, 1, 1, 0, 704, 100
32006, V, 1, 1, 1, 1, 0, 704, 100
32007, V, 1, 1, 1, 1, 0, 704, 100
32008, V, 1, 1, 1, 1, 0, 704, 100
32009, V, 1, 1, 1, 1, 0, 704, 100
32010, V, 1, 1, 1, 1, 0, 704, 100
32011, V, 1, 1, 1, 1, 0, 704, 100
32012, V, 1, 1, 1, 1, 0, 704, 100
32013, V, 1, 1, 1, 1, 0, 704, 100
32014, V, 1, 1, 1, 1, 0, 704, 100
32015, V, 1, 1, 1, 1, 0, 704, 100
32016, V, 1, 1, 1, 1, 0, 704, 100
32017, V, 1, 1, 1, 1, 0, 704, 100
32018, V, 1, 1, 1, 1, 0, 704, 100
32019, V, 1, 1, 1, 1, 0, 704, 100
32020, V, 1, 1, 1, 1, 0, 704, 100
32021, V, 1, 1, 1, 1, 0, 704, 100
32022, V, 1, 1, 1, 1, 0, 704, 100
32023, V, 1, 1, 1, 1, 0, 704, 100
32024, V, 1, 1, 1, 1, 0, 704, 100
32025, V, 1, 1, 1, 1, 0, 704, 100
32026, V, 1, 1, 1, 1, 0, 704, 100
32027, V, 1, 1, 1, 1, 0, 704, 100
32028, V, 1, 1, 1, 1, 0, 704, 100
32029, V, 1, 1, 1, 1, 0, 704, 100
32030, V, 1, 1, 1, 1, 0, 704, 100
32031, V, 1, 1, 1, 1, 0, 704, 100
32032, V, 1, 1, 1, 1, 0, 704, 100
32033, V, 1, 1, 1, 1, 0, 704, 100
32034, V, 1, 1, 1, 1, 0, 704, 100
32035, V, 1, 1, 1, 1, 0, 704, 100
32036, V, 1, 1, 1, 1, 0, 704, 100
32037, V, 1, 1, 1, 1, 0, 704, 100
32038, V, 1, 1, 1, 1, 0, 704, 100
32039, V, 1, 1, 1, 1, 0, 704, 100
32040, V, 1, 1, 1, 1, 0, 704, 100
32041, V, 1, 1, 1, 1, 0, 704, 100
32043, V, 1, 1, 1, 1, 0, 704, 100
32044, V, 1, 1, 1, 1, 0, 704, 100
32045, V, 1, 1, 1, 1, 0, 704, 100
32046, V, 1, 1, 1, 1, 0, 704, 100
32047, V, 1, 1, 1, 1, 0, 704, 100
32048, V, 1, 1, 1, 1, 0, 704, 100
32049, V, 1, 1, 1, 1, 0, 704, 100
32050, V, 1, 1, 1, 1, 0, 704, 100
32051, V, 1, 1, 1, 1, 0, 704, 100
32052, V, 1, 1, 1, 1, 0, 704, 100
32053, V, 1, 1, 1, 1, 0, 704, 100
32054, V, 1, 1, 1, 1, 0, 704, 100
32055, V, 1, 1, 1, 1, 0, 704, 100
32056, V, 1, 1, 1, 1, 0, 704, 100
32057, V, 1, 1, 1, 1, 0, 704, 100
32058, V, 1, 1, 1, 1, 0, 704, 100
32059, V, 1, 1, 1, 1, 0, 704, 100
32060, V, 1, 0, 0, 1, 0, 704, 100
32060, V, 1, 0, 0, 0, 0, 704, 100
32061, V, 1, 1, 0, 0, 0, 704, 100
32061, V, 1, 1, 0, 0, 0, 704, 100
32062, V, 1, 1, 1, 1, 0, 704, 100
32063, V, 1, 1, 1, 1, 0, 704, 100
32064, V, 1, 1, 1, 1, 0, 704, 100
32065, V, 1, 1, 1, 1, 0, 704, 100
32066, V, 1, 1, 1, 1, 0, 704, 100
32067, V, 1, 1, 1, 1, 0, 704, 99
32068, V, 1, 1, 1, 1, 0, 704, 99
32069, V, 1, 1, 1, 1, 0, 704, 99
32070, V, 1, 1, 1, 1, 0, 704, 99
32071, V, 1, 1, 1, 1, 0, 704, 99
32072, V, 1, 1, 1, 1, 0, 704, 99
32073, V, 1, 1, 1, 1, 0, 704, 99
32074, V, 1, 1, 1, 1, 0, 704, 99
32075, V, 1, 1, 1, 1, 0, 704, 99
32076, V, 1, 1, 1, 1, 0, 704, 99
32077, V, 1, 1, 1, 1, 0, 704, 99
32078, V, 1, 1, 1, 1, 0, 704, 99
32079, V, 1, 1, 1, 1, 0, 704, 99
32080, V, 1, 1, 1, 1, 0, 704, 99
32081, V, 1, 1, 1, 1, 0, 704, 99
32082, V, 1, 1, 1, 1, 0, 704, 99
32083, V, 1, 1, 1, 1, 0, 704, 99
32084, V, 1, 1, 1, 1, 0, 704, 99
32086, V, 1, 1, 1, 1, 0, 704, 99
32087, V, 1, 1, 1, 1, 0, 704, 99
32088, V, 1, 1, 1, 1, 0, 704, 99
32089, V, 1, 1, 1, 1, 0, 704, 99
32090, V, 1, 1, 1, 1, 0, 704, 99
32091, V, 1, 1, 1, 1, 0, 704, 100
32092, V, 1, 1, 1, 1, 0, 704, 100
32093, V, 1, 1, 1, 1, 0, 704, 100
32094, V, 1, 1, 1, 1, 0, 704, 100
32095, V, 1, 1, 1, 1, 0, 704, 100
32096, V, 1, 1, 1, 1, 0, 704, 100
32097, V, 1, 1, 1, 1, 0, 704, 100
32098, V, 1, 1, 1, 1, 0, 704, 100
32099, V, 1, 1, 1, 1, 0, 704, 100
32100, V, 1, 1, 1, 1, 0, 704, 100
32101, V, 1, 1, 1, 1, 0, 704, 100
32102, V, 1, 1, 1, 1, 0, 704, 100
32103, V, 1, 1, 1, 1, 0, 704, 100
32104, V, 1, 1, 1, 1, 0, 704, 100
32105, V, 1, 1, 1, 1, 0, 704, 100
32106, V, 1, 1, 1, 1, 0, 704, 100
32107, V, 1, 1, 1, 1, 0, 704, 100
32108, V, 1, 1, 1, 1, 0, 704, 100
32109, V, 1, 1, 1, 1, 0, 704, 100
32110, V, 1, 1, 1, 1, 0, 704, 100
32111, V, 1, 1, 1, 1, 0, 704, 100
32112, V, 1, 1, 1, 1, 0, 704, 100
32113, V, 1, 1, 1, 1, 0, 704, 100
32114, V, 1, 1, 1, 1, 0, 704, 100
32115, V, 1, 1, 1, 1, 0, 704, 100
32116, V, 1, 1, 1, 1, 0, 704, 100
32117, V, 1, 1, 1, 1, 0, 704, 100
32118, V, 1, 1, 1, 1, 0, 704, 100
32119, V, 1, 1, 1, 1, 0, 704, 100
32120, V, 1, 1, 1, 1, 0, 704, 100
32121, V, 1, 1, 1, 1, 0, 704, 100
32122, V, 1, 1, 1, 1, 0, 704, 100
32123, V, 1, 1, 1, 1, 0, 704, 100
32124, V, 1, 1, 1, 1, 0, 704, 100
32125, V, 1, 1, 1, 1, 0, 704, 100
32126, V, 1, 1, 1, 1, 0, 704, 100
32128, V, 1, 1, 1, 1, 0, 704, 100
32129, V, 1, 1, 1, 1, 0, 704, 100
32130, V, 1, 1, 1, 1, 0, 704, 100
32131, V, 1, 1, 1, 1, 0, 704, 100
32132, V, 1, 1, 1, 1, 0, 704, 100
32133, V, 1, 1, 1, 1, 0, 704, 100
32134, V, 1, 1, 1, 1, 0, 704, 100
32135, V, 1, 1, 1, 1, 0, 704, 100
32136, V, 1, 1, 1, 1, 0, 704, 100
32137, V, 1, 1, 1, 1, 0, 704, 100
32138, V, 1, 1, 1, 1, 0, 704, 100
32139, V, 1, 1, 1, 1, 0, 704, 100
32140, V, 1, 1, 1, 1, 0, 704, 100
32141, V, 1, 1, 1, 1, 0, 704, 100
32142, V, 1, 1, 1, 1, 0, 704, 100
32143, V, 1, 1, 1, 1, 0, 704, 100
32144, V, 1, 1, 1, 1, 0, 704, 100
32145, V, 1, 1, 1, 1, 0, 704, 100
32146, V, 1, 1, 1, 1, 0, 704, 100
32147, V, 1, 1, 1, 1, 0, 704, 100
32148, V, 1, 1, 1, 1, 0, 704, 100
32149, V, 1, 1, 1, 1, 0, 704, 100
32150, V, 1, 1, 1, 1, 0, 704, 100
32151, V, 1, 1, 1, 1, 0, 704, 100
32152, V, 1, 1, 1, 1, 0, 704, 100
32153, V, 1, 1, 1, 1, 0, 704, 100
32154, V, 1, 1, 1, 1, 0, 704, 100
32155, V, 1, 1, 1, 1, 0, 704, 100
32156, V, 1, 1, 1, 1, 0, 704, 100
32157, V, 1, 1, 1, 1, 0, 704, 100
32158, V, 1, 1, 1, 1, 0, 704, 100
32159, V, 1, 1, 1, 1, 0, 704, 100
32160, V, 1, 1, 1, 1, 0, 704, 100
32161, V, 1, 1, 1, 1, 0, 704, 100
32162, V, 1, 1, 1, 1, 0, 704, 100
32163, V, 1, 1, 1, 1, 0, 704, 100
32164, V, 1, 1, 1, 1, 0, 704, 100
32165, V, 1, 1, 1, 1, 0, 704, 100
32166, V, 1, 1, 1, 1, 0, 704, 100
32167, V, 1, 1, 1, 1, 0, 704, 100
32168, V, 1, 1, 1, 1, 0, 704, 100
32169, V, 1, 1, 1, 1, 0, 704, 100
32171, V, 1, 1, 1, 1, 0, 704, 100
32172, V, 1, 1, 1, 1, 0, 704, 100
32173, V, 1, 1, 1, 1, 0, 704, 100
32174, V, 1, 1, 1, 1, 0, 704, 100
32175, V, 1, 1, 1, 1, 0, 704, 100
32176, V, 1, 1, 1, 1, 0, 704, 100
32177, V, 1, 1, 1, 1, 0, 704, 100
32178, V, 1, 1, 1, 1, 0, 704, 100
32179, V, 1, 1, 1, 1, 0, 704, 100
32180, V, 1, 1, 1, 1, 0, 704, 100
32181, V, 1, 1, 1, 1, 0, 704, 100
32182, V, 1, 1, 1, 1, 0, 704, 100
32183, V, 1, 1, 1, 1, 0, 704, 100
32184, V, 1, 1, 1, 1, 0, 704, 100
32185, V, 1, 1, 1, 1, 0, 704, 100
32186, V, 1, 1, 1, 1, 0, 704, 100
32187, V, 1, 1, 1, 1, 0, 704, 100
32188, V, 1, 1, 1, 1, 0, 704, 100
32189, V, 1, 1, 1, 1, 0, 704, 100
32190, V, 1, 1, 1, 1, 0, 704, 100
32191, V, 1, 1, 1, 1, 0, 704, 100
32192, V, 1, 1, 1, 1, 0, 704, 100
32193, V, 1, 1, 1, 1, 0, 704, 100
32194, V, 1, 1, 1, 1, 0, 704, 100
32195, V, 1, 1, 1, 1, 0, 704, 100
32196, V, 1, 1, 1, 1, 0, 704, 100
32197, V, 1, 1, 1, 1, 0, 704, 100
32198, V, 1, 1, 1, 1, 0, 704, 100
32199, V, 1, 1, 1, 1, 0, 704, 100
32200, V, 1, 1, 1, 1, 0, 704, 100
32201, V, 1, 1, 1, 1, 0, 704, 100
32202, V, 1, 1, 1, 1, 0, 704, 100
32203, V, 1, 1, 1, 1, 0, 704, 100
32204, V, 1, 1, 1, 1, 0, 704, 100
32205, V, 1, 1, 1, 1, 0, 704, 100
32206, V, 1, 1, 1, 1, 0, 704, 100
32207, V, 1, 1, 1, 1, 0, 704, 100
32208, V, 1, 1, 1, 1, 0, 704, 100
32209, V, 1, 1, 1, 1, 0, 704, 100
32210, V, 1, 1, 1, 1, 0, 704, 100
32211, V, 1, 1, 1, 1, 0, 704, 100
32212, V, 1, 1, 1, 1, 0, 704, 100
32214, V, 1, 1, 1, 1, 0, 704, 100
32215, V, 1, 1, 1, 1, 0, 704, 100
32216, V, 1, 1, 1, 1, 0, 704, 100
32217, V, 1, 1, 1, 1, 0, 704, 100
32218, V, 1, 1, 1, 1, 0, 704, 100
32219, V, 1, 1, 1, 1, 0, 704, 100
32220, V, 1, 1, 1, 1, 0, 704, 100
32221, V, 1, 1, 1, 1, 0, 704, 100
32222, V, 1, 1, 1, 1, 0, 704, 100
32223, V, 1, 1, 1, 1, 0, 704, 100
32224, V, 1, 1, 1, 1, 0, 704, 100
32225, V, 1, 1, 1, 1, 0, 704, 100
32226, V, 1, 1, 1, 1, 0, 704, 100
32227, V, 1, 1, 1, 1, 0, 704, 100
32228, V, 1, 1, 1, 1, 0, 704, 100
32229, V, 1, 1, 1, 1, 0, 704, 100
32230, V, 1, 1, 1, 1, 0, 704, 100
32231, V, 1, 1, 1, 1, 0, 704, 100
32232, V, 1, 1, 1, 1, 0, 704, 100
32233, V, 1, 1, 1, 1, 0, 704, 100
32234, V, 1, 1, 1, 1, 0, 704, 100
32235, V, 1, 1, 1, 1, 0, 704, 100
32236, V, 1, 1, 1, 1, 0, 704, 100
32237, V, 1, 1, 1, 1, 0, 704, 100
32238, V, 1, 1, 1, 1, 0, 704, 100
32239, V, 1, 1, 1, 1, 0, 704, 100
32240, V, 1, 1, 1, 1, 0, 704, 100
32241, V, 1, 1, 1, 1, 0, 704, 100
32242, V, 1, 1, 1, 1, 0, 704, 100
32243, V, 1, 1, 1, 1, 0, 704, 100
32244, V, 1, 1, 1, 1, 0, 704, 100
32245, V, 1, 1, 1, 1, 0, 704, 100
32246, V, 1, 1, 1, 1, 0, 704, 100
32247, V, 1, 1, 1, 1, 0, 704, 100
32248, V, 1, 1, 1, 1, 0, 704, 100
32249, V, 1, 1, 1, 1, 0, 704, 100
32250, V, 1, 1, 1, 1, 0, 704, 100
32251, V, 1, 1, 1, 1, 0, 704, 100
32252, V, 1, 1, 1, 1, 0, 704, 100
32253, V, 1, 1, 1, 1, 0, 704, 100
32254, V, 1, 1, 1, 1, 0, 704, 100
32256, V, 1, 1, 1, 1, 0, 704, 100
32257, V, 1, 1, 1, 1, 0, 704, 100
32258, V, 1, 1, 1, 1, 0, 704, 100
32259, V, 1, 1, 1, 1, 0, 704, 100
32260, V, 1, 1, 1, 1, 0, 704, 100
32261, V, 1, 1, 1, 1, 0, 704, 100
32262, V, 1, 1, 1, 1, 0, 704, 100
32263, V, 1, 1, 1, 1, 0, 704, 100
32264, V, 1, 1, 1, 1, 0, 704, 100
32265, V, 1, 1, 1, 1, 0, 704, 100
32266, V, 1, 1, 1, 1, 0, 704, 100
32267, V, 1, 1, 1, 1, 0, 704, 100
32268, V, 1, 1, 1, 1, 0, 704, 100
32269, V, 1, 1, 1, 1, 0, 704, 100
32270, V, 1, 1, 1, 1, 0, 704, 100
32271, V, 1, 1, 1, 1, 0, 704, 100
32272, V, 1, 1, 1, 1, 0, 704, 100
32273, V, 1, 1, 1, 1, 0, 704, 100
32274, V, 1, 1, 1, 1, 0, 704, 100
32275, V, 1, 1, 1, 1, 0, 704, 100
32276, V, 1, 1, 1, 1, 0, 704, 100
32277, V, 1, 1, 1, 1, 0, 704, 100
32278, V, 1, 1, 1, 1, 0, 704, 100
32279, V, 1, 1, 1, 1, 0, 704, 100
32280, V, 1, 1, 1, 1, 0, 704, 100
32281, V, 1, 1, 1, 1, 0, 704, 100
32282, V, 1, 1, 1, 1, 0, 704, 100
32283, V, 1, 1, 1, 1, 0, 704, 100
32284, V, 1, 1, 1, 1, 0, 704, 100
32285, V, 1, 1, 1, 1, 0, 704, 100
32286, V, 1, 1, 1, 1, 0, 704, 100
32287, V, 1, 1, 1, 1, 0, 704, 100
32288, V, 1, 1, 1, 1, 0, 704, 100
32289, V, 1, 1, 1, 1, 0, 704, 100
32290, V, 1, 1, 1, 1, 0, 704, 100
32291, V, 1, 1, 1, 1, 0, 704, 100
32292, V, 1, 1, 1, 1, 0, 704, 100
32293, V, 1, 1, 1, 1, 0, 704, 100
32294, V, 1, 1, 1, 1, 0, 704, 100
32295, V, 1, 1, 1, 1, 0, 704, 100
32296, V, 1, 1, 1, 1, 0, 704, 100
32297, V, 1, 1, 1, 1, 0, 704, 100
32299, V, 1, 1, 1, 1, 0, 704, 100
32300, V, 1, 1, 1, 1, 0, 704, 100
32301, V, 1, 1, 1, 1, 0, 704, 100
32302, V, 1, 1, 1, 1, 0, 704, 100
32303, V, 1, 1, 1, 1, 0, 704, 100
32304, V, 1, 1, 1, 1, 0, 704, 100
32305, V, 1, 1, 1, 1, 0, 704, 100
32306, V, 1, 1, 1, 1, 0, 704, 100
32307, V, 1, 1, 1, 1, 0, 704, 100
32308, V, 1, 1, 1, 1, 0, 704, 100
32309, V, 1, 1, 1, 1, 0, 704, 100
32310, V, 1, 1, 1, 1, 0, 704, 100
32311, V, 1, 1, 1, 1, 0, 704, 100
32312, V, 1, 1, 1, 1, 0, 704, 100
32313, V, 1, 1, 1, 1, 0, 704, 100
32314, V, 1, 1, 1, 1, 0, 704, 100
32315, V, 1, 1, 1, 1, 0, 704, 100
32316, V, 1, 1, 1, 1, 0, 704, 100
32317, V, 1, 1, 1, 1, 0, 704, 100
32318, V, 1, 1, 1, 1, 0, 704, 100
32319, V, 1, 1, 1, 1, 0, 704, 100
32320, V, 1, 1, 1, 1, 0, 704, 100
32321, V, 1, 1, 1, 1, 0, 704, 100
32322, V, 1, 1, 1, 1, 0, 704, 100
32323, V, 1, 1, 1, 1, 0, 704, 100
32324, V, 1, 1, 1, 1, 0, 704, 100
32325, V, 1, 1, 1, 1, 0, 704, 100
32326, V, 1, 1, 1, 1, 0, 704, 100
32327, V, 1, 1, 1, 1, 0, 704, 100
32328, V, 1, 1, 1, 1, 0, 704, 100
32329, V, 1, 1, 1, 1, 0, 704, 100
32330, V, 1, 1, 1, 1, 0, 704, 100
32331, V, 1, 1, 1, 1, 0, 704, 100
32332, V, 1, 1, 1, 1, 0, 704, 100
32333, V, 1, 1, 1, 1, 0, 704, 100
32334, V, 1, 1, 1, 1, 0, 704, 100
32335, V, 1, 1, 1, 1, 0, 704, 100
32336, V, 1, 1, 1, 1, 0, 704, 100
32337, V, 1, 1, 1, 1, 0, 704, 100
32338, V, 1, 1, 1, 1, 0, 704, 100
32339, V, 1, 1, 1, 1, 0, 704, 100
32340, V, 1, 1, 1, 1, 0, 704, 100
32342, V, 1, 1, 1, 1, 0, 704, 100
32343, V, 1, 1, 1, 1, 0, 704, 100
32344, V, 1, 1, 1, 1, 0, 704, 100
32345, V, 1, 1, 1, 1, 0, 704, 100
32346, V, 1, 1, 1, 1, 0, 704, 100
32347, V, 1, 1, 1, 1, 0, 704, 100
32348, V, 1, 1, 1, 1, 0, 704, 100
32349, V, 1, 1, 1, 1, 0, 704, 100
32350, V, 1, 1, 1, 1, 0, 704, 100
32351, V, 1, 1, 1, 1, 0, 704, 100
32352, V, 1, 1, 1, 1, 0, 704, 100
32353, V, 1, 1, 1, 1, 0, 704, 100
32354, V, 1, 1, 1, 1, 0, 704, 100
32355, V, 1, 1, 1, 1, 0, 704, 100
32356, V, 1, 1, 1, 1, 0, 704, 100
32357, V, 1, 1, 1, 1, 0, 704, 100
32358, V, 1, 1, 1, 1, 0, 704, 100
32359, V, 1, 1, 1, 1, 0, 704, 100
32360, V, 1, 1, 1, 1, 0, 704, 100
32361, V, 1, 1, 1, 1, 0, 704, 100
32362, V, 1, 1, 1, 1, 0, 704, 100
32363, V, 1, 1, 1, 1, 0, 704, 100
32364, V, 1, 1, 1, 1, 0, 704, 100
32365, V, 1, 1, 1, 1, 0, 704, 100
32366, V, 1, 1, 1, 1, 0, 704, 100
32367, V, 1, 1, 1, 1, 0, 704, 100
32368, V, 1, 1, 1, 1, 0, 704, 100
32369, V, 1, 1, 1, 1, 0, 704, 100
32370, V, 1, 1, 1, 1, 0, 704, 100
32371, V, 1, 1, 1, 1, 0, 704, 100
32372, V, 1, 1, 1, 1, 0, 704, 100
32373, V, 1, 1, 1, 1, 0, 704, 100
32374, V, 1, 1, 1, 1, 0, 704, 100
32375, V, 1, 1, 1, 1, 0, 704, 100
32376, V, 1, 1, 1, 1, 0, 704, 100
32377, V, 1, 1, 1, 1, 0, 704, 100
32378, V, 1, 1, 1, 1, 0, 704, 100
32379, V, 1, 1, 1, 1, 0, 704, 100
32380, V, 1, 1, 1, 1, 0, 704, 100
32381, V, 1, 1, 1, 1, 0, 704, 100
32382, V, 1, 1, 1, 1, 0, 704, 100
32384, V, 1, 1, 1, 1, 0, 704, 100
32385, V, 1, 1, 1, 1, 0, 704, 100
32386, V, 1, 1, 1, 1, 0, 704, 100
32387, V, 1, 1, 1, 1, 0, 704, 100
32388, V, 1, 1, 1, 1, 0, 704, 100
32389, V, 1, 1, 1, 1, 0, 704, 100
32390, V, 1, 1, 1, 1, 0, 704, 100
32391, V, 1, 1, 1, 1, 0, 704, 100
32392, V, 1, 1, 1, 1, 0, 704, 100
32393, V, 1, 1, 1, 1, 0, 704, 100
32394, V, 1, 1, 1, 1, 0, 704, 100
32395, V, 1, 1, 1, 1, 0, 704, 100
32396, V, 1, 1, 1, 1, 0, 704, 100
32397, V, 1, 1, 1, 1, 0, 704, 100
32398, V, 1, 1, 1, 1, 0, 704, 100
32399, V, 1, 1, 1, 1, 0, 704, 100
32400, V, 1, 1, 1, 1, 0, 704, 100
32401, V, 1, 1, 1, 1, 0, 704, 100
32402, V, 1, 1, 1, 1, 0, 704, 100
32403, V, 1, 1, 1, 1, 0, 704, 100
32404, V, 1, 1, 1, 1, 0, 704, 100
32405, V, 1, 1, 1, 1, 0, 704, 100
32406, V, 1, 1, 1, 1, 0, 704, 100
32407, V, 1, 1, 1, 1, 0, 704, 100
32408, V, 1, 1, 1, 1, 0, 704, 100
32409, V, 1, 1, 1, 1, 0, 704, 100
32410, V, 1, 1, 1, 1, 0, 704, 100
32411, V, 1, 1, 1, 1, 0, 704, 100
32412, V, 1, 1, 1, 1, 0, 704, 100
32413, V, 1, 1, 1, 1, 0, 704, 100
32414, V, 1, 1, 1, 1, 0, 704, 100
32415, V, 1, 1, 1, 1, 0, 704, 100
32416, V, 1, 1, 1, 1, 0, 704, 100
32417, V, 1, 1, 1, 1, 0, 704, 100
32418, V, 1, 1, 1, 1, 0, 704, 100
32419, V, 1, 1, 1, 1, 0, 704, 100
32420, V, 1, 1, 1, 1, 0, 704, 100
32421, V, 1, 1, 1, 1, 0, 704, 100
32422, V, 1, 1, 1, 1, 0, 704, 100
32423, V, 1, 1, 1, 1, 0, 704, 100
32424, V, 1, 1, 1, 1, 0, 704, 100
32425, V, 1, 1, 1, 1, 0, 704, 100
32427, V, 1, 1, 1, 1, 0, 704, 100
32428, V, 1, 1, 1, 1, 0, 704, 100
32429, V, 1, 1, 1, 1, 0, 704, 100
32430, V, 1, 1, 1, 1, 0, 704, 100
32431, V, 1, 1, 1, 1, 0, 704, 100
32432, V, 1, 1, 1, 1, 0, 704, 100
32433, V, 1, 1, 1, 1, 0, 704, 100
32434, V, 1, 1, 1, 1, 0, 704, 100
32435, V, 1, 1, 1, 1, 0, 704, 100
32436, V, 1, 1, 1, 1, 0, 704, 100
32437, V, 1, 1, 1, 1, 0, 704, 100
32438, V, 1, 1, 1, 1, 0, 704, 100
32439, V, 1, 1, 1, 1, 0, 704, 100
32440, V, 1, 1, 1, 1, 0, 704, 100
32441, V, 1, 1, 1, 1, 0, 704, 100
32442, V, 1, 1, 1, 1, 0, 704, 100
32443, V, 1, 1, 1, 1, 0, 704, 100
32444, V, 1, 1, 1, 1, 0, 704, 100
32445, V, 1, 1, 1, 1, 0, 704, 100
32446, V, 1, 1, 1, 1, 0, 704, 100
32447, V, 1, 1, 1, 1, 0, 704, 100
32448, V, 1, 1, 1, 1, 0, 704, 100
32449, V, 1, 1, 1, 1, 0, 704, 100
32450, V, 1, 1, 1, 1, 0, 704, 100
32451, V, 1, 1, 1, 1, 0, 704, 100
32452, V, 1, 1, 1, 1, 0, 704, 100
32453, V, 1, 1, 1, 1, 0, 704, 100
32454, V, 1, 1, 1, 1, 0, 704, 100
32455, V, 1, 1, 1, 1, 0, 704, 100
32456, V, 1, 1, 1, 1, 0, 704, 100
32457, V, 1, 1, 1, 1, 0, 704, 100
32458, V, 1, 1, 1, 1, 0, 704, 100
32459, V, 1, 1, 1, 1, 0, 704, 100
32460, V, 1, 1, 1, 1, 0, 704, 100
32461, V, 1, 1, 1, 1, 0, 704, 100
32462, V, 1, 1, 1, 1, 0, 704, 100
32463, V, 1, 1, 1, 1, 0, 704, 100
32464, V, 1, 1, 1, 1, 0, 704, 100
32465, V, 1, 1, 1, 1, 0, 704, 100
32466, V, 1, 1, 1, 1, 0, 704, 100
32467, V, 1, 1, 1, 1, 0, 704, 100
32468, V, 1, 1, 1, 1, 0, 704, 100
32470, V, 1, 1, 1, 1, 0, 704, 100
32471, V, 1, 1, 1, 1, 0, 704, 100
32472, V, 1, 1, 1, 1, 0, 704, 100
32473, V, 1, 1, 1, 1, 0, 704, 100
32474, V, 1, 1, 1, 1, 0, 704, 100
32475, V, 1, 1, 1, 1, 0, 704, 100
32476, V, 1, 1, 1, 1, 0, 704, 100
32477, V, 1, 1, 1, 1, 0, 704, 100
32478, V, 1, 1, 1, 1, 0, 704, 100
32479, V, 1, 1, 1, 1, 0, 704, 100
32480, V, 1, 1, 1, 1, 0, 704, 100
32481, V, 1, 1, 1, 1, 0, 704, 100
32482, V, 1, 1, 1, 1, 0, 704, 100
32483, V, 1, 1, 1, 1, 0, 704, 100
32484, V, 1, 1, 1, 1, 0, 704, 100
32485, V, 1, 1, 1, 1, 0, 704, 100
32486, V, 1, 1, 1, 1, 0, 704, 100
32487, V, 1, 1, 1, 1, 0, 704, 100
32488, V, 1, 1, 1, 1, 0, 704, 100
32489, V, 1, 1, 1, 1, 0, 704, 100
32490, V, 1, 1, 1, 1, 0, 704, 100
32491, V, 1, 1, 1, 1, 0, 704, 100
32492, V, 1, 1, 1, 1, 0, 704, 100
32493, V, 1, 1, 1, 1, 0, 704, 100
32494, V, 1, 1, 1, 1, 0, 704, 100
32495, V, 1, 1, 1, 1, 0, 704, 100
32496, V, 1, 1, 1, 1, 0, 704, 100
32497, V, 1, 1, 1, 1, 0, 704, 100
32498, V, 1, 1, 1, 1, 0, 704, 100
32499, V, 1, 1, 1, 1, 0, 704, 100
32500, V, 1, 1, 1, 1, 0, 704, 100
32501, V, 1, 1, 1, 1, 0, 704, 100
32502, V, 1, 1, 1, 1, 0, 704, 100
32503, V, 1, 1, 1, 1, 0, 704, 100
32504, V, 1, 1, 1, 1, 0, 704, 100
32505, V, 1, 1, 1, 1, 0, 704, 100
32506, V, 1, 1, 1, 1, 0, 704, 100
32507, V, 1, 1, 1, 1, 0, 704, 100
32508, V, 1, 1, 1, 1, 0, 704, 100
32509, V, 1, 1, 1, 1, 0, 704, 100
32510, V, 1, 1, 1, 1, 0, 704, 100
32512, V, 1, 1, 1, 1, 0, 704, 100
32513, V, 1, 1, 1, 1, 0, 704, 100
32514, V, 1, 1, 1, 1, 0, 704, 100
32515, V, 1, 1, 1, 1, 0, 704, 100
32516, V, 1, 1, 1, 1, 0, 704, 100
32517, V, 1, 1, 1, 1, 0, 704, 100
32518, V, 1, 1, 1, 1, 0, 704, 100
32519, V, 1, 1, 1, 1, 0, 704, 100
32520, V, 1, 1, 1, 1, 0, 704, 100
32521, V, 1, 1, 1, 1, 0, 704, 100
32522, V, 1, 1, 1, 1, 0, 704, 100
32523, V, 1, 1, 1, 1, 0, 704, 100
32524, V, 1, 1, 1, 1, 0, 704, 100
32525, V, 1, 1, 1, 1, 0, 704, 100
32526, V, 1, 1, 1, 1, 0, 704, 100
32527, V, 1, 1, 1, 1, 0, 704, 100
32528, V, 1, 1, 1, 1, 0, 704, 100
32529, V, 1, 1, 1, 1, 0, 704, 100
32530, V, 1, 1, 1, 1, 0, 704, 100
32531, V, 1, 1, 1, 1, 0, 704, 100
32532, V, 1, 1, 1, 1, 0, 704, 100
32533, V, 1, 1, 1, 1, 0, 704, 100
32534, V, 1, 1, 1, 1, 0, 704, 100
32535, V, 1, 1, 1, 1, 0, 704, 100
32536, V, 1, 1, 1, 1, 0, 704, 100
32537, V, 1, 1, 1, 1, 0, 704, 100
32538, V, 1, 1, 1, 1, 0, 704, 100
32539, V, 1, 1, 1, 1, 0, 704, 100
32540, V, 1, 1, 1, 1, 0, 704, 100
32541, V, 1, 1, 1, 1, 0, 704, 100
32542, V, 1, 1, 1, 1, 0, 704, 100
32543, V, 1, 1, 1, 1, 0, 704, 100
32544, V, 1, 1, 1, 1, 0, 704, 100
32545, V, 1, 1, 1, 1, 0, 704, 100
32546, V, 1, 1, 1, 1, 0, 704, 100
32547, V, 1, 1, 1, 1, 0, 704, 100
32548, V, 1, 1, 1, 1, 0, 704, 100
32549, V, 1, 1, 1, 1, 0, 704, 100
32550, V, 1, 1, 1, 1, 0, 704, 100
32551, V, 1, 1, 1, 1, 0, 704, 100
32552, V, 1, 1, 1, 1, 0, 704, 100
32553, V, 1, 1, 1, 1, 0, 704, 100
32555, V, 1, 1, 1, 1, 0, 704, 100
32556, V, 1, 1, 1, 1, 0, 704, 100
32557, V, 1, 1, 1, 1, 0, 704, 100
32558, V, 1, 1, 1, 1, 0, 704, 100
32559, V, 1, 1, 1, 1, 0, 704, 100
32560, V, 1, 1, 1, 1, 0, 704, 100
32561, V, 1, 1, 1, 1, 0, 704, 100
32562, V, 1, 1, 1, 1, 0, 704, 100
32563, V, 1, 1, 1, 1, 0, 704, 100
32564, V, 1, 1, 1, 1, 0, 704, 100
32565, V, 1, 1, 1, 1, 0, 704, 100
32566, V, 1, 1, 1, 1, 0, 704, 100
32567, V, 1, 1, 1, 1, 0, 704, 100
32568, V, 1, 1, 1, 1, 0, 704, 100
32569, V, 1, 1, 1, 1, 0, 704, 100
32570, V, 1, 1, 1, 1, 0, 704, 100
32571, V, 1, 1, 1, 1, 0, 704, 100
32572, V, 1, 1, 1, 1, 0, 704, 100
32573, V, 1, 1, 1, 1, 0, 704, 100
32574, V, 1, 1, 1, 1, 0, 704, 100
32575, V, 1, 1, 1, 1, 0, 704, 100
32576, V, 1, 1, 1, 1, 0, 704, 100
32577, V, 1, 1, 1, 1, 0, 704, 100
32578, V, 1, 1, 1, 1, 0, 704, 100
32579, V, 1, 1, 1, 1, 0, 704, 100
32580, V, 1, 1, 1, 1, 0, 704, 100
32581, V, 1, 1, 1, 1, 0, 704, 100
32582, V, 1, 1, 1, 1, 0, 704, 100
32583, V, 1, 1, 1, 1, 0, 704, 100
32584, V, 1, 1, 1, 1, 0, 704, 100
32585, V, 1, 1, 1, 1, 0, 704, 100
32586, V, 1, 1, 1, 1, 0, 704, 100
32587, V, 1, 1, 1, 1, 0, 704, 100
32588, V, 1, 1, 1, 1, 0, 704, 100
32589, V, 1, 1, 1, 1, 0, 704, 100
32590, V, 1, 1, 1, 1, 0, 704, 100
32591, V, 1, 1, 1, 1, 0, 704, 100
32592, V, 1, 1, 1, 1, 0, 704, 100
32593, V, 1, 1, 1, 1, 0, 704, 100
32594, V, 1, 1, 1, 1, 0, 704, 100
32595, V, 1, 1, 1, 1, 0, 704, 100
32596, V, 1, 1, 1, 1, 0, 704, 100
32598, V, 1, 1, 1, 1, 0, 704, 100
32599, V, 1, 1, 1, 1, 0, 704, 100
32600, V, 1, 1, 1, 1, 0, 704, 100
32601, V, 1, 1, 1, 1, 0, 704, 100
32602, V, 1, 1, 1, 1, 0, 704, 100
32603, V, 1, 1, 1, 1, 0, 704, 100
32604, V, 1, 1, 1, 1, 0, 704, 100
32605, V, 1, 1, 1, 1, 0, 704, 100
32606, V, 1, 1, 1, 1, 0, 704, 100
32607, V, 1, 1, 1, 1, 0, 704, 100
32608, V, 1, 1, 1, 1, 0, 704, 100
32609, V, 1, 1, 1, 1, 0, 704, 100
32610, V, 1, 1, 1, 1, 0, 704, 100
32611, V, 1, 1, 1, 1, 0, 704, 100
32612, V, 1, 1, 1, 1, 0, 704, 100
32613, V, 1, 1, 1, 1, 0, 704, 100
32614, V, 1, 1, 1, 1, 0, 704, 100
32615, V, 1, 1, 1, 1, 0, 704, 100
32616, V, 1, 1, 1, 1, 0, 704, 100
32617, V, 1, 1, 1, 1, 0, 704, 100
32618, V, 1, 1, 1, 1, 0, 704, 100
32619, V, 1, 1, 1, 1, 0, 704, 100
32620, V, 1, 1, 1, 1, 0, 704, 100
32621, V, 1, 1, 1, 1, 0, 704, 100
32622, V, 1, 1, 1, 1, 0, 704, 100
32623, V, 1, 1, 1, 1, 0, 704, 100
32624, V, 1, 1, 1, 1, 0, 704, 100
32625, V, 1, 1, 1, 1, 0, 704, 100
32626, V, 1, 1, 1, 1, 0, 704, 100
32627, V, 1, 1, 1, 1, 0, 704, 100
32628, V, 1, 1, 1, 1, 0, 704, 100
32629, V, 1, 1, 1, 1, 0, 704, 100
32630, V, 1, 1, 1, 1, 0, 704, 100
32631, V, 1, 1, 1, 1, 0, 704, 100
32632, V, 1, 1, 1, 1, 0, 704, 100
32633, V, 1, 1, 1, 1, 0, 704, 100
32634, V, 1, 1, 1, 1, 0, 704, 100
32635, V, 1, 1, 1, 1, 0, 704, 100
32636, V, 1, 1, 1, 1, 0, 704, 100
32637, V, 1, 1, 1, 1, 0, 704, 100
32638, V, 1, 1, 1, 1, 0, 704, 100
32640, V, 1, 1, 1, 1, 0, 704, 100
32641, V, 1, 1, 1, 1, 0, 704, 100
32642, V, 1, 1, 1, 1, 0, 704, 100
32643, V, 1, 1, 1, 1, 0, 704, 100
32644, V, 1, 1, 1, 1, 0, 704, 100
32645, V, 1, 1, 1, 1, 0, 704, 100
32646, V, 1, 1, 1, 1, 0, 704, 100
32647, V, 1, 1, 1, 1, 0, 704, 100
32648, V, 1, 1, 1, 1, 0, 704, 100
32649, V, 1, 1, 1, 1, 0, 704, 100
32650, V, 1, 1, 1, 1, 0, 704, 100
32651, V, 1, 1, 1, 1, 0, 704, 100
32652, V, 1, 1, 1, 1, 0, 704, 100
32653, V, 1, 1, 1, 1, 0, 704, 100
32654, V, 1, 1, 1, 1, 0, 704, 100
32655, V, 1, 1, 1, 1, 0, 704, 100
32656, V, 1, 1, 1, 1, 0, 704, 100
32657, V, 1, 1, 1, 1, 0, 704, 100
32658, V, 1, 1, 1, 1, 0, 704, 100
32659, V, 1, 1, 1, 1, 0, 704, 100
32660, V, 1, 1, 1, 1, 0, 704, 100
32661, V, 1, 1, 1, 1, 0, 704, 100
32662, V, 1, 1, 1, 1, 0, 704, 100
32663, V, 1, 1, 1, 1, 0, 704, 100
32664, V, 1, 1, 1, 1, 0, 704, 100
32665, V, 1, 1, 1, 1, 0, 704, 100
32666, V, 1, 1, 1, 1, 0, 704, 100
32667, V, 1, 1, 1, 1, 0, 704, 100
32668, V, 1, 1, 1, 1, 0, 704, 100
32669, V, 1, 1, 1, 1, 0, 704, 100
32670, V, 1, 1, 1, 1, 0, 704, 100
32671, V, 1, 1, 1, 1, 0, 704, 100
32672, V, 1, 1, 1, 1, 0, 704, 100
32673, V, 1, 1, 1, 1, 0, 704, 100
32674, V, 1, 1, 1, 1, 0, 704, 100
32675, V, 1, 1, 1, 1, 0, 704, 100
32676, V, 1, 1, 1, 1, 0, 704, 100
32677, V, 1, 1, 1, 1, 0, 704, 100
32678, V, 1, 1, 1, 1, 0, 704, 100
32679, V, 1, 1, 1, 1, 0, 704, 100
32680, V, 1, 1, 1, 1, 0, 704, 100
32681, V, 1, 1, 1, 1, 0, 704, 100
32683, V, 1, 1, 1, 1, 0, 704, 100
32684, V, 1, 1, 1, 1, 0, 704, 100
32685, V, 1, 1, 1, 1, 0, 704, 100
32686, V, 1, 1, 1, 1, 0, 704, 100
32687, V, 1, 1, 1, 1, 0, 704, 100
32688, V, 1, 1, 1, 1, 0, 704, 100
32689, V, 1, 1, 1, 1, 0, 704, 100
32690, V, 1, 1, 1, 1, 0, 704, 100
32691, V, 1, 1, 1, 1, 0, 704, 100
32692, V, 1, 1, 1, 1, 0, 704, 100
32693, V, 1, 1, 1, 1, 0, 704, 100
32694, V, 1, 1, 1, 1, 0, 704, 100
32695, V, 1, 1, 1, 1, 0, 704, 100
32696, V, 1, 1, 1, 1, 0, 704, 100
32697, V, 1, 1, 1, 1, 0, 704, 100
32698, V, 1, 1, 1, 1, 0, 704, 100
32699, V, 1, 1, 1, 1, 0, 704, 100
32700, V, 1, 1, 1, 1, 0, 704, 100
32701, V, 1, 1, 1, 1, 0, 704, 100
32702, V, 1, 1, 1, 1, 0, 704, 100
32703, V, 1, 1, 1, 1, 0, 704, 100
32704, V, 1, 1, 1, 1, 0, 704, 100
32705, V, 1, 1, 1, 1, 0, 704, 100
32706, V, 1, 1, 1, 1, 0, 704, 100
32707, V, 1, 1, 1, 1, 0, 704, 100
32708, V, 1, 1, 1, 1, 0, 704, 100
32709, V, 1, 1, 1, 1, 0, 704, 100
32710, V, 1, 1, 1, 1, 0, 704, 100
32711, V, 1, 1, 1, 1, 0, 704, 100
32712, V, 1, 1, 1, 1, 0, 704, 100
32713, V, 1, 1, 1, 1, 0, 704, 100
32714, V, 1, 1, 1, 1, 0, 704, 100
32715, V, 1, 1, 1, 1, 0, 704, 100
32716, V, 1, 1, 1, 1, 0, 704, 100
32717, V, 1, 1, 1, 1, 0, 704, 100
32718, V, 1, 1, 1, 1, 0, 704, 100
32719, V, 1, 1, 1, 1, 0, 704, 100
32720, V, 1, 1, 1, 1, 0, 704, 100
32721, V, 1, 1, 1, 1, 0, 704, 100
32722, V, 1, 1, 1, 1, 0, 704, 100
32723, V, 1, 1, 1, 1, 0, 704, 100
32724, V, 1, 1, 1, 1, 0, 704, 100
32726, V, 1, 1, 1, 1, 0, 704, 100
32727, V, 1, 1, 1, 1, 0, 704, 100
32728, V, 1, 1, 1, 1, 0, 704, 100
32729, V, 1, 1, 1, 1, 0, 704, 100
32730, V, 1, 1, 1, 1, 0, 704, 100
32731, V, 1, 1, 1, 1, 0, 704, 100
32732, V, 1, 1, 1, 1, 0, 704, 100
32733, V, 1, 1, 1, 1, 0, 704, 100
32734, V, 1, 1, 1, 1, 0, 704, 100
32735, V, 1, 1, 1, 1, 0, 704, 100
32736, V, 1, 1, 1, 1, 0, 704, 100
32737, V, 1, 1, 1, 1, 0, 704, 100
32738, V, 1, 1, 1, 1, 0, 704, 100
32739, V, 1, 1, 1, 1, 0, 704, 100
32740, V, 1, 1, 1, 1, 0, 704, 100
32741, V, 1, 1, 1, 1, 0, 704, 100
32742, V, 1, 1, 1, 1, 0, 704, 100
32743, V, 1, 1, 1, 1, 0, 704, 100
32744, V, 1, 1, 1, 1, 0, 704, 100
32745, V, 1, 1, 1, 1, 0, 704, 100
32746, V, 1, 1, 1, 1, 0, 704, 100
32747, V, 1, 1, 1, 1, 0, 704, 100
32748, V, 1, 1, 1, 1, 0, 704, 100
32749, V, 1, 1, 1, 1, 0, 704, 100
32750, V, 1, 1, 1, 1, 0, 704, 100
32751, V, 1, 1, 1, 1, 0, 704, 100
32752, V, 1, 1, 1, 1, 0, 704, 100
32753, V, 1, 1, 1, 1, 0, 704, 100
32754, V, 1, 1, 1, 1, 0, 704, 100
32755, V, 1, 1, 1, 1, 0, 704, 100
32756, V, 1, 1, 1, 1, 0, 704, 100
32757, V, 1, 1, 1, 1, 0, 704, 100
32758, V, 1, 1, 1, 1, 0, 704, 100
32759, V, 1, 1, 1, 1, 0, 704, 100
32760, V, 1, 1, 1, 1, 0, 704, 100
32761, V, 1, 1, 1, 1, 0, 704, 100
32762, V, 1, 1, 1, 1, 0, 704, 100
32763, V, 1, 1, 1, 1, 0, 704, 100
32764, V, 1, 1, 1, 1, 0, 704, 100
32765, V, 1, 1, 1, 1, 0, 704, 100
32766, V, 1, 1, 1, 1, 0, 704, 100
32768, V, 1, 1, 1, 1, 0, 704, 100
32769, V, 1, 1, 1, 1, 0, 704, 100
32770, V, 1, 1, 1, 1, 0, 704, 100
32771, V, 1, 1, 1, 1, 0, 704, 100
32772, V, 1, 1, 1, 1, 0, 704, 100
32773, V, 1, 1, 1, 1, 0, 704, 100
32774, V, 1, 1, 1, 1, 0, 704, 100
32775, V, 1, 1, 1, 1, 0, 704, 100
32776, V, 1, 1, 1, 1, 0, 704, 100
32777, V, 1, 1, 1, 1, 0, 704, 100
32778, V, 1, 1, 1, 1, 0, 704, 100
32779, V, 1, 1, 1, 1, 0, 704, 100
32780, V, 1, 1, 1, 1, 0, 704, 100
32781, V, 1, 1, 1, 1, 0, 704, 100
32782, V, 1, 1, 1, 1, 0, 704, 100
32783, V, 1, 1, 1, 1, 0, 704, 100
32784, V, 1, 1, 1, 1, 0, 704, 100
32785, V, 1, 1, 1, 1, 0, 704, 100
32786, V, 1, 1, 1, 1, 0, 704, 100
32787, V, 1, 1, 1, 1, 0, 704, 100
32788, V, 1, 1, 1, 1, 0, 704, 100
32789, V, 1, 1, 1, 1, 0, 704, 100
32790, V, 1, 1, 1, 1, 0, 704, 100
32791, V, 1, 1, 1, 1, 0, 704, 100
32792, V, 1, 1, 1, 1, 0, 704, 100
32793, V, 1, 1, 1, 1, 0, 704, 100
32794, V, 1, 1, 1, 1, 0, 704, 100
32795, V, 1, 1, 1, 1, 0, 704, 100
32796, V, 1, 1, 1, 1, 0, 704, 100
32797, V, 1, 1, 1, 1, 0, 704, 100
32798, V, 1, 1, 1, 1, 0, 704, 100
32799, V, 1, 1, 1, 1, 0, 704, 100
32800, V, 1, 1, 1, 1, 0, 704, 100
32801, V, 1, 1, 1, 1, 0, 704, 100
32802, V, 1, 1, 1, 1, 0, 704, 100
32803, V, 1, 1, 1, 1, 0, 704, 100
32804, V, 1, 1, 1, 1, 0, 704, 100
32805, V, 1, 1, 1, 1, 0, 704, 100
32806, V, 1, 1, 1, 1, 0, 704, 100
32807, V, 1, 1, 1, 1, 0, 704, 100
32808, V, 1, 1, 1, 1, 0, 704, 100
32809, V, 1, 1, 1, 1, 0, 704, 100
32811, V, 1, 1, 1, 1, 0, 704, 100
32812, V, 1, 1, 1, 1, 0, 704, 100
32813, V, 1, 1, 1, 1, 0, 704, 100
32814, V, 1, 1, 1, 1, 0, 704, 100
32815, V, 1, 1, 1, 1, 0, 704, 100
32816, V, 1, 1, 1, 1, 0, 704, 100
32817, V, 1, 1, 1, 1, 0, 704, 100
32818, V, 1, 1, 1, 1, 0, 704, 100
32819, V, 1, 1, 1, 1, 0, 704, 100
32820, V, 1, 1, 1, 1, 0, 704, 100
32821, V, 1, 1, 1, 1, 0, 704, 100
32822, V, 1, 1, 1, 1, 0, 704, 100
32823, V, 1, 1, 1, 1, 0, 704, 100
32824, V, 1, 1, 1, 1, 0, 704, 100
32825, V, 1, 1, 1, 1, 0, 704, 100
32826, V, 1, 1, 1, 1, 0, 704, 100
32827, V, 1, 1, 1, 1, 0, 704, 100
32828, V, 1, 1, 1, 1, 0, 704, 100
32829, V, 1, 1, 1, 1, 0, 704, 100
32830, V, 1, 1, 1, 1, 0, 704, 100
32831, V, 1, 1, 1, 1, 0, 704, 100
32832, V, 1, 1, 1, 1, 0, 704, 100
32833, V, 1, 1, 1, 1, 0, 704, 100
32834, V, 1, 1, 1, 1, 0, 704, 100
32835, V, 1, 1, 1, 1, 0, 704, 100
32836, V, 1, 1, 1, 1, 0, 704, 100
32837, V, 1, 1, 1, 1, 0, 704, 100
32838, V, 1, 1, 1, 1, 0, 704, 100
32839, V, 1, 1, 1, 1, 0, 704, 100
32840, V, 1, 1, 1, 1, 0, 704, 100
32841, V, 1, 1, 1, 1, 0, 704, 100
32842, V, 1, 1, 1, 1, 0, 704, 100
32843, V, 1, 1, 1, 1, 0, 704, 100
32844, V, 1, 1, 1, 1, 0, 704, 100
32845, V, 1, 1, 1, 1, 0, 704, 100
32846, V, 1, 1, 1, 1, 0, 704, 100
32847, V, 1, 1, 1, 1, 0, 704, 100
32848, V, 1, 1, 1, 1, 0, 704, 100
32849, V, 1, 1, 1, 1, 0, 704, 100
32850, V, 1, 1, 1, 1, 0, 704, 100
32851, V, 1, 1, 1, 1, 0, 704, 100
32852, V, 1, 1, 1, 1, 0, 704, 100
32854, V, 1, 1, 1, 1, 0, 704, 100
32855, V, 1, 1, 1, 1, 0, 704, 100
32856, V, 1, 1, 1, 1, 0, 704, 100
32857, V, 1, 1, 1, 1, 0, 704, 100
32858, V, 1, 1, 1, 1, 0, 704, 100
32859, V, 1, 1, 1, 1, 0, 704, 100
32860, V, 1, 1, 1, 1, 0, 704, 100
32861, V, 1, 1, 1, 1, 0, 704, 100
32862, V, 1, 1, 1, 1, 0, 704, 100
32863, V, 1, 1, 1, 1, 0, 704, 100
32864, V, 1, 1, 1, 1, 0, 704, 100
32865, V, 1, 1, 1, 1, 0, 704, 100
32866, V, 1, 1, 1, 1, 0, 704, 100
32867, V, 1, 1, 1, 1, 0, 704, 100
32868, V, 1, 1, 1, 1, 0, 704, 100
32869, V, 1, 1, 1, 1, 0, 704, 100
32870, V, 1, 1, 1, 1, 0, 704, 100
32871, V, 1, 1, 1, 1, 0, 704, 100
32872, V, 1, 1, 1, 1, 0, 704, 100
32873, V, 1, 1, 1, 1, 0, 704, 100
32874, V, 1, 1, 1, 1, 0, 704, 100
32875, V, 1, 1, 1, 1, 0, 704, 100
32876, V, 1, 1, 1, 1, 0, 704, 100
32877, V, 1, 1, 1, 1, 0, 704, 100
32878, V, 1, 1, 1, 1, 0, 704, 100
32879, V, 1, 1, 1, 1, 0, 704, 100
32880, V, 1, 1, 1, 1, 0, 704, 100
32881, V, 1, 1, 1, 1, 0, 704, 100
32882, V, 1, 1, 1, 1, 0, 704, 100
32883, V, 1, 1, 1, 1, 0, 704, 100
32884, V, 1, 1, 1, 1, 0, 704, 100
32885, V, 1, 1, 1, 1, 0, 704, 100
32886, V, 1, 1, 1, 1, 0, 704, 100
32887, V, 1, 1, 1, 1, 0, 704, 100
32888, V, 1, 1, 1, 1, 0, 704, 100
32889, V, 1, 1, 1, 1, 0, 704, 100
32890, V, 1, 1, 1, 1, 0, 704, 100
32891, V, 1, 1, 1, 1, 0, 704, 100
32892, V, 1, 1, 1, 1, 0, 704, 100
32893, V, 1, 1, 1, 1, 0, 704, 100
32894, V, 1, 1, 1, 1, 0, 704, 100
32896, V, 1, 1, 1, 1, 0, 704, 100
32897, V, 1, 1, 1, 1, 0, 704, 100
32898, V, 1, 1, 1, 1, 0, 704, 100
32899, V, 1, 1, 1, 1, 0, 704, 100
32900, V, 1, 1, 1, 1, 0, 704, 100
32901, V, 1, 1, 1, 1, 0, 704, 100
32902, V, 1, 1, 1, 1, 0, 704, 100
32903, V, 1, 1, 1, 1, 0, 704, 100
32904, V, 1, 1, 1, 1, 0, 704, 100
32905, V, 1, 1, 1, 1, 0, 704, 100
32906, V, 1, 1, 1, 1, 0, 704, 100
32907, V, 1, 1, 1, 1, 0, 704, 100
32908, V, 1, 1, 1, 1, 0, 704, 100
32909, V, 1, 1, 1, 1, 0, 704, 100
32910, V, 1, 1, 1, 1, 0, 704, 100
32911, V, 1, 1, 1, 1, 0, 704, 100
32912, V, 1, 1, 1, 1, 0, 704, 100
32913, V, 1, 1, 1, 1, 0, 704, 100
32914, V, 1, 1, 1, 1, 0, 704, 100
32915, V, 1, 1, 1, 1, 0, 704, 100
32916, V, 1, 1, 1, 1, 0, 704, 100
32917, V, 1, 1, 1, 1, 0, 704, 100
32918, V, 1, 1, 1, 1, 0, 704, 100
32919, V, 1, 1, 1, 1, 0, 704, 100
32920, V, 1, 1, 1, 1, 0, 704, 100
32921, V, 1, 1, 1, 1, 0, 704, 100
32922, V, 1, 1, 1, 1, 0, 704, 100
32923, V, 1, 1, 1, 1, 0, 704, 100
32924, V, 1, 1, 1, 1, 0, 704, 100
32925, V, 1, 1, 1, 1, 0, 704, 100
32926, V, 1, 1, 1, 1, 0, 704, 100
32927, V, 1, 1, 1, 1, 0, 704, 100
32928, V, 1, 1, 1, 1, 0, 704, 100
32929, V, 1, 1, 1, 1, 0, 704, 100
32930, V, 1, 1, 1, 1, 0, 704, 100
32931, V, 1, 1, 1, 1, 0, 704, 100
32932, V, 1, 1, 1, 1, 0, 704, 100
32933, V, 1, 1, 1, 1, 0, 704, 100
32934, V, 1, 1, 1, 1, 0, 704, 100
32935, V, 1, 1, 1, 1, 0, 704, 100
32936, V, 1, 1, 1, 1, 0, 704, 100
32937, V, 1, 1, 1, 1, 0, 704, 100
32939, V, 1, 1, 1, 1, 0, 704, 100
32940, V, 1, 1, 1, 1, 0, 704, 100
32941, V, 1, 1, 1, 1, 0, 704, 100
32942, V, 1, 1, 1, 1, 0, 704, 100
32943, V, 1, 1, 1, 1, 0, 704, 100
32944, V, 1, 1, 1, 1, 0, 704, 100
32945, V, 1, 1, 1, 1, 0, 704, 100
32946, V, 1, 1, 1, 1, 0, 704, 100
32947, V, 1, 1, 1, 1, 0, 704, 100
32948, V, 1, 1, 1, 1, 0, 704, 100
32949, V, 1, 1, 1, 1, 0, 704, 100
32950, V, 1, 1, 1, 1, 0, 704, 100
32951, V, 1, 1, 1, 1, 0, 704, 100
32952, V, 1, 1, 1, 1, 0, 704, 100
32953, V, 1, 1, 1, 1, 0, 704, 100
32954, V, 1, 1, 1, 1, 0, 704, 100
32955, V, 1, 1, 1, 1, 0, 704, 100
32956, V, 1, 1, 1, 1, 0, 704, 100
32957, V, 1, 1, 1, 1, 0, 704, 100
32958, V, 1, 1, 1, 1, 0, 704, 100
32959, V, 1, 1, 1, 1, 0, 704, 100
32960, V, 1, 1, 1, 1, 0, 704, 100
32961, V, 1, 1, 1, 1, 0, 704, 100
32962, V, 1, 1, 1, 1, 0, 704, 100
32963, V, 1, 1, 1, 1, 0, 704, 100
32964, V, 1, 1, 1, 1, 0, 704, 100
32965, V, 1, 1, 1, 1, 0, 704, 100
32966, V, 1, 1, 1, 1, 0, 704, 100
32967, V, 1, 1, 1, 1, 0, 704, 100
32968, V, 1, 1, 1, 1, 0, 704, 100
32969, V, 1, 1, 1, 1, 0, 704, 100
32970, V, 1, 1, 1, 1, 0, 704, 100
32971, V, 1, 1, 1, 1, 0, 704, 100
32972, V, 1, 1, 1, 1, 0, 704, 100
32973, V, 1, 1, 1, 1, 0, 704, 100
32974, V, 1, 1, 1, 1, 0, 704, 100
32975, V, 1, 1, 1, 1, 0, 704, 100
32976, V, 1, 1, 1, 1, 0, 704, 100
32977, V, 1, 1, 1, 1, 0, 704, 100
32978, V, 1, 1, 1, 1, 0, 704, 100
32979, V, 1, 1, 1, 1, 0, 704, 100
32980, V, 1, 1, 1, 1, 0, 704, 100
32982, V, 1, 1, 1, 1, 0, 704, 100
32983, V, 1, 1, 1, 1, 0, 704, 100
32984, V, 1, 1, 1, 1, 0, 704, 100
32985, V, 1, 1, 1, 1, 0, 704, 100
32986, V, 1, 1, 1, 1, 0, 704, 100
32987, V, 1, 1, 1, 1, 0, 704, 100
32988, V, 1, 1, 1, 1, 0, 704, 100
32989, V, 1, 1, 1, 1, 0, 704, 100
32990, V, 1, 1, 1, 1, 0, 704, 100
32991, V, 1, 1, 1, 1, 0, 704, 100
32992, V, 1, 1, 1, 1, 0, 704, 100
32993, V, 1, 1, 1, 1, 0, 704, 100
32994, V, 1, 1, 1, 1, 0, 704, 100
32995, V, 1, 1, 1, 1, 0, 704, 100
32996, V, 1, 1, 1, 1, 0, 704, 100
32997, V, 1, 1, 1, 1, 0, 704, 100
32998, V, 1, 1, 1, 1, 0, 704, 100
32999, V, 1, 1, 1, 1, 0, 704, 100
33000, V, 1, 1, 1, 1, 0, 704, 100
33001, V, 1, 1, 1, 1, 0, 704, 100
33002, V, 1, 1, 1, 1, 0, 704, 100
33003, V, 1, 1, 1, 1, 0, 704, 100
33004, V, 1, 1, 1, 1, 0, 704, 100
33005, V, 1, 1, 1, 1, 0, 704, 100
33006, V, 1, 1, 1, 1, 0, 704, 100
33007, V, 1, 1, 1, 1, 0, 704, 100
33008, V, 1, 1, 1, 1, 0, 704, 100
33009, V, 1, 1, 1, 1, 0, 704, 100
33010, V, 1, 1, 1, 1, 0, 704, 100
33011, V, 1, 1, 1, 1, 0, 704, 100
33012, V, 1, 1, 1, 1, 0, 704, 100
33013, V, 1, 1, 1, 1, 0, 704, 100
33014, V, 1, 1, 1, 1, 0, 704, 100
33015, V, 1, 1, 1, 1, 0, 704, 100
33016, V, 1, 1, 1, 1, 0, 704, 100
33017, V, 1, 1, 1, 1, 0, 704, 100
33018, V, 1, 1, 1, 1, 0, 704, 100
33019, V, 1, 1, 1, 1, 0, 704, 100
33020, V, 1, 1, 1, 1, 0, 704, 100
33021, V, 1, 1, 1, 1, 0, 704, 100
33022, V, 1, 1, 1, 1, 0, 704, 100
33024, V, 1, 1, 1, 1, 0, 704, 100
33025, V, 1, 1, 1, 1, 0, 704, 100
33026, V, 1, 1, 1, 1, 0, 704, 100
33027, V, 1, 1, 1, 1, 0, 704, 100
33028, V, 1, 1, 1, 1, 0, 704, 100
33029, V, 1, 1, 1, 1, 0, 704, 100
33030, V, 1, 1, 1, 1, 0, 704, 100
33031, V, 1, 1, 1, 1, 0, 704, 100
33032, V, 1, 1, 1, 1, 0, 704, 100
33033, V, 1, 1, 1, 1, 0, 704, 100
33034, V, 1, 1, 1, 1, 0, 704, 100
33035, V, 1, 1, 1, 1, 0, 704, 100
33036, V, 1, 1, 1, 1, 0, 704, 100
33037, V, 1, 1, 1, 1, 0, 704, 100
33038, V, 1, 1, 1, 1, 0, 704, 100
33039, V, 1, 1, 1, 1, 0, 704, 100
33040, V, 1, 1, 1, 1, 0, 704, 100
33041, V, 1, 1, 1, 1, 0, 704, 100
33042, V, 1, 1, 1, 1, 0, 704, 100
33043, V, 1, 1, 1, 1, 0, 704, 100
33044, V, 1, 1, 1, 1, 0, 704, 100
33045, V, 1, 1, 1, 1, 0, 704, 100
33046, V, 1, 1, 1, 1, 0, 704, 100
33047, V, 1, 1, 1, 1, 0, 704, 100
33048, V, 1, 1, 1, 1, 0, 704, 100
33049, V, 1, 1, 1, 1, 0, 704, 100
33050, V, 1, 1, 1, 1, 0, 704, 100
33051, V, 1, 1, 1, 1, 0, 704, 100
33052, V, 1, 1, 1, 1, 0, 704, 100
33053, V, 1, 1, 1, 1, 0, 704, 100
33054, V, 1, 1, 1, 1, 0, 704, 100
33055, V, 1, 1, 1, 1, 0, 704, 100
33056, V, 1, 1, 1, 1, 0, 704, 100
33057, V, 1, 1, 1, 1, 0, 704, 100
33058, V, 1, 1, 1, 1, 0, 704, 100
33059, V, 1, 1, 1, 1, 0, 704, 100
33060, V, 1, 1, 1, 1, 0, 704, 100
33061, V, 1, 1, 1, 1, 0, 704, 100
33062, V, 1, 1, 1, 1, 0, 704, 100
33063, V, 1, 1, 1, 1, 0, 704, 100
33064, V, 1, 1, 1, 1, 0, 704, 100
33065, V, 1, 1, 1, 1, 0, 704, 100
33067, V, 1, 1, 1, 1, 0, 704, 100
33068, V, 1, 1, 1, 1, 0, 704, 100
33069, V, 1, 1, 1, 1, 0, 704, 100
33070, V, 1, 1, 1, 1, 0, 704, 100
33071, V, 1, 1, 1, 1, 0, 704, 100
33072, V, 1, 1, 1, 1, 0, 704, 100
33073, V, 1, 1, 1, 1, 0, 704, 100
33074, V, 1, 1, 1, 1, 0, 704, 100
33075, V, 1, 1, 1, 1, 0, 704, 100
33076, V, 1, 1, 1, 1, 0, 704, 100
33077, V, 1, 1, 1, 1, 0, 704, 100
33078, V, 1, 1, 1, 1, 0, 704, 100
33079, V, 1, 1, 1, 1, 0, 704, 100
33080, V, 1, 1, 1, 1, 0, 704, 100
33081, V, 1, 1, 1, 1, 0, 704, 100
33082, V, 1, 1, 1, 1, 0, 704, 100
33083, V, 1, 1, 1, 1, 0, 704, 100
33084, V, 1, 1, 1, 1, 0, 704, 100
33085, V, 1, 1, 1, 1, 0, 704, 100
33086, V, 1, 1, 1, 1, 0, 704, 100
33087, V, 1, 1, 1, 1, 0, 704, 100
33088, V, 1, 1, 1, 1, 0, 704, 100
33089, V, 1, 1, 1, 1, 0, 704, 100
33090, V, 1, 1, 1, 1, 0, 704, 100
33091, V, 1, 1, 1, 1, 0, 704, 100
33092, V, 1, 1, 1, 1, 0, 704, 100
33093, V, 1, 1, 1, 1, 0, 704, 100
33094, V, 1, 1, 1, 1, 0, 704, 100
33095, V, 1, 1, 1, 1, 0, 704, 100
33096, V, 1, 1, 1, 1, 0, 704, 100
33097, V, 1, 1, 1, 1, 0, 704, 100
33098, V, 1, 1, 1, 1, 0, 704, 100
33099, V, 1, 1, 1, 1, 0, 704, 100
33100, V, 1, 1, 1, 1, 0, 704, 100
33101, V, 1, 1, 1, 1, 0, 704, 100
33102, V, 1, 1, 1, 1, 0, 704, 100
33103, V, 1, 1, 1, 1, 0, 704, 100
33104, V, 1, 1, 1, 1, 0, 704, 100
33105, V, 1, 1, 1, 1, 0, 704, 100
33106, V, 1, 1, 1, 1, 0, 704, 100
33107, V, 1, 1, 1, 1, 0, 704, 100
33108, V, 1, 1, 1, 1, 0, 704, 100
33110, V, 1, 1, 1, 1, 0, 704, 100
33111, V, 1, 1, 1, 1, 0, 704, 100
33112, V, 1, 1, 1, 1, 0, 704, 100
33113, V, 1, 1, 1, 1, 0, 704, 100
33114, V, 1, 1, 1, 1, 0, 704, 100
33115, V, 1, 1, 1, 1, 0, 704, 100
33116, V, 1, 1, 1, 1, 0, 704, 100
33117, V, 1, 1, 1, 1, 0, 704, 100
33118, V, 1, 1, 1, 1, 0, 704, 100
33119, V, 1, 1, 1, 1, 0, 704, 100
33120, V, 1, 1, 1, 1, 0, 704, 100
33121, V, 1, 1, 1, 1, 0, 704, 100
33122, V, 1, 1, 1, 1, 0, 704, 100
33123, V, 1, 1, 1, 1, 0, 704, 100
33124, V, 1, 1, 1, 1, 0, 704, 100
33125, V, 1, 1, 1, 1, 0, 704, 100
33126, V, 1, 1, 1, 1, 0, 704, 100
33127, V, 1, 1, 1, 1, 0, 704, 100
33128, V, 1, 1, 1, 1, 0, 704, 100
33129, V, 1, 1, 1, 1, 0, 704, 100
33130, V, 1, 1, 1, 1, 0, 704, 100
33131, V, 1, 1, 1, 1, 0, 704, 100
33132, V, 1, 1, 1, 1, 0, 704, 100
33133, V, 1, 1, 1, 1, 0, 704, 100
33134, V, 1, 1, 1, 1, 0, 704, 100
33135, V, 1, 1, 1, 1, 0, 704, 100
33136, V, 1, 1, 1, 1, 0, 704, 100
33137, V, 1, 1, 1, 1, 0, 704, 100
33138, V, 1, 1, 1, 1, 0, 704, 100
33139, V, 1, 1, 1, 1, 0, 704, 100
33140, V, 1, 1, 1, 1, 0, 704, 100
33141, V, 1, 1, 1, 1, 0, 704, 100
33142, V, 1, 1, 1, 1, 0, 704, 100
33143, V, 1, 1, 1, 1, 0, 704, 100
33144, V, 1, 1, 1, 1, 0, 704, 100
33145, V, 1, 1, 1, 1, 0, 704, 100
33146, V, 1, 1, 1, 1, 0, 704, 100
33147, V, 1, 1, 1, 1, 0, 704, 100
33148, V, 1, 1, 1, 1, 0, 704, 100
33149, V, 1, 1, 1, 1, 0, 704, 100
33150, V, 1, 1, 1, 1, 0, 704, 100
33152, V, 1, 1, 1, 1, 0, 704, 100
33153, V, 1, 1, 1, 1, 0, 704, 100
33154, V, 1, 1, 1, 1, 0, 704, 100
33155, V, 1, 1, 1, 1, 0, 704, 100
33156, V, 1, 1, 1, 1, 0, 704, 100
33157, V, 1, 1, 1, 1, 0, 704, 100
33158, V, 1, 1, 1, 1, 0, 704, 100
33159, V, 1, 1, 1, 1, 0, 704, 100
33160, V, 1, 1, 1, 1, 0, 704, 100
33161, V, 1, 1, 1, 1, 0, 704, 100
33162, V, 1, 1, 1, 1, 0, 704, 100
33163, V, 1, 1, 1, 1, 0, 704, 100
33164, V, 1, 1, 1, 1, 0, 704, 100
33165, V, 1, 1, 1, 1, 0, 704, 100
33166, V, 1, 1, 1, 1, 0, 704, 100
33167, V, 1, 1, 1, 1, 0, 704, 100
33168, V, 1, 1, 1, 1, 0, 704, 100
33169, V, 1, 1, 1, 1, 0, 704, 100
33170, V, 1, 1, 1, 1, 0, 704, 100
33171, V, 1, 1, 1, 1, 0, 704, 100
33172, V, 1, 1, 1, 1, 0, 704, 100
33173, V, 1, 1, 1, 1, 0, 704, 100
33174, V, 1, 1, 1, 1, 0, 704, 100
33175, V, 1, 1, 1, 1, 0, 704, 100
33176, V, 1, 1, 1, 1, 0, 704, 100
33177, V, 1, 1, 1, 1, 0, 704, 100
33178, V, 1, 1, 1, 1, 0, 704, 100
33179, V, 1, 1, 1, 1, 0, 704, 100
33180, V, 1, 1, 1, 1, 0, 704, 100
33181, V, 1, 1, 1, 1, 0, 704, 100
33182, V, 1, 1, 1, 1, 0, 704, 100
33183, V, 1, 1, 1, 1, 0, 704, 100
33184, V, 1, 1, 1, 1, 0, 704, 100
33185, V, 1, 1, 1, 1, 0, 704, 100
33186, V, 1, 1, 1, 1, 0, 704, 100
33187, V, 1, 1, 1, 1, 0, 704, 100
33188, V, 1, 1, 1, 1, 0, 704, 100
33189, V, 1, 1, 1, 1, 0, 704, 100
33190, V, 1, 1, 1, 1, 0, 704, 100
33191, V, 1, 1, 1, 1, 0, 704, 100
33192, V, 1, 1, 1, 1, 0, 704, 100
33193, V, 1, 1, 1, 1, 0, 704, 100
33195, V, 1, 1, 1, 1, 0, 704, 100
33196, V, 1, 1, 1, 1, 0, 704, 100
33197, V, 1, 1, 1, 1, 0, 704, 100
33198, V, 1, 1, 1, 1, 0, 704, 100
33199, V, 1, 1, 1, 1, 0, 704, 100
33200, V, 1, 1, 1, 1, 0, 704, 100
33201, V, 1, 1, 1, 1, 0, 704, 100
33202, V, 1, 1, 1, 1, 0, 704, 100
33203, V, 1, 1, 1, 1, 0, 704, 100
33204, V, 1, 1, 1, 1, 0, 704, 100
33205, V, 1, 1, 1, 1, 0, 704, 100
33206, V, 1, 1, 1, 1, 0, 704, 100
33207, V, 1, 1, 1, 1, 0, 704, 100
33208, V, 1, 1, 1, 1, 0, 704, 100
33209, V, 1, 1, 1, 1, 0, 704, 100
33210, V, 1, 1, 1, 1, 0, 704, 100
33211, V, 1, 1, 1, 1, 0, 704, 100
33212, V, 1, 1, 1, 1, 0, 704, 100
33213, V, 1, 1, 1, 1, 0, 704, 100
33214, V, 1, 1, 1, 1, 0, 704, 100
33215, V, 1, 1, 1, 1, 0, 704, 100
33216, V, 1, 1, 1, 1, 0, 704, 100
33217, V, 1, 1, 1, 1, 0, 704, 100
33218, V, 1, 1, 1, 1, 0, 704, 100
33219, V, 1, 1, 1, 1, 0, 704, 100
33220, V, 1, 1, 1, 1, 0, 704, 100
33221, V, 1, 1, 1, 1, 0, 704, 100
33222, V, 1, 1, 1, 1, 0, 704, 100
33223, V, 1, 1, 1, 1, 0, 704, 100
33224, V, 1, 1, 1, 1, 0, 704, 100
33225, V, 1, 1, 1, 1, 0, 704, 100
33226, V, 1, 1, 1, 1, 0, 704, 100
33227, V, 1, 1, 1, 1, 0, 704, 100
33228, V, 1, 1, 1, 1, 0, 704, 100
33229, V, 1, 1, 1, 1, 0, 704, 100
33230, V, 1, 1, 1, 1, 0, 704, 100
33231, V, 1, 1, 1, 1, 0, 704, 100
33232, V, 1, 1, 1, 1, 0, 704, 100
33233, V, 1, 1, 1, 1, 0, 704, 100
33234, V, 1, 1, 1, 1, 0, 704, 100
33235, V, 1, 1, 1, 1, 0, 704, 100
33236, V, 1, 1, 1, 1, 0, 704, 100
33238, V, 1, 1, 1, 1, 0, 704, 100
33239, V, 1, 1, 1, 1, 0, 704, 100
33240, V, 1, 1, 1, 1, 0, 704, 100
33241, V, 1, 1, 1, 1, 0, 704, 100
33242, V, 1, 1, 1, 1, 0, 704, 100
33243, V, 1, 1, 1, 1, 0, 704, 100
33244, V, 1, 1, 1, 1, 0, 704, 100
33245, V, 1, 1, 1, 1, 0, 704, 100
33246, V, 1, 1, 1, 1, 0, 704, 100
33247, V, 1, 1, 1, 1, 0, 704, 100
33248, V, 1, 1, 1, 1, 0, 704, 100
33249, V, 1, 1, 1, 1, 0, 704, 100
33250, V, 1, 1, 1, 1, 0, 704, 100
33251, V, 1, 1, 1, 1, 0, 704, 100
33252, V, 1, 1, 1, 1, 0, 704, 100
33253, V, 1, 1, 1, 1, 0, 704, 100
33254, V, 1, 1, 1, 1, 0, 704, 100
33255, V, 1, 1, 1, 1, 0, 704, 100
33256, V, 1, 1, 1, 1, 0, 704, 100
33257, V, 1, 1, 1, 1, 0, 704, 100
33258, V, 1, 1, 1, 1, 0, 704, 100
33259, V, 1, 1, 1, 1, 0, 704, 100
33260, V, 1, 1, 1, 1, 0, 704, 100
33261, V, 1, 1, 1, 1, 0, 704, 100
33262, V, 1, 1, 1, 1, 0, 704, 100
33263, V, 1, 1, 1, 1, 0, 704, 100
33264, V, 1, 1, 1, 1, 0, 704, 100
33265, V, 1, 1, 1, 1, 0, 704, 100
33266, V, 1, 1, 1, 1, 0, 704, 100
33267, V, 1, 1, 1, 1, 0, 704, 100
33268, V, 1, 1, 1, 1, 0, 704, 100
33269, V, 1, 1, 1, 1, 0, 704, 100
33270, V, 1, 1, 1, 1, 0, 704, 100
33271, V, 1, 1, 1, 1, 0, 704, 100
33272, V, 1, 1, 1, 1, 0, 704, 100
33273, V, 1, 1, 1, 1, 0, 704, 100
33274, V, 1, 1, 1, 1, 0, 704, 100
33275, V, 1, 1, 1, 1, 0, 704, 100
33276, V, 1, 1, 1, 1, 0, 704, 100
33277, V, 1, 1, 1, 1, 0, 704, 100
33278, V, 1, 1, 1, 1, 0, 704, 100
33280, V, 1, 1, 1, 1, 0, 704, 100
33281, V, 1, 1, 1, 1, 0, 704, 100
33282, V, 1, 1, 1, 1, 0, 704, 100
33283, V, 1, 1, 1, 1, 0, 704, 100
33284, V, 1, 1, 1, 1, 0, 704, 100
33285, V, 1, 1, 1, 1, 0, 704, 100
33286, V, 1, 1, 1, 1, 0, 704, 100
33287, V, 1, 1, 1, 1, 0, 704, 100
33288, V, 1, 1, 1, 1, 0, 704, 100
33289, V, 1, 1, 1, 1, 0, 704, 100
33290, V, 1, 1, 1, 1, 0, 704, 100
33291, V, 1, 1, 1, 1, 0, 704, 100
33292, V, 1, 1, 1, 1, 0, 704, 100
33293, V, 1, 1, 1, 1, 0, 704, 100
33294, V, 1, 1, 1, 1, 0, 704, 100
33295, V, 1, 1, 1, 1, 0, 704, 100
33296, V, 1, 1, 1, 1, 0, 704, 100
33297, V, 1, 1, 1, 1, 0, 704, 100
33298, V, 1, 1, 1, 1, 0, 704, 100
33299, V, 1, 1, 1, 1, 0, 704, 100
33300, V, 1, 1, 1, 1, 0, 704, 100
33301, V, 1, 1, 1, 1, 0, 704, 100
33302, V, 1, 1, 1, 1, 0, 704, 100
33303, V, 1, 1, 1, 1, 0, 704, 100
33304, V, 1, 1, 1, 1, 0, 704, 100
33305, V, 1, 1, 1, 1, 0, 704, 100
33306, V, 1, 1, 1, 1, 0, 704, 100
33307, V, 1, 1, 1, 1, 0, 704, 100
33308, V, 1, 1, 1, 1, 0, 704, 100
33309, V, 1, 1, 1, 1, 0, 704, 100
33310, V, 1, 1, 1, 1, 0, 704, 100
33311, V, 1, 1, 1, 1, 0, 704, 100
33312, V, 1, 1, 1, 1, 0, 704, 100
33313, V, 1, 1, 1, 1, 0, 704, 100
33314, V, 1, 1, 1, 1, 0, 704, 100
33315, V, 1, 1, 1, 1, 0, 704, 100
33316, V, 1, 1, 1, 1, 0, 704, 100
33317, V, 1, 1, 1, 1, 0, 704, 100
33318, V, 1, 1, 1, 1, 0, 704, 100
33319, V, 1, 1, 1, 1, 0, 704, 100
33320, V, 1, 1, 1, 1, 0, 704, 100
33321, V, 1, 1, 1, 1, 0, 704, 100
33323, V, 1, 1, 1, 1, 0, 704, 100
33324, V, 1, 1, 1, 1, 0, 704, 100
33325, V, 1, 1, 1, 1, 0, 704, 100
33326, V, 1, 1, 1, 1, 0, 704, 100
33327, V, 1, 1, 1, 1, 0, 704, 100
33328, V, 1, 1, 1, 1, 0, 704, 100
33329, V, 1, 1, 1, 1, 0, 704, 100
33330, V, 1, 1, 1, 1, 0, 704, 100
33331, V, 1, 1, 1, 1, 0, 704, 100
33332, V, 1, 1, 1, 1, 0, 704, 100
33333, V, 1, 1, 1, 1, 0, 704, 100
33334, V, 1, 1, 1, 1, 0, 704, 100
33335, V, 1, 1, 1, 1, 0, 704, 100
33336, V, 1, 1, 1, 1, 0, 704, 100
33337, V, 1, 1, 1, 1, 0, 704, 100
33338, V, 1, 1, 1, 1, 0, 704, 100
33339, V, 1, 1, 1, 1, 0, 704, 100
33340, V, 1, 1, 1, 1, 0, 704, 100
33341, V, 1, 1, 1, 1, 0, 704, 100
33342, V, 1, 1, 1, 1, 0, 704, 100
33343, V, 1, 1, 1, 1, 0, 704, 100
33344, V, 1, 1, 1, 1, 0, 704, 100
33345, V, 1, 1, 1, 1, 0, 704, 100
33346, V, 1, 1, 1, 1, 0, 704, 100
33347, V, 1, 1, 1, 1, 0, 704, 100
33348, V, 1, 1, 1, 1, 0, 704, 100
33349, V, 1, 1, 1, 1, 0, 704, 100
33350, V, 1, 1, 1, 1, 0, 704, 100
33351, V, 1, 1, 1, 1, 0, 704, 100
33352, V, 1, 1, 1, 1, 0, 704, 100
33353, V, 1, 1, 1, 1, 0, 704, 100
33354, V, 1, 1, 1, 1, 0, 704, 100
33355, V, 1, 1, 1, 1, 0, 704, 100
33356, V, 1, 1, 1, 1, 0, 704, 100
33357, V, 1, 1, 1, 1, 0, 704, 100
33358, V, 1, 1, 1, 1, 0, 704, 100
33359, V, 1, 1, 1, 1, 0, 704, 100
33360, V, 1, 1, 1, 1, 0, 704, 100
33361, V, 1, 1, 1, 1, 0, 704, 100
33362, V, 1, 1, 1, 1, 0, 704, 100
33363, V, 1, 1, 1, 1, 0, 704, 100
33364, V, 1, 1, 1, 1, 0, 704, 100
33366, V, 1, 1, 1, 1, 0, 704, 100
33367, V, 1, 1, 1, 1, 0, 704, 100
33368, V, 1, 1, 1, 1, 0, 704, 100
33369, V, 1, 1, 1, 1, 0, 704, 100
33370, V, 1, 1, 1, 1, 0, 704, 100
33371, V, 1, 1, 1, 1, 0, 704, 100
33372, V, 1, 1, 1, 1, 0, 704, 100
33373, V, 1, 1, 1, 1, 0, 704, 100
33374, V, 1, 1, 1, 1, 0, 704, 100
33375, V, 1, 1, 1, 1, 0, 704, 100
33376, V, 1, 1, 1, 1, 0, 704, 100
33377, V, 1, 1, 1, 1, 0, 704, 100
33378, V, 1, 1, 1, 1, 0, 704, 100
33379, V, 1, 1, 1, 1, 0, 704, 100
33380, V, 1, 1, 1, 1, 0, 704, 100
33381, V, 1, 1, 1, 1, 0, 704, 100
33382, V, 1, 1, 1, 1, 0, 704, 100
33383, V, 1, 1, 1, 1, 0, 704, 100
33384, V, 1, 1, 1, 1, 0, 704, 100
33385, V, 1, 1, 1, 1, 0, 704, 100
33386, V, 1, 1, 1, 1, 0, 704, 100
33387, V, 1, 1, 1, 1, 0, 704, 100
33388, V, 1, 1, 1, 1, 0, 704, 100
33389, V, 1, 1, 1, 1, 0, 704, 100
33390, V, 1, 1, 1, 1, 0, 704, 100
33391, V, 1, 1, 1, 1, 0, 704, 100
33392, V, 1, 1, 1, 1, 0, 704, 100
33393, V, 1, 1, 1, 1, 0, 704, 100
33394, V, 1, 1, 1, 1, 0, 704, 100
33395, V, 1, 1, 1, 1, 0, 704, 100
33396, V, 1, 1, 1, 1, 0, 704, 100
33397, V, 1, 1, 1, 1, 0, 704, 100
33398, V, 1, 1, 1, 1, 0, 704, 100
33399, V, 1, 1, 1, 1, 0, 704, 100
33400, V, 1, 1, 1, 1, 0, 704, 100
33401, V, 1, 1, 1, 1, 0, 704, 100
33402, V, 1, 1, 1, 1, 0, 704, 100
33403, V, 1, 1, 1, 1, 0, 704, 100
33404, V, 1, 1, 1, 1, 0, 704, 100
33405, V, 1, 1, 1, 1, 0, 704, 100
33406, V, 1, 1, 1, 1, 0, 704, 100
33408, V, 1, 1, 1, 1, 0, 704, 100
33409, V, 1, 1, 1, 1, 0, 704, 100
33410, V, 1, 1, 1, 1, 0, 704, 100
33411, V, 1, 1, 1, 1, 0, 704, 100
33412, V, 1, 1, 1, 1, 0, 704, 100
33413, V, 1, 1, 1, 1, 0, 704, 100
33414, V, 1, 1, 1, 1, 0, 704, 100
33415, V, 1, 1, 1, 1, 0, 704, 100
33416, V, 1, 1, 1, 1, 0, 704, 100
33417, V, 1, 1, 1, 1, 0, 704, 100
33418, V, 1, 1, 1, 1, 0, 704, 100
33419, V, 1, 1, 1, 1, 0, 704, 100
33420, V, 1, 1, 1, 1, 0, 704, 100
33421, V, 1, 1, 1, 1, 0, 704, 100
33422, V, 1, 1, 1, 1, 0, 704, 100
33423, V, 1, 1, 1, 1, 0, 704, 100
33424, V, 1, 1, 1, 1, 0, 704, 100
33425, V, 1, 1, 1, 1, 0, 704, 100
33426, V, 1, 1, 1, 1, 0, 704, 100
33427, V, 1, 1, 1, 1, 0, 704, 100
33428, V, 1, 1, 1, 1, 0, 704, 100
33429, V, 1, 1, 1, 1, 0, 704, 100
33430, V, 1, 1, 1, 1, 0, 704, 100
33431, V, 1, 1, 1, 1, 0, 704, 100
33432, V, 1, 1, 1, 1, 0, 704, 100
33433, V, 1, 1, 1, 1, 0, 704, 100
33434, V, 1, 1, 1, 1, 0, 704, 100
33435, V, 1, 1, 1, 1, 0, 704, 100
33436, V, 1, 1, 1, 1, 0, 704, 100
33437, V, 1, 1, 1, 1, 0, 704, 100
33438, V, 1, 1, 1, 1, 0, 704, 100
33439, V, 1, 1, 1, 1, 0, 704, 100
33440, V, 1, 1, 1, 1, 0, 704, 100
33441, V, 1, 1, 1, 1, 0, 704, 100
33442, V, 1, 1, 1, 1, 0, 704, 100
33443, V, 1, 1, 1, 1, 0, 704, 100
33444, V, 1, 1, 1, 1, 0, 704, 100
33445, V, 1, 1, 1, 1, 0, 704, 100
33446, V, 1, 1, 1, 1, 0, 704, 100
33447, V, 1, 1, 1, 1, 0, 704, 100
33448, V, 1, 1, 1, 1, 0, 704, 100
33449, V, 1, 1, 1, 1, 0, 704, 100
33451, V, 1, 1, 1, 1, 0, 704, 100
33452, V, 1, 1, 1, 1, 0, 704, 100
33453, V, 1, 1, 1, 1, 0, 704, 100
33454, V, 1, 1, 1, 1, 0, 704, 100
33455, V, 1, 1, 1, 1, 0, 704, 100
33456, V, 1, 1, 1, 1, 0, 704, 100
33457, V, 1, 1, 1, 1, 0, 704, 100
33458, V, 1, 1, 1, 1, 0, 704, 100
33459, V, 1, 1, 1, 1, 0, 704, 100
33460, V, 1, 1, 1, 1, 0, 704, 100
33461, V, 1, 1, 1, 1, 0, 704, 100
33462, V, 1, 1, 1, 1, 0, 704, 100
33463, V, 1, 1, 1, 1, 0, 704, 100
33464, V, 1, 1, 1, 1, 0, 704, 100
33465, V, 1, 1, 1, 1, 0, 704, 100
33466, V, 1, 1, 1, 1, 0, 704, 100
33467, V, 1, 1, 1, 1, 0, 704, 100
33468, V, 1, 1, 1, 1, 0, 704, 100
33469, V, 1, 1, 1, 1, 0, 704, 100
33470, V, 1, 1, 1, 1, 0, 704, 100
33471, V, 1, 1, 1, 1, 0, 704, 100
33472, V, 1, 1, 1, 1, 0, 704, 100
33473, V, 1, 1, 1, 1, 0, 704, 100
33474, V, 1, 1, 1, 1, 0, 704, 100
33475, V, 1, 1, 1, 1, 0, 704, 100
33476, V, 1, 1, 1, 1, 0, 704, 100
33477, V, 1, 1, 1, 1, 0, 704, 100
33478, V, 1, 1, 1, 1, 0, 704, 100
33479, V, 1, 1, 1, 1, 0, 704, 100
33480, V, 1, 1, 1, 1, 0, 704, 100
33481, V, 1, 1, 1, 1, 0, 704, 100
33482, V, 1, 1, 1, 1, 0, 704, 100
33483, V, 1, 1, 1, 1, 0, 704, 100
33484, V, 1, 1, 1, 1, 0, 704, 100
33485, V, 1, 1, 1, 1, 0, 704, 100
33486, V, 1, 1, 1, 1, 0, 704, 100
33487, V, 1, 1, 1, 1, 0, 704, 100
33488, V, 1, 1, 1, 1, 0, 704, 100
33489, V, 1, 1, 1, 1, 0, 704, 100
33490, V, 1, 1, 1, 1, 0, 704, 100
33491, V, 1, 1, 1, 1, 0, 704, 100
33492, V, 1, 1, 1, 1, 0, 704, 100
33494, V, 1, 1, 1, 1, 0, 704, 100
33495, V, 1, 1, 1, 1, 0, 704, 100
33496, V, 1, 1, 1, 1, 0, 704, 100
33497, V, 1, 1, 1, 1, 0, 704, 100
33498, V, 1, 1, 1, 1, 0, 704, 100
33499, V, 1, 1, 1, 1, 0, 704, 100
33500, V, 1, 1, 1, 1, 0, 704, 100
33501, V, 1, 1, 1, 1, 0, 704, 100
33502, V, 1, 1, 1, 1, 0, 704, 100
33503, V, 1, 1, 1, 1, 0, 704, 100
33504, V, 1, 1, 1, 1, 0, 704, 100
33505, V, 1, 1, 1, 1, 0, 704, 100
33506, V, 1, 1, 1, 1, 0, 704, 100
33507, V, 1, 1, 1, 1, 0, 704, 100
33508, V, 1, 1, 1, 1, 0, 704, 100
33509, V, 1, 1, 1, 1, 0, 704, 100
33510, V, 1, 1, 1, 1, 0, 704, 100
33511, V, 1, 1, 1, 1, 0, 704, 100
33512, V, 1, 1, 1, 1, 0, 704, 100
33513, V, 1, 1, 1, 1, 0, 704, 100
33514, V, 1, 1, 1, 1, 0, 704, 100
33515, V, 1, 1, 1, 1, 0, 704, 100
33516, V, 1, 1, 1, 1, 0, 704, 100
33517, V, 1, 1, 1, 1, 0, 704, 100
33518, V, 1, 1, 1, 1, 0, 704, 100
33519, V, 1, 1, 1, 1, 0, 704, 100
33520, V, 1, 1, 1, 1, 0, 704, 100
33521, V, 1, 1, 1, 1, 0, 704, 100
33522, V, 1, 1, 1, 1, 0, 704, 100
33523, V, 1, 1, 1, 1, 0, 704, 100
33524, V, 1, 1, 1, 1, 0, 704, 100
33525, V, 1, 1, 1, 1, 0, 704, 100
33526, V, 1, 1, 1, 1, 0, 704, 100
33527, V, 1, 1, 1, 1, 0, 704, 100
33528, V, 1, 1, 1, 1, 0, 704, 100
33529, V, 1, 1, 1, 1, 0, 704, 100
33530, V, 1, 1, 1, 1, 0, 704, 100
33531, V, 1, 1, 1, 1, 0, 704, 100
33532, V, 1, 1, 1, 1, 0, 704, 100
33533, V, 1, 1, 1, 1, 0, 704, 100
33534, V, 1, 1, 1, 1, 0, 704, 100
33536, V, 1, 1, 1, 1, 0, 704, 100
33537, V, 1, 1, 1, 1, 0, 704, 100
33538, V, 1, 1, 1, 1, 0, 704, 100
33539, V, 1, 1, 1, 1, 0, 704, 100
33540, V, 1, 1, 1, 1, 0, 704, 100
33541, V, 1, 1, 1, 1, 0, 704, 100
33542, V, 1, 1, 1, 1, 0, 704, 100
33543, V, 1, 1, 1, 1, 0, 704, 100
33544, V, 1, 1, 1, 1, 0, 704, 100
33545, V, 1, 1, 1, 1, 0, 704, 100
33546, V, 1, 1, 1, 1, 0, 704, 100
33547, V, 1, 1, 1, 1, 0, 704, 100
33548, V, 1, 1, 1, 1, 0, 704, 100
33549, V, 1, 1, 1, 1, 0, 704, 100
33550, V, 1, 1, 1, 1, 0, 704, 100
33551, V, 1, 1, 1, 1, 0, 704, 100
33552, V, 1, 1, 1, 1, 0, 704, 100
33553, V, 1, 1, 1, 1, 0, 704, 100
33554, V, 1, 1, 1, 1, 0, 704, 100
33555, V, 1, 1, 1, 1, 0, 704, 100
33556, V, 1, 1, 1, 1, 0, 704, 100
33557, V, 1, 1, 1, 1, 0, 704, 100
33558, V, 1, 1, 1, 1, 0, 704, 100
33559, V, 1, 1, 1, 1, 0, 704, 100
33560, V, 1, 1, 1, 1, 0, 704, 100
33561, V, 1, 1, 1, 1, 0, 704, 100
33562, V, 1, 1, 1, 1, 0, 704, 100
33563, V, 1, 1, 1, 1, 0, 704, 100
33564, V, 1, 1, 1, 1, 0, 704, 100
33565, V, 1, 1, 1, 1, 0, 704, 100
33566, V, 1, 1, 1, 1, 0, 704, 100
33567, V, 1, 1, 1, 1, 0, 704, 100
33568, V, 1, 1, 1, 1, 0, 704, 100
33569, V, 1, 1, 1, 1, 0, 704, 100
33570, V, 1, 1, 1, 1, 0, 704, 100
33571, V, 1, 1, 1, 1, 0, 704, 100
33572, V, 1, 1, 1, 1, 0, 704, 100
33573, V, 1, 1, 1, 1, 0, 704, 100
33574, V, 1, 1, 1, 1, 0, 704, 100
33575, V, 1, 1, 1, 1, 0, 704, 100
33576, V, 1, 1, 1, 1, 0, 704, 100
33577, V, 1, 1, 1, 1, 0, 704, 100
33579, V, 1, 1, 1, 1, 0, 704, 100
33580, V, 1, 1, 1, 1, 0, 704, 100
33581, V, 1, 1, 1, 1, 0, 704, 100
33582, V, 1, 1, 1, 1, 0, 704, 100
33583, V, 1, 1, 1, 1, 0, 704, 100
33584, V, 1, 1, 1, 1, 0, 704, 100
33585, V, 1, 1, 1, 1, 0, 704, 100
33586, V, 1, 1, 1, 1, 0, 704, 100
33587, V, 1, 1, 1, 1, 0, 704, 100
33588, V, 1, 1, 1, 1, 0, 704, 100
33589, V, 1, 1, 1, 1, 0, 704, 100
33590, V, 1, 1, 1, 1, 0, 704, 100
33591, V, 1, 1, 1, 1, 0, 704, 100
33592, V, 1, 1, 1, 1, 0, 704, 100
33593, V, 1, 1, 1, 1, 0, 704, 100
33594, V, 1, 1, 1, 1, 0, 704, 100
33595, V, 1, 1, 1, 1, 0, 704, 100
33596, V, 1, 1, 1, 1, 0, 704, 100
33597, V, 1, 1, 1, 1, 0, 704, 100
33598, V, 1, 1, 1, 1, 0, 704, 100
33599, V, 1, 1, 1, 1, 0, 704, 100
33600, V, 1, 1, 1, 1, 0, 704, 100
33601, V, 1, 1, 1, 1, 0, 704, 100
33602, V, 1, 1, 1, 1, 0, 704, 100
33603, V, 1, 1, 1, 1, 0, 704, 100
33604, V, 1, 1, 1, 1, 0, 704, 100
33605, V, 1, 1, 1, 1, 0, 704, 100
33606, V, 1, 1, 1, 1, 0, 704, 100
33607, V, 1, 1, 1, 1, 0, 704, 100
33608, V, 1, 1, 1, 1, 0, 704, 100
33609, V, 1, 1, 1, 1, 0, 704, 100
33610, V, 1, 1, 1, 1, 0, 704, 100
33611, V, 1, 1, 1, 1, 0, 704, 100
33612, V, 1, 1, 1, 1, 0, 704, 100
33613, V, 1, 1, 1, 1, 0, 704, 100
33614, V, 1, 1, 1, 1, 0, 704, 100
33615, V, 1, 1, 1, 1, 0, 704, 100
33616, V, 1, 1, 1, 1, 0, 704, 100
33617, V, 1, 1, 1, 1, 0, 704, 100
33618, V, 1, 1, 1, 1, 0, 704, 100
33619, V, 1, 1, 1, 1, 0, 704, 100
33620, V, 1, 1, 1, 1, 0, 704, 100
33622, V, 1, 1, 1, 1, 0, 704, 100
33623, V, 1, 1, 1, 1, 0, 704, 100
33624, V, 1, 1, 1, 1, 0, 704, 100
33625, V, 1, 1, 1, 1, 0, 704, 100
33626, V, 1, 1, 1, 1, 0, 704, 100
33627, V, 1, 1, 1, 1, 0, 704, 100
33628, V, 1, 1, 1, 1, 0, 704, 100
33629, V, 1, 1, 1, 1, 0, 704, 100
33630, V, 1, 1, 1, 1, 0, 704, 100
33631, V, 1, 1, 1, 1, 0, 704, 100
33632, V, 1, 1, 1, 1, 0, 704, 100
33633, V, 1, 1, 1, 1, 0, 704, 100
33634, V, 1, 1, 1, 1, 0, 704, 100
33635, V, 1, 1, 1, 1, 0, 704, 100
33636, V, 1, 1, 1, 1, 0, 704, 100
33637, V, 1, 1, 1, 1, 0, 704, 100
33638, V, 1, 1, 1, 1, 0, 704, 100
33639, V, 1, 1, 1, 1, 0, 704, 100
33640, V, 1, 1, 1, 1, 0, 704, 100
33641, V, 1, 1, 1, 1, 0, 704, 100
33642, V, 1, 1, 1, 1, 0, 704, 100
33643, V, 1, 1, 1, 1, 0, 704, 100
33644, V, 1, 1, 1, 1, 0, 704, 100
33645, V, 1, 1, 1, 1, 0, 704, 100
33646, V, 1, 1, 1, 1, 0, 704, 100
33647, V, 1, 1, 1, 1, 0, 704, 100
33648, V, 1, 1, 1, 1, 0, 704, 100
33649, V, 1, 1, 1, 1, 0, 704, 100
33650, V, 1, 1, 1, 1, 0, 704, 100
33651, V, 1, 1, 1, 1, 0, 704, 100
33652, V, 1, 1, 1, 1, 0, 704, 100
33653, V, 1, 1, 1, 1, 0, 704, 100
33654, V, 1, 1, 1, 1, 0, 704, 100
33655, V, 1, 1, 1, 1, 0, 704, 100
33656, V, 1, 1, 1, 1, 0, 704, 100
33657, V, 1, 1, 1, 1, 0, 704, 100
33658, V, 1, 1, 1, 1, 0, 704, 100
33659, V, 1, 1, 1, 1, 0, 704, 100
33660, V, 1, 1, 1, 1, 0, 704, 100
33661, V, 1, 1, 1, 1, 0, 704, 100
33662, V, 1, 1, 1, 1, 0, 704, 100
33664, V, 1, 1, 1, 1, 0, 704, 100
33665, V, 1, 1, 1, 1, 0, 704, 100
33666, V, 1, 1, 1, 1, 0, 704, 100
33667, V, 1, 1, 1, 1, 0, 704, 100
33668, V, 1, 1, 1, 1, 0, 704, 100
33669, V, 1, 1, 1, 1, 0, 704, 100
33670, V, 1, 1, 1, 1, 0, 704, 100
33671, V, 1, 1, 1, 1, 0, 704, 100
33672, V, 1, 1, 1, 1, 0, 704, 100
33673, V, 1, 1, 1, 1, 0, 704, 100
33674, V, 1, 1, 1, 1, 0, 704, 100
33675, V, 1, 1, 1, 1, 0, 704, 100
33676, V, 1, 1, 1, 1, 0, 704, 100
33677, V, 1, 1, 1, 1, 0, 704, 100
33678, V, 1, 1, 1, 1, 0, 704, 100
33679, V, 1, 1, 1, 1, 0, 704, 100
33680, V, 1, 1, 1, 1, 0, 704, 100
33681, V, 1, 1, 1, 1, 0, 704, 100
33682, V, 1, 1, 1, 1, 0, 704, 100
33683, V, 1, 1, 1, 1, 0, 704, 100
33684, V, 1, 1, 1, 1, 0, 704, 100
33685, V, 1, 1, 1, 1, 0, 704, 100
33686, V, 1, 1, 1, 1, 0, 704, 100
33687, V, 1, 1, 1, 1, 0, 704, 100
33688, V, 1, 1, 1, 1, 0, 704, 100
33689, V, 1, 1, 1, 1, 0, 704, 100
33690, V, 1, 1, 1, 1, 0, 704, 100
33691, V, 1, 1, 1, 1, 0, 704, 100
33692, V, 1, 1, 1, 1, 0, 704, 100
33693, V, 1, 1, 1, 1, 0, 704, 100
33694, V, 1, 1, 1, 1, 0, 704, 100
33695, V, 1, 1, 1, 1, 0, 704, 100
33696, V, 1, 1, 1, 1, 0, 704, 100
33697, V, 1, 1, 1, 1, 0, 704, 100
33698, V, 1, 1, 1, 1, 0, 704, 100
33699, V, 1, 1, 1, 1, 0, 704, 100
33700, V, 1, 1, 1, 1, 0, 704, 100
33701, V, 1, 1, 1, 1, 0, 704, 100
33702, V, 1, 1, 1, 1, 0, 704, 100
33703, V, 1, 1, 1, 1, 0, 704, 100
33704, V, 1, 1, 1, 1, 0, 704, 100
33705, V, 1, 1, 1, 1, 0, 704, 100
33707, V, 1, 1, 1, 1, 0, 704, 100
33708, V, 1, 1, 1, 1, 0, 704, 100
33709, V, 1, 1, 1, 1, 0, 704, 100
33710, V, 1, 1, 1, 1, 0, 704, 100
33711, V, 1, 1, 1, 1, 0, 704, 100
33712, V, 1, 1, 1, 1, 0, 704, 100
33713, V, 1, 1, 1, 1, 0, 704, 100
33714, V, 1, 1, 1, 1, 0, 704, 100
33715, V, 1, 1, 1, 1, 0, 704, 100
33716, V, 1, 1, 1, 1, 0, 704, 100
33717, V, 1, 1, 1, 1, 0, 704, 100
33718, V, 1, 1, 1, 1, 0, 704, 100
33719, V, 1, 1, 1, 1, 0, 704, 100
33720, V, 1, 1, 1, 1, 0, 704, 100
33721, V, 1, 1, 1, 1, 0, 704, 100
33722, V, 1, 1, 1, 1, 0, 704, 100
33723, V, 1, 1, 1, 1, 0, 704, 100
33724, V, 1, 1, 1, 1, 0, 704, 100
33725, V, 1, 1, 1, 1, 0, 704, 100
33726, V, 1, 1, 1, 1, 0, 704, 100
33727, V, 1, 1, 1, 1, 0, 704, 100
33728, V, 1, 1, 1, 1, 0, 704, 100
33729, V, 1, 1, 1, 1, 0, 704, 100
33730, V, 1, 1, 1, 1, 0, 704, 100
33731, V, 1, 1, 1, 1, 0, 704, 100
33732, V, 1, 1, 1, 1, 0, 704, 100
33733, V, 1, 1, 1, 1, 0, 704, 100
33734, V, 1, 1, 1, 1, 0, 704, 100
33735, V, 1, 1, 1, 1, 0, 704, 100
33736, V, 1, 1, 1, 1, 0, 704, 100
33737, V, 1, 1, 1, 1, 0, 704, 100
33738, V, 1, 1, 1, 1, 0, 704, 100
33739, V, 1, 1, 1, 1, 0, 704, 100
33740, V, 1, 1, 1, 1, 0, 704, 100
33741, V, 1, 1, 1, 1, 0, 704, 100
33742, V, 1, 1, 1, 1, 0, 704, 100
33743, V, 1, 1, 1, 1, 0, 704, 100
33744, V, 1, 1, 1, 1, 0, 704, 100
33745, V, 1, 1, 1, 1, 0, 704, 100
33746, V, 1, 1, 1, 1, 0, 704, 100
33747, V, 1, 1, 1, 1, 0, 704, 100
33748, V, 1, 1, 1, 1, 0, 704, 100
33750, V, 1, 1, 1, 1, 0, 704, 100
33751, V, 1, 1, 1, 1, 0, 704, 100
33752, V, 1, 1, 1, 1, 0, 704, 100
33753, V, 1, 1, 1, 1, 0, 704, 100
33754, V, 1, 1, 1, 1, 0, 704, 100
33755, V, 1, 1, 1, 1, 0, 704, 100
33756, V, 1, 1, 1, 1, 0, 704, 100
33757, V, 1, 1, 1, 1, 0, 704, 100
33758, V, 1, 1, 1, 1, 0, 704, 100
33759, V, 1, 1, 1, 1, 0, 704, 100
33760, V, 1, 1, 1, 1, 0, 704, 100
33761, V, 1, 1, 1, 1, 0, 704, 100
33762, V, 1, 1, 1, 1, 0, 704, 100
33763, V, 1, 1, 1, 1, 0, 704, 100
33764, V, 1, 1, 1, 1, 0, 704, 100
33765, V, 1, 1, 1, 1, 0, 704, 100
33766, V, 1, 1, 1, 1, 0, 704, 100
33767, V, 1, 1, 1, 1, 0, 704, 100
33768, V, 1, 1, 1, 1, 0, 704, 100
33769, V, 1, 1, 1, 1, 0, 704, 100
33770, V, 1, 1, 1, 1, 0, 704, 100
33771, V, 1, 1, 1, 1, 0, 704, 100
33772, V, 1, 1, 1, 1, 0, 704, 100
33773, V, 1, 1, 1, 1, 0, 704, 100
33774, V, 1, 1, 1, 1, 0, 704, 100
33775, V, 1, 1, 1, 1, 0, 704, 100
33776, V, 1, 1, 1, 1, 0, 704, 100
33777, V, 1, 1, 1, 1, 0, 704, 100
33778, V, 1, 1, 1, 1, 0, 704, 100
33779, V, 1, 1, 1, 1, 0, 704, 100
33780, V, 1, 1, 1, 1, 0, 704, 100
33781, V, 1, 1, 1, 1, 0, 704, 100
33782, V, 1, 1, 1, 1, 0, 704, 100
33783, V, 1, 1, 1, 1, 0, 704, 100
33784, V, 1, 1, 1, 1, 0, 704, 100
33785, V, 1, 1, 1, 1, 0, 704, 100
33786, V, 1, 1, 1, 1, 0, 704, 100
33787, V, 1, 1, 1, 1, 0, 704, 100
33788, V, 1, 1, 1, 1, 0, 704, 100
33789, V, 1, 1, 1, 1, 0, 704, 100
33790, V, 1, 1, 1, 1, 0, 704, 100
33792, V, 1, 1, 1, 1, 0, 704, 100
33793, V, 1, 1, 1, 1, 0, 704, 100
33794, V, 1, 1, 1, 1, 0, 704, 100
33795, V, 1, 1, 1, 1, 0, 704, 100
33796, V, 1, 1, 1, 1, 0, 704, 100
33797, V, 1, 1, 1, 1, 0, 704, 100
33798, V, 1, 1, 1, 1, 0, 704, 100
33799, V, 1, 1, 1, 1, 0, 704, 100
33800, V, 1, 1, 1, 1, 0, 704, 100
33801, V, 1, 1, 1, 1, 0, 704, 100
33802, V, 1, 1, 1, 1, 0, 704, 100
33803, V, 1, 1, 1, 1, 0, 704, 100
33804, V, 1, 1, 1, 1, 0, 704, 100
33805, V, 1, 1, 1, 1, 0, 704, 100
33806, V, 1, 1, 1, 1, 0, 704, 100
33807, V, 1, 1, 1, 1, 0, 704, 100
33808, V, 1, 1, 1, 1, 0, 704, 100
33809, V, 1, 1, 1, 1, 0, 704, 100
33810, V, 1, 1, 1, 1, 0, 704, 100
33811, V, 1, 1, 1, 1, 0, 704, 100
33812, V, 1, 1, 1, 1, 0, 704, 100
33813, V, 1, 1, 1, 1, 0, 704, 100
33814, V, 1, 1, 1, 1, 0, 704, 100
33815, V, 1, 1, 1, 1, 0, 704, 100
33816, V, 1, 1, 1, 1, 0, 704, 100
33817, V, 1, 1, 1, 1, 0, 704, 100
33818, V, 1, 1, 1, 1, 0, 704, 100
33819, V, 1, 1, 1, 1, 0, 704, 100
33820, V, 1, 1, 1, 1, 0, 704, 100
33821, V, 1, 1, 1, 1, 0, 704, 100
33822, V, 1, 1, 1, 1, 0, 704, 100
33823, V, 1, 1, 1, 1, 0, 704, 100
33824, V, 1, 1, 1, 1, 0, 704, 100
33825, V, 1, 1, 1, 1, 0, 704, 100
33826, V, 1, 1, 1, 1, 0, 704, 100
33827, V, 1, 1, 1, 1, 0, 704, 100
33828, V, 1, 1, 1, 1, 0, 704, 100
33829, V, 1, 1, 1, 1, 0, 704, 100
33830, V, 1, 1, 1, 1, 0, 704, 100
33831, V, 1, 1, 1, 1, 0, 704, 100
33832, V, 1, 1, 1, 1, 0, 704, 100
33833, V, 1, 1, 1, 1, 0, 704, 100
33835, V, 1, 1, 1, 1, 0, 704, 100
33836, V, 1, 1, 1, 1, 0, 704, 100
33837, V, 1, 1, 1, 1, 0, 704, 100
33838, V, 1, 1, 1, 1, 0, 704, 100
33839, V, 1, 1, 1, 1, 0, 704, 100
33840, V, 1, 1, 1, 1, 0, 704, 100
33841, V, 1, 1, 1, 1, 0, 704, 100
33842, V, 1, 1, 1, 1, 0, 704, 100
33843, V, 1, 1, 1, 1, 0, 704, 100
33844, V, 1, 1, 1, 1, 0, 704, 100
33845, V, 1, 1, 1, 1, 0, 704, 100
33846, V, 1, 1, 1, 1, 0, 704, 100
33847, V, 1, 1, 1, 1, 0, 704, 100
33848, V, 1, 1, 1, 1, 0, 704, 100
33849, V, 1, 1, 1, 1, 0, 704, 100
33850, V, 1, 1, 1, 1, 0, 704, 100
33851, V, 1, 1, 1, 1, 0, 704, 100
33852, V, 1, 1, 1, 1, 0, 704, 100
33853, V, 1, 1, 1, 1, 0, 704, 100
33854, V, 1, 1, 1, 1, 0, 704, 100
33855, V, 1, 1, 1, 1, 0, 704, 100
33856, V, 1, 1, 1, 1, 0, 704, 100
33857, V, 1, 1, 1, 1, 0, 704, 100
33858, V, 1, 1, 1, 1, 0, 704, 100
33859, V, 1, 1, 1, 1, 0, 704, 100
33860, V, 1, 1, 1, 1, 0, 704, 100
33861, V, 1, 1, 1, 1, 0, 704, 100
33862, V, 1, 1, 1, 1, 0, 704, 100
33863, V, 1, 1, 1, 1, 0, 704, 100
33864, V, 1, 1, 1, 1, 0, 704, 100
33865, V, 1, 1, 1, 1, 0, 704, 100
33866, V, 1, 1, 1, 1, 0, 704, 100
33867, V, 1, 1, 1, 1, 0, 704, 100
33868, V, 1, 1, 1, 1, 0, 704, 100
33869, V, 1, 1, 1, 1, 0, 704, 100
33870, V, 1, 1, 1, 1, 0, 704, 100
33871, V, 1, 1, 1, 1, 0, 704, 100
33872, V, 1, 1, 1, 1, 0, 704, 100
33873, V, 1, 1, 1, 1, 0, 704, 100
33874, V, 1, 1, 1, 1, 0, 704, 100
33875, V, 1, 1, 1, 1, 0, 704, 100
33876, V, 1, 1, 1, 1, 0, 704, 100
33878, V, 1, 1, 1, 1, 0, 704, 100
33879, V, 1, 1, 1, 1, 0, 704, 100
33880, V, 1, 1, 1, 1, 0, 704, 100
33881, V, 1, 1, 1, 1, 0, 704, 100
33882, V, 1, 1, 1, 1, 0, 704, 100
33883, V, 1, 1, 1, 1, 0, 704, 100
33884, V, 1, 1, 1, 1, 0, 704, 100
33885, V, 1, 1, 1, 1, 0, 704, 100
33886, V, 1, 1, 1, 1, 0, 704, 100
33887, V, 1, 1, 1, 1, 0, 704, 100
33888, V, 1, 1, 1, 1, 0, 704, 100
33889, V, 1, 1, 1, 1, 0, 704, 100
33890, V, 1, 1, 1, 1, 0, 704, 100
33891, V, 1, 1, 1, 1, 0, 704, 100
33892, V, 1, 1, 1, 1, 0, 704, 100
33893, V, 1, 1, 1, 1, 0, 704, 100
33894, V, 1, 1, 1, 1, 0, 704, 100
33895, V, 1, 1, 1, 1, 0, 704, 100
33896, V, 1, 1, 1, 1, 0, 704, 100
33897, V, 1, 1, 1, 1, 0, 704, 100
33898, V, 1, 1, 1, 1, 0, 704, 100
33899, V, 1, 1, 1, 1, 0, 704, 100
33900, V, 1, 1, 1, 1, 0, 704, 100
33901, V, 1, 1, 1, 1, 0, 704, 100
33902, V, 1, 1, 1, 1, 0, 704, 100
33903, V, 1, 1, 1, 1, 0, 704, 100
33904, V, 1, 1, 1, 1, 0, 704, 100
33905, V, 1, 1, 1, 1, 0, 704, 100
33906, V, 1, 1, 1, 1, 0, 704, 100
33907, V, 1, 1, 1, 1, 0, 704, 100
33908, V, 1, 1, 1, 1, 0, 704, 100
33909, V, 1, 1, 1, 1, 0, 704, 100
33910, V, 1, 1, 1, 1, 0, 704, 100
33911, V, 1, 1, 1, 1, 0, 704, 100
33912, V, 1, 1, 1, 1, 0, 704, 100
33913, V, 1, 1, 1, 1, 0, 704, 100
33914, V, 1, 1, 1, 1, 0, 704, 100
33915, V, 1, 1, 1, 1, 0, 704, 100
33916, V, 1, 1, 1, 1, 0, 704, 100
33917, V, 1, 1, 1, 1, 0, 704, 100
33918, V, 1, 1, 1, 1, 0, 704, 100
33920, V, 1, 1, 1, 1, 0, 704, 100
33921, V, 1, 1, 1, 1, 0, 704, 100
33922, V, 1, 1, 1, 1, 0, 704, 100
33923, V, 1, 1, 1, 1, 0, 704, 100
33924, V, 1, 1, 1, 1, 0, 704, 100
33925, V, 1, 1, 1, 1, 0, 704, 100
33926, V, 1, 1, 1, 1, 0, 704, 100
33927, V, 1, 1, 1, 1, 0, 704, 100
33928, V, 1, 1, 1, 1, 0, 704, 100
33929, V, 1, 1, 1, 1, 0, 704, 100
33930, V, 1, 1, 1, 1, 0, 704, 100
33931, V, 1, 1, 1, 1, 0, 704, 100
33932, V, 1, 1, 1, 1, 0, 704, 100
33933, V, 1, 1, 1, 1, 0, 704, 100
33934, V, 1, 1, 1, 1, 0, 704, 100
33935, V, 1, 1, 1, 1, 0, 704, 100
33936, V, 1, 1, 1, 1, 0, 704, 100
33937, V, 1, 1, 1, 1, 0, 704, 100
33938, V, 1, 1, 1, 1, 0, 704, 100
33939, V, 1, 1, 1, 1, 0, 704, 100
33940, V, 1, 1, 1, 1, 0, 704, 100
33941, V, 1, 1, 1, 1, 0, 704, 100
33942, V, 1, 1, 1, 1, 0, 704, 100
33943, V, 1, 1, 1, 1, 0, 704, 100
33944, V, 1, 1, 1, 1, 0, 704, 100
33945, V, 1, 1, 1, 1, 0, 704, 100
33946, V, 1, 1, 1, 1, 0, 704, 100
33947, V, 1, 1, 1, 1, 0, 704, 100
33948, V, 1, 1, 1, 1, 0, 704, 100
33949, V, 1, 1, 1, 1, 0, 704, 100
33950, V, 1, 1, 1, 1, 0, 704, 100
33951, V, 1, 1, 1, 1, 0, 704, 100
33952, V, 1, 1, 1, 1, 0, 704, 100
33953, V, 1, 1, 1, 1, 0, 704, 100
33954, V, 1, 1, 1, 1, 0, 704, 100
33955, V, 1, 1, 1, 1, 0, 704, 100
33956, V, 1, 1, 1, 1, 0, 704, 100
33957, V, 1, 1, 1, 1, 0, 704, 100
33958, V, 1, 1, 1, 1, 0, 704, 100
33959, V, 1, 1, 1, 1, 0, 704, 100
33960, V, 1, 1, 1, 1, 0, 704, 100
33961, V, 1, 1, 1, 1, 0, 704, 100
33963, V, 1, 1, 1, 1, 0, 704, 100
33964, V, 1, 1, 1, 1, 0, 704, 100
33965, V, 1, 1, 1, 1, 0, 704, 100
33966, V, 1, 1, 1, 1, 0, 704, 100
33967, V, 1, 1, 1, 1, 0, 704, 100
33968, V, 1, 1, 1, 1, 0, 704, 100
33969, V, 1, 1, 1, 1, 0, 704, 100
33970, V, 1, 1, 1, 1, 0, 704, 100
33971, V, 1, 1, 1, 1, 0, 704, 100
33972, V, 1, 1, 1, 1, 0, 704, 100
33973, V, 1, 1, 1, 1, 0, 704, 100
33974, V, 1, 1, 1, 1, 0, 704, 100
33975, V, 1, 1, 1, 1, 0, 704, 100
33976, V, 1, 1, 1, 1, 0, 704, 100
33977, V, 1, 1, 1, 1, 0, 704, 100
33978, V, 1, 1, 1, 1, 0, 704, 100
33979, V, 1, 1, 1, 1, 0, 704, 100
33980, V, 1, 1, 1, 1, 0, 704, 100
33981, V, 1, 1, 1, 1, 0, 704, 100
33982, V, 1, 1, 1, 1, 0, 704, 100
33983, V, 1, 1, 1, 1, 0, 704, 100
33984, V, 1, 1, 1, 1, 0, 704, 100
33985, V, 1, 1, 1, 1, 0, 704, 100
33986, V, 1, 1, 1, 1, 0, 704, 100
33987, V, 1, 1, 1, 1, 0, 704, 100
33988, V, 1, 1, 1, 1, 0, 704, 100
33989, V, 1, 1, 1, 1, 0, 704, 100
33990, V, 1, 1, 1, 1, 0, 704, 100
33991, V, 1, 1, 1, 1, 0, 704, 100
33992, V, 1, 1, 1, 1, 0, 704, 100
33993, V, 1, 1, 1, 1, 0, 704, 100
33994, V, 1, 1, 1, 1, 0, 704, 100
33995, V, 1, 1, 1, 1, 0, 704, 100
33996, V, 1, 1, 1, 1, 0, 704, 100
33997, V, 1, 1, 1, 1, 0, 704, 100
33998, V, 1, 1, 1, 1, 0, 704, 100
33999, V, 1, 1, 1, 1, 0, 704, 100
34000, V, 1, 1, 1, 1, 0, 704, 100
34001, V, 1, 1, 1, 1, 0, 704, 100
34002, V, 1, 1, 1, 1, 0, 704, 100
34003, V, 1, 1, 1, 1, 0, 704, 100
34004, V, 1, 1, 1, 1, 0, 704, 100
34006, V, 1, 1, 1, 1, 0, 704, 100
34007, V, 1, 1, 1, 1, 0, 704, 100
34008, V, 1, 1, 1, 1, 0, 704, 100
34009, V, 1, 1, 1, 1, 0, 704, 100
34010, V, 1, 1, 1, 1, 0, 704, 100
34011, V, 1, 1, 1, 1, 0, 704, 100
34012, V, 1, 1, 1, 1, 0, 704, 100
34013, V, 1, 1, 1, 1, 0, 704, 100
34014, V, 1, 1, 1, 1, 0, 704, 100
34015, V, 1, 1, 1, 1, 0, 704, 100
34016, V, 1, 1, 1, 1, 0, 704, 100
34017, V, 1, 1, 1, 1, 0, 704, 100
34018, V, 1, 1, 1, 1, 0, 704, 100
34019, V, 1, 1, 1, 1, 0, 704, 100
34020, V, 1, 1, 1, 1, 0, 704, 100
34021, V, 1, 1, 1, 1, 0, 704, 100
34022, V, 1, 1, 1, 1, 0, 704, 100
34023, V, 1, 1, 1, 1, 0, 704, 100
34024, V, 1, 1, 1, 1, 0, 704, 100
34025, V, 1, 1, 1, 1, 0, 704, 100
34026, V, 1, 1, 1, 1, 0, 704, 100
34027, V, 1, 1, 1, 1, 0, 704, 100
34028, V, 1, 1, 1, 1, 0, 704, 100
34029, V, 1, 1, 1, 1, 0, 704, 100
34030, V, 1, 1, 1, 1, 0, 704, 100
34031, V, 1, 1, 1, 1, 0, 704, 100
34032, V, 1, 1, 1, 1, 0, 704, 100
34033, V, 1, 1, 1, 1, 0, 704, 100
34034, V, 1, 1, 1, 1, 0, 704, 100
34035, V, 1, 1, 1, 1, 0, 704, 100
34036, V, 1, 1, 1, 1, 0, 704, 100
34037, V, 1, 1, 1, 1, 0, 704, 100
34038, V, 1, 1, 1, 1, 0, 704, 100
34039, V, 1, 1, 1, 1, 0, 704, 100
34040, V, 1, 1, 1, 1, 0, 704, 100
34041, V, 1, 1, 1, 1, 0, 704, 100
34042, V, 1, 1, 1, 1, 0, 704, 100
34043, V, 1, 1, 1, 1, 0, 704, 100
34044, V, 1, 1, 1, 1, 0, 704, 100
34045, V, 1, 1, 1, 1, 0, 704, 100
34046, V, 1, 1, 1, 1, 0, 704, 100
34048, V, 1, 1, 1, 1, 0, 704, 100
34049, V, 1, 1, 1, 1, 0, 704, 100
34050, V, 1, 1, 1, 1, 0, 704, 100
34051, V, 1, 1, 1, 1, 0, 704, 100
34052, V, 1, 1, 1, 1, 0, 704, 100
34053, V, 1, 1, 1, 1, 0, 704, 100
34054, V, 1, 1, 1, 1, 0, 704, 100
34055, V, 1, 1, 1, 1, 0, 704, 100
34056, V, 1, 1, 1, 1, 0, 704, 100
34057, V, 1, 1, 1, 1, 0, 704, 100
34058, V, 1, 1, 1, 1, 0, 704, 100
34059, V, 1, 1, 1, 1, 0, 704, 100
34060, V, 1, 1, 1, 1, 0, 704, 100
34061, V, 1, 1, 1, 1, 0, 704, 100
34062, V, 1, 1, 1, 1, 0, 704, 100
34063, V, 1, 1, 1, 1, 0, 704, 100
34064, V, 1, 1, 1, 1, 0, 704, 100
34065, V, 1, 1, 1, 1, 0, 704, 100
34066, V, 1, 1, 1, 1, 0, 704, 100
34067, V, 1, 1, 1, 1, 0, 704, 100
34068, V, 1, 1, 1, 1, 0, 704, 100
34069, V, 1, 1, 1, 1, 0, 704, 100
34070, V, 1, 1, 1, 1, 0, 704, 100
34071, V, 1, 1, 1, 1, 0, 704, 100
34072, V, 1, 1, 1, 1, 0, 704, 100
34073, V, 1, 1, 1, 1, 0, 704, 100
34074, V, 1, 1, 1, 1, 0, 704, 100
34075, V, 1, 1, 1, 1, 0, 704, 100
34076, V, 1, 1, 1, 1, 0, 704, 100
34077, V, 1, 1, 1, 1, 0, 704, 100
34078, V, 1, 1, 1, 1, 0, 704, 100
34079, V, 1, 1, 1, 1, 0, 704, 100
34080, V, 1, 1, 1, 1, 0, 704, 100
34081, V, 1, 1, 1, 1, 0, 704, 100
34082, V, 1, 1, 1, 1, 0, 704, 100
34083, V, 1, 1, 1, 1, 0, 704, 100
34084, V, 1, 1, 1, 1, 0, 704, 100
34085, V, 1, 1, 1, 1, 0, 704, 100
34086, V, 1, 1, 1, 1, 0, 704, 100
34087, V, 1, 1, 1, 1, 0, 704, 100
34088, V, 1, 1, 1, 1, 0, 704, 100
34089, V, 1, 1, 1, 1, 0, 704, 100
34091, V, 1, 1, 1, 1, 0, 704, 100
34092, V, 1, 1, 1, 1, 0, 704, 100
34093, V, 1, 1, 1, 1, 0, 704, 100
34094, V, 1, 1, 1, 1, 0, 704, 100
34095, V, 1, 1, 1, 1, 0, 704, 100
34096, V, 1, 1, 1, 1, 0, 704, 100
34097, V, 1, 1, 1, 1, 0, 704, 100
34098, V, 1, 1, 1, 1, 0, 704, 100
34099, V, 1, 1, 1, 1, 0, 704, 100
34100, V, 1, 1, 1, 1, 0, 704, 100
34101, V, 1, 1, 1, 1, 0, 704, 100
34102, V, 1, 1, 1, 1, 0, 704, 100
34103, V, 1, 1, 1, 1, 0, 704, 100
34104, V, 1, 1, 1, 1, 0, 704, 100
34105, V, 1, 1, 1, 1, 0, 704, 100
34106, V, 1, 1, 1, 1, 0, 704, 100
34107, V, 1, 1, 1, 1, 0, 704, 100
34108, V, 1, 1, 1, 1, 0, 704, 100
34109, V, 1, 1, 1, 1, 0, 704, 100
34110, V, 1, 1, 1, 1, 0, 704, 100
34111, V, 1, 1, 1, 1, 0, 704, 100
34112, V, 1, 1, 1, 1, 0, 704, 100
34113, V, 1, 1, 1, 1, 0, 704, 100
34114, V, 1, 1, 1, 1, 0, 704, 100
34115, V, 1, 1, 1, 1, 0, 704, 100
34116, V, 1, 1, 1, 1, 0, 704, 100
34117, V, 1, 1, 1, 1, 0, 704, 100
34118, V, 1, 1, 1, 1, 0, 704, 100
34119, V, 1, 1, 1, 1, 0, 704, 100
34120, V, 1, 1, 1, 1, 0, 704, 100
34121, V, 1, 1, 1, 1, 0, 704, 100
34122, V, 1, 1, 1, 1, 0, 704, 100
34123, V, 1, 1, 1, 1, 0, 704, 100
34124, V, 1, 1, 1, 1, 0, 704, 100
34125, V, 1, 1, 1, 1, 0, 704, 100
34126, V, 1, 1, 1, 1, 0, 704, 100
34127, V, 1, 1, 1, 1, 0, 704, 100
34128, V, 1, 1, 1, 1, 0, 704, 100
34129, V, 1, 1, 1, 1, 0, 704, 100
34130, V, 1, 1, 1, 1, 0, 704, 100
34131, V, 1, 1, 1, 1, 0, 704, 100
34132, V, 1, 1, 1, 1, 0, 704, 100
34134, V, 1, 1, 1, 1, 0, 704, 100
34135, V, 1, 1, 1, 1, 0, 704, 100
34136, V, 1, 1, 1, 1, 0, 704, 100
34137, V, 1, 1, 1, 1, 0, 704, 100
34138, V, 1, 1, 1, 1, 0, 704, 100
34139, V, 1, 1, 1, 1, 0, 704, 100
34140, V, 1, 1, 1, 1, 0, 704, 100
34141, V, 1, 1, 1, 1, 0, 704, 100
34142, V, 1, 1, 1, 1, 0, 704, 100
34143, V, 1, 1, 1, 1, 0, 704, 100
34144, V, 1, 1, 1, 1, 0, 704, 100
34145, V, 1, 1, 1, 1, 0, 704, 100
34146, V, 1, 1, 1, 1, 0, 704, 100
34147, V, 1, 1, 1, 1, 0, 704, 100
34148, V, 1, 1, 1, 1, 0, 704, 100
34149, V, 1, 1, 1, 1, 0, 704, 100
34150, V, 1, 1, 1, 1, 0, 704, 100
34151, V, 1, 1, 1, 1, 0, 704, 100
34152, V, 1, 1, 1, 1, 0, 704, 100
34153, V, 1, 1, 1, 1, 0, 704, 100
34154, V, 1, 1, 1, 1, 0, 704, 100
34155, V, 1, 1, 1, 1, 0, 704, 100
34156, V, 1, 1, 1, 1, 0, 704, 100
34157, V, 1, 1, 1, 1, 0, 704, 100
34158, V, 1, 1, 1, 1, 0, 704, 100
34159, V, 1, 1, 1, 1, 0, 704, 100
34160, V, 1, 1, 1, 1, 0, 704, 100
34161, V, 1, 1, 1, 1, 0, 704, 100
34162, V, 1, 1, 1, 1, 0, 704, 100
34163, V, 1, 1, 1, 1, 0, 704, 100
34164, V, 1, 1, 1, 1, 0, 704, 100
34165, V, 1, 1, 1, 1, 0, 704, 100
34166, V, 1, 1, 1, 1, 0, 704, 100
34167, V, 1, 1, 1, 1, 0, 704, 100
34168, V, 1, 1, 1, 1, 0, 704, 100
34169, V, 1, 1, 1, 1, 0, 704, 100
34170, V, 1, 1, 1, 1, 0, 704, 100
34171, V, 1, 1, 1, 1, 0, 704, 100
34172, V, 1, 1, 1, 1, 0, 704, 100
34173, V, 1, 1, 1, 1, 0, 704, 100
34174, V, 1, 1, 1, 1, 0, 704, 100
34176, V, 1, 1, 1, 1, 0, 704, 100
34177, V, 1, 1, 1, 1, 0, 704, 100
34178, V, 1, 1, 1, 1, 0, 704, 100
34179, V, 1, 1, 1, 1, 0, 704, 100
34180, V, 1, 1, 1, 1, 0, 704, 100
34181, V, 1, 1, 1, 1, 0, 704, 100
34182, V, 1, 1, 1, 1, 0, 704, 100
34183, V, 1, 1, 1, 1, 0, 704, 100
34184, V, 1, 1, 1, 1, 0, 704, 100
34185, V, 1, 1, 1, 1, 0, 704, 100
34186, V, 1, 1, 1, 1, 0, 704, 100
34187, V, 1, 1, 1, 1, 0, 704, 100
34188, V, 1, 1, 1, 1, 0, 704, 100
34189, V, 1, 1, 1, 1, 0, 704, 100
34190, V, 1, 1, 1, 1, 0, 704, 100
34191, V, 1, 1, 1, 1, 0, 704, 100
34192, V, 1, 1, 1, 1, 0, 704, 100
34193, V, 1, 1, 1, 1, 0, 704, 100
34194, V, 1, 1, 1, 1, 0, 704, 100
34195, V, 1, 1, 1, 1, 0, 704, 100
34196, V, 1, 1, 1, 1, 0, 704, 100
34197, V, 1, 1, 1, 1, 0, 704, 100
34198, V, 1, 1, 1, 1, 0, 704, 100
34199, V, 1, 1, 1, 1, 0, 704, 100
34200, V, 1, 1, 1, 1, 0, 704, 100
34201, V, 1, 0, 0, 1, 0, 704, 100
34201, V, 1, 0, 0, 0, 0, 704, 100
34202, V, 1, 1, 0, 0, 0, 704, 100
34202, V, 1, 1, 0, 0, 0, 704, 100
34203, V, 1, 1, 1, 1, 0, 704, 100
34204, V, 1, 1, 1, 1, 0, 704, 100
34205, V, 1, 1, 1, 1, 0, 704, 100
34206, V, 1, 1, 1, 1, 0, 704, 100
34207, V, 1, 1, 1, 1, 0, 704, 100
34208, V, 1, 1, 1, 1, 0, 704, 99
34209, V, 1, 1, 1, 1, 0, 704, 99
34210, V, 1, 1, 1, 1, 0, 704, 99
34211, V, 1, 1, 1, 1, 0, 704, 99
34212, V, 1, 1, 1, 1, 0, 704, 99
34213, V, 1, 1, 1, 1, 0, 704, 99
34214, V, 1, 1, 1, 1, 0, 704, 99
34215, V, 1, 1, 1, 1, 0, 704, 99
34216, V, 1, 1, 1, 1, 0, 704, 99
34217, V, 1, 1, 1, 1, 0, 704, 99
34219, V, 1, 1, 1, 1, 0, 704, 99
34220, V, 1, 1, 1, 1, 0, 704, 99
34221, V, 1, 1, 1, 1, 0, 704, 99
34222, V, 1, 1, 1, 1, 0, 704, 99
34223, V, 1, 1, 1, 1, 0, 704, 99
34224, V, 1, 1, 1, 1, 0, 704, 99
34225, V, 1, 1, 1, 1, 0, 704, 100
34226, V, 1, 1, 1, 1, 0, 704, 99
34227, V, 1, 1, 1, 1, 0, 704, 99
34228, V, 1, 1, 1, 1, 0, 704, 99
34229, V, 1, 1, 1, 1, 0, 704, 99
34230, V, 1, 1, 1, 1, 0, 704, 99
34231, V, 1, 1, 1, 1, 0, 704, 99
34232, V, 1, 1, 1, 1, 0, 704, 100
34233, V, 1, 1, 1, 1, 0, 704, 99
34234, V, 1, 1, 1, 1, 0, 704, 99
34235, V, 1, 1, 1, 1, 0, 704, 100
34236, V, 1, 1, 1, 1, 0, 704, 99
34237, V, 1, 1, 1, 1, 0, 704, 100
34238, V, 1, 1, 1, 1, 0, 704, 99
34239, V, 1, 1, 1, 1, 0, 704, 100
34240, V, 1, 1, 1, 1, 0, 704, 99
34241, V, 1, 1, 1, 1, 0, 704, 99
34242, V, 1, 1, 1, 1, 0, 704, 100
34243, V, 1, 1, 1, 1, 0, 704, 99
34244, V, 1, 1, 1, 1, 0, 704, 100
34245, V, 1, 1, 1, 1, 0, 704, 100
34246, V, 1, 1, 1, 1, 0, 704, 99
34247, V, 1, 1, 1, 1, 0, 704, 99
34248, V, 1, 1, 1, 1, 0, 704, 100
34249, V, 1, 1, 1, 1, 0, 704, 100
34250, V, 1, 1, 1, 1, 0, 704, 100
34251, V, 1, 1, 1, 1, 0, 704, 100
34252, V, 1, 1, 1, 1, 0, 704, 100
34253, V, 1, 1, 1, 1, 0, 704, 100
34254, V, 1, 1, 1, 1, 0, 704, 100
34255, V, 1, 1, 1, 1, 0, 704, 100
34256, V, 1, 1, 1, 1, 0, 704, 100
34257, V, 1, 1, 1, 1, 0, 704, 100
34258, V, 1, 1, 1, 1, 0, 704, 100
34259, V, 1, 1, 1, 1, 0, 704, 100
34260, V, 1, 1, 1, 1, 0, 704, 100
34262, V, 1, 1, 1, 1, 0, 704, 100
34263, V, 1, 1, 1, 1, 0, 704, 100
34264, V, 1, 1, 1, 1, 0, 704, 100
34265, V, 1, 1, 1, 1, 0, 704, 100
34266, V, 1, 1, 1, 1, 0, 704, 100
34267, V, 1, 1, 1, 1, 0, 704, 100
34268, V, 1, 1, 1, 1, 0, 704, 100
34269, V, 1, 1, 1, 1, 0, 704, 100
34270, V, 1, 1, 1, 1, 0, 704, 100
34271, V, 1, 1, 1, 1, 0, 704, 100
34272, V, 1, 1, 1, 1, 0, 704, 100
34273, V, 1, 1, 1, 1, 0, 704, 100
34274, V, 1, 1, 1, 1, 0, 704, 100
34275, V, 1, 1, 1, 1, 0, 704, 100
34276, V, 1, 1, 1, 1, 0, 704, 100
34277, V, 1, 1, 1, 1, 0, 704, 100
34278, V, 1, 1, 1, 1, 0, 704, 100
34279, V, 1, 1, 1, 1, 0, 704, 100
34280, V, 1, 1, 1, 1, 0, 704, 100
34281, V, 1, 1, 1, 1, 0, 704, 100
34282, V, 1, 1, 1, 1, 0, 704, 100
34283, V, 1, 1, 1, 1, 0, 704, 100
34284, V, 1, 1, 1, 1, 0, 704, 100
34285, V, 1, 1, 1, 1, 0, 704, 100
34286, V, 1, 1, 1, 1, 0, 704, 100
34287, V, 1, 1, 1, 1, 0, 704, 100
34288, V, 1, 1, 1, 1, 0, 704, 100
34289, V, 1, 1, 1, 1, 0, 704, 100
34290, V, 1, 1, 1, 1, 0, 704, 100
34291, V, 1, 1, 1, 1, 0, 704, 100
34292, V, 1, 1, 1, 1, 0, 704, 100
34293, V, 1, 1, 1, 1, 0, 704, 100
34294, V, 1, 1, 1, 1, 0, 704, 100
34295, V, 1, 1, 1, 1, 0, 704, 100
34296, V, 1, 1, 1, 1, 0, 704, 100
34297, V, 1, 1, 1, 1, 0, 704, 100
34298, V, 1, 1, 1, 1, 0, 704, 100
34299, V, 1, 1, 1, 1, 0, 704, 100
34300, V, 1, 1, 1, 1, 0, 704, 100
34301, V, 1, 1, 1, 1, 0, 704, 100
34302, V, 1, 1, 1, 1, 0, 704, 100
34304, V, 1, 1, 1, 1, 0, 704, 100
34305, V, 1, 1, 1, 1, 0, 704, 100
34306, V, 1, 1, 1, 1, 0, 704, 100
34307, V, 1, 1, 1, 1, 0, 704, 100
34308, V, 1, 1, 1, 1, 0, 704, 100
34309, V, 1, 1, 1, 1, 0, 704, 100
34310, V, 1, 1, 1, 1, 0, 704, 100
34311, V, 1, 1, 1, 1, 0, 704, 100
34312, V, 1, 1, 1, 1, 0, 704, 100
34313, V, 1, 1, 1, 1, 0, 704, 100
34314, V, 1, 1, 1, 1, 0, 704, 100
34315, V, 1, 1, 1, 1, 0, 704, 100
34316, V, 1, 1, 1, 1, 0, 704, 100
34317, V, 1, 1, 1, 1, 0, 704, 100
34318, V, 1, 1, 1, 1, 0, 704, 100
34319, V, 1, 1, 1, 1, 0, 704, 100
34320, V, 1, 1, 1, 1, 0, 704, 100
34321, V, 1, 1, 1, 1, 0, 704, 100
34322, V, 1, 1, 1, 1, 0, 704, 100
34323, V, 1, 1, 1, 1, 0, 704, 100
34324, V, 1, 1, 1, 1, 0, 704, 100
34325, V, 1, 1, 1, 1, 0, 704, 100
34326, V, 1, 1, 1, 1, 0, 704, 100
34327, V, 1, 1, 1, 1, 0, 704, 100
34328, V, 1, 1, 1, 1, 0, 704, 100
34329, V, 1, 1, 1, 1, 0, 704, 100
34330, V, 1, 1, 1, 1, 0, 704, 100
34331, V, 1, 1, 1, 1, 0, 704, 100
34332, V, 1, 1, 1, 1, 0, 704, 100
34333, V, 1, 1, 1, 1, 0, 704, 100
34334, V, 1, 1, 1, 1, 0, 704, 100
34335, V, 1, 1, 1, 1, 0, 704, 100
34336, V, 1, 1, 1, 1, 0, 704, 100
34337, V, 1, 1, 1, 1, 0, 704, 100
34338, V, 1, 1, 1, 1, 0, 704, 100
34339, V, 1, 1, 1, 1, 0, 704, 100
34340, V, 1, 1, 1, 1, 0, 704, 100
34341, V, 1, 1, 1, 1, 0, 704, 100
34342, V, 1, 1, 1, 1, 0, 704, 100
34343, V, 1, 1, 1, 1, 0, 704, 100
34344, V, 1, 1, 1, 1, 0, 704, 100
34345, V, 1, 1, 1, 1, 0, 704, 100
34347, V, 1, 1, 1, 1, 0, 704, 100
34348, V, 1, 1, 1, 1, 0, 704, 100
34349, V, 1, 1, 1, 1, 0, 704, 100
34350, V, 1, 1, 1, 1, 0, 704, 100
34351, V, 1, 1, 1, 1, 0, 704, 100
34352, V, 1, 1, 1, 1, 0, 704, 100
34353, V, 1, 1, 1, 1, 0, 704, 100
34354, V, 1, 1, 1, 1, 0, 704, 100
34355, V, 1, 1, 1, 1, 0, 704, 100
34356, V, 1, 1, 1, 1, 0, 704, 100
34357, V, 1, 1, 1, 1, 0, 704, 100
34358, V, 1, 1, 1, 1, 0, 704, 100
34359, V, 1, 1, 1, 1, 0, 704, 100
34360, V, 1, 1, 1, 1, 0, 704, 100
34361, V, 1, 1, 1, 1, 0, 704, 100
34362, V, 1, 1, 1, 1, 0, 704, 100
34363, V, 1, 1, 1, 1, 0, 704, 100
34364, V, 1, 1, 1, 1, 0, 704, 100
34365, V, 1, 1, 1, 1, 0, 704, 100
34366, V, 1, 1, 1, 1, 0, 704, 100
34367, V, 1, 1, 1, 1, 0, 704, 100
34368, V, 1, 1, 1, 1, 0, 704, 100
34369, V, 1, 1, 1, 1, 0, 704, 100
34370, V, 1, 1, 1, 1, 0, 704, 100
34371, V, 1, 1, 1, 1, 0, 704, 100
34372, V, 1, 1, 1, 1, 0, 704, 100
34373, V, 1, 1, 1, 1, 0, 704, 100
34374, V, 1, 1, 1, 1, 0, 704, 100
34375, V, 1, 1, 1, 1, 0, 704, 100
34376, V, 1, 1, 1, 1, 0, 704, 100
34377, V, 1, 1, 1, 1, 0, 704, 100
34378, V, 1, 1, 1, 1, 0, 704, 100
34379, V, 1, 1, 1, 1, 0, 704, 100
34380, V, 1, 1, 1, 1, 0, 704, 100
34381, V, 1, 1, 1, 1, 0, 704, 100
34382, V, 1, 1, 1, 1, 0, 704, 100
34383, V, 1, 1, 1, 1, 0, 704, 100
34384, V, 1, 1, 1, 1, 0, 704, 100
34385, V, 1, 1, 1, 1, 0, 704, 100
34386, V, 1, 1, 1, 1, 0, 704, 100
34387, V, 1, 1, 1, 1, 0, 704, 100
34388, V, 1, 1, 1, 1, 0, 704, 100
34390, V, 1, 1, 1, 1, 0, 704, 100
34391, V, 1, 1, 1, 1, 0, 704, 100
34392, V, 1, 1, 1, 1, 0, 704, 100
34393, V, 1, 1, 1, 1, 0, 704, 100
34394, V, 1, 1, 1, 1, 0, 704, 100
34395, V, 1, 1, 1, 1, 0, 704, 100
34396, V, 1, 1, 1, 1, 0, 704, 100
34397, V, 1, 1, 1, 1, 0, 704, 100
34398, V, 1, 1, 1, 1, 0, 704, 100
34399, V, 1, 1, 1, 1, 0, 704, 100
34400, V, 1, 1, 1, 1, 0, 704, 100
34401, V, 1, 1, 1, 1, 0, 704, 100
34402, V, 1, 1, 1, 1, 0, 704, 100
34403, V, 1, 1, 1, 1, 0, 704, 100
34404, V, 1, 1, 1, 1, 0, 704, 100
34405, V, 1, 1, 1, 1, 0, 704, 100
34406, V, 1, 1, 1, 1, 0, 704, 100
34407, V, 1, 1, 1, 1, 0, 704, 100
34408, V, 1, 1, 1, 1, 0, 704, 100
34409, V, 1, 1, 1, 1, 0, 704, 100
34410, V, 1, 1, 1, 1, 0, 704, 100
34411, V, 1, 1, 1, 1, 0, 704, 100
34412, V, 1, 1, 1, 1, 0, 704, 100
34413, V, 1, 1, 1, 1, 0, 704, 100
34414, V, 1, 1, 1, 1, 0, 704, 100
34415, V, 1, 1, 1, 1, 0, 704, 100
34416, V, 1, 1, 1, 1, 0, 704, 100
34417, V, 1, 1, 1, 1, 0, 704, 100
34418, V, 1, 1, 1, 1, 0, 704, 100
34419, V, 1, 1, 1, 1, 0, 704, 100
34420, V, 1, 1, 1, 1, 0, 704, 100
34421, V, 1, 1, 1, 1, 0, 704, 100
34422, V, 1, 1, 1, 1, 0, 704, 100
34423, V, 1, 1, 1, 1, 0, 704, 100
34424, V, 1, 1, 1, 1, 0, 704, 100
34425, V, 1, 1, 1, 1, 0, 704, 100
34426, V, 1, 1, 1, 1, 0, 704, 100
34427, V, 1, 1, 1, 1, 0, 704, 100
34428, V, 1, 1, 1, 1, 0, 704, 100
34429, V, 1, 1, 1, 1, 0, 704, 100
34430, V, 1, 1, 1, 1, 0, 704, 100
34432, V, 1, 1, 1, 1, 0, 704, 100
34433, V, 1, 1, 1, 1, 0, 704, 100
34434, V, 1, 1, 1, 1, 0, 704, 100
34435, V, 1, 1, 1, 1, 0, 704, 100
34436, V, 1, 1, 1, 1, 0, 704, 100
34437, V, 1, 1, 1, 1, 0, 704, 100
34438, V, 1, 1, 1, 1, 0, 704, 100
34439, V, 1, 1, 1, 1, 0, 704, 100
34440, V, 1, 1, 1, 1, 0, 704, 100
34441, V, 1, 1, 1, 1, 0, 704, 100
34442, V, 1, 1, 1, 1, 0, 704, 100
34443, V, 1, 1, 1, 1, 0, 704, 100
34444, V, 1, 1, 1, 1, 0, 704, 100
34445, V, 1, 1, 1, 1, 0, 704, 100
34446, V, 1, 1, 1, 1, 0, 704, 100
34447, V, 1, 1, 1, 1, 0, 704, 100
34448, V, 1, 1, 1, 1, 0, 704, 100
34449, V, 1, 1, 1, 1, 0, 704, 100
34450, V, 1, 1, 1, 1, 0, 704, 100
34451, V, 1, 1, 1, 1, 0, 704, 100
34452, V, 1, 1, 1, 1, 0, 704, 100
34453, V, 1, 1, 1, 1, 0, 704, 100
34454, V, 1, 1, 1, 1, 0, 704, 100
34455, V, 1, 1, 1, 1, 0, 704, 100
34456, V, 1, 1, 1, 1, 0, 704, 100
34457, V, 1, 1, 1, 1, 0, 704, 100
34458, V, 1, 1, 1, 1, 0, 704, 100
34459, V, 1, 1, 1, 1, 0, 704, 100
34460, V, 1, 1, 1, 1, 0, 704, 100
34461, V, 1, 1, 1, 1, 0, 704, 100
34462, V, 1, 1, 1, 1, 0, 704, 100
34463, V, 1, 1, 1, 1, 0, 704, 100
34464, V, 1, 1, 1, 1, 0, 704, 100
34465, V, 1, 1, 1, 1, 0, 704, 100
34466, V, 1, 1, 1, 1, 0, 704, 100
34467, V, 1, 1, 1, 1, 0, 704, 100
34468, V, 1, 1, 1, 1, 0, 704, 100
34469, V, 1, 1, 1, 1, 0, 704, 100
34470, V, 1, 1, 1, 1, 0, 704, 100
34471, V, 1, 1, 1, 1, 0, 704, 100
34472, V, 1, 1, 1, 1, 0, 704, 100
34473, V, 1, 1, 1, 1, 0, 704, 100
34475, V, 1, 1, 1, 1, 0, 704, 100
34476, V, 1, 1, 1, 1, 0, 704, 100
34477, V, 1, 1, 1, 1, 0, 704, 100
34478, V, 1, 1, 1, 1, 0, 704, 100
34479, V, 1, 1, 1, 1, 0, 704, 100
34480, V, 1, 1, 1, 1, 0, 704, 100
34481, V, 1, 1, 1, 1, 0, 704, 100
34482, V, 1, 1, 1, 1, 0, 704, 100
34483, V, 1, 1, 1, 1, 0, 704, 100
34484, V, 1, 1, 1, 1, 0, 704, 100
34485, V, 1, 1, 1, 1, 0, 704, 100
34486, V, 1, 1, 1, 1, 0, 704, 100
34487, V, 1, 1, 1, 1, 0, 704, 100
34488, V, 1, 1, 1, 1, 0, 704, 100
34489, V, 1, 1, 1, 1, 0, 704, 100
34490, V, 1, 1, 1, 1, 0, 704, 100
34491, V, 1, 1, 1, 1, 0, 704, 100
34492, V, 1, 1, 1, 1, 0, 704, 100
34493, V, 1, 1, 1, 1, 0, 704, 100
34494, V, 1, 1, 1, 1, 0, 704, 100
34495, V, 1, 1, 1, 1, 0, 704, 100
34496, V, 1, 1, 1, 1, 0, 704, 100
34497, V, 1, 1, 1, 1, 0, 704, 100
34498, V, 1, 1, 1, 1, 0, 704, 100
34499, V, 1, 1, 1, 1, 0, 704, 100
34500, V, 1, 1, 1, 1, 0, 704, 100
34501, V, 1, 1, 1, 1, 0, 704, 100
34502, V, 1, 1, 1, 1, 0, 704, 100
34503, V, 1, 1, 1, 1, 0, 704, 100
34504, V, 1, 1, 1, 1, 0, 704, 100
34505, V, 1, 1, 1, 1, 0, 704, 100
34506, V, 1, 1, 1, 1, 0, 704, 100
34507, V, 1, 1, 1, 1, 0, 704, 100
34508, V, 1, 1, 1, 1, 0, 704, 100
34509, V, 1, 1, 1, 1, 0, 704, 100
34510, V, 1, 1, 1, 1, 0, 704, 100
34511, V, 1, 1, 1, 1, 0, 704, 100
34512, V, 1, 1, 1, 1, 0, 704, 100
34513, V, 1, 1, 1, 1, 0, 704, 100
34514, V, 1, 1, 1, 1, 0, 704, 100
34515, V, 1, 1, 1, 1, 0, 704, 100
34516, V, 1, 1, 1, 1, 0, 704, 100
34518, V, 1, 1, 1, 1, 0, 704, 100
34519, V, 1, 1, 1, 1, 0, 704, 100
34520, V, 1, 1, 1, 1, 0, 704, 100
34521, V, 1, 1, 1, 1, 0, 704, 100
34522, V, 1, 1, 1, 1, 0, 704, 100
34523, V, 1, 1, 1, 1, 0, 704, 100
34524, V, 1, 1, 1, 1, 0, 704, 100
34525, V, 1, 1, 1, 1, 0, 704, 100
34526, V, 1, 1, 1, 1, 0, 704, 100
34527, V, 1, 1, 1, 1, 0, 704, 100
34528, V, 1, 1, 1, 1, 0, 704, 100
34529, V, 1, 1, 1, 1, 0, 704, 100
34530, V, 1, 1, 1, 1, 0, 704, 100
34531, V, 1, 1, 1, 1, 0, 704, 100
34532, V, 1, 1, 1, 1, 0, 704, 100
34533, V, 1, 1, 1, 1, 0, 704, 100
34534, V, 1, 1, 1, 1, 0, 704, 100
34535, V, 1, 1, 1, 1, 0, 704, 100
34536, V, 1, 1, 1, 1, 0, 704, 100
34537, V, 1, 1, 1, 1, 0, 704, 100
34538, V, 1, 1, 1, 1, 0, 704, 100
34539, V, 1, 1, 1, 1, 0, 704, 100
34540, V, 1, 1, 1, 1, 0, 704, 100
34541, V, 1, 1, 1, 1, 0, 704, 100
34542, V, 1, 1, 1, 1, 0, 704, 100
34543, V, 1, 1, 1, 1, 0, 704, 100
34544, V, 1, 1, 1, 1, 0, 704, 100
34545, V, 1, 1, 1, 1, 0, 704, 100
34546, V, 1, 1, 1, 1, 0, 704, 100
34547, V, 1, 1, 1, 1, 0, 704, 100
34548, V, 1, 1, 1, 1, 0, 704, 100
34549, V, 1, 1, 1, 1, 0, 704, 100
34550, V, 1, 1, 1, 1, 0, 704, 100
34551, V, 1, 1, 1, 1, 0, 704, 100
34552, V, 1, 1, 1, 1, 0, 704, 100
34553, V, 1, 1, 1, 1, 0, 704, 100
34554, V, 1, 1, 1, 1, 0, 704, 100
34555, V, 1, 1, 1, 1, 0, 704, 100
34556, V, 1, 1, 1, 1, 0, 704, 100
34557, V, 1, 1, 1, 1, 0, 704, 100
34558, V, 1, 1, 1, 1, 0, 704, 100
34560, V, 1, 1, 1, 1, 0, 704, 100
34561, V, 1, 1, 1, 1, 0, 704, 100
34562, V, 1, 1, 1, 1, 0, 704, 100
34563, V, 1, 1, 1, 1, 0, 704, 100
34564, V, 1, 1, 1, 1, 0, 704, 100
34565, V, 1, 1, 1, 1, 0, 704, 100
34566, V, 1, 1, 1, 1, 0, 704, 100
34567, V, 1, 1, 1, 1, 0, 704, 100
34568, V, 1, 1, 1, 1, 0, 704, 100
34569, V, 1, 1, 1, 1, 0, 704, 100
34570, V, 1, 1, 1, 1, 0, 704, 100
34571, V, 1, 1, 1, 1, 0, 704, 100
34572, V, 1, 1, 1, 1, 0, 704, 100
34573, V, 1, 1, 1, 1, 0, 704, 100
34574, V, 1, 1, 1, 1, 0, 704, 100
34575, V, 1, 1, 1, 1, 0, 704, 100
34576, V, 1, 1, 1, 1, 0, 704, 100
34577, V, 1, 1, 1, 1, 0, 704, 100
34578, V, 1, 1, 1, 1, 0, 704, 100
34579, V, 1, 1, 1, 1, 0, 704, 100
34580, V, 1, 1, 1, 1, 0, 704, 100
34581, V, 1, 1, 1, 1, 0, 704, 100
34582, V, 1, 1, 1, 1, 0, 704, 100
34583, V, 1, 1, 1, 1, 0, 704, 100
34584, V, 1, 1, 1, 1, 0, 704, 100
34585, V, 1, 1, 1, 1, 0, 704, 100
34586, V, 1, 1, 1, 1, 0, 704, 100
34587, V, 1, 1, 1, 1, 0, 704, 100
34588, V, 1, 1, 1, 1, 0, 704, 100
34589, V, 1, 1, 1, 1, 0, 704, 100
34590, V, 1, 1, 1, 1, 0, 704, 100
34591, V, 1, 1, 1, 1, 0, 704, 100
34592, V, 1, 1, 1, 1, 0, 704, 100
34593, V, 1, 1, 1, 1, 0, 704, 100
34594, V, 1, 1, 1, 1, 0, 704, 100
34595, V, 1, 1, 1, 1, 0, 704, 100
34596, V, 1, 1, 1, 1, 0, 704, 100
34597, V, 1, 1, 1, 1, 0, 704, 100
34598, V, 1, 1, 1, 1, 0, 704, 100
34599, V, 1, 1, 1, 1, 0, 704, 100
34600, V, 1, 1, 1, 1, 0, 704, 100
34601, V, 1, 1, 1, 1, 0, 704, 100
34603, V, 1, 1, 1, 1, 0, 704, 100
34604, V, 1, 1, 1, 1, 0, 704, 100
34605, V, 1, 1, 1, 1, 0, 704, 100
34606, V, 1, 1, 1, 1, 0, 704, 100
34607, V, 1, 1, 1, 1, 0, 704, 100
34608, V, 1, 1, 1, 1, 0, 704, 100
34609, V, 1, 1, 1, 1, 0, 704, 100
34610, V, 1, 1, 1, 1, 0, 704, 100
34611, V, 1, 1, 1, 1, 0, 704, 100
34612, V, 1, 1, 1, 1, 0, 704, 100
34613, V, 1, 1, 1, 1, 0, 704, 100
34614, V, 1, 1, 1, 1, 0, 704, 100
34615, V, 1, 1, 1, 1, 0, 704, 100
34616, V, 1, 1, 1, 1, 0, 704, 100
34617, V, 1, 1, 1, 1, 0, 704, 100
34618, V, 1, 1, 1, 1, 0, 704, 100
34619, V, 1, 1, 1, 1, 0, 704, 100
34620, V, 1, 1, 1, 1, 0, 704, 100
34621, V, 1, 1, 1, 1, 0, 704, 100
34622, V, 1, 1, 1, 1, 0, 704, 100
34623, V, 1, 1, 1, 1, 0, 704, 100
34624, V, 1, 1, 1, 1, 0, 704, 100
34625, V, 1, 1, 1, 1, 0, 704, 100
34626, V, 1, 1, 1, 1, 0, 704, 100
34627, V, 1, 1, 1, 1, 0, 704, 100
34628, V, 1, 1, 1, 1, 0, 704, 100
34629, V, 1, 1, 1, 1, 0, 704, 100
34630, V, 1, 1, 1, 1, 0, 704, 100
34631, V, 1, 1, 1, 1, 0, 704, 100
34632, V, 1, 1, 1, 1, 0, 704, 100
34633, V, 1, 1, 1, 1, 0, 704, 100
34634, V, 1, 1, 1, 1, 0, 704, 100
34635, V, 1, 1, 1, 1, 0, 704, 100
34636, V, 1, 1, 1, 1, 0, 704, 100
34637, V, 1, 1, 1, 1, 0, 704, 100
34638, V, 1, 1, 1, 1, 0, 704, 100
34639, V, 1, 1, 1, 1, 0, 704, 100
34640, V, 1, 1, 1, 1, 0, 704, 100
34641, V, 1, 1, 1, 1, 0, 704, 100
34642, V, 1, 1, 1, 1, 0, 704, 100
34643, V, 1, 1, 1, 1, 0, 704, 100
34644, V, 1, 1, 1, 1, 0, 704, 100
34646, V, 1, 1, 1, 1, 0, 704, 100
34647, V, 1, 1, 1, 1, 0, 704, 100
34648, V, 1, 1, 1, 1, 0, 704, 100
34649, V, 1, 1, 1, 1, 0, 704, 100
34650, V, 1, 1, 1, 1, 0, 704, 100
34651, V, 1, 1, 1, 1, 0, 704, 100
34652, V, 1, 1, 1, 1, 0, 704, 100
34653, V, 1, 1, 1, 1, 0, 704, 100
34654, V, 1, 1, 1, 1, 0, 704, 100
34655, V, 1, 1, 1, 1, 0, 704, 100
34656, V, 1, 1, 1, 1, 0, 704, 100
34657, V, 1, 1, 1, 1, 0, 704, 100
34658, V, 1, 1, 1, 1, 0, 704, 100
34659, V, 1, 1, 1, 1, 0, 704, 100
34660, V, 1, 1, 1, 1, 0, 704, 100
34661, V, 1, 1, 1, 1, 0, 704, 100
34662, V, 1, 1, 1, 1, 0, 704, 100
34663, V, 1, 1, 1, 1, 0, 704, 100
34664, V, 1, 1, 1, 1, 0, 704, 100
34665, V, 1, 1, 1, 1, 0, 704, 100
34666, V, 1, 1, 1, 1, 0, 704, 100
34667, V, 1, 1, 1, 1, 0, 704, 100
34668, V, 1, 1, 1, 1, 0, 704, 100
34669, V, 1, 1, 1, 1, 0, 704, 100
34670, V, 1, 1, 1, 1, 0, 704, 100
34671, V, 1, 1, 1, 1, 0, 704, 100
34672, V, 1, 1, 1, 1, 0, 704, 100
34673, V, 1, 1, 1, 1, 0, 704, 100
34674, V, 1, 1, 1, 1, 0, 704, 100
34675, V, 1, 1, 1, 1, 0, 704, 100
34676, V, 1, 1, 1, 1, 0, 704, 100
34677, V, 1, 1, 1, 1, 0, 704, 100
34678, V, 1, 1, 1, 1, 0, 704, 100
34679, V, 1, 1, 1, 1, 0, 704, 100
34680, V, 1, 1, 1, 1, 0, 704, 100
34681, V, 1, 1, 1, 1, 0, 704, 100
34682, V, 1, 1, 1, 1, 0, 704, 100
34683, V, 1, 1, 1, 1, 0, 704, 100
34684, V, 1, 1, 1, 1, 0, 704, 100
34685, V, 1, 1, 1, 1, 0, 704, 100
34686, V, 1, 1, 1, 1, 0, 704, 100
34688, V, 1, 1, 1, 1, 0, 704, 100
34689, V, 1, 1, 1, 1, 0, 704, 100
34690, V, 1, 1, 1, 1, 0, 704, 100
34691, V, 1, 1, 1, 1, 0, 704, 100
34692, V, 1, 1, 1, 1, 0, 704, 100
34693, V, 1, 1, 1, 1, 0, 704, 100
34694, V, 1, 1, 1, 1, 0, 704, 100
34695, V, 1, 1, 1, 1, 0, 704, 100
34696, V, 1, 1, 1, 1, 0, 704, 100
34697, V, 1, 1, 1, 1, 0, 704, 100
34698, V, 1, 1, 1, 1, 0, 704, 100
34699, V, 1, 1, 1, 1, 0, 704, 100
34700, V, 1, 1, 1, 1, 0, 704, 100
34701, V, 1, 1, 1, 1, 0, 704, 100
34702, V, 1, 1, 1, 1, 0, 704, 100
34703, V, 1, 1, 1, 1, 0, 704, 100
34704, V, 1, 1, 1, 1, 0, 704, 100
34705, V, 1, 1, 1, 1, 0, 704, 100
34706, V, 1, 1, 1, 1, 0, 704, 100
34707, V, 1, 1, 1, 1, 0, 704, 100
34708, V, 1, 1, 1, 1, 0, 704, 100
34709, V, 1, 1, 1, 1, 0, 704, 100
34710, V, 1, 1, 1, 1, 0, 704, 100
34711, V, 1, 1, 1, 1, 0, 704, 100
34712, V, 1, 1, 1, 1, 0, 704, 100
34713, V, 1, 1, 1, 1, 0, 704, 100
34714, V, 1, 1, 1, 1, 0, 704, 100
34715, V, 1, 1, 1, 1, 0, 704, 100
34716, V, 1, 1, 1, 1, 0, 704, 100
34717, V, 1, 1, 1, 1, 0, 704, 100
34718, V, 1, 1, 1, 1, 0, 704, 100
34719, V, 1, 1, 1, 1, 0, 704, 100
34720, V, 1, 1, 1, 1, 0, 704, 100
34721, V, 1, 1, 1, 1, 0, 704, 100
34722, V, 1, 1, 1, 1, 0, 704, 100
34723, V, 1, 1, 1, 1, 0, 704, 100
34724, V, 1, 1, 1, 1, 0, 704, 100
34725, V, 1, 1, 1, 1, 0, 704, 100
34726, V, 1, 1, 1, 1, 0, 704, 100
34727, V, 1, 1, 1, 1, 0, 704, 100
34728, V, 1, 1, 1, 1, 0, 704, 100
34729, V, 1, 1, 1, 1, 0, 704, 100
34731, V, 1, 1, 1, 1, 0, 704, 100
34732, V, 1, 1, 1, 1, 0, 704, 100
34733, V, 1, 1, 1, 1, 0, 704, 100
34734, V, 1, 1, 1, 1, 0, 704, 100
34735, V, 1, 1, 1, 1, 0, 704, 100
34736, V, 1, 1, 1, 1, 0, 704, 100
34737, V, 1, 1, 1, 1, 0, 704, 100
34738, V, 1, 1, 1, 1, 0, 704, 100
34739, V, 1, 1, 1, 1, 0, 704, 100
34740, V, 1, 1, 1, 1, 0, 704, 100
34741, V, 1, 1, 1, 1, 0, 704, 100
34742, V, 1, 1, 1, 1, 0, 704, 100
34743, V, 1, 1, 1, 1, 0, 704, 100
34744, V, 1, 1, 1, 1, 0, 704, 100
34745, V, 1, 1, 1, 1, 0, 704, 100
34746, V, 1, 1, 1, 1, 0, 704, 100
34747, V, 1, 1, 1, 1, 0, 704, 100
34748, V, 1, 1, 1, 1, 0, 704, 100
34749, V, 1, 1, 1, 1, 0, 704, 100
34750, V, 1, 1, 1, 1, 0, 704, 100
34751, V, 1, 1, 1, 1, 0, 704, 100
34752, V, 1, 1, 1, 1, 0, 704, 100
34753, V, 1, 1, 1, 1, 0, 704, 100
34754, V, 1, 1, 1, 1, 0, 704, 100
34755, V, 1, 1, 1, 1, 0, 704, 100
34756, V, 1, 1, 1, 1, 0, 704, 100
34757, V, 1, 1, 1, 1, 0, 704, 100
34758, V, 1, 1, 1, 1, 0, 704, 100
34759, V, 1, 1, 1, 1, 0, 704, 100
34760, V, 1, 1, 1, 1, 0, 704, 100
34761, V, 1, 1, 1, 1, 0, 704, 100
34762, V, 1, 1, 1, 1, 0, 704, 100
34763, V, 1, 1, 1, 1, 0, 704, 100
34764, V, 1, 1, 1, 1, 0, 704, 100
34765, V, 1, 1, 1, 1, 0, 704, 100
34766, V, 1, 1, 1, 1, 0, 704, 100
34767, V, 1, 1, 1, 1, 0, 704, 100
34768, V, 1, 1, 1, 1, 0, 704, 100
34769, V, 1, 1, 1, 1, 0, 704, 100
34770, V, 1, 1, 1, 1, 0, 704, 100
34771, V, 1, 1, 1, 1, 0, 704, 100
34772, V, 1, 1, 1, 1, 0, 704, 100
34774, V, 1, 1, 1, 1, 0, 704, 100
34775, V, 1, 1, 1, 1, 0, 704, 100
34776, V, 1, 1, 1, 1, 0, 704, 100
34777, V, 1, 1, 1, 1, 0, 704, 100
34778, V, 1, 1, 1, 1, 0, 704, 100
34779, V, 1, 1, 1, 1, 0, 704, 100
34780, V, 1, 1, 1, 1, 0, 704, 100
34781, V, 1, 1, 1, 1, 0, 704, 100
34782, V, 1, 1, 1, 1, 0, 704, 100
34783, V, 1, 1, 1, 1, 0, 704, 100
34784, V, 1, 1, 1, 1, 0, 704, 100
34785, V, 1, 1, 1, 1, 0, 704, 100
34786, V, 1, 1, 1, 1, 0, 704, 100
34787, V, 1, 1, 1, 1, 0, 704, 100
34788, V, 1, 1, 1, 1, 0, 704, 100
34789, V, 1, 1, 1, 1, 0, 704, 100
34790, V, 1, 1, 1, 1, 0, 704, 100
34791, V, 1, 1, 1, 1, 0, 704, 100
34792, V, 1, 1, 1, 1, 0, 704, 100
34793, V, 1, 1, 1, 1, 0, 704, 100
34794, V, 1, 1, 1, 1, 0, 704, 100
34795, V, 1, 1, 1, 1, 0, 704, 100
34796, V, 1, 1, 1, 1, 0, 704, 100
34797, V, 1, 1, 1, 1, 0, 704, 100
34798, V, 1, 1, 1, 1, 0, 704, 100
34799, V, 1, 1, 1, 1, 0, 704, 100
34800, V, 1, 1, 1, 1, 0, 704, 100
34801, V, 1, 1, 1, 1, 0, 704, 100
34802, V, 1, 1, 1, 1, 0, 704, 100
34803, V, 1, 1, 1, 1, 0, 704, 100
34804, V, 1, 1, 1, 1, 0, 704, 100
34805, V, 1, 1, 1, 1, 0, 704, 100
34806, V, 1, 1, 1, 1, 0, 704, 100
34807, V, 1, 1, 1, 1, 0, 704, 100
34808, V, 1, 1, 1, 1, 0, 704, 100
34809, V, 1, 1, 1, 1, 0, 704, 100
34810, V, 1, 1, 1, 1, 0, 704, 100
34811, V, 1, 1, 1, 1, 0, 704, 100
34812, V, 1, 1, 1, 1, 0, 704, 100
34813, V, 1, 1, 1, 1, 0, 704, 100
34814, V, 1, 1, 1, 1, 0, 704, 100
34816, V, 1, 1, 1, 1, 0, 704, 100
34817, V, 1, 1, 1, 1, 0, 704, 100
34818, V, 1, 1, 1, 1, 0, 704, 100
34819, V, 1, 1, 1, 1, 0, 704, 100
34820, V, 1, 1, 1, 1, 0, 704, 100
34821, V, 1, 1, 1, 1, 0, 704, 100
34822, V, 1, 1, 1, 1, 0, 704, 100
34823, V, 1, 1, 1, 1, 0, 704, 100
34824, V, 1, 1, 1, 1, 0, 704, 100
34825, V, 1, 1, 1, 1, 0, 704, 100
34826, V, 1, 1, 1, 1, 0, 704, 100
34827, V, 1, 1, 1, 1, 0, 704, 100
34828, V, 1, 1, 1, 1, 0, 704, 100
34829, V, 1, 1, 1, 1, 0, 704, 100
34830, V, 1, 1, 1, 1, 0, 704, 100
34831, V, 1, 1, 1, 1, 0, 704, 100
34832, V, 1, 1, 1, 1, 0, 704, 100
34833, V, 1, 1, 1, 1, 0, 704, 100
34834, V, 1, 1, 1, 1, 0, 704, 100
34835, V, 1, 1, 1, 1, 0, 704, 100
34836, V, 1, 1, 1, 1, 0, 704, 100
34837, V, 1, 1, 1, 1, 0, 704, 100
34838, V, 1, 1, 1, 1, 0, 704, 100
34839, V, 1, 1, 1, 1, 0, 704, 100
34840, V, 1, 1, 1, 1, 0, 704, 100
34841, V, 1, 1, 1, 1, 0, 704, 100
34842, V, 1, 1, 1, 1, 0, 704, 100
34843, V, 1, 1, 1, 1, 0, 704, 100
34844, V, 1, 1, 1, 1, 0, 704, 100
34845, V, 1, 1, 1, 1, 0, 704, 100
34846, V, 1, 1, 1, 1, 0, 704, 100
34847, V, 1, 1, 1, 1, 0, 704, 100
34848, V, 1, 1, 1, 1, 0, 704, 100
34849, V, 1, 1, 1, 1, 0, 704, 100
34850, V, 1, 1, 1, 1, 0, 704, 100
34851, V, 1, 1, 1, 1, 0, 704, 100
34852, V, 1, 1, 1, 1, 0, 704, 100
34853, V, 1, 1, 1, 1, 0, 704, 100
34854, V, 1, 1, 1, 1, 0, 704, 100
34855, V, 1, 1, 1, 1, 0, 704, 100
34856, V, 1, 1, 1, 1, 0, 704, 100
34857, V, 1, 1, 1, 1, 0, 704, 100
34859, V, 1, 1, 1, 1, 0, 704, 100
34860, V, 1, 1, 1, 1, 0, 704, 100
34861, V, 1, 1, 1, 1, 0, 704, 100
34862, V, 1, 1, 1, 1, 0, 704, 100
34863, V, 1, 1, 1, 1, 0, 704, 100
34864, V, 1, 1, 1, 1, 0, 704, 100
34865, V, 1, 1, 1, 1, 0, 704, 100
34866, V, 1, 1, 1, 1, 0, 704, 100
34867, V, 1, 1, 1, 1, 0, 704, 100
34868, V, 1, 1, 1, 1, 0, 704, 100
34869, V, 1, 1, 1, 1, 0, 704, 100
34870, V, 1, 1, 1, 1, 0, 704, 100
34871, V, 1, 1, 1, 1, 0, 704, 100
34872, V, 1, 1, 1, 1, 0, 704, 100
34873, V, 1, 1, 1, 1, 0, 704, 100
34874, V, 1, 1, 1, 1, 0, 704, 100
34875, V, 1, 1, 1, 1, 0, 704, 100
34876, V, 1, 1, 1, 1, 0, 704, 100
34877, V, 1, 1, 1, 1, 0, 704, 100
34878, V, 1, 1, 1, 1, 0, 704, 100
34879, V, 1, 1, 1, 1, 0, 704, 100
34880, V, 1, 1, 1, 1, 0, 704, 100
34881, V, 1, 1, 1, 1, 0, 704, 100
34882, V, 1, 1, 1, 1, 0, 704, 100
34883, V, 1, 1, 1, 1, 0, 704, 100
34884, V, 1, 1, 1, 1, 0, 704, 100
34885, V, 1, 1, 1, 1, 0, 704, 100
34886, V, 1, 1, 1, 1, 0, 704, 100
34887, V, 1, 1, 1, 1, 0, 704, 100
34888, V, 1, 1, 1, 1, 0, 704, 100
34889, V, 1, 1, 1, 1, 0, 704, 100
34890, V, 1, 1, 1, 1, 0, 704, 100
34891, V, 1, 1, 1, 1, 0, 704, 100
34892, V, 1, 1, 1, 1, 0, 704, 100
34893, V, 1, 1, 1, 1, 0, 704, 100
34894, V, 1, 1, 1, 1, 0, 704, 100
34895, V, 1, 1, 1, 1, 0, 704, 100
34896, V, 1, 1, 1, 1, 0, 704, 100
34897, V, 1, 1, 1, 1, 0, 704, 100
34898, V, 1, 1, 1, 1, 0, 704, 100
34899, V, 1, 1, 1, 1, 0, 704, 100
34900, V, 1, 1, 1, 1, 0, 704, 100
34902, V, 1, 1, 1, 1, 0, 704, 100
34903, V, 1, 1, 1, 1, 0, 704, 100
34904, V, 1, 1, 1, 1, 0, 704, 100
34905, V, 1, 1, 1, 1, 0, 704, 100
34906, V, 1, 1, 1, 1, 0, 704, 100
34907, V, 1, 1, 1, 1, 0, 704, 100
34908, V, 1, 1, 1, 1, 0, 704, 100
34909, V, 1, 1, 1, 1, 0, 704, 100
34910, V, 1, 1, 1, 1, 0, 704, 100
34911, V, 1, 1, 1, 1, 0, 704, 100
34912, V, 1, 1, 1, 1, 0, 704, 100
34913, V, 1, 1, 1, 1, 0, 704, 100
34914, V, 1, 1, 1, 1, 0, 704, 100
34915, V, 1, 1, 1, 1, 0, 704, 100
34916, V, 1, 1, 1, 1, 0, 704, 100
34917, V, 1, 1, 1, 1, 0, 704, 100
34918, V, 1, 1, 1, 1, 0, 704, 100
34919, V, 1, 1, 1, 1, 0, 704, 100
34920, V, 1, 1, 1, 1, 0, 704, 100
34921, V, 1, 1, 1, 1, 0, 704, 100
34922, V, 1, 1, 1, 1, 0, 704, 100
34923, V, 1, 1, 1, 1, 0, 704, 100
34924, V, 1, 1, 1, 1, 0, 704, 100
34925, V, 1, 1, 1, 1, 0, 704, 100
34926, V, 1, 1, 1, 1, 0, 704, 100
34927, V, 1, 1, 1, 1, 0, 704, 100
34928, V, 1, 1, 1, 1, 0, 704, 100
34929, V, 1, 1, 1, 1, 0, 704, 100
34930, V, 1, 1, 1, 1, 0, 704, 100
34931, V, 1, 1, 1, 1, 0, 704, 100
34932, V, 1, 1, 1, 1, 0, 704, 100
34933, V, 1, 1, 1, 1, 0, 704, 100
34934, V, 1, 1, 1, 1, 0, 704, 100
34935, V, 1, 1, 1, 1, 0, 704, 100
34936, V, 1, 1, 1, 1, 0, 704, 100
34937, V, 1, 1, 1, 1, 0, 704, 100
34938, V, 1, 1, 1, 1, 0, 704, 100
34939, V, 1, 1, 1, 1, 0, 704, 100
34940, V, 1, 1, 1, 1, 0, 704, 100
34941, V, 1, 1, 1, 1, 0, 704, 100
34942, V, 1, 1, 1, 1, 0, 704, 100
34944, V, 1, 1, 1, 1, 0, 704, 100
34945, V, 1, 1, 1, 1, 0, 704, 100
34946, V, 1, 1, 1, 1, 0, 704, 100
34947, V, 1, 1, 1, 1, 0, 704, 100
34948, V, 1, 1, 1, 1, 0, 704, 100
34949, V, 1, 1, 1, 1, 0, 704, 100
34950, V, 1, 1, 1, 1, 0, 704, 100
34951, V, 1, 1, 1, 1, 0, 704, 100
34952, V, 1, 1, 1, 1, 0, 704, 100
34953, V, 1, 1, 1, 1, 0, 704, 100
34954, V, 1, 1, 1, 1, 0, 704, 100
34955, V, 1, 1, 1, 1, 0, 704, 100
34956, V, 1, 1, 1, 1, 0, 704, 100
34957, V, 1, 1, 1, 1, 0, 704, 100
34958, V, 1, 1, 1, 1, 0, 704, 100
34959, V, 1, 1, 1, 1, 0, 704, 100
34960, V, 1, 1, 1, 1, 0, 704, 100
34961, V, 1, 1, 1, 1, 0, 704, 100
34962, V, 1, 1, 1, 1, 0, 704, 100
34963, V, 1, 1, 1, 1, 0, 704, 100
34964, V, 1, 1, 1, 1, 0, 704, 100
34965, V, 1, 1, 1, 1, 0, 704, 100
34966, V, 1, 1, 1, 1, 0, 704, 100
34967, V, 1, 1, 1, 1, 0, 704, 100
34968, V, 1, 1, 1, 1, 0, 704, 100
34969, V, 1, 1, 1, 1, 0, 704, 100
34970, V, 1, 1, 1, 1, 0, 704, 100
34971, V, 1, 1, 1, 1, 0, 704, 100
34972, V, 1, 1, 1, 1, 0, 704, 100
34973, V, 1, 1, 1, 1, 0, 704, 100
34974, V, 1, 1, 1, 1, 0, 704, 100
34975, V, 1, 1, 1, 1, 0, 704, 100
34976, V, 1, 1, 1, 1, 0, 704, 100
34977, V, 1, 1, 1, 1, 0, 704, 100
34978, V, 1, 1, 1, 1, 0, 704, 100
34979, V, 1, 1, 1, 1, 0, 704, 100
34980, V, 1, 1, 1, 1, 0, 704, 100
34981, V, 1, 1, 1, 1, 0, 704, 100
34982, V, 1, 1, 1, 1, 0, 704, 100
34983, V, 1, 1, 1, 1, 0, 704, 100
34984, V, 1, 1, 1, 1, 0, 704, 100
34985, V, 1, 1, 1, 1, 0, 704, 100
34987, V, 1, 1, 1, 1, 0, 704, 100
34988, V, 1, 1, 1, 1, 0, 704, 100
34989, V, 1, 1, 1, 1, 0, 704, 100
34990, V, 1, 1, 1, 1, 0, 704, 100
34991, V, 1, 1, 1, 1, 0, 704, 100
34992, V, 1, 1, 1, 1, 0, 704, 100
34993, V, 1, 1, 1, 1, 0, 704, 100
34994, V, 1, 1, 1, 1, 0, 704, 100
34995, V, 1, 1, 1, 1, 0, 704, 100
34996, V, 1, 1, 1, 1, 0, 704, 100
34997, V, 1, 1, 1, 1, 0, 704, 100
34998, V, 1, 1, 1, 1, 0, 704, 100
34999, V, 1, 1, 1, 1, 0, 704, 100
35000, V, 1, 1, 1, 1, 0, 704, 100
35001, V, 1, 1, 1, 1, 0, 704, 100
35002, V, 1, 1, 1, 1, 0, 704, 100
35003, V, 1, 1, 1, 1, 0, 704, 100
35004, V, 1, 1, 1, 1, 0, 704, 100
35005, V, 1, 1, 1, 1, 0, 704, 100
35006, V, 1, 1, 1, 1, 0, 704, 100
35007, V, 1, 1, 1, 1, 0, 704, 100
35008, V, 1, 1, 1, 1, 0, 704, 100
35009, V, 1, 1, 1, 1, 0, 704, 100
35010, V, 1, 1, 1, 1, 0, 704, 100
35011, V, 1, 1, 1, 1, 0, 704, 100
35012, V, 1, 1, 1, 1, 0, 704, 100
35013, V, 1, 1, 1, 1, 0, 704, 100
35014, V, 1, 1, 1, 1, 0, 704, 100
35015, V, 1, 1, 1, 1, 0, 704, 100
35016, V, 1, 1, 1, 1, 0, 704, 100
35017, V, 1, 1, 1, 1, 0, 704, 100
35018, V, 1, 1, 1, 1, 0, 704, 100
35019, V, 1, 1, 1, 1, 0, 704, 100
35020, V, 1, 1, 1, 1, 0, 704, 100
35021, V, 1, 1, 1, 1, 0, 704, 100
35022, V, 1, 1, 1, 1, 0, 704, 100
35023, V, 1, 1, 1, 1, 0, 704, 100
35024, V, 1, 1, 1, 1, 0, 704, 100
35025, V, 1, 1, 1, 1, 0, 704, 100
35026, V, 1, 1, 1, 1, 0, 704, 100
35027, V, 1, 1, 1, 1, 0, 704, 100
35028, V, 1, 1, 1, 1, 0, 704, 100
35030, V, 1, 1, 1, 1, 0, 704, 100
35031, V, 1, 1, 1, 1, 0, 704, 100
35032, V, 1, 1, 1, 1, 0, 704, 100
35033, V, 1, 1, 1, 1, 0, 704, 100
35034, V, 1, 1, 1, 1, 0, 704, 100
35035, V, 1, 1, 1, 1, 0, 704, 100
35036, V, 1, 1, 1, 1, 0, 704, 100
35037, V, 1, 1, 1, 1, 0, 704, 100
35038, V, 1, 1, 1, 1, 0, 704, 100
35039, V, 1, 1, 1, 1, 0, 704, 100
35040, V, 1, 1, 1, 1, 0, 704, 100
35041, V, 1, 1, 1, 1, 0, 704, 100
35042, V, 1, 1, 1, 1, 0, 704, 100
35043, V, 1, 1, 1, 1, 0, 704, 100
35044, V, 1, 1, 1, 1, 0, 704, 100
35045, V, 1, 1, 1, 1, 0, 704, 100
35046, V, 1, 1, 1, 1, 0, 704, 100
35047, V, 1, 1, 1, 1, 0, 704, 100
35048, V, 1, 1, 1, 1, 0, 704, 100
35049, V, 1, 1, 1, 1, 0, 704, 100
35050, V, 1, 1, 1, 1, 0, 704, 100
35051, V, 1, 1, 1, 1, 0, 704, 100
35052, V, 1, 1, 1, 1, 0, 704, 100
35053, V, 1, 1, 1, 1, 0, 704, 100
35054, V, 1, 1, 1, 1, 0, 704, 100
35055, V, 1, 1, 1, 1, 0, 704, 100
35056, V, 1, 1, 1, 1, 0, 704, 100
35057, V, 1, 1, 1, 1, 0, 704, 100
35058, V, 1, 1, 1, 1, 0, 704, 100
35059, V, 1, 1, 1, 1, 0, 704, 100
35060, V, 1, 1, 1, 1, 0, 704, 100
35061, V, 1, 1, 1, 1, 0, 704, 100
35062, V, 1, 1, 1, 1, 0, 704, 100
35063, V, 1, 1, 1, 1, 0, 704, 100
35064, V, 1, 1, 1, 1, 0, 704, 100
35065, V, 1, 1, 1, 1, 0, 704, 100
35066, V, 1, 1, 1, 1, 0, 704, 100
35067, V, 1, 1, 1, 1, 0, 704, 100
35068, V, 1, 1, 1, 1, 0, 704, 100
35069, V, 1, 1, 1, 1, 0, 704, 100
35070, V, 1, 1, 1, 1, 0, 704, 100
35072, V, 1, 1, 1, 1, 0, 704, 100
35073, V, 1, 1, 1, 1, 0, 704, 100
35074, V, 1, 1, 1, 1, 0, 704, 100
35075, V, 1, 1, 1, 1, 0, 704, 100
35076, V, 1, 1, 1, 1, 0, 704, 100
35077, V, 1, 1, 1, 1, 0, 704, 100
35078, V, 1, 1, 1, 1, 0, 704, 100
35079, V, 1, 1, 1, 1, 0, 704, 100
35080, V, 1, 1, 1, 1, 0, 704, 100
35081, V, 1, 1, 1, 1, 0, 704, 100
35082, V, 1, 1, 1, 1, 0, 704, 100
35083, V, 1, 1, 1, 1, 0, 704, 100
35084, V, 1, 1, 1, 1, 0, 704, 100
35085, V, 1, 1, 1, 1, 0, 704, 100
35086, V, 1, 1, 1, 1, 0, 704, 100
35087, V, 1, 1, 1, 1, 0, 704, 100
35088, V, 1, 1, 1, 1, 0, 704, 100
35089, V, 1, 1, 1, 1, 0, 704, 100
35090, V, 1, 1, 1, 1, 0, 704, 100
35091, V, 1, 1, 1, 1, 0, 704, 100
35092, V, 1, 1, 1, 1, 0, 704, 100
35093, V, 1, 1, 1, 1, 0, 704, 100
35094, V, 1, 1, 1, 1, 0, 704, 100
35095, V, 1, 1, 1, 1, 0, 704, 100
35096, V, 1, 1, 1, 1, 0, 704, 100
35097, V, 1, 1, 1, 1, 0, 704, 100
35098, V, 1, 1, 1, 1, 0, 704, 100
35099, V, 1, 1, 1, 1, 0, 704, 100
35100, V, 1, 1, 1, 1, 0, 704, 100
35101, V, 1, 1, 1, 1, 0, 704, 100
35102, V, 1, 1, 1, 1, 0, 704, 100
35103, V, 1, 1, 1, 1, 0, 704, 100
35104, V, 1, 1, 1, 1, 0, 704, 100
35105, V, 1, 1, 1, 1, 0, 704, 100
35106, V, 1, 1, 1, 1, 0, 704, 100
35107, V, 1, 1, 1, 1, 0, 704, 100
35108, V, 1, 1, 1, 1, 0, 704, 100
35109, V, 1, 1, 1, 1, 0, 704, 100
35110, V, 1, 1, 1, 1, 0, 704, 100
35111, V, 1, 1, 1, 1, 0, 704, 100
35112, V, 1, 1, 1, 1, 0, 704, 100
35113, V, 1, 1, 1, 1, 0, 704, 100
35115, V, 1, 1, 1, 1, 0, 704, 100
35116, V, 1, 1, 1, 1, 0, 704, 100
35117, V, 1, 1, 1, 1, 0, 704, 100
35118, V, 1, 1, 1, 1, 0, 704, 100
35119, V, 1, 1, 1, 1, 0, 704, 100
35120, V, 1, 1, 1, 1, 0, 704, 100
35121, V, 1, 1, 1, 1, 0, 704, 100
35122, V, 1, 1, 1, 1, 0, 704, 100
35123, V, 1, 1, 1, 1, 0, 704, 100
35124, V, 1, 1, 1, 1, 0, 704, 100
35125, V, 1, 1, 1, 1, 0, 704, 100
35126, V, 1, 1, 1, 1, 0, 704, 100
35127, V, 1, 1, 1, 1, 0, 704, 100
35128, V, 1, 1, 1, 1, 0, 704, 100
35129, V, 1, 1, 1, 1, 0, 704, 100
35130, V, 1, 1, 1, 1, 0, 704, 100
35131, V, 1, 1, 1, 1, 0, 704, 100
35132, V, 1, 1, 1, 1, 0, 704, 100
35133, V, 1, 1, 1, 1, 0, 704, 100
35134, V, 1, 1, 1, 1, 0, 704, 100
35135, V, 1, 1, 1, 1, 0, 704, 100
35136, V, 1, 1, 1, 1, 0, 704, 100
35137, V, 1, 1, 1, 1, 0, 704, 100
35138, V, 1, 1, 1, 1, 0, 704, 100
35139, V, 1, 1, 1, 1, 0, 704, 100
35140, V, 1, 1, 1, 1, 0, 704, 100
35141, V, 1, 1, 1, 1, 0, 704, 100
35142, V, 1, 1, 1, 1, 0, 704, 100
35143, V, 1, 1, 1, 1, 0, 704, 100
35144, V, 1, 1, 1, 1, 0, 704, 100
35145, V, 1, 1, 1, 1, 0, 704, 100
35146, V, 1, 1, 1, 1, 0, 704, 100
35147, V, 1, 1, 1, 1, 0, 704, 100
35148, V, 1, 1, 1, 1, 0, 704, 100
35149, V, 1, 1, 1, 1, 0, 704, 100
35150, V, 1, 1, 1, 1, 0, 704, 100
35151, V, 1, 1, 1, 1, 0, 704, 100
35152, V, 1, 1, 1, 1, 0, 704, 100
35153, V, 1, 1, 1, 1, 0, 704, 100
35154, V, 1, 1, 1, 1, 0, 704, 100
35155, V, 1, 1, 1, 1, 0, 704, 100
35156, V, 1, 1, 1, 1, 0, 704, 100
35158, V, 1, 1, 1, 1, 0, 704, 100
35159, V, 1, 1, 1, 1, 0, 704, 100
35160, V, 1, 1, 1, 1, 0, 704, 100
35161, V, 1, 1, 1, 1, 0, 704, 100
35162, V, 1, 1, 1, 1, 0, 704, 100
35163, V, 1, 1, 1, 1, 0, 704, 100
35164, V, 1, 1, 1, 1, 0, 704, 100
35165, V, 1, 1, 1, 1, 0, 704, 100
35166, V, 1, 1, 1, 1, 0, 704, 100
35167, V, 1, 1, 1, 1, 0, 704, 100
35168, V, 1, 1, 1, 1, 0, 704, 100
35169, V, 1, 1, 1, 1, 0, 704, 100
35170, V, 1, 1, 1, 1, 0, 704, 100
35171, V, 1, 1, 1, 1, 0, 704, 100
35172, V, 1, 1, 1, 1, 0, 704, 100
35173, V, 1, 1, 1, 1, 0, 704, 100
35174, V, 1, 1, 1, 1, 0, 704, 100
35175, V, 1, 1, 1, 1, 0, 704, 100
35176, V, 1, 1, 1, 1, 0, 704, 100
35177, V, 1, 1, 1, 1, 0, 704, 100
35178, V, 1, 1, 1, 1, 0, 704, 100
35179, V, 1, 1, 1, 1, 0, 704, 100
35180, V, 1, 1, 1, 1, 0, 704, 100
35181, V, 1, 1, 1, 1, 0, 704, 100
35182, V, 1, 1, 1, 1, 0, 704, 100
35183, V, 1, 1, 1, 1, 0, 704, 100
35184, V, 1, 1, 1, 1, 0, 704, 100
35185, V, 1, 1, 1, 1, 0, 704, 100
35186, V, 1, 1, 1, 1, 0, 704, 100
35187, V, 1, 1, 1, 1, 0, 704, 100
35188, V, 1, 1, 1, 1, 0, 704, 100
35189, V, 1, 1, 1, 1, 0, 704, 100
35190, V, 1, 1, 1, 1, 0, 704, 100
35191, V, 1, 1, 1, 1, 0, 704, 100
35192, V, 1, 1, 1, 1, 0, 704, 100
35193, V, 1, 1, 1, 1, 0, 704, 100
35194, V, 1, 1, 1, 1, 0, 704, 100
35195, V, 1, 1, 1, 1, 0, 704, 100
35196, V, 1, 1, 1, 1, 0, 704, 100
35197, V, 1, 1, 1, 1, 0, 704, 100
35198, V, 1, 1, 1, 1, 0, 704, 100
35200, V, 1, 1, 1, 1, 0, 704, 100
35201, V, 1, 1, 1, 1, 0, 704, 100
35202, V, 1, 1, 1, 1, 0, 704, 100
35203, V, 1, 1, 1, 1, 0, 704, 100
35204, V, 1, 1, 1, 1, 0, 704, 100
35205, V, 1, 1, 1, 1, 0, 704, 100
35206, V, 1, 1, 1, 1, 0, 704, 100
35207, V, 1, 1, 1, 1, 0, 704, 100
35208, V, 1, 1, 1, 1, 0, 704, 100
35209, V, 1, 1, 1, 1, 0, 704, 100
35210, V, 1, 1, 1, 1, 0, 704, 100
35211, V, 1, 1, 1, 1, 0, 704, 100
35212, V, 1, 1, 1, 1, 0, 704, 100
35213, V, 1, 1, 1, 1, 0, 704, 100
35214, V, 1, 1, 1, 1, 0, 704, 100
35215, V, 1, 1, 1, 1, 0, 704, 100
35216, V, 1, 1, 1, 1, 0, 704, 100
35217, V, 1, 1, 1, 1, 0, 704, 100
35218, V, 1, 1, 1, 1, 0, 704, 100
35219, V, 1, 1, 1, 1, 0, 704, 100
35220, V, 1, 1, 1, 1, 0, 704, 100
35221, V, 1, 1, 1, 1, 0, 704, 100
35222, V, 1, 1, 1, 1, 0, 704, 100
35223, V, 1, 1, 1, 1, 0, 704, 100
35224, V, 1, 1, 1, 1, 0, 704, 100
35225, V, 1, 1, 1, 1, 0, 704, 100
35226, V, 1, 1, 1, 1, 0, 704, 100
35227, V, 1, 1, 1, 1, 0, 704, 100
35228, V, 1, 1, 1, 1, 0, 704, 100
35229, V, 1, 1, 1, 1, 0, 704, 100
35230, V, 1, 1, 1, 1, 0, 704, 100
35231, V, 1, 1, 1, 1, 0, 704, 100
35232, V, 1, 1, 1, 1, 0, 704, 100
35233, V, 1, 1, 1, 1, 0, 704, 100
35234, V, 1, 1, 1, 1, 0, 704, 100
35235, V, 1, 1, 1, 1, 0, 704, 100
35236, V, 1, 1, 1, 1, 0, 704, 100
35237, V, 1, 1, 1, 1, 0, 704, 100
35238, V, 1, 1, 1, 1, 0, 704, 100
35239, V, 1, 1, 1, 1, 0, 704, 100
35240, V, 1, 1, 1, 1, 0, 704, 100
35241, V, 1, 1, 1, 1, 0, 704, 100
35243, V, 1, 1, 1, 1, 0, 704, 100
35244, V, 1, 1, 1, 1, 0, 704, 100
35245, V, 1, 1, 1, 1, 0, 704, 100
35246, V, 1, 1, 1, 1, 0, 704, 100
35247, V, 1, 1, 1, 1, 0, 704, 100
35248, V, 1, 1, 1, 1, 0, 704, 100
35249, V, 1, 1, 1, 1, 0, 704, 100
35250, V, 1, 1, 1, 1, 0, 704, 100
35251, V, 1, 1, 1, 1, 0, 704, 100
35252, V, 1, 1, 1, 1, 0, 704, 100
35253, V, 1, 1, 1, 1, 0, 704, 100
35254, V, 1, 1, 1, 1, 0, 704, 100
35255, V, 1, 1, 1, 1, 0, 704, 100
35256, V, 1, 1, 1, 1, 0, 704, 100
35257, V, 1, 1, 1, 1, 0, 704, 100
35258, V, 1, 1, 1, 1, 0, 704, 100
35259, V, 1, 1, 1, 1, 0, 704, 100
35260, V, 1, 1, 1, 1, 0, 704, 100
35261, V, 1, 1, 1, 1, 0, 704, 100
35262, V, 1, 1, 1, 1, 0, 704, 100
35263, V, 1, 1, 1, 1, 0, 704, 100
35264, V, 1, 1, 1, 1, 0, 704, 100
35265, V, 1, 1, 1, 1, 0, 704, 100
35266, V, 1, 1, 1, 1, 0, 704, 100
35267, V, 1, 1, 1, 1, 0, 704, 100
35268, V, 1, 1, 1, 1, 0, 704, 100
35269, V, 1, 1, 1, 1, 0, 704, 100
35270, V, 1, 1, 1, 1, 0, 704, 100
35271, V, 1, 1, 1, 1, 0, 704, 100
35272, V, 1, 1, 1, 1, 0, 704, 100
35273, V, 1, 1, 1, 1, 0, 704, 100
35274, V, 1, 1, 1, 1, 0, 704, 100
35275, V, 1, 1, 1, 1, 0, 704, 100
35276, V, 1, 1, 1, 1, 0, 704, 100
35277, V, 1, 1, 1, 1, 0, 704, 100
35278, V, 1, 1, 1, 1, 0, 704, 100
35279, V, 1, 1, 1, 1, 0, 704, 100
35280, V, 1, 1, 1, 1, 0, 704, 100
35281, V, 1, 1, 1, 1, 0, 704, 100
35282, V, 1, 1, 1, 1, 0, 704, 100
35283, V, 1, 1, 1, 1, 0, 704, 100
35284, V, 1, 1, 1, 1, 0, 704, 100
35286, V, 1, 1, 1, 1, 0, 704, 100
35287, V, 1, 1, 1, 1, 0, 704, 100
35288, V, 1, 1, 1, 1, 0, 704, 100
35289, V, 1, 1, 1, 1, 0, 704, 100
35290, V, 1, 1, 1, 1, 0, 704, 100
35291, V, 1, 1, 1, 1, 0, 704, 100
35292, V, 1, 1, 1, 1, 0, 704, 100
35293, V, 1, 1, 1, 1, 0, 704, 100
35294, V, 1, 1, 1, 1, 0, 704, 100
35295, V, 1, 1, 1, 1, 0, 704, 100
35296, V, 1, 1, 1, 1, 0, 704, 100
35297, V, 1, 1, 1, 1, 0, 704, 100
35298, V, 1, 1, 1, 1, 0, 704, 100
35299, V, 1, 1, 1, 1, 0, 704, 100
35300, V, 1, 1, 1, 1, 0, 704, 100
35301, V, 1, 1, 1, 1, 0, 704, 100
35302, V, 1, 1, 1, 1, 0, 704, 100
35303, V, 1, 1, 1, 1, 0, 704, 100
35304, V, 1, 1, 1, 1, 0, 704, 100
35305, V, 1, 1, 1, 1, 0, 704, 100
35306, V, 1, 1, 1, 1, 0, 704, 100
35307, V, 1, 1, 1, 1, 0, 704, 100
35308, V, 1, 1, 1, 1, 0, 704, 100
35309, V, 1, 1, 1, 1, 0, 704, 100
35310, V, 1, 1, 1, 1, 0, 704, 100
35311, V, 1, 1, 1, 1, 0, 704, 100
35312, V, 1, 1, 1, 1, 0, 704, 100
35313, V, 1, 1, 1, 1, 0, 704, 100
35314, V, 1, 1, 1, 1, 0, 704, 100
35315, V, 1, 1, 1, 1, 0, 704, 100
35316, V, 1, 1, 1, 1, 0, 704, 100
35317, V, 1, 1, 1, 1, 0, 704, 100
35318, V, 1, 1, 1, 1, 0, 704, 100
35319, V, 1, 1, 1, 1, 0, 704, 100
35320, V, 1, 1, 1, 1, 0, 704, 100
35321, V, 1, 1, 1, 1, 0, 704, 100
35322, V, 1, 1, 1, 1, 0, 704, 100
35323, V, 1, 1, 1, 1, 0, 704, 100
35324, V, 1, 1, 1, 1, 0, 704, 100
35325, V, 1, 1, 1, 1, 0, 704, 100
35326, V, 1, 1, 1, 1, 0, 704, 100
35328, V, 1, 1, 1, 1, 0, 704, 100
35329, V, 1, 1, 1, 1, 0, 704, 100
35330, V, 1, 1, 1, 1, 0, 704, 100
35331, V, 1, 1, 1, 1, 0, 704, 100
35332, V, 1, 1, 1, 1, 0, 704, 100
35333, V, 1, 1, 1, 1, 0, 704, 100
35334, V, 1, 1, 1, 1, 0, 704, 100
35335, V, 1, 1, 1, 1, 0, 704, 100
35336, V, 1, 1, 1, 1, 0, 704, 100
35337, V, 1, 1, 1, 1, 0, 704, 100
35338, V, 1, 1, 1, 1, 0, 704, 100
35339, V, 1, 1, 1, 1, 0, 704, 100
35340, V, 1, 1, 1, 1, 0, 704, 100
35341, V, 1, 1, 1, 1, 0, 704, 100
35342, V, 1, 1, 1, 1, 0, 704, 100
35343, V, 1, 1, 1, 1, 0, 704, 100
35344, V, 1, 1, 1, 1, 0, 704, 100
35345, V, 1, 1, 1, 1, 0, 704, 100
35346, V, 1, 1, 1, 1, 0, 704, 100
35347, V, 1, 1, 1, 1, 0, 704, 100
35348, V, 1, 1, 1, 1, 0, 704, 100
35349, V, 1, 1, 1, 1, 0, 704, 100
35350, V, 1, 1, 1, 1, 0, 704, 100
35351, V, 1, 1, 1, 1, 0, 704, 100
35352, V, 1, 1, 1, 1, 0, 704, 100
35353, V, 1, 1, 1, 1, 0, 704, 100
35354, V, 1, 1, 1, 1, 0, 704, 100
35355, V, 1, 1, 1, 1, 0, 704, 100
35356, V, 1, 1, 1, 1, 0, 704, 100
35357, V, 1, 1, 1, 1, 0, 704, 100
35358, V, 1, 1, 1, 1, 0, 704, 100
35359, V, 1, 1, 1, 1, 0, 704, 100
35360, V, 1, 1, 1, 1, 0, 704, 100
35361, V, 1, 1, 1, 1, 0, 704, 100
35362, V, 1, 1, 1, 1, 0, 704, 100
35363, V, 1, 1, 1, 1, 0, 704, 100
35364, V, 1, 1, 1, 1, 0, 704, 100
35365, V, 1, 1, 1, 1, 0, 704, 100
35366, V, 1, 1, 1, 1, 0, 704, 100
35367, V, 1, 1, 1, 1, 0, 704, 100
35368, V, 1, 1, 1, 1, 0, 704, 100
35369, V, 1, 1, 1, 1, 0, 704, 100
35371, V, 1, 1, 1, 1, 0, 704, 100
35372, V, 1, 1, 1, 1, 0, 704, 100
35373, V, 1, 1, 1, 1, 0, 704, 100
35374, V, 1, 1, 1, 1, 0, 704, 100
35375, V, 1, 1, 1, 1, 0, 704, 100
35376, V, 1, 1, 1, 1, 0, 704, 100
35377, V, 1, 1, 1, 1, 0, 704, 100
35378, V, 1, 1, 1, 1, 0, 704, 100
35379, V, 1, 1, 1, 1, 0, 704, 100
35380, V, 1, 1, 1, 1, 0, 704, 100
35381, V, 1, 1, 1, 1, 0, 704, 100
35382, V, 1, 1, 1, 1, 0, 704, 100
35383, V, 1, 1, 1, 1, 0, 704, 100
35384, V, 1, 1, 1, 1, 0, 704, 100
35385, V, 1, 1, 1, 1, 0, 704, 100
35386, V, 1, 1, 1, 1, 0, 704, 100
35387, V, 1, 1, 1, 1, 0, 704, 100
35388, V, 1, 1, 1, 1, 0, 704, 100
35389, V, 1, 1, 1, 1, 0, 704, 100
35390, V, 1, 1, 1, 1, 0, 704, 100
35391, V, 1, 1, 1, 1, 0, 704, 100
35392, V, 1, 1, 1, 1, 0, 704, 100
35393, V, 1, 1, 1, 1, 0, 704, 100
35394, V, 1, 1, 1, 1, 0, 704, 100
35395, V, 1, 1, 1, 1, 0, 704, 100
35396, V, 1, 1, 1, 1, 0, 704, 100
35397, V, 1, 1, 1, 1, 0, 704, 100
35398, V, 1, 1, 1, 1, 0, 704, 100
35399, V, 1, 1, 1, 1, 0, 704, 100
35400, V, 1, 1, 1, 1, 0, 704, 100
35401, V, 1, 1, 1, 1, 0, 704, 100
35402, V, 1, 1, 1, 1, 0, 704, 100
35403, V, 1, 1, 1, 1, 0, 704, 100
35404, V, 1, 1, 1, 1, 0, 704, 100
35405, V, 1, 1, 1, 1, 0, 704, 100
35406, V, 1, 1, 1, 1, 0, 704, 100
35407, V, 1, 1, 1, 1, 0, 704, 100
35408, V, 1, 1, 1, 1, 0, 704, 100
35409, V, 1, 1, 1, 1, 0, 704, 100
35410, V, 1, 1, 1, 1, 0, 704, 100
35411, V, 1, 1, 1, 1, 0, 704, 100
35412, V, 1, 1, 1, 1, 0, 704, 100
35414, V, 1, 1, 1, 1, 0, 704, 100
35415, V, 1, 1, 1, 1, 0, 704, 100
35416, V, 1, 1, 1, 1, 0, 704, 100
35417, V, 1, 1, 1, 1, 0, 704, 100
35418, V, 1, 1, 1, 1, 0, 704, 100
35419, V, 1, 1, 1, 1, 0, 704, 100
35420, V, 1, 1, 1, 1, 0, 704, 100
35421, V, 1, 1, 1, 1, 0, 704, 100
35422, V, 1, 1, 1, 1, 0, 704, 100
35423, V, 1, 1, 1, 1, 0, 704, 100
35424, V, 1, 1, 1, 1, 0, 704, 100
35425, V, 1, 1, 1, 1, 0, 704, 100
35426, V, 1, 1, 1, 1, 0, 704, 100
35427, V, 1, 1, 1, 1, 0, 704, 100
35428, V, 1, 1, 1, 1, 0, 704, 100
35429, V, 1, 1, 1, 1, 0, 704, 100
35430, V, 1, 1, 1, 1, 0, 704, 100
35431, V, 1, 1, 1, 1, 0, 704, 100
35432, V, 1, 1, 1, 1, 0, 704, 100
35433, V, 1, 1, 1, 1, 0, 704, 100
35434, V, 1, 1, 1, 1, 0, 704, 100
35435, V, 1, 1, 1, 1, 0, 704, 100
35436, V, 1, 1, 1, 1, 0, 704, 100
35437, V, 1, 1, 1, 1, 0, 704, 100
35438, V, 1, 1, 1, 1, 0, 704, 100
35439, V, 1, 1, 1, 1, 0, 704, 100
35440, V, 1, 1, 1, 1, 0, 704, 100
35441, V, 1, 1, 1, 1, 0, 704, 100
35442, V, 1, 1, 1, 1, 0, 704, 100
35443, V, 1, 1, 1, 1, 0, 704, 100
35444, V, 1, 1, 1, 1, 0, 704, 100
35445, V, 1, 1, 1, 1, 0, 704, 100
35446, V, 1, 1, 1, 1, 0, 704, 100
35447, V, 1, 1, 1, 1, 0, 704, 100
35448, V, 1, 1, 1, 1, 0, 704, 100
35449, V, 1, 1, 1, 1, 0, 704, 100
35450, V, 1, 1, 1, 1, 0, 704, 100
35451, V, 1, 1, 1, 1, 0, 704, 100
35452, V, 1, 1, 1, 1, 0, 704, 100
35453, V, 1, 1, 1, 1, 0, 704, 100
35454, V, 1, 1, 1, 1, 0, 704, 100
35456, V, 1, 1, 1, 1, 0, 704, 100
35457, V, 1, 1, 1, 1, 0, 704, 100
35458, V, 1, 1, 1, 1, 0, 704, 100
35459, V, 1, 1, 1, 1, 0, 704, 100
35460, V, 1, 1, 1, 1, 0, 704, 100
35461, V, 1, 1, 1, 1, 0, 704, 100
35462, V, 1, 1, 1, 1, 0, 704, 100
35463, V, 1, 1, 1, 1, 0, 704, 100
35464, V, 1, 1, 1, 1, 0, 704, 100
35465, V, 1, 1, 1, 1, 0, 704, 100
35466, V, 1, 1, 1, 1, 0, 704, 100
35467, V, 1, 1, 1, 1, 0, 704, 100
35468, V, 1, 1, 1, 1, 0, 704, 100
35469, V, 1, 1, 1, 1, 0, 704, 100
35470, V, 1, 1, 1, 1, 0, 704, 100
35471, V, 1, 1, 1, 1, 0, 704, 100
35472, V, 1, 1, 1, 1, 0, 704, 100
35473, V, 1, 1, 1, 1, 0, 704, 100
35474, V, 1, 1, 1, 1, 0, 704, 100
35475, V, 1, 1, 1, 1, 0, 704, 100
35476, V, 1, 1, 1, 1, 0, 704, 100
35477, V, 1, 1, 1, 1, 0, 704, 100
35478, V, 1, 1, 1, 1, 0, 704, 100
35479, V, 1, 1, 1, 1, 0, 704, 100
35480, V, 1, 1, 1, 1, 0, 704, 100
35481, V, 1, 1, 1, 1, 0, 704, 100
35482, V, 1, 1, 1, 1, 0, 704, 100
35483, V, 1, 1, 1, 1, 0, 704, 100
35484, V, 1, 1, 1, 1, 0, 704, 100
35485, V, 1, 1, 1, 1, 0, 704, 100
35486, V, 1, 1, 1, 1, 0, 704, 100
35487, V, 1, 1, 1, 1, 0, 704, 100
35488, V, 1, 1, 1, 1, 0, 704, 100
35489, V, 1, 1, 1, 1, 0, 704, 100
35490, V, 1, 1, 1, 1, 0, 704, 100
35491, V, 1, 1, 1, 1, 0, 704, 100
35492, V, 1, 1, 1, 1, 0, 704, 100
35493, V, 1, 1, 1, 1, 0, 704, 100
35494, V, 1, 1, 1, 1, 0, 704, 100
35495, V, 1, 1, 1, 1, 0, 704, 100
35496, V, 1, 1, 1, 1, 0, 704, 100
35497, V, 1, 1, 1, 1, 0, 704, 100
35499, V, 1, 1, 1, 1, 0, 704, 100
35500, V, 1, 1, 1, 1, 0, 704, 100
35501, V, 1, 1, 1, 1, 0, 704, 100
35502, V, 1, 1, 1, 1, 0, 704, 100
35503, V, 1, 1, 1, 1, 0, 704, 100
35504, V, 1, 1, 1, 1, 0, 704, 100
35505, V, 1, 1, 1, 1, 0, 704, 100
35506, V, 1, 1, 1, 1, 0, 704, 100
35507, V, 1, 1, 1, 1, 0, 704, 100
35508, V, 1, 1, 1, 1, 0, 704, 100
35509, V, 1, 1, 1, 1, 0, 704, 100
35510, V, 1, 1, 1, 1, 0, 704, 100
35511, V, 1, 1, 1, 1, 0, 704, 100
35512, V, 1, 1, 1, 1, 0, 704, 100
35513, V, 1, 1, 1, 1, 0, 704, 100
35514, V, 1, 1, 1, 1, 0, 704, 100
35515, V, 1, 1, 1, 1, 0, 704, 100
35516, V, 1, 1, 1, 1, 0, 704, 100
35517, V, 1, 1, 1, 1, 0, 704, 100
35518, V, 1, 1, 1, 1, 0, 704, 100
35519, V, 1, 1, 1, 1, 0, 704, 100
35520, V, 1, 1, 1, 1, 0, 704, 100
35521, V, 1, 1, 1, 1, 0, 704, 100
35522, V, 1, 1, 1, 1, 0, 704, 100
35523, V, 1, 1, 1, 1, 0, 704, 100
35524, V, 1, 1, 1, 1, 0, 704, 100
35525, V, 1, 1, 1, 1, 0, 704, 100
35526, V, 1, 1, 1, 1, 0, 704, 100
35527, V, 1, 1, 1, 1, 0, 704, 100
35528, V, 1, 1, 1, 1, 0, 704, 100
35529, V, 1, 1, 1, 1, 0, 704, 100
35530, V, 1, 1, 1, 1, 0, 704, 100
35531, V, 1, 1, 1, 1, 0, 704, 100
35532, V, 1, 1, 1, 1, 0, 704, 100
35533, V, 1, 1, 1, 1, 0, 704, 100
35534, V, 1, 1, 1, 1, 0, 704, 100
35535, V, 1, 1, 1, 1, 0, 704, 100
35536, V, 1, 1, 1, 1, 0, 704, 100
35537, V, 1, 1, 1, 1, 0, 704, 100
35538, V, 1, 1, 1, 1, 0, 704, 100
35539, V, 1, 1, 1, 1, 0, 704, 100
35540, V, 1, 1, 1, 1, 0, 704, 100
35542, V, 1, 1, 1, 1, 0, 704, 100
35543, V, 1, 1, 1, 1, 0, 704, 100
35544, V, 1, 1, 1, 1, 0, 704, 100
35545, V, 1, 1, 1, 1, 0, 704, 100
35546, V, 1, 1, 1, 1, 0, 704, 100
35547, V, 1, 1, 1, 1, 0, 704, 100
35548, V, 1, 1, 1, 1, 0, 704, 100
35549, V, 1, 1, 1, 1, 0, 704, 100
35550, V, 1, 1, 1, 1, 0, 704, 100
35551, V, 1, 1, 1, 1, 0, 704, 100
35552, V, 1, 1, 1, 1, 0, 704, 100
35553, V, 1, 1, 1, 1, 0, 704, 100
35554, V, 1, 1, 1, 1, 0, 704, 100
35555, V, 1, 1, 1, 1, 0, 704, 100
35556, V, 1, 1, 1, 1, 0, 704, 100
35557, V, 1, 1, 1, 1, 0, 704, 100
35558, V, 1, 1, 1, 1, 0, 704, 100
35559, V, 1, 1, 1, 1, 0, 704, 100
35560, V, 1, 1, 1, 1, 0, 704, 100
35561, V, 1, 1, 1, 1, 0, 704, 100
35562, V, 1, 1, 1, 1, 0, 704, 100
35563, V, 1, 1, 1, 1, 0, 704, 100
35564, V, 1, 1, 1, 1, 0, 704, 100
35565, V, 1, 1, 1, 1, 0, 704, 100
35566, V, 1, 1, 1, 1, 0, 704, 100
35567, V, 1, 1, 1, 1, 0, 704, 100
35568, V, 1, 1, 1, 1, 0, 704, 100
35569, V, 1, 1, 1, 1, 0, 704, 100
35570, V, 1, 1, 1, 1, 0, 704, 100
35571, V, 1, 1, 1, 1, 0, 704, 100
35572, V, 1, 1, 1, 1, 0, 704, 100
35573, V, 1, 1, 1, 1, 0, 704, 100
35574, V, 1, 1, 1, 1, 0, 704, 100
35575, V, 1, 1, 1, 1, 0, 704, 100
35576, V, 1, 1, 1, 1, 0, 704, 100
35577, V, 1, 1, 1, 1, 0, 704, 100
35578, V, 1, 1, 1, 1, 0, 704, 100
35579, V, 1, 1, 1, 1, 0, 704, 100
35580, V, 1, 1, 1, 1, 0, 704, 100
35581, V, 1, 1, 1, 1, 0, 704, 100
35582, V, 1, 1, 1, 1, 0, 704, 100
35584, V, 1, 1, 1, 1, 0, 704, 100
35585, V, 1, 1, 1, 1, 0, 704, 100
35586, V, 1, 1, 1, 1, 0, 704, 100
35587, V, 1, 1, 1, 1, 0, 704, 100
35588, V, 1, 1, 1, 1, 0, 704, 100
35589, V, 1, 1, 1, 1, 0, 704, 100
35590, V, 1, 1, 1, 1, 0, 704, 100
35591, V, 1, 1, 1, 1, 0, 704, 100
35592, V, 1, 1, 1, 1, 0, 704, 100
35593, V, 1, 1, 1, 1, 0, 704, 100
35594, V, 1, 1, 1, 1, 0, 704, 100
35595, V, 1, 1, 1, 1, 0, 704, 100
35596, V, 1, 1, 1, 1, 0, 704, 100
35597, V, 1, 1, 1, 1, 0, 704, 100
35598, V, 1, 1, 1, 1, 0, 704, 100
35599, V, 1, 1, 1, 1, 0, 704, 100
35600, V, 1, 1, 1, 1, 0, 704, 100
35601, V, 1, 1, 1, 1, 0, 704, 100
35602, V, 1, 1, 1, 1, 0, 704, 100
35603, V, 1, 1, 1, 1, 0, 704, 100
35604, V, 1, 1, 1, 1, 0, 704, 100
35605, V, 1, 1, 1, 1, 0, 704, 100
35606, V, 1, 1, 1, 1, 0, 704, 100
35607, V, 1, 1, 1, 1, 0, 704, 100
35608, V, 1, 1, 1, 1, 0, 704, 100
35609, V, 1, 1, 1, 1, 0, 704, 100
35610, V, 1, 1, 1, 1, 0, 704, 100
35611, V, 1, 1, 1, 1, 0, 704, 100
35612, V, 1, 1, 1, 1, 0, 704, 100
35613, V, 1, 1, 1, 1, 0, 704, 100
35614, V, 1, 1, 1, 1, 0, 704, 100
35615, V, 1, 1, 1, 1, 0, 704, 100
35616, V, 1, 1, 1, 1, 0, 704, 100
35617, V, 1, 1, 1, 1, 0, 704, 100
35618, V, 1, 1, 1, 1, 0, 704, 100
35619, V, 1, 1, 1, 1, 0, 704, 100
35620, V, 1, 1, 1, 1, 0, 704, 100
35621, V, 1, 1, 1, 1, 0, 704, 100
35622, V, 1, 1, 1, 1, 0, 704, 100
35623, V, 1, 1, 1, 1, 0, 704, 100
35624, V, 1, 1, 1, 1, 0, 704, 100
35625, V, 1, 1, 1, 1, 0, 704, 100
35627, V, 1, 1, 1, 1, 0, 704, 100
35628, V, 1, 1, 1, 1, 0, 704, 100
35629, V, 1, 1, 1, 1, 0, 704, 100
35630, V, 1, 1, 1, 1, 0, 704, 100
35631, V, 1, 1, 1, 1, 0, 704, 100
35632, V, 1, 1, 1, 1, 0, 704, 100
35633, V, 1, 1, 1, 1, 0, 704, 100
35634, V, 1, 1, 1, 1, 0, 704, 100
35635, V, 1, 1, 1, 1, 0, 704, 100
35636, V, 1, 1, 1, 1, 0, 704, 100
35637, V, 1, 1, 1, 1, 0, 704, 100
35638, V, 1, 1, 1, 1, 0, 704, 100
35639, V, 1, 1, 1, 1, 0, 704, 100
35640, V, 1, 1, 1, 1, 0, 704, 100
35641, V, 1, 1, 1, 1, 0, 704, 100
35642, V, 1, 1, 1, 1, 0, 704, 100
35643, V, 1, 1, 1, 1, 0, 704, 100
35644, V, 1, 1, 1, 1, 0, 704, 100
35645, V, 1, 1, 1, 1, 0, 704, 100
35646, V, 1, 1, 1, 1, 0, 704, 100
35647, V, 1, 1, 1, 1, 0, 704, 100
35648, V, 1, 1, 1, 1, 0, 704, 100
35649, V, 1, 1, 1, 1, 0, 704, 100
35650, V, 1, 1, 1, 1, 0, 704, 100
35651, V, 1, 1, 1, 1, 0, 704, 100
35652, V, 1, 1, 1, 1, 0, 704, 100
35653, V, 1, 1, 1, 1, 0, 704, 100
35654, V, 1, 1, 1, 1, 0, 704, 100
35655, V, 1, 1, 1, 1, 0, 704, 100
35656, V, 1, 1, 1, 1, 0, 704, 100
35657, V, 1, 1, 1, 1, 0, 704, 100
35658, V, 1, 1, 1, 1, 0, 704, 100
35659, V, 1, 1, 1, 1, 0, 704, 100
35660, V, 1, 1, 1, 1, 0, 704, 100
35661, V, 1, 1, 1, 1, 0, 704, 100
35662, V, 1, 1, 1, 1, 0, 704, 100
35663, V, 1, 1, 1, 1, 0, 704, 100
35664, V, 1, 1, 1, 1, 0, 704, 100
35665, V, 1, 1, 1, 1, 0, 704, 100
35666, V, 1, 1, 1, 1, 0, 704, 100
35667, V, 1, 1, 1, 1, 0, 704, 100
35668, V, 1, 1, 1, 1, 0, 704, 100
35670, V, 1, 1, 1, 1, 0, 704, 100
35671, V, 1, 1, 1, 1, 0, 704, 100
35672, V, 1, 1, 1, 1, 0, 704, 100
35673, V, 1, 1, 1, 1, 0, 704, 100
35674, V, 1, 1, 1, 1, 0, 704, 100
35675, V, 1, 1, 1, 1, 0, 704, 100
35676, V, 1, 1, 1, 1, 0, 704, 100
35677, V, 1, 0, 0, 1, 0, 704, 100
35677, V, 1, 0, 0, 0, 0, 704, 100
35678, V, 1, 1, 0, 0, 0, 704, 100
35678, V, 1, 1, 0, 0, 0, 704, 100
35679, V, 1, 1, 1, 1, 0, 704, 100
35680, V, 1, 1, 1, 1, 0, 704, 100
35681, V, 1, 1, 1, 1, 0, 704, 100
35682, V, 1, 1, 1, 1, 0, 704, 100
35683, V, 1, 1, 1, 1, 0, 704, 99
35684, V, 1, 1, 1, 1, 0, 704, 99
35685, V, 1, 1, 1, 1, 0, 704, 99
35686, V, 1, 1, 1, 1, 0, 704, 99
35687, V, 1, 1, 1, 1, 0, 704, 99
35688, V, 1, 1, 1, 1, 0, 704, 99
35689, V, 1, 1, 1, 1, 0, 704, 99
35690, V, 1, 1, 1, 1, 0, 704, 99
35691, V, 1, 1, 1, 1, 0, 704, 99
35692, V, 1, 1, 1, 1, 0, 704, 99
35693, V, 1, 1, 1, 1, 0, 704, 99
35694, V, 1, 1, 1, 1, 0, 704, 99
35695, V, 1, 1, 1, 1, 0, 704, 99
35696, V, 1, 1, 1, 1, 0, 704, 99
35697, V, 1, 1, 1, 1, 0, 704, 99
35698, V, 1, 1, 1, 1, 0, 704, 100
35699, V, 1, 1, 1, 1, 0, 704, 99
35700, V, 1, 1, 1, 1, 0, 704, 99
35701, V, 1, 1, 1, 1, 0, 704, 99
35702, V, 1, 1, 1, 1, 0, 704, 99
35703, V, 1, 1, 1, 1, 0, 704, 100
35704, V, 1, 1, 1, 1, 0, 704, 99
35705, V, 1, 1, 1, 1, 0, 704, 100
35706, V, 1, 1, 1, 1, 0, 704, 100
35707, V, 1, 1, 1, 1, 0, 704, 99
35708, V, 1, 1, 1, 1, 0, 704, 100
35709, V, 1, 1, 1, 1, 0, 704, 100
35710, V, 1, 1, 1, 1, 0, 704, 100
35712, V, 1, 1, 1, 1, 0, 704, 100
35713, V, 1, 1, 1, 1, 0, 704, 100
35714, V, 1, 1, 1, 1, 0, 704, 100
35715, V, 1, 1, 1, 1, 0, 704, 100
35716, V, 1, 1, 1, 1, 0, 704, 100
35717, V, 1, 1, 1, 1, 0, 704, 100
35718, V, 1, 1, 1, 1, 0, 704, 100
35719, V, 1, 1, 1, 1, 0, 704, 100
35720, V, 1, 1, 1, 1, 0, 704, 100
35721, V, 1, 1, 1, 1, 0, 704, 100
35722, V, 1, 1, 1, 1, 0, 704, 100
35723, V, 1, 1, 1, 1, 0, 704, 100
35724, V, 1, 1, 1, 1, 0, 704, 100
35725, V, 1, 1, 1, 1, 0, 704, 100
35726, V, 1, 1, 1, 1, 0, 704, 100
35727, V, 1, 1, 1, 1, 0, 704, 100
35728, V, 1, 1, 1, 1, 0, 704, 100
35729, V, 1, 1, 1, 1, 0, 704, 100
35730, V, 1, 1, 1, 1, 0, 704, 100
35731, V, 1, 1, 1, 1, 0, 704, 100
35732, V, 1, 1, 1, 1, 0, 704, 100
35733, V, 1, 1, 1, 1, 0, 704, 100
35734, V, 1, 1, 1, 1, 0, 704, 100
35735, V, 1, 1, 1, 1, 0, 704, 100
35736, V, 1, 1, 1, 1, 0, 704, 100
35737, V, 1, 1, 1, 1, 0, 704, 100
35738, V, 1, 1, 1, 1, 0, 704, 100
35739, V, 1, 1, 1, 1, 0, 704, 100
35740, V, 1, 1, 1, 1, 0, 704, 100
35741, V, 1, 1, 1, 1, 0, 704, 100
35742, V, 1, 1, 1, 1, 0, 704, 100
35743, V, 1, 1, 1, 1, 0, 704, 100
35744, V, 1, 1, 1, 1, 0, 704, 100
35745, V, 1, 1, 1, 1, 0, 704, 100
35746, V, 1, 1, 1, 1, 0, 704, 100
35747, V, 1, 1, 1, 1, 0, 704, 100
35748, V, 1, 1, 1, 1, 0, 704, 100
35749, V, 1, 1, 1, 1, 0, 704, 100
35750, V, 1, 1, 1, 1, 0, 704, 100
35751, V, 1, 1, 1, 1, 0, 704, 100
35752, V, 1, 1, 1, 1, 0, 704, 100
35753, V, 1, 1, 1, 1, 0, 704, 100
35755, V, 1, 1, 1, 1, 0, 704, 100
35756, V, 1, 1, 1, 1, 0, 704, 100
35757, V, 1, 1, 1, 1, 0, 704, 100
35758, V, 1, 1, 1, 1, 0, 704, 100
35759, V, 1, 1, 1, 1, 0, 704, 100
35760, V, 1, 1, 1, 1, 0, 704, 100
35761, V, 1, 1, 1, 1, 0, 704, 100
35762, V, 1, 1, 1, 1, 0, 704, 100
35763, V, 1, 1, 1, 1, 0, 704, 100
35764, V, 1, 1, 1, 1, 0, 704, 100
35765, V, 1, 1, 1, 1, 0, 704, 100
35766, V, 1, 1, 1, 1, 0, 704, 100
35767, V, 1, 1, 1, 1, 0, 704, 100
35768, V, 1, 1, 1, 1, 0, 704, 100
35769, V, 1, 1, 1, 1, 0, 704, 100
35770, V, 1, 1, 1, 1, 0, 704, 100
35771, V, 1, 1, 1, 1, 0, 704, 100
35772, V, 1, 1, 1, 1, 0, 704, 100
35773, V, 1, 1, 1, 1, 0, 704, 100
35774, V, 1, 1, 1, 1, 0, 704, 100
35775, V, 1, 1, 1, 1, 0, 704, 100
35776, V, 1, 1, 1, 1, 0, 704, 100
35777, V, 1, 1, 1, 1, 0, 704, 100
35778, V, 1, 1, 1, 1, 0, 704, 100
35779, V, 1, 1, 1, 1, 0, 704, 100
35780, V, 1, 1, 1, 1, 0, 704, 100
35781, V, 1, 1, 1, 1, 0, 704, 100
35782, V, 1, 1, 1, 1, 0, 704, 100
35783, V, 1, 1, 1, 1, 0, 704, 100
35784, V, 1, 1, 1, 1, 0, 704, 100
35785, V, 1, 1, 1, 1, 0, 704, 100
35786, V, 1, 1, 1, 1, 0, 704, 100
35787, V, 1, 1, 1, 1, 0, 704, 100
35788, V, 1, 1, 1, 1, 0, 704, 100
35789, V, 1, 1, 1, 1, 0, 704, 100
35790, V, 1, 1, 1, 1, 0, 704, 100
35791, V, 1, 1, 1, 1, 0, 704, 100
35792, V, 1, 1, 1, 1, 0, 704, 100
35793, V, 1, 1, 1, 1, 0, 704, 100
35794, V, 1, 1, 1, 1, 0, 704, 100
35795, V, 1, 1, 1, 1, 0, 704, 100
35796, V, 1, 1, 1, 1, 0, 704, 100
35798, V, 1, 1, 1, 1, 0, 704, 100
35799, V, 1, 1, 1, 1, 0, 704, 100
35800, V, 1, 1, 1, 1, 0, 704, 100
35801, V, 1, 1, 1, 1, 0, 704, 100
35802, V, 1, 1, 1, 1, 0, 704, 100
35803, V, 1, 1, 1, 1, 0, 704, 100
35804, V, 1, 1, 1, 1, 0, 704, 100
35805, V, 1, 1, 1, 1, 0, 704, 100
35806, V, 1, 1, 1, 1, 0, 704, 100
35807, V, 1, 1, 1, 1, 0, 704, 100
35808, V, 1, 1, 1, 1, 0, 704, 100
35809, V, 1, 1, 1, 1, 0, 704, 100
35810, V, 1, 1, 1, 1, 0, 704, 100
35811, V, 1, 1, 1, 1, 0, 704, 100
35812, V, 1, 1, 1, 1, 0, 704, 100
35813, V, 1, 1, 1, 1, 0, 704, 100
35814, V, 1, 1, 1, 1, 0, 704, 100
35815, V, 1, 1, 1, 1, 0, 704, 100
35816, V, 1, 1, 1, 1, 0, 704, 100
35817, V, 1, 1, 1, 1, 0, 704, 100
35818, V, 1, 1, 1, 1, 0, 704, 100
35819, V, 1, 1, 1, 1, 0, 704, 100
35820, V, 1, 1, 1, 1, 0, 704, 100
35821, V, 1, 1, 1, 1, 0, 704, 100
35822, V, 1, 1, 1, 1, 0, 704, 100
35823, V, 1, 1, 1, 1, 0, 704, 100
35824, V, 1, 1, 1, 1, 0, 704, 100
35825, V, 1, 1, 1, 1, 0, 704, 100
35826, V, 1, 1, 1, 1, 0, 704, 100
35827, V, 1, 1, 1, 1, 0, 704, 100
35828, V, 1, 1, 1, 1, 0, 704, 100
35829, V, 1, 1, 1, 1, 0, 704, 100
35830, V, 1, 1, 1, 1, 0, 704, 100
35831, V, 1, 1, 1, 1, 0, 704, 100
35832, V, 1, 1, 1, 1, 0, 704, 100
35833, V, 1, 1, 1, 1, 0, 704, 100
35834, V, 1, 1, 1, 1, 0, 704, 100
35835, V, 1, 1, 1, 1, 0, 704, 100
35836, V, 1, 1, 1, 1, 0, 704, 100
35837, V, 1, 1, 1, 1, 0, 704, 100
35838, V, 1, 1, 1, 1, 0, 704, 100
35840, V, 1, 1, 1, 1, 0, 704, 100
35841, V, 1, 1, 1, 1, 0, 704, 100
35842, V, 1, 1, 1, 1, 0, 704, 100
35843, V, 1, 1, 1, 1, 0, 704, 100
35844, V, 1, 1, 1, 1, 0, 704, 100
35845, V, 1, 1, 1, 1, 0, 704, 100
35846, V, 1, 1, 1, 1, 0, 704, 100
35847, V, 1, 1, 1, 1, 0, 704, 100
35848, V, 1, 1, 1, 1, 0, 704, 100
35849, V, 1, 1, 1, 1, 0, 704, 100
35850, V, 1, 1, 1, 1, 0, 704, 100
35851, V, 1, 1, 1, 1, 0, 704, 100
35852, V, 1, 1, 1, 1, 0, 704, 100
35853, V, 1, 1, 1, 1, 0, 704, 100
35854, V, 1, 1, 1, 1, 0, 704, 100
35855, V, 1, 1, 1, 1, 0, 704, 100
35856, V, 1, 1, 1, 1, 0, 704, 100
35857, V, 1, 1, 1, 1, 0, 704, 100
35858, V, 1, 1, 1, 1, 0, 704, 100
35859, V, 1, 1, 1, 1, 0, 704, 100
35860, V, 1, 1, 1, 1, 0, 704, 100
35861, V, 1, 1, 1, 1, 0, 704, 100
35862, V, 1, 1, 1, 1, 0, 704, 100
35863, V, 1, 1, 1, 1, 0, 704, 100
35864, V, 1, 1, 1, 1, 0, 704, 100
35865, V, 1, 1, 1, 1, 0, 704, 100
35866, V, 1, 1, 1, 1, 0, 704, 100
35867, V, 1, 1, 1, 1, 0, 704, 100
35868, V, 1, 1, 1, 1, 0, 704, 100
35869, V, 1, 1, 1, 1, 0, 704, 100
35870, V, 1, 1, 1, 1, 0, 704, 100
35871, V, 1, 1, 1, 1, 0, 704, 100
35872, V, 1, 1, 1, 1, 0, 704, 100
35873, V, 1, 1, 1, 1, 0, 704, 100
35874, V, 1, 1, 1, 1, 0, 704, 100
35875, V, 1, 1, 1, 1, 0, 704, 100
35876, V, 1, 1, 1, 1, 0, 704, 100
35877, V, 1, 1, 1, 1, 0, 704, 100
35878, V, 1, 1, 1, 1, 0, 704, 100
35879, V, 1, 1, 1, 1, 0, 704, 100
35880, V, 1, 1, 1, 1, 0, 704, 100
35881, V, 1, 1, 1, 1, 0, 704, 100
35883, V, 1, 1, 1, 1, 0, 704, 100
35884, V, 1, 1, 1, 1, 0, 704, 100
35885, V, 1, 1, 1, 1, 0, 704, 100
35886, V, 1, 1, 1, 1, 0, 704, 100
35887, V, 1, 1, 1, 1, 0, 704, 100
35888, V, 1, 1, 1, 1, 0, 704, 100
35889, V, 1, 1, 1, 1, 0, 704, 100
35890, V, 1, 1, 1, 1, 0, 704, 100
35891, V, 1, 1, 1, 1, 0, 704, 100
35892, V, 1, 1, 1, 1, 0, 704, 100
35893, V, 1, 1, 1, 1, 0, 704, 100
35894, V, 1, 1, 1, 1, 0, 704, 100
35895, V, 1, 1, 1, 1, 0, 704, 100
35896, V, 1, 1, 1, 1, 0, 704, 100
35897, V, 1, 1, 1, 1, 0, 704, 100
35898, V, 1, 1, 1, 1, 0, 704, 100
35899, V, 1, 1, 1, 1, 0, 704, 100
35900, V, 1, 1, 1, 1, 0, 704, 100
35901, V, 1, 1, 1, 1, 0, 704, 100
35902, V, 1, 1, 1, 1, 0, 704, 100
35903, V, 1, 1, 1, 1, 0, 704, 100
35904, V, 1, 1, 1, 1, 0, 704, 100
35905, V, 1, 1, 1, 1, 0, 704, 100
35906, V, 1, 1, 1, 1, 0, 704, 100
35907, V, 1, 1, 1, 1, 0, 704, 100
35908, V, 1, 1, 1, 1, 0, 704, 100
35909, V, 1, 1, 1, 1, 0, 704, 100
35910, V, 1, 1, 1, 1, 0, 704, 100
35911, V, 1, 1, 1, 1, 0, 704, 100
35912, V, 1, 1, 1, 1, 0, 704, 100
35913, V, 1, 1, 1, 1, 0, 704, 100
35914, V, 1, 1, 1, 1, 0, 704, 100
35915, V, 1, 1, 1, 1, 0, 704, 100
35916, V, 1, 1, 1, 1, 0, 704, 100
35917, V, 1, 1, 1, 1, 0, 704, 100
35918, V, 1, 1, 1, 1, 0, 704, 100
35919, V, 1, 1, 1, 1, 0, 704, 100
35920, V, 1, 1, 1, 1, 0, 704, 100
35921, V, 1, 1, 1, 1, 0, 704, 100
35922, V, 1, 1, 1, 1, 0, 704, 100
35923, V, 1, 1, 1, 1, 0, 704, 100
35924, V, 1, 1, 1, 1, 0, 704, 100
35926, V, 1, 1, 1, 1, 0, 704, 100
35927, V, 1, 1, 1, 1, 0, 704, 100
35928, V, 1, 1, 1, 1, 0, 704, 100
35929, V, 1, 1, 1, 1, 0, 704, 100
35930, V, 1, 1, 1, 1, 0, 704, 100
35931, V, 1, 1, 1, 1, 0, 704, 100
35932, V, 1, 1, 1, 1, 0, 704, 100
35933, V, 1, 1, 1, 1, 0, 704, 100
35934, V, 1, 1, 1, 1, 0, 704, 100
35935, V, 1, 1, 1, 1, 0, 704, 100
35936, V, 1, 1, 1, 1, 0, 704, 100
35937, V, 1, 1, 1, 1, 0, 704, 100
35938, V, 1, 1, 1, 1, 0, 704, 100
35939, V, 1, 1, 1, 1, 0, 704, 100
35940, V, 1, 1, 1, 1, 0, 704, 100
35941, V, 1, 1, 1, 1, 0, 704, 100
35942, V, 1, 1, 1, 1, 0, 704, 100
35943, V, 1, 1, 1, 1, 0, 704, 100
35944, V, 1, 1, 1, 1, 0, 704, 100
35945, V, 1, 1, 1, 1, 0, 704, 100
35946, V, 1, 1, 1, 1, 0, 704, 100
35947, V, 1, 1, 1, 1, 0, 704, 100
35948, V, 1, 1, 1, 1, 0, 704, 100
35949, V, 1, 1, 1, 1, 0, 704, 100
35950, V, 1, 1, 1, 1, 0, 704, 100
35951, V, 1, 1, 1, 1, 0, 704, 100
35952, V, 1, 1, 1, 1, 0, 704, 100
35953, V, 1, 1, 1, 1, 0, 704, 100
35954, V, 1, 1, 1, 1, 0, 704, 100
35955, V, 1, 1, 1, 1, 0, 704, 100
35956, V, 1, 1, 1, 1, 0, 704, 100
35957, V, 1, 1, 1, 1, 0, 704, 100
35958, V, 1, 1, 1, 1, 0, 704, 100
35959, V, 1, 1, 1, 1, 0, 704, 100
35960, V, 1, 1, 1, 1, 0, 704, 100
35961, V, 1, 1, 1, 1, 0, 704, 100
35962, V, 1, 1, 1, 1, 0, 704, 100
35963, V, 1, 1, 1, 1, 0, 704, 100
35964, V, 1, 1, 1, 1, 0, 704, 100
35965, V, 1, 1, 1, 1, 0, 704, 100
35966, V, 1, 1, 1, 1, 0, 704, 100
35968, V, 1, 1, 1, 1, 0, 704, 100
35969, V, 1, 1, 1, 1, 0, 704, 100
35970, V, 1, 1, 1, 1, 0, 704, 100
35971, V, 1, 1, 1, 1, 0, 704, 100
35972, V, 1, 1, 1, 1, 0, 704, 100
35973, V, 1, 1, 1, 1, 0, 704, 100
35974, V, 1, 1, 1, 1, 0, 704, 100
35975, V, 1, 1, 1, 1, 0, 704, 100
35976, V, 1, 1, 1, 1, 0, 704, 100
35977, V, 1, 1, 1, 1, 0, 704, 100
35978, V, 1, 1, 1, 1, 0, 704, 100
35979, V, 1, 1, 1, 1, 0, 704, 100
35980, V, 1, 1, 1, 1, 0, 704, 100
35981, V, 1, 1, 1, 1, 0, 704, 100
35982, V, 1, 1, 1, 1, 0, 704, 100
35983, V, 1, 1, 1, 1, 0, 704, 100
35984, V, 1, 1, 1, 1, 0, 704, 100
35985, V, 1, 1, 1, 1, 0, 704, 100
35986, V, 1, 1, 1, 1, 0, 704, 100
35987, V, 1, 1, 1, 1, 0, 704, 100
35988, V, 1, 1, 1, 1, 0, 704, 100
35989, V, 1, 1, 1, 1, 0, 704, 100
35990, V, 1, 1, 1, 1, 0, 704, 100
35991, V, 1, 1, 1, 1, 0, 704, 100
35992, V, 1, 1, 1, 1, 0, 704, 100
35993, V, 1, 1, 1, 1, 0, 704, 100
35994, V, 1, 1, 1, 1, 0, 704, 100
35995, V, 1, 1, 1, 1, 0, 704, 100
35996, V, 1, 1, 1, 1, 0, 704, 100
35997, V, 1, 1, 1, 1, 0, 704, 100
35998, V, 1, 1, 1, 1, 0, 704, 100
35999, V, 1, 1, 1, 1, 0, 704, 100
36000, V, 1, 1, 1, 1, 0, 704, 100
36001, V, 1, 1, 1, 1, 0, 704, 100
36002, V, 1, 1, 1, 1, 0, 704, 100
36003, V, 1, 1, 1, 1, 0, 704, 100
36004, V, 1, 1, 1, 1, 0, 704, 100
36005, V, 1, 1, 1, 1, 0, 704, 100
36006, V, 1, 1, 1, 1, 0, 704, 100
36007, V, 1, 1, 1, 1, 0, 704, 100
36008, V, 1, 1, 1, 1, 0, 704, 100
36009, V, 1, 1, 1, 1, 0, 704, 100
36011, V, 1, 1, 1, 1, 0, 704, 100
36012, V, 1, 1, 1, 1, 0, 704, 100
36013, V, 1, 1, 1, 1, 0, 704, 100
36014, V, 1, 1, 1, 1, 0, 704, 100
36015, V, 1, 1, 1, 1, 0, 704, 100
36016, V, 1, 1, 1, 1, 0, 704, 100
36017, V, 1, 1, 1, 1, 0, 704, 100
36018, V, 1, 1, 1, 1, 0, 704, 100
36019, V, 1, 1, 1, 1, 0, 704, 100
36020, V, 1, 1, 1, 1, 0, 704, 100
36021, V, 1, 1, 1, 1, 0, 704, 100
36022, V, 1, 1, 1, 1, 0, 704, 100
36023, V, 1, 1, 1, 1, 0, 704, 100
36024, V, 1, 1, 1, 1, 0, 704, 100
36025, V, 1, 1, 1, 1, 0, 704, 100
36026, V, 1, 1, 1, 1, 0, 704, 100
36027, V, 1, 1, 1, 1, 0, 704, 100
36028, V, 1, 1, 1, 1, 0, 704, 100
36029, V, 1, 1, 1, 1, 0, 704, 100
36030, V, 1, 1, 1, 1, 0, 704, 100
36031, V, 1, 1, 1, 1, 0, 704, 100
36032, V, 1, 1, 1, 1, 0, 704, 100
36033, V, 1, 1, 1, 1, 0, 704, 100
36034, V, 1, 1, 1, 1, 0, 704, 100
36035, V, 1, 1, 1, 1, 0, 704, 100
36036, V, 1, 1, 1, 1, 0, 704, 100
36037, V, 1, 1, 1, 1, 0, 704, 100
36038, V, 1, 1, 1, 1, 0, 704, 100
36039, V, 1, 1, 1, 1, 0, 704, 100
36040, V, 1, 1, 1, 1, 0, 704, 100
36041, V, 1, 1, 1, 1, 0, 704, 100
36042, V, 1, 1, 1, 1, 0, 704, 100
36043, V, 1, 1, 1, 1, 0, 704, 100
36044, V, 1, 1, 1, 1, 0, 704, 100
36045, V, 1, 1, 1, 1, 0, 704, 100
36046, V, 1, 1, 1, 1, 0, 704, 100
36047, V, 1, 1, 1, 1, 0, 704, 100
36048, V, 1, 1, 1, 1, 0, 704, 100
36049, V, 1, 1, 1, 1, 0, 704, 100
36050, V, 1, 1, 1, 1, 0, 704, 100
36051, V, 1, 1, 1, 1, 0, 704, 100
36052, V, 1, 1, 1, 1, 0, 704, 100
36054, V, 1, 1, 1, 1, 0, 704, 100
36055, V, 1, 1, 1, 1, 0, 704, 100
36056, V, 1, 1, 1, 1, 0, 704, 100
36057, V, 1, 1, 1, 1, 0, 704, 100
36058, V, 1, 1, 1, 1, 0, 704, 100
36059, V, 1, 1, 1, 1, 0, 704, 100
36060, V, 1, 1, 1, 1, 0, 704, 100
36061, V, 1, 1, 1, 1, 0, 704, 100
36062, V, 1, 1, 1, 1, 0, 704, 100
36063, V, 1, 1, 1, 1, 0, 704, 100
36064, V, 1, 1, 1, 1, 0, 704, 100
36065, V, 1, 1, 1, 1, 0, 704, 100
36066, V, 1, 1, 1, 1, 0, 704, 100
36067, V, 1, 1, 1, 1, 0, 704, 100
36068, V, 1, 1, 1, 1, 0, 704, 100
36069, V, 1, 1, 1, 1, 0, 704, 100
36070, V, 1, 1, 1, 1, 0, 704, 100
36071, V, 1, 1, 1, 1, 0, 704, 100
36072, V, 1, 1, 1, 1, 0, 704, 100
36073, V, 1, 1, 1, 1, 0, 704, 100
36074, V, 1, 1, 1, 1, 0, 704, 100
36075, V, 1, 1, 1, 1, 0, 704, 100
36076, V, 1, 1, 1, 1, 0, 704, 100
36077, V, 1, 1, 1, 1, 0, 704, 100
36078, V, 1, 1, 1, 1, 0, 704, 100
36079, V, 1, 1, 1, 1, 0, 704, 100
36080, V, 1, 1, 1, 1, 0, 704, 100
36081, V, 1, 1, 1, 1, 0, 704, 100
36082, V, 1, 1, 1, 1, 0, 704, 100
36083, V, 1, 1, 1, 1, 0, 704, 100
36084, V, 1, 1, 1, 1, 0, 704, 100
36085, V, 1, 1, 1, 1, 0, 704, 100
36086, V, 1, 1, 1, 1, 0, 704, 100
36087, V, 1, 1, 1, 1, 0, 704, 100
36088, V, 1, 1, 1, 1, 0, 704, 100
36089, V, 1, 1, 1, 1, 0, 704, 100
36090, V, 1, 1, 1, 1, 0, 704, 100
36091, V, 1, 1, 1, 1, 0, 704, 100
36092, V, 1, 1, 1, 1, 0, 704, 100
36093, V, 1, 1, 1, 1, 0, 704, 100
36094, V, 1, 1, 1, 1, 0, 704, 100
36096, V, 1, 1, 1, 1, 0, 704, 100
36097, V, 1, 1, 1, 1, 0, 704, 100
36098, V, 1, 1, 1, 1, 0, 704, 100
36099, V, 1, 1, 1, 1, 0, 704, 100
36100, V, 1, 1, 1, 1, 0, 704, 100
36101, V, 1, 1, 1, 1, 0, 704, 100
36102, V, 1, 1, 1, 1, 0, 704, 100
36103, V, 1, 1, 1, 1, 0, 704, 100
36104, V, 1, 1, 1, 1, 0, 704, 100
36105, V, 1, 1, 1, 1, 0, 704, 100
36106, V, 1, 1, 1, 1, 0, 704, 100
36107, V, 1, 1, 1, 1, 0, 704, 100
36108, V, 1, 1, 1, 1, 0, 704, 100
36109, V, 1, 1, 1, 1, 0, 704, 100
36110, V, 1, 1, 1, 1, 0, 704, 100
36111, V, 1, 1, 1, 1, 0, 704, 100
36112, V, 1, 1, 1, 1, 0, 704, 100
36113, V, 1, 1, 1, 1, 0, 704, 100
36114, V, 1, 1, 1, 1, 0, 704, 100
36115, V, 1, 1, 1, 1, 0, 704, 100
36116, V, 1, 1, 1, 1, 0, 704, 100
36117, V, 1, 1, 1, 1, 0, 704, 100
36118, V, 1, 1, 1, 1, 0, 704, 100
36119, V, 1, 1, 1, 1, 0, 704, 100
36120, V, 1, 1, 1, 1, 0, 704, 100
36121, V, 1, 1, 1, 1, 0, 704, 100
36122, V, 1, 1, 1, 1, 0, 704, 100
36123, V, 1, 1, 1, 1, 0, 704, 100
36124, V, 1, 1, 1, 1, 0, 704, 100
36125, V, 1, 1, 1, 1, 0, 704, 100
36126, V, 1, 1, 1, 1, 0, 704, 100
36127, V, 1, 1, 1, 1, 0, 704, 100
36128, V, 1, 1, 1, 1, 0, 704, 100
36129, V, 1, 1, 1, 1, 0, 704, 100
36130, V, 1, 1, 1, 1, 0, 704, 100
36131, V, 1, 1, 1, 1, 0, 704, 100
36132, V, 1, 1, 1, 1, 0, 704, 100
36133, V, 1, 1, 1, 1, 0, 704, 100
36134, V, 1, 1, 1, 1, 0, 704, 100
36135, V, 1, 1, 1, 1, 0, 704, 100
36136, V, 1, 1, 1, 1, 0, 704, 100
36137, V, 1, 1, 1, 1, 0, 704, 100
36139, V, 1, 1, 1, 1, 0, 704, 100
36140, V, 1, 1, 1, 1, 0, 704, 100
36141, V, 1, 1, 1, 1, 0, 704, 100
36142, V, 1, 1, 1, 1, 0, 704, 100
36143, V, 1, 1, 1, 1, 0, 704, 100
36144, V, 1, 1, 1, 1, 0, 704, 100
36145, V, 1, 1, 1, 1, 0, 704, 100
36146, V, 1, 1, 1, 1, 0, 704, 100
36147, V, 1, 1, 1, 1, 0, 704, 100
36148, V, 1, 1, 1, 1, 0, 704, 100
36149, V, 1, 1, 1, 1, 0, 704, 100
36150, V, 1, 1, 1, 1, 0, 704, 100
36151, V, 1, 1, 1, 1, 0, 704, 100
36152, V, 1, 1, 1, 1, 0, 704, 100
36153, V, 1, 1, 1, 1, 0, 704, 100
36154, V, 1, 1, 1, 1, 0, 704, 100
36155, V, 1, 1, 1, 1, 0, 704, 100
36156, V, 1, 1, 1, 1, 0, 704, 100
36157, V, 1, 1, 1, 1, 0, 704, 100
36158, V, 1, 1, 1, 1, 0, 704, 100
36159, V, 1, 1, 1, 1, 0, 704, 100
36160, V, 1, 1, 1, 1, 0, 704, 100
36161, V, 1, 1, 1, 1, 0, 704, 100
36162, V, 1, 1, 1, 1, 0, 704, 100
36163, V, 1, 1, 1, 1, 0, 704, 100
36164, V, 1, 1, 1, 1, 0, 704, 100
36165, V, 1, 1, 1, 1, 0, 704, 100
36166, V, 1, 1, 1, 1, 0, 704, 100
36167, V, 1, 1, 1, 1, 0, 704, 100
36168, V, 1, 1, 1, 1, 0, 704, 100
36169, V, 1, 1, 1, 1, 0, 704, 100
36170, V, 1, 1, 1, 1, 0, 704, 100
36171, V, 1, 1, 1, 1, 0, 704, 100
36172, V, 1, 1, 1, 1, 0, 704, 100
36173, V, 1, 1, 1, 1, 0, 704, 100
36174, V, 1, 1, 1, 1, 0, 704, 100
36175, V, 1, 1, 1, 1, 0, 704, 100
36176, V, 1, 1, 1, 1, 0, 704, 100
36177, V, 1, 1, 1, 1, 0, 704, 100
36178, V, 1, 1, 1, 1, 0, 704, 100
36179, V, 1, 1, 1, 1, 0, 704, 100
36180, V, 1, 1, 1, 1, 0, 704, 100
36182, V, 1, 1, 1, 1, 0, 704, 100
36183, V, 1, 1, 1, 1, 0, 704, 100
36184, V, 1, 1, 1, 1, 0, 704, 100
36185, V, 1, 1, 1, 1, 0, 704, 100
36186, V, 1, 1, 1, 1, 0, 704, 100
36187, V, 1, 1, 1, 1, 0, 704, 100
36188, V, 1, 1, 1, 1, 0, 704, 100
36189, V, 1, 1, 1, 1, 0, 704, 100
36190, V, 1, 1, 1, 1, 0, 704, 100
36191, V, 1, 1, 1, 1, 0, 704, 100
36192, V, 1, 1, 1, 1, 0, 704, 100
36193, V, 1, 1, 1, 1, 0, 704, 100
36194, V, 1, 1, 1, 1, 0, 704, 100
36195, V, 1, 1, 1, 1, 0, 704, 100
36196, V, 1, 1, 1, 1, 0, 704, 100
36197, V, 1, 1, 1, 1, 0, 704, 100
36198, V, 1, 1, 1, 1, 0, 704, 100
36199, V, 1, 1, 1, 1, 0, 704, 100
36200, V, 1, 1, 1, 1, 0, 704, 100
36201, V, 1, 1, 1, 1, 0, 704, 100
36202, V, 1, 1, 1, 1, 0, 704, 100
36203, V, 1, 1, 1, 1, 0, 704, 100
36204, V, 1, 1, 1, 1, 0, 704, 100
36205, V, 1, 1, 1, 1, 0, 704, 100
36206, V, 1, 1, 1, 1, 0, 704, 100
36207, V, 1, 1, 1, 1, 0, 704, 100
36208, V, 1, 1, 1, 1, 0, 704, 100
36209, V, 1, 1, 1, 1, 0, 704, 100
36210, V, 1, 1, 1, 1, 0, 704, 100
36211, V, 1, 1, 1, 1, 0, 704, 100
36212, V, 1, 1, 1, 1, 0, 704, 100
36213, V, 1, 1, 1, 1, 0, 704, 100
36214, V, 1, 1, 1, 1, 0, 704, 100
36215, V, 1, 1, 1, 1, 0, 704, 100
36216, V, 1, 1, 1, 1, 0, 704, 100
36217, V, 1, 1, 1, 1, 0, 704, 100
36218, V, 1, 1, 1, 1, 0, 704, 100
36219, V, 1, 1, 1, 1, 0, 704, 100
36220, V, 1, 1, 1, 1, 0, 704, 100
36221, V, 1, 1, 1, 1, 0, 704, 100
36222, V, 1, 1, 1, 1, 0, 704, 100
36224, V, 1, 1, 1, 1, 0, 704, 100
36225, V, 1, 1, 1, 1, 0, 704, 100
36226, V, 1, 1, 1, 1, 0, 704, 100
36227, V, 1, 1, 1, 1, 0, 704, 100
36228, V, 1, 1, 1, 1, 0, 704, 100
36229, V, 1, 1, 1, 1, 0, 704, 100
36230, V, 1, 1, 1, 1, 0, 704, 100
36231, V, 1, 1, 1, 1, 0, 704, 100
36232, V, 1, 1, 1, 1, 0, 704, 100
36233, V, 1, 1, 1, 1, 0, 704, 100
36234, V, 1, 1, 1, 1, 0, 704, 100
36235, V, 1, 1, 1, 1, 0, 704, 100
36236, V, 1, 1, 1, 1, 0, 704, 100
36237, V, 1, 1, 1, 1, 0, 704, 100
36238, V, 1, 1, 1, 1, 0, 704, 100
36239, V, 1, 1, 1, 1, 0, 704, 100
36240, V, 1, 1, 1, 1, 0, 704, 100
36241, V, 1, 1, 1, 1, 0, 704, 100
36242, V, 1, 1, 1, 1, 0, 704, 100
36243, V, 1, 1, 1, 1, 0, 704, 100
36244, V, 1, 1, 1, 1, 0, 704, 100
36245, V, 1, 1, 1, 1, 0, 704, 100
36246, V, 1, 1, 1, 1, 0, 704, 100
36247, V, 1, 1, 1, 1, 0, 704, 100
36248, V, 1, 1, 1, 1, 0, 704, 100
36249, V, 1, 1, 1, 1, 0, 704, 100
36250, V, 1, 1, 1, 1, 0, 704, 100
36251, V, 1, 1, 1, 1, 0, 704, 100
36252, V, 1, 1, 1, 1, 0, 704, 100
36253, V, 1, 1, 1, 1, 0, 704, 100
36254, V, 1, 1, 1, 1, 0, 704, 100
36255, V, 1, 1, 1, 1, 0, 704, 100
36256, V, 1, 1, 1, 1, 0, 704, 100
36257, V, 1, 1, 1, 1, 0, 704, 100
36258, V, 1, 1, 1, 1, 0, 704, 100
36259, V, 1, 1, 1, 1, 0, 704, 100
36260, V, 1, 1, 1, 1, 0, 704, 100
36261, V, 1, 1, 1, 1, 0, 704, 100
36262, V, 1, 1, 1, 1, 0, 704, 100
36263, V, 1, 1, 1, 1, 0, 704, 100
36264, V, 1, 1, 1, 1, 0, 704, 100
36265, V, 1, 1, 1, 1, 0, 704, 100
36267, V, 1, 1, 1, 1, 0, 704, 100
36268, V, 1, 1, 1, 1, 0, 704, 100
36269, V, 1, 1, 1, 1, 0, 704, 100
36270, V, 1, 1, 1, 1, 0, 704, 100
36271, V, 1, 1, 1, 1, 0, 704, 100
36272, V, 1, 1, 1, 1, 0, 704, 100
36273, V, 1, 1, 1, 1, 0, 704, 100
36274, V, 1, 1, 1, 1, 0, 704, 100
36275, V, 1, 1, 1, 1, 0, 704, 100
36276, V, 1, 1, 1, 1, 0, 704, 100
36277, V, 1, 1, 1, 1, 0, 704, 100
36278, V, 1, 1, 1, 1, 0, 704, 100
36279, V, 1, 1, 1, 1, 0, 704, 100
36280, V, 1, 1, 1, 1, 0, 704, 100
36281, V, 1, 1, 1, 1, 0, 704, 100
36282, V, 1, 1, 1, 1, 0, 704, 100
36283, V, 1, 1, 1, 1, 0, 704, 100
36284, V, 1, 1, 1, 1, 0, 704, 100
36285, V, 1, 1, 1, 1, 0, 704, 100
36286, V, 1, 1, 1, 1, 0, 704, 100
36287, V, 1, 1, 1, 1, 0, 704, 100
36288, V, 1, 1, 1, 1, 0, 704, 100
36289, V, 1, 1, 1, 1, 0, 704, 100
36290, V, 1, 1, 1, 1, 0, 704, 100
36291, V, 1, 1, 1, 1, 0, 704, 100
36292, V, 1, 1, 1, 1, 0, 704, 100
36293, V, 1, 1, 1, 1, 0, 704, 100
36294, V, 1, 1, 1, 1, 0, 704, 100
36295, V, 1, 1, 1, 1, 0, 704, 100
36296, V, 1, 1, 1, 1, 0, 704, 100
36297, V, 1, 1, 1, 1, 0, 704, 100
36298, V, 1, 1, 1, 1, 0, 704, 100
36299, V, 1, 1, 1, 1, 0, 704, 100
36300, V, 1, 1, 1, 1, 0, 704, 100
36301, V, 1, 1, 1, 1, 0, 704, 100
36302, V, 1, 1, 1, 1, 0, 704, 100
36303, V, 1, 1, 1, 1, 0, 704, 100
36304, V, 1, 1, 1, 1, 0, 704, 100
36305, V, 1, 1, 1, 1, 0, 704, 100
36306, V, 1, 1, 1, 1, 0, 704, 100
36307, V, 1, 1, 1, 1, 0, 704, 100
36308, V, 1, 1, 1, 1, 0, 704, 100
36310, V, 1, 1, 1, 1, 0, 704, 100
36311, V, 1, 1, 1, 1, 0, 704, 100
36312, V, 1, 1, 1, 1, 0, 704, 100
36313, V, 1, 1, 1, 1, 0, 704, 100
36314, V, 1, 1, 1, 1, 0, 704, 100
36315, V, 1, 1, 1, 1, 0, 704, 100
36316, V, 1, 1, 1, 1, 0, 704, 100
36317, V, 1, 1, 1, 1, 0, 704, 100
36318, V, 1, 1, 1, 1, 0, 704, 100
36319, V, 1, 1, 1, 1, 0, 704, 100
36320, V, 1, 1, 1, 1, 0, 704, 100
36321, V, 1, 1, 1, 1, 0, 704, 100
36322, V, 1, 1, 1, 1, 0, 704, 100
36323, V, 1, 1, 1, 1, 0, 704, 100
36324, V, 1, 1, 1, 1, 0, 704, 100
36325, V, 1, 1, 1, 1, 0, 704, 100
36326, V, 1, 1, 1, 1, 0, 704, 100
36327, V, 1, 1, 1, 1, 0, 704, 100
36328, V, 1, 1, 1, 1, 0, 704, 100
36329, V, 1, 1, 1, 1, 0, 704, 100
36330, V, 1, 1, 1, 1, 0, 704, 100
36331, V, 1, 1, 1, 1, 0, 704, 100
36332, V, 1, 1, 1, 1, 0, 704, 100
36333, V, 1, 1, 1, 1, 0, 704, 100
36334, V, 1, 1, 1, 1, 0, 704, 100
36335, V, 1, 1, 1, 1, 0, 704, 100
36336, V, 1, 1, 1, 1, 0, 704, 100
36337, V, 1, 1, 1, 1, 0, 704, 100
36338, V, 1, 1, 1, 1, 0, 704, 100
36339, V, 1, 1, 1, 1, 0, 704, 100
36340, V, 1, 1, 1, 1, 0, 704, 100
36341, V, 1, 1, 1, 1, 0, 704, 100
36342, V, 1, 1, 1, 1, 0, 704, 100
36343, V, 1, 1, 1, 1, 0, 704, 100
36344, V, 1, 1, 1, 1, 0, 704, 100
36345, V, 1, 1, 1, 1, 0, 704, 100
36346, V, 1, 1, 1, 1, 0, 704, 100
36347, V, 1, 1, 1, 1, 0, 704, 100
36348, V, 1, 1, 1, 1, 0, 704, 100
36349, V, 1, 1, 1, 1, 0, 704, 100
36350, V, 1, 1, 1, 1, 0, 704, 100
36352, V, 1, 1, 1, 1, 0, 704, 100
36353, V, 1, 1, 1, 1, 0, 704, 100
36354, V, 1, 1, 1, 1, 0, 704, 100
36355, V, 1, 1, 1, 1, 0, 704, 100
36356, V, 1, 1, 1, 1, 0, 704, 100
36357, V, 1, 1, 1, 1, 0, 704, 100
36358, V, 1, 1, 1, 1, 0, 704, 100
36359, V, 1, 1, 1, 1, 0, 704, 100
36360, V, 1, 1, 1, 1, 0, 704, 100
36361, V, 1, 1, 1, 1, 0, 704, 100
36362, V, 1, 1, 1, 1, 0, 704, 100
36363, V, 1, 1, 1, 1, 0, 704, 100
36364, V, 1, 1, 1, 1, 0, 704, 100
36365, V, 1, 1, 1, 1, 0, 704, 100
36366, V, 1, 1, 1, 1, 0, 704, 100
36367, V, 1, 1, 1, 1, 0, 704, 100
36368, V, 1, 1, 1, 1, 0, 704, 100
36369, V, 1, 1, 1, 1, 0, 704, 100
36370, V, 1, 1, 1, 1, 0, 704, 100
36371, V, 1, 1, 1, 1, 0, 704, 100
36372, V, 1, 1, 1, 1, 0, 704, 100
36373, V, 1, 1, 1, 1, 0, 704, 100
36374, V, 1, 1, 1, 1, 0, 704, 100
36375, V, 1, 1, 1, 1, 0, 704, 100
36376, V, 1, 1, 1, 1, 0, 704, 100
36377, V, 1, 1, 1, 1, 0, 704, 100
36378, V, 1, 1, 1, 1, 0, 704, 100
36379, V, 1, 1, 1, 1, 0, 704, 100
36380, V, 1, 1, 1, 1, 0, 704, 100
36381, V, 1, 1, 1, 1, 0, 704, 100
36382, V, 1, 1, 1, 1, 0, 704, 100
36383, V, 1, 1, 1, 1, 0, 704, 100
36384, V, 1, 1, 1, 1, 0, 704, 100
36385, V, 1, 1, 1, 1, 0, 704, 100
36386, V, 1, 1, 1, 1, 0, 704, 100
36387, V, 1, 1, 1, 1, 0, 704, 100
36388, V, 1, 1, 1, 1, 0, 704, 100
36389, V, 1, 1, 1, 1, 0, 704, 100
36390, V, 1, 1, 1, 1, 0, 704, 100
36391, V, 1, 1, 1, 1, 0, 704, 100
36392, V, 1, 1, 1, 1, 0, 704, 100
36393, V, 1, 1, 1, 1, 0, 704, 100
36395, V, 1, 1, 1, 1, 0, 704, 100
36396, V, 1, 1, 1, 1, 0, 704, 100
36397, V, 1, 1, 1, 1, 0, 704, 100
36398, V, 1, 1, 1, 1, 0, 704, 100
36399, V, 1, 1, 1, 1, 0, 704, 100
36400, V, 1, 1, 1, 1, 0, 704, 100
36401, V, 1, 1, 1, 1, 0, 704, 100
36402, V, 1, 1, 1, 1, 0, 704, 100
36403, V, 1, 1, 1, 1, 0, 704, 100
36404, V, 1, 1, 1, 1, 0, 704, 100
36405, V, 1, 1, 1, 1, 0, 704, 100
36406, V, 1, 1, 1, 1, 0, 704, 100
36407, V, 1, 1, 1, 1, 0, 704, 100
36408, V, 1, 1, 1, 1, 0, 704, 100
36409, V, 1, 1, 1, 1, 0, 704, 100
36410, V, 1, 1, 1, 1, 0, 704, 100
36411, V, 1, 1, 1, 1, 0, 704, 100
36412, V, 1, 1, 1, 1, 0, 704, 100
36413, V, 1, 1, 1, 1, 0, 704, 100
36414, V, 1, 1, 1, 1, 0, 704, 100
36415, V, 1, 1, 1, 1, 0, 704, 100
36416, V, 1, 1, 1, 1, 0, 704, 100
36417, V, 1, 1, 1, 1, 0, 704, 100
36418, V, 1, 1, 1, 1, 0, 704, 100
36419, V, 1, 1, 1, 1, 0, 704, 100
36420, V, 1, 1, 1, 1, 0, 704, 100
36421, V, 1, 1, 1, 1, 0, 704, 100
36422, V, 1, 1, 1, 1, 0, 704, 100
36423, V, 1, 1, 1, 1, 0, 704, 100
36424, V, 1, 1, 1, 1, 0, 704, 100
36425, V, 1, 1, 1, 1, 0, 704, 100
36426, V, 1, 1, 1, 1, 0, 704, 100
36427, V, 1, 1, 1, 1, 0, 704, 100
36428, V, 1, 1, 1, 1, 0, 704, 100
36429, V, 1, 1, 1, 1, 0, 704, 100
36430, V, 1, 1, 1, 1, 0, 704, 100
36431, V, 1, 1, 1, 1, 0, 704, 100
36432, V, 1, 1, 1, 1, 0, 704, 100
36433, V, 1, 1, 1, 1, 0, 704, 100
36434, V, 1, 1, 1, 1, 0, 704, 100
36435, V, 1, 1, 1, 1, 0, 704, 100
36436, V, 1, 1, 1, 1, 0, 704, 100
36438, V, 1, 1, 1, 1, 0, 704, 100
36439, V, 1, 1, 1, 1, 0, 704, 100
36440, V, 1, 1, 1, 1, 0, 704, 100
36441, V, 1, 1, 1, 1, 0, 704, 100
36442, V, 1, 1, 1, 1, 0, 704, 100
36443, V, 1, 1, 1, 1, 0, 704, 100
36444, V, 1, 1, 1, 1, 0, 704, 100
36445, V, 1, 1, 1, 1, 0, 704, 100
36446, V, 1, 1, 1, 1, 0, 704, 100
36447, V, 1, 1, 1, 1, 0, 704, 100
36448, V, 1, 1, 1, 1, 0, 704, 100
36449, V, 1, 1, 1, 1, 0, 704, 100
36450, V, 1, 1, 1, 1, 0, 704, 100
36451, V, 1, 1, 1, 1, 0, 704, 100
36452, V, 1, 1, 1, 1, 0, 704, 100
36453, V, 1, 1, 1, 1, 0, 704, 100
36454, V, 1, 1, 1, 1, 0, 704, 100
36455, V, 1, 1, 1, 1, 0, 704, 100
36456, V, 1, 1, 1, 1, 0, 704, 100
36457, V, 1, 1, 1, 1, 0, 704, 100
36458, V, 1, 1, 1, 1, 0, 704, 100
36459, V, 1, 1, 1, 1, 0, 704, 100
36460, V, 1, 1, 1, 1, 0, 704, 100
36461, V, 1, 1, 1, 1, 0, 704, 100
36462, V, 1, 1, 1, 1, 0, 704, 100
36463, V, 1, 1, 1, 1, 0, 704, 100
36464, V, 1, 1, 1, 1, 0, 704, 100
36465, V, 1, 1, 1, 1, 0, 704, 100
36466, V, 1, 1, 1, 1, 0, 704, 100
36467, V, 1, 1, 1, 1, 0, 704, 100
36468, V, 1, 1, 1, 1, 0, 704, 100
36469, V, 1, 1, 1, 1, 0, 704, 100
36470, V, 1, 1, 1, 1, 0, 704, 100
36471, V, 1, 1, 1, 1, 0, 704, 100
36472, V, 1, 1, 1, 1, 0, 704, 100
36473, V, 1, 1, 1, 1, 0, 704, 100
36474, V, 1, 1, 1, 1, 0, 704, 100
36475, V, 1, 1, 1, 1, 0, 704, 100
36476, V, 1, 1, 1, 1, 0, 704, 100
36477, V, 1, 1, 1, 1, 0, 704, 100
36478, V, 1, 1, 1, 1, 0, 704, 100
36480, V, 1, 1, 1, 1, 0, 704, 100
36481, V, 1, 1, 1, 1, 0, 704, 100
36482, V, 1, 1, 1, 1, 0, 704, 100
36483, V, 1, 1, 1, 1, 0, 704, 100
36484, V, 1, 1, 1, 1, 0, 704, 100
36485, V, 1, 1, 1, 1, 0, 704, 100
36486, V, 1, 1, 1, 1, 0, 704, 100
36487, V, 1, 1, 1, 1, 0, 704, 100
36488, V, 1, 1, 1, 1, 0, 704, 100
36489, V, 1, 1, 1, 1, 0, 704, 100
36490, V, 1, 1, 1, 1, 0, 704, 100
36491, V, 1, 1, 1, 1, 0, 704, 100
36492, V, 1, 1, 1, 1, 0, 704, 100
36493, V, 1, 1, 1, 1, 0, 704, 100
36494, V, 1, 1, 1, 1, 0, 704, 100
36495, V, 1, 1, 1, 1, 0, 704, 100
36496, V, 1, 1, 1, 1, 0, 704, 100
36497, V, 1, 1, 1, 1, 0, 704, 100
36498, V, 1, 1, 1, 1, 0, 704, 100
36499, V, 1, 1, 1, 1, 0, 704, 100
36500, V, 1, 1, 1, 1, 0, 704, 100
36501, V, 1, 1, 1, 1, 0, 704, 100
36502, V, 1, 1, 1, 1, 0, 704, 100
36503, V, 1, 1, 1, 1, 0, 704, 100
36504, V, 1, 1, 1, 1, 0, 704, 100
36505, V, 1, 1, 1, 1, 0, 704, 100
36506, V, 1, 1, 1, 1, 0, 704, 100
36507, V, 1, 1, 1, 1, 0, 704, 100
36508, V, 1, 1, 1, 1, 0, 704, 100
36509, V, 1, 1, 1, 1, 0, 704, 100
36510, V, 1, 1, 1, 1, 0, 704, 100
36511, V, 1, 1, 1, 1, 0, 704, 100
36512, V, 1, 1, 1, 1, 0, 704, 100
36513, V, 1, 1, 1, 1, 0, 704, 100
36514, V, 1, 1, 1, 1, 0, 704, 100
36515, V, 1, 1, 1, 1, 0, 704, 100
36516, V, 1, 1, 1, 1, 0, 704, 100
36517, V, 1, 1, 1, 1, 0, 704, 100
36518, V, 1, 1, 1, 1, 0, 704, 100
36519, V, 1, 1, 1, 1, 0, 704, 100
36520, V, 1, 1, 1, 1, 0, 704, 100
36521, V, 1, 1, 1, 1, 0, 704, 100
36523, V, 1, 1, 1, 1, 0, 704, 100
36524, V, 1, 1, 1, 1, 0, 704, 100
36525, V, 1, 1, 1, 1, 0, 704, 100
36526, V, 1, 1, 1, 1, 0, 704, 100
36527, V, 1, 1, 1, 1, 0, 704, 100
36528, V, 1, 1, 1, 1, 0, 704, 100
36529, V, 1, 1, 1, 1, 0, 704, 100
36530, V, 1, 1, 1, 1, 0, 704, 100
36531, V, 1, 1, 1, 1, 0, 704, 100
36532, V, 1, 1, 1, 1, 0, 704, 100
36533, V, 1, 1, 1, 1, 0, 704, 100
36534, V, 1, 1, 1, 1, 0, 704, 100
36535, V, 1, 1, 1, 1, 0, 704, 100
36536, V, 1, 1, 1, 1, 0, 704, 100
36537, V, 1, 0, 0, 1, 0, 704, 100
36537, V, 1, 0, 0, 0, 0, 704, 100
36538, V, 1, 1, 0, 0, 0, 704, 100
36538, V, 1, 1, 0, 0, 0, 704, 100
36539, V, 1, 1, 1, 1, 0, 704, 100
36540, V, 1, 1, 1, 1, 0, 704, 100
36541, V, 1, 1, 1, 1, 0, 704, 100
36542, V, 1, 1, 1, 1, 0, 704, 99
36543, V, 1, 1, 1, 1, 0, 704, 99
36544, V, 1, 1, 1, 1, 0, 704, 99
36545, V, 1, 1, 1, 1, 0, 704, 99
36546, V, 1, 1, 1, 1, 0, 704, 99
36547, V, 1, 1, 1, 1, 0, 704, 99
36548, V, 1, 1, 1, 1, 0, 704, 99
36549, V, 1, 1, 1, 1, 0, 704, 99
36550, V, 1, 1, 1, 1, 0, 704, 99
36551, V, 1, 1, 1, 1, 0, 704, 99
36552, V, 1, 1, 1, 1, 0, 704, 99
36553, V, 1, 1, 1, 1, 0, 704, 99
36554, V, 1, 1, 1, 1, 0, 704, 99
36555, V, 1, 1, 1, 1, 0, 704, 99
36556, V, 1, 1, 1, 1, 0, 704, 99
36557, V, 1, 1, 1, 1, 0, 704, 99
36558, V, 1, 1, 1, 1, 0, 704, 99
36559, V, 1, 1, 1, 1, 0, 704, 99
36560, V, 1, 1, 1, 1, 0, 704, 99
36561, V, 1, 1, 1, 1, 0, 704, 99
36562, V, 1, 1, 1, 1, 0, 704, 99
36563, V, 1, 1, 1, 1, 0, 704, 99
36564, V, 1, 1, 1, 1, 0, 704, 99
36566, V, 1, 1, 1, 1, 0, 704, 99
36567, V, 1, 1, 1, 1, 0, 704, 99
36568, V, 1, 1, 1, 1, 0, 704, 99
36569, V, 1, 1, 1, 1, 0, 704, 99
36570, V, 1, 1, 1, 1, 0, 704, 99
36571, V, 1, 1, 1, 1, 0, 704, 99
36572, V, 1, 1, 1, 1, 0, 704, 99
36573, V, 1, 1, 1, 1, 0, 704, 99
36574, V, 1, 1, 1, 1, 0, 704, 99
36575, V, 1, 1, 1, 1, 0, 704, 99
36576, V, 1, 1, 1, 1, 0, 704, 99
36577, V, 1, 1, 1, 1, 0, 704, 99
36578, V, 1, 1, 1, 1, 0, 704, 100
36579, V, 1, 1, 1, 1, 0, 704, 99
36580, V, 1, 1, 1, 1, 0, 704, 99
36581, V, 1, 1, 1, 1, 0, 704, 99
36582, V, 1, 1, 1, 1, 0, 704, 100
36583, V, 1, 1, 1, 1, 0, 704, 99
36584, V, 1, 1, 1, 1, 0, 704, 100
36585, V, 1, 1, 1, 1, 0, 704, 99
36586, V, 1, 1, 1, 1, 0, 704, 100
36587, V, 1, 1, 1, 1, 0, 704, 100
36588, V, 1, 1, 1, 1, 0, 704, 100
36589, V, 1, 1, 1, 1, 0, 704, 100
36590, V, 1, 1, 1, 1, 0, 704, 100
36591, V, 1, 1, 1, 1, 0, 704, 100
36592, V, 1, 1, 1, 1, 0, 704, 100
36593, V, 1, 1, 1, 1, 0, 704, 100
36594, V, 1, 1, 1, 1, 0, 704, 100
36595, V, 1, 1, 1, 1, 0, 704, 100
36596, V, 1, 1, 1, 1, 0, 704, 100
36597, V, 1, 1, 1, 1, 0, 704, 100
36598, V, 1, 1, 1, 1, 0, 704, 100
36599, V, 1, 1, 1, 1, 0, 704, 100
36600, V, 1, 1, 1, 1, 0, 704, 100
36601, V, 1, 1, 1, 1, 0, 704, 100
36602, V, 1, 1, 1, 1, 0, 704, 100
36603, V, 1, 1, 1, 1, 0, 704, 100
36604, V, 1, 1, 1, 1, 0, 704, 100
36605, V, 1, 1, 1, 1, 0, 704, 100
36606, V, 1, 1, 1, 1, 0, 704, 100
36608, V, 1, 1, 1, 1, 0, 704, 100
36609, V, 1, 1, 1, 1, 0, 704, 100
36610, V, 1, 1, 1, 1, 0, 704, 100
36611, V, 1, 1, 1, 1, 0, 704, 100
36612, V, 1, 1, 1, 1, 0, 704, 100
36613, V, 1, 1, 1, 1, 0, 704, 100
36614, V, 1, 1, 1, 1, 0, 704, 100
36615, V, 1, 1, 1, 1, 0, 704, 100
36616, V, 1, 1, 1, 1, 0, 704, 100
36617, V, 1, 1, 1, 1, 0, 704, 100
36618, V, 1, 1, 1, 1, 0, 704, 100
36619, V, 1, 1, 1, 1, 0, 704, 100
36620, V, 1, 1, 1, 1, 0, 704, 100
36621, V, 1, 1, 1, 1, 0, 704, 100
36622, V, 1, 1, 1, 1, 0, 704, 100
36623, V, 1, 1, 1, 1, 0, 704, 100
36624, V, 1, 1, 1, 1, 0, 704, 100
36625, V, 1, 1, 1, 1, 0, 704, 100
36626, V, 1, 1, 1, 1, 0, 704, 100
36627, V, 1, 1, 1, 1, 0, 704, 100
36628, V, 1, 1, 1, 1, 0, 704, 99
36629, V, 1, 1, 1, 1, 0, 704, 100
36630, V, 1, 1, 1, 1, 0, 704, 100
36631, V, 1, 1, 1, 1, 0, 704, 100
36632, V, 1, 1, 1, 1, 0, 704, 100
36633, V, 1, 1, 1, 1, 0, 704, 100
36634, V, 1, 1, 1, 1, 0, 704, 100
36635, V, 1, 1, 1, 1, 0, 704, 100
36636, V, 1, 1, 1, 1, 0, 704, 100
36637, V, 1, 1, 1, 1, 0, 704, 100
36638, V, 1, 1, 1, 1, 0, 704, 100
36639, V, 1, 1, 1, 1, 0, 704, 100
36640, V, 1, 1, 1, 1, 0, 704, 100
36641, V, 1, 1, 1, 1, 0, 704, 100
36642, V, 1, 1, 1, 1, 0, 704, 100
36643, V, 1, 1, 1, 1, 0, 704, 100
36644, V, 1, 1, 1, 1, 0, 704, 100
36645, V, 1, 1, 1, 1, 0, 704, 100
36646, V, 1, 1, 1, 1, 0, 704, 100
36647, V, 1, 1, 1, 1, 0, 704, 100
36648, V, 1, 1, 1, 1, 0, 704, 100
36649, V, 1, 1, 1, 1, 0, 704, 100
36651, V, 1, 1, 1, 1, 0, 704, 100
36652, V, 1, 1, 1, 1, 0, 704, 100
36653, V, 1, 1, 1, 1, 0, 704, 100
36654, V, 1, 1, 1, 1, 0, 704, 100
36655, V, 1, 1, 1, 1, 0, 704, 100
36656, V, 1, 1, 1, 1, 0, 704, 100
36657, V, 1, 1, 1, 1, 0, 704, 100
36658, V, 1, 1, 1, 1, 0, 704, 100
36659, V, 1, 1, 1, 1, 0, 704, 100
36660, V, 1, 1, 1, 1, 0, 704, 100
36661, V, 1, 1, 1, 1, 0, 704, 100
36662, V, 1, 1, 1, 1, 0, 704, 100
36663, V, 1, 1, 1, 1, 0, 704, 100
36664, V, 1, 1, 1, 1, 0, 704, 100
36665, V, 1, 1, 1, 1, 0, 704, 100
36666, V, 1, 1, 1, 1, 0, 704, 100
36667, V, 1, 1, 1, 1, 0, 704, 100
36668, V, 1, 1, 1, 1, 0, 704, 100
36669, V, 1, 1, 1, 1, 0, 704, 100
36670, V, 1, 1, 1, 1, 0, 704, 100
36671, V, 1, 1, 1, 1, 0, 704, 100
36672, V, 1, 1, 1, 1, 0, 704, 100
36673, V, 1, 1, 1, 1, 0, 704, 100
36674, V, 1, 1, 1, 1, 0, 704, 100
36675, V, 1, 1, 1, 1, 0, 704, 100
36676, V, 1, 1, 1, 1, 0, 704, 100
36677, V, 1, 1, 1, 1, 0, 704, 100
36678, V, 1, 1, 1, 1, 0, 704, 100
36679, V, 1, 1, 1, 1, 0, 704, 100
36680, V, 1, 1, 1, 1, 0, 704, 100
36681, V, 1, 1, 1, 1, 0, 704, 100
36682, V, 1, 1, 1, 1, 0, 704, 100
36683, V, 1, 1, 1, 1, 0, 704, 100
36684, V, 1, 1, 1, 1, 0, 704, 100
36685, V, 1, 1, 1, 1, 0, 704, 100
36686, V, 1, 1, 1, 1, 0, 704, 100
36687, V, 1, 1, 1, 1, 0, 704, 100
36688, V, 1, 1, 1, 1, 0, 704, 100
36689, V, 1, 1, 1, 1, 0, 704, 100
36690, V, 1, 1, 1, 1, 0, 704, 100
36691, V, 1, 1, 1, 1, 0, 704, 100
36692, V, 1, 1, 1, 1, 0, 704, 100
36694, V, 1, 1, 1, 1, 0, 704, 100
36695, V, 1, 1, 1, 1, 0, 704, 100
36696, V, 1, 1, 1, 1, 0, 704, 100
36697, V, 1, 1, 1, 1, 0, 704, 100
36698, V, 1, 1, 1, 1, 0, 704, 100
36699, V, 1, 1, 1, 1, 0, 704, 100
36700, V, 1, 1, 1, 1, 0, 704, 100
36701, V, 1, 1, 1, 1, 0, 704, 100
36702, V, 1, 1, 1, 1, 0, 704, 100
36703, V, 1, 1, 1, 1, 0, 704, 100
36704, V, 1, 1, 1, 1, 0, 704, 100
36705, V, 1, 1, 1, 1, 0, 704, 100
36706, V, 1, 1, 1, 1, 0, 704, 100
36707, V, 1, 1, 1, 1, 0, 704, 100
36708, V, 1, 1, 1, 1, 0, 704, 100
36709, V, 1, 1, 1, 1, 0, 704, 100
36710, V, 1, 1, 1, 1, 0, 704, 100
36711, V, 1, 1, 1, 1, 0, 704, 100
36712, V, 1, 1, 1, 1, 0, 704, 100
36713, V, 1, 1, 1, 1, 0, 704, 100
36714, V, 1, 1, 1, 1, 0, 704, 100
36715, V, 1, 1, 1, 1, 0, 704, 100
36716, V, 1, 1, 1, 1, 0, 704, 100
36717, V, 1, 1, 1, 1, 0, 704, 100
36718, V, 1, 1, 1, 1, 0, 704, 100
36719, V, 1, 1, 1, 1, 0, 704, 100
36720, V, 1, 1, 1, 1, 0, 704, 100
36721, V, 1, 1, 1, 1, 0, 704, 100
36722, V, 1, 1, 1, 1, 0, 704, 100
36723, V, 1, 1, 1, 1, 0, 704, 100
36724, V, 1, 1, 1, 1, 0, 704, 100
36725, V, 1, 1, 1, 1, 0, 704, 100
36726, V, 1, 1, 1, 1, 0, 704, 100
36727, V, 1, 1, 1, 1, 0, 704, 100
36728, V, 1, 1, 1, 1, 0, 704, 100
36729, V, 1, 1, 1, 1, 0, 704, 100
36730, V, 1, 1, 1, 1, 0, 704, 100
36731, V, 1, 1, 1, 1, 0, 704, 100
36732, V, 1, 1, 1, 1, 0, 704, 100
36733, V, 1, 1, 1, 1, 0, 704, 100
36734, V, 1, 1, 1, 1, 0, 704, 100
36736, V, 1, 1, 1, 1, 0, 704, 100
36737, V, 1, 1, 1, 1, 0, 704, 100
36738, V, 1, 1, 1, 1, 0, 704, 100
36739, V, 1, 1, 1, 1, 0, 704, 100
36740, V, 1, 1, 1, 1, 0, 704, 100
36741, V, 1, 1, 1, 1, 0, 704, 100
36742, V, 1, 1, 1, 1, 0, 704, 100
36743, V, 1, 1, 1, 1, 0, 704, 100
36744, V, 1, 1, 1, 1, 0, 704, 100
36745, V, 1, 1, 1, 1, 0, 704, 100
36746, V, 1, 1, 1, 1, 0, 704, 100
36747, V, 1, 1, 1, 1, 0, 704, 100
36748, V, 1, 1, 1, 1, 0, 704, 100
36749, V, 1, 1, 1, 1, 0, 704, 100
36750, V, 1, 1, 1, 1, 0, 704, 100
36751, V, 1, 1, 1, 1, 0, 704, 100
36752, V, 1, 1, 1, 1, 0, 704, 100
36753, V, 1, 1, 1, 1, 0, 704, 100
36754, V, 1, 1, 1, 1, 0, 704, 100
36755, V, 1, 1, 1, 1, 0, 704, 100
36756, V, 1, 1, 1, 1, 0, 704, 100
36757, V, 1, 1, 1, 1, 0, 704, 100
36758, V, 1, 1, 1, 1, 0, 704, 100
36759, V, 1, 1, 1, 1, 0, 704, 100
36760, V, 1, 1, 1, 1, 0, 704, 100
36761, V, 1, 1, 1, 1, 0, 704, 100
36762, V, 1, 1, 1, 1, 0, 704, 100
36763, V, 1, 1, 1, 1, 0, 704, 100
36764, V, 1, 1, 1, 1, 0, 704, 100
36765, V, 1, 1, 1, 1, 0, 704, 100
36766, V, 1, 1, 1, 1, 0, 704, 100
36767, V, 1, 1, 1, 1, 0, 704, 100
36768, V, 1, 1, 1, 1, 0, 704, 100
36769, V, 1, 1, 1, 1, 0, 704, 100
36770, V, 1, 1, 1, 1, 0, 704, 100
36771, V, 1, 1, 1, 1, 0, 704, 100
36772, V, 1, 1, 1, 1, 0, 704, 100
36773, V, 1, 1, 1, 1, 0, 704, 100
36774, V, 1, 1, 1, 1, 0, 704, 100
36775, V, 1, 1, 1, 1, 0, 704, 100
36776, V, 1, 1, 1, 1, 0, 704, 100
36777, V, 1, 1, 1, 1, 0, 704, 100
36779, V, 1, 1, 1, 1, 0, 704, 100
36780, V, 1, 1, 1, 1, 0, 704, 100
36781, V, 1, 1, 1, 1, 0, 704, 100
36782, V, 1, 1, 1, 1, 0, 704, 100
36783, V, 1, 1, 1, 1, 0, 704, 100
36784, V, 1, 1, 1, 1, 0, 704, 100
36785, V, 1, 1, 1, 1, 0, 704, 100
36786, V, 1, 1, 1, 1, 0, 704, 100
36787, V, 1, 1, 1, 1, 0, 704, 100
36788, V, 1, 1, 1, 1, 0, 704, 100
36789, V, 1, 1, 1, 1, 0, 704, 100
36790, V, 1, 1, 1, 1, 0, 704, 100
36791, V, 1, 1, 1, 1, 0, 704, 100
36792, V, 1, 1, 1, 1, 0, 704, 100
36793, V, 1, 1, 1, 1, 0, 704, 100
36794, V, 1, 1, 1, 1, 0, 704, 100
36795, V, 1, 1, 1, 1, 0, 704, 100
36796, V, 1, 1, 1, 1, 0, 704, 100
36797, V, 1, 1, 1, 1, 0, 704, 100
36798, V, 1, 1, 1, 1, 0, 704, 100
36799, V, 1, 1, 1, 1, 0, 704, 100
36800, V, 1, 1, 1, 1, 0, 704, 100
36801, V, 1, 1, 1, 1, 0, 704, 100
36802, V, 1, 1, 1, 1, 0, 704, 100
36803, V, 1, 1, 1, 1, 0, 704, 100
36804, V, 1, 1, 1, 1, 0, 704, 100
36805, V, 1, 1, 1, 1, 0, 704, 100
36806, V, 1, 1, 1, 1, 0, 704, 100
36807, V, 1, 1, 1, 1, 0, 704, 100
36808, V, 1, 1, 1, 1, 0, 704, 100
36809, V, 1, 1, 1, 1, 0, 704, 100
36810, V, 1, 1, 1, 1, 0, 704, 100
36811, V, 1, 1, 1, 1, 0, 704, 100
36812, V, 1, 1, 1, 1, 0, 704, 100
36813, V, 1, 1, 1, 1, 0, 704, 100
36814, V, 1, 1, 1, 1, 0, 704, 100
36815, V, 1, 1, 1, 1, 0, 704, 100
36816, V, 1, 1, 1, 1, 0, 704, 100
36817, V, 1, 1, 1, 1, 0, 704, 100
36818, V, 1, 1, 1, 1, 0, 704, 100
36819, V, 1, 1, 1, 1, 0, 704, 100
36820, V, 1, 1, 1, 1, 0, 704, 100
36822, V, 1, 1, 1, 1, 0, 704, 100
36823, V, 1, 1, 1, 1, 0, 704, 100
36824, V, 1, 1, 1, 1, 0, 704, 100
36825, V, 1, 1, 1, 1, 0, 704, 100
36826, V, 1, 1, 1, 1, 0, 704, 100
36827, V, 1, 1, 1, 1, 0, 704, 100
36828, V, 1, 1, 1, 1, 0, 704, 100
36829, V, 1, 1, 1, 1, 0, 704, 100
36830, V, 1, 1, 1, 1, 0, 704, 100
36831, V, 1, 1, 1, 1, 0, 704, 100
36832, V, 1, 1, 1, 1, 0, 704, 100
36833, V, 1, 1, 1, 1, 0, 704, 100
36834, V, 1, 1, 1, 1, 0, 704, 100
36835, V, 1, 1, 1, 1, 0, 704, 100
36836, V, 1, 1, 1, 1, 0, 704, 100
36837, V, 1, 1, 1, 1, 0, 704, 100
36838, V, 1, 1, 1, 1, 0, 704, 100
36839, V, 1, 1, 1, 1, 0, 704, 100
36840, V, 1, 1, 1, 1, 0, 704, 100
36841, V, 1, 1, 1, 1, 0, 704, 100
36842, V, 1, 1, 1, 1, 0, 704, 100
36843, V, 1, 1, 1, 1, 0, 704, 100
36844, V, 1, 1, 1, 1, 0, 704, 100
36845, V, 1, 1, 1, 1, 0, 704, 100
36846, V, 1, 1, 1, 1, 0, 704, 100
36847, V, 1, 1, 1, 1, 0, 704, 100
36848, V, 1, 1, 1, 1, 0, 704, 100
36849, V, 1, 1, 1, 1, 0, 704, 100
36850, V, 1, 1, 1, 1, 0, 704, 100
36851, V, 1, 1, 1, 1, 0, 704, 100
36852, V, 1, 1, 1, 1, 0, 704, 100
36853, V, 1, 1, 1, 1, 0, 704, 100
36854, V, 1, 1, 1, 1, 0, 704, 100
36855, V, 1, 1, 1, 1, 0, 704, 100
36856, V, 1, 1, 1, 1, 0, 704, 100
36857, V, 1, 1, 1, 1, 0, 704, 100
36858, V, 1, 1, 1, 1, 0, 704, 100
36859, V, 1, 1, 1, 1, 0, 704, 100
36860, V, 1, 1, 1, 1, 0, 704, 100
36861, V, 1, 1, 1, 1, 0, 704, 100
36862, V, 1, 1, 1, 1, 0, 704, 100
36864, V, 1, 1, 1, 1, 0, 704, 100
36865, V, 1, 1, 1, 1, 0, 704, 100
36866, V, 1, 1, 1, 1, 0, 704, 100
36867, V, 1, 1, 1, 1, 0, 704, 100
36868, V, 1, 1, 1, 1, 0, 704, 100
36869, V, 1, 1, 1, 1, 0, 704, 100
36870, V, 1, 1, 1, 1, 0, 704, 100
36871, V, 1, 1, 1, 1, 0, 704, 100
36872, V, 1, 1, 1, 1, 0, 704, 100
36873, V, 1, 1, 1, 1, 0, 704, 100
36874, V, 1, 1, 1, 1, 0, 704, 100
36875, V, 1, 1, 1, 1, 0, 704, 100
36876, V, 1, 1, 1, 1, 0, 704, 100
36877, V, 1, 1, 1, 1, 0, 704, 100
36878, V, 1, 1, 1, 1, 0, 704, 100
36879, V, 1, 1, 1, 1, 0, 704, 100
36880, V, 1, 1, 1, 1, 0, 704, 100
36881, V, 1, 1, 1, 1, 0, 704, 100
36882, V, 1, 1, 1, 1, 0, 704, 100
36883, V, 1, 1, 1, 1, 0, 704, 100
36884, V, 1, 1, 1, 1, 0, 704, 100
36885, V, 1, 1, 1, 1, 0, 704, 100
36886, V, 1, 1, 1, 1, 0, 704, 100
36887, V, 1, 1, 1, 1, 0, 704, 100
36888, V, 1, 1, 1, 1, 0, 704, 100
36889, V, 1, 1, 1, 1, 0, 704, 100
36890, V, 1, 1, 1, 1, 0, 704, 100
36891, V, 1, 1, 1, 1, 0, 704, 100
36892, V, 1, 1, 1, 1, 0, 704, 100
36893, V, 1, 1, 1, 1, 0, 704, 100
36894, V, 1, 1, 1, 1, 0, 704, 100
36895, V, 1, 1, 1, 1, 0, 704, 100
36896, V, 1, 1, 1, 1, 0, 704, 100
36897, V, 1, 1, 1, 1, 0, 704, 100
36898, V, 1, 1, 1, 1, 0, 704, 100
36899, V, 1, 1, 1, 1, 0, 704, 100
36900, V, 1, 1, 1, 1, 0, 704, 100
36901, V, 1, 1, 1, 1, 0, 704, 100
36902, V, 1, 1, 1, 1, 0, 704, 100
36903, V, 1, 1, 1, 1, 0, 704, 100
36904, V, 1, 1, 1, 1, 0, 704, 100
36905, V, 1, 1, 1, 1, 0, 704, 100
36907, V, 1, 1, 1, 1, 0, 704, 100
36908, V, 1, 1, 1, 1, 0, 704, 100
36909, V, 1, 1, 1, 1, 0, 704, 100
36910, V, 1, 1, 1, 1, 0, 704, 100
36911, V, 1, 1, 1, 1, 0, 704, 100
36912, V, 1, 1, 1, 1, 0, 704, 100
36913, V, 1, 1, 1, 1, 0, 704, 100
36914, V, 1, 1, 1, 1, 0, 704, 100
36915, V, 1, 1, 1, 1, 0, 704, 100
36916, V, 1, 1, 1, 1, 0, 704, 100
36917, V, 1, 1, 1, 1, 0, 704, 100
36918, V, 1, 1, 1, 1, 0, 704, 100
36919, V, 1, 1, 1, 1, 0, 704, 100
36920, V, 1, 1, 1, 1, 0, 704, 100
36921, V, 1, 1, 1, 1, 0, 704, 100
36922, V, 1, 1, 1, 1, 0, 704, 100
36923, V, 1, 1, 1, 1, 0, 704, 100
36924, V, 1, 1, 1, 1, 0, 704, 100
36925, V, 1, 1, 1, 1, 0, 704, 100
36926, V, 1, 1, 1, 1, 0, 704, 100
36927, V, 1, 1, 1, 1, 0, 704, 100
36928, V, 1, 1, 1, 1, 0, 704, 100
36929, V, 1, 1, 1, 1, 0, 704, 100
36930, V, 1, 1, 1, 1, 0, 704, 100
36931, V, 1, 1, 1, 1, 0, 704, 100
36932, V, 1, 1, 1, 1, 0, 704, 100
36933, V, 1, 1, 1, 1, 0, 704, 100
36934, V, 1, 1, 1, 1, 0, 704, 100
36935, V, 1, 1, 1, 1, 0, 704, 100
36936, V, 1, 1, 1, 1, 0, 704, 100
36937, V, 1, 1, 1, 1, 0, 704, 100
36938, V, 1, 1, 1, 1, 0, 704, 100
36939, V, 1, 1, 1, 1, 0, 704, 100
36940, V, 1, 1, 1, 1, 0, 704, 100
36941, V, 1, 1, 1, 1, 0, 704, 100
36942, V, 1, 1, 1, 1, 0, 704, 100
36943, V, 1, 1, 1, 1, 0, 704, 100
36944, V, 1, 1, 1, 1, 0, 704, 100
36945, V, 1, 1, 1, 1, 0, 704, 100
36946, V, 1, 1, 1, 1, 0, 704, 100
36947, V, 1, 1, 1, 1, 0, 704, 100
36948, V, 1, 1, 1, 1, 0, 704, 100
36950, V, 1, 1, 1, 1, 0, 704, 100
36951, V, 1, 1, 1, 1, 0, 704, 100
36952, V, 1, 1, 1, 1, 0, 704, 100
36953, V, 1, 1, 1, 1, 0, 704, 100
36954, V, 1, 1, 1, 1, 0, 704, 100
36955, V, 1, 1, 1, 1, 0, 704, 100
36956, V, 1, 1, 1, 1, 0, 704, 100
36957, V, 1, 1, 1, 1, 0, 704, 100
36958, V, 1, 1, 1, 1, 0, 704, 100
36959, V, 1, 1, 1, 1, 0, 704, 100
36960, V, 1, 1, 1, 1, 0, 704, 100
36961, V, 1, 1, 1, 1, 0, 704, 100
36962, V, 1, 1, 1, 1, 0, 704, 100
36963, V, 1, 1, 1, 1, 0, 704, 100
36964, V, 1, 1, 1, 1, 0, 704, 100
36965, V, 1, 1, 1, 1, 0, 704, 100
36966, V, 1, 1, 1, 1, 0, 704, 100
36967, V, 1, 1, 1, 1, 0, 704, 100
36968, V, 1, 1, 1, 1, 0, 704, 100
36969, V, 1, 1, 1, 1, 0, 704, 100
36970, V, 1, 1, 1, 1, 0, 704, 100
36971, V, 1, 1, 1, 1, 0, 704, 100
36972, V, 1, 1, 1, 1, 0, 704, 100
36973, V, 1, 1, 1, 1, 0, 704, 100
36974, V, 1, 1, 1, 1, 0, 704, 100
36975, V, 1, 1, 1, 1, 0, 704, 100
36976, V, 1, 1, 1, 1, 0, 704, 100
36977, V, 1, 1, 1, 1, 0, 704, 100
36978, V, 1, 1, 1, 1, 0, 704, 100
36979, V, 1, 1, 1, 1, 0, 704, 100
36980, V, 1, 1, 1, 1, 0, 704, 100
36981, V, 1, 1, 1, 1, 0, 704, 100
36982, V, 1, 1, 1, 1, 0, 704, 100
36983, V, 1, 1, 1, 1, 0, 704, 100
36984, V, 1, 1, 1, 1, 0, 704, 100
36985, V, 1, 1, 1, 1, 0, 704, 100
36986, V, 1, 1, 1, 1, 0, 704, 100
36987, V, 1, 1, 1, 1, 0, 704, 100
36988, V, 1, 1, 1, 1, 0, 704, 100
36989, V, 1, 1, 1, 1, 0, 704, 100
36990, V, 1, 1, 1, 1, 0, 704, 100
36992, V, 1, 1, 1, 1, 0, 704, 100
36993, V, 1, 1, 1, 1, 0, 704, 100
36994, V, 1, 1, 1, 1, 0, 704, 100
36995, V, 1, 1, 1, 1, 0, 704, 100
36996, V, 1, 1, 1, 1, 0, 704, 100
36997, V, 1, 1, 1, 1, 0, 704, 100
36998, V, 1, 1, 1, 1, 0, 704, 100
36999, V, 1, 1, 1, 1, 0, 704, 100
37000, V, 1, 1, 1, 1, 0, 704, 100
37001, V, 1, 1, 1, 1, 0, 704, 100
37002, V, 1, 1, 1, 1, 0, 704, 100
37003, V, 1, 1, 1, 1, 0, 704, 100
37004, V, 1, 1, 1, 1, 0, 704, 100
37005, V, 1, 1, 1, 1, 0, 704, 100
37006, V, 1, 1, 1, 1, 0, 704, 100
37007, V, 1, 1, 1, 1, 0, 704, 100
37008, V, 1, 1, 1, 1, 0, 704, 100
37009, V, 1, 1, 1, 1, 0, 704, 100
37010, V, 1, 1, 1, 1, 0, 704, 100
37011, V, 1, 1, 1, 1, 0, 704, 100
37012, V, 1, 1, 1, 1, 0, 704, 100
37013, V, 1, 1, 1, 1, 0, 704, 100
37014, V, 1, 1, 1, 1, 0, 704, 100
37015, V, 1, 1, 1, 1, 0, 704, 100
37016, V, 1, 1, 1, 1, 0, 704, 100
37017, V, 1, 1, 1, 1, 0, 704, 100
37018, V, 1, 1, 1, 1, 0, 704, 100
37019, V, 1, 1, 1, 1, 0, 704, 100
37020, V, 1, 1, 1, 1, 0, 704, 100
37021, V, 1, 1, 1, 1, 0, 704, 100
37022, V, 1, 1, 1, 1, 0, 704, 100
37023, V, 1, 1, 1, 1, 0, 704, 100
37024, V, 1, 1, 1, 1, 0, 704, 100
37025, V, 1, 1, 1, 1, 0, 704, 100
37026, V, 1, 1, 1, 1, 0, 704, 100
37027, V, 1, 1, 1, 1, 0, 704, 100
37028, V, 1, 1, 1, 1, 0, 704, 100
37029, V, 1, 1, 1, 1, 0, 704, 100
37030, V, 1, 1, 1, 1, 0, 704, 100
37031, V, 1, 1, 1, 1, 0, 704, 100
37032, V, 1, 1, 1, 1, 0, 704, 100
37033, V, 1, 1, 1, 1, 0, 704, 100
37035, V, 1, 1, 1, 1, 0, 704, 100
37036, V, 1, 1, 1, 1, 0, 704, 100
37037, V, 1, 1, 1, 1, 0, 704, 100
37038, V, 1, 1, 1, 1, 0, 704, 100
37039, V, 1, 1, 1, 1, 0, 704, 100
37040, V, 1, 1, 1, 1, 0, 704, 100
37041, V, 1, 1, 1, 1, 0, 704, 100
37042, V, 1, 1, 1, 1, 0, 704, 100
37043, V, 1, 1, 1, 1, 0, 704, 100
37044, V, 1, 1, 1, 1, 0, 704, 100
37045, V, 1, 1, 1, 1, 0, 704, 100
37046, V, 1, 1, 1, 1, 0, 704, 100
37047, V, 1, 1, 1, 1, 0, 704, 100
37048, V, 1, 1, 1, 1, 0, 704, 100
37049, V, 1, 1, 1, 1, 0, 704, 100
37050, V, 1, 1, 1, 1, 0, 704, 100
37051, V, 1, 1, 1, 1, 0, 704, 100
37052, V, 1, 1, 1, 1, 0, 704, 100
37053, V, 1, 1, 1, 1, 0, 704, 100
37054, V, 1, 1, 1, 1, 0, 704, 100
37055, V, 1, 1, 1, 1, 0, 704, 100
37056, V, 1, 1, 1, 1, 0, 704, 100
37057, V, 1, 1, 1, 1, 0, 704, 100
37058, V, 1, 1, 1, 1, 0, 704, 100
37059, V, 1, 1, 1, 1, 0, 704, 100
37060, V, 1, 1, 1, 1, 0, 704, 100
37061, V, 1, 1, 1, 1, 0, 704, 100
37062, V, 1, 1, 1, 1, 0, 704, 100
37063, V, 1, 1, 1, 1, 0, 704, 100
37064, V, 1, 1, 1, 1, 0, 704, 100
37065, V, 1, 1, 1, 1, 0, 704, 100
37066, V, 1, 1, 1, 1, 0, 704, 100
37067, V, 1, 1, 1, 1, 0, 704, 100
37068, V, 1, 1, 1, 1, 0, 704, 100
37069, V, 1, 1, 1, 1, 0, 704, 100
37070, V, 1, 1, 1, 1, 0, 704, 100
37071, V, 1, 1, 1, 1, 0, 704, 100
37072, V, 1, 1, 1, 1, 0, 704, 100
37073, V, 1, 1, 1, 1, 0, 704, 100
37074, V, 1, 1, 1, 1, 0, 704, 100
37075, V, 1, 1, 1, 1, 0, 704, 100
37076, V, 1, 1, 1, 1, 0, 704, 100
37078, V, 1, 1, 1, 1, 0, 704, 100
37079, V, 1, 1, 1, 1, 0, 704, 100
37080, V, 1, 1, 1, 1, 0, 704, 100
37081, V, 1, 1, 1, 1, 0, 704, 100
37082, V, 1, 1, 1, 1, 0, 704, 100
37083, V, 1, 1, 1, 1, 0, 704, 100
37084, V, 1, 1, 1, 1, 0, 704, 100
37085, V, 1, 1, 1, 1, 0, 704, 100
37086, V, 1, 1, 1, 1, 0, 704, 100
37087, V, 1, 1, 1, 1, 0, 704, 100
37088, V, 1, 1, 1, 1, 0, 704, 100
37089, V, 1, 1, 1, 1, 0, 704, 100
37090, V, 1, 1, 1, 1, 0, 704, 100
37091, V, 1, 1, 1, 1, 0, 704, 100
37092, V, 1, 1, 1, 1, 0, 704, 100
37093, V, 1, 1, 1, 1, 0, 704, 100
37094, V, 1, 1, 1, 1, 0, 704, 100
37095, V, 1, 1, 1, 1, 0, 704, 100
37096, V, 1, 1, 1, 1, 0, 704, 100
37097, V, 1, 1, 1, 1, 0, 704, 100
37098, V, 1, 1, 1, 1, 0, 704, 100
37099, V, 1, 1, 1, 1, 0, 704, 100
37100, V, 1, 1, 1, 1, 0, 704, 100
37101, V, 1, 1, 1, 1, 0, 704, 100
37102, V, 1, 1, 1, 1, 0, 704, 100
37103, V, 1, 1, 1, 1, 0, 704, 100
37104, V, 1, 1, 1, 1, 0, 704, 100
37105, V, 1, 1, 1, 1, 0, 704, 100
37106, V, 1, 1, 1, 1, 0, 704, 100
37107, V, 1, 1, 1, 1, 0, 704, 100
37108, V, 1, 1, 1, 1, 0, 704, 100
37109, V, 1, 1, 1, 1, 0, 704, 100
37110, V, 1, 1, 1, 1, 0, 704, 100
37111, V, 1, 1, 1, 1, 0, 704, 100
37112, V, 1, 1, 1, 1, 0, 704, 100
37113, V, 1, 1, 1, 1, 0, 704, 100
37114, V, 1, 1, 1, 1, 0, 704, 100
37115, V, 1, 1, 1, 1, 0, 704, 100
37116, V, 1, 1, 1, 1, 0, 704, 100
37117, V, 1, 1, 1, 1, 0, 704, 100
37118, V, 1, 1, 1, 1, 0, 704, 100
37120, V, 1, 1, 1, 1, 0, 704, 100
37121, V, 1, 1, 1, 1, 0, 704, 100
37122, V, 1, 1, 1, 1, 0, 704, 100
37123, V, 1, 1, 1, 1, 0, 704, 100
37124, V, 1, 1, 1, 1, 0, 704, 100
37125, V, 1, 1, 1, 1, 0, 704, 100
37126, V, 1, 1, 1, 1, 0, 704, 100
37127, V, 1, 1, 1, 1, 0, 704, 100
37128, V, 1, 1, 1, 1, 0, 704, 100
37129, V, 1, 1, 1, 1, 0, 704, 100
37130, V, 1, 1, 1, 1, 0, 704, 100
37131, V, 1, 1, 1, 1, 0, 704, 100
37132, V, 1, 1, 1, 1, 0, 704, 100
37133, V, 1, 1, 1, 1, 0, 704, 100
37134, V, 1, 1, 1, 1, 0, 704, 100
37135, V, 1, 1, 1, 1, 0, 704, 100
37136, V, 1, 1, 1, 1, 0, 704, 100
37137, V, 1, 1, 1, 1, 0, 704, 100
37138, V, 1, 1, 1, 1, 0, 704, 100
37139, V, 1, 1, 1, 1, 0, 704, 100
37140, V, 1, 1, 1, 1, 0, 704, 100
37141, V, 1, 1, 1, 1, 0, 704, 100
37142, V, 1, 1, 1, 1, 0, 704, 100
37143, V, 1, 1, 1, 1, 0, 704, 100
37144, V, 1, 1, 1, 1, 0, 704, 100
37145, V, 1, 1, 1, 1, 0, 704, 100
37146, V, 1, 1, 1, 1, 0, 704, 100
37147, V, 1, 1, 1, 1, 0, 704, 100
37148, V, 1, 1, 1, 1, 0, 704, 100
37149, V, 1, 1, 1, 1, 0, 704, 100
37150, V, 1, 1, 1, 1, 0, 704, 100
37151, V, 1, 1, 1, 1, 0, 704, 100
37152, V, 1, 1, 1, 1, 0, 704, 100
37153, V, 1, 1, 1, 1, 0, 704, 100
37154, V, 1, 1, 1, 1, 0, 704, 100
37155, V, 1, 1, 1, 1, 0, 704, 100
37156, V, 1, 1, 1, 1, 0, 704, 100
37157, V, 1, 1, 1, 1, 0, 704, 100
37158, V, 1, 1, 1, 1, 0, 704, 100
37159, V, 1, 1, 1, 1, 0, 704, 100
37160, V, 1, 1, 1, 1, 0, 704, 100
37161, V, 1, 1, 1, 1, 0, 704, 100
37163, V, 1, 1, 1, 1, 0, 704, 100
37164, V, 1, 1, 1, 1, 0, 704, 100
37165, V, 1, 1, 1, 1, 0, 704, 100
37166, V, 1, 1, 1, 1, 0, 704, 100
37167, V, 1, 1, 1, 1, 0, 704, 100
37168, V, 1, 1, 1, 1, 0, 704, 100
37169, V, 1, 1, 1, 1, 0, 704, 100
37170, V, 1, 1, 1, 1, 0, 704, 100
37171, V, 1, 1, 1, 1, 0, 704, 100
37172, V, 1, 1, 1, 1, 0, 704, 100
37173, V, 1, 1, 1, 1, 0, 704, 100
37174, V, 1, 1, 1, 1, 0, 704, 100
37175, V, 1, 1, 1, 1, 0, 704, 100
37176, V, 1, 1, 1, 1, 0, 704, 100
37177, V, 1, 1, 1, 1, 0, 704, 100
37178, V, 1, 1, 1, 1, 0, 704, 100
37179, V, 1, 1, 1, 1, 0, 704, 100
37180, V, 1, 1, 1, 1, 0, 704, 100
37181, V, 1, 1, 1, 1, 0, 704, 100
37182, V, 1, 1, 1, 1, 0, 704, 100
37183, V, 1, 1, 1, 1, 0, 704, 100
37184, V, 1, 1, 1, 1, 0, 704, 100
37185, V, 1, 1, 1, 1, 0, 704, 100
37186, V, 1, 1, 1, 1, 0, 704, 100
37187, V, 1, 1, 1, 1, 0, 704, 100
37188, V, 1, 1, 1, 1, 0, 704, 100
37189, V, 1, 1, 1, 1, 0, 704, 100
37190, V, 1, 1, 1, 1, 0, 704, 100
37191, V, 1, 1, 1, 1, 0, 704, 100
37192, V, 1, 1, 1, 1, 0, 704, 100
37193, V, 1, 1, 1, 1, 0, 704, 100
37194, V, 1, 1, 1, 1, 0, 704, 100
37195, V, 1, 1, 1, 1, 0, 704, 100
37196, V, 1, 1, 1, 1, 0, 704, 100
37197, V, 1, 1, 1, 1, 0, 704, 100
37198, V, 1, 1, 1, 1, 0, 704, 100
37199, V, 1, 1, 1, 1, 0, 704, 100
37200, V, 1, 1, 1, 1, 0, 704, 100
37201, V, 1, 1, 1, 1, 0, 704, 100
37202, V, 1, 1, 1, 1, 0, 704, 100
37203, V, 1, 1, 1, 1, 0, 704, 100
37204, V, 1, 1, 1, 1, 0, 704, 100
37206, V, 1, 1, 1, 1, 0, 704, 100
37207, V, 1, 1, 1, 1, 0, 704, 100
37208, V, 1, 1, 1, 1, 0, 704, 100
37209, V, 1, 1, 1, 1, 0, 704, 100
37210, V, 1, 1, 1, 1, 0, 704, 100
37211, V, 1, 1, 1, 1, 0, 704, 100
37212, V, 1, 1, 1, 1, 0, 704, 100
37213, V, 1, 1, 1, 1, 0, 704, 100
37214, V, 1, 1, 1, 1, 0, 704, 100
37215, V, 1, 1, 1, 1, 0, 704, 100
37216, V, 1, 1, 1, 1, 0, 704, 100
37217, V, 1, 1, 1, 1, 0, 704, 100
37218, V, 1, 1, 1, 1, 0, 704, 100
37219, V, 1, 1, 1, 1, 0, 704, 100
37220, V, 1, 1, 1, 1, 0, 704, 100
37221, V, 1, 1, 1, 1, 0, 704, 100
37222, V, 1, 1, 1, 1, 0, 704, 100
37223, V, 1, 1, 1, 1, 0, 704, 100
37224, V, 1, 1, 1, 1, 0, 704, 100
37225, V, 1, 1, 1, 1, 0, 704, 100
37226, V, 1, 1, 1, 1, 0, 704, 100
37227, V, 1, 1, 1, 1, 0, 704, 100
37228, V, 1, 1, 1, 1, 0, 704, 100
37229, V, 1, 1, 1, 1, 0, 704, 100
37230, V, 1, 1, 1, 1, 0, 704, 100
37231, V, 1, 1, 1, 1, 0, 704, 100
37232, V, 1, 1, 1, 1, 0, 704, 100
37233, V, 1, 1, 1, 1, 0, 704, 100
37234, V, 1, 1, 1, 1, 0, 704, 100
37235, V, 1, 1, 1, 1, 0, 704, 100
37236, V, 1, 1, 1, 1, 0, 704, 100
37237, V, 1, 1, 1, 1, 0, 704, 100
37238, V, 1, 1, 1, 1, 0, 704, 100
37239, V, 1, 1, 1, 1, 0, 704, 100
37240, V, 1, 1, 1, 1, 0, 704, 100
37241, V, 1, 1, 1, 1, 0, 704, 100
37242, V, 1, 1, 1, 1, 0, 704, 100
37243, V, 1, 1, 1, 1, 0, 704, 100
37244, V, 1, 1, 1, 1, 0, 704, 100
37245, V, 1, 1, 1, 1, 0, 704, 100
37246, V, 1, 1, 1, 1, 0, 704, 100
37248, V, 1, 1, 1, 1, 0, 704, 100
37249, V, 1, 1, 1, 1, 0, 704, 100
37250, V, 1, 1, 1, 1, 0, 704, 100
37251, V, 1, 1, 1, 1, 0, 704, 100
37252, V, 1, 1, 1, 1, 0, 704, 100
37253, V, 1, 1, 1, 1, 0, 704, 100
37254, V, 1, 1, 1, 1, 0, 704, 100
37255, V, 1, 1, 1, 1, 0, 704, 100
37256, V, 1, 1, 1, 1, 0, 704, 100
37257, V, 1, 1, 1, 1, 0, 704, 100
37258, V, 1, 1, 1, 1, 0, 704, 100
37259, V, 1, 1, 1, 1, 0, 704, 100
37260, V, 1, 1, 1, 1, 0, 704, 100
37261, V, 1, 1, 1, 1, 0, 704, 100
37262, V, 1, 1, 1, 1, 0, 704, 100
37263, V, 1, 1, 1, 1, 0, 704, 100
37264, V, 1, 1, 1, 1, 0, 704, 100
37265, V, 1, 1, 1, 1, 0, 704, 100
37266, V, 1, 1, 1, 1, 0, 704, 100
37267, V, 1, 1, 1, 1, 0, 704, 100
37268, V, 1, 1, 1, 1, 0, 704, 100
37269, V, 1, 1, 1, 1, 0, 704, 100
37270, V, 1, 1, 1, 1, 0, 704, 100
37271, V, 1, 1, 1, 1, 0, 704, 100
37272, V, 1, 1, 1, 1, 0, 704, 100
37273, V, 1, 1, 1, 1, 0, 704, 100
37274, V, 1, 1, 1, 1, 0, 704, 100
37275, V, 1, 1, 1, 1, 0, 704, 100
37276, V, 1, 1, 1, 1, 0, 704, 100
37277, V, 1, 1, 1, 1, 0, 704, 100
37278, V, 1, 1, 1, 1, 0, 704, 100
37279, V, 1, 1, 1, 1, 0, 704, 100
37280, V, 1, 1, 1, 1, 0, 704, 100
37281, V, 1, 1, 1, 1, 0, 704, 100
37282, V, 1, 1, 1, 1, 0, 704, 100
37283, V, 1, 1, 1, 1, 0, 704, 100
37284, V, 1, 1, 1, 1, 0, 704, 100
37285, V, 1, 1, 1, 1, 0, 704, 100
37286, V, 1, 1, 1, 1, 0, 704, 100
37287, V, 1, 1, 1, 1, 0, 704, 100
37288, V, 1, 1, 1, 1, 0, 704, 100
37289, V, 1, 1, 1, 1, 0, 704, 100
37291, V, 1, 1, 1, 1, 0, 704, 100
37292, V, 1, 1, 1, 1, 0, 704, 100
37293, V, 1, 1, 1, 1, 0, 704, 100
37294, V, 1, 1, 1, 1, 0, 704, 100
37295, V, 1, 1, 1, 1, 0, 704, 100
37296, V, 1, 1, 1, 1, 0, 704, 100
37297, V, 1, 1, 1, 1, 0, 704, 100
37298, V, 1, 1, 1, 1, 0, 704, 100
37299, V, 1, 1, 1, 1, 0, 704, 100
37300, V, 1, 1, 1, 1, 0, 704, 100
37301, V, 1, 1, 1, 1, 0, 704, 100
37302, V, 1, 1, 1, 1, 0, 704, 100
37303, V, 1, 1, 1, 1, 0, 704, 100
37304, V, 1, 1, 1, 1, 0, 704, 100
37305, V, 1, 1, 1, 1, 0, 704, 100
37306, V, 1, 1, 1, 1, 0, 704, 100
37307, V, 1, 1, 1, 1, 0, 704, 100
37308, V, 1, 1, 1, 1, 0, 704, 100
37309, V, 1, 1, 1, 1, 0, 704, 100
37310, V, 1, 1, 1, 1, 0, 704, 100
37311, V, 1, 1, 1, 1, 0, 704, 100
37312, V, 1, 1, 1, 1, 0, 704, 100
37313, V, 1, 1, 1, 1, 0, 704, 100
37314, V, 1, 1, 1, 1, 0, 704, 100
37315, V, 1, 1, 1, 1, 0, 704, 100
37316, V, 1, 1, 1, 1, 0, 704, 100
37317, V, 1, 1, 1, 1, 0, 704, 100
37318, V, 1, 1, 1, 1, 0, 704, 100
37319, V, 1, 1, 1, 1, 0, 704, 100
37320, V, 1, 1, 1, 1, 0, 704, 100
37321, V, 1, 1, 1, 1, 0, 704, 100
37322, V, 1, 1, 1, 1, 0, 704, 100
37323, V, 1, 1, 1, 1, 0, 704, 100
37324, V, 1, 1, 1, 1, 0, 704, 100
37325, V, 1, 1, 1, 1, 0, 704, 100
37326, V, 1, 1, 1, 1, 0, 704, 100
37327, V, 1, 1, 1, 1, 0, 704, 100
37328, V, 1, 1, 1, 1, 0, 704, 100
37329, V, 1, 1, 1, 1, 0, 704, 100
37330, V, 1, 1, 1, 1, 0, 704, 100
37331, V, 1, 1, 1, 1, 0, 704, 100
37332, V, 1, 1, 1, 1, 0, 704, 100
37334, V, 1, 1, 1, 1, 0, 704, 100
37335, V, 1, 1, 1, 1, 0, 704, 100
37336, V, 1, 1, 1, 1, 0, 704, 100
37337, V, 1, 1, 1, 1, 0, 704, 100
37338, V, 1, 1, 1, 1, 0, 704, 100
37339, V, 1, 1, 1, 1, 0, 704, 100
37340, V, 1, 1, 1, 1, 0, 704, 100
37341, V, 1, 1, 1, 1, 0, 704, 100
37342, V, 1, 1, 1, 1, 0, 704, 100
37343, V, 1, 1, 1, 1, 0, 704, 100
37344, V, 1, 1, 1, 1, 0, 704, 100
37345, V, 1, 1, 1, 1, 0, 704, 100
37346, V, 1, 1, 1, 1, 0, 704, 100
37347, V, 1, 1, 1, 1, 0, 704, 100
37348, V, 1, 1, 1, 1, 0, 704, 100
37349, V, 1, 1, 1, 1, 0, 704, 100
37350, V, 1, 1, 1, 1, 0, 704, 100
37351, V, 1, 1, 1, 1, 0, 704, 100
37352, V, 1, 1, 1, 1, 0, 704, 100
37353, V, 1, 1, 1, 1, 0, 704, 100
37354, V, 1, 1, 1, 1, 0, 704, 100
37355, V, 1, 1, 1, 1, 0, 704, 100
37356, V, 1, 1, 1, 1, 0, 704, 100
37357, V, 1, 1, 1, 1, 0, 704, 100
37358, V, 1, 1, 1, 1, 0, 704, 100
37359, V, 1, 1, 1, 1, 0, 704, 100
37360, V, 1, 1, 1, 1, 0, 704, 100
37361, V, 1, 1, 1, 1, 0, 704, 100
37362, V, 1, 1, 1, 1, 0, 704, 100
37363, V, 1, 1, 1, 1, 0, 704, 100
37364, V, 1, 1, 1, 1, 0, 704, 100
37365, V, 1, 1, 1, 1, 0, 704, 100
37366, V, 1, 1, 1, 1, 0, 704, 100
37367, V, 1, 1, 1, 1, 0, 704, 100
37368, V, 1, 1, 1, 1, 0, 704, 100
37369, V, 1, 1, 1, 1, 0, 704, 100
37370, V, 1, 1, 1, 1, 0, 704, 100
37371, V, 1, 1, 1, 1, 0, 704, 100
37372, V, 1, 1, 1, 1, 0, 704, 100
37373, V, 1, 1, 1, 1, 0, 704, 100
37374, V, 1, 1, 1, 1, 0, 704, 100
37376, V, 1, 1, 1, 1, 0, 704, 100
37377, V, 1, 1, 1, 1, 0, 704, 100
37378, V, 1, 1, 1, 1, 0, 704, 100
37379, V, 1, 1, 1, 1, 0, 704, 100
37380, V, 1, 1, 1, 1, 0, 704, 100
37381, V, 1, 1, 1, 1, 0, 704, 100
37382, V, 1, 1, 1, 1, 0, 704, 100
37383, V, 1, 1, 1, 1, 0, 704, 100
37384, V, 1, 1, 1, 1, 0, 704, 100
37385, V, 1, 1, 1, 1, 0, 704, 100
37386, V, 1, 1, 1, 1, 0, 704, 100
37387, V, 1, 1, 1, 1, 0, 704, 100
37388, V, 1, 1, 1, 1, 0, 704, 100
37389, V, 1, 1, 1, 1, 0, 704, 100
37390, V, 1, 1, 1, 1, 0, 704, 100
37391, V, 1, 1, 1, 1, 0, 704, 100
37392, V, 1, 1, 1, 1, 0, 704, 100
37393, V, 1, 1, 1, 1, 0, 704, 100
37394, V, 1, 1, 1, 1, 0, 704, 100
37395, V, 1, 1, 1, 1, 0, 704, 100
37396, V, 1, 1, 1, 1, 0, 704, 100
37397, V, 1, 1, 1, 1, 0, 704, 100
37398, V, 1, 1, 1, 1, 0, 704, 100
37399, V, 1, 1, 1, 1, 0, 704, 100
37400, V, 1, 1, 1, 1, 0, 704, 100
37401, V, 1, 1, 1, 1, 0, 704, 100
37402, V, 1, 1, 1, 1, 0, 704, 100
37403, V, 1, 1, 1, 1, 0, 704, 100
37404, V, 1, 1, 1, 1, 0, 704, 100
37405, V, 1, 1, 1, 1, 0, 704, 100
37406, V, 1, 1, 1, 1, 0, 704, 100
37407, V, 1, 1, 1, 1, 0, 704, 100
37408, V, 1, 1, 1, 1, 0, 704, 100
37409, V, 1, 1, 1, 1, 0, 704, 100
37410, V, 1, 1, 1, 1, 0, 704, 100
37411, V, 1, 1, 1, 1, 0, 704, 100
37412, V, 1, 1, 1, 1, 0, 704, 100
37413, V, 1, 1, 1, 1, 0, 704, 100
37414, V, 1, 1, 1, 1, 0, 704, 100
37415, V, 1, 1, 1, 1, 0, 704, 100
37416, V, 1, 1, 1, 1, 0, 704, 100
37417, V, 1, 1, 1, 1, 0, 704, 100
37419, V, 1, 1, 1, 1, 0, 704, 100
37420, V, 1, 1, 1, 1, 0, 704, 100
37421, V, 1, 1, 1, 1, 0, 704, 100
37422, V, 1, 1, 1, 1, 0, 704, 100
37423, V, 1, 1, 1, 1, 0, 704, 100
37424, V, 1, 1, 1, 1, 0, 704, 100
37425, V, 1, 1, 1, 1, 0, 704, 100
37426, V, 1, 1, 1, 1, 0, 704, 100
37427, V, 1, 1, 1, 1, 0, 704, 100
37428, V, 1, 1, 1, 1, 0, 704, 100
37429, V, 1, 1, 1, 1, 0, 704, 100
37430, V, 1, 1, 1, 1, 0, 704, 100
37431, V, 1, 1, 1, 1, 0, 704, 100
37432, V, 1, 1, 1, 1, 0, 704, 100
37433, V, 1, 1, 1, 1, 0, 704, 100
37434, V, 1, 1, 1, 1, 0, 704, 100
37435, V, 1, 1, 1, 1, 0, 704, 100
37436, V, 1, 1, 1, 1, 0, 704, 100
37437, V, 1, 1, 1, 1, 0, 704, 100
37438, V, 1, 1, 1, 1, 0, 704, 100
37439, V, 1, 1, 1, 1, 0, 704, 100
37440, V, 1, 1, 1, 1, 0, 704, 100
37441, V, 1, 1, 1, 1, 0, 704, 100
37442, V, 1, 1, 1, 1, 0, 704, 100
37443, V, 1, 1, 1, 1, 0, 704, 100
37444, V, 1, 1, 1, 1, 0, 704, 100
37445, V, 1, 1, 1, 1, 0, 704, 100
37446, V, 1, 1, 1, 1, 0, 704, 100
37447, V, 1, 1, 1, 1, 0, 704, 100
37448, V, 1, 1, 1, 1, 0, 704, 100
37449, V, 1, 1, 1, 1, 0, 704, 100
37450, V, 1, 1, 1, 1, 0, 704, 100
37451, V, 1, 1, 1, 1, 0, 704, 100
37452, V, 1, 1, 1, 1, 0, 704, 100
37453, V, 1, 1, 1, 1, 0, 704, 100
37454, V, 1, 1, 1, 1, 0, 704, 100
37455, V, 1, 1, 1, 1, 0, 704, 100
37456, V, 1, 1, 1, 1, 0, 704, 100
37457, V, 1, 1, 1, 1, 0, 704, 100
37458, V, 1, 1, 1, 1, 0, 704, 100
37459, V, 1, 1, 1, 1, 0, 704, 100
37460, V, 1, 1, 1, 1, 0, 704, 100
37462, V, 1, 1, 1, 1, 0, 704, 100
37463, V, 1, 1, 1, 1, 0, 704, 100
37464, V, 1, 1, 1, 1, 0, 704, 100
37465, V, 1, 1, 1, 1, 0, 704, 100
37466, V, 1, 1, 1, 1, 0, 704, 100
37467, V, 1, 1, 1, 1, 0, 704, 100
37468, V, 1, 1, 1, 1, 0, 704, 100
37469, V, 1, 1, 1, 1, 0, 704, 100
37470, V, 1, 1, 1, 1, 0, 704, 100
37471, V, 1, 1, 1, 1, 0, 704, 100
37472, V, 1, 1, 1, 1, 0, 704, 100
37473, V, 1, 1, 1, 1, 0, 704, 100
37474, V, 1, 1, 1, 1, 0, 704, 100
37475, V, 1, 1, 1, 1, 0, 704, 100
37476, V, 1, 1, 1, 1, 0, 704, 100
37477, V, 1, 1, 1, 1, 0, 704, 100
37478, V, 1, 1, 1, 1, 0, 704, 100
37479, V, 1, 1, 1, 1, 0, 704, 100
37480, V, 1, 1, 1, 1, 0, 704, 100
37481, V, 1, 1, 1, 1, 0, 704, 100
37482, V, 1, 1, 1, 1, 0, 704, 100
37483, V, 1, 1, 1, 1, 0, 704, 100
37484, V, 1, 1, 1, 1, 0, 704, 100
37485, V, 1, 1, 1, 1, 0, 704, 100
37486, V, 1, 1, 1, 1, 0, 704, 100
37487, V, 1, 1, 1, 1, 0, 704, 100
37488, V, 1, 1, 1, 1, 0, 704, 100
37489, V, 1, 1, 1, 1, 0, 704, 100
37490, V, 1, 1, 1, 1, 0, 704, 100
37491, V, 1, 1, 1, 1, 0, 704, 100
37492, V, 1, 1, 1, 1, 0, 704, 100
37493, V, 1, 1, 1, 1, 0, 704, 100
37494, V, 1, 1, 1, 1, 0, 704, 100
37495, V, 1, 1, 1, 1, 0, 704, 100
37496, V, 1, 1, 1, 1, 0, 704, 100
37497, V, 1, 1, 1, 1, 0, 704, 100
37498, V, 1, 1, 1, 1, 0, 704, 100
37499, V, 1, 1, 1, 1, 0, 704, 100
37500, V, 1, 1, 1, 1, 0, 704, 100
37501, V, 1, 1, 1, 1, 0, 704, 100
37502, V, 1, 1, 1, 1, 0, 704, 100
37504, V, 1, 1, 1, 1, 0, 704, 100
37505, V, 1, 1, 1, 1, 0, 704, 100
37506, V, 1, 1, 1, 1, 0, 704, 100
37507, V, 1, 1, 1, 1, 0, 704, 100
37508, V, 1, 1, 1, 1, 0, 704, 100
37509, V, 1, 1, 1, 1, 0, 704, 100
37510, V, 1, 1, 1, 1, 0, 704, 100
37511, V, 1, 1, 1, 1, 0, 704, 100
37512, V, 1, 1, 1, 1, 0, 704, 100
37513, V, 1, 1, 1, 1, 0, 704, 100
37514, V, 1, 1, 1, 1, 0, 704, 100
37515, V, 1, 1, 1, 1, 0, 704, 100
37516, V, 1, 1, 1, 1, 0, 704, 100
37517, V, 1, 1, 1, 1, 0, 704, 100
37518, V, 1, 1, 1, 1, 0, 704, 100
37519, V, 1, 1, 1, 1, 0, 704, 100
37520, V, 1, 1, 1, 1, 0, 704, 100
37521, V, 1, 1, 1, 1, 0, 704, 100
37522, V, 1, 1, 1, 1, 0, 704, 100
37523, V, 1, 1, 1, 1, 0, 704, 100
37524, V, 1, 1, 1, 1, 0, 704, 100
37525, V, 1, 1, 1, 1, 0, 704, 100
37526, V, 1, 1, 1, 1, 0, 704, 100
37527, V, 1, 1, 1, 1, 0, 704, 100
37528, V, 1, 1, 1, 1, 0, 704, 100
37529, V, 1, 1, 1, 1, 0, 704, 100
37530, V, 1, 1, 1, 1, 0, 704, 100
37531, V, 1, 1, 1, 1, 0, 704, 100
37532, V, 1, 1, 1, 1, 0, 704, 100
37533, V, 1, 1, 1, 1, 0, 704, 100
37534, V, 1, 1, 1, 1, 0, 704, 100
37535, V, 1, 1, 1, 1, 0, 704, 100
37536, V, 1, 1, 1, 1, 0, 704, 100
37537, V, 1, 1, 1, 1, 0, 704, 100
37538, V, 1, 1, 1, 1, 0, 704, 100
37539, V, 1, 1, 1, 1, 0, 704, 100
37540, V, 1, 1, 1, 1, 0, 704, 100
37541, V, 1, 1, 1, 1, 0, 704, 100
37542, V, 1, 1, 1, 1, 0, 704, 100
37543, V, 1, 1, 1, 1, 0, 704, 100
37544, V, 1, 1, 1, 1, 0, 704, 100
37545, V, 1, 1, 1, 1, 0, 704, 100
37547, V, 1, 1, 1, 1, 0, 704, 100
37548, V, 1, 1, 1, 1, 0, 704, 100
37549, V, 1, 1, 1, 1, 0, 704, 100
37550, V, 1, 1, 1, 1, 0, 704, 100
37551, V, 1, 1, 1, 1, 0, 704, 100
37552, V, 1, 1, 1, 1, 0, 704, 100
37553, V, 1, 1, 1, 1, 0, 704, 100
37554, V, 1, 1, 1, 1, 0, 704, 100
37555, V, 1, 1, 1, 1, 0, 704, 100
37556, V, 1, 1, 1, 1, 0, 704, 100
37557, V, 1, 1, 1, 1, 0, 704, 100
37558, V, 1, 1, 1, 1, 0, 704, 100
37559, V, 1, 1, 1, 1, 0, 704, 100
37560, V, 1, 1, 1, 1, 0, 704, 100
37561, V, 1, 1, 1, 1, 0, 704, 100
37562, V, 1, 1, 1, 1, 0, 704, 100
37563, V, 1, 1, 1, 1, 0, 704, 100
37564, V, 1, 1, 1, 1, 0, 704, 100
37565, V, 1, 1, 1, 1, 0, 704, 100
37566, V, 1, 1, 1, 1, 0, 704, 100
37567, V, 1, 1, 1, 1, 0, 704, 100
37568, V, 1, 1, 1, 1, 0, 704, 100
37569, V, 1, 1, 1, 1, 0, 704, 100
37570, V, 1, 1, 1, 1, 0, 704, 100
37571, V, 1, 1, 1, 1, 0, 704, 100
37572, V, 1, 1, 1, 1, 0, 704, 100
37573, V, 1, 1, 1, 1, 0, 704, 100
37574, V, 1, 1, 1, 1, 0, 704, 100
37575, V, 1, 1, 1, 1, 0, 704, 100
37576, V, 1, 1, 1, 1, 0, 704, 100
37577, V, 1, 1, 1, 1, 0, 704, 100
37578, V, 1, 1, 1, 1, 0, 704, 100
37579, V, 1, 1, 1, 1, 0, 704, 100
37580, V, 1, 1, 1, 1, 0, 704, 100
37581, V, 1, 1, 1, 1, 0, 704, 100
37582, V, 1, 1, 1, 1, 0, 704, 100
37583, V, 1, 1, 1, 1, 0, 704, 100
37584, V, 1, 1, 1, 1, 0, 704, 100
37585, V, 1, 1, 1, 1, 0, 704, 100
37586, V, 1, 1, 1, 1, 0, 704, 100
37587, V, 1, 1, 1, 1, 0, 704, 100
37588, V, 1, 1, 1, 1, 0, 704, 100
37590, V, 1, 1, 1, 1, 0, 704, 100
37591, V, 1, 1, 1, 1, 0, 704, 100
37592, V, 1, 1, 1, 1, 0, 704, 100
37593, V, 1, 1, 1, 1, 0, 704, 100
37594, V, 1, 1, 1, 1, 0, 704, 100
37595, V, 1, 1, 1, 1, 0, 704, 100
37596, V, 1, 1, 1, 1, 0, 704, 100
37597, V, 1, 1, 1, 1, 0, 704, 100
37598, V, 1, 1, 1, 1, 0, 704, 100
37599, V, 1, 1, 1, 1, 0, 704, 100
37600, V, 1, 1, 1, 1, 0, 704, 100
37601, V, 1, 1, 1, 1, 0, 704, 100
37602, V, 1, 1, 1, 1, 0, 704, 100
37603, V, 1, 1, 1, 1, 0, 704, 100
37604, V, 1, 1, 1, 1, 0, 704, 100
37605, V, 1, 1, 1, 1, 0, 704, 100
37606, V, 1, 1, 1, 1, 0, 704, 100
37607, V, 1, 1, 1, 1, 0, 704, 100
37608, V, 1, 1, 1, 1, 0, 704, 100
37609, V, 1, 1, 1, 1, 0, 704, 100
37610, V, 1, 1, 1, 1, 0, 704, 100
37611, V, 1, 1, 1, 1, 0, 704, 100
37612, V, 1, 1, 1, 1, 0, 704, 100
37613, V, 1, 1, 1, 1, 0, 704, 100
37614, V, 1, 1, 1, 1, 0, 704, 100
37615, V, 1, 1, 1, 1, 0, 704, 100
37616, V, 1, 1, 1, 1, 0, 704, 100
37617, V, 1, 1, 1, 1, 0, 704, 100
37618, V, 1, 1, 1, 1, 0, 704, 100
37619, V, 1, 1, 1, 1, 0, 704, 100
37620, V, 1, 1, 1, 1, 0, 704, 100
37621, V, 1, 1, 1, 1, 0, 704, 100
37622, V, 1, 1, 1, 1, 0, 704, 100
37623, V, 1, 1, 1, 1, 0, 704, 100
37624, V, 1, 1, 1, 1, 0, 704, 100
37625, V, 1, 1, 1, 1, 0, 704, 100
37626, V, 1, 1, 1, 1, 0, 704, 100
37627, V, 1, 1, 1, 1, 0, 704, 100
37628, V, 1, 1, 1, 1, 0, 704, 100
37629, V, 1, 1, 1, 1, 0, 704, 100
37630, V, 1, 1, 1, 1, 0, 704, 100
37632, V, 1, 1, 1, 1, 0, 704, 100
37633, V, 1, 1, 1, 1, 0, 704, 100
37634, V, 1, 1, 1, 1, 0, 704, 100
37635, V, 1, 1, 1, 1, 0, 704, 100
37636, V, 1, 1, 1, 1, 0, 704, 100
37637, V, 1, 1, 1, 1, 0, 704, 100
37638, V, 1, 1, 1, 1, 0, 704, 100
37639, V, 1, 1, 1, 1, 0, 704, 100
37640, V, 1, 1, 1, 1, 0, 704, 100
37641, V, 1, 1, 1, 1, 0, 704, 100
37642, V, 1, 1, 1, 1, 0, 704, 100
37643, V, 1, 1, 1, 1, 0, 704, 100
37644, V, 1, 1, 1, 1, 0, 704, 100
37645, V, 1, 1, 1, 1, 0, 704, 100
37646, V, 1, 1, 1, 1, 0, 704, 100
37647, V, 1, 1, 1, 1, 0, 704, 100
37648, V, 1, 1, 1, 1, 0, 704, 100
37649, V, 1, 1, 1, 1, 0, 704, 100
37650, V, 1, 1, 1, 1, 0, 704, 100
37651, V, 1, 1, 1, 1, 0, 704, 100
37652, V, 1, 1, 1, 1, 0, 704, 100
37653, V, 1, 1, 1, 1, 0, 704, 100
37654, V, 1, 1, 1, 1, 0, 704, 100
37655, V, 1, 1, 1, 1, 0, 704, 100
37656, V, 1, 1, 1, 1, 0, 704, 100
37657, V, 1, 1, 1, 1, 0, 704, 100
37658, V, 1, 1, 1, 1, 0, 704, 100
37659, V, 1, 1, 1, 1, 0, 704, 100
37660, V, 1, 1, 1, 1, 0, 704, 100
37661, V, 1, 1, 1, 1, 0, 704, 100
37662, V, 1, 1, 1, 1, 0, 704, 100
37663, V, 1, 1, 1, 1, 0, 704, 100
37664, V, 1, 1, 1, 1, 0, 704, 100
37665, V, 1, 1, 1, 1, 0, 704, 100
37666, V, 1, 1, 1, 1, 0, 704, 100
37667, V, 1, 1, 1, 1, 0, 704, 100
37668, V, 1, 1, 1, 1, 0, 704, 100
37669, V, 1, 1, 1, 1, 0, 704, 100
37670, V, 1, 1, 1, 1, 0, 704, 100
37671, V, 1, 1, 1, 1, 0, 704, 100
37672, V, 1, 1, 1, 1, 0, 704, 100
37673, V, 1, 1, 1, 1, 0, 704, 100
37675, V, 1, 1, 1, 1, 0, 704, 100
37676, V, 1, 1, 1, 1, 0, 704, 100
37677, V, 1, 1, 1, 1, 0, 704, 100
37678, V, 1, 1, 1, 1, 0, 704, 100
37679, V, 1, 1, 1, 1, 0, 704, 100
37680, V, 1, 1, 1, 1, 0, 704, 100
37681, V, 1, 1, 1, 1, 0, 704, 100
37682, V, 1, 1, 1, 1, 0, 704, 100
37683, V, 1, 1, 1, 1, 0, 704, 100
37684, V, 1, 1, 1, 1, 0, 704, 100
37685, V, 1, 1, 1, 1, 0, 704, 100
37686, V, 1, 1, 1, 1, 0, 704, 100
37687, V, 1, 1, 1, 1, 0, 704, 100
37688, V, 1, 1, 1, 1, 0, 704, 100
37689, V, 1, 1, 1, 1, 0, 704, 100
37690, V, 1, 1, 1, 1, 0, 704, 100
37691, V, 1, 1, 1, 1, 0, 704, 100
37692, V, 1, 1, 1, 1, 0, 704, 100
37693, V, 1, 1, 1, 1, 0, 704, 100
37694, V, 1, 1, 1, 1, 0, 704, 100
37695, V, 1, 1, 1, 1, 0, 704, 100
37696, V, 1, 1, 1, 1, 0, 704, 100
37697, V, 1, 1, 1, 1, 0, 704, 100
37698, V, 1, 1, 1, 1, 0, 704, 100
37699, V, 1, 1, 1, 1, 0, 704, 100
37700, V, 1, 1, 1, 1, 0, 704, 100
37701, V, 1, 1, 1, 1, 0, 704, 100
37702, V, 1, 1, 1, 1, 0, 704, 100
37703, V, 1, 1, 1, 1, 0, 704, 99
37704, V, 1, 1, 1, 1, 0, 704, 100
37705, V, 1, 1, 1, 1, 0, 704, 99
37706, V, 1, 1, 1, 1, 0, 704, 100
37707, V, 1, 1, 1, 1, 0, 704, 100
37708, V, 1, 1, 1, 1, 0, 704, 99
37709, V, 1, 1, 1, 1, 0, 704, 100
37710, V, 1, 1, 1, 1, 0, 704, 100
37711, V, 1, 1, 1, 1, 0, 704, 100
37712, V, 1, 1, 1, 1, 0, 704, 100
37713, V, 1, 1, 1, 1, 0, 704, 100
37714, V, 1, 1, 1, 1, 0, 704, 100
37715, V, 1, 1, 1, 1, 0, 704, 100
37716, V, 1, 1, 1, 1, 0, 704, 100
37718, V, 1, 1, 1, 1, 0, 704, 100
37719, V, 1, 1, 1, 1, 0, 704, 100
37720, V, 1, 1, 1, 1, 0, 704, 100
37721, V, 1, 1, 1, 1, 0, 704, 100
37722, V, 1, 1, 1, 1, 0, 704, 100
37723, V, 1, 1, 1, 1, 0, 704, 100
37724, V, 1, 1, 1, 1, 0, 704, 100
37725, V, 1, 1, 1, 1, 0, 704, 100
37726, V, 1, 1, 1, 1, 0, 704, 100
37727, V, 1, 1, 1, 1, 0, 704, 100
37728, V, 1, 1, 1, 1, 0, 704, 100
37729, V, 1, 1, 1, 1, 0, 704, 100
37730, V, 1, 1, 1, 1, 0, 704, 100
37731, V, 1, 1, 1, 1, 0, 704, 100
37732, V, 1, 1, 1, 1, 0, 704, 100
37733, V, 1, 1, 1, 1, 0, 704, 100
37734, V, 1, 1, 1, 1, 0, 704, 100
37735, V, 1, 1, 1, 1, 0, 704, 100
37736, V, 1, 1, 1, 1, 0, 704, 100
37737, V, 1, 1, 1, 1, 0, 704, 100
37738, V, 1, 1, 1, 1, 0, 704, 100
37739, V, 1, 1, 1, 1, 0, 704, 100
37740, V, 1, 1, 1, 1, 0, 704, 100
37741, V, 1, 1, 1, 1, 0, 704, 100
37742, V, 1, 1, 1, 1, 0, 704, 100
37743, V, 1, 1, 1, 1, 0, 704, 100
37744, V, 1, 1, 1, 1, 0, 704, 100
37745, V, 1, 1, 1, 1, 0, 704, 100
37746, V, 1, 1, 1, 1, 0, 704, 100
37747, V, 1, 1, 1, 1, 0, 704, 100
37748, V, 1, 1, 1, 1, 0, 704, 100
37749, V, 1, 1, 1, 1, 0, 704, 100
37750, V, 1, 1, 1, 1, 0, 704, 100
37751, V, 1, 1, 1, 1, 0, 704, 100
37752, V, 1, 1, 1, 1, 0, 704, 100
37753, V, 1, 1, 1, 1, 0, 704, 100
37754, V, 1, 1, 1, 1, 0, 704, 100
37755, V, 1, 1, 1, 1, 0, 704, 100
37756, V, 1, 1, 1, 1, 0, 704, 100
37757, V, 1, 1, 1, 1, 0, 704, 100
37758, V, 1, 1, 1, 1, 0, 704, 100
37760, V, 1, 1, 1, 1, 0, 704, 100
37761, V, 1, 1, 1, 1, 0, 704, 100
37762, V, 1, 1, 1, 1, 0, 704, 100
37763, V, 1, 1, 1, 1, 0, 704, 100
37764, V, 1, 1, 1, 1, 0, 704, 100
37765, V, 1, 1, 1, 1, 0, 704, 100
37766, V, 1, 1, 1, 1, 0, 704, 100
37767, V, 1, 1, 1, 1, 0, 704, 100
37768, V, 1, 1, 1, 1, 0, 704, 100
37769, V, 1, 1, 1, 1, 0, 704, 100
37770, V, 1, 1, 1, 1, 0, 704, 100
37771, V, 1, 1, 1, 1, 0, 704, 100
37772, V, 1, 1, 1, 1, 0, 704, 100
37773, V, 1, 1, 1, 1, 0, 704, 100
37774, V, 1, 1, 1, 1, 0, 704, 100
37775, V, 1, 1, 1, 1, 0, 704, 100
37776, V, 1, 1, 1, 1, 0, 704, 100
37777, V, 1, 1, 1, 1, 0, 704, 99
37778, V, 1, 1, 1, 1, 0, 704, 100
37779, V, 1, 1, 1, 1, 0, 704, 100
37780, V, 1, 1, 1, 1, 0, 704, 100
37781, V, 1, 1, 1, 1, 0, 704, 99
37782, V, 1, 1, 1, 1, 0, 704, 100
37783, V, 1, 1, 1, 1, 0, 704, 100
37784, V, 1, 1, 1, 1, 0, 704, 100
37785, V, 1, 1, 1, 1, 0, 704, 100
37786, V, 1, 1, 1, 1, 0, 704, 100
37787, V, 1, 1, 1, 1, 0, 704, 100
37788, V, 1, 1, 1, 1, 0, 704, 100
37789, V, 1, 1, 1, 1, 0, 704, 100
37790, V, 1, 1, 1, 1, 0, 704, 100
37791, V, 1, 1, 1, 1, 0, 704, 100
37792, V, 1, 1, 1, 1, 0, 704, 100
37793, V, 1, 1, 1, 1, 0, 704, 100
37794, V, 1, 1, 1, 1, 0, 704, 100
37795, V, 1, 1, 1, 1, 0, 704, 100
37796, V, 1, 1, 1, 1, 0, 704, 100
37797, V, 1, 1, 1, 1, 0, 704, 100
37798, V, 1, 1, 1, 1, 0, 704, 100
37799, V, 1, 1, 1, 1, 0, 704, 100
37800, V, 1, 1, 1, 1, 0, 704, 100
37801, V, 1, 1, 1, 1, 0, 704, 100
37803, V, 1, 1, 1, 1, 0, 704, 100
37804, V, 1, 1, 1, 1, 0, 704, 100
37805, V, 1, 1, 1, 1, 0, 704, 100
37806, V, 1, 1, 1, 1, 0, 704, 100
37807, V, 1, 1, 1, 1, 0, 704, 100
37808, V, 1, 1, 1, 1, 0, 704, 100
37809, V, 1, 1, 1, 1, 0, 704, 100
37810, V, 1, 1, 1, 1, 0, 704, 100
37811, V, 1, 1, 1, 1, 0, 704, 100
37812, V, 1, 1, 1, 1, 0, 704, 100
37813, V, 1, 1, 1, 1, 0, 704, 100
37814, V, 1, 1, 1, 1, 0, 704, 100
37815, V, 1, 1, 1, 1, 0, 704, 100
37816, V, 1, 1, 1, 1, 0, 704, 100
37817, V, 1, 1, 1, 1, 0, 704, 100
37818, V, 1, 1, 1, 1, 0, 704, 100
37819, V, 1, 1, 1, 1, 0, 704, 100
37820, V, 1, 1, 1, 1, 0, 704, 100
37821, V, 1, 1, 1, 1, 0, 704, 100
37822, V, 1, 1, 1, 1, 0, 704, 100
37823, V, 1, 1, 1, 1, 0, 704, 100
37824, V, 1, 1, 1, 1, 0, 704, 100
37825, V, 1, 1, 1, 1, 0, 704, 100
37826, V, 1, 1, 1, 1, 0, 704, 100
37827, V, 1, 1, 1, 1, 0, 704, 100
37828, V, 1, 1, 1, 1, 0, 704, 100
37829, V, 1, 1, 1, 1, 0, 704, 100
37830, V, 1, 1, 1, 1, 0, 704, 100
37831, V, 1, 1, 1, 1, 0, 704, 100
37832, V, 1, 1, 1, 1, 0, 704, 100
37833, V, 1, 1, 1, 1, 0, 704, 100
37834, V, 1, 1, 1, 1, 0, 704, 100
37835, V, 1, 1, 1, 1, 0, 704, 100
37836, V, 1, 1, 1, 1, 0, 704, 100
37837, V, 1, 1, 1, 1, 0, 704, 100
37838, V, 1, 1, 1, 1, 0, 704, 100
37839, V, 1, 1, 1, 1, 0, 704, 100
37840, V, 1, 1, 1, 1, 0, 704, 100
37841, V, 1, 1, 1, 1, 0, 704, 100
37842, V, 1, 1, 1, 1, 0, 704, 100
37843, V, 1, 1, 1, 1, 0, 704, 100
37844, V, 1, 1, 1, 1, 0, 704, 100
37846, V, 1, 1, 1, 1, 0, 704, 100
37847, V, 1, 1, 1, 1, 0, 704, 100
37848, V, 1, 1, 1, 1, 0, 704, 100
37849, V, 1, 1, 1, 1, 0, 704, 100
37850, V, 1, 1, 1, 1, 0, 704, 100
37851, V, 1, 1, 1, 1, 0, 704, 100
37852, V, 1, 1, 1, 1, 0, 704, 100
37853, V, 1, 1, 1, 1, 0, 704, 100
37854, V, 1, 1, 1, 1, 0, 704, 100
37855, V, 1, 1, 1, 1, 0, 704, 100
37856, V, 1, 1, 1, 1, 0, 704, 100
37857, V, 1, 1, 1, 1, 0, 704, 100
37858, V, 1, 1, 1, 1, 0, 704, 100
37859, V, 1, 1, 1, 1, 0, 704, 100
37860, V, 1, 1, 1, 1, 0, 704, 100
37861, V, 1, 1, 1, 1, 0, 704, 100
37862, V, 1, 1, 1, 1, 0, 704, 99
37863, V, 1, 1, 1, 1, 0, 704, 100
37864, V, 1, 1, 1, 1, 0, 704, 100
37865, V, 1, 1, 1, 1, 0, 704, 100
37866, V, 1, 1, 1, 1, 0, 704, 100
37867, V, 1, 1, 1, 1, 0, 704, 100
37868, V, 1, 1, 1, 1, 0, 704, 100
37869, V, 1, 1, 1, 1, 0, 704, 100
37870, V, 1, 1, 1, 1, 0, 704, 100
37871, V, 1, 1, 1, 1, 0, 704, 100
37872, V, 1, 1, 1, 1, 0, 704, 100
37873, V, 1, 1, 1, 1, 0, 704, 100
37874, V, 1, 1, 1, 1, 0, 704, 100
37875, V, 1, 1, 1, 1, 0, 704, 100
37876, V, 1, 1, 1, 1, 0, 704, 100
37877, V, 1, 1, 1, 1, 0, 704, 100
37878, V, 1, 1, 1, 1, 0, 704, 100
37879, V, 1, 1, 1, 1, 0, 704, 100
37880, V, 1, 1, 1, 1, 0, 704, 100
37881, V, 1, 1, 1, 1, 0, 704, 100
37882, V, 1, 1, 1, 1, 0, 704, 100
37883, V, 1, 1, 1, 1, 0, 704, 100
37884, V, 1, 1, 1, 1, 0, 704, 100
37885, V, 1, 1, 1, 1, 0, 704, 100
37886, V, 1, 1, 1, 1, 0, 704, 100
37888, V, 1, 1, 1, 1, 0, 704, 100
37889, V, 1, 1, 1, 1, 0, 704, 100
37890, V, 1, 1, 1, 1, 0, 704, 100
37891, V, 1, 1, 1, 1, 0, 704, 100
37892, V, 1, 1, 1, 1, 0, 704, 100
37893, V, 1, 1, 1, 1, 0, 704, 100
37894, V, 1, 1, 1, 1, 0, 704, 100
37895, V, 1, 1, 1, 1, 0, 704, 100
37896, V, 1, 1, 1, 1, 0, 704, 100
37897, V, 1, 1, 1, 1, 0, 704, 100
37898, V, 1, 1, 1, 1, 0, 704, 100
37899, V, 1, 1, 1, 1, 0, 704, 100
37900, V, 1, 1, 1, 1, 0, 704, 100
37901, V, 1, 1, 1, 1, 0, 704, 100
37902, V, 1, 1, 1, 1, 0, 704, 100
37903, V, 1, 1, 1, 1, 0, 704, 100
37904, V, 1, 1, 1, 1, 0, 704, 100
37905, V, 1, 1, 1, 1, 0, 704, 100
37906, V, 1, 1, 1, 1, 0, 704, 100
37907, V, 1, 1, 1, 1, 0, 704, 100
37908, V, 1, 1, 1, 1, 0, 704, 100
37909, V, 1, 1, 1, 1, 0, 704, 100
37910, V, 1, 1, 1, 1, 0, 704, 100
37911, V, 1, 1, 1, 1, 0, 704, 100
37912, V, 1, 1, 1, 1, 0, 704, 100
37913, V, 1, 1, 1, 1, 0, 704, 100
37914, V, 1, 1, 1, 1, 0, 704, 100
37915, V, 1, 1, 1, 1, 0, 704, 100
37916, V, 1, 1, 1, 1, 0, 704, 100
37917, V, 1, 1, 1, 1, 0, 704, 100
37918, V, 1, 1, 1, 1, 0, 704, 100
37919, V, 1, 1, 1, 1, 0, 704, 100
37920, V, 1, 1, 1, 1, 0, 704, 100
37921, V, 1, 1, 1, 1, 0, 704, 100
37922, V, 1, 1, 1, 1, 0, 704, 100
37923, V, 1, 1, 1, 1, 0, 704, 100
37924, V, 1, 1, 1, 1, 0, 704, 100
37925, V, 1, 1, 1, 1, 0, 704, 100
37926, V, 1, 1, 1, 1, 0, 704, 100
37927, V, 1, 1, 1, 1, 0, 704, 100
37928, V, 1, 1, 1, 1, 0, 704, 100
37929, V, 1, 1, 1, 1, 0, 704, 100
37931, V, 1, 1, 1, 1, 0, 704, 100
37932, V, 1, 1, 1, 1, 0, 704, 100
37933, V, 1, 1, 1, 1, 0, 704, 100
37934, V, 1, 1, 1, 1, 0, 704, 100
37935, V, 1, 1, 1, 1, 0, 704, 100
37936, V, 1, 1, 1, 1, 0, 704, 100
37937, V, 1, 1, 1, 1, 0, 704, 100
37938, V, 1, 1, 1, 1, 0, 704, 100
37939, V, 1, 1, 1, 1, 0, 704, 100
37940, V, 1, 1, 1, 1, 0, 704, 100
37941, V, 1, 1, 1, 1, 0, 704, 99
37942, V, 1, 1, 1, 1, 0, 704, 99
37943, V, 1, 1, 1, 1, 0, 704, 100
37944, V, 1, 1, 1, 1, 0, 704, 100
37945, V, 1, 1, 1, 1, 0, 704, 100
37946, V, 1, 1, 1, 1, 0, 704, 100
37947, V, 1, 1, 1, 1, 0, 704, 100
37948, V, 1, 1, 1, 1, 0, 704, 100
37949, V, 1, 1, 1, 1, 0, 704, 100
37950, V, 1, 1, 1, 1, 0, 704, 100
37951, V, 1, 1, 1, 1, 0, 704, 100
37952, V, 1, 1, 1, 1, 0, 704, 100
37953, V, 1, 1, 1, 1, 0, 704, 100
37954, V, 1, 1, 1, 1, 0, 704, 100
37955, V, 1, 1, 1, 1, 0, 704, 100
37956, V, 1, 1, 1, 1, 0, 704, 100
37957, V, 1, 1, 1, 1, 0, 704, 100
37958, V, 1, 1, 1, 1, 0, 704, 100
37959, V, 1, 1, 1, 1, 0, 704, 100
37960, V, 1, 1, 1, 1, 0, 704, 100
37961, V, 1, 1, 1, 1, 0, 704, 100
37962, V, 1, 1, 1, 1, 0, 704, 100
37963, V, 1, 1, 1, 1, 0, 704, 100
37964, V, 1, 1, 1, 1, 0, 704, 100
37965, V, 1, 1, 1, 1, 0, 704, 100
37966, V, 1, 1, 1, 1, 0, 704, 100
37967, V, 1, 1, 1, 1, 0, 704, 100
37968, V, 1, 1, 1, 1, 0, 704, 100
37969, V, 1, 1, 1, 1, 0, 704, 100
37970, V, 1, 1, 1, 1, 0, 704, 100
37971, V, 1, 1, 1, 1, 0, 704, 100
37972, V, 1, 1, 1, 1, 0, 704, 100
37974, V, 1, 1, 1, 1, 0, 704, 100
37975, V, 1, 1, 1, 1, 0, 704, 100
37976, V, 1, 1, 1, 1, 0, 704, 100
37977, V, 1, 1, 1, 1, 0, 704, 100
37978, V, 1, 1, 1, 1, 0, 704, 100
37979, V, 1, 1, 1, 1, 0, 704, 100
37980, V, 1, 1, 1, 1, 0, 704, 100
37981, V, 1, 1, 1, 1, 0, 704, 100
37982, V, 1, 1, 1, 1, 0, 704, 100
37983, V, 1, 1, 1, 1, 0, 704, 100
37984, V, 1, 1, 1, 1, 0, 704, 100
37985, V, 1, 1, 1, 1, 0, 704, 100
37986, V, 1, 1, 1, 1, 0, 704, 100
37987, V, 1, 1, 1, 1, 0, 704, 100
37988, V, 1, 1, 1, 1, 0, 704, 100
37989, V, 1, 1, 1, 1, 0, 704, 100
37990, V, 1, 1, 1, 1, 0, 704, 100
37991, V, 1, 1, 1, 1, 0, 704, 100
37992, V, 1, 1, 1, 1, 0, 704, 100
37993, V, 1, 1, 1, 1, 0, 704, 100
37994, V, 1, 1, 1, 1, 0, 704, 100
37995, V, 1, 1, 1, 1, 0, 704, 100
37996, V, 1, 1, 1, 1, 0, 704, 99
37997, V, 1, 1, 1, 1, 0, 704, 100
37998, V, 1, 1, 1, 1, 0, 704, 100
37999, V, 1, 1, 1, 1, 0, 704, 99
38000, V, 1, 1, 1, 1, 0, 704, 100
38001, V, 1, 1, 1, 1, 0, 704, 99
38002, V, 1, 1, 1, 1, 0, 704, 99
38003, V, 1, 1, 1, 1, 0, 704, 100
38004, V, 1, 1, 1, 1, 0, 704, 100
38005, V, 1, 1, 1, 1, 0, 704, 100
38006, V, 1, 1, 1, 1, 0, 704, 99
38007, V, 1, 1, 1, 1, 0, 704, 99
38008, V, 1, 1, 1, 1, 0, 704, 99
38009, V, 1, 1, 1, 1, 0, 704, 100
38010, V, 1, 1, 1, 1, 0, 704, 100
38011, V, 1, 1, 1, 1, 0, 704, 99
38012, V, 1, 1, 1, 1, 0, 704, 99
38013, V, 1, 1, 1, 1, 0, 704, 100
38014, V, 1, 1, 1, 1, 0, 704, 99
38016, V, 1, 1, 1, 1, 0, 704, 100
38017, V, 1, 1, 1, 1, 0, 704, 100
38018, V, 1, 1, 1, 1, 0, 704, 100
38019, V, 1, 1, 1, 1, 0, 704, 99
38020, V, 1, 1, 1, 1, 0, 704, 99
38021, V, 1, 1, 1, 1, 0, 704, 99
38022, V, 1, 1, 1, 1, 0, 704, 100
38023, V, 1, 1, 1, 1, 0, 704, 100
38024, V, 1, 1, 1, 1, 0, 704, 100
38025, V, 1, 1, 1, 1, 0, 704, 100
38026, V, 1, 1, 1, 1, 0, 704, 100
38027, V, 1, 1, 1, 1, 0, 704, 100
38028, V, 1, 1, 1, 1, 0, 704, 100
38029, V, 1, 1, 1, 1, 0, 704, 100
38030, V, 1, 1, 1, 1, 0, 704, 100
38031, V, 1, 1, 1, 1, 0, 704, 100
38032, V, 1, 1, 1, 1, 0, 704, 100
38033, V, 1, 1, 1, 1, 0, 704, 100
38034, V, 1, 1, 1, 1, 0, 704, 100
38035, V, 1, 1, 1, 1, 0, 704, 100
38036, V, 1, 1, 1, 1, 0, 704, 100
38037, V, 1, 1, 1, 1, 0, 704, 100
38038, V, 1, 1, 1, 1, 0, 704, 100
38039, V, 1, 1, 1, 1, 0, 704, 100
38040, V, 1, 1, 1, 1, 0, 704, 100
38041, V, 1, 1, 1, 1, 0, 704, 100
38042, V, 1, 1, 1, 1, 0, 704, 100
38043, V, 1, 1, 1, 1, 0, 704, 100
38044, V, 1, 1, 1, 1, 0, 704, 100
38045, V, 1, 1, 1, 1, 0, 704, 100
38046, V, 1, 1, 1, 1, 0, 704, 100
38047, V, 1, 1, 1, 1, 0, 704, 100
38048, V, 1, 1, 1, 1, 0, 704, 100
38049, V, 1, 1, 1, 1, 0, 704, 100
38050, V, 1, 1, 1, 1, 0, 704, 100
38051, V, 1, 1, 1, 1, 0, 704, 100
38052, V, 1, 1, 1, 1, 0, 704, 100
38053, V, 1, 1, 1, 1, 0, 704, 100
38054, V, 1, 1, 1, 1, 0, 704, 100
38055, V, 1, 1, 1, 1, 0, 704, 100
38056, V, 1, 1, 1, 1, 0, 704, 100
38057, V, 1, 1, 1, 1, 0, 704, 100
38059, V, 1, 1, 1, 1, 0, 704, 100
38060, V, 1, 1, 1, 1, 0, 704, 100
38061, V, 1, 1, 1, 1, 0, 704, 100
38062, V, 1, 1, 1, 1, 0, 704, 100
38063, V, 1, 1, 1, 1, 0, 704, 100
38064, V, 1, 1, 1, 1, 0, 704, 100
38065, V, 1, 1, 1, 1, 0, 704, 100
38066, V, 1, 1, 1, 1, 0, 704, 100
38067, V, 1, 1, 1, 1, 0, 704, 100
38068, V, 1, 1, 1, 1, 0, 704, 100
38069, V, 1, 1, 1, 1, 0, 704, 100
38070, V, 1, 0, 0, 1, 0, 704, 100
38070, V, 1, 0, 0, 0, 0, 704, 100
38071, V, 1, 1, 0, 0, 0, 704, 100
38071, V, 1, 1, 0, 0, 0, 704, 100
38072, V, 1, 1, 1, 1, 0, 704, 100
38073, V, 1, 1, 1, 1, 0, 704, 100
38074, V, 1, 1, 1, 1, 0, 704, 99
38075, V, 1, 1, 1, 1, 0, 704, 99
38076, V, 1, 1, 1, 1, 0, 704, 99
38077, V, 1, 1, 1, 1, 0, 704, 99
38078, V, 1, 1, 1, 1, 0, 704, 99
38079, V, 1, 1, 1, 1, 0, 704, 99
38080, V, 1, 1, 1, 1, 0, 704, 99
38081, V, 1, 1, 1, 1, 0, 704, 99
38082, V, 1, 1, 1, 1, 0, 704, 99
38083, V, 1, 1, 1, 1, 0, 704, 99
38084, V, 1, 1, 1, 1, 0, 704, 99
38085, V, 1, 1, 1, 1, 0, 704, 99
38086, V, 1, 1, 1, 1, 0, 704, 99
38087, V, 1, 1, 1, 1, 0, 704, 99
38088, V, 1, 1, 1, 1, 0, 704, 99
38089, V, 1, 1, 1, 1, 0, 704, 99
38090, V, 1, 1, 1, 1, 0, 704, 99
38091, V, 1, 1, 1, 1, 0, 704, 99
38092, V, 1, 1, 1, 1, 0, 704, 99
38093, V, 1, 1, 1, 1, 0, 704, 99
38094, V, 1, 1, 1, 1, 0, 704, 99
38095, V, 1, 1, 1, 1, 0, 704, 99
38096, V, 1, 1, 1, 1, 0, 704, 99
38097, V, 1, 1, 1, 1, 0, 704, 99
38098, V, 1, 1, 1, 1, 0, 704, 99
38099, V, 1, 1, 1, 1, 0, 704, 99
38100, V, 1, 1, 1, 1, 0, 704, 99
38102, V, 1, 1, 1, 1, 0, 704, 99
38103, V, 1, 1, 1, 1, 0, 704, 99
38104, V, 1, 1, 1, 1, 0, 704, 99
38105, V, 1, 1, 1, 1, 0, 704, 99
38106, V, 1, 1, 1, 1, 0, 704, 99
38107, V, 1, 1, 1, 1, 0, 704, 99
38108, V, 1, 1, 1, 1, 0, 704, 99
38109, V, 1, 1, 1, 1, 0, 704, 99
38110, V, 1, 1, 1, 1, 0, 704, 99
38111, V, 1, 1, 1, 1, 0, 704, 99
38112, V, 1, 1, 1, 1, 0, 704, 99
38113, V, 1, 1, 1, 1, 0, 704, 99
38114, V, 1, 1, 1, 1, 0, 704, 99
38115, V, 1, 1, 1, 1, 0, 704, 99
38116, V, 1, 1, 1, 1, 0, 704, 99
38117, V, 1, 1, 1, 1, 0, 704, 99
38118, V, 1, 1, 1, 1, 0, 704, 99
38119, V, 1, 1, 1, 1, 0, 704, 99
38120, V, 1, 1, 1, 1, 0, 704, 99
38121, V, 1, 1, 1, 1, 0, 704, 99
38122, V, 1, 1, 1, 1, 0, 704, 99
38123, V, 1, 1, 1, 1, 0, 704, 99
38124, V, 1, 1, 1, 1, 0, 704, 99
38125, V, 1, 1, 1, 1, 0, 704, 99
38126, V, 1, 1, 1, 1, 0, 704, 99
38127, V, 1, 1, 1, 1, 0, 704, 99
38128, V, 1, 1, 1, 1, 0, 704, 99
38129, V, 1, 1, 1, 1, 0, 704, 99
38130, V, 1, 1, 1, 1, 0, 704, 99
38131, V, 1, 1, 1, 1, 0, 704, 99
38132, V, 1, 1, 1, 1, 0, 704, 99
38133, V, 1, 1, 1, 1, 0, 704, 99
38134, V, 1, 1, 1, 1, 0, 704, 99
38135, V, 1, 1, 1, 1, 0, 704, 99
38136, V, 1, 1, 1, 1, 0, 704, 99
38137, V, 1, 1, 1, 1, 0, 704, 99
38138, V, 1, 1, 1, 1, 0, 704, 99
38139, V, 1, 1, 1, 1, 0, 704, 99
38140, V, 1, 1, 1, 1, 0, 704, 99
38141, V, 1, 1, 1, 1, 0, 704, 99
38142, V, 1, 1, 1, 1, 0, 704, 99
38144, V, 1, 1, 1, 1, 0, 704, 99
38145, V, 1, 1, 1, 1, 0, 704, 99
38146, V, 1, 1, 1, 1, 0, 704, 99
38147, V, 1, 1, 1, 1, 0, 704, 99
38148, V, 1, 1, 1, 1, 0, 704, 99
38149, V, 1, 1, 1, 1, 0, 704, 99
38150, V, 1, 1, 1, 1, 0, 704, 99
38151, V, 1, 1, 1, 1, 0, 704, 99
38152, V, 1, 1, 1, 1, 0, 704, 99
38153, V, 1, 1, 1, 1, 0, 704, 99
38154, V, 1, 1, 1, 1, 0, 704, 99
38155, V, 1, 1, 1, 1, 0, 704, 99
38156, V, 1, 1, 1, 1, 0, 704, 99
38157, V, 1, 1, 1, 1, 0, 704, 99
38158, V, 1, 1, 1, 1, 0, 704, 99
38159, V, 1, 1, 1, 1, 0, 704, 99
38160, V, 1, 1, 1, 1, 0, 704, 99
38161, V, 1, 1, 1, 1, 0, 704, 99
38162, V, 1, 1, 1, 1, 0, 704, 99
38163, V, 1, 1, 1, 1, 0, 704, 99
38164, V, 1, 1, 1, 1, 0, 704, 99
38165, V, 1, 1, 1, 1, 0, 704, 99
38166, V, 1, 1, 1, 1, 0, 704, 99
38167, V, 1, 1, 1, 1, 0, 704, 99
38168, V, 1, 1, 1, 1, 0, 704, 99
38169, V, 1, 1, 1, 1, 0, 704, 99
38170, V, 1, 1, 1, 1, 0, 704, 99
38171, V, 1, 1, 1, 1, 0, 704, 99
38172, V, 1, 1, 1, 1, 0, 704, 99
38173, V, 1, 1, 1, 1, 0, 704, 99
38174, V, 1, 1, 1, 1, 0, 704, 99
38175, V, 1, 1, 1, 1, 0, 704, 99
38176, V, 1, 1, 1, 1, 0, 704, 99
38177, V, 1, 1, 1, 1, 0, 704, 99
38178, V, 1, 1, 1, 1, 0, 704, 99
38179, V, 1, 1, 1, 1, 0, 704, 99
38180, V, 1, 1, 1, 1, 0, 704, 99
38181, V, 1, 1, 1, 1, 0, 704, 99
38182, V, 1, 1, 1, 1, 0, 704, 99
38183, V, 1, 1, 1, 1, 0, 704, 99
38184, V, 1, 1, 1, 1, 0, 704, 99
38185, V, 1, 1, 1, 1, 0, 704, 99
38187, V, 1, 1, 1, 1, 0, 704, 99
38188, V, 1, 1, 1, 1, 0, 704, 99
38189, V, 1, 1, 1, 1, 0, 704, 99
38190, V, 1, 1, 1, 1, 0, 704, 99
38191, V, 1, 1, 1, 1, 0, 704, 99
38192, V, 1, 1, 1, 1, 0, 704, 100
38193, V, 1, 1, 1, 1, 0, 704, 100
38194, V, 1, 1, 1, 1, 0, 704, 100
38195, V, 1, 1, 1, 1, 0, 704, 100
38196, V, 1, 1, 1, 1, 0, 704, 99
38197, V, 1, 1, 1, 1, 0, 704, 100
38198, V, 1, 1, 1, 1, 0, 704, 100
38199, V, 1, 1, 1, 1, 0, 704, 100
38200, V, 1, 1, 1, 1, 0, 704, 100
38201, V, 1, 1, 1, 1, 0, 704, 99
38202, V, 1, 1, 1, 1, 0, 704, 100
38203, V, 1, 1, 1, 1, 0, 704, 100
38204, V, 1, 1, 1, 1, 0, 704, 100
38205, V, 1, 1, 1, 1, 0, 704, 100
38206, V, 1, 1, 1, 1, 0, 704, 100
38207, V, 1, 1, 1, 1, 0, 704, 100
38208, V, 1, 1, 1, 1, 0, 704, 100
38209, V, 1, 1, 1, 1, 0, 704, 100
38210, V, 1, 1, 1, 1, 0, 704, 100
38211, V, 1, 1, 1, 1, 0, 704, 100
38212, V, 1, 1, 1, 1, 0, 704, 99
38213, V, 1, 1, 1, 1, 0, 704, 100
38214, V, 1, 1, 1, 1, 0, 704, 100
38215, V, 1, 1, 1, 1, 0, 704, 100
38216, V, 1, 1, 1, 1, 0, 704, 99
38217, V, 1, 1, 1, 1, 0, 704, 100
38218, V, 1, 1, 1, 1, 0, 704, 99
38219, V, 1, 1, 1, 1, 0, 704, 99
38220, V, 1, 1, 1, 1, 0, 704, 99
38221, V, 1, 1, 1, 1, 0, 704, 99
38222, V, 1, 1, 1, 1, 0, 704, 99
38223, V, 1, 1, 1, 1, 0, 704, 99
38224, V, 1, 1, 1, 1, 0, 704, 99
38225, V, 1, 1, 1, 1, 0, 704, 99
38226, V, 1, 1, 1, 1, 0, 704, 99
38227, V, 1, 1, 1, 1, 0, 704, 100
38228, V, 1, 1, 1, 1, 0, 704, 99
38230, V, 1, 1, 1, 1, 0, 704, 99
38231, V, 1, 1, 1, 1, 0, 704, 99
38232, V, 1, 1, 1, 1, 0, 704, 99
38233, V, 1, 1, 1, 1, 0, 704, 99
38234, V, 1, 1, 1, 1, 0, 704, 99
38235, V, 1, 1, 1, 1, 0, 704, 100
38236, V, 1, 1, 1, 1, 0, 704, 99
38237, V, 1, 1, 1, 1, 0, 704, 99
38238, V, 1, 1, 1, 1, 0, 704, 99
38239, V, 1, 1, 1, 1, 0, 704, 99
38240, V, 1, 1, 1, 1, 0, 704, 99
38241, V, 1, 1, 1, 1, 0, 704, 99
38242, V, 1, 1, 1, 1, 0, 704, 99
38243, V, 1, 1, 1, 1, 0, 704, 99
38244, V, 1, 1, 1, 1, 0, 704, 99
38245, V, 1, 1, 1, 1, 0, 704, 99
38246, V, 1, 1, 1, 1, 0, 704, 99
38247, V, 1, 1, 1, 1, 0, 704, 99
38248, V, 1, 1, 1, 1, 0, 704, 100
38249, V, 1, 1, 1, 1, 0, 704, 99
38250, V, 1, 1, 1, 1, 0, 704, 100
38251, V, 1, 1, 1, 1, 0, 704, 99
38252, V, 1, 1, 1, 1, 0, 704, 100
38253, V, 1, 1, 1, 1, 0, 704, 100
38254, V, 1, 1, 1, 1, 0, 704, 99
38255, V, 1, 1, 1, 1, 0, 704, 99
38256, V, 1, 1, 1, 1, 0, 704, 99
38257, V, 1, 1, 1, 1, 0, 704, 99
38258, V, 1, 1, 1, 1, 0, 704, 99
38259, V, 1, 1, 1, 1, 0, 704, 100
38260, V, 1, 1, 1, 1, 0, 704, 100
38261, V, 1, 1, 1, 1, 0, 704, 100
38262, V, 1, 1, 1, 1, 0, 704, 100
38263, V, 1, 1, 1, 1, 0, 704, 100
38264, V, 1, 1, 1, 1, 0, 704, 99
38265, V, 1, 1, 1, 1, 0, 704, 100
38266, V, 1, 1, 1, 1, 0, 704, 100
38267, V, 1, 1, 1, 1, 0, 704, 100
38268, V, 1, 1, 1, 1, 0, 704, 100
38269, V, 1, 1, 1, 1, 0, 704, 100
38270, V, 1, 1, 1, 1, 0, 704, 100
38272, V, 1, 1, 1, 1, 0, 704, 100
38273, V, 1, 1, 1, 1, 0, 704, 100
38274, V, 1, 1, 1, 1, 0, 704, 100
38275, V, 1, 1, 1, 1, 0, 704, 100
38276, V, 1, 1, 1, 1, 0, 704, 100
38277, V, 1, 1, 1, 1, 0, 704, 100
38278, V, 1, 1, 1, 1, 0, 704, 100
38279, V, 1, 1, 1, 1, 0, 704, 100
38280, V, 1, 1, 1, 1, 0, 704, 100
38281, V, 1, 1, 1, 1, 0, 704, 100
38282, V, 1, 1, 1, 1, 0, 704, 100
38283, V, 1, 1, 1, 1, 0, 704, 100
38284, V, 1, 1, 1, 1, 0, 704, 100
38285, V, 1, 1, 1, 1, 0, 704, 100
38286, V, 1, 1, 1, 1, 0, 704, 99
38287, V, 1, 1, 1, 1, 0, 704, 99
38288, V, 1, 1, 1, 1, 0, 704, 100
38289, V, 1, 1, 1, 1, 0, 704, 100
38290, V, 1, 1, 1, 1, 0, 704, 99
38291, V, 1, 1, 1, 1, 0, 704, 99
38292, V, 1, 1, 1, 1, 0, 704, 99
38293, V, 1, 1, 1, 1, 0, 704, 100
38294, V, 1, 1, 1, 1, 0, 704, 99
38295, V, 1, 1, 1, 1, 0, 704, 99
38296, V, 1, 1, 1, 1, 0, 704, 99
38297, V, 1, 1, 1, 1, 0, 704, 99
38298, V, 1, 1, 1, 1, 0, 704, 99
38299, V, 1, 1, 1, 1, 0, 704, 99
38300, V, 1, 1, 1, 1, 0, 704, 99
38301, V, 1, 1, 1, 1, 0, 704, 99
38302, V, 1, 1, 1, 1, 0, 704, 99
38303, V, 1, 1, 1, 1, 0, 704, 99
38304, V, 1, 1, 1, 1, 0, 704, 99
38305, V, 1, 1, 1, 1, 0, 704, 99
38306, V, 1, 1, 1, 1, 0, 704, 99
38307, V, 1, 1, 1, 1, 0, 704, 99
38308, V, 1, 1, 1, 1, 0, 704, 99
38309, V, 1, 1, 1, 1, 0, 704, 99
38310, V, 1, 1, 1, 1, 0, 704, 99
38311, V, 1, 1, 1, 1, 0, 704, 99
38312, V, 1, 1, 1, 1, 0, 704, 99
38313, V, 1, 1, 1, 1, 0, 704, 99
38315, V, 1, 1, 1, 1, 0, 704, 99
38316, V, 1, 1, 1, 1, 0, 704, 99
38317, V, 1, 1, 1, 1, 0, 704, 99
38318, V, 1, 1, 1, 1, 0, 704, 99
38319, V, 1, 1, 1, 1, 0, 704, 99
38320, V, 1, 1, 1, 1, 0, 704, 99
38321, V, 1, 1, 1, 1, 0, 704, 99
38322, V, 1, 1, 1, 1, 0, 704, 99
38323, V, 1, 1, 1, 1, 0, 704, 99
38324, V, 1, 1, 1, 1, 0, 704, 99
38325, V, 1, 1, 1, 1, 0, 704, 99
38326, V, 1, 1, 1, 1, 0, 704, 99
38327, V, 1, 1, 1, 1, 0, 704, 99
38328, V, 1, 1, 1, 1, 0, 704, 99
38329, V, 1, 1, 1, 1, 0, 704, 100
38330, V, 1, 1, 1, 1, 0, 704, 99
38331, V, 1, 1, 1, 1, 0, 704, 100
38332, V, 1, 1, 1, 1, 0, 704, 100
38333, V, 1, 1, 1, 1, 0, 704, 100
38334, V, 1, 1, 1, 1, 0, 704, 100
38335, V, 1, 1, 1, 1, 0, 704, 99
38336, V, 1, 1, 1, 1, 0, 704, 100
38337, V, 1, 1, 1, 1, 0, 704, 100
38338, V, 1, 1, 1, 1, 0, 704, 100
38339, V, 1, 1, 1, 1, 0, 704, 100
38340, V, 1, 1, 1, 1, 0, 704, 100
38341, V, 1, 1, 1, 1, 0, 704, 100
38342, V, 1, 1, 1, 1, 0, 704, 100
38343, V, 1, 1, 1, 1, 0, 704, 100
38344, V, 1, 1, 1, 1, 0, 704, 100
38345, V, 1, 1, 1, 1, 0, 704, 100
38346, V, 1, 1, 1, 1, 0, 704, 100
38347, V, 1, 1, 1, 1, 0, 704, 99
38348, V, 1, 1, 1, 1, 0, 704, 100
38349, V, 1, 1, 1, 1, 0, 704, 100
38350, V, 1, 1, 1, 1, 0, 704, 100
38351, V, 1, 1, 1, 1, 0, 704, 100
38352, V, 1, 1, 1, 1, 0, 704, 100
38353, V, 1, 1, 1, 1, 0, 704, 100
38354, V, 1, 1, 1, 1, 0, 704, 100
38355, V, 1, 1, 1, 1, 0, 704, 100
38356, V, 1, 1, 1, 1, 0, 704, 100
38358, V, 1, 1, 1, 1, 0, 704, 100
38359, V, 1, 1, 1, 1, 0, 704, 100
38360, V, 1, 1, 1, 1, 0, 704, 100
38361, V, 1, 1, 1, 1, 0, 704, 100
38362, V, 1, 1, 1, 1, 0, 704, 100
38363, V, 1, 1, 1, 1, 0, 704, 100
38364, V, 1, 1, 1, 1, 0, 704, 100
38365, V, 1, 1, 1, 1, 0, 704, 100
38366, V, 1, 1, 1, 1, 0, 704, 100
38367, V, 1, 1, 1, 1, 0, 704, 100
38368, V, 1, 1, 1, 1, 0, 704, 100
38369, V, 1, 1, 1, 1, 0, 704, 100
38370, V, 1, 1, 1, 1, 0, 704, 100
38371, V, 1, 1, 1, 1, 0, 704, 100
38372, V, 1, 1, 1, 1, 0, 704, 100
38373, V, 1, 1, 1, 1, 0, 704, 100
38374, V, 1, 1, 1, 1, 0, 704, 100
38375, V, 1, 1, 1, 1, 0, 704, 100
38376, V, 1, 1, 1, 1, 0, 704, 100
38377, V, 1, 1, 1, 1, 0, 704, 100
38378, V, 1, 1, 1, 1, 0, 704, 99
38379, V, 1, 1, 1, 1, 0, 704, 100
38380, V, 1, 1, 1, 1, 0, 704, 99
38381, V, 1, 1, 1, 1, 0, 704, 99
38382, V, 1, 1, 1, 1, 0, 704, 100
38383, V, 1, 1, 1, 1, 0, 704, 99
38384, V, 1, 1, 1, 1, 0, 704, 99
38385, V, 1, 1, 1, 1, 0, 704, 99
38386, V, 1, 1, 1, 1, 0, 704, 99
38387, V, 1, 1, 1, 1, 0, 704, 99
38388, V, 1, 1, 1, 1, 0, 704, 99
38389, V, 1, 1, 1, 1, 0, 704, 99
38390, V, 1, 1, 1, 1, 0, 704, 99
38391, V, 1, 1, 1, 1, 0, 704, 100
38392, V, 1, 1, 1, 1, 0, 704, 100
38393, V, 1, 1, 1, 1, 0, 704, 99
38394, V, 1, 1, 1, 1, 0, 704, 99
38395, V, 1, 1, 1, 1, 0, 704, 99
38396, V, 1, 1, 1, 1, 0, 704, 99
38397, V, 1, 1, 1, 1, 0, 704, 100
38398, V, 1, 1, 1, 1, 0, 704, 99
38400, V, 1, 1, 1, 1, 0, 704, 100
38401, V, 1, 1, 1, 1, 0, 704, 99
38402, V, 1, 1, 1, 1, 0, 704, 100
38403, V, 1, 1, 1, 1, 0, 704, 100
38404, V, 1, 1, 1, 1, 0, 704, 100
38405, V, 1, 1, 1, 1, 0, 704, 100
38406, V, 1, 1, 1, 1, 0, 704, 99
38407, V, 1, 1, 1, 1, 0, 704, 100
38408, V, 1, 1, 1, 1, 0, 704, 100
38409, V, 1, 1, 1, 1, 0, 704, 100
38410, V, 1, 1, 1, 1, 0, 704, 100
38411, V, 1, 1, 1, 1, 0, 704, 100
38412, V, 1, 1, 1, 1, 0, 704, 100
38413, V, 1, 1, 1, 1, 0, 704, 100
38414, V, 1, 1, 1, 1, 0, 704, 100
38415, V, 1, 1, 1, 1, 0, 704, 100
38416, V, 1, 1, 1, 1, 0, 704, 100
38417, V, 1, 1, 1, 1, 0, 704, 100
38418, V, 1, 1, 1, 1, 0, 704, 100
38419, V, 1, 1, 1, 1, 0, 704, 100
38420, V, 1, 1, 1, 1, 0, 704, 100
38421, V, 1, 1, 1, 1, 0, 704, 100
38422, V, 1, 1, 1, 1, 0, 704, 100
38423, V, 1, 1, 1, 1, 0, 704, 100
38424, V, 1, 1, 1, 1, 0, 704, 100
38425, V, 1, 1, 1, 1, 0, 704, 100
38426, V, 1, 1, 1, 1, 0, 704, 99
38427, V, 1, 1, 1, 1, 0, 704, 100
38428, V, 1, 1, 1, 1, 0, 704, 100
38429, V, 1, 1, 1, 1, 0, 704, 100
38430, V, 1, 1, 1, 1, 0, 704, 100
38431, V, 1, 1, 1, 1, 0, 704, 100
38432, V, 1, 1, 1, 1, 0, 704, 100
38433, V, 1, 1, 1, 1, 0, 704, 100
38434, V, 1, 1, 1, 1, 0, 704, 100
38435, V, 1, 1, 1, 1, 0, 704, 100
38436, V, 1, 1, 1, 1, 0, 704, 100
38437, V, 1, 1, 1, 1, 0, 704, 100
38438, V, 1, 1, 1, 1, 0, 704, 100
38439, V, 1, 1, 1, 1, 0, 704, 100
38440, V, 1, 1, 1, 1, 0, 704, 100
38441, V, 1, 1, 1, 1, 0, 704, 100
38443, V, 1, 1, 1, 1, 0, 704, 100
38444, V, 1, 1, 1, 1, 0, 704, 100
38445, V, 1, 1, 1, 1, 0, 704, 100
38446, V, 1, 1, 1, 1, 0, 704, 100
38447, V, 1, 1, 1, 1, 0, 704, 100
38448, V, 1, 1, 1, 1, 0, 704, 100
38449, V, 1, 1, 1, 1, 0, 704, 99
38450, V, 1, 1, 1, 1, 0, 704, 99
38451, V, 1, 1, 1, 1, 0, 704, 100
38452, V, 1, 1, 1, 1, 0, 704, 100
38453, V, 1, 1, 1, 1, 0, 704, 100
38454, V, 1, 1, 1, 1, 0, 704, 99
38455, V, 1, 1, 1, 1, 0, 704, 99
38456, V, 1, 1, 1, 1, 0, 704, 99
38457, V, 1, 1, 1, 1, 0, 704, 99
38458, V, 1, 1, 1, 1, 0, 704, 99
38459, V, 1, 1, 1, 1, 0, 704, 99
38460, V, 1, 1, 1, 1, 0, 704, 99
38461, V, 1, 1, 1, 1, 0, 704, 99
38462, V, 1, 1, 1, 1, 0, 704, 99
38463, V, 1, 1, 1, 1, 0, 704, 99
38464, V, 1, 1, 1, 1, 0, 704, 99
38465, V, 1, 1, 1, 1, 0, 704, 99
38466, V, 1, 1, 1, 1, 0, 704, 99
38467, V, 1, 1, 1, 1, 0, 704, 99
38468, V, 1, 1, 1, 1, 0, 704, 99
38469, V, 1, 1, 1, 1, 0, 704, 99
38470, V, 1, 1, 1, 1, 0, 704, 99
38471, V, 1, 1, 1, 1, 0, 704, 99
38472, V, 1, 1, 1, 1, 0, 704, 99
38473, V, 1, 1, 1, 1, 0, 704, 99
38474, V, 1, 1, 1, 1, 0, 704, 99
38475, V, 1, 1, 1, 1, 0, 704, 99
38476, V, 1, 1, 1, 1, 0, 704, 99
38477, V, 1, 1, 1, 1, 0, 704, 99
38478, V, 1, 1, 1, 1, 0, 704, 99
38479, V, 1, 1, 1, 1, 0, 704, 99
38480, V, 1, 1, 1, 1, 0, 704, 99
38481, V, 1, 1, 1, 1, 0, 704, 99
38482, V, 1, 1, 1, 1, 0, 704, 99
38483, V, 1, 1, 1, 1, 0, 704, 99
38484, V, 1, 1, 1, 1, 0, 704, 99
38486, V, 1, 1, 1, 1, 0, 704, 99
38487, V, 1, 1, 1, 1, 0, 704, 99
38488, V, 1, 1, 1, 1, 0, 704, 100
38489, V, 1, 1, 1, 1, 0, 704, 100
38490, V, 1, 1, 1, 1, 0, 704, 100
38491, V, 1, 1, 1, 1, 0, 704, 100
38492, V, 1, 1, 1, 1, 0, 704, 99
38493, V, 1, 1, 1, 1, 0, 704, 100
38494, V, 1, 1, 1, 1, 0, 704, 100
38495, V, 1, 1, 1, 1, 0, 704, 100
38496, V, 1, 1, 1, 1, 0, 704, 100
38497, V, 1, 1, 1, 1, 0, 704, 100
38498, V, 1, 1, 1, 1, 0, 704, 100
38499, V, 1, 1, 1, 1, 0, 704, 100
38500, V, 1, 1, 1, 1, 0, 704, 100
38501, V, 1, 1, 1, 1, 0, 704, 100
38502, V, 1, 1, 1, 1, 0, 704, 100
38503, V, 1, 1, 1, 1, 0, 704, 100
38504, V, 1, 1, 1, 1, 0, 704, 100
38505, V, 1, 1, 1, 1, 0, 704, 100
38506, V, 1, 1, 1, 1, 0, 704, 100
38507, V, 1, 1, 1, 1, 0, 704, 100
38508, V, 1, 1, 1, 1, 0, 704, 100
38509, V, 1, 1, 1, 1, 0, 704, 100
38510, V, 1, 1, 1, 1, 0, 704, 100
38511, V, 1, 1, 1, 1, 0, 704, 100
38512, V, 1, 1, 1, 1, 0, 704, 100
38513, V, 1, 1, 1, 1, 0, 704, 100
38514, V, 1, 1, 1, 1, 0, 704, 100
38515, V, 1, 1, 1, 1, 0, 704, 100
38516, V, 1, 1, 1, 1, 0, 704, 100
38517, V, 1, 1, 1, 1, 0, 704, 100
38518, V, 1, 1, 1, 1, 0, 704, 100
38519, V, 1, 1, 1, 1, 0, 704, 99
38520, V, 1, 1, 1, 1, 0, 704, 99
38521, V, 1, 1, 1, 1, 0, 704, 100
38522, V, 1, 1, 1, 1, 0, 704, 99
38523, V, 1, 1, 1, 1, 0, 704, 100
38524, V, 1, 1, 1, 1, 0, 704, 99
38525, V, 1, 1, 1, 1, 0, 704, 99
38526, V, 1, 1, 1, 1, 0, 704, 100
38528, V, 1, 1, 1, 1, 0, 704, 99
38529, V, 1, 1, 1, 1, 0, 704, 99
38530, V, 1, 1, 1, 1, 0, 704, 99
38531, V, 1, 1, 1, 1, 0, 704, 99
38532, V, 1, 1, 1, 1, 0, 704, 99
38533, V, 1, 1, 1, 1, 0, 704, 99
38534, V, 1, 1, 1, 1, 0, 704, 99
38535, V, 1, 1, 1, 1, 0, 704, 99
38536, V, 1, 1, 1, 1, 0, 704, 99
38537, V, 1, 1, 1, 1, 0, 704, 99
38538, V, 1, 1, 1, 1, 0, 704, 99
38539, V, 1, 1, 1, 1, 0, 704, 99
38540, V, 1, 1, 1, 1, 0, 704, 99
38541, V, 1, 1, 1, 1, 0, 704, 99
38542, V, 1, 1, 1, 1, 0, 704, 99
38543, V, 1, 1, 1, 1, 0, 704, 99
38544, V, 1, 1, 1, 1, 0, 704, 99
38545, V, 1, 1, 1, 1, 0, 704, 99
38546, V, 1, 1, 1, 1, 0, 704, 99
38547, V, 1, 1, 1, 1, 0, 704, 99
38548, V, 1, 1, 1, 1, 0, 704, 99
38549, V, 1, 1, 1, 1, 0, 704, 99
38550, V, 1, 1, 1, 1, 0, 704, 99
38551, V, 1, 1, 1, 1, 0, 704, 99
38552, V, 1, 1, 1, 1, 0, 704, 99
38553, V, 1, 1, 1, 1, 0, 704, 100
38554, V, 1, 1, 1, 1, 0, 704, 99
38555, V, 1, 1, 1, 1, 0, 704, 99
38556, V, 1, 1, 1, 1, 0, 704, 99
38557, V, 1, 1, 1, 1, 0, 704, 99
38558, V, 1, 1, 1, 1, 0, 704, 99
38559, V, 1, 1, 1, 1, 0, 704, 99
38560, V, 1, 1, 1, 1, 0, 704, 99
38561, V, 1, 1, 1, 1, 0, 704, 100
38562, V, 1, 1, 1, 1, 0, 704, 99
38563, V, 1, 1, 1, 1, 0, 704, 99
38564, V, 1, 1, 1, 1, 0, 704, 99
38565, V, 1, 1, 1, 1, 0, 704, 99
38566, V, 1, 1, 1, 1, 0, 704, 100
38567, V, 1, 1, 1, 1, 0, 704, 100
38568, V, 1, 1, 1, 1, 0, 704, 100
38569, V, 1, 1, 1, 1, 0, 704, 100
38571, V, 1, 1, 1, 1, 0, 704, 99
38572, V, 1, 1, 1, 1, 0, 704, 100
38573, V, 1, 1, 1, 1, 0, 704, 100
38574, V, 1, 1, 1, 1, 0, 704, 100
38575, V, 1, 1, 1, 1, 0, 704, 100
38576, V, 1, 1, 1, 1, 0, 704, 100
38577, V, 1, 1, 1, 1, 0, 704, 100
38578, V, 1, 1, 1, 1, 0, 704, 100
38579, V, 1, 1, 1, 1, 0, 704, 100
38580, V, 1, 1, 1, 1, 0, 704, 100
38581, V, 1, 1, 1, 1, 0, 704, 100
38582, V, 1, 1, 1, 1, 0, 704, 100
38583, V, 1, 1, 1, 1, 0, 704, 100
38584, V, 1, 1, 1, 1, 0, 704, 100
38585, V, 1, 1, 1, 1, 0, 704, 100
38586, V, 1, 1, 1, 1, 0, 704, 100
38587, V, 1, 1, 1, 1, 0, 704, 100
38588, V, 1, 1, 1, 1, 0, 704, 100
38589, V, 1, 1, 1, 1, 0, 704, 100
38590, V, 1, 1, 1, 1, 0, 704, 100
38591, V, 1, 1, 1, 1, 0, 704, 100
38592, V, 1, 1, 1, 1, 0, 704, 100
38593, V, 1, 1, 1, 1, 0, 704, 99
38594, V, 1, 1, 1, 1, 0, 704, 100
38595, V, 1, 1, 1, 1, 0, 704, 99
38596, V, 1, 1, 1, 1, 0, 704, 99
38597, V, 1, 1, 1, 1, 0, 704, 99
38598, V, 1, 1, 1, 1, 0, 704, 99
38599, V, 1, 1, 1, 1, 0, 704, 99
38600, V, 1, 1, 1, 1, 0, 704, 99
38601, V, 1, 1, 1, 1, 0, 704, 99
38602, V, 1, 1, 1, 1, 0, 704, 99
38603, V, 1, 1, 1, 1, 0, 704, 99
38604, V, 1, 1, 1, 1, 0, 704, 99
38605, V, 1, 1, 1, 1, 0, 704, 99
38606, V, 1, 1, 1, 1, 0, 704, 99
38607, V, 1, 1, 1, 1, 0, 704, 99
38608, V, 1, 1, 1, 1, 0, 704, 99
38609, V, 1, 1, 1, 1, 0, 704, 99
38610, V, 1, 1, 1, 1, 0, 704, 99
38611, V, 1, 1, 1, 1, 0, 704, 99
38612, V, 1, 1, 1, 1, 0, 704, 99
38614, V, 1, 1, 1, 1, 0, 704, 99
38615, V, 1, 1, 1, 1, 0, 704, 99
38616, V, 1, 1, 1, 1, 0, 704, 99
38617, V, 1, 1, 1, 1, 0, 704, 99
38618, V, 1, 1, 1, 1, 0, 704, 99
38619, V, 1, 1, 1, 1, 0, 704, 99
38620, V, 1, 1, 1, 1, 0, 704, 99
38621, V, 1, 1, 1, 1, 0, 704, 99
38622, V, 1, 1, 1, 1, 0, 704, 99
38623, V, 1, 1, 1, 1, 0, 704, 99
38624, V, 1, 1, 1, 1, 0, 704, 99
38625, V, 1, 1, 1, 1, 0, 704, 99
38626, V, 1, 1, 1, 1, 0, 704, 99
38627, V, 1, 1, 1, 1, 0, 704, 99
38628, V, 1, 1, 1, 1, 0, 704, 99
38629, V, 1, 1, 1, 1, 0, 704, 99
38630, V, 1, 1, 1, 1, 0, 704, 99
38631, V, 1, 1, 1, 1, 0, 704, 99
38632, V, 1, 1, 1, 1, 0, 704, 99
38633, V, 1, 1, 1, 1, 0, 704, 99
38634, V, 1, 1, 1, 1, 0, 704, 99
38635, V, 1, 1, 1, 1, 0, 704, 99
38636, V, 1, 1, 1, 1, 0, 704, 99
38637, V, 1, 1, 1, 1, 0, 704, 99
38638, V, 1, 1, 1, 1, 0, 704, 99
38639, V, 1, 1, 1, 1, 0, 704, 99
38640, V, 1, 1, 1, 1, 0, 704, 100
38641, V, 1, 1, 1, 1, 0, 704, 99
38642, V, 1, 1, 1, 1, 0, 704, 100
38643, V, 1, 1, 1, 1, 0, 704, 99
38644, V, 1, 1, 1, 1, 0, 704, 99
38645, V, 1, 1, 1, 1, 0, 704, 100
38646, V, 1, 1, 1, 1, 0, 704, 100
38647, V, 1, 1, 1, 1, 0, 704, 100
38648, V, 1, 1, 1, 1, 0, 704, 100
38649, V, 1, 1, 1, 1, 0, 704, 100
38650, V, 1, 1, 1, 1, 0, 704, 100
38651, V, 1, 1, 1, 1, 0, 704, 100
38652, V, 1, 1, 1, 1, 0, 704, 100
38653, V, 1, 1, 1, 1, 0, 704, 100
38654, V, 1, 1, 1, 1, 0, 704, 100
38656, V, 1, 1, 1, 1, 0, 704, 99
38657, V, 1, 1, 1, 1, 0, 704, 99
38658, V, 1, 1, 1, 1, 0, 704, 100
38659, V, 1, 1, 1, 1, 0, 704, 100
38660, V, 1, 1, 1, 1, 0, 704, 100
38661, V, 1, 1, 1, 1, 0, 704, 100
38662, V, 1, 1, 1, 1, 0, 704, 99
38663, V, 1, 1, 1, 1, 0, 704, 100
38664, V, 1, 1, 1, 1, 0, 704, 100
38665, V, 1, 1, 1, 1, 0, 704, 100
38666, V, 1, 1, 1, 1, 0, 704, 99
38667, V, 1, 1, 1, 1, 0, 704, 100
38668, V, 1, 1, 1, 1, 0, 704, 100
38669, V, 1, 1, 1, 1, 0, 704, 100
38670, V, 1, 1, 1, 1, 0, 704, 100
38671, V, 1, 1, 1, 1, 0, 704, 99
38672, V, 1, 1, 1, 1, 0, 704, 100
38673, V, 1, 1, 1, 1, 0, 704, 99
38674, V, 1, 1, 1, 1, 0, 704, 100
38675, V, 1, 1, 1, 1, 0, 704, 99
38676, V, 1, 1, 1, 1, 0, 704, 99
38677, V, 1, 1, 1, 1, 0, 704, 99
38678, V, 1, 1, 1, 1, 0, 704, 99
38679, V, 1, 1, 1, 1, 0, 704, 99
38680, V, 1, 1, 1, 1, 0, 704, 99
38681, V, 1, 1, 1, 1, 0, 704, 99
38682, V, 1, 1, 1, 1, 0, 704, 99
38683, V, 1, 1, 1, 1, 0, 704, 99
38684, V, 1, 1, 1, 1, 0, 704, 99
38685, V, 1, 1, 1, 1, 0, 704, 99
38686, V, 1, 1, 1, 1, 0, 704, 99
38687, V, 1, 1, 1, 1, 0, 704, 99
38688, V, 1, 1, 1, 1, 0, 704, 99
38689, V, 1, 1, 1, 1, 0, 704, 99
38690, V, 1, 1, 1, 1, 0, 704, 99
38691, V, 1, 1, 1, 1, 0, 704, 99
38692, V, 1, 1, 1, 1, 0, 704, 99
38693, V, 1, 1, 1, 1, 0, 704, 99
38694, V, 1, 1, 1, 1, 0, 704, 99
38695, V, 1, 1, 1, 1, 0, 704, 99
38696, V, 1, 1, 1, 1, 0, 704, 99
38697, V, 1, 1, 1, 1, 0, 704, 99
38699, V, 1, 1, 1, 1, 0, 704, 99
38700, V, 1, 1, 1, 1, 0, 704, 99
38701, V, 1, 1, 1, 1, 0, 704, 99
38702, V, 1, 1, 1, 1, 0, 704, 99
38703, V, 1, 1, 1, 1, 0, 704, 99
38704, V, 1, 1, 1, 1, 0, 704, 99
38705, V, 1, 1, 1, 1, 0, 704, 99
38706, V, 1, 1, 1, 1, 0, 704, 99
38707, V, 1, 1, 1, 1, 0, 704, 99
38708, V, 1, 1, 1, 1, 0, 704, 99
38709, V, 1, 1, 1, 1, 0, 704, 99
38710, V, 1, 1, 1, 1, 0, 704, 99
38711, V, 1, 1, 1, 1, 0, 704, 99
38712, V, 1, 1, 1, 1, 0, 704, 99
38713, V, 1, 1, 1, 1, 0, 704, 99
38714, V, 1, 1, 1, 1, 0, 704, 99
38715, V, 1, 1, 1, 1, 0, 704, 99
38716, V, 1, 1, 1, 1, 0, 704, 99
38717, V, 1, 1, 1, 1, 0, 704, 99
38718, V, 1, 1, 1, 1, 0, 704, 99
38719, V, 1, 1, 1, 1, 0, 704, 100
38720, V, 1, 1, 1, 1, 0, 704, 100
38721, V, 1, 1, 1, 1, 0, 704, 100
38722, V, 1, 1, 1, 1, 0, 704, 99
38723, V, 1, 1, 1, 1, 0, 704, 100
38724, V, 1, 1, 1, 1, 0, 704, 100
38725, V, 1, 1, 1, 1, 0, 704, 100
38726, V, 1, 1, 1, 1, 0, 704, 100
38727, V, 1, 1, 1, 1, 0, 704, 100
38728, V, 1, 1, 1, 1, 0, 704, 100
38729, V, 1, 1, 1, 1, 0, 704, 100
38730, V, 1, 1, 1, 1, 0, 704, 100
38731, V, 1, 1, 1, 1, 0, 704, 100
38732, V, 1, 1, 1, 1, 0, 704, 100
38733, V, 1, 1, 1, 1, 0, 704, 100
38734, V, 1, 1, 1, 1, 0, 704, 100
38735, V, 1, 1, 1, 1, 0, 704, 100
38736, V, 1, 1, 1, 1, 0, 704, 100
38737, V, 1, 1, 1, 1, 0, 704, 100
38738, V, 1, 1, 1, 1, 0, 704, 100
38739, V, 1, 1, 1, 1, 0, 704, 100
38740, V, 1, 1, 1, 1, 0, 704, 100
38742, V, 1, 1, 1, 1, 0, 704, 100
38743, V, 1, 1, 1, 1, 0, 704, 100
38744, V, 1, 1, 1, 1, 0, 704, 100
38745, V, 1, 1, 1, 1, 0, 704, 100
38746, V, 1, 1, 1, 1, 0, 704, 100
38747, V, 1, 1, 1, 1, 0, 704, 100
38748, V, 1, 1, 1, 1, 0, 704, 100
38749, V, 1, 1, 1, 1, 0, 704, 100
38750, V, 1, 1, 1, 1, 0, 704, 100
38751, V, 1, 1, 1, 1, 0, 704, 100
38752, V, 1, 1, 1, 1, 0, 704, 99
38753, V, 1, 1, 1, 1, 0, 704, 99
38754, V, 1, 1, 1, 1, 0, 704, 99
38755, V, 1, 1, 1, 1, 0, 704, 99
38756, V, 1, 1, 1, 1, 0, 704, 99
38757, V, 1, 1, 1, 1, 0, 704, 99
38758, V, 1, 1, 1, 1, 0, 704, 99
38759, V, 1, 1, 1, 1, 0, 704, 99
38760, V, 1, 1, 1, 1, 0, 704, 99
38761, V, 1, 1, 1, 1, 0, 704, 99
38762, V, 1, 1, 1, 1, 0, 704, 99
38763, V, 1, 1, 1, 1, 0, 704, 99
38764, V, 1, 1, 1, 1, 0, 704, 99
38765, V, 1, 1, 1, 1, 0, 704, 99
38766, V, 1, 1, 1, 1, 0, 704, 99
38767, V, 1, 1, 1, 1, 0, 704, 99
38768, V, 1, 1, 1, 1, 0, 704, 99
38769, V, 1, 1, 1, 1, 0, 704, 99
38770, V, 1, 1, 1, 1, 0, 704, 99
38771, V, 1, 1, 1, 1, 0, 704, 99
38772, V, 1, 1, 1, 1, 0, 704, 99
38773, V, 1, 1, 1, 1, 0, 704, 99
38774, V, 1, 1, 1, 1, 0, 704, 99
38775, V, 1, 1, 1, 1, 0, 704, 99
38776, V, 1, 1, 1, 1, 0, 704, 99
38777, V, 1, 1, 1, 1, 0, 704, 99
38778, V, 1, 1, 1, 1, 0, 704, 99
38779, V, 1, 1, 1, 1, 0, 704, 99
38780, V, 1, 1, 1, 1, 0, 704, 99
38781, V, 1, 1, 1, 1, 0, 704, 99
38782, V, 1, 1, 1, 1, 0, 704, 99
38784, V, 1, 1, 1, 1, 0, 704, 99
38785, V, 1, 1, 1, 1, 0, 704, 99
38786, V, 1, 1, 1, 1, 0, 704, 99
38787, V, 1, 1, 1, 1, 0, 704, 99
38788, V, 1, 1, 1, 1, 0, 704, 99
38789, V, 1, 1, 1, 1, 0, 704, 99
38790, V, 1, 1, 1, 1, 0, 704, 99
38791, V, 1, 1, 1, 1, 0, 704, 99
38792, V, 1, 1, 1, 1, 0, 704, 100
38793, V, 1, 1, 1, 1, 0, 704, 99
38794, V, 1, 1, 1, 1, 0, 704, 100
38795, V, 1, 1, 1, 1, 0, 704, 99
38796, V, 1, 1, 1, 1, 0, 704, 99
38797, V, 1, 1, 1, 1, 0, 704, 100
38798, V, 1, 1, 1, 1, 0, 704, 99
38799, V, 1, 1, 1, 1, 0, 704, 100
38800, V, 1, 1, 1, 1, 0, 704, 99
38801, V, 1, 1, 1, 1, 0, 704, 99
38802, V, 1, 1, 1, 1, 0, 704, 100
38803, V, 1, 1, 1, 1, 0, 704, 99
38804, V, 1, 1, 1, 1, 0, 704, 100
38805, V, 1, 1, 1, 1, 0, 704, 100
38806, V, 1, 1, 1, 1, 0, 704, 99
38807, V, 1, 1, 1, 1, 0, 704, 100
38808, V, 1, 1, 1, 1, 0, 704, 100
38809, V, 1, 1, 1, 1, 0, 704, 100
38810, V, 1, 1, 1, 1, 0, 704, 100
38811, V, 1, 1, 1, 1, 0, 704, 100
38812, V, 1, 1, 1, 1, 0, 704, 100
38813, V, 1, 1, 1, 1, 0, 704, 99
38814, V, 1, 1, 1, 1, 0, 704, 100
38815, V, 1, 1, 1, 1, 0, 704, 100
38816, V, 1, 1, 1, 1, 0, 704, 100
38817, V, 1, 1, 1, 1, 0, 704, 100
38818, V, 1, 1, 1, 1, 0, 704, 100
38819, V, 1, 1, 1, 1, 0, 704, 99
38820, V, 1, 1, 1, 1, 0, 704, 100
38821, V, 1, 1, 1, 1, 0, 704, 99
38822, V, 1, 1, 1, 1, 0, 704, 100
38823, V, 1, 1, 1, 1, 0, 704, 99
38824, V, 1, 1, 1, 1, 0, 704, 99
38825, V, 1, 1, 1, 1, 0, 704, 99
38827, V, 1, 1, 1, 1, 0, 704, 100
38828, V, 1, 1, 1, 1, 0, 704, 99
38829, V, 1, 1, 1, 1, 0, 704, 99
38830, V, 1, 1, 1, 1, 0, 704, 100
38831, V, 1, 1, 1, 1, 0, 704, 99
38832, V, 1, 1, 1, 1, 0, 704, 99
38833, V, 1, 1, 1, 1, 0, 704, 99
38834, V, 1, 1, 1, 1, 0, 704, 99
38835, V, 1, 1, 1, 1, 0, 704, 99
38836, V, 1, 1, 1, 1, 0, 704, 99
38837, V, 1, 1, 1, 1, 0, 704, 99
38838, V, 1, 1, 1, 1, 0, 704, 100
38839, V, 1, 1, 1, 1, 0, 704, 99
38840, V, 1, 1, 1, 1, 0, 704, 99
38841, V, 1, 1, 1, 1, 0, 704, 99
38842, V, 1, 1, 1, 1, 0, 704, 99
38843, V, 1, 1, 1, 1, 0, 704, 99
38844, V, 1, 1, 1, 1, 0, 704, 99
38845, V, 1, 1, 1, 1, 0, 704, 99
38846, V, 1, 1, 1, 1, 0, 704, 99
38847, V, 1, 1, 1, 1, 0, 704, 99
38848, V, 1, 1, 1, 1, 0, 704, 99
38849, V, 1, 1, 1, 1, 0, 704, 99
38850, V, 1, 1, 1, 1, 0, 704, 99
38851, V, 1, 1, 1, 1, 0, 704, 99
38852, V, 1, 1, 1, 1, 0, 704, 99
38853, V, 1, 1, 1, 1, 0, 704, 99
38854, V, 1, 1, 1, 1, 0, 704, 99
38855, V, 1, 1, 1, 1, 0, 704, 99
38856, V, 1, 1, 1, 1, 0, 704, 99
38857, V, 1, 1, 1, 1, 0, 704, 99
38858, V, 1, 1, 1, 1, 0, 704, 99
38859, V, 1, 1, 1, 1, 0, 704, 99
38860, V, 1, 1, 1, 1, 0, 704, 100
38861, V, 1, 1, 1, 1, 0, 704, 99
38862, V, 1, 1, 1, 1, 0, 704, 99
38863, V, 1, 1, 1, 1, 0, 704, 99
38864, V, 1, 1, 1, 1, 0, 704, 99
38865, V, 1, 1, 1, 1, 0, 704, 99
38866, V, 1, 1, 1, 1, 0, 704, 99
38867, V, 1, 1, 1, 1, 0, 704, 99
38868, V, 1, 1, 1, 1, 0, 704, 99
38870, V, 1, 1, 1, 1, 0, 704, 100
38871, V, 1, 1, 1, 1, 0, 704, 99
38872, V, 1, 1, 1, 1, 0, 704, 100
38873, V, 1, 1, 1, 1, 0, 704, 100
38874, V, 1, 1, 1, 1, 0, 704, 100
38875, V, 1, 1, 1, 1, 0, 704, 99
38876, V, 1, 1, 1, 1, 0, 704, 99
38877, V, 1, 1, 1, 1, 0, 704, 99
38878, V, 1, 1, 1, 1, 0, 704, 100
38879, V, 1, 1, 1, 1, 0, 704, 100
38880, V, 1, 1, 1, 1, 0, 704, 100
38881, V, 1, 1, 1, 1, 0, 704, 100
38882, V, 1, 1, 1, 1, 0, 704, 99
38883, V, 1, 1, 1, 1, 0, 704, 100
38884, V, 1, 1, 1, 1, 0, 704, 100
38885, V, 1, 1, 1, 1, 0, 704, 99
38886, V, 1, 1, 1, 1, 0, 704, 100
38887, V, 1, 1, 1, 1, 0, 704, 100
38888, V, 1, 1, 1, 1, 0, 704, 100
38889, V, 1, 1, 1, 1, 0, 704, 100
38890, V, 1, 1, 1, 1, 0, 704, 100
38891, V, 1, 1, 1, 1, 0, 704, 100
38892, V, 1, 1, 1, 1, 0, 704, 100
38893, V, 1, 1, 1, 1, 0, 704, 100
38894, V, 1, 1, 1, 1, 0, 704, 99
38895, V, 1, 1, 1, 1, 0, 704, 99
38896, V, 1, 1, 1, 1, 0, 704, 100
38897, V, 1, 1, 1, 1, 0, 704, 99
38898, V, 1, 1, 1, 1, 0, 704, 99
38899, V, 1, 1, 1, 1, 0, 704, 100
38900, V, 1, 1, 1, 1, 0, 704, 99
38901, V, 1, 1, 1, 1, 0, 704, 99
38902, V, 1, 1, 1, 1, 0, 704, 99
38903, V, 1, 1, 1, 1, 0, 704, 99
38904, V, 1, 1, 1, 1, 0, 704, 99
38905, V, 1, 1, 1, 1, 0, 704, 99
38906, V, 1, 1, 1, 1, 0, 704, 99
38907, V, 1, 1, 1, 1, 0, 704, 100
38908, V, 1, 1, 1, 1, 0, 704, 99
38909, V, 1, 1, 1, 1, 0, 704, 99
38910, V, 1, 1, 1, 1, 0, 704, 99
38912, V, 1, 1, 1, 1, 0, 704, 99
38913, V, 1, 1, 1, 1, 0, 704, 99
38914, V, 1, 1, 1, 1, 0, 704, 99
38915, V, 1, 1, 1, 1, 0, 704, 99
38916, V, 1, 1, 1, 1, 0, 704, 99
38917, V, 1, 1, 1, 1, 0, 704, 99
38918, V, 1, 1, 1, 1, 0, 704, 99
38919, V, 1, 1, 1, 1, 0, 704, 99
38920, V, 1, 1, 1, 1, 0, 704, 99
38921, V, 1, 1, 1, 1, 0, 704, 99
38922, V, 1, 1, 1, 1, 0, 704, 99
38923, V, 1, 1, 1, 1, 0, 704, 99
38924, V, 1, 1, 1, 1, 0, 704, 99
38925, V, 1, 1, 1, 1, 0, 704, 99
38926, V, 1, 1, 1, 1, 0, 704, 99
38927, V, 1, 1, 1, 1, 0, 704, 99
38928, V, 1, 1, 1, 1, 0, 704, 99
38929, V, 1, 1, 1, 1, 0, 704, 99
38930, V, 1, 1, 1, 1, 0, 704, 99
38931, V, 1, 1, 1, 1, 0, 704, 99
38932, V, 1, 1, 1, 1, 0, 704, 99
38933, V, 1, 1, 1, 1, 0, 704, 99
38934, V, 1, 1, 1, 1, 0, 704, 99
38935, V, 1, 1, 1, 1, 0, 704, 99
38936, V, 1, 1, 1, 1, 0, 704, 100
38937, V, 1, 1, 1, 1, 0, 704, 99
38938, V, 1, 1, 1, 1, 0, 704, 99
38939, V, 1, 1, 1, 1, 0, 704, 99
38940, V, 1, 1, 1, 1, 0, 704, 99
38941, V, 1, 1, 1, 1, 0, 704, 99
38942, V, 1, 1, 1, 1, 0, 704, 99
38943, V, 1, 1, 1, 1, 0, 704, 99
38944, V, 1, 1, 1, 1, 0, 704, 99
38945, V, 1, 1, 1, 1, 0, 704, 100
38946, V, 1, 1, 1, 1, 0, 704, 99
38947, V, 1, 1, 1, 1, 0, 704, 99
38948, V, 1, 1, 1, 1, 0, 704, 100
38949, V, 1, 1, 1, 1, 0, 704, 100
38950, V, 1, 1, 1, 1, 0, 704, 100
38951, V, 1, 1, 1, 1, 0, 704, 100
38952, V, 1, 1, 1, 1, 0, 704, 100
38953, V, 1, 1, 1, 1, 0, 704, 100
38955, V, 1, 1, 1, 1, 0, 704, 100
38956, V, 1, 1, 1, 1, 0, 704, 100
38957, V, 1, 1, 1, 1, 0, 704, 100
38958, V, 1, 1, 1, 1, 0, 704, 100
38959, V, 1, 1, 1, 1, 0, 704, 100
38960, V, 1, 1, 1, 1, 0, 704, 100
38961, V, 1, 1, 1, 1, 0, 704, 100
38962, V, 1, 1, 1, 1, 0, 704, 100
38963, V, 1, 1, 1, 1, 0, 704, 100
38964, V, 1, 1, 1, 1, 0, 704, 100
38965, V, 1, 1, 1, 1, 0, 704, 100
38966, V, 1, 1, 1, 1, 0, 704, 100
38967, V, 1, 1, 1, 1, 0, 704, 99
38968, V, 1, 1, 1, 1, 0, 704, 100
38969, V, 1, 1, 1, 1, 0, 704, 100
38970, V, 1, 1, 1, 1, 0, 704, 100
38971, V, 1, 1, 1, 1, 0, 704, 100
38972, V, 1, 1, 1, 1, 0, 704, 100
38973, V, 1, 1, 1, 1, 0, 704, 100
38974, V, 1, 1, 1, 1, 0, 704, 100
38975, V, 1, 1, 1, 1, 0, 704, 100
38976, V, 1, 1, 1, 1, 0, 704, 100
38977, V, 1, 1, 1, 1, 0, 704, 100
38978, V, 1, 1, 1, 1, 0, 704, 99
38979, V, 1, 1, 1, 1, 0, 704, 100
38980, V, 1, 1, 1, 1, 0, 704, 99
38981, V, 1, 1, 1, 1, 0, 704, 99
38982, V, 1, 1, 1, 1, 0, 704, 99
38983, V, 1, 1, 1, 1, 0, 704, 99
38984, V, 1, 1, 1, 1, 0, 704, 99
38985, V, 1, 1, 1, 1, 0, 704, 99
38986, V, 1, 1, 1, 1, 0, 704, 100
38987, V, 1, 1, 1, 1, 0, 704, 99
38988, V, 1, 1, 1, 1, 0, 704, 99
38989, V, 1, 1, 1, 1, 0, 704, 99
38990, V, 1, 1, 1, 1, 0, 704, 99
38991, V, 1, 1, 1, 1, 0, 704, 99
38992, V, 1, 1, 1, 1, 0, 704, 99
38993, V, 1, 1, 1, 1, 0, 704, 99
38994, V, 1, 1, 1, 1, 0, 704, 99
38995, V, 1, 1, 1, 1, 0, 704, 99
38996, V, 1, 1, 1, 1, 0, 704, 99
38998, V, 1, 1, 1, 1, 0, 704, 99
38999, V, 1, 1, 1, 1, 0, 704, 99
39000, V, 1, 1, 1, 1, 0, 704, 99
39001, V, 1, 1, 1, 1, 0, 704, 99
39002, V, 1, 1, 1, 1, 0, 704, 99
39003, V, 1, 1, 1, 1, 0, 704, 99
39004, V, 1, 1, 1, 1, 0, 704, 99
39005, V, 1, 1, 1, 1, 0, 704, 99
39006, V, 1, 1, 1, 1, 0, 704, 99
39007, V, 1, 1, 1, 1, 0, 704, 99
39008, V, 1, 1, 1, 1, 0, 704, 99
39009, V, 1, 1, 1, 1, 0, 704, 100
39010, V, 1, 1, 1, 1, 0, 704, 99
39011, V, 1, 1, 1, 1, 0, 704, 100
39012, V, 1, 1, 1, 1, 0, 704, 99
39013, V, 1, 1, 1, 1, 0, 704, 99
39014, V, 1, 1, 1, 1, 0, 704, 100
39015, V, 1, 1, 1, 1, 0, 704, 99
39016, V, 1, 1, 1, 1, 0, 704, 99
39017, V, 1, 1, 1, 1, 0, 704, 100
39018, V, 1, 1, 1, 1, 0, 704, 99
39019, V, 1, 1, 1, 1, 0, 704, 100
39020, V, 1, 1, 1, 1, 0, 704, 100
39021, V, 1, 1, 1, 1, 0, 704, 100
39022, V, 1, 1, 1, 1, 0, 704, 100
39023, V, 1, 1, 1, 1, 0, 704, 100
39024, V, 1, 1, 1, 1, 0, 704, 100
39025, V, 1, 1, 1, 1, 0, 704, 100
39026, V, 1, 1, 1, 1, 0, 704, 100
39027, V, 1, 1, 1, 1, 0, 704, 100
39028, V, 1, 1, 1, 1, 0, 704, 100
39029, V, 1, 1, 1, 1, 0, 704, 100
39030, V, 1, 1, 1, 1, 0, 704, 100
39031, V, 1, 1, 1, 1, 0, 704, 100
39032, V, 1, 1, 1, 1, 0, 704, 100
39033, V, 1, 1, 1, 1, 0, 704, 100
39034, V, 1, 1, 1, 1, 0, 704, 100
39035, V, 1, 1, 1, 1, 0, 704, 100
39036, V, 1, 1, 1, 1, 0, 704, 100
39037, V, 1, 1, 1, 1, 0, 704, 100
39038, V, 1, 1, 1, 1, 0, 704, 100
39040, V, 1, 1, 1, 1, 0, 704, 100
39041, V, 1, 1, 1, 1, 0, 704, 100
39042, V, 1, 1, 1, 1, 0, 704, 100
39043, V, 1, 1, 1, 1, 0, 704, 100
39044, V, 1, 1, 1, 1, 0, 704, 100
39045, V, 1, 1, 1, 1, 0, 704, 100
39046, V, 1, 1, 1, 1, 0, 704, 100
39047, V, 1, 1, 1, 1, 0, 704, 100
39048, V, 1, 1, 1, 1, 0, 704, 100
39049, V, 1, 1, 1, 1, 0, 704, 99
39050, V, 1, 1, 1, 1, 0, 704, 100
39051, V, 1, 1, 1, 1, 0, 704, 100
39052, V, 1, 1, 1, 1, 0, 704, 100
39053, V, 1, 1, 1, 1, 0, 704, 100
39054, V, 1, 1, 1, 1, 0, 704, 100
39055, V, 1, 1, 1, 1, 0, 704, 99
39056, V, 1, 1, 1, 1, 0, 704, 99
39057, V, 1, 1, 1, 1, 0, 704, 99
39058, V, 1, 1, 1, 1, 0, 704, 99
39059, V, 1, 1, 1, 1, 0, 704, 99
39060, V, 1, 1, 1, 1, 0, 704, 99
39061, V, 1, 1, 1, 1, 0, 704, 99
39062, V, 1, 1, 1, 1, 0, 704, 99
39063, V, 1, 1, 1, 1, 0, 704, 99
39064, V, 1, 1, 1, 1, 0, 704, 100
39065, V, 1, 1, 1, 1, 0, 704, 99
39066, V, 1, 1, 1, 1, 0, 704, 99
39067, V, 1, 1, 1, 1, 0, 704, 99
39068, V, 1, 1, 1, 1, 0, 704, 99
39069, V, 1, 1, 1, 1, 0, 704, 99
39070, V, 1, 1, 1, 1, 0, 704, 99
39071, V, 1, 1, 1, 1, 0, 704, 99
39072, V, 1, 1, 1, 1, 0, 704, 99
39073, V, 1, 1, 1, 1, 0, 704, 99
39074, V, 1, 1, 1, 1, 0, 704, 99
39075, V, 1, 1, 1, 1, 0, 704, 99
39076, V, 1, 1, 1, 1, 0, 704, 99
39077, V, 1, 1, 1, 1, 0, 704, 99
39078, V, 1, 1, 1, 1, 0, 704, 99
39079, V, 1, 1, 1, 1, 0, 704, 99
39080, V, 1, 1, 1, 1, 0, 704, 99
39081, V, 1, 1, 1, 1, 0, 704, 99
39083, V, 1, 1, 1, 1, 0, 704, 99
39084, V, 1, 1, 1, 1, 0, 704, 99
39085, V, 1, 1, 1, 1, 0, 704, 99
39086, V, 1, 1, 1, 1, 0, 704, 99
39087, V, 1, 1, 1, 1, 0, 704, 99
39088, V, 1, 1, 1, 1, 0, 704, 99
39089, V, 1, 1, 1, 1, 0, 704, 100
39090, V, 1, 1, 1, 1, 0, 704, 99
39091, V, 1, 1, 1, 1, 0, 704, 99
39092, V, 1, 1, 1, 1, 0, 704, 99
39093, V, 1, 1, 1, 1, 0, 704, 99
39094, V, 1, 1, 1, 1, 0, 704, 99
39095, V, 1, 1, 1, 1, 0, 704, 100
39096, V, 1, 1, 1, 1, 0, 704, 99
39097, V, 1, 1, 1, 1, 0, 704, 99
39098, V, 1, 1, 1, 1, 0, 704, 99
39099, V, 1, 1, 1, 1, 0, 704, 99
39100, V, 1, 1, 1, 1, 0, 704, 100
39101, V, 1, 1, 1, 1, 0, 704, 100
39102, V, 1, 1, 1, 1, 0, 704, 99
39103, V, 1, 1, 1, 1, 0, 704, 100
39104, V, 1, 1, 1, 1, 0, 704, 99
39105, V, 1, 1, 1, 1, 0, 704, 100
39106, V, 1, 1, 1, 1, 0, 704, 99
39107, V, 1, 1, 1, 1, 0, 704, 100
39108, V, 1, 1, 1, 1, 0, 704, 100
39109, V, 1, 1, 1, 1, 0, 704, 100
39110, V, 1, 1, 1, 1, 0, 704, 100
39111, V, 1, 1, 1, 1, 0, 704, 100
39112, V, 1, 1, 1, 1, 0, 704, 100
39113, V, 1, 1, 1, 1, 0, 704, 100
39114, V, 1, 1, 1, 1, 0, 704, 100
39115, V, 1, 1, 1, 1, 0, 704, 100
39116, V, 1, 1, 1, 1, 0, 704, 99
39117, V, 1, 1, 1, 1, 0, 704, 100
39118, V, 1, 1, 1, 1, 0, 704, 99
39119, V, 1, 1, 1, 1, 0, 704, 100
39120, V, 1, 1, 1, 1, 0, 704, 100
39121, V, 1, 1, 1, 1, 0, 704, 99
39122, V, 1, 1, 1, 1, 0, 704, 100
39123, V, 1, 1, 1, 1, 0, 704, 100
39124, V, 1, 1, 1, 1, 0, 704, 100
39126, V, 1, 1, 1, 1, 0, 704, 100
39127, V, 1, 1, 1, 1, 0, 704, 100
39128, V, 1, 1, 1, 1, 0, 704, 100
39129, V, 1, 1, 1, 1, 0, 704, 99
39130, V, 1, 1, 1, 1, 0, 704, 100
39131, V, 1, 1, 1, 1, 0, 704, 99
39132, V, 1, 1, 1, 1, 0, 704, 99
39133, V, 1, 1, 1, 1, 0, 704, 100
39134, V, 1, 1, 1, 1, 0, 704, 99
39135, V, 1, 1, 1, 1, 0, 704, 99
39136, V, 1, 1, 1, 1, 0, 704, 99
39137, V, 1, 1, 1, 1, 0, 704, 99
39138, V, 1, 1, 1, 1, 0, 704, 99
39139, V, 1, 1, 1, 1, 0, 704, 99
39140, V, 1, 1, 1, 1, 0, 704, 99
39141, V, 1, 1, 1, 1, 0, 704, 99
39142, V, 1, 1, 1, 1, 0, 704, 99
39143, V, 1, 1, 1, 1, 0, 704, 99
39144, V, 1, 1, 1, 1, 0, 704, 99
39145, V, 1, 1, 1, 1, 0, 704, 99
39146, V, 1, 1, 1, 1, 0, 704, 99
39147, V, 1, 1, 1, 1, 0, 704, 99
39148, V, 1, 1, 1, 1, 0, 704, 99
39149, V, 1, 1, 1, 1, 0, 704, 99
39150, V, 1, 1, 1, 1, 0, 704, 99
39151, V, 1, 1, 1, 1, 0, 704, 99
39152, V, 1, 1, 1, 1, 0, 704, 99
39153, V, 1, 1, 1, 1, 0, 704, 99
39154, V, 1, 1, 1, 1, 0, 704, 99
39155, V, 1, 1, 1, 1, 0, 704, 99
39156, V, 1, 1, 1, 1, 0, 704, 99
39157, V, 1, 1, 1, 1, 0, 704, 99
39158, V, 1, 1, 1, 1, 0, 704, 99
39159, V, 1, 1, 1, 1, 0, 704, 99
39160, V, 1, 1, 1, 1, 0, 704, 99
39161, V, 1, 1, 1, 1, 0, 704, 99
39162, V, 1, 1, 1, 1, 0, 704, 99
39163, V, 1, 1, 1, 1, 0, 704, 99
39164, V, 1, 1, 1, 1, 0, 704, 99
39165, V, 1, 1, 1, 1, 0, 704, 99
39166, V, 1, 1, 1, 1, 0, 704, 99
39168, V, 1, 1, 1, 1, 0, 704, 99
39169, V, 1, 1, 1, 1, 0, 704, 99
39170, V, 1, 1, 1, 1, 0, 704, 99
39171, V, 1, 1, 1, 1, 0, 704, 99
39172, V, 1, 1, 1, 1, 0, 704, 99
39173, V, 1, 1, 1, 1, 0, 704, 99
39174, V, 1, 1, 1, 1, 0, 704, 99
39175, V, 1, 1, 1, 1, 0, 704, 99
39176, V, 1, 1, 1, 1, 0, 704, 100
39177, V, 1, 1, 1, 1, 0, 704, 99
39178, V, 1, 1, 1, 1, 0, 704, 99
39179, V, 1, 1, 1, 1, 0, 704, 100
39180, V, 1, 1, 1, 1, 0, 704, 100
39181, V, 1, 1, 1, 1, 0, 704, 100
39182, V, 1, 1, 1, 1, 0, 704, 99
39183, V, 1, 1, 1, 1, 0, 704, 99
39184, V, 1, 1, 1, 1, 0, 704, 100
39185, V, 1, 1, 1, 1, 0, 704, 100
39186, V, 1, 1, 1, 1, 0, 704, 100
39187, V, 1, 1, 1, 1, 0, 704, 100
39188, V, 1, 1, 1, 1, 0, 704, 100
39189, V, 1, 1, 1, 1, 0, 704, 100
39190, V, 1, 1, 1, 1, 0, 704, 100
39191, V, 1, 1, 1, 1, 0, 704, 100
39192, V, 1, 1, 1, 1, 0, 704, 100
39193, V, 1, 1, 1, 1, 0, 704, 100
39194, V, 1, 1, 1, 1, 0, 704, 100
39195, V, 1, 1, 1, 1, 0, 704, 99
39196, V, 1, 1, 1, 1, 0, 704, 100
39197, V, 1, 1, 1, 1, 0, 704, 100
39198, V, 1, 1, 1, 1, 0, 704, 100
39199, V, 1, 1, 1, 1, 0, 704, 100
39200, V, 1, 1, 1, 1, 0, 704, 100
39201, V, 1, 1, 1, 1, 0, 704, 99
39202, V, 1, 1, 1, 1, 0, 704, 99
39203, V, 1, 1, 1, 1, 0, 704, 99
39204, V, 1, 1, 1, 1, 0, 704, 100
39205, V, 1, 1, 1, 1, 0, 704, 99
39206, V, 1, 1, 1, 1, 0, 704, 99
39207, V, 1, 1, 1, 1, 0, 704, 99
39208, V, 1, 1, 1, 1, 0, 704, 99
39209, V, 1, 1, 1, 1, 0, 704, 99
39211, V, 1, 1, 1, 1, 0, 704, 99
39212, V, 1, 1, 1, 1, 0, 704, 99
39213, V, 1, 1, 1, 1, 0, 704, 99
39214, V, 1, 1, 1, 1, 0, 704, 99
39215, V, 1, 1, 1, 1, 0, 704, 99
39216, V, 1, 1, 1, 1, 0, 704, 99
39217, V, 1, 1, 1, 1, 0, 704, 99
39218, V, 1, 1, 1, 1, 0, 704, 99
39219, V, 1, 1, 1, 1, 0, 704, 99
39220, V, 1, 1, 1, 1, 0, 704, 99
39221, V, 1, 1, 1, 1, 0, 704, 99
39222, V, 1, 1, 1, 1, 0, 704, 99
39223, V, 1, 1, 1, 1, 0, 704, 99
39224, V, 1, 1, 1, 1, 0, 704, 99
39225, V, 1, 1, 1, 1, 0, 704, 99
39226, V, 1, 1, 1, 1, 0, 704, 99
39227, V, 1, 1, 1, 1, 0, 704, 99
39228, V, 1, 1, 1, 1, 0, 704, 99
39229, V, 1, 1, 1, 1, 0, 704, 99
39230, V, 1, 1, 1, 1, 0, 704, 99
39231, V, 1, 1, 1, 1, 0, 704, 99
39232, V, 1, 1, 1, 1, 0, 704, 99
39233, V, 1, 1, 1, 1, 0, 704, 99
39234, V, 1, 1, 1, 1, 0, 704, 99
39235, V, 1, 1, 1, 1, 0, 704, 99
39236, V, 1, 1, 1, 1, 0, 704, 99
39237, V, 1, 1, 1, 1, 0, 704, 99
39238, V, 1, 1, 1, 1, 0, 704, 99
39239, V, 1, 1, 1, 1, 0, 704, 99
39240, V, 1, 1, 1, 1, 0, 704, 99
39241, V, 1, 1, 1, 1, 0, 704, 99
39242, V, 1, 1, 1, 1, 0, 704, 99
39243, V, 1, 1, 1, 1, 0, 704, 99
39244, V, 1, 1, 1, 1, 0, 704, 99
39245, V, 1, 1, 1, 1, 0, 704, 99
39246, V, 1, 1, 1, 1, 0, 704, 99
39247, V, 1, 1, 1, 1, 0, 704, 99
39248, V, 1, 1, 1, 1, 0, 704, 99
39249, V, 1, 1, 1, 1, 0, 704, 99
39250, V, 1, 1, 1, 1, 0, 704, 99
39251, V, 1, 1, 1, 1, 0, 704, 99
39252, V, 1, 1, 1, 1, 0, 704, 99
39254, V, 1, 1, 1, 1, 0, 704, 100
39255, V, 1, 1, 1, 1, 0, 704, 99
39256, V, 1, 1, 1, 1, 0, 704, 99
39257, V, 1, 1, 1, 1, 0, 704, 100
39258, V, 1, 1, 1, 1, 0, 704, 100
39259, V, 1, 1, 1, 1, 0, 704, 100
39260, V, 1, 1, 1, 1, 0, 704, 100
39261, V, 1, 1, 1, 1, 0, 704, 99
39262, V, 1, 1, 1, 1, 0, 704, 100
39263, V, 1, 1, 1, 1, 0, 704, 100
39264, V, 1, 1, 1, 1, 0, 704, 100
39265, V, 1, 1, 1, 1, 0, 704, 100
39266, V, 1, 1, 1, 1, 0, 704, 100
39267, V, 1, 1, 1, 1, 0, 704, 100
39268, V, 1, 1, 1, 1, 0, 704, 99
39269, V, 1, 1, 1, 1, 0, 704, 100
39270, V, 1, 1, 1, 1, 0, 704, 100
39271, V, 1, 1, 1, 1, 0, 704, 100
39272, V, 1, 1, 1, 1, 0, 704, 100
39273, V, 1, 1, 1, 1, 0, 704, 100
39274, V, 1, 1, 1, 1, 0, 704, 100
39275, V, 1, 1, 1, 1, 0, 704, 100
39276, V, 1, 1, 1, 1, 0, 704, 99
39277, V, 1, 1, 1, 1, 0, 704, 100
39278, V, 1, 1, 1, 1, 0, 704, 100
39279, V, 1, 1, 1, 1, 0, 704, 99
39280, V, 1, 1, 1, 1, 0, 704, 99
39281, V, 1, 1, 1, 1, 0, 704, 99
39282, V, 1, 1, 1, 1, 0, 704, 100
39283, V, 1, 1, 1, 1, 0, 704, 99
39284, V, 1, 1, 1, 1, 0, 704, 99
39285, V, 1, 1, 1, 1, 0, 704, 99
39286, V, 1, 1, 1, 1, 0, 704, 100
39287, V, 1, 1, 1, 1, 0, 704, 100
39288, V, 1, 1, 1, 1, 0, 704, 100
39289, V, 1, 1, 1, 1, 0, 704, 99
39290, V, 1, 1, 1, 1, 0, 704, 99
39291, V, 1, 1, 1, 1, 0, 704, 99
39292, V, 1, 1, 1, 1, 0, 704, 99
39293, V, 1, 1, 1, 1, 0, 704, 99
39294, V, 1, 1, 1, 1, 0, 704, 99
39296, V, 1, 1, 1, 1, 0, 704, 99
39297, V, 1, 1, 1, 1, 0, 704, 99
39298, V, 1, 1, 1, 1, 0, 704, 99
39299, V, 1, 1, 1, 1, 0, 704, 99
39300, V, 1, 1, 1, 1, 0, 704, 99
39301, V, 1, 1, 1, 1, 0, 704, 99
39302, V, 1, 1, 1, 1, 0, 704, 99
39303, V, 1, 1, 1, 1, 0, 704, 99
39304, V, 1, 1, 1, 1, 0, 704, 99
39305, V, 1, 1, 1, 1, 0, 704, 99
39306, V, 1, 1, 1, 1, 0, 704, 99
39307, V, 1, 1, 1, 1, 0, 704, 99
39308, V, 1, 1, 1, 1, 0, 704, 99
39309, V, 1, 1, 1, 1, 0, 704, 99
39310, V, 1, 1, 1, 1, 0, 704, 99
39311, V, 1, 1, 1, 1, 0, 704, 99
39312, V, 1, 1, 1, 1, 0, 704, 99
39313, V, 1, 1, 1, 1, 0, 704, 99
39314, V, 1, 1, 1, 1, 0, 704, 99
39315, V, 1, 1, 1, 1, 0, 704, 99
39316, V, 1, 1, 1, 1, 0, 704, 99
39317, V, 1, 1, 1, 1, 0, 704, 99
39318, V, 1, 1, 1, 1, 0, 704, 99
39319, V, 1, 1, 1, 1, 0, 704, 99
39320, V, 1, 1, 1, 1, 0, 704, 99
39321, V, 1, 1, 1, 1, 0, 704, 99
39322, V, 1, 1, 1, 1, 0, 704, 99
39323, V, 1, 1, 1, 1, 0, 704, 99
39324, V, 1, 1, 1, 1, 0, 704, 99
39325, V, 1, 1, 1, 1, 0, 704, 99
39326, V, 1, 1, 1, 1, 0, 704, 99
39327, V, 1, 1, 1, 1, 0, 704, 99
39328, V, 1, 1, 1, 1, 0, 704, 99
39329, V, 1, 1, 1, 1, 0, 704, 99
39330, V, 1, 1, 1, 1, 0, 704, 100
39331, V, 1, 1, 1, 1, 0, 704, 99
39332, V, 1, 1, 1, 1, 0, 704, 99
39333, V, 1, 1, 1, 1, 0, 704, 99
39334, V, 1, 1, 1, 1, 0, 704, 99
39335, V, 1, 1, 1, 1, 0, 704, 100
39336, V, 1, 1, 1, 1, 0, 704, 100
39337, V, 1, 1, 1, 1, 0, 704, 100
39339, V, 1, 1, 1, 1, 0, 704, 99
39340, V, 1, 1, 1, 1, 0, 704, 100
39341, V, 1, 1, 1, 1, 0, 704, 99
39342, V, 1, 1, 1, 1, 0, 704, 100
39343, V, 1, 1, 1, 1, 0, 704, 100
39344, V, 1, 1, 1, 1, 0, 704, 100
39345, V, 1, 1, 1, 1, 0, 704, 99
39346, V, 1, 1, 1, 1, 0, 704, 100
39347, V, 1, 1, 1, 1, 0, 704, 99
39348, V, 1, 1, 1, 1, 0, 704, 100
39349, V, 1, 1, 1, 1, 0, 704, 100
39350, V, 1, 1, 1, 1, 0, 704, 100
39351, V, 1, 1, 1, 1, 0, 704, 100
39352, V, 1, 1, 1, 1, 0, 704, 99
39353, V, 1, 1, 1, 1, 0, 704, 99
39354, V, 1, 1, 1, 1, 0, 704, 99
39355, V, 1, 1, 1, 1, 0, 704, 100
39356, V, 1, 1, 1, 1, 0, 704, 100
39357, V, 1, 1, 1, 1, 0, 704, 99
39358, V, 1, 1, 1, 1, 0, 704, 100
39359, V, 1, 1, 1, 1, 0, 704, 99
39360, V, 1, 1, 1, 1, 0, 704, 99
39361, V, 1, 1, 1, 1, 0, 704, 99
39362, V, 1, 1, 1, 1, 0, 704, 99
39363, V, 1, 1, 1, 1, 0, 704, 99
39364, V, 1, 1, 1, 1, 0, 704, 99
39365, V, 1, 1, 1, 1, 0, 704, 99
39366, V, 1, 1, 1, 1, 0, 704, 99
39367, V, 1, 1, 1, 1, 0, 704, 99
39368, V, 1, 1, 1, 1, 0, 704, 99
39369, V, 1, 1, 1, 1, 0, 704, 99
39370, V, 1, 1, 1, 1, 0, 704, 99
39371, V, 1, 1, 1, 1, 0, 704, 99
39372, V, 1, 1, 1, 1, 0, 704, 99
39373, V, 1, 1, 1, 1, 0, 704, 99
39374, V, 1, 1, 1, 1, 0, 704, 99
39375, V, 1, 1, 1, 1, 0, 704, 99
39376, V, 1, 1, 1, 1, 0, 704, 99
39377, V, 1, 1, 1, 1, 0, 704, 99
39378, V, 1, 1, 1, 1, 0, 704, 99
39379, V, 1, 1, 1, 1, 0, 704, 99
39380, V, 1, 1, 1, 1, 0, 704, 99
39382, V, 1, 1, 1, 1, 0, 704, 99
39383, V, 1, 1, 1, 1, 0, 704, 99
39384, V, 1, 1, 1, 1, 0, 704, 99
39385, V, 1, 1, 1, 1, 0, 704, 99
39386, V, 1, 1, 1, 1, 0, 704, 99
39387, V, 1, 1, 1, 1, 0, 704, 99
39388, V, 1, 1, 1, 1, 0, 704, 99
39389, V, 1, 1, 1, 1, 0, 704, 99
39390, V, 1, 1, 1, 1, 0, 704, 99
39391, V, 1, 1, 1, 1, 0, 704, 99
39392, V, 1, 1, 1, 1, 0, 704, 99
39393, V, 1, 1, 1, 1, 0, 704, 99
39394, V, 1, 1, 1, 1, 0, 704, 99
39395, V, 1, 1, 1, 1, 0, 704, 99
39396, V, 1, 1, 1, 1, 0, 704, 99
39397, V, 1, 1, 1, 1, 0, 704, 99
39398, V, 1, 1, 1, 1, 0, 704, 99
39399, V, 1, 1, 1, 1, 0, 704, 99
39400, V, 1, 1, 1, 1, 0, 704, 99
39401, V, 1, 1, 1, 1, 0, 704, 100
39402, V, 1, 1, 1, 1, 0, 704, 99
39403, V, 1, 1, 1, 1, 0, 704, 99
39404, V, 1, 1, 1, 1, 0, 704, 99
39405, V, 1, 1, 1, 1, 0, 704, 99
39406, V, 1, 1, 1, 1, 0, 704, 99
39407, V, 1, 1, 1, 1, 0, 704, 99
39408, V, 1, 1, 1, 1, 0, 704, 99
39409, V, 1, 1, 1, 1, 0, 704, 100
39410, V, 1, 1, 1, 1, 0, 704, 99
39411, V, 1, 1, 1, 1, 0, 704, 100
39412, V, 1, 1, 1, 1, 0, 704, 99
39413, V, 1, 1, 1, 1, 0, 704, 99
39414, V, 1, 1, 1, 1, 0, 704, 100
39415, V, 1, 1, 1, 1, 0, 704, 99
39416, V, 1, 1, 1, 1, 0, 704, 100
39417, V, 1, 1, 1, 1, 0, 704, 99
39418, V, 1, 1, 1, 1, 0, 704, 99
39419, V, 1, 1, 1, 1, 0, 704, 99
39420, V, 1, 1, 1, 1, 0, 704, 99
39421, V, 1, 1, 1, 1, 0, 704, 100
39422, V, 1, 1, 1, 1, 0, 704, 100
39424, V, 1, 1, 1, 1, 0, 704, 100
39425, V, 1, 1, 1, 1, 0, 704, 100
39426, V, 1, 1, 1, 1, 0, 704, 99
39427, V, 1, 1, 1, 1, 0, 704, 99
39428, V, 1, 1, 1, 1, 0, 704, 99
39429, V, 1, 1, 1, 1, 0, 704, 99
39430, V, 1, 1, 1, 1, 0, 704, 99
39431, V, 1, 1, 1, 1, 0, 704, 99
39432, V, 1, 1, 1, 1, 0, 704, 99
39433, V, 1, 1, 1, 1, 0, 704, 99
39434, V, 1, 1, 1, 1, 0, 704, 99
39435, V, 1, 1, 1, 1, 0, 704, 99
39436, V, 1, 1, 1, 1, 0, 704, 99
39437, V, 1, 1, 1, 1, 0, 704, 99
39438, V, 1, 1, 1, 1, 0, 704, 99
39439, V, 1, 1, 1, 1, 0, 704, 99
39440, V, 1, 1, 1, 1, 0, 704, 99
39441, V, 1, 1, 1, 1, 0, 704, 99
39442, V, 1, 1, 1, 1, 0, 704, 99
39443, V, 1, 1, 1, 1, 0, 704, 99
39444, V, 1, 1, 1, 1, 0, 704, 99
39445, V, 1, 1, 1, 1, 0, 704, 99
39446, V, 1, 1, 1, 1, 0, 704, 99
39447, V, 1, 1, 1, 1, 0, 704, 99
39448, V, 1, 1, 1, 1, 0, 704, 99
39449, V, 1, 1, 1, 1, 0, 704, 99
39450, V, 1, 1, 1, 1, 0, 704, 99
39451, V, 1, 1, 1, 1, 0, 704, 99
39452, V, 1, 1, 1, 1, 0, 704, 99
39453, V, 1, 1, 1, 1, 0, 704, 99
39454, V, 1, 1, 1, 1, 0, 704, 99
39455, V, 1, 1, 1, 1, 0, 704, 99
39456, V, 1, 1, 1, 1, 0, 704, 99
39457, V, 1, 1, 1, 1, 0, 704, 99
39458, V, 1, 1, 1, 1, 0, 704, 99
39459, V, 1, 1, 1, 1, 0, 704, 99
39460, V, 1, 1, 1, 1, 0, 704, 99
39461, V, 1, 1, 1, 1, 0, 704, 99
39462, V, 1, 1, 1, 1, 0, 704, 99
39463, V, 1, 1, 1, 1, 0, 704, 99
39464, V, 1, 1, 1, 1, 0, 704, 99
39465, V, 1, 1, 1, 1, 0, 704, 99
39467, V, 1, 1, 1, 1, 0, 704, 99
39468, V, 1, 1, 1, 1, 0, 704, 99
39469, V, 1, 1, 1, 1, 0, 704, 99
39470, V, 1, 1, 1, 1, 0, 704, 99
39471, V, 1, 1, 1, 1, 0, 704, 99
39472, V, 1, 1, 1, 1, 0, 704, 99
39473, V, 1, 1, 1, 1, 0, 704, 99
39474, V, 1, 1, 1, 1, 0, 704, 99
39475, V, 1, 1, 1, 1, 0, 704, 99
39476, V, 1, 1, 1, 1, 0, 704, 99
39477, V, 1, 1, 1, 1, 0, 704, 99
39478, V, 1, 1, 1, 1, 0, 704, 99
39479, V, 1, 1, 1, 1, 0, 704, 99
39480, V, 1, 1, 1, 1, 0, 704, 99
39481, V, 1, 1, 1, 1, 0, 704, 99
39482, V, 1, 1, 1, 1, 0, 704, 99
39483, V, 1, 1, 1, 1, 0, 704, 99
39484, V, 1, 1, 1, 1, 0, 704, 99
39485, V, 1, 1, 1, 1, 0, 704, 100
39486, V, 1, 1, 1, 1, 0, 704, 100
39487, V, 1, 1, 1, 1, 0, 704, 100
39488, V, 1, 1, 1, 1, 0, 704, 99
39489, V, 1, 1, 1, 1, 0, 704, 100
39490, V, 1, 1, 1, 1, 0, 704, 100
39491, V, 1, 1, 1, 1, 0, 704, 100
39492, V, 1, 1, 1, 1, 0, 704, 100
39493, V, 1, 1, 1, 1, 0, 704, 99
39494, V, 1, 1, 1, 1, 0, 704, 100
39495, V, 1, 1, 1, 1, 0, 704, 100
39496, V, 1, 1, 1, 1, 0, 704, 99
39497, V, 1, 1, 1, 1, 0, 704, 100
39498, V, 1, 1, 1, 1, 0, 704, 99
39499, V, 1, 1, 1, 1, 0, 704, 100
39500, V, 1, 1, 1, 1, 0, 704, 100
39501, V, 1, 1, 1, 1, 0, 704, 99
39502, V, 1, 1, 1, 1, 0, 704, 99
39503, V, 1, 1, 1, 1, 0, 704, 99
39504, V, 1, 1, 1, 1, 0, 704, 99
39505, V, 1, 1, 1, 1, 0, 704, 100
39506, V, 1, 1, 1, 1, 0, 704, 99
39507, V, 1, 1, 1, 1, 0, 704, 99
39508, V, 1, 1, 1, 1, 0, 704, 99
39510, V, 1, 1, 1, 1, 0, 704, 99
39511, V, 1, 1, 1, 1, 0, 704, 99
39512, V, 1, 1, 1, 1, 0, 704, 99
39513, V, 1, 1, 1, 1, 0, 704, 99
39514, V, 1, 1, 1, 1, 0, 704, 99
39515, V, 1, 1, 1, 1, 0, 704, 99
39516, V, 1, 1, 1, 1, 0, 704, 99
39517, V, 1, 1, 1, 1, 0, 704, 99
39518, V, 1, 1, 1, 1, 0, 704, 99
39519, V, 1, 1, 1, 1, 0, 704, 99
39520, V, 1, 1, 1, 1, 0, 704, 99
39521, V, 1, 1, 1, 1, 0, 704, 99
39522, V, 1, 1, 1, 1, 0, 704, 99
39523, V, 1, 1, 1, 1, 0, 704, 99
39524, V, 1, 1, 1, 1, 0, 704, 99
39525, V, 1, 1, 1, 1, 0, 704, 99
39526, V, 1, 1, 1, 1, 0, 704, 99
39527, V, 1, 1, 1, 1, 0, 704, 99
39528, V, 1, 1, 1, 1, 0, 704, 99
39529, V, 1, 1, 1, 1, 0, 704, 99
39530, V, 1, 1, 1, 1, 0, 704, 99
39531, V, 1, 1, 1, 1, 0, 704, 99
39532, V, 1, 1, 1, 1, 0, 704, 99
39533, V, 1, 1, 1, 1, 0, 704, 99
39534, V, 1, 1, 1, 1, 0, 704, 99
39535, V, 1, 1, 1, 1, 0, 704, 99
39536, V, 1, 1, 1, 1, 0, 704, 99
39537, V, 1, 1, 1, 1, 0, 704, 99
39538, V, 1, 1, 1, 1, 0, 704, 99
39539, V, 1, 1, 1, 1, 0, 704, 99
39540, V, 1, 1, 1, 1, 0, 704, 99
39541, V, 1, 1, 1, 1, 0, 704, 99
39542, V, 1, 1, 1, 1, 0, 704, 99
39543, V, 1, 1, 1, 1, 0, 704, 99
39544, V, 1, 1, 1, 1, 0, 704, 99
39545, V, 1, 1, 1, 1, 0, 704, 99
39546, V, 1, 1, 1, 1, 0, 704, 99
39547, V, 1, 1, 1, 1, 0, 704, 99
39548, V, 1, 1, 1, 1, 0, 704, 99
39549, V, 1, 1, 1, 1, 0, 704, 99
39550, V, 1, 1, 1, 1, 0, 704, 99
39552, V, 1, 1, 1, 1, 0, 704, 99
39553, V, 1, 1, 1, 1, 0, 704, 99
39554, V, 1, 1, 1, 1, 0, 704, 99
39555, V, 1, 1, 1, 1, 0, 704, 99
39556, V, 1, 1, 1, 1, 0, 704, 99
39557, V, 1, 1, 1, 1, 0, 704, 99
39558, V, 1, 1, 1, 1, 0, 704, 99
39559, V, 1, 1, 1, 1, 0, 704, 99
39560, V, 1, 1, 1, 1, 0, 704, 99
39561, V, 1, 1, 1, 1, 0, 704, 100
39562, V, 1, 1, 1, 1, 0, 704, 99
39563, V, 1, 1, 1, 1, 0, 704, 99
39564, V, 1, 1, 1, 1, 0, 704, 100
39565, V, 1, 1, 1, 1, 0, 704, 99
39566, V, 1, 1, 1, 1, 0, 704, 100
39567, V, 1, 1, 1, 1, 0, 704, 100
39568, V, 1, 1, 1, 1, 0, 704, 100
39569, V, 1, 1, 1, 1, 0, 704, 99
39570, V, 1, 1, 1, 1, 0, 704, 100
39571, V, 1, 1, 1, 1, 0, 704, 100
39572, V, 1, 1, 1, 1, 0, 704, 100
39573, V, 1, 1, 1, 1, 0, 704, 99
39574, V, 1, 1, 1, 1, 0, 704, 99
39575, V, 1, 1, 1, 1, 0, 704, 99
39576, V, 1, 1, 1, 1, 0, 704, 99
39577, V, 1, 1, 1, 1, 0, 704, 99
39578, V, 1, 1, 1, 1, 0, 704, 99
39579, V, 1, 1, 1, 1, 0, 704, 99
39580, V, 1, 1, 1, 1, 0, 704, 100
39581, V, 1, 1, 1, 1, 0, 704, 99
39582, V, 1, 1, 1, 1, 0, 704, 99
39583, V, 1, 1, 1, 1, 0, 704, 99
39584, V, 1, 1, 1, 1, 0, 704, 99
39585, V, 1, 1, 1, 1, 0, 704, 99
39586, V, 1, 1, 1, 1, 0, 704, 99
39587, V, 1, 1, 1, 1, 0, 704, 99
39588, V, 1, 1, 1, 1, 0, 704, 99
39589, V, 1, 1, 1, 1, 0, 704, 99
39590, V, 1, 1, 1, 1, 0, 704, 99
39591, V, 1, 1, 1, 1, 0, 704, 99
39592, V, 1, 1, 1, 1, 0, 704, 99
39593, V, 1, 1, 1, 1, 0, 704, 99
39595, V, 1, 1, 1, 1, 0, 704, 99
39596, V, 1, 1, 1, 1, 0, 704, 99
39597, V, 1, 1, 1, 1, 0, 704, 99
39598, V, 1, 1, 1, 1, 0, 704, 99
39599, V, 1, 1, 1, 1, 0, 704, 99
39600, V, 1, 1, 1, 1, 0, 704, 99
39601, V, 1, 1, 1, 1, 0, 704, 99
39602, V, 1, 1, 1, 1, 0, 704, 99
39603, V, 1, 1, 1, 1, 0, 704, 99
39604, V, 1, 1, 1, 1, 0, 704, 99
39605, V, 1, 1, 1, 1, 0, 704, 99
39606, V, 1, 1, 1, 1, 0, 704, 99
39607, V, 1, 1, 1, 1, 0, 704, 99
39608, V, 1, 1, 1, 1, 0, 704, 99
39609, V, 1, 1, 1, 1, 0, 704, 99
39610, V, 1, 1, 1, 1, 0, 704, 99
39611, V, 1, 1, 1, 1, 0, 704, 99
39612, V, 1, 1, 1, 1, 0, 704, 99
39613, V, 1, 1, 1, 1, 0, 704, 99
39614, V, 1, 1, 1, 1, 0, 704, 99
39615, V, 1, 1, 1, 1, 0, 704, 99
39616, V, 1, 1, 1, 1, 0, 704, 99
39617, V, 1, 1, 1, 1, 0, 704, 99
39618, V, 1, 1, 1, 1, 0, 704, 99
39619, V, 1, 1, 1, 1, 0, 704, 99
39620, V, 1, 1, 1, 1, 0, 704, 99
39621, V, 1, 1, 1, 1, 0, 704, 99
39622, V, 1, 1, 1, 1, 0, 704, 99
39623, V, 1, 1, 1, 1, 0, 704, 99
39624, V, 1, 1, 1, 1, 0, 704, 99
39625, V, 1, 1, 1, 1, 0, 704, 99
39626, V, 1, 1, 1, 1, 0, 704, 99
39627, V, 1, 1, 1, 1, 0, 704, 99
39628, V, 1, 1, 1, 1, 0, 704, 99
39629, V, 1, 1, 1, 1, 0, 704, 99
39630, V, 1, 1, 1, 1, 0, 704, 99
39631, V, 1, 1, 1, 1, 0, 704, 99
39632, V, 1, 1, 1, 1, 0, 704, 100
39633, V, 1, 1, 1, 1, 0, 704, 100
39634, V, 1, 1, 1, 1, 0, 704, 99
39635, V, 1, 1, 1, 1, 0, 704, 99
39636, V, 1, 1, 1, 1, 0, 704, 99
39638, V, 1, 1, 1, 1, 0, 704, 99
39639, V, 1, 1, 1, 1, 0, 704, 100
39640, V, 1, 1, 1, 1, 0, 704, 100
39641, V, 1, 1, 1, 1, 0, 704, 99
39642, V, 1, 1, 1, 1, 0, 704, 99
39643, V, 1, 1, 1, 1, 0, 704, 99
39644, V, 1, 1, 1, 1, 0, 704, 100
39645, V, 1, 1, 1, 1, 0, 704, 99
39646, V, 1, 1, 1, 1, 0, 704, 100
39647, V, 1, 1, 1, 1, 0, 704, 100
39648, V, 1, 1, 1, 1, 0, 704, 99
39649, V, 1, 1, 1, 1, 0, 704, 100
39650, V, 1, 1, 1, 1, 0, 704, 100
39651, V, 1, 1, 1, 1, 0, 704, 99
39652, V, 1, 1, 1, 1, 0, 704, 99
39653, V, 1, 1, 1, 1, 0, 704, 99
39654, V, 1, 1, 1, 1, 0, 704, 99
39655, V, 1, 1, 1, 1, 0, 704, 99
39656, V, 1, 1, 1, 1, 0, 704, 99
39657, V, 1, 1, 1, 1, 0, 704, 100
39658, V, 1, 1, 1, 1, 0, 704, 99
39659, V, 1, 1, 1, 1, 0, 704, 99
39660, V, 1, 1, 1, 1, 0, 704, 99
39661, V, 1, 1, 1, 1, 0, 704, 99
39662, V, 1, 1, 1, 1, 0, 704, 99
39663, V, 1, 1, 1, 1, 0, 704, 99
39664, V, 1, 1, 1, 1, 0, 704, 99
39665, V, 1, 1, 1, 1, 0, 704, 99
39666, V, 1, 1, 1, 1, 0, 704, 99
39667, V, 1, 1, 1, 1, 0, 704, 99
39668, V, 1, 1, 1, 1, 0, 704, 99
39669, V, 1, 1, 1, 1, 0, 704, 99
39670, V, 1, 1, 1, 1, 0, 704, 99
39671, V, 1, 1, 1, 1, 0, 704, 99
39672, V, 1, 1, 1, 1, 0, 704, 99
39673, V, 1, 1, 1, 1, 0, 704, 99
39674, V, 1, 1, 1, 1, 0, 704, 99
39675, V, 1, 1, 1, 1, 0, 704, 99
39676, V, 1, 1, 1, 1, 0, 704, 99
39677, V, 1, 1, 1, 1, 0, 704, 99
39678, V, 1, 1, 1, 1, 0, 704, 99
39680, V, 1, 1, 1, 1, 0, 704, 99
39681, V, 1, 1, 1, 1, 0, 704, 99
39682, V, 1, 1, 1, 1, 0, 704, 99
39683, V, 1, 1, 1, 1, 0, 704, 99
39684, V, 1, 1, 1, 1, 0, 704, 99
39685, V, 1, 1, 1, 1, 0, 704, 99
39686, V, 1, 1, 1, 1, 0, 704, 99
39687, V, 1, 1, 1, 1, 0, 704, 99
39688, V, 1, 1, 1, 1, 0, 704, 99
39689, V, 1, 1, 1, 1, 0, 704, 99
39690, V, 1, 1, 1, 1, 0, 704, 99
39691, V, 1, 1, 1, 1, 0, 704, 99
39692, V, 1, 1, 1, 1, 0, 704, 99
39693, V, 1, 1, 1, 1, 0, 704, 99
39694, V, 1, 1, 1, 1, 0, 704, 99
39695, V, 1, 1, 1, 1, 0, 704, 99
39696, V, 1, 1, 1, 1, 0, 704, 99
39697, V, 1, 1, 1, 1, 0, 704, 99
39698, V, 1, 1, 1, 1, 0, 704, 99
39699, V, 1, 1, 1, 1, 0, 704, 99
39700, V, 1, 1, 1, 1, 0, 704, 99
39701, V, 1, 1, 1, 1, 0, 704, 99
39702, V, 1, 1, 1, 1, 0, 704, 99
39703, V, 1, 1, 1, 1, 0, 704, 99
39704, V, 1, 1, 1, 1, 0, 704, 99
39705, V, 1, 1, 1, 1, 0, 704, 99
39706, V, 1, 1, 1, 1, 0, 704, 99
39707, V, 1, 1, 1, 1, 0, 704, 99
39708, V, 1, 1, 1, 1, 0, 704, 99
39709, V, 1, 1, 1, 1, 0, 704, 99
39710, V, 1, 1, 1, 1, 0, 704, 100
39711, V, 1, 1, 1, 1, 0, 704, 99
39712, V, 1, 1, 1, 1, 0, 704, 100
39713, V, 1, 1, 1, 1, 0, 704, 99
39714, V, 1, 1, 1, 1, 0, 704, 99
39715, V, 1, 1, 1, 1, 0, 704, 99
39716, V, 1, 1, 1, 1, 0, 704, 99
39717, V, 1, 1, 1, 1, 0, 704, 99
39718, V, 1, 1, 1, 1, 0, 704, 99
39719, V, 1, 1, 1, 1, 0, 704, 99
39720, V, 1, 1, 1, 1, 0, 704, 99
39721, V, 1, 1, 1, 1, 0, 704, 99
39723, V, 1, 1, 1, 1, 0, 704, 99
39724, V, 1, 1, 1, 1, 0, 704, 99
39725, V, 1, 1, 1, 1, 0, 704, 99
39726, V, 1, 1, 1, 1, 0, 704, 99
39727, V, 1, 1, 1, 1, 0, 704, 99
39728, V, 1, 1, 1, 1, 0, 704, 99
39729, V, 1, 1, 1, 1, 0, 704, 99
39730, V, 1, 1, 1, 1, 0, 704, 99
39731, V, 1, 1, 1, 1, 0, 704, 99
39732, V, 1, 1, 1, 1, 0, 704, 99
39733, V, 1, 1, 1, 1, 0, 704, 99
39734, V, 1, 1, 1, 1, 0, 704, 99
39735, V, 1, 1, 1, 1, 0, 704, 99
39736, V, 1, 1, 1, 1, 0, 704, 99
39737, V, 1, 1, 1, 1, 0, 704, 99
39738, V, 1, 1, 1, 1, 0, 704, 99
39739, V, 1, 1, 1, 1, 0, 704, 99
39740, V, 1, 1, 1, 1, 0, 704, 99
39741, V, 1, 1, 1, 1, 0, 704, 99
39742, V, 1, 1, 1, 1, 0, 704, 99
39743, V, 1, 1, 1, 1, 0, 704, 99
39744, V, 1, 1, 1, 1, 0, 704, 99
39745, V, 1, 1, 1, 1, 0, 704, 99
39746, V, 1, 1, 1, 1, 0, 704, 99
39747, V, 1, 1, 1, 1, 0, 704, 99
39748, V, 1, 1, 1, 1, 0, 704, 99
39749, V, 1, 1, 1, 1, 0, 704, 99
39750, V, 1, 1, 1, 1, 0, 704, 99
39751, V, 1, 1, 1, 1, 0, 704, 99
39752, V, 1, 1, 1, 1, 0, 704, 99
39753, V, 1, 1, 1, 1, 0, 704, 99
39754, V, 1, 1, 1, 1, 0, 704, 99
39755, V, 1, 1, 1, 1, 0, 704, 99
39756, V, 1, 1, 1, 1, 0, 704, 99
39757, V, 1, 1, 1, 1, 0, 704, 99
39758, V, 1, 1, 1, 1, 0, 704, 99
39759, V, 1, 1, 1, 1, 0, 704, 99
39760, V, 1, 1, 1, 1, 0, 704, 99
39761, V, 1, 1, 1, 1, 0, 704, 99
39762, V, 1, 1, 1, 1, 0, 704, 99
39763, V, 1, 1, 1, 1, 0, 704, 99
39764, V, 1, 1, 1, 1, 0, 704, 99
39766, V, 1, 1, 1, 1, 0, 704, 99
39767, V, 1, 1, 1, 1, 0, 704, 99
39768, V, 1, 1, 1, 1, 0, 704, 99
39769, V, 1, 1, 1, 1, 0, 704, 99
39770, V, 1, 1, 1, 1, 0, 704, 99
39771, V, 1, 1, 1, 1, 0, 704, 99
39772, V, 1, 1, 1, 1, 0, 704, 99
39773, V, 1, 1, 1, 1, 0, 704, 99
39774, V, 1, 1, 1, 1, 0, 704, 99
39775, V, 1, 1, 1, 1, 0, 704, 99
39776, V, 1, 1, 1, 1, 0, 704, 99
39777, V, 1, 1, 1, 1, 0, 704, 99
39778, V, 1, 1, 1, 1, 0, 704, 100
39779, V, 1, 1, 1, 1, 0, 704, 99
39780, V, 1, 1, 1, 1, 0, 704, 99
39781, V, 1, 1, 1, 1, 0, 704, 99
39782, V, 1, 1, 1, 1, 0, 704, 99
39783, V, 1, 1, 1, 1, 0, 704, 99
39784, V, 1, 1, 1, 1, 0, 704, 99
39785, V, 1, 1, 1, 1, 0, 704, 99
39786, V, 1, 1, 1, 1, 0, 704, 100
39787, V, 1, 1, 1, 1, 0, 704, 99
39788, V, 1, 1, 1, 1, 0, 704, 100
39789, V, 1, 1, 1, 1, 0, 704, 100
39790, V, 1, 1, 1, 1, 0, 704, 100
39791, V, 1, 1, 1, 1, 0, 704, 100
39792, V, 1, 1, 1, 1, 0, 704, 100
39793, V, 1, 1, 1, 1, 0, 704, 100
39794, V, 1, 1, 1, 1, 0, 704, 100
39795, V, 1, 1, 1, 1, 0, 704, 100
39796, V, 1, 1, 1, 1, 0, 704, 100
39797, V, 1, 1, 1, 1, 0, 704, 100
39798, V, 1, 1, 1, 1, 0, 704, 100
39799, V, 1, 1, 1, 1, 0, 704, 100
39800, V, 1, 1, 1, 1, 0, 704, 100
39801, V, 1, 1, 1, 1, 0, 704, 100
39802, V, 1, 1, 1, 1, 0, 704, 100
39803, V, 1, 1, 1, 1, 0, 704, 100
39804, V, 1, 1, 1, 1, 0, 704, 99
39805, V, 1, 1, 1, 1, 0, 704, 100
39806, V, 1, 1, 1, 1, 0, 704, 100
39808, V, 1, 1, 1, 1, 0, 704, 100
39809, V, 1, 1, 1, 1, 0, 704, 100
39810, V, 1, 1, 1, 1, 0, 704, 100
39811, V, 1, 1, 1, 1, 0, 704, 99
39812, V, 1, 1, 1, 1, 0, 704, 99
39813, V, 1, 1, 1, 1, 0, 704, 99
39814, V, 1, 1, 1, 1, 0, 704, 100
39815, V, 1, 1, 1, 1, 0, 704, 99
39816, V, 1, 1, 1, 1, 0, 704, 99
39817, V, 1, 1, 1, 1, 0, 704, 99
39818, V, 1, 1, 1, 1, 0, 704, 99
39819, V, 1, 1, 1, 1, 0, 704, 99
39820, V, 1, 1, 1, 1, 0, 704, 99
39821, V, 1, 1, 1, 1, 0, 704, 99
39822, V, 1, 1, 1, 1, 0, 704, 99
39823, V, 1, 1, 1, 1, 0, 704, 99
39824, V, 1, 1, 1, 1, 0, 704, 99
39825, V, 1, 1, 1, 1, 0, 704, 99
39826, V, 1, 1, 1, 1, 0, 704, 99
39827, V, 1, 1, 1, 1, 0, 704, 99
39828, V, 1, 1, 1, 1, 0, 704, 99
39829, V, 1, 1, 1, 1, 0, 704, 99
39830, V, 1, 1, 1, 1, 0, 704, 99
39831, V, 1, 1, 1, 1, 0, 704, 99
39832, V, 1, 1, 1, 1, 0, 704, 99
39833, V, 1, 1, 1, 1, 0, 704, 99
39834, V, 1, 1, 1, 1, 0, 704, 99
39835, V, 1, 1, 1, 1, 0, 704, 99
39836, V, 1, 1, 1, 1, 0, 704, 99
39837, V, 1, 1, 1, 1, 0, 704, 99
39838, V, 1, 1, 1, 1, 0, 704, 99
39839, V, 1, 1, 1, 1, 0, 704, 99
39840, V, 1, 1, 1, 1, 0, 704, 99
39841, V, 1, 1, 1, 1, 0, 704, 99
39842, V, 1, 1, 1, 1, 0, 704, 99
39843, V, 1, 1, 1, 1, 0, 704, 99
39844, V, 1, 1, 1, 1, 0, 704, 99
39845, V, 1, 1, 1, 1, 0, 704, 99
39846, V, 1, 1, 1, 1, 0, 704, 99
39847, V, 1, 1, 1, 1, 0, 704, 99
39848, V, 1, 1, 1, 1, 0, 704, 99
39849, V, 1, 1, 1, 1, 0, 704, 99
39851, V, 1, 1, 1, 1, 0, 704, 99
39852, V, 1, 1, 1, 1, 0, 704, 99
39853, V, 1, 1, 1, 1, 0, 704, 99
39854, V, 1, 1, 1, 1, 0, 704, 99
39855, V, 1, 1, 1, 1, 0, 704, 99
39856, V, 1, 1, 1, 1, 0, 704, 99
39857, V, 1, 1, 1, 1, 0, 704, 99
39858, V, 1, 1, 1, 1, 0, 704, 99
39859, V, 1, 1, 1, 1, 0, 704, 99
39860, V, 1, 1, 1, 1, 0, 704, 99
39861, V, 1, 1, 1, 1, 0, 704, 99
39862, V, 1, 1, 1, 1, 0, 704, 99
39863, V, 1, 1, 1, 1, 0, 704, 99
39864, V, 1, 1, 1, 1, 0, 704, 100
39865, V, 1, 1, 1, 1, 0, 704, 99
39866, V, 1, 1, 1, 1, 0, 704, 99
39867, V, 1, 1, 1, 1, 0, 704, 100
39868, V, 1, 1, 1, 1, 0, 704, 100
39869, V, 1, 1, 1, 1, 0, 704, 100
39870, V, 1, 1, 1, 1, 0, 704, 100
39871, V, 1, 1, 1, 1, 0, 704, 99
39872, V, 1, 1, 1, 1, 0, 704, 100
39873, V, 1, 1, 1, 1, 0, 704, 99
39874, V, 1, 1, 1, 1, 0, 704, 100
39875, V, 1, 1, 1, 1, 0, 704, 99
39876, V, 1, 1, 1, 1, 0, 704, 99
39877, V, 1, 1, 1, 1, 0, 704, 99
39878, V, 1, 1, 1, 1, 0, 704, 99
39879, V, 1, 1, 1, 1, 0, 704, 100
39880, V, 1, 1, 1, 1, 0, 704, 99
39881, V, 1, 1, 1, 1, 0, 704, 100
39882, V, 1, 1, 1, 1, 0, 704, 99
39883, V, 1, 1, 1, 1, 0, 704, 99
39884, V, 1, 1, 1, 1, 0, 704, 99
39885, V, 1, 1, 1, 1, 0, 704, 100
39886, V, 1, 1, 1, 1, 0, 704, 100
39887, V, 1, 1, 1, 1, 0, 704, 99
39888, V, 1, 1, 1, 1, 0, 704, 99
39889, V, 1, 1, 1, 1, 0, 704, 100
39890, V, 1, 1, 1, 1, 0, 704, 99
39891, V, 1, 1, 1, 1, 0, 704, 99
39892, V, 1, 1, 1, 1, 0, 704, 99
39894, V, 1, 1, 1, 1, 0, 704, 99
39895, V, 1, 1, 1, 1, 0, 704, 99
39896, V, 1, 1, 1, 1, 0, 704, 99
39897, V, 1, 1, 1, 1, 0, 704, 99
39898, V, 1, 1, 1, 1, 0, 704, 99
39899, V, 1, 1, 1, 1, 0, 704, 99
39900, V, 1, 1, 1, 1, 0, 704, 99
39901, V, 1, 1, 1, 1, 0, 704, 99
39902, V, 1, 1, 1, 1, 0, 704, 99
39903, V, 1, 1, 1, 1, 0, 704, 99
39904, V, 1, 1, 1, 1, 0, 704, 99
39905, V, 1, 1, 1, 1, 0, 704, 99
39906, V, 1, 1, 1, 1, 0, 704, 99
39907, V, 1, 1, 1, 1, 0, 704, 99
39908, V, 1, 1, 1, 1, 0, 704, 99
39909, V, 1, 1, 1, 1, 0, 704, 99
39910, V, 1, 1, 1, 1, 0, 704, 99
39911, V, 1, 1, 1, 1, 0, 704, 99
39912, V, 1, 1, 1, 1, 0, 704, 99
39913, V, 1, 1, 1, 1, 0, 704, 99
39914, V, 1, 1, 1, 1, 0, 704, 99
39915, V, 1, 1, 1, 1, 0, 704, 99
39916, V, 1, 1, 1, 1, 0, 704, 99
39917, V, 1, 1, 1, 1, 0, 704, 99
39918, V, 1, 1, 1, 1, 0, 704, 99
39919, V, 1, 1, 1, 1, 0, 704, 99
39920, V, 1, 1, 1, 1, 0, 704, 99
39921, V, 1, 1, 1, 1, 0, 704, 99
39922, V, 1, 1, 1, 1, 0, 704, 99
39923, V, 1, 1, 1, 1, 0, 704, 99
39924, V, 1, 1, 1, 1, 0, 704, 99
39925, V, 1, 1, 1, 1, 0, 704, 99
39926, V, 1, 1, 1, 1, 0, 704, 99
39927, V, 1, 1, 1, 1, 0, 704, 100
39928, V, 1, 1, 1, 1, 0, 704, 99
39929, V, 1, 1, 1, 1, 0, 704, 100
39930, V, 1, 1, 1, 1, 0, 704, 99
39931, V, 1, 1, 1, 1, 0, 704, 99
39932, V, 1, 1, 1, 1, 0, 704, 100
39933, V, 1, 1, 1, 1, 0, 704, 99
39934, V, 1, 1, 1, 1, 0, 704, 99
39936, V, 1, 1, 1, 1, 0, 704, 99
39937, V, 1, 1, 1, 1, 0, 704, 100
39938, V, 1, 1, 1, 1, 0, 704, 99
39939, V, 1, 1, 1, 1, 0, 704, 100
39940, V, 1, 1, 1, 1, 0, 704, 100
39941, V, 1, 1, 1, 1, 0, 704, 100
39942, V, 1, 1, 1, 1, 0, 704, 100
39943, V, 1, 1, 1, 1, 0, 704, 99
39944, V, 1, 1, 1, 1, 0, 704, 99
39945, V, 1, 1, 1, 1, 0, 704, 100
39946, V, 1, 1, 1, 1, 0, 704, 99
39947, V, 1, 1, 1, 1, 0, 704, 100
39948, V, 1, 1, 1, 1, 0, 704, 100
39949, V, 1, 1, 1, 1, 0, 704, 99
39950, V, 1, 1, 1, 1, 0, 704, 99
39951, V, 1, 1, 1, 1, 0, 704, 99
39952, V, 1, 1, 1, 1, 0, 704, 100
39953, V, 1, 1, 1, 1, 0, 704, 100
39954, V, 1, 1, 1, 1, 0, 704, 99
39955, V, 1, 1, 1, 1, 0, 704, 99
39956, V, 1, 1, 1, 1, 0, 704, 99
39957, V, 1, 1, 1, 1, 0, 704, 99
39958, V, 1, 1, 1, 1, 0, 704, 99
39959, V, 1, 1, 1, 1, 0, 704, 99
39960, V, 1, 1, 1, 1, 0, 704, 99
39961, V, 1, 1, 1, 1, 0, 704, 99
39962, V, 1, 1, 1, 1, 0, 704, 100
39963, V, 1, 1, 1, 1, 0, 704, 99
39964, V, 1, 1, 1, 1, 0, 704, 99
39965, V, 1, 1, 1, 1, 0, 704, 99
39966, V, 1, 1, 1, 1, 0, 704, 99
39967, V, 1, 1, 1, 1, 0, 704, 99
39968, V, 1, 1, 1, 1, 0, 704, 99
39969, V, 1, 1, 1, 1, 0, 704, 99
39970, V, 1, 1, 1, 1, 0, 704, 99
39971, V, 1, 1, 1, 1, 0, 704, 99
39972, V, 1, 1, 1, 1, 0, 704, 99
39973, V, 1, 1, 1, 1, 0, 704, 99
39974, V, 1, 1, 1, 1, 0, 704, 99
39975, V, 1, 1, 1, 1, 0, 704, 99
39976, V, 1, 1, 1, 1, 0, 704, 99
39977, V, 1, 1, 1, 1, 0, 704, 99
39979, V, 1, 1, 1, 1, 0, 704, 99
39980, V, 1, 1, 1, 1, 0, 704, 99
39981, V, 1, 1, 1, 1, 0, 704, 99
39982, V, 1, 1, 1, 1, 0, 704, 99
39983, V, 1, 1, 1, 1, 0, 704, 99
39984, V, 1, 1, 1, 1, 0, 704, 99
39985, V, 1, 1, 1, 1, 0, 704, 99
39986, V, 1, 1, 1, 1, 0, 704, 99
39987, V, 1, 1, 1, 1, 0, 704, 99
39988, V, 1, 1, 1, 1, 0, 704, 99
39989, V, 1, 1, 1, 1, 0, 704, 99
39990, V, 1, 1, 1, 1, 0, 704, 99
39991, V, 1, 1, 1, 1, 0, 704, 99
39992, V, 1, 1, 1, 1, 0, 704, 99
39993, V, 1, 1, 1, 1, 0, 704, 99
39994, V, 1, 1, 1, 1, 0, 704, 99
39995, V, 1, 1, 1, 1, 0, 704, 99
39996, V, 1, 1, 1, 1, 0, 704, 99
39997, V, 1, 1, 1, 1, 0, 704, 99
39998, V, 1, 1, 1, 1, 0, 704, 99
39999, V, 1, 1, 1, 1, 0, 704, 99
40000, V, 1, 1, 1, 1, 0, 704, 99
40001, V, 1, 1, 1, 1, 0, 704, 99
40002, V, 1, 1, 1, 1, 0, 704, 99
40003, V, 1, 1, 1, 1, 0, 704, 99
40004, V, 1, 1, 1, 1, 0, 704, 99
40005, V, 1, 1, 1, 1, 0, 704, 99
40006, V, 1, 1, 1, 1, 0, 704, 99
40007, V, 1, 1, 1, 1, 0, 704, 99
40008, V, 1, 1, 1, 1, 0, 704, 99
40009, V, 1, 1, 1, 1, 0, 704, 99
40010, V, 1, 1, 1, 1, 0, 704, 99
40011, V, 1, 1, 1, 1, 0, 704, 100
40012, V, 1, 1, 1, 1, 0, 704, 99
40013, V, 1, 1, 1, 1, 0, 704, 99
40014, V, 1, 1, 1, 1, 0, 704, 99
40015, V, 1, 1, 1, 1, 0, 704, 99
40016, V, 1, 1, 1, 1, 0, 704, 99
40017, V, 1, 1, 1, 1, 0, 704, 99
40018, V, 1, 1, 1, 1, 0, 704, 99
40019, V, 1, 1, 1, 1, 0, 704, 99
40020, V, 1, 1, 1, 1, 0, 704, 99
40022, V, 1, 1, 1, 1, 0, 704, 99
40023, V, 1, 1, 1, 1, 0, 704, 99
40024, V, 1, 1, 1, 1, 0, 704, 100
40025, V, 1, 1, 1, 1, 0, 704, 99
40026, V, 1, 1, 1, 1, 0, 704, 99
40027, V, 1, 1, 1, 1, 0, 704, 99
40028, V, 1, 1, 1, 1, 0, 704, 99
40029, V, 1, 1, 1, 1, 0, 704, 99
40030, V, 1, 1, 1, 1, 0, 704, 99
40031, V, 1, 1, 1, 1, 0, 704, 99
40032, V, 1, 1, 1, 1, 0, 704, 99
40033, V, 1, 1, 1, 1, 0, 704, 99
40034, V, 1, 1, 1, 1, 0, 704, 99
40035, V, 1, 1, 1, 1, 0, 704, 99
40036, V, 1, 1, 1, 1, 0, 704, 99
40037, V, 1, 1, 1, 1, 0, 704, 99
40038, V, 1, 1, 1, 1, 0, 704, 99
40039, V, 1, 1, 1, 1, 0, 704, 99
40040, V, 1, 1, 1, 1, 0, 704, 99
40041, V, 1, 1, 1, 1, 0, 704, 99
40042, V, 1, 1, 1, 1, 0, 704, 99
40043, V, 1, 1, 1, 1, 0, 704, 99
40044, V, 1, 1, 1, 1, 0, 704, 99
40045, V, 1, 1, 1, 1, 0, 704, 99
40046, V, 1, 1, 1, 1, 0, 704, 99
40047, V, 1, 1, 1, 1, 0, 704, 99
40048, V, 1, 1, 1, 1, 0, 704, 99
40049, V, 1, 1, 1, 1, 0, 704, 99
40050, V, 1, 1, 1, 1, 0, 704, 99
40051, V, 1, 1, 1, 1, 0, 704, 99
40052, V, 1, 1, 1, 1, 0, 704, 99
40053, V, 1, 1, 1, 1, 0, 704, 99
40054, V, 1, 1, 1, 1, 0, 704, 99
40055, V, 1, 1, 1, 1, 0, 704, 99
40056, V, 1, 1, 1, 1, 0, 704, 99
40057, V, 1, 1, 1, 1, 0, 704, 99
40058, V, 1, 1, 1, 1, 0, 704, 99
40059, V, 1, 1, 1, 1, 0, 704, 99
40060, V, 1, 1, 1, 1, 0, 704, 99
40061, V, 1, 1, 1, 1, 0, 704, 99
40062, V, 1, 1, 1, 1, 0, 704, 99
40064, V, 1, 1, 1, 1, 0, 704, 99
40065, V, 1, 1, 1, 1, 0, 704, 99
40066, V, 1, 1, 1, 1, 0, 704, 99
40067, V, 1, 1, 1, 1, 0, 704, 99
40068, V, 1, 1, 1, 1, 0, 704, 99
40069, V, 1, 1, 1, 1, 0, 704, 99
40070, V, 1, 1, 1, 1, 0, 704, 99
40071, V, 1, 1, 1, 1, 0, 704, 99
40072, V, 1, 1, 1, 1, 0, 704, 99
40073, V, 1, 1, 1, 1, 0, 704, 99
40074, V, 1, 1, 1, 1, 0, 704, 99
40075, V, 1, 1, 1, 1, 0, 704, 99
40076, V, 1, 1, 1, 1, 0, 704, 99
40077, V, 1, 1, 1, 1, 0, 704, 99
40078, V, 1, 1, 1, 1, 0, 704, 99
40079, V, 1, 1, 1, 1, 0, 704, 99
40080, V, 1, 1, 1, 1, 0, 704, 99
40081, V, 1, 1, 1, 1, 0, 704, 99
40082, V, 1, 1, 1, 1, 0, 704, 99
40083, V, 1, 1, 1, 1, 0, 704, 99
40084, V, 1, 1, 1, 1, 0, 704, 99
40085, V, 1, 1, 1, 1, 0, 704, 99
40086, V, 1, 1, 1, 1, 0, 704, 99
40087, V, 1, 1, 1, 1, 0, 704, 100
40088, V, 1, 1, 1, 1, 0, 704, 99
40089, V, 1, 1, 1, 1, 0, 704, 99
40090, V, 1, 1, 1, 1, 0, 704, 99
40091, V, 1, 1, 1, 1, 0, 704, 100
40092, V, 1, 1, 1, 1, 0, 704, 99
40093, V, 1, 1, 1, 1, 0, 704, 99
40094, V, 1, 1, 1, 1, 0, 704, 99
40095, V, 1, 1, 1, 1, 0, 704, 99
40096, V, 1, 1, 1, 1, 0, 704, 99
40097, V, 1, 1, 1, 1, 0, 704, 99
40098, V, 1, 1, 1, 1, 0, 704, 99
40099, V, 1, 1, 1, 1, 0, 704, 99
40100, V, 1, 1, 1, 1, 0, 704, 100
40101, V, 1, 1, 1, 1, 0, 704, 99
40102, V, 1, 1, 1, 1, 0, 704, 99
40103, V, 1, 1, 1, 1, 0, 704, 99
40104, V, 1, 1, 1, 1, 0, 704, 99
40105, V, 1, 1, 1, 1, 0, 704, 99
40107, V, 1, 1, 1, 1, 0, 704, 99
40108, V, 1, 1, 1, 1, 0, 704, 99
40109, V, 1, 1, 1, 1, 0, 704, 99
40110, V, 1, 1, 1, 1, 0, 704, 99
40111, V, 1, 1, 1, 1, 0, 704, 99
40112, V, 1, 1, 1, 1, 0, 704, 99
40113, V, 1, 1, 1, 1, 0, 704, 99
40114, V, 1, 1, 1, 1, 0, 704, 99
40115, V, 1, 1, 1, 1, 0, 704, 99
40116, V, 1, 1, 1, 1, 0, 704, 99
40117, V, 1, 1, 1, 1, 0, 704, 99
40118, V, 1, 1, 1, 1, 0, 704, 99
40119, V, 1, 1, 1, 1, 0, 704, 99
40120, V, 1, 1, 1, 1, 0, 704, 99
40121, V, 1, 1, 1, 1, 0, 704, 99
40122, V, 1, 1, 1, 1, 0, 704, 99
40123, V, 1, 1, 1, 1, 0, 704, 99
40124, V, 1, 1, 1, 1, 0, 704, 99
40125, V, 1, 1, 1, 1, 0, 704, 99
40126, V, 1, 1, 1, 1, 0, 704, 99
40127, V, 1, 1, 1, 1, 0, 704, 99
40128, V, 1, 1, 1, 1, 0, 704, 99
40129, V, 1, 1, 1, 1, 0, 704, 99
40130, V, 1, 1, 1, 1, 0, 704, 99
40131, V, 1, 1, 1, 1, 0, 704, 99
40132, V, 1, 1, 1, 1, 0, 704, 99
40133, V, 1, 1, 1, 1, 0, 704, 99
40134, V, 1, 1, 1, 1, 0, 704, 99
40135, V, 1, 1, 1, 1, 0, 704, 99
40136, V, 1, 1, 1, 1, 0, 704, 99
40137, V, 1, 1, 1, 1, 0, 704, 99
40138, V, 1, 1, 1, 1, 0, 704, 99
40139, V, 1, 1, 1, 1, 0, 704, 99
40140, V, 1, 1, 1, 1, 0, 704, 99
40141, V, 1, 1, 1, 1, 0, 704, 99
40142, V, 1, 1, 1, 1, 0, 704, 99
40143, V, 1, 1, 1, 1, 0, 704, 99
40144, V, 1, 1, 1, 1, 0, 704, 99
40145, V, 1, 1, 1, 1, 0, 704, 99
40146, V, 1, 1, 1, 1, 0, 704, 99
40147, V, 1, 1, 1, 1, 0, 704, 99
40148, V, 1, 1, 1, 1, 0, 704, 99
40150, V, 1, 1, 1, 1, 0, 704, 99
40151, V, 1, 1, 1, 1, 0, 704, 99
40152, V, 1, 1, 1, 1, 0, 704, 99
40153, V, 1, 1, 1, 1, 0, 704, 99
40154, V, 1, 1, 1, 1, 0, 704, 99
40155, V, 1, 1, 1, 1, 0, 704, 99
40156, V, 1, 1, 1, 1, 0, 704, 99
40157, V, 1, 1, 1, 1, 0, 704, 99
40158, V, 1, 1, 1, 1, 0, 704, 99
40159, V, 1, 1, 1, 1, 0, 704, 99
40160, V, 1, 1, 1, 1, 0, 704, 99
40161, V, 1, 1, 1, 1, 0, 704, 99
40162, V, 1, 1, 1, 1, 0, 704, 99
40163, V, 1, 1, 1, 1, 0, 704, 99
40164, V, 1, 1, 1, 1, 0, 704, 99
40165, V, 1, 1, 1, 1, 0, 704, 99
40166, V, 1, 1, 1, 1, 0, 704, 99
40167, V, 1, 1, 1, 1, 0, 704, 99
40168, V, 1, 1, 1, 1, 0, 704, 99
40169, V, 1, 1, 1, 1, 0, 704, 99
40170, V, 1, 1, 1, 1, 0, 704, 99
40171, V, 1, 1, 1, 1, 0, 704, 99
40172, V, 1, 1, 1, 1, 0, 704, 99
40173, V, 1, 1, 1, 1, 0, 704, 99
40174, V, 1, 1, 1, 1, 0, 704, 99
40175, V, 1, 1, 1, 1, 0, 704, 99
40176, V, 1, 1, 1, 1, 0, 704, 99
40177, V, 1, 1, 1, 1, 0, 704, 99
40178, V, 1, 1, 1, 1, 0, 704, 99
40179, V, 1, 1, 1, 1, 0, 704, 99
40180, V, 1, 1, 1, 1, 0, 704, 99
40181, V, 1, 1, 1, 1, 0, 704, 99
40182, V, 1, 1, 1, 1, 0, 704, 99
40183, V, 1, 1, 1, 1, 0, 704, 99
40184, V, 1, 1, 1, 1, 0, 704, 99
40185, V, 1, 1, 1, 1, 0, 704, 100
40186, V, 1, 1, 1, 1, 0, 704, 99
40187, V, 1, 1, 1, 1, 0, 704, 99
40188, V, 1, 1, 1, 1, 0, 704, 99
40189, V, 1, 1, 1, 1, 0, 704, 99
40190, V, 1, 1, 1, 1, 0, 704, 99
40192, V, 1, 1, 1, 1, 0, 704, 99
40193, V, 1, 1, 1, 1, 0, 704, 99
40194, V, 1, 1, 1, 1, 0, 704, 99
40195, V, 1, 1, 1, 1, 0, 704, 99
40196, V, 1, 1, 1, 1, 0, 704, 99
40197, V, 1, 1, 1, 1, 0, 704, 99
40198, V, 1, 1, 1, 1, 0, 704, 99
40199, V, 1, 1, 1, 1, 0, 704, 99
40200, V, 1, 1, 1, 1, 0, 704, 99
40201, V, 1, 1, 1, 1, 0, 704, 99
40202, V, 1, 1, 1, 1, 0, 704, 99
40203, V, 1, 1, 1, 1, 0, 704, 99
40204, V, 1, 1, 1, 1, 0, 704, 99
40205, V, 1, 1, 1, 1, 0, 704, 99
40206, V, 1, 1, 1, 1, 0, 704, 99
40207, V, 1, 1, 1, 1, 0, 704, 99
40208, V, 1, 1, 1, 1, 0, 704, 99
40209, V, 1, 1, 1, 1, 0, 704, 99
40210, V, 1, 1, 1, 1, 0, 704, 99
40211, V, 1, 1, 1, 1, 0, 704, 99
40212, V, 1, 1, 1, 1, 0, 704, 99
40213, V, 1, 1, 1, 1, 0, 704, 99
40214, V, 1, 1, 1, 1, 0, 704, 99
40215, V, 1, 1, 1, 1, 0, 704, 99
40216, V, 1, 1, 1, 1, 0, 704, 99
40217, V, 1, 1, 1, 1, 0, 704, 99
40218, V, 1, 1, 1, 1, 0, 704, 99
40219, V, 1, 1, 1, 1, 0, 704, 99
40220, V, 1, 1, 1, 1, 0, 704, 99
40221, V, 1, 1, 1, 1, 0, 704, 99
40222, V, 1, 1, 1, 1, 0, 704, 99
40223, V, 1, 1, 1, 1, 0, 704, 99
40224, V, 1, 1, 1, 1, 0, 704, 99
40225, V, 1, 1, 1, 1, 0, 704, 99
40226, V, 1, 1, 1, 1, 0, 704, 99
40227, V, 1, 1, 1, 1, 0, 704, 99
40228, V, 1, 1, 1, 1, 0, 704, 99
40229, V, 1, 1, 1, 1, 0, 704, 99
40230, V, 1, 1, 1, 1, 0, 704, 99
40231, V, 1, 1, 1, 1, 0, 704, 99
40232, V, 1, 1, 1, 1, 0, 704, 99
40233, V, 1, 1, 1, 1, 0, 704, 99
40235, V, 1, 1, 1, 1, 0, 704, 99
40236, V, 1, 1, 1, 1, 0, 704, 99
40237, V, 1, 1, 1, 1, 0, 704, 99
40238, V, 1, 1, 1, 1, 0, 704, 99
40239, V, 1, 1, 1, 1, 0, 704, 99
40240, V, 1, 1, 1, 1, 0, 704, 99
40241, V, 1, 1, 1, 1, 0, 704, 99
40242, V, 1, 1, 1, 1, 0, 704, 99
40243, V, 1, 1, 1, 1, 0, 704, 99
40244, V, 1, 1, 1, 1, 0, 704, 99
40245, V, 1, 1, 1, 1, 0, 704, 99
40246, V, 1, 1, 1, 1, 0, 704, 99
40247, V, 1, 1, 1, 1, 0, 704, 99
40248, V, 1, 1, 1, 1, 0, 704, 99
40249, V, 1, 1, 1, 1, 0, 704, 100
40250, V, 1, 1, 1, 1, 0, 704, 99
40251, V, 1, 1, 1, 1, 0, 704, 99
40252, V, 1, 1, 1, 1, 0, 704, 99
40253, V, 1, 1, 1, 1, 0, 704, 99
40254, V, 1, 1, 1, 1, 0, 704, 99
40255, V, 1, 1, 1, 1, 0, 704, 99
40256, V, 1, 1, 1, 1, 0, 704, 99
40257, V, 1, 1, 1, 1, 0, 704, 99
40258, V, 1, 1, 1, 1, 0, 704, 99
40259, V, 1, 1, 1, 1, 0, 704, 99
40260, V, 1, 1, 1, 1, 0, 704, 99
40261, V, 1, 1, 1, 1, 0, 704, 99
40262, V, 1, 1, 1, 1, 0, 704, 99
40263, V, 1, 1, 1, 1, 0, 704, 99
40264, V, 1, 1, 1, 1, 0, 704, 99
40265, V, 1, 1, 1, 1, 0, 704, 99
40266, V, 1, 1, 1, 1, 0, 704, 99
40267, V, 1, 1, 1, 1, 0, 704, 99
40268, V, 1, 1, 1, 1, 0, 704, 99
40269, V, 1, 1, 1, 1, 0, 704, 99
40270, V, 1, 1, 1, 1, 0, 704, 99
40271, V, 1, 1, 1, 1, 0, 704, 99
40272, V, 1, 1, 1, 1, 0, 704, 99
40273, V, 1, 1, 1, 1, 0, 704, 99
40274, V, 1, 1, 1, 1, 0, 704, 99
40275, V, 1, 1, 1, 1, 0, 704, 99
40276, V, 1, 1, 1, 1, 0, 704, 99
40278, V, 1, 1, 1, 1, 0, 704, 99
40279, V, 1, 1, 1, 1, 0, 704, 99
40280, V, 1, 1, 1, 1, 0, 704, 99
40281, V, 1, 1, 1, 1, 0, 704, 99
40282, V, 1, 1, 1, 1, 0, 704, 99
40283, V, 1, 1, 1, 1, 0, 704, 99
40284, V, 1, 1, 1, 1, 0, 704, 99
40285, V, 1, 1, 1, 1, 0, 704, 99
40286, V, 1, 1, 1, 1, 0, 704, 99
40287, V, 1, 1, 1, 1, 0, 704, 99
40288, V, 1, 1, 1, 1, 0, 704, 99
40289, V, 1, 1, 1, 1, 0, 704, 99
40290, V, 1, 1, 1, 1, 0, 704, 99
40291, V, 1, 1, 1, 1, 0, 704, 99
40292, V, 1, 1, 1, 1, 0, 704, 99
40293, V, 1, 1, 1, 1, 0, 704, 99
40294, V, 1, 1, 1, 1, 0, 704, 99
40295, V, 1, 1, 1, 1, 0, 704, 99
40296, V, 1, 1, 1, 1, 0, 704, 99
40297, V, 1, 1, 1, 1, 0, 704, 99
40298, V, 1, 1, 1, 1, 0, 704, 99
40299, V, 1, 1, 1, 1, 0, 704, 99
40300, V, 1, 1, 1, 1, 0, 704, 99
40301, V, 1, 1, 1, 1, 0, 704, 99
40302, V, 1, 1, 1, 1, 0, 704, 99
40303, V, 1, 1, 1, 1, 0, 704, 99
40304, V, 1, 1, 1, 1, 0, 704, 99
40305, V, 1, 1, 1, 1, 0, 704, 99
40306, V, 1, 1, 1, 1, 0, 704, 99
40307, V, 1, 1, 1, 1, 0, 704, 99
40308, V, 1, 1, 1, 1, 0, 704, 99
40309, V, 1, 1, 1, 1, 0, 704, 99
40310, V, 1, 1, 1, 1, 0, 704, 99
40311, V, 1, 1, 1, 1, 0, 704, 99
40312, V, 1, 1, 1, 1, 0, 704, 99
40313, V, 1, 1, 1, 1, 0, 704, 99
40314, V, 1, 1, 1, 1, 0, 704, 99
40315, V, 1, 1, 1, 1, 0, 704, 99
40316, V, 1, 1, 1, 1, 0, 704, 99
40317, V, 1, 1, 1, 1, 0, 704, 99
40318, V, 1, 1, 1, 1, 0, 704, 99
40320, V, 1, 1, 1, 1, 0, 704, 99
40321, V, 1, 1, 1, 1, 0, 704, 99
40322, V, 1, 1, 1, 1, 0, 704, 100
40323, V, 1, 1, 1, 1, 0, 704, 99
40324, V, 1, 1, 1, 1, 0, 704, 99
40325, V, 1, 1, 1, 1, 0, 704, 99
40326, V, 1, 1, 1, 1, 0, 704, 99
40327, V, 1, 1, 1, 1, 0, 704, 100
40328, V, 1, 1, 1, 1, 0, 704, 99
40329, V, 1, 1, 1, 1, 0, 704, 99
40330, V, 1, 1, 1, 1, 0, 704, 99
40331, V, 1, 1, 1, 1, 0, 704, 99
40332, V, 1, 1, 1, 1, 0, 704, 99
40333, V, 1, 1, 1, 1, 0, 704, 99
40334, V, 1, 1, 1, 1, 0, 704, 99
40335, V, 1, 1, 1, 1, 0, 704, 99
40336, V, 1, 1, 1, 1, 0, 704, 99
40337, V, 1, 1, 1, 1, 0, 704, 99
40338, V, 1, 1, 1, 1, 0, 704, 99
40339, V, 1, 1, 1, 1, 0, 704, 99
40340, V, 1, 1, 1, 1, 0, 704, 99
40341, V, 1, 1, 1, 1, 0, 704, 99
40342, V, 1, 1, 1, 1, 0, 704, 99
40343, V, 1, 1, 1, 1, 0, 704, 99
40344, V, 1, 1, 1, 1, 0, 704, 99
40345, V, 1, 1, 1, 1, 0, 704, 99
40346, V, 1, 1, 1, 1, 0, 704, 99
40347, V, 1, 1, 1, 1, 0, 704, 99
40348, V, 1, 1, 1, 1, 0, 704, 99
40349, V, 1, 1, 1, 1, 0, 704, 99
40350, V, 1, 1, 1, 1, 0, 704, 99
40351, V, 1, 1, 1, 1, 0, 704, 99
40352, V, 1, 1, 1, 1, 0, 704, 99
40353, V, 1, 1, 1, 1, 0, 704, 99
40354, V, 1, 1, 1, 1, 0, 704, 99
40355, V, 1, 1, 1, 1, 0, 704, 99
40356, V, 1, 1, 1, 1, 0, 704, 99
40357, V, 1, 1, 1, 1, 0, 704, 99
40358, V, 1, 1, 1, 1, 0, 704, 99
40359, V, 1, 1, 1, 1, 0, 704, 99
40360, V, 1, 1, 1, 1, 0, 704, 99
40361, V, 1, 1, 1, 1, 0, 704, 99
40363, V, 1, 1, 1, 1, 0, 704, 99
40364, V, 1, 1, 1, 1, 0, 704, 99
40365, V, 1, 1, 1, 1, 0, 704, 99
40366, V, 1, 1, 1, 1, 0, 704, 99
40367, V, 1, 1, 1, 1, 0, 704, 99
40368, V, 1, 1, 1, 1, 0, 704, 99
40369, V, 1, 1, 1, 1, 0, 704, 99
40370, V, 1, 1, 1, 1, 0, 704, 99
40371, V, 1, 1, 1, 1, 0, 704, 99
40372, V, 1, 1, 1, 1, 0, 704, 99
40373, V, 1, 1, 1, 1, 0, 704, 99
40374, V, 1, 1, 1, 1, 0, 704, 99
40375, V, 1, 1, 1, 1, 0, 704, 99
40376, V, 1, 1, 1, 1, 0, 704, 99
40377, V, 1, 1, 1, 1, 0, 704, 99
40378, V, 1, 1, 1, 1, 0, 704, 99
40379, V, 1, 1, 1, 1, 0, 704, 99
40380, V, 1, 1, 1, 1, 0, 704, 99
40381, V, 1, 1, 1, 1, 0, 704, 99
40382, V, 1, 1, 1, 1, 0, 704, 99
40383, V, 1, 1, 1, 1, 0, 704, 99
40384, V, 1, 1, 1, 1, 0, 704, 99
40385, V, 1, 1, 1, 1, 0, 704, 99
40386, V, 1, 1, 1, 1, 0, 704, 99
40387, V, 1, 1, 1, 1, 0, 704, 99
40388, V, 1, 1, 1, 1, 0, 704, 99
40389, V, 1, 1, 1, 1, 0, 704, 99
40390, V, 1, 1, 1, 1, 0, 704, 99
40391, V, 1, 1, 1, 1, 0, 704, 99
40392, V, 1, 1, 1, 1, 0, 704, 99
40393, V, 1, 1, 1, 1, 0, 704, 99
40394, V, 1, 1, 1, 1, 0, 704, 99
40395, V, 1, 1, 1, 1, 0, 704, 99
40396, V, 1, 1, 1, 1, 0, 704, 99
40397, V, 1, 1, 1, 1, 0, 704, 99
40398, V, 1, 1, 1, 1, 0, 704, 99
40399, V, 1, 1, 1, 1, 0, 704, 99
40400, V, 1, 1, 1, 1, 0, 704, 99
40401, V, 1, 1, 1, 1, 0, 704, 99
40402, V, 1, 1, 1, 1, 0, 704, 99
40403, V, 1, 1, 1, 1, 0, 704, 99
40404, V, 1, 1, 1, 1, 0, 704, 99
40406, V, 1, 1, 1, 1, 0, 704, 100
40407, V, 1, 1, 1, 1, 0, 704, 99
40408, V, 1, 1, 1, 1, 0, 704, 100
40409, V, 1, 1, 1, 1, 0, 704, 99
40410, V, 1, 1, 1, 1, 0, 704, 99
40411, V, 1, 1, 1, 1, 0, 704, 99
40412, V, 1, 1, 1, 1, 0, 704, 99
40413, V, 1, 1, 1, 1, 0, 704, 99
40414, V, 1, 1, 1, 1, 0, 704, 99
40415, V, 1, 1, 1, 1, 0, 704, 99
40416, V, 1, 1, 1, 1, 0, 704, 99
40417, V, 1, 1, 1, 1, 0, 704, 99
40418, V, 1, 1, 1, 1, 0, 704, 99
40419, V, 1, 1, 1, 1, 0, 704, 99
40420, V, 1, 1, 1, 1, 0, 704, 99
40421, V, 1, 1, 1, 1, 0, 704, 99
40422, V, 1, 1, 1, 1, 0, 704, 99
40423, V, 1, 1, 1, 1, 0, 704, 99
40424, V, 1, 1, 1, 1, 0, 704, 99
40425, V, 1, 1, 1, 1, 0, 704, 99
40426, V, 1, 1, 1, 1, 0, 704, 99
40427, V, 1, 1, 1, 1, 0, 704, 99
40428, V, 1, 1, 1, 1, 0, 704, 99
40429, V, 1, 1, 1, 1, 0, 704, 99
40430, V, 1, 1, 1, 1, 0, 704, 99
40431, V, 1, 1, 1, 1, 0, 704, 99
40432, V, 1, 1, 1, 1, 0, 704, 99
40433, V, 1, 1, 1, 1, 0, 704, 99
40434, V, 1, 1, 1, 1, 0, 704, 99
40435, V, 1, 1, 1, 1, 0, 704, 99
40436, V, 1, 1, 1, 1, 0, 704, 99
40437, V, 1, 1, 1, 1, 0, 704, 99
40438, V, 1, 1, 1, 1, 0, 704, 99
40439, V, 1, 1, 1, 1, 0, 704, 99
40440, V, 1, 1, 1, 1, 0, 704, 99
40441, V, 1, 1, 1, 1, 0, 704, 99
40442, V, 1, 1, 1, 1, 0, 704, 99
40443, V, 1, 1, 1, 1, 0, 704, 99
40444, V, 1, 1, 1, 1, 0, 704, 99
40445, V, 1, 1, 1, 1, 0, 704, 99
40446, V, 1, 1, 1, 1, 0, 704, 99
40448, V, 1, 1, 1, 1, 0, 704, 99
40449, V, 1, 1, 1, 1, 0, 704, 99
40450, V, 1, 1, 1, 1, 0, 704, 99
40451, V, 1, 1, 1, 1, 0, 704, 99
40452, V, 1, 1, 1, 1, 0, 704, 99
40453, V, 1, 1, 1, 1, 0, 704, 99
40454, V, 1, 1, 1, 1, 0, 704, 99
40455, V, 1, 1, 1, 1, 0, 704, 99
40456, V, 1, 1, 1, 1, 0, 704, 99
40457, V, 1, 1, 1, 1, 0, 704, 99
40458, V, 1, 1, 1, 1, 0, 704, 99
40459, V, 1, 1, 1, 1, 0, 704, 99
40460, V, 1, 1, 1, 1, 0, 704, 99
40461, V, 1, 1, 1, 1, 0, 704, 99
40462, V, 1, 1, 1, 1, 0, 704, 99
40463, V, 1, 1, 1, 1, 0, 704, 99
40464, V, 1, 1, 1, 1, 0, 704, 99
40465, V, 1, 1, 1, 1, 0, 704, 99
40466, V, 1, 1, 1, 1, 0, 704, 99
40467, V, 1, 1, 1, 1, 0, 704, 99
40468, V, 1, 1, 1, 1, 0, 704, 99
40469, V, 1, 1, 1, 1, 0, 704, 99
40470, V, 1, 1, 1, 1, 0, 704, 99
40471, V, 1, 1, 1, 1, 0, 704, 100
40472, V, 1, 1, 1, 1, 0, 704, 99
40473, V, 1, 1, 1, 1, 0, 704, 99
40474, V, 1, 1, 1, 1, 0, 704, 99
40475, V, 1, 1, 1, 1, 0, 704, 99
40476, V, 1, 1, 1, 1, 0, 704, 99
40477, V, 1, 1, 1, 1, 0, 704, 99
40478, V, 1, 1, 1, 1, 0, 704, 99
40479, V, 1, 1, 1, 1, 0, 704, 99
40480, V, 1, 1, 1, 1, 0, 704, 99
40481, V, 1, 1, 1, 1, 0, 704, 99
40482, V, 1, 1, 1, 1, 0, 704, 99
40483, V, 1, 1, 1, 1, 0, 704, 99
40484, V, 1, 1, 1, 1, 0, 704, 99
40485, V, 1, 1, 1, 1, 0, 704, 99
40486, V, 1, 1, 1, 1, 0, 704, 99
40487, V, 1, 1, 1, 1, 0, 704, 99
40488, V, 1, 1, 1, 1, 0, 704, 99
40489, V, 1, 1, 1, 1, 0, 704, 100
40491, V, 1, 1, 1, 1, 0, 704, 99
40492, V, 1, 1, 1, 1, 0, 704, 99
40493, V, 1, 1, 1, 1, 0, 704, 99
40494, V, 1, 1, 1, 1, 0, 704, 99
40495, V, 1, 1, 1, 1, 0, 704, 99
40496, V, 1, 1, 1, 1, 0, 704, 99
40497, V, 1, 1, 1, 1, 0, 704, 99
40498, V, 1, 1, 1, 1, 0, 704, 99
40499, V, 1, 1, 1, 1, 0, 704, 99
40500, V, 1, 1, 1, 1, 0, 704, 99
40501, V, 1, 1, 1, 1, 0, 704, 99
40502, V, 1, 1, 1, 1, 0, 704, 99
40503, V, 1, 1, 1, 1, 0, 704, 99
40504, V, 1, 1, 1, 1, 0, 704, 99
40505, V, 1, 1, 1, 1, 0, 704, 99
40506, V, 1, 1, 1, 1, 0, 704, 99
40507, V, 1, 1, 1, 1, 0, 704, 99
40508, V, 1, 1, 1, 1, 0, 704, 99
40509, V, 1, 1, 1, 1, 0, 704, 99
40510, V, 1, 1, 1, 1, 0, 704, 99
40511, V, 1, 1, 1, 1, 0, 704, 99
40512, V, 1, 1, 1, 1, 0, 704, 99
40513, V, 1, 1, 1, 1, 0, 704, 99
40514, V, 1, 1, 1, 1, 0, 704, 99
40515, V, 1, 1, 1, 1, 0, 704, 99
40516, V, 1, 1, 1, 1, 0, 704, 99
40517, V, 1, 1, 1, 1, 0, 704, 99
40518, V, 1, 1, 1, 1, 0, 704, 99
40519, V, 1, 1, 1, 1, 0, 704, 99
40520, V, 1, 1, 1, 1, 0, 704, 99
40521, V, 1, 1, 1, 1, 0, 704, 99
40522, V, 1, 1, 1, 1, 0, 704, 99
40523, V, 1, 1, 1, 1, 0, 704, 99
40524, V, 1, 1, 1, 1, 0, 704, 99
40525, V, 1, 1, 1, 1, 0, 704, 99
40526, V, 1, 1, 1, 1, 0, 704, 99
40527, V, 1, 1, 1, 1, 0, 704, 99
40528, V, 1, 1, 1, 1, 0, 704, 99
40529, V, 1, 1, 1, 1, 0, 704, 99
40530, V, 1, 1, 1, 1, 0, 704, 99
40531, V, 1, 1, 1, 1, 0, 704, 99
40532, V, 1, 1, 1, 1, 0, 704, 99
40534, V, 1, 1, 1, 1, 0, 704, 99
40535, V, 1, 1, 1, 1, 0, 704, 99
40536, V, 1, 1, 1, 1, 0, 704, 99
40537, V, 1, 1, 1, 1, 0, 704, 99
40538, V, 1, 1, 1, 1, 0, 704, 99
40539, V, 1, 1, 1, 1, 0, 704, 99
40540, V, 1, 1, 1, 1, 0, 704, 99
40541, V, 1, 1, 1, 1, 0, 704, 99
40542, V, 1, 1, 1, 1, 0, 704, 99
40543, V, 1, 1, 1, 1, 0, 704, 99
40544, V, 1, 1, 1, 1, 0, 704, 99
40545, V, 1, 1, 1, 1, 0, 704, 100
40546, V, 1, 1, 1, 1, 0, 704, 99
40547, V, 1, 1, 1, 1, 0, 704, 99
40548, V, 1, 1, 1, 1, 0, 704, 99
40549, V, 1, 1, 1, 1, 0, 704, 99
40550, V, 1, 1, 1, 1, 0, 704, 100
40551, V, 1, 1, 1, 1, 0, 704, 99
40552, V, 1, 1, 1, 1, 0, 704, 99
40553, V, 1, 1, 1, 1, 0, 704, 99
40554, V, 1, 1, 1, 1, 0, 704, 99
40555, V, 1, 1, 1, 1, 0, 704, 99
40556, V, 1, 1, 1, 1, 0, 704, 100
40557, V, 1, 1, 1, 1, 0, 704, 100
40558, V, 1, 1, 1, 1, 0, 704, 99
40559, V, 1, 1, 1, 1, 0, 704, 99
40560, V, 1, 1, 1, 1, 0, 704, 99
40561, V, 1, 1, 1, 1, 0, 704, 99
40562, V, 1, 1, 1, 1, 0, 704, 99
40563, V, 1, 1, 1, 1, 0, 704, 99
40564, V, 1, 1, 1, 1, 0, 704, 99
40565, V, 1, 1, 1, 1, 0, 704, 99
40566, V, 1, 1, 1, 1, 0, 704, 99
40567, V, 1, 1, 1, 1, 0, 704, 99
40568, V, 1, 1, 1, 1, 0, 704, 99
40569, V, 1, 1, 1, 1, 0, 704, 99
40570, V, 1, 1, 1, 1, 0, 704, 99
40571, V, 1, 1, 1, 1, 0, 704, 99
40572, V, 1, 1, 1, 1, 0, 704, 99
40573, V, 1, 1, 1, 1, 0, 704, 99
40574, V, 1, 1, 1, 1, 0, 704, 99
40576, V, 1, 1, 1, 1, 0, 704, 99
40577, V, 1, 1, 1, 1, 0, 704, 99
40578, V, 1, 1, 1, 1, 0, 704, 99
40579, V, 1, 1, 1, 1, 0, 704, 99
40580, V, 1, 1, 1, 1, 0, 704, 99
40581, V, 1, 1, 1, 1, 0, 704, 99
40582, V, 1, 1, 1, 1, 0, 704, 99
40583, V, 1, 1, 1, 1, 0, 704, 99
40584, V, 1, 1, 1, 1, 0, 704, 99
40585, V, 1, 1, 1, 1, 0, 704, 99
40586, V, 1, 1, 1, 1, 0, 704, 99
40587, V, 1, 1, 1, 1, 0, 704, 99
40588, V, 1, 1, 1, 1, 0, 704, 99
40589, V, 1, 1, 1, 1, 0, 704, 99
40590, V, 1, 1, 1, 1, 0, 704, 99
40591, V, 1, 1, 1, 1, 0, 704, 99
40592, V, 1, 1, 1, 1, 0, 704, 99
40593, V, 1, 1, 1, 1, 0, 704, 99
40594, V, 1, 1, 1, 1, 0, 704, 99
40595, V, 1, 1, 1, 1, 0, 704, 99
40596, V, 1, 1, 1, 1, 0, 704, 99
40597, V, 1, 1, 1, 1, 0, 704, 99
40598, V, 1, 1, 1, 1, 0, 704, 99
40599, V, 1, 1, 1, 1, 0, 704, 99
40600, V, 1, 1, 1, 1, 0, 704, 99
40601, V, 1, 1, 1, 1, 0, 704, 99
40602, V, 1, 1, 1, 1, 0, 704, 99
40603, V, 1, 1, 1, 1, 0, 704, 99
40604, V, 1, 1, 1, 1, 0, 704, 99
40605, V, 1, 1, 1, 1, 0, 704, 99
40606, V, 1, 1, 1, 1, 0, 704, 99
40607, V, 1, 1, 1, 1, 0, 704, 99
40608, V, 1, 1, 1, 1, 0, 704, 99
40609, V, 1, 1, 1, 1, 0, 704, 99
40610, V, 1, 1, 1, 1, 0, 704, 99
40611, V, 1, 1, 1, 1, 0, 704, 99
40612, V, 1, 1, 1, 1, 0, 704, 99
40613, V, 1, 1, 1, 1, 0, 704, 99
40614, V, 1, 1, 1, 1, 0, 704, 99
40615, V, 1, 1, 1, 1, 0, 704, 99
40616, V, 1, 1, 1, 1, 0, 704, 99
40617, V, 1, 1, 1, 1, 0, 704, 99
40619, V, 1, 1, 1, 1, 0, 704, 99
40620, V, 1, 1, 1, 1, 0, 704, 99
40621, V, 1, 1, 1, 1, 0, 704, 99
40622, V, 1, 1, 1, 1, 0, 704, 99
40623, V, 1, 1, 1, 1, 0, 704, 99
40624, V, 1, 1, 1, 1, 0, 704, 99
40625, V, 1, 1, 1, 1, 0, 704, 99
40626, V, 1, 1, 1, 1, 0, 704, 99
40627, V, 1, 1, 1, 1, 0, 704, 99
40628, V, 1, 1, 1, 1, 0, 704, 100
40629, V, 1, 1, 1, 1, 0, 704, 99
40630, V, 1, 1, 1, 1, 0, 704, 99
40631, V, 1, 1, 1, 1, 0, 704, 99
40632, V, 1, 1, 1, 1, 0, 704, 99
40633, V, 1, 1, 1, 1, 0, 704, 99
40634, V, 1, 1, 1, 1, 0, 704, 99
40635, V, 1, 1, 1, 1, 0, 704, 99
40636, V, 1, 1, 1, 1, 0, 704, 99
40637, V, 1, 1, 1, 1, 0, 704, 99
40638, V, 1, 1, 1, 1, 0, 704, 99
40639, V, 1, 1, 1, 1, 0, 704, 99
40640, V, 1, 1, 1, 1, 0, 704, 99
40641, V, 1, 1, 1, 1, 0, 704, 99
40642, V, 1, 1, 1, 1, 0, 704, 99
40643, V, 1, 1, 1, 1, 0, 704, 99
40644, V, 1, 1, 1, 1, 0, 704, 100
40645, V, 1, 1, 1, 1, 0, 704, 99
40646, V, 1, 1, 1, 1, 0, 704, 99
40647, V, 1, 1, 1, 1, 0, 704, 99
40648, V, 1, 1, 1, 1, 0, 704, 99
40649, V, 1, 1, 1, 1, 0, 704, 99
40650, V, 1, 1, 1, 1, 0, 704, 99
40651, V, 1, 1, 1, 1, 0, 704, 99
40652, V, 1, 1, 1, 1, 0, 704, 99
40653, V, 1, 1, 1, 1, 0, 704, 99
40654, V, 1, 1, 1, 1, 0, 704, 99
40655, V, 1, 1, 1, 1, 0, 704, 99
40656, V, 1, 1, 1, 1, 0, 704, 99
40657, V, 1, 1, 1, 1, 0, 704, 99
40658, V, 1, 1, 1, 1, 0, 704, 99
40659, V, 1, 1, 1, 1, 0, 704, 99
40660, V, 1, 1, 1, 1, 0, 704, 99
40662, V, 1, 1, 1, 1, 0, 704, 99
40663, V, 1, 1, 1, 1, 0, 704, 99
40664, V, 1, 1, 1, 1, 0, 704, 99
40665, V, 1, 1, 1, 1, 0, 704, 99
40666, V, 1, 1, 1, 1, 0, 704, 99
40667, V, 1, 1, 1, 1, 0, 704, 99
40668, V, 1, 1, 1, 1, 0, 704, 99
40669, V, 1, 1, 1, 1, 0, 704, 99
40670, V, 1, 1, 1, 1, 0, 704, 99
40671, V, 1, 1, 1, 1, 0, 704, 99
40672, V, 1, 1, 1, 1, 0, 704, 99
40673, V, 1, 1, 1, 1, 0, 704, 99
40674, V, 1, 1, 1, 1, 0, 704, 99
40675, V, 1, 1, 1, 1, 0, 704, 99
40676, V, 1, 1, 1, 1, 0, 704, 99
40677, V, 1, 1, 1, 1, 0, 704, 99
40678, V, 1, 1, 1, 1, 0, 704, 99
40679, V, 1, 1, 1, 1, 0, 704, 99
40680, V, 1, 1, 1, 1, 0, 704, 99
40681, V, 1, 1, 1, 1, 0, 704, 99
40682, V, 1, 1, 1, 1, 0, 704, 99
40683, V, 1, 1, 1, 1, 0, 704, 99
40684, V, 1, 1, 1, 1, 0, 704, 99
40685, V, 1, 1, 1, 1, 0, 704, 99
40686, V, 1, 1, 1, 1, 0, 704, 99
40687, V, 1, 1, 1, 1, 0, 704, 99
40688, V, 1, 1, 1, 1, 0, 704, 99
40689, V, 1, 1, 1, 1, 0, 704, 99
40690, V, 1, 1, 1, 1, 0, 704, 99
40691, V, 1, 1, 1, 1, 0, 704, 99
40692, V, 1, 1, 1, 1, 0, 704, 99
40693, V, 1, 1, 1, 1, 0, 704, 99
40694, V, 1, 1, 1, 1, 0, 704, 99
40695, V, 1, 1, 1, 1, 0, 704, 99
40696, V, 1, 1, 1, 1, 0, 704, 99
40697, V, 1, 1, 1, 1, 0, 704, 99
40698, V, 1, 1, 1, 1, 0, 704, 99
40699, V, 1, 1, 1, 1, 0, 704, 99
40700, V, 1, 1, 1, 1, 0, 704, 99
40701, V, 1, 1, 1, 1, 0, 704, 99
40702, V, 1, 1, 1, 1, 0, 704, 99
40704, V, 1, 1, 1, 1, 0, 704, 99
40705, V, 1, 1, 1, 1, 0, 704, 99
40706, V, 1, 1, 1, 1, 0, 704, 99
40707, V, 1, 1, 1, 1, 0, 704, 100
40708, V, 1, 1, 1, 1, 0, 704, 99
40709, V, 1, 1, 1, 1, 0, 704, 100
40710, V, 1, 1, 1, 1, 0, 704, 99
40711, V, 1, 1, 1, 1, 0, 704, 100
40712, V, 1, 1, 1, 1, 0, 704, 100
40713, V, 1, 1, 1, 1, 0, 704, 99
40714, V, 1, 1, 1, 1, 0, 704, 99
40715, V, 1, 1, 1, 1, 0, 704, 99
40716, V, 1, 1, 1, 1, 0, 704, 99
40717, V, 1, 1, 1, 1, 0, 704, 99
40718, V, 1, 1, 1, 1, 0, 704, 99
40719, V, 1, 1, 1, 1, 0, 704, 99
40720, V, 1, 1, 1, 1, 0, 704, 99
40721, V, 1, 1, 1, 1, 0, 704, 99
40722, V, 1, 1, 1, 1, 0, 704, 99
40723, V, 1, 1, 1, 1, 0, 704, 99
40724, V, 1, 1, 1, 1, 0, 704, 99
40725, V, 1, 1, 1, 1, 0, 704, 99
40726, V, 1, 1, 1, 1, 0, 704, 99
40727, V, 1, 1, 1, 1, 0, 704, 99
40728, V, 1, 1, 1, 1, 0, 704, 99
40729, V, 1, 1, 1, 1, 0, 704, 99
40730, V, 1, 1, 1, 1, 0, 704, 99
40731, V, 1, 1, 1, 1, 0, 704, 99
40732, V, 1, 1, 1, 1, 0, 704, 99
40733, V, 1, 1, 1, 1, 0, 704, 99
40734, V, 1, 1, 1, 1, 0, 704, 99
40735, V, 1, 1, 1, 1, 0, 704, 99
40736, V, 1, 1, 1, 1, 0, 704, 99
40737, V, 1, 1, 1, 1, 0, 704, 99
40738, V, 1, 1, 1, 1, 0, 704, 99
40739, V, 1, 1, 1, 1, 0, 704, 99
40740, V, 1, 1, 1, 1, 0, 704, 99
40741, V, 1, 1, 1, 1, 0, 704, 99
40742, V, 1, 1, 1, 1, 0, 704, 99
40743, V, 1, 1, 1, 1, 0, 704, 99
40744, V, 1, 1, 1, 1, 0, 704, 99
40745, V, 1, 1, 1, 1, 0, 704, 99
40747, V, 1, 1, 1, 1, 0, 704, 99
40748, V, 1, 1, 1, 1, 0, 704, 99
40749, V, 1, 1, 1, 1, 0, 704, 99
40750, V, 1, 1, 1, 1, 0, 704, 99
40751, V, 1, 1, 1, 1, 0, 704, 99
40752, V, 1, 1, 1, 1, 0, 704, 99
40753, V, 1, 1, 1, 1, 0, 704, 99
40754, V, 1, 1, 1, 1, 0, 704, 99
40755, V, 1, 1, 1, 1, 0, 704, 99
40756, V, 1, 1, 1, 1, 0, 704, 99
40757, V, 1, 1, 1, 1, 0, 704, 99
40758, V, 1, 1, 1, 1, 0, 704, 99
40759, V, 1, 1, 1, 1, 0, 704, 99
40760, V, 1, 1, 1, 1, 0, 704, 99
40761, V, 1, 1, 1, 1, 0, 704, 99
40762, V, 1, 1, 1, 1, 0, 704, 99
40763, V, 1, 1, 1, 1, 0, 704, 99
40764, V, 1, 1, 1, 1, 0, 704, 99
40765, V, 1, 1, 1, 1, 0, 704, 99
40766, V, 1, 1, 1, 1, 0, 704, 99
40767, V, 1, 1, 1, 1, 0, 704, 99
40768, V, 1, 1, 1, 1, 0, 704, 99
40769, V, 1, 1, 1, 1, 0, 704, 99
40770, V, 1, 1, 1, 1, 0, 704, 99
40771, V, 1, 1, 1, 1, 0, 704, 99
40772, V, 1, 1, 1, 1, 0, 704, 99
40773, V, 1, 1, 1, 1, 0, 704, 99
40774, V, 1, 1, 1, 1, 0, 704, 99
40775, V, 1, 1, 1, 1, 0, 704, 99
40776, V, 1, 1, 1, 1, 0, 704, 99
40777, V, 1, 1, 1, 1, 0, 704, 99
40778, V, 1, 1, 1, 1, 0, 704, 99
40779, V, 1, 1, 1, 1, 0, 704, 99
40780, V, 1, 1, 1, 1, 0, 704, 99
40781, V, 1, 1, 1, 1, 0, 704, 99
40782, V, 1, 1, 1, 1, 0, 704, 99
40783, V, 1, 1, 1, 1, 0, 704, 99
40784, V, 1, 1, 1, 1, 0, 704, 99
40785, V, 1, 1, 1, 1, 0, 704, 100
40786, V, 1, 1, 1, 1, 0, 704, 99
40787, V, 1, 1, 1, 1, 0, 704, 99
40788, V, 1, 1, 1, 1, 0, 704, 99
40790, V, 1, 1, 1, 1, 0, 704, 99
40791, V, 1, 1, 1, 1, 0, 704, 99
40792, V, 1, 1, 1, 1, 0, 704, 99
40793, V, 1, 1, 1, 1, 0, 704, 99
40794, V, 1, 1, 1, 1, 0, 704, 99
40795, V, 1, 1, 1, 1, 0, 704, 99
40796, V, 1, 1, 1, 1, 0, 704, 99
40797, V, 1, 1, 1, 1, 0, 704, 99
40798, V, 1, 1, 1, 1, 0, 704, 99
40799, V, 1, 1, 1, 1, 0, 704, 99
40800, V, 1, 1, 1, 1, 0, 704, 99
40801, V, 1, 1, 1, 1, 0, 704, 99
40802, V, 1, 1, 1, 1, 0, 704, 99
40803, V, 1, 1, 1, 1, 0, 704, 99
40804, V, 1, 1, 1, 1, 0, 704, 99
40805, V, 1, 1, 1, 1, 0, 704, 99
40806, V, 1, 1, 1, 1, 0, 704, 99
40807, V, 1, 1, 1, 1, 0, 704, 99
40808, V, 1, 1, 1, 1, 0, 704, 99
40809, V, 1, 1, 1, 1, 0, 704, 99
40810, V, 1, 1, 1, 1, 0, 704, 99
40811, V, 1, 1, 1, 1, 0, 704, 99
40812, V, 1, 1, 1, 1, 0, 704, 99
40813, V, 1, 1, 1, 1, 0, 704, 99
40814, V, 1, 1, 1, 1, 0, 704, 99
40815, V, 1, 1, 1, 1, 0, 704, 99
40816, V, 1, 1, 1, 1, 0, 704, 99
40817, V, 1, 1, 1, 1, 0, 704, 99
40818, V, 1, 1, 1, 1, 0, 704, 99
40819, V, 1, 1, 1, 1, 0, 704, 99
40820, V, 1, 1, 1, 1, 0, 704, 99
40821, V, 1, 1, 1, 1, 0, 704, 99
40822, V, 1, 1, 1, 1, 0, 704, 99
40823, V, 1, 1, 1, 1, 0, 704, 99
40824, V, 1, 1, 1, 1, 0, 704, 99
40825, V, 1, 1, 1, 1, 0, 704, 99
40826, V, 1, 1, 1, 1, 0, 704, 99
40827, V, 1, 1, 1, 1, 0, 704, 99
40828, V, 1, 1, 1, 1, 0, 704, 99
40829, V, 1, 1, 1, 1, 0, 704, 99
40830, V, 1, 1, 1, 1, 0, 704, 99
40832, V, 1, 1, 1, 1, 0, 704, 99
40833, V, 1, 1, 1, 1, 0, 704, 99
40834, V, 1, 1, 1, 1, 0, 704, 99
40835, V, 1, 1, 1, 1, 0, 704, 99
40836, V, 1, 1, 1, 1, 0, 704, 99
40837, V, 1, 1, 1, 1, 0, 704, 99
40838, V, 1, 1, 1, 1, 0, 704, 99
40839, V, 1, 1, 1, 1, 0, 704, 99
40840, V, 1, 1, 1, 1, 0, 704, 99
40841, V, 1, 1, 1, 1, 0, 704, 99
40842, V, 1, 1, 1, 1, 0, 704, 99
40843, V, 1, 1, 1, 1, 0, 704, 99
40844, V, 1, 1, 1, 1, 0, 704, 99
40845, V, 1, 1, 1, 1, 0, 704, 99
40846, V, 1, 1, 1, 1, 0, 704, 99
40847, V, 1, 1, 1, 1, 0, 704, 99
40848, V, 1, 1, 1, 1, 0, 704, 100
40849, V, 1, 1, 1, 1, 0, 704, 100
40850, V, 1, 1, 1, 1, 0, 704, 100
40851, V, 1, 1, 1, 1, 0, 704, 100
40852, V, 1, 1, 1, 1, 0, 704, 100
40853, V, 1, 1, 1, 1, 0, 704, 100
40854, V, 1, 1, 1, 1, 0, 704, 100
40855, V, 1, 1, 1, 1, 0, 704, 100
40856, V, 1, 1, 1, 1, 0, 704, 100
40857, V, 1, 1, 1, 1, 0, 704, 100
40858, V, 1, 1, 1, 1, 0, 704, 100
40859, V, 1, 1, 1, 1, 0, 704, 99
40860, V, 1, 1, 1, 1, 0, 704, 100
40861, V, 1, 1, 1, 1, 0, 704, 100
40862, V, 1, 1, 1, 1, 0, 704, 100
40863, V, 1, 1, 1, 1, 0, 704, 100
40864, V, 1, 1, 1, 1, 0, 704, 100
40865, V, 1, 1, 1, 1, 0, 704, 100
40866, V, 1, 1, 1, 1, 0, 704, 100
40867, V, 1, 1, 1, 1, 0, 704, 100
40868, V, 1, 1, 1, 1, 0, 704, 100
40869, V, 1, 1, 1, 1, 0, 704, 100
40870, V, 1, 1, 1, 1, 0, 704, 100
40871, V, 1, 1, 1, 1, 0, 704, 100
40872, V, 1, 1, 1, 1, 0, 704, 100
40873, V, 1, 1, 1, 1, 0, 704, 100
40875, V, 1, 1, 1, 1, 0, 704, 100
40876, V, 1, 1, 1, 1, 0, 704, 100
40877, V, 1, 1, 1, 1, 0, 704, 100
40878, V, 1, 1, 1, 1, 0, 704, 100
40879, V, 1, 1, 1, 1, 0, 704, 100
40880, V, 1, 1, 1, 1, 0, 704, 100
40881, V, 1, 1, 1, 1, 0, 704, 100
40882, V, 1, 1, 1, 1, 0, 704, 100
40883, V, 1, 1, 1, 1, 0, 704, 100
40884, V, 1, 1, 1, 1, 0, 704, 100
40885, V, 1, 1, 1, 1, 0, 704, 100
40886, V, 1, 1, 1, 1, 0, 704, 100
40887, V, 1, 1, 1, 1, 0, 704, 100
40888, V, 1, 1, 1, 1, 0, 704, 100
40889, V, 1, 1, 1, 1, 0, 704, 100
40890, V, 1, 1, 1, 1, 0, 704, 100
40891, V, 1, 1, 1, 1, 0, 704, 100
40892, V, 1, 1, 1, 1, 0, 704, 100
40893, V, 1, 1, 1, 1, 0, 704, 100
40894, V, 1, 1, 1, 1, 0, 704, 100
40895, V, 1, 1, 1, 1, 0, 704, 99
40896, V, 1, 1, 1, 1, 0, 704, 100
40897, V, 1, 1, 1, 1, 0, 704, 99
40898, V, 1, 1, 1, 1, 0, 704, 99
40899, V, 1, 1, 1, 1, 0, 704, 100
40900, V, 1, 1, 1, 1, 0, 704, 99
40901, V, 1, 1, 1, 1, 0, 704, 100
40902, V, 1, 1, 1, 1, 0, 704, 99
40903, V, 1, 1, 1, 1, 0, 704, 99
40904, V, 1, 1, 1, 1, 0, 704, 99
40905, V, 1, 1, 1, 1, 0, 704, 99
40906, V, 1, 1, 1, 1, 0, 704, 99
40907, V, 1, 1, 1, 1, 0, 704, 99
40908, V, 1, 1, 1, 1, 0, 704, 100
40909, V, 1, 1, 1, 1, 0, 704, 99
40910, V, 1, 1, 1, 1, 0, 704, 99
40911, V, 1, 1, 1, 1, 0, 704, 99
40912, V, 1, 1, 1, 1, 0, 704, 99
40913, V, 1, 1, 1, 1, 0, 704, 99
40914, V, 1, 1, 1, 1, 0, 704, 99
40915, V, 1, 1, 1, 1, 0, 704, 99
40916, V, 1, 1, 1, 1, 0, 704, 99
40918, V, 1, 1, 1, 1, 0, 704, 99
40919, V, 1, 1, 1, 1, 0, 704, 99
40920, V, 1, 1, 1, 1, 0, 704, 99
40921, V, 1, 1, 1, 1, 0, 704, 99
40922, V, 1, 1, 1, 1, 0, 704, 99
40923, V, 1, 1, 1, 1, 0, 704, 99
40924, V, 1, 1, 1, 1, 0, 704, 99
40925, V, 1, 1, 1, 1, 0, 704, 99
40926, V, 1, 1, 1, 1, 0, 704, 99
40927, V, 1, 1, 1, 1, 0, 704, 99
40928, V, 1, 1, 1, 1, 0, 704, 100
40929, V, 1, 1, 1, 1, 0, 704, 99
40930, V, 1, 1, 1, 1, 0, 704, 99
40931, V, 1, 1, 1, 1, 0, 704, 99
40932, V, 1, 1, 1, 1, 0, 704, 99
40933, V, 1, 1, 1, 1, 0, 704, 99
40934, V, 1, 1, 1, 1, 0, 704, 99
40935, V, 1, 1, 1, 1, 0, 704, 99
40936, V, 1, 1, 1, 1, 0, 704, 99
40937, V, 1, 1, 1, 1, 0, 704, 99
40938, V, 1, 1, 1, 1, 0, 704, 99
40939, V, 1, 1, 1, 1, 0, 704, 99
40940, V, 1, 1, 1, 1, 0, 704, 99
40941, V, 1, 1, 1, 1, 0, 704, 99
40942, V, 1, 1, 1, 1, 0, 704, 99
40943, V, 1, 1, 1, 1, 0, 704, 99
40944, V, 1, 1, 1, 1, 0, 704, 100
40945, V, 1, 1, 1, 1, 0, 704, 99
40946, V, 1, 1, 1, 1, 0, 704, 99
40947, V, 1, 1, 1, 1, 0, 704, 99
40948, V, 1, 1, 1, 1, 0, 704, 99
40949, V, 1, 1, 1, 1, 0, 704, 100
40950, V, 1, 1, 1, 1, 0, 704, 99
40951, V, 1, 1, 1, 1, 0, 704, 99
40952, V, 1, 1, 1, 1, 0, 704, 100
40953, V, 1, 1, 1, 1, 0, 704, 99
40954, V, 1, 1, 1, 1, 0, 704, 99
40955, V, 1, 1, 1, 1, 0, 704, 99
40956, V, 1, 1, 1, 1, 0, 704, 99
40957, V, 1, 1, 1, 1, 0, 704, 99
40958, V, 1, 1, 1, 1, 0, 704, 99
40960, V, 1, 1, 1, 1, 0, 704, 99
40961, V, 1, 1, 1, 1, 0, 704, 99
40962, V, 1, 1, 1, 1, 0, 704, 99
40963, V, 1, 1, 1, 1, 0, 704, 99
40964, V, 1, 1, 1, 1, 0, 704, 99
40965, V, 1, 1, 1, 1, 0, 704, 99
40966, V, 1, 1, 1, 1, 0, 704, 99
40967, V, 1, 1, 1, 1, 0, 704, 99
40968, V, 1, 1, 1, 1, 0, 704, 99
40969, V, 1, 1, 1, 1, 0, 704, 99
40970, V, 1, 1, 1, 1, 0, 704, 99
40971, V, 1, 1, 1, 1, 0, 704, 99
40972, V, 1, 1, 1, 1, 0, 704, 99
40973, V, 1, 1, 1, 1, 0, 704, 99
40974, V, 1, 1, 1, 1, 0, 704, 99
40975, V, 1, 1, 1, 1, 0, 704, 99
40976, V, 1, 1, 1, 1, 0, 704, 99
40977, V, 1, 1, 1, 1, 0, 704, 99
40978, V, 1, 1, 1, 1, 0, 704, 99
40979, V, 1, 1, 1, 1, 0, 704, 99
40980, V, 1, 1, 1, 1, 0, 704, 99
40981, V, 1, 1, 1, 1, 0, 704, 99
40982, V, 1, 1, 1, 1, 0, 704, 99
40983, V, 1, 1, 1, 1, 0, 704, 99
40984, V, 1, 1, 1, 1, 0, 704, 99
40985, V, 1, 1, 1, 1, 0, 704, 99
40986, V, 1, 1, 1, 1, 0, 704, 99
40987, V, 1, 1, 1, 1, 0, 704, 99
40988, V, 1, 1, 1, 1, 0, 704, 99
40989, V, 1, 1, 1, 1, 0, 704, 99
40990, V, 1, 1, 1, 1, 0, 704, 99
40991, V, 1, 1, 1, 1, 0, 704, 99
40992, V, 1, 1, 1, 1, 0, 704, 99
40993, V, 1, 1, 1, 1, 0, 704, 99
40994, V, 1, 1, 1, 1, 0, 704, 99
40995, V, 1, 1, 1, 1, 0, 704, 99
40996, V, 1, 1, 1, 1, 0, 704, 99
40997, V, 1, 1, 1, 1, 0, 704, 99
40998, V, 1, 1, 1, 1, 0, 704, 99
40999, V, 1, 1, 1, 1, 0, 704, 99
41000, V, 1, 1, 1, 1, 0, 704, 99
41001, V, 1, 1, 1, 1, 0, 704, 99
41003, V, 1, 1, 1, 1, 0, 704, 99
41004, V, 1, 1, 1, 1, 0, 704, 99
41005, V, 1, 1, 1, 1, 0, 704, 99
41006, V, 1, 1, 1, 1, 0, 704, 99
41007, V, 1, 1, 1, 1, 0, 704, 99
41008, V, 1, 1, 1, 1, 0, 704, 99
41009, V, 1, 1, 1, 1, 0, 704, 99
41010, V, 1, 1, 1, 1, 0, 704, 99
41011, V, 1, 1, 1, 1, 0, 704, 99
41012, V, 1, 1, 1, 1, 0, 704, 99
41013, V, 1, 1, 1, 1, 0, 704, 99
41014, V, 1, 1, 1, 1, 0, 704, 99
41015, V, 1, 1, 1, 1, 0, 704, 99
41016, V, 1, 1, 1, 1, 0, 704, 99
41017, V, 1, 1, 1, 1, 0, 704, 99
41018, V, 1, 1, 1, 1, 0, 704, 99
41019, V, 1, 1, 1, 1, 0, 704, 99
41020, V, 1, 1, 1, 1, 0, 704, 99
41021, V, 1, 1, 1, 1, 0, 704, 99
41022, V, 1, 1, 1, 1, 0, 704, 100
41023, V, 1, 1, 1, 1, 0, 704, 100
41024, V, 1, 1, 1, 1, 0, 704, 100
41025, V, 1, 1, 1, 1, 0, 704, 100
41026, V, 1, 1, 1, 1, 0, 704, 99
41027, V, 1, 1, 1, 1, 0, 704, 100
41028, V, 1, 1, 1, 1, 0, 704, 100
41029, V, 1, 1, 1, 1, 0, 704, 100
41030, V, 1, 1, 1, 1, 0, 704, 100
41031, V, 1, 1, 1, 1, 0, 704, 100
41032, V, 1, 1, 1, 1, 0, 704, 100
41033, V, 1, 1, 1, 1, 0, 704, 100
41034, V, 1, 1, 1, 1, 0, 704, 99
41035, V, 1, 1, 1, 1, 0, 704, 100
41036, V, 1, 1, 1, 1, 0, 704, 100
41037, V, 1, 1, 1, 1, 0, 704, 100
41038, V, 1, 1, 1, 1, 0, 704, 100
41039, V, 1, 1, 1, 1, 0, 704, 100
41040, V, 1, 1, 1, 1, 0, 704, 100
41041, V, 1, 1, 1, 1, 0, 704, 100
41042, V, 1, 1, 1, 1, 0, 704, 100
41043, V, 1, 1, 1, 1, 0, 704, 100
41044, V, 1, 1, 1, 1, 0, 704, 100
41046, V, 1, 1, 1, 1, 0, 704, 100
41047, V, 1, 1, 1, 1, 0, 704, 100
41048, V, 1, 1, 1, 1, 0, 704, 100
41049, V, 1, 1, 1, 1, 0, 704, 100
41050, V, 1, 1, 1, 1, 0, 704, 100
41051, V, 1, 1, 1, 1, 0, 704, 100
41052, V, 1, 1, 1, 1, 0, 704, 99
41053, V, 1, 1, 1, 1, 0, 704, 100
41054, V, 1, 1, 1, 1, 0, 704, 100
41055, V, 1, 1, 1, 1, 0, 704, 99
41056, V, 1, 1, 1, 1, 0, 704, 99
41057, V, 1, 1, 1, 1, 0, 704, 100
41058, V, 1, 1, 1, 1, 0, 704, 99
41059, V, 1, 1, 1, 1, 0, 704, 100
41060, V, 1, 1, 1, 1, 0, 704, 100
41061, V, 1, 1, 1, 1, 0, 704, 100
41062, V, 1, 1, 1, 1, 0, 704, 100
41063, V, 1, 1, 1, 1, 0, 704, 100
41064, V, 1, 1, 1, 1, 0, 704, 100
41065, V, 1, 1, 1, 1, 0, 704, 100
41066, V, 1, 1, 1, 1, 0, 704, 100
41067, V, 1, 1, 1, 1, 0, 704, 100
41068, V, 1, 1, 1, 1, 0, 704, 100
41069, V, 1, 1, 1, 1, 0, 704, 100
41070, V, 1, 1, 1, 1, 0, 704, 100
41071, V, 1, 1, 1, 1, 0, 704, 99
41072, V, 1, 1, 1, 1, 0, 704, 99
41073, V, 1, 1, 1, 1, 0, 704, 99
41074, V, 1, 1, 1, 1, 0, 704, 99
41075, V, 1, 1, 1, 1, 0, 704, 99
41076, V, 1, 1, 1, 1, 0, 704, 99
41077, V, 1, 1, 1, 1, 0, 704, 100
41078, V, 1, 1, 1, 1, 0, 704, 100
41079, V, 1, 1, 1, 1, 0, 704, 99
41080, V, 1, 1, 1, 1, 0, 704, 99
41081, V, 1, 1, 1, 1, 0, 704, 99
41082, V, 1, 1, 1, 1, 0, 704, 100
41083, V, 1, 1, 1, 1, 0, 704, 100
41084, V, 1, 1, 1, 1, 0, 704, 99
41085, V, 1, 1, 1, 1, 0, 704, 99
41086, V, 1, 1, 1, 1, 0, 704, 100
41088, V, 1, 1, 1, 1, 0, 704, 99
41089, V, 1, 1, 1, 1, 0, 704, 100
41090, V, 1, 1, 1, 1, 0, 704, 100
41091, V, 1, 1, 1, 1, 0, 704, 100
41092, V, 1, 1, 1, 1, 0, 704, 99
41093, V, 1, 1, 1, 1, 0, 704, 99
41094, V, 1, 1, 1, 1, 0, 704, 99
41095, V, 1, 1, 1, 1, 0, 704, 99
41096, V, 1, 1, 1, 1, 0, 704, 100
41097, V, 1, 1, 1, 1, 0, 704, 99
41098, V, 1, 1, 1, 1, 0, 704, 100
41099, V, 1, 1, 1, 1, 0, 704, 100
41100, V, 1, 1, 1, 1, 0, 704, 99
41101, V, 1, 1, 1, 1, 0, 704, 100
41102, V, 1, 1, 1, 1, 0, 704, 100
41103, V, 1, 1, 1, 1, 0, 704, 100
41104, V, 1, 1, 1, 1, 0, 704, 100
41105, V, 1, 1, 1, 1, 0, 704, 100
41106, V, 1, 1, 1, 1, 0, 704, 100
41107, V, 1, 1, 1, 1, 0, 704, 100
41108, V, 1, 1, 1, 1, 0, 704, 100
41109, V, 1, 1, 1, 1, 0, 704, 100
41110, V, 1, 1, 1, 1, 0, 704, 100
41111, V, 1, 1, 1, 1, 0, 704, 100
41112, V, 1, 1, 1, 1, 0, 704, 100
41113, V, 1, 1, 1, 1, 0, 704, 100
41114, V, 1, 1, 1, 1, 0, 704, 100
41115, V, 1, 1, 1, 1, 0, 704, 100
41116, V, 1, 1, 1, 1, 0, 704, 100
41117, V, 1, 1, 1, 1, 0, 704, 100
41118, V, 1, 1, 1, 1, 0, 704, 100
41119, V, 1, 1, 1, 1, 0, 704, 100
41120, V, 1, 1, 1, 1, 0, 704, 100
41121, V, 1, 1, 1, 1, 0, 704, 100
41122, V, 1, 1, 1, 1, 0, 704, 99
41123, V, 1, 1, 1, 1, 0, 704, 100
41124, V, 1, 1, 1, 1, 0, 704, 100
41125, V, 1, 1, 1, 1, 0, 704, 100
41126, V, 1, 1, 1, 1, 0, 704, 100
41127, V, 1, 1, 1, 1, 0, 704, 100
41128, V, 1, 1, 1, 1, 0, 704, 100
41129, V, 1, 1, 1, 1, 0, 704, 100
41131, V, 1, 1, 1, 1, 0, 704, 100
41132, V, 1, 1, 1, 1, 0, 704, 100
41133, V, 1, 1, 1, 1, 0, 704, 100
41134, V, 1, 1, 1, 1, 0, 704, 100
41135, V, 1, 1, 1, 1, 0, 704, 100
41136, V, 1, 1, 1, 1, 0, 704, 100
41137, V, 1, 1, 1, 1, 0, 704, 100
41138, V, 1, 1, 1, 1, 0, 704, 100
41139, V, 1, 1, 1, 1, 0, 704, 100
41140, V, 1, 1, 1, 1, 0, 704, 99
41141, V, 1, 1, 1, 1, 0, 704, 99
41142, V, 1, 1, 1, 1, 0, 704, 100
41143, V, 1, 1, 1, 1, 0, 704, 100
41144, V, 1, 1, 1, 1, 0, 704, 100
41145, V, 1, 1, 1, 1, 0, 704, 100
41146, V, 1, 1, 1, 1, 0, 704, 99
41147, V, 1, 1, 1, 1, 0, 704, 100
41148, V, 1, 1, 1, 1, 0, 704, 99
41149, V, 1, 1, 1, 1, 0, 704, 99
41150, V, 1, 1, 1, 1, 0, 704, 99
41151, V, 1, 1, 1, 1, 0, 704, 99
41152, V, 1, 1, 1, 1, 0, 704, 99
41153, V, 1, 1, 1, 1, 0, 704, 99
41154, V, 1, 1, 1, 1, 0, 704, 99
41155, V, 1, 1, 1, 1, 0, 704, 99
41156, V, 1, 1, 1, 1, 0, 704, 99
41157, V, 1, 1, 1, 1, 0, 704, 99
41158, V, 1, 1, 1, 1, 0, 704, 99
41159, V, 1, 1, 1, 1, 0, 704, 99
41160, V, 1, 1, 1, 1, 0, 704, 99
41161, V, 1, 1, 1, 1, 0, 704, 99
41162, V, 1, 1, 1, 1, 0, 704, 99
41163, V, 1, 1, 1, 1, 0, 704, 99
41164, V, 1, 1, 1, 1, 0, 704, 99
41165, V, 1, 1, 1, 1, 0, 704, 99
41166, V, 1, 1, 1, 1, 0, 704, 99
41167, V, 1, 1, 1, 1, 0, 704, 99
41168, V, 1, 1, 1, 1, 0, 704, 99
41169, V, 1, 1, 1, 1, 0, 704, 99
41170, V, 1, 1, 1, 1, 0, 704, 99
41171, V, 1, 1, 1, 1, 0, 704, 99
41172, V, 1, 1, 1, 1, 0, 704, 99
41174, V, 1, 1, 1, 1, 0, 704, 99
41175, V, 1, 1, 1, 1, 0, 704, 99
41176, V, 1, 1, 1, 1, 0, 704, 99
41177, V, 1, 1, 1, 1, 0, 704, 99
41178, V, 1, 1, 1, 1, 0, 704, 99
41179, V, 1, 1, 1, 1, 0, 704, 100
41180, V, 1, 1, 1, 1, 0, 704, 100
41181, V, 1, 1, 1, 1, 0, 704, 99
41182, V, 1, 1, 1, 1, 0, 704, 100
41183, V, 1, 1, 1, 1, 0, 704, 100
41184, V, 1, 1, 1, 1, 0, 704, 99
41185, V, 1, 1, 1, 1, 0, 704, 100
41186, V, 1, 1, 1, 1, 0, 704, 100
41187, V, 1, 1, 1, 1, 0, 704, 100
41188, V, 1, 1, 1, 1, 0, 704, 100
41189, V, 1, 1, 1, 1, 0, 704, 100
41190, V, 1, 1, 1, 1, 0, 704, 100
41191, V, 1, 1, 1, 1, 0, 704, 100
41192, V, 1, 1, 1, 1, 0, 704, 100
41193, V, 1, 1, 1, 1, 0, 704, 100
41194, V, 1, 1, 1, 1, 0, 704, 100
41195, V, 1, 1, 1, 1, 0, 704, 100
41196, V, 1, 1, 1, 1, 0, 704, 100
41197, V, 1, 1, 1, 1, 0, 704, 100
41198, V, 1, 1, 1, 1, 0, 704, 100
41199, V, 1, 1, 1, 1, 0, 704, 100
41200, V, 1, 1, 1, 1, 0, 704, 100
41201, V, 1, 1, 1, 1, 0, 704, 100
41202, V, 1, 1, 1, 1, 0, 704, 100
41203, V, 1, 1, 1, 1, 0, 704, 100
41204, V, 1, 1, 1, 1, 0, 704, 100
41205, V, 1, 1, 1, 1, 0, 704, 100
41206, V, 1, 1, 1, 1, 0, 704, 100
41207, V, 1, 1, 1, 1, 0, 704, 100
41208, V, 1, 1, 1, 1, 0, 704, 100
41209, V, 1, 1, 1, 1, 0, 704, 100
41210, V, 1, 1, 1, 1, 0, 704, 100
41211, V, 1, 1, 1, 1, 0, 704, 100
41212, V, 1, 1, 1, 1, 0, 704, 100
41213, V, 1, 1, 1, 1, 0, 704, 100
41214, V, 1, 1, 1, 1, 0, 704, 100
41216, V, 1, 1, 1, 1, 0, 704, 100
41217, V, 1, 1, 1, 1, 0, 704, 100
41218, V, 1, 1, 1, 1, 0, 704, 100
41219, V, 1, 1, 1, 1, 0, 704, 100
41220, V, 1, 1, 1, 1, 0, 704, 100
41221, V, 1, 1, 1, 1, 0, 704, 100
41222, V, 1, 1, 1, 1, 0, 704, 100
41223, V, 1, 1, 1, 1, 0, 704, 100
41224, V, 1, 1, 1, 1, 0, 704, 100
41225, V, 1, 1, 1, 1, 0, 704, 100
41226, V, 1, 1, 1, 1, 0, 704, 100
41227, V, 1, 1, 1, 1, 0, 704, 100
41228, V, 1, 1, 1, 1, 0, 704, 100
41229, V, 1, 1, 1, 1, 0, 704, 100
41230, V, 1, 1, 1, 1, 0, 704, 100
41231, V, 1, 1, 1, 1, 0, 704, 100
41232, V, 1, 1, 1, 1, 0, 704, 100
41233, V, 1, 1, 1, 1, 0, 704, 100
41234, V, 1, 1, 1, 1, 0, 704, 100
41235, V, 1, 1, 1, 1, 0, 704, 100
41236, V, 1, 1, 1, 1, 0, 704, 100
41237, V, 1, 1, 1, 1, 0, 704, 99
41238, V, 1, 1, 1, 1, 0, 704, 100
41239, V, 1, 1, 1, 1, 0, 704, 99
41240, V, 1, 1, 1, 1, 0, 704, 100
41241, V, 1, 1, 1, 1, 0, 704, 99
41242, V, 1, 1, 1, 1, 0, 704, 99
41243, V, 1, 1, 1, 1, 0, 704, 99
41244, V, 1, 1, 1, 1, 0, 704, 99
41245, V, 1, 1, 1, 1, 0, 704, 99
41246, V, 1, 1, 1, 1, 0, 704, 99
41247, V, 1, 1, 1, 1, 0, 704, 99
41248, V, 1, 1, 1, 1, 0, 704, 99
41249, V, 1, 1, 1, 1, 0, 704, 99
41250, V, 1, 1, 1, 1, 0, 704, 99
41251, V, 1, 1, 1, 1, 0, 704, 99
41252, V, 1, 1, 1, 1, 0, 704, 99
41253, V, 1, 1, 1, 1, 0, 704, 99
41254, V, 1, 1, 1, 1, 0, 704, 99
41255, V, 1, 1, 1, 1, 0, 704, 99
41256, V, 1, 1, 1, 1, 0, 704, 99
41257, V, 1, 1, 1, 1, 0, 704, 99
41259, V, 1, 1, 1, 1, 0, 704, 99
41260, V, 1, 1, 1, 1, 0, 704, 99
41261, V, 1, 1, 1, 1, 0, 704, 99
41262, V, 1, 1, 1, 1, 0, 704, 99
41263, V, 1, 1, 1, 1, 0, 704, 99
41264, V, 1, 1, 1, 1, 0, 704, 99
41265, V, 1, 1, 1, 1, 0, 704, 99
41266, V, 1, 1, 1, 1, 0, 704, 99
41267, V, 1, 1, 1, 1, 0, 704, 99
41268, V, 1, 1, 1, 1, 0, 704, 99
41269, V, 1, 1, 1, 1, 0, 704, 99
41270, V, 1, 1, 1, 1, 0, 704, 99
41271, V, 1, 1, 1, 1, 0, 704, 99
41272, V, 1, 1, 1, 1, 0, 704, 99
41273, V, 1, 1, 1, 1, 0, 704, 99
41274, V, 1, 1, 1, 1, 0, 704, 99
41275, V, 1, 1, 1, 1, 0, 704, 99
41276, V, 1, 1, 1, 1, 0, 704, 99
41277, V, 1, 1, 1, 1, 0, 704, 99
41278, V, 1, 1, 1, 1, 0, 704, 99
41279, V, 1, 1, 1, 1, 0, 704, 99
41280, V, 1, 1, 1, 1, 0, 704, 99
41281, V, 1, 1, 1, 1, 0, 704, 99
41282, V, 1, 1, 1, 1, 0, 704, 99
41283, V, 1, 1, 1, 1, 0, 704, 99
41284, V, 1, 1, 1, 1, 0, 704, 99
41285, V, 1, 1, 1, 1, 0, 704, 99
41286, V, 1, 1, 1, 1, 0, 704, 100
41287, V, 1, 1, 1, 1, 0, 704, 100
41288, V, 1, 1, 1, 1, 0, 704, 100
41289, V, 1, 1, 1, 1, 0, 704, 100
41290, V, 1, 1, 1, 1, 0, 704, 100
41291, V, 1, 1, 1, 1, 0, 704, 100
41292, V, 1, 1, 1, 1, 0, 704, 100
41293, V, 1, 1, 1, 1, 0, 704, 100
41294, V, 1, 1, 1, 1, 0, 704, 100
41295, V, 1, 1, 1, 1, 0, 704, 100
41296, V, 1, 1, 1, 1, 0, 704, 100
41297, V, 1, 1, 1, 1, 0, 704, 100
41298, V, 1, 1, 1, 1, 0, 704, 100
41299, V, 1, 1, 1, 1, 0, 704, 100
41300, V, 1, 1, 1, 1, 0, 704, 100
41302, V, 1, 1, 1, 1, 0, 704, 100
41303, V, 1, 1, 1, 1, 0, 704, 100
41304, V, 1, 1, 1, 1, 0, 704, 100
41305, V, 1, 1, 1, 1, 0, 704, 100
41306, V, 1, 1, 1, 1, 0, 704, 100
41307, V, 1, 1, 1, 1, 0, 704, 100
41308, V, 1, 1, 1, 1, 0, 704, 100
41309, V, 1, 1, 1, 1, 0, 704, 100
41310, V, 1, 1, 1, 1, 0, 704, 100
41311, V, 1, 1, 1, 1, 0, 704, 100
41312, V, 1, 1, 1, 1, 0, 704, 100
41313, V, 1, 1, 1, 1, 0, 704, 100
41314, V, 1, 1, 1, 1, 0, 704, 100
41315, V, 1, 1, 1, 1, 0, 704, 100
41316, V, 1, 1, 1, 1, 0, 704, 100
41317, V, 1, 1, 1, 1, 0, 704, 100
41318, V, 1, 1, 1, 1, 0, 704, 100
41319, V, 1, 1, 1, 1, 0, 704, 100
41320, V, 1, 1, 1, 1, 0, 704, 100
41321, V, 1, 1, 1, 1, 0, 704, 100
41322, V, 1, 1, 1, 1, 0, 704, 100
41323, V, 1, 1, 1, 1, 0, 704, 100
41324, V, 1, 1, 1, 1, 0, 704, 100
41325, V, 1, 1, 1, 1, 0, 704, 100
41326, V, 1, 1, 1, 1, 0, 704, 100
41327, V, 1, 1, 1, 1, 0, 704, 100
41328, V, 1, 1, 1, 1, 0, 704, 100
41329, V, 1, 1, 1, 1, 0, 704, 100
41330, V, 1, 1, 1, 1, 0, 704, 100
41331, V, 1, 1, 1, 1, 0, 704, 100
41332, V, 1, 1, 1, 1, 0, 704, 100
41333, V, 1, 1, 1, 1, 0, 704, 100
41334, V, 1, 1, 1, 1, 0, 704, 100
41335, V, 1, 1, 1, 1, 0, 704, 100
41336, V, 1, 1, 1, 1, 0, 704, 100
41337, V, 1, 1, 1, 1, 0, 704, 100
41338, V, 1, 1, 1, 1, 0, 704, 100
41339, V, 1, 1, 1, 1, 0, 704, 100
41340, V, 1, 1, 1, 1, 0, 704, 100
41341, V, 1, 1, 1, 1, 0, 704, 100
41342, V, 1, 1, 1, 1, 0, 704, 100
41344, V, 1, 1, 1, 1, 0, 704, 100
41345, V, 1, 1, 1, 1, 0, 704, 100
41346, V, 1, 1, 1, 1, 0, 704, 100
41347, V, 1, 1, 1, 1, 0, 704, 100
41348, V, 1, 1, 1, 1, 0, 704, 100
41349, V, 1, 1, 1, 1, 0, 704, 100
41350, V, 1, 1, 1, 1, 0, 704, 100
41351, V, 1, 1, 1, 1, 0, 704, 100
41352, V, 1, 1, 1, 1, 0, 704, 100
41353, V, 1, 1, 1, 1, 0, 704, 100
41354, V, 1, 1, 1, 1, 0, 704, 100
41355, V, 1, 1, 1, 1, 0, 704, 99
41356, V, 1, 1, 1, 1, 0, 704, 99
41357, V, 1, 1, 1, 1, 0, 704, 100
41358, V, 1, 1, 1, 1, 0, 704, 99
41359, V, 1, 1, 1, 1, 0, 704, 100
41360, V, 1, 1, 1, 1, 0, 704, 99
41361, V, 1, 1, 1, 1, 0, 704, 99
41362, V, 1, 1, 1, 1, 0, 704, 99
41363, V, 1, 1, 1, 1, 0, 704, 99
41364, V, 1, 1, 1, 1, 0, 704, 99
41365, V, 1, 1, 1, 1, 0, 704, 99
41366, V, 1, 1, 1, 1, 0, 704, 99
41367, V, 1, 1, 1, 1, 0, 704, 99
41368, V, 1, 1, 1, 1, 0, 704, 99
41369, V, 1, 1, 1, 1, 0, 704, 99
41370, V, 1, 1, 1, 1, 0, 704, 99
41371, V, 1, 1, 1, 1, 0, 704, 99
41372, V, 1, 1, 1, 1, 0, 704, 99
41373, V, 1, 1, 1, 1, 0, 704, 99
41374, V, 1, 1, 1, 1, 0, 704, 99
41375, V, 1, 1, 1, 1, 0, 704, 99
41376, V, 1, 1, 1, 1, 0, 704, 99
41377, V, 1, 1, 1, 1, 0, 704, 99
41378, V, 1, 1, 1, 1, 0, 704, 99
41379, V, 1, 1, 1, 1, 0, 704, 100
41380, V, 1, 1, 1, 1, 0, 704, 99
41381, V, 1, 1, 1, 1, 0, 704, 99
41382, V, 1, 1, 1, 1, 0, 704, 99
41383, V, 1, 1, 1, 1, 0, 704, 100
41384, V, 1, 1, 1, 1, 0, 704, 99
41385, V, 1, 1, 1, 1, 0, 704, 99
41387, V, 1, 1, 1, 1, 0, 704, 99
41388, V, 1, 1, 1, 1, 0, 704, 100
41389, V, 1, 1, 1, 1, 0, 704, 99
41390, V, 1, 1, 1, 1, 0, 704, 99
41391, V, 1, 1, 1, 1, 0, 704, 100
41392, V, 1, 1, 1, 1, 0, 704, 100
41393, V, 1, 1, 1, 1, 0, 704, 100
41394, V, 1, 1, 1, 1, 0, 704, 100
41395, V, 1, 1, 1, 1, 0, 704, 99
41396, V, 1, 1, 1, 1, 0, 704, 100
41397, V, 1, 1, 1, 1, 0, 704, 100
41398, V, 1, 1, 1, 1, 0, 704, 100
41399, V, 1, 1, 1, 1, 0, 704, 100
41400, V, 1, 1, 1, 1, 0, 704, 100
41401, V, 1, 1, 1, 1, 0, 704, 100
41402, V, 1, 1, 1, 1, 0, 704, 100
41403, V, 1, 1, 1, 1, 0, 704, 100
41404, V, 1, 1, 1, 1, 0, 704, 100
41405, V, 1, 1, 1, 1, 0, 704, 100
41406, V, 1, 1, 1, 1, 0, 704, 100
41407, V, 1, 1, 1, 1, 0, 704, 100
41408, V, 1, 1, 1, 1, 0, 704, 100
41409, V, 1, 1, 1, 1, 0, 704, 100
41410, V, 1, 1, 1, 1, 0, 704, 100
41411, V, 1, 1, 1, 1, 0, 704, 100
41412, V, 1, 1, 1, 1, 0, 704, 100
41413, V, 1, 1, 1, 1, 0, 704, 100
41414, V, 1, 1, 1, 1, 0, 704, 100
41415, V, 1, 1, 1, 1, 0, 704, 100
41416, V, 1, 1, 1, 1, 0, 704, 100
41417, V, 1, 1, 1, 1, 0, 704, 100
41418, V, 1, 1, 1, 1, 0, 704, 100
41419, V, 1, 1, 1, 1, 0, 704, 100
41420, V, 1, 1, 1, 1, 0, 704, 100
41421, V, 1, 1, 1, 1, 0, 704, 100
41422, V, 1, 1, 1, 1, 0, 704, 100
41423, V, 1, 1, 1, 1, 0, 704, 100
41424, V, 1, 1, 1, 1, 0, 704, 100
41425, V, 1, 1, 1, 1, 0, 704, 100
41426, V, 1, 1, 1, 1, 0, 704, 100
41427, V, 1, 1, 1, 1, 0, 704, 100
41428, V, 1, 1, 1, 1, 0, 704, 100
41430, V, 1, 1, 1, 1, 0, 704, 100
41431, V, 1, 1, 1, 1, 0, 704, 100
41432, V, 1, 1, 1, 1, 0, 704, 100
41433, V, 1, 1, 1, 1, 0, 704, 100
41434, V, 1, 1, 1, 1, 0, 704, 100
41435, V, 1, 1, 1, 1, 0, 704, 100
41436, V, 1, 1, 1, 1, 0, 704, 100
41437, V, 1, 1, 1, 1, 0, 704, 100
41438, V, 1, 1, 1, 1, 0, 704, 100
41439, V, 1, 1, 1, 1, 0, 704, 100
41440, V, 1, 1, 1, 1, 0, 704, 100
41441, V, 1, 1, 1, 1, 0, 704, 100
41442, V, 1, 1, 1, 1, 0, 704, 100
41443, V, 1, 1, 1, 1, 0, 704, 100
41444, V, 1, 1, 1, 1, 0, 704, 100
41445, V, 1, 1, 1, 1, 0, 704, 100
41446, V, 1, 1, 1, 1, 0, 704, 100
41447, V, 1, 1, 1, 1, 0, 704, 100
41448, V, 1, 1, 1, 1, 0, 704, 100
41449, V, 1, 1, 1, 1, 0, 704, 100
41450, V, 1, 1, 1, 1, 0, 704, 100
41451, V, 1, 1, 1, 1, 0, 704, 100
41452, V, 1, 1, 1, 1, 0, 704, 100
41453, V, 1, 1, 1, 1, 0, 704, 100
41454, V, 1, 1, 1, 1, 0, 704, 100
41455, V, 1, 1, 1, 1, 0, 704, 100
41456, V, 1, 1, 1, 1, 0, 704, 100
41457, V, 1, 1, 1, 1, 0, 704, 100
41458, V, 1, 1, 1, 1, 0, 704, 100
41459, V, 1, 1, 1, 1, 0, 704, 100
41460, V, 1, 1, 1, 1, 0, 704, 100
41461, V, 1, 1, 1, 1, 0, 704, 100
41462, V, 1, 1, 1, 1, 0, 704, 100
41463, V, 1, 1, 1, 1, 0, 704, 100
41464, V, 1, 1, 1, 1, 0, 704, 100
41465, V, 1, 1, 1, 1, 0, 704, 100
41466, V, 1, 1, 1, 1, 0, 704, 100
41467, V, 1, 1, 1, 1, 0, 704, 100
41468, V, 1, 1, 1, 1, 0, 704, 100
41469, V, 1, 1, 1, 1, 0, 704, 100
41470, V, 1, 1, 1, 1, 0, 704, 100
41472, V, 1, 1, 1, 1, 0, 704, 100
41473, V, 1, 1, 1, 1, 0, 704, 100
41474, V, 1, 1, 1, 1, 0, 704, 100
41475, V, 1, 1, 1, 1, 0, 704, 100
41476, V, 1, 1, 1, 1, 0, 704, 100
41477, V, 1, 1, 1, 1, 0, 704, 100
41478, V, 1, 1, 1, 1, 0, 704, 100
41479, V, 1, 1, 1, 1, 0, 704, 100
41480, V, 1, 1, 1, 1, 0, 704, 100
41481, V, 1, 1, 1, 1, 0, 704, 100
41482, V, 1, 1, 1, 1, 0, 704, 100
41483, V, 1, 1, 1, 1, 0, 704, 100
41484, V, 1, 1, 1, 1, 0, 704, 100
41485, V, 1, 1, 1, 1, 0, 704, 100
41486, V, 1, 1, 1, 1, 0, 704, 100
41487, V, 1, 1, 1, 1, 0, 704, 100
41488, V, 1, 1, 1, 1, 0, 704, 100
41489, V, 1, 1, 1, 1, 0, 704, 100
41490, V, 1, 1, 1, 1, 0, 704, 100
41491, V, 1, 1, 1, 1, 0, 704, 100
41492, V, 1, 1, 1, 1, 0, 704, 100
41493, V, 1, 1, 1, 1, 0, 704, 100
41494, V, 1, 1, 1, 1, 0, 704, 100
41495, V, 1, 1, 1, 1, 0, 704, 100
41496, V, 1, 1, 1, 1, 0, 704, 100
41497, V, 1, 1, 1, 1, 0, 704, 100
41498, V, 1, 1, 1, 1, 0, 704, 100
41499, V, 1, 1, 1, 1, 0, 704, 99
41500, V, 1, 1, 1, 1, 0, 704, 100
41501, V, 1, 1, 1, 1, 0, 704, 100
41502, V, 1, 1, 1, 1, 0, 704, 99
41503, V, 1, 1, 1, 1, 0, 704, 100
41504, V, 1, 1, 1, 1, 0, 704, 100
41505, V, 1, 1, 1, 1, 0, 704, 100
41506, V, 1, 1, 1, 1, 0, 704, 100
41507, V, 1, 1, 1, 1, 0, 704, 100
41508, V, 1, 1, 1, 1, 0, 704, 100
41509, V, 1, 1, 1, 1, 0, 704, 100
41510, V, 1, 1, 1, 1, 0, 704, 100
41511, V, 1, 1, 1, 1, 0, 704, 100
41512, V, 1, 1, 1, 1, 0, 704, 99
41513, V, 1, 1, 1, 1, 0, 704, 99
41515, V, 1, 1, 1, 1, 0, 704, 99
41516, V, 1, 1, 1, 1, 0, 704, 99
41517, V, 1, 1, 1, 1, 0, 704, 99
41518, V, 1, 1, 1, 1, 0, 704, 99
41519, V, 1, 1, 1, 1, 0, 704, 100
41520, V, 1, 1, 1, 1, 0, 704, 99
41521, V, 1, 1, 1, 1, 0, 704, 100
41522, V, 1, 1, 1, 1, 0, 704, 99
41523, V, 1, 1, 1, 1, 0, 704, 99
41524, V, 1, 1, 1, 1, 0, 704, 99
41525, V, 1, 1, 1, 1, 0, 704, 99
41526, V, 1, 1, 1, 1, 0, 704, 100
41527, V, 1, 1, 1, 1, 0, 704, 100
41528, V, 1, 1, 1, 1, 0, 704, 100
41529, V, 1, 1, 1, 1, 0, 704, 100
41530, V, 1, 1, 1, 1, 0, 704, 99
41531, V, 1, 1, 1, 1, 0, 704, 100
41532, V, 1, 1, 1, 1, 0, 704, 100
41533, V, 1, 1, 1, 1, 0, 704, 100
41534, V, 1, 1, 1, 1, 0, 704, 100
41535, V, 1, 1, 1, 1, 0, 704, 100
41536, V, 1, 1, 1, 1, 0, 704, 100
41537, V, 1, 1, 1, 1, 0, 704, 100
41538, V, 1, 1, 1, 1, 0, 704, 100
41539, V, 1, 1, 1, 1, 0, 704, 100
41540, V, 1, 1, 1, 1, 0, 704, 100
41541, V, 1, 1, 1, 1, 0, 704, 100
41542, V, 1, 1, 1, 1, 0, 704, 100
41543, V, 1, 1, 1, 1, 0, 704, 100
41544, V, 1, 1, 1, 1, 0, 704, 100
41545, V, 1, 1, 1, 1, 0, 704, 100
41546, V, 1, 1, 1, 1, 0, 704, 100
41547, V, 1, 1, 1, 1, 0, 704, 100
41548, V, 1, 1, 1, 1, 0, 704, 100
41549, V, 1, 1, 1, 1, 0, 704, 100
41550, V, 1, 1, 1, 1, 0, 704, 100
41551, V, 1, 1, 1, 1, 0, 704, 100
41552, V, 1, 1, 1, 1, 0, 704, 100
41553, V, 1, 1, 1, 1, 0, 704, 100
41554, V, 1, 1, 1, 1, 0, 704, 100
41555, V, 1, 1, 1, 1, 0, 704, 100
41556, V, 1, 1, 1, 1, 0, 704, 100
41558, V, 1, 1, 1, 1, 0, 704, 100
41559, V, 1, 1, 1, 1, 0, 704, 100
41560, V, 1, 1, 1, 1, 0, 704, 100
41561, V, 1, 1, 1, 1, 0, 704, 100
41562, V, 1, 1, 1, 1, 0, 704, 100
41563, V, 1, 1, 1, 1, 0, 704, 100
41564, V, 1, 1, 1, 1, 0, 704, 100
41565, V, 1, 1, 1, 1, 0, 704, 100
41566, V, 1, 1, 1, 1, 0, 704, 100
41567, V, 1, 1, 1, 1, 0, 704, 100
41568, V, 1, 1, 1, 1, 0, 704, 100
41569, V, 1, 1, 1, 1, 0, 704, 100
41570, V, 1, 1, 1, 1, 0, 704, 100
41571, V, 1, 1, 1, 1, 0, 704, 100
41572, V, 1, 1, 1, 1, 0, 704, 100
41573, V, 1, 1, 1, 1, 0, 704, 100
41574, V, 1, 1, 1, 1, 0, 704, 100
41575, V, 1, 1, 1, 1, 0, 704, 100
41576, V, 1, 1, 1, 1, 0, 704, 100
41577, V, 1, 1, 1, 1, 0, 704, 100
41578, V, 1, 1, 1, 1, 0, 704, 100
41579, V, 1, 1, 1, 1, 0, 704, 100
41580, V, 1, 1, 1, 1, 0, 704, 100
41581, V, 1, 1, 1, 1, 0, 704, 100
41582, V, 1, 1, 1, 1, 0, 704, 100
41583, V, 1, 1, 1, 1, 0, 704, 100
41584, V, 1, 1, 1, 1, 0, 704, 100
41585, V, 1, 1, 1, 1, 0, 704, 100
41586, V, 1, 1, 1, 1, 0, 704, 100
41587, V, 1, 1, 1, 1, 0, 704, 100
41588, V, 1, 1, 1, 1, 0, 704, 100
41589, V, 1, 1, 1, 1, 0, 704, 100
41590, V, 1, 1, 1, 1, 0, 704, 100
41591, V, 1, 1, 1, 1, 0, 704, 100
41592, V, 1, 1, 1, 1, 0, 704, 100
41593, V, 1, 1, 1, 1, 0, 704, 100
41594, V, 1, 1, 1, 1, 0, 704, 100
41595, V, 1, 1, 1, 1, 0, 704, 100
41596, V, 1, 1, 1, 1, 0, 704, 100
41597, V, 1, 1, 1, 1, 0, 704, 100
41598, V, 1, 1, 1, 1, 0, 704, 100
41600, V, 1, 1, 1, 1, 0, 704, 100
41601, V, 1, 1, 1, 1, 0, 704, 100
41602, V, 1, 1, 1, 1, 0, 704, 100
41603, V, 1, 1, 1, 1, 0, 704, 100
41604, V, 1, 1, 1, 1, 0, 704, 100
41605, V, 1, 1, 1, 1, 0, 704, 100
41606, V, 1, 1, 1, 1, 0, 704, 100
41607, V, 1, 1, 1, 1, 0, 704, 100
41608, V, 1, 1, 1, 1, 0, 704, 100
41609, V, 1, 1, 1, 1, 0, 704, 100
41610, V, 1, 1, 1, 1, 0, 704, 100
41611, V, 1, 1, 1, 1, 0, 704, 100
41612, V, 1, 1, 1, 1, 0, 704, 100
41613, V, 1, 1, 1, 1, 0, 704, 100
41614, V, 1, 1, 1, 1, 0, 704, 100
41615, V, 1, 1, 1, 1, 0, 704, 100
41616, V, 1, 1, 1, 1, 0, 704, 100
41617, V, 1, 1, 1, 1, 0, 704, 100
41618, V, 1, 1, 1, 1, 0, 704, 100
41619, V, 1, 1, 1, 1, 0, 704, 100
41620, V, 1, 1, 1, 1, 0, 704, 100
41621, V, 1, 1, 1, 1, 0, 704, 100
41622, V, 1, 1, 1, 1, 0, 704, 100
41623, V, 1, 1, 1, 1, 0, 704, 100
41624, V, 1, 1, 1, 1, 0, 704, 100
41625, V, 1, 1, 1, 1, 0, 704, 100
41626, V, 1, 1, 1, 1, 0, 704, 100
41627, V, 1, 1, 1, 1, 0, 704, 100
41628, V, 1, 1, 1, 1, 0, 704, 100
41629, V, 1, 1, 1, 1, 0, 704, 100
41630, V, 1, 1, 1, 1, 0, 704, 100
41631, V, 1, 1, 1, 1, 0, 704, 100
41632, V, 1, 1, 1, 1, 0, 704, 100
41633, V, 1, 1, 1, 1, 0, 704, 100
41634, V, 1, 1, 1, 1, 0, 704, 100
41635, V, 1, 1, 1, 1, 0, 704, 100
41636, V, 1, 1, 1, 1, 0, 704, 100
41637, V, 1, 1, 1, 1, 0, 704, 100
41638, V, 1, 1, 1, 1, 0, 704, 100
41639, V, 1, 1, 1, 1, 0, 704, 100
41640, V, 1, 1, 1, 1, 0, 704, 100
41641, V, 1, 1, 1, 1, 0, 704, 100
41643, V, 1, 1, 1, 1, 0, 704, 100
41644, V, 1, 1, 1, 1, 0, 704, 100
41645, V, 1, 1, 1, 1, 0, 704, 100
41646, V, 1, 1, 1, 1, 0, 704, 100
41647, V, 1, 1, 1, 1, 0, 704, 100
41648, V, 1, 1, 1, 1, 0, 704, 100
41649, V, 1, 1, 1, 1, 0, 704, 100
41650, V, 1, 1, 1, 1, 0, 704, 100
41651, V, 1, 1, 1, 1, 0, 704, 100
41652, V, 1, 1, 1, 1, 0, 704, 100
41653, V, 1, 1, 1, 1, 0, 704, 100
41654, V, 1, 1, 1, 1, 0, 704, 100
41655, V, 1, 1, 1, 1, 0, 704, 100
41656, V, 1, 1, 1, 1, 0, 704, 100
41657, V, 1, 1, 1, 1, 0, 704, 100
41658, V, 1, 1, 1, 1, 0, 704, 100
41659, V, 1, 1, 1, 1, 0, 704, 100
41660, V, 1, 1, 1, 1, 0, 704, 100
41661, V, 1, 1, 1, 1, 0, 704, 100
41662, V, 1, 1, 1, 1, 0, 704, 100
41663, V, 1, 1, 1, 1, 0, 704, 100
41664, V, 1, 1, 1, 1, 0, 704, 100
41665, V, 1, 1, 1, 1, 0, 704, 100
41666, V, 1, 1, 1, 1, 0, 704, 100
41667, V, 1, 1, 1, 1, 0, 704, 100
41668, V, 1, 1, 1, 1, 0, 704, 100
41669, V, 1, 1, 1, 1, 0, 704, 100
41670, V, 1, 1, 1, 1, 0, 704, 100
41671, V, 1, 1, 1, 1, 0, 704, 100
41672, V, 1, 1, 1, 1, 0, 704, 100
41673, V, 1, 1, 1, 1, 0, 704, 100
41674, V, 1, 1, 1, 1, 0, 704, 100
41675, V, 1, 1, 1, 1, 0, 704, 100
41676, V, 1, 1, 1, 1, 0, 704, 100
41677, V, 1, 1, 1, 1, 0, 704, 100
41678, V, 1, 1, 1, 1, 0, 704, 100
41679, V, 1, 1, 1, 1, 0, 704, 100
41680, V, 1, 1, 1, 1, 0, 704, 100
41681, V, 1, 1, 1, 1, 0, 704, 100
41682, V, 1, 1, 1, 1, 0, 704, 100
41683, V, 1, 1, 1, 1, 0, 704, 100
41684, V, 1, 1, 1, 1, 0, 704, 100
41686, V, 1, 1, 1, 1, 0, 704, 100
41687, V, 1, 1, 1, 1, 0, 704, 100
41688, V, 1, 1, 1, 1, 0, 704, 100
41689, V, 1, 1, 1, 1, 0, 704, 100
41690, V, 1, 1, 1, 1, 0, 704, 100
41691, V, 1, 1, 1, 1, 0, 704, 100
41692, V, 1, 1, 1, 1, 0, 704, 100
41693, V, 1, 1, 1, 1, 0, 704, 100
41694, V, 1, 1, 1, 1, 0, 704, 100
41695, V, 1, 1, 1, 1, 0, 704, 100
41696, V, 1, 1, 1, 1, 0, 704, 100
41697, V, 1, 1, 1, 1, 0, 704, 100
41698, V, 1, 1, 1, 1, 0, 704, 100
41699, V, 1, 1, 1, 1, 0, 704, 100
41700, V, 1, 1, 1, 1, 0, 704, 100
41701, V, 1, 1, 1, 1, 0, 704, 100
41702, V, 1, 1, 1, 1, 0, 704, 100
41703, V, 1, 1, 1, 1, 0, 704, 100
41704, V, 1, 1, 1, 1, 0, 704, 100
41705, V, 1, 1, 1, 1, 0, 704, 100
41706, V, 1, 1, 1, 1, 0, 704, 100
41707, V, 1, 1, 1, 1, 0, 704, 100
41708, V, 1, 1, 1, 1, 0, 704, 100
41709, V, 1, 1, 1, 1, 0, 704, 100
41710, V, 1, 1, 1, 1, 0, 704, 100
41711, V, 1, 1, 1, 1, 0, 704, 100
41712, V, 1, 1, 1, 1, 0, 704, 100
41713, V, 1, 1, 1, 1, 0, 704, 100
41714, V, 1, 1, 1, 1, 0, 704, 100
41715, V, 1, 1, 1, 1, 0, 704, 100
41716, V, 1, 1, 1, 1, 0, 704, 100
41717, V, 1, 1, 1, 1, 0, 704, 100
41718, V, 1, 1, 1, 1, 0, 704, 100
41719, V, 1, 1, 1, 1, 0, 704, 100
41720, V, 1, 1, 1, 1, 0, 704, 100
41721, V, 1, 1, 1, 1, 0, 704, 100
41722, V, 1, 1, 1, 1, 0, 704, 100
41723, V, 1, 1, 1, 1, 0, 704, 100
41724, V, 1, 1, 1, 1, 0, 704, 100
41725, V, 1, 1, 1, 1, 0, 704, 100
41726, V, 1, 1, 1, 1, 0, 704, 100
41728, V, 1, 1, 1, 1, 0, 704, 100
41729, V, 1, 1, 1, 1, 0, 704, 100
41730, V, 1, 1, 1, 1, 0, 704, 100
41731, V, 1, 1, 1, 1, 0, 704, 100
41732, V, 1, 1, 1, 1, 0, 704, 100
41733, V, 1, 1, 1, 1, 0, 704, 100
41734, V, 1, 1, 1, 1, 0, 704, 100
41735, V, 1, 1, 1, 1, 0, 704, 100
41736, V, 1, 1, 1, 1, 0, 704, 100
41737, V, 1, 1, 1, 1, 0, 704, 100
41738, V, 1, 1, 1, 1, 0, 704, 100
41739, V, 1, 1, 1, 1, 0, 704, 100
41740, V, 1, 1, 1, 1, 0, 704, 100
41741, V, 1, 1, 1, 1, 0, 704, 100
41742, V, 1, 1, 1, 1, 0, 704, 100
41743, V, 1, 1, 1, 1, 0, 704, 100
41744, V, 1, 1, 1, 1, 0, 704, 100
41745, V, 1, 1, 1, 1, 0, 704, 100
41746, V, 1, 1, 1, 1, 0, 704, 100
41747, V, 1, 1, 1, 1, 0, 704, 100
41748, V, 1, 1, 1, 1, 0, 704, 100
41749, V, 1, 1, 1, 1, 0, 704, 100
41750, V, 1, 1, 1, 1, 0, 704, 100
41751, V, 1, 1, 1, 1, 0, 704, 100
41752, V, 1, 1, 1, 1, 0, 704, 100
41753, V, 1, 1, 1, 1, 0, 704, 100
41754, V, 1, 1, 1, 1, 0, 704, 100
41755, V, 1, 1, 1, 1, 0, 704, 100
41756, V, 1, 1, 1, 1, 0, 704, 100
41757, V, 1, 1, 1, 1, 0, 704, 100
41758, V, 1, 1, 1, 1, 0, 704, 100
41759, V, 1, 1, 1, 1, 0, 704, 100
41760, V, 1, 1, 1, 1, 0, 704, 100
41761, V, 1, 1, 1, 1, 0, 704, 100
41762, V, 1, 1, 1, 1, 0, 704, 100
41763, V, 1, 1, 1, 1, 0, 704, 100
41764, V, 1, 1, 1, 1, 0, 704, 100
41765, V, 1, 1, 1, 1, 0, 704, 100
41766, V, 1, 1, 1, 1, 0, 704, 100
41767, V, 1, 1, 1, 1, 0, 704, 100
41768, V, 1, 1, 1, 1, 0, 704, 100
41769, V, 1, 1, 1, 1, 0, 704, 100
41771, V, 1, 1, 1, 1, 0, 704, 100
41772, V, 1, 1, 1, 1, 0, 704, 100
41773, V, 1, 1, 1, 1, 0, 704, 100
41774, V, 1, 1, 1, 1, 0, 704, 100
41775, V, 1, 1, 1, 1, 0, 704, 100
41776, V, 1, 1, 1, 1, 0, 704, 100
41777, V, 1, 1, 1, 1, 0, 704, 100
41778, V, 1, 1, 1, 1, 0, 704, 100
41779, V, 1, 1, 1, 1, 0, 704, 100
41780, V, 1, 1, 1, 1, 0, 704, 100
41781, V, 1, 1, 1, 1, 0, 704, 100
41782, V, 1, 1, 1, 1, 0, 704, 100
41783, V, 1, 1, 1, 1, 0, 704, 100
41784, V, 1, 1, 1, 1, 0, 704, 100
41785, V, 1, 1, 1, 1, 0, 704, 100
41786, V, 1, 1, 1, 1, 0, 704, 100
41787, V, 1, 1, 1, 1, 0, 704, 100
41788, V, 1, 1, 1, 1, 0, 704, 100
41789, V, 1, 1, 1, 1, 0, 704, 100
41790, V, 1, 1, 1, 1, 0, 704, 100
41791, V, 1, 1, 1, 1, 0, 704, 100
41792, V, 1, 1, 1, 1, 0, 704, 100
41793, V, 1, 1, 1, 1, 0, 704, 100
41794, V, 1, 1, 1, 1, 0, 704, 100
41795, V, 1, 1, 1, 1, 0, 704, 100
41796, V, 1, 1, 1, 1, 0, 704, 100
41797, V, 1, 1, 1, 1, 0, 704, 100
41798, V, 1, 1, 1, 1, 0, 704, 100
41799, V, 1, 1, 1, 1, 0, 704, 100
41800, V, 1, 1, 1, 1, 0, 704, 100
41801, V, 1, 1, 1, 1, 0, 704, 100
41802, V, 1, 1, 1, 1, 0, 704, 100
41803, V, 1, 1, 1, 1, 0, 704, 100
41804, V, 1, 1, 1, 1, 0, 704, 100
41805, V, 1, 1, 1, 1, 0, 704, 100
41806, V, 1, 1, 1, 1, 0, 704, 100
41807, V, 1, 1, 1, 1, 0, 704, 100
41808, V, 1, 1, 1, 1, 0, 704, 100
41809, V, 1, 1, 1, 1, 0, 704, 100
41810, V, 1, 1, 1, 1, 0, 704, 100
41811, V, 1, 1, 1, 1, 0, 704, 100
41812, V, 1, 1, 1, 1, 0, 704, 100
41814, V, 1, 1, 1, 1, 0, 704, 100
41815, V, 1, 1, 1, 1, 0, 704, 100
41816, V, 1, 1, 1, 1, 0, 704, 100
41817, V, 1, 1, 1, 1, 0, 704, 100
41818, V, 1, 1, 1, 1, 0, 704, 100
41819, V, 1, 1, 1, 1, 0, 704, 100
41820, V, 1, 1, 1, 1, 0, 704, 100
41821, V, 1, 1, 1, 1, 0, 704, 100
41822, V, 1, 1, 1, 1, 0, 704, 100
41823, V, 1, 1, 1, 1, 0, 704, 100
41824, V, 1, 1, 1, 1, 0, 704, 100
41825, V, 1, 1, 1, 1, 0, 704, 100
41826, V, 1, 1, 1, 1, 0, 704, 100
41827, V, 1, 1, 1, 1, 0, 704, 100
41828, V, 1, 1, 1, 1, 0, 704, 100
41829, V, 1, 1, 1, 1, 0, 704, 100
41830, V, 1, 1, 1, 1, 0, 704, 100
41831, V, 1, 1, 1, 1, 0, 704, 100
41832, V, 1, 1, 1, 1, 0, 704, 100
41833, V, 1, 1, 1, 1, 0, 704, 100
41834, V, 1, 1, 1, 1, 0, 704, 100
41835, V, 1, 1, 1, 1, 0, 704, 100
41836, V, 1, 1, 1, 1, 0, 704, 100
41837, V, 1, 1, 1, 1, 0, 704, 100
41838, V, 1, 1, 1, 1, 0, 704, 100
41839, V, 1, 1, 1, 1, 0, 704, 100
41840, V, 1, 1, 1, 1, 0, 704, 100
41841, V, 1, 1, 1, 1, 0, 704, 100
41842, V, 1, 1, 1, 1, 0, 704, 100
41843, V, 1, 1, 1, 1, 0, 704, 100
41844, V, 1, 1, 1, 1, 0, 704, 100
41845, V, 1, 1, 1, 1, 0, 704, 100
41846, V, 1, 1, 1, 1, 0, 704, 100
41847, V, 1, 1, 1, 1, 0, 704, 100
41848, V, 1, 1, 1, 1, 0, 704, 100
41849, V, 1, 1, 1, 1, 0, 704, 100
41850, V, 1, 1, 1, 1, 0, 704, 100
41851, V, 1, 1, 1, 1, 0, 704, 100
41852, V, 1, 1, 1, 1, 0, 704, 100
41853, V, 1, 1, 1, 1, 0, 704, 100
41854, V, 1, 1, 1, 1, 0, 704, 100
41856, V, 1, 1, 1, 1, 0, 704, 100
41857, V, 1, 1, 1, 1, 0, 704, 100
41858, V, 1, 1, 1, 1, 0, 704, 100
41859, V, 1, 1, 1, 1, 0, 704, 100
41860, V, 1, 1, 1, 1, 0, 704, 100
41861, V, 1, 1, 1, 1, 0, 704, 100
41862, V, 1, 1, 1, 1, 0, 704, 100
41863, V, 1, 1, 1, 1, 0, 704, 100
41864, V, 1, 1, 1, 1, 0, 704, 100
41865, V, 1, 1, 1, 1, 0, 704, 100
41866, V, 1, 1, 1, 1, 0, 704, 100
41867, V, 1, 1, 1, 1, 0, 704, 100
41868, V, 1, 1, 1, 1, 0, 704, 100
41869, V, 1, 1, 1, 1, 0, 704, 100
41870, V, 1, 1, 1, 1, 0, 704, 100
41871, V, 1, 1, 1, 1, 0, 704, 100
41872, V, 1, 1, 1, 1, 0, 704, 100
41873, V, 1, 1, 1, 1, 0, 704, 100
41874, V, 1, 1, 1, 1, 0, 704, 100
41875, V, 1, 1, 1, 1, 0, 704, 100
41876, V, 1, 1, 1, 1, 0, 704, 100
41877, V, 1, 1, 1, 1, 0, 704, 100
41878, V, 1, 1, 1, 1, 0, 704, 100
41879, V, 1, 1, 1, 1, 0, 704, 100
41880, V, 1, 1, 1, 1, 0, 704, 100
41881, V, 1, 1, 1, 1, 0, 704, 100
41882, V, 1, 1, 1, 1, 0, 704, 100
41883, V, 1, 1, 1, 1, 0, 704, 100
41884, V, 1, 1, 1, 1, 0, 704, 100
41885, V, 1, 1, 1, 1, 0, 704, 100
41886, V, 1, 1, 1, 1, 0, 704, 100
41887, V, 1, 1, 1, 1, 0, 704, 100
41888, V, 1, 1, 1, 1, 0, 704, 100
41889, V, 1, 1, 1, 1, 0, 704, 100
41890, V, 1, 1, 1, 1, 0, 704, 100
41891, V, 1, 1, 1, 1, 0, 704, 100
41892, V, 1, 1, 1, 1, 0, 704, 100
41893, V, 1, 1, 1, 1, 0, 704, 100
41894, V, 1, 1, 1, 1, 0, 704, 100
41895, V, 1, 1, 1, 1, 0, 704, 100
41896, V, 1, 1, 1, 1, 0, 704, 100
41897, V, 1, 1, 1, 1, 0, 704, 100
41899, V, 1, 1, 1, 1, 0, 704, 100
41900, V, 1, 1, 1, 1, 0, 704, 100
41901, V, 1, 1, 1, 1, 0, 704, 100
41902, V, 1, 1, 1, 1, 0, 704, 100
41903, V, 1, 1, 1, 1, 0, 704, 100
41904, V, 1, 1, 1, 1, 0, 704, 100
41905, V, 1, 1, 1, 1, 0, 704, 100
41906, V, 1, 1, 1, 1, 0, 704, 100
41907, V, 1, 1, 1, 1, 0, 704, 100
41908, V, 1, 1, 1, 1, 0, 704, 100
41909, V, 1, 1, 1, 1, 0, 704, 100
41910, V, 1, 1, 1, 1, 0, 704, 100
41911, V, 1, 1, 1, 1, 0, 704, 100
41912, V, 1, 1, 1, 1, 0, 704, 100
41913, V, 1, 1, 1, 1, 0, 704, 100
41914, V, 1, 1, 1, 1, 0, 704, 100
41915, V, 1, 1, 1, 1, 0, 704, 100
41916, V, 1, 1, 1, 1, 0, 704, 100
41917, V, 1, 1, 1, 1, 0, 704, 100
41918, V, 1, 1, 1, 1, 0, 704, 100
41919, V, 1, 1, 1, 1, 0, 704, 100
41920, V, 1, 1, 1, 1, 0, 704, 100
41921, V, 1, 1, 1, 1, 0, 704, 100
41922, V, 1, 1, 1, 1, 0, 704, 100
41923, V, 1, 1, 1, 1, 0, 704, 100
41924, V, 1, 1, 1, 1, 0, 704, 100
41925, V, 1, 1, 1, 1, 0, 704, 100
41926, V, 1, 1, 1, 1, 0, 704, 100
41927, V, 1, 1, 1, 1, 0, 704, 100
41928, V, 1, 1, 1, 1, 0, 704, 100
41929, V, 1, 1, 1, 1, 0, 704, 100
41930, V, 1, 1, 1, 1, 0, 704, 100
41931, V, 1, 1, 1, 1, 0, 704, 100
41932, V, 1, 1, 1, 1, 0, 704, 100
41933, V, 1, 1, 1, 1, 0, 704, 100
41934, V, 1, 1, 1, 1, 0, 704, 100
41935, V, 1, 1, 1, 1, 0, 704, 100
41936, V, 1, 1, 1, 1, 0, 704, 100
41937, V, 1, 1, 1, 1, 0, 704, 100
41938, V, 1, 1, 1, 1, 0, 704, 100
41939, V, 1, 1, 1, 1, 0, 704, 100
41940, V, 1, 1, 1, 1, 0, 704, 100
41942, V, 1, 1, 1, 1, 0, 704, 100
41943, V, 1, 1, 1, 1, 0, 704, 100
41944, V, 1, 1, 1, 1, 0, 704, 100
41945, V, 1, 1, 1, 1, 0, 704, 100
41946, V, 1, 1, 1, 1, 0, 704, 100
41947, V, 1, 1, 1, 1, 0, 704, 100
41948, V, 1, 1, 1, 1, 0, 704, 100
41949, V, 1, 1, 1, 1, 0, 704, 100
41950, V, 1, 1, 1, 1, 0, 704, 100
41951, V, 1, 1, 1, 1, 0, 704, 100
41952, V, 1, 1, 1, 1, 0, 704, 100
41953, V, 1, 1, 1, 1, 0, 704, 100
41954, V, 1, 1, 1, 1, 0, 704, 100
41955, V, 1, 1, 1, 1, 0, 704, 100
41956, V, 1, 1, 1, 1, 0, 704, 100
41957, V, 1, 1, 1, 1, 0, 704, 100
41958, V, 1, 1, 1, 1, 0, 704, 100
41959, V, 1, 1, 1, 1, 0, 704, 100
41960, V, 1, 1, 1, 1, 0, 704, 100
41961, V, 1, 1, 1, 1, 0, 704, 100
41962, V, 1, 1, 1, 1, 0, 704, 100
41963, V, 1, 1, 1, 1, 0, 704, 100
41964, V, 1, 1, 1, 1, 0, 704, 100
41965, V, 1, 1, 1, 1, 0, 704, 100
41966, V, 1, 1, 1, 1, 0, 704, 100
41967, V, 1, 1, 1, 1, 0, 704, 100
41968, V, 1, 1, 1, 1, 0, 704, 100
41969, V, 1, 1, 1, 1, 0, 704, 100
41970, V, 1, 1, 1, 1, 0, 704, 100
41971, V, 1, 1, 1, 1, 0, 704, 100
41972, V, 1, 1, 1, 1, 0, 704, 100
41973, V, 1, 1, 1, 1, 0, 704, 100
41974, V, 1, 1, 1, 1, 0, 704, 100
41975, V, 1, 1, 1, 1, 0, 704, 100
41976, V, 1, 1, 1, 1, 0, 704, 100
41977, V, 1, 1, 1, 1, 0, 704, 100
41978, V, 1, 1, 1, 1, 0, 704, 100
41979, V, 1, 1, 1, 1, 0, 704, 100
41980, V, 1, 1, 1, 1, 0, 704, 100
41981, V, 1, 1, 1, 1, 0, 704, 100
41982, V, 1, 1, 1, 1, 0, 704, 100
41984, V, 1, 1, 1, 1, 0, 704, 100
41985, V, 1, 1, 1, 1, 0, 704, 100
41986, V, 1, 1, 1, 1, 0, 704, 100
41987, V, 1, 1, 1, 1, 0, 704, 100
41988, V, 1, 1, 1, 1, 0, 704, 100
41989, V, 1, 1, 1, 1, 0, 704, 100
41990, V, 1, 1, 1, 1, 0, 704, 100
41991, V, 1, 1, 1, 1, 0, 704, 100
41992, V, 1, 1, 1, 1, 0, 704, 100
41993, V, 1, 1, 1, 1, 0, 704, 100
41994, V, 1, 1, 1, 1, 0, 704, 100
41995, V, 1, 1, 1, 1, 0, 704, 100
41996, V, 1, 1, 1, 1, 0, 704, 100
41997, V, 1, 1, 1, 1, 0, 704, 100
41998, V, 1, 1, 1, 1, 0, 704, 100
41999, V, 1, 1, 1, 1, 0, 704, 100
42000, V, 1, 1, 1, 1, 0, 704, 100
42001, V, 1, 1, 1, 1, 0, 704, 100
42002, V, 1, 1, 1, 1, 0, 704, 100
42003, V, 1, 1, 1, 1, 0, 704, 100
42004, V, 1, 1, 1, 1, 0, 704, 100
42005, V, 1, 1, 1, 1, 0, 704, 100
42006, V, 1, 1, 1, 1, 0, 704, 100
42007, V, 1, 1, 1, 1, 0, 704, 100
42008, V, 1, 1, 1, 1, 0, 704, 100
42009, V, 1, 1, 1, 1, 0, 704, 100
42010, V, 1, 1, 1, 1, 0, 704, 100
42011, V, 1, 1, 1, 1, 0, 704, 100
42012, V, 1, 1, 1, 1, 0, 704, 100
42013, V, 1, 1, 1, 1, 0, 704, 100
42014, V, 1, 1, 1, 1, 0, 704, 100
42015, V, 1, 1, 1, 1, 0, 704, 100
42016, V, 1, 1, 1, 1, 0, 704, 100
42017, V, 1, 1, 1, 1, 0, 704, 100
42018, V, 1, 1, 1, 1, 0, 704, 100
42019, V, 1, 1, 1, 1, 0, 704, 100
42020, V, 1, 1, 1, 1, 0, 704, 100
42021, V, 1, 1, 1, 1, 0, 704, 100
42022, V, 1, 1, 1, 1, 0, 704, 100
42023, V, 1, 1, 1, 1, 0, 704, 100
42024, V, 1, 1, 1, 1, 0, 704, 100
42025, V, 1, 1, 1, 1, 0, 704, 100
42027, V, 1, 1, 1, 1, 0, 704, 100
42028, V, 1, 1, 1, 1, 0, 704, 100
42029, V, 1, 1, 1, 1, 0, 704, 100
42030, V, 1, 1, 1, 1, 0, 704, 100
42031, V, 1, 1, 1, 1, 0, 704, 100
42032, V, 1, 1, 1, 1, 0, 704, 100
42033, V, 1, 1, 1, 1, 0, 704, 100
42034, V, 1, 1, 1, 1, 0, 704, 100
42035, V, 1, 1, 1, 1, 0, 704, 100
42036, V, 1, 1, 1, 1, 0, 704, 100
42037, V, 1, 1, 1, 1, 0, 704, 100
42038, V, 1, 1, 1, 1, 0, 704, 100
42039, V, 1, 1, 1, 1, 0, 704, 100
42040, V, 1, 1, 1, 1, 0, 704, 100
42041, V, 1, 1, 1, 1, 0, 704, 100
42042, V, 1, 1, 1, 1, 0, 704, 100
42043, V, 1, 1, 1, 1, 0, 704, 100
42044, V, 1, 1, 1, 1, 0, 704, 100
42045, V, 1, 1, 1, 1, 0, 704, 100
42046, V, 1, 1, 1, 1, 0, 704, 100
42047, V, 1, 1, 1, 1, 0, 704, 100
42048, V, 1, 1, 1, 1, 0, 704, 100
42049, V, 1, 1, 1, 1, 0, 704, 100
42050, V, 1, 1, 1, 1, 0, 704, 100
42051, V, 1, 1, 1, 1, 0, 704, 100
42052, V, 1, 1, 1, 1, 0, 704, 100
42053, V, 1, 1, 1, 1, 0, 704, 100
42054, V, 1, 1, 1, 1, 0, 704, 100
42055, V, 1, 1, 1, 1, 0, 704, 100
42056, V, 1, 1, 1, 1, 0, 704, 100
42057, V, 1, 1, 1, 1, 0, 704, 100
42058, V, 1, 1, 1, 1, 0, 704, 100
42059, V, 1, 1, 1, 1, 0, 704, 100
42060, V, 1, 1, 1, 1, 0, 704, 100
42061, V, 1, 1, 1, 1, 0, 704, 100
42062, V, 1, 1, 1, 1, 0, 704, 100
42063, V, 1, 1, 1, 1, 0, 704, 100
42064, V, 1, 1, 1, 1, 0, 704, 100
42065, V, 1, 1, 1, 1, 0, 704, 100
42066, V, 1, 1, 1, 1, 0, 704, 100
42067, V, 1, 1, 1, 1, 0, 704, 100
42068, V, 1, 1, 1, 1, 0, 704, 100
42070, V, 1, 1, 1, 1, 0, 704, 100
42071, V, 1, 1, 1, 1, 0, 704, 100
42072, V, 1, 1, 1, 1, 0, 704, 100
42073, V, 1, 1, 1, 1, 0, 704, 100
42074, V, 1, 1, 1, 1, 0, 704, 100
42075, V, 1, 1, 1, 1, 0, 704, 100
42076, V, 1, 1, 1, 1, 0, 704, 100
42077, V, 1, 1, 1, 1, 0, 704, 100
42078, V, 1, 1, 1, 1, 0, 704, 100
42079, V, 1, 1, 1, 1, 0, 704, 100
42080, V, 1, 1, 1, 1, 0, 704, 100
42081, V, 1, 1, 1, 1, 0, 704, 100
42082, V, 1, 1, 1, 1, 0, 704, 100
42083, V, 1, 1, 1, 1, 0, 704, 100
42084, V, 1, 1, 1, 1, 0, 704, 100
42085, V, 1, 1, 1, 1, 0, 704, 100
42086, V, 1, 1, 1, 1, 0, 704, 100
42087, V, 1, 1, 1, 1, 0, 704, 100
42088, V, 1, 1, 1, 1, 0, 704, 100
42089, V, 1, 1, 1, 1, 0, 704, 100
42090, V, 1, 1, 1, 1, 0, 704, 100
42091, V, 1, 1, 1, 1, 0, 704, 100
42092, V, 1, 1, 1, 1, 0, 704, 100
42093, V, 1, 1, 1, 1, 0, 704, 100
42094, V, 1, 1, 1, 1, 0, 704, 100
42095, V, 1, 1, 1, 1, 0, 704, 100
42096, V, 1, 1, 1, 1, 0, 704, 100
42097, V, 1, 1, 1, 1, 0, 704, 100
42098, V, 1, 1, 1, 1, 0, 704, 100
42099, V, 1, 1, 1, 1, 0, 704, 100
42100, V, 1, 1, 1, 1, 0, 704, 100
42101, V, 1, 1, 1, 1, 0, 704, 100
42102, V, 1, 1, 1, 1, 0, 704, 100
42103, V, 1, 1, 1, 1, 0, 704, 100
42104, V, 1, 1, 1, 1, 0, 704, 100
42105, V, 1, 1, 1, 1, 0, 704, 100
42106, V, 1, 1, 1, 1, 0, 704, 100
42107, V, 1, 1, 1, 1, 0, 704, 100
42108, V, 1, 1, 1, 1, 0, 704, 100
42109, V, 1, 1, 1, 1, 0, 704, 100
42110, V, 1, 1, 1, 1, 0, 704, 100
42112, V, 1, 1, 1, 1, 0, 704, 100
42113, V, 1, 1, 1, 1, 0, 704, 100
42114, V, 1, 1, 1, 1, 0, 704, 100
42115, V, 1, 1, 1, 1, 0, 704, 100
42116, V, 1, 1, 1, 1, 0, 704, 100
42117, V, 1, 1, 1, 1, 0, 704, 100
42118, V, 1, 1, 1, 1, 0, 704, 100
42119, V, 1, 1, 1, 1, 0, 704, 100
42120, V, 1, 1, 1, 1, 0, 704, 100
42121, V, 1, 1, 1, 1, 0, 704, 100
42122, V, 1, 1, 1, 1, 0, 704, 100
42123, V, 1, 1, 1, 1, 0, 704, 100
42124, V, 1, 1, 1, 1, 0, 704, 100
42125, V, 1, 1, 1, 1, 0, 704, 100
42126, V, 1, 1, 1, 1, 0, 704, 100
42127, V, 1, 1, 1, 1, 0, 704, 100
42128, V, 1, 1, 1, 1, 0, 704, 100
42129, V, 1, 1, 1, 1, 0, 704, 100
42130, V, 1, 1, 1, 1, 0, 704, 100
42131, V, 1, 1, 1, 1, 0, 704, 100
42132, V, 1, 1, 1, 1, 0, 704, 100
42133, V, 1, 1, 1, 1, 0, 704, 100
42134, V, 1, 1, 1, 1, 0, 704, 100
42135, V, 1, 1, 1, 1, 0, 704, 100
42136, V, 1, 1, 1, 1, 0, 704, 100
42137, V, 1, 1, 1, 1, 0, 704, 100
42138, V, 1, 1, 1, 1, 0, 704, 100
42139, V, 1, 1, 1, 1, 0, 704, 100
42140, V, 1, 1, 1, 1, 0, 704, 100
42141, V, 1, 1, 1, 1, 0, 704, 100
42142, V, 1, 1, 1, 1, 0, 704, 100
42143, V, 1, 1, 1, 1, 0, 704, 100
42144, V, 1, 1, 1, 1, 0, 704, 100
42145, V, 1, 0, 0, 1, 0, 704, 100
42145, V, 1, 0, 0, 0, 0, 704, 100
42146, V, 1, 1, 0, 0, 0, 704, 100
42146, V, 1, 1, 0, 0, 0, 704, 100
42147, V, 1, 1, 1, 1, 0, 704, 100
42148, V, 1, 1, 1, 1, 0, 704, 100
42149, V, 1, 1, 1, 1, 0, 704, 100
42150, V, 1, 1, 1, 1, 0, 704, 100
42151, V, 1, 1, 1, 1, 0, 704, 100
42152, V, 1, 1, 1, 1, 0, 704, 99
42153, V, 1, 1, 1, 1, 0, 704, 99
42155, V, 1, 1, 1, 1, 0, 704, 99
42156, V, 1, 1, 1, 1, 0, 704, 99
42157, V, 1, 1, 1, 1, 0, 704, 99
42158, V, 1, 1, 1, 1, 0, 704, 99
42159, V, 1, 1, 1, 1, 0, 704, 99
42160, V, 1, 1, 1, 1, 0, 704, 99
42161, V, 1, 1, 1, 1, 0, 704, 99
42162, V, 1, 1, 1, 1, 0, 704, 99
42163, V, 1, 1, 1, 1, 0, 704, 99
42164, V, 1, 1, 1, 1, 0, 704, 99
42165, V, 1, 1, 1, 1, 0, 704, 99
42166, V, 1, 1, 1, 1, 0, 704, 99
42167, V, 1, 1, 1, 1, 0, 704, 99
42168, V, 1, 1, 1, 1, 0, 704, 99
42169, V, 1, 1, 1, 1, 0, 704, 99
42170, V, 1, 1, 1, 1, 0, 704, 99
42171, V, 1, 1, 1, 1, 0, 704, 99
42172, V, 1, 1, 1, 1, 0, 704, 99
42173, V, 1, 1, 1, 1, 0, 704, 99
42174, V, 1, 1, 1, 1, 0, 704, 99
42175, V, 1, 1, 1, 1, 0, 704, 99
42176, V, 1, 1, 1, 1, 0, 704, 99
42177, V, 1, 1, 1, 1, 0, 704, 100
42178, V, 1, 1, 1, 1, 0, 704, 99
42179, V, 1, 1, 1, 1, 0, 704, 99
42180, V, 1, 1, 1, 1, 0, 704, 100
42181, V, 1, 1, 1, 1, 0, 704, 100
42182, V, 1, 1, 1, 1, 0, 704, 100
42183, V, 1, 1, 1, 1, 0, 704, 100
42184, V, 1, 1, 1, 1, 0, 704, 100
42185, V, 1, 1, 1, 1, 0, 704, 100
42186, V, 1, 1, 1, 1, 0, 704, 100
42187, V, 1, 1, 1, 1, 0, 704, 100
42188, V, 1, 1, 1, 1, 0, 704, 100
42189, V, 1, 1, 1, 1, 0, 704, 100
42190, V, 1, 1, 1, 1, 0, 704, 100
42191, V, 1, 1, 1, 1, 0, 704, 100
42192, V, 1, 1, 1, 1, 0, 704, 100
42193, V, 1, 1, 1, 1, 0, 704, 100
42194, V, 1, 1, 1, 1, 0, 704, 100
42195, V, 1, 1, 1, 1, 0, 704, 100
42196, V, 1, 1, 1, 1, 0, 704, 100
42198, V, 1, 1, 1, 1, 0, 704, 100
42199, V, 1, 1, 1, 1, 0, 704, 100
42200, V, 1, 1, 1, 1, 0, 704, 100
42201, V, 1, 1, 1, 1, 0, 704, 100
42202, V, 1, 1, 1, 1, 0, 704, 100
42203, V, 1, 1, 1, 1, 0, 704, 100
42204, V, 1, 1, 1, 1, 0, 704, 100
42205, V, 1, 1, 1, 1, 0, 704, 100
42206, V, 1, 1, 1, 1, 0, 704, 100
42207, V, 1, 1, 1, 1, 0, 704, 100
42208, V, 1, 1, 1, 1, 0, 704, 100
42209, V, 1, 1, 1, 1, 0, 704, 100
42210, V, 1, 1, 1, 1, 0, 704, 100
42211, V, 1, 1, 1, 1, 0, 704, 100
42212, V, 1, 1, 1, 1, 0, 704, 100
42213, V, 1, 1, 1, 1, 0, 704, 100
42214, V, 1, 1, 1, 1, 0, 704, 100
42215, V, 1, 1, 1, 1, 0, 704, 100
42216, V, 1, 1, 1, 1, 0, 704, 100
42217, V, 1, 1, 1, 1, 0, 704, 100
42218, V, 1, 1, 1, 1, 0, 704, 100
42219, V, 1, 1, 1, 1, 0, 704, 100
42220, V, 1, 1, 1, 1, 0, 704, 100
42221, V, 1, 1, 1, 1, 0, 704, 100
42222, V, 1, 1, 1, 1, 0, 704, 100
42223, V, 1, 1, 1, 1, 0, 704, 100
42224, V, 1, 1, 1, 1, 0, 704, 100
42225, V, 1, 1, 1, 1, 0, 704, 100
42226, V, 1, 1, 1, 1, 0, 704, 100
42227, V, 1, 1, 1, 1, 0, 704, 100
42228, V, 1, 1, 1, 1, 0, 704, 100
42229, V, 1, 1, 1, 1, 0, 704, 100
42230, V, 1, 1, 1, 1, 0, 704, 100
42231, V, 1, 1, 1, 1, 0, 704, 100
42232, V, 1, 1, 1, 1, 0, 704, 100
42233, V, 1, 1, 1, 1, 0, 704, 100
42234, V, 1, 1, 1, 1, 0, 704, 100
42235, V, 1, 1, 1, 1, 0, 704, 100
42236, V, 1, 1, 1, 1, 0, 704, 100
42237, V, 1, 1, 1, 1, 0, 704, 100
42238, V, 1, 1, 1, 1, 0, 704, 100
42240, V, 1, 1, 1, 1, 0, 704, 100
42241, V, 1, 1, 1, 1, 0, 704, 100
42242, V, 1, 1, 1, 1, 0, 704, 100
42243, V, 1, 1, 1, 1, 0, 704, 100
42244, V, 1, 1, 1, 1, 0, 704, 100
42245, V, 1, 1, 1, 1, 0, 704, 100
42246, V, 1, 1, 1, 1, 0, 704, 100
42247, V, 1, 1, 1, 1, 0, 704, 100
42248, V, 1, 1, 1, 1, 0, 704, 100
42249, V, 1, 1, 1, 1, 0, 704, 100
42250, V, 1, 1, 1, 1, 0, 704, 100
42251, V, 1, 1, 1, 1, 0, 704, 100
42252, V, 1, 1, 1, 1, 0, 704, 100
42253, V, 1, 1, 1, 1, 0, 704, 100
42254, V, 1, 1, 1, 1, 0, 704, 100
42255, V, 1, 1, 1, 1, 0, 704, 100
42256, V, 1, 1, 1, 1, 0, 704, 100
42257, V, 1, 1, 1, 1, 0, 704, 100
42258, V, 1, 1, 1, 1, 0, 704, 100
42259, V, 1, 1, 1, 1, 0, 704, 100
42260, V, 1, 1, 1, 1, 0, 704, 100
42261, V, 1, 1, 1, 1, 0, 704, 100
42262, V, 1, 1, 1, 1, 0, 704, 100
42263, V, 1, 1, 1, 1, 0, 704, 100
42264, V, 1, 1, 1, 1, 0, 704, 100
42265, V, 1, 1, 1, 1, 0, 704, 100
42266, V, 1, 1, 1, 1, 0, 704, 100
42267, V, 1, 1, 1, 1, 0, 704, 100
42268, V, 1, 1, 1, 1, 0, 704, 100
42269, V, 1, 1, 1, 1, 0, 704, 100
42270, V, 1, 1, 1, 1, 0, 704, 100
42271, V, 1, 1, 1, 1, 0, 704, 100
42272, V, 1, 1, 1, 1, 0, 704, 100
42273, V, 1, 1, 1, 1, 0, 704, 100
42274, V, 1, 1, 1, 1, 0, 704, 100
42275, V, 1, 1, 1, 1, 0, 704, 100
42276, V, 1, 1, 1, 1, 0, 704, 100
42277, V, 1, 1, 1, 1, 0, 704, 100
42278, V, 1, 1, 1, 1, 0, 704, 100
42279, V, 1, 1, 1, 1, 0, 704, 100
42280, V, 1, 1, 1, 1, 0, 704, 100
42281, V, 1, 1, 1, 1, 0, 704, 100
42283, V, 1, 1, 1, 1, 0, 704, 100
42284, V, 1, 1, 1, 1, 0, 704, 100
42285, V, 1, 1, 1, 1, 0, 704, 100
42286, V, 1, 1, 1, 1, 0, 704, 100
42287, V, 1, 1, 1, 1, 0, 704, 100
42288, V, 1, 1, 1, 1, 0, 704, 100
42289, V, 1, 1, 1, 1, 0, 704, 100
42290, V, 1, 1, 1, 1, 0, 704, 100
42291, V, 1, 1, 1, 1, 0, 704, 100
42292, V, 1, 1, 1, 1, 0, 704, 100
42293, V, 1, 1, 1, 1, 0, 704, 100
42294, V, 1, 1, 1, 1, 0, 704, 100
42295, V, 1, 1, 1, 1, 0, 704, 100
42296, V, 1, 1, 1, 1, 0, 704, 100
42297, V, 1, 1, 1, 1, 0, 704, 100
42298, V, 1, 1, 1, 1, 0, 704, 100
42299, V, 1, 1, 1, 1, 0, 704, 100
42300, V, 1, 1, 1, 1, 0, 704, 100
42301, V, 1, 1, 1, 1, 0, 704, 100
42302, V, 1, 1, 1, 1, 0, 704, 100
42303, V, 1, 1, 1, 1, 0, 704, 100
42304, V, 1, 1, 1, 1, 0, 704, 100
42305, V, 1, 1, 1, 1, 0, 704, 100
42306, V, 1, 1, 1, 1, 0, 704, 100
42307, V, 1, 1, 1, 1, 0, 704, 100
42308, V, 1, 1, 1, 1, 0, 704, 100
42309, V, 1, 1, 1, 1, 0, 704, 100
42310, V, 1, 1, 1, 1, 0, 704, 100
42311, V, 1, 1, 1, 1, 0, 704, 100
42312, V, 1, 1, 1, 1, 0, 704, 100
42313, V, 1, 1, 1, 1, 0, 704, 100
42314, V, 1, 1, 1, 1, 0, 704, 100
42315, V, 1, 1, 1, 1, 0, 704, 100
42316, V, 1, 1, 1, 1, 0, 704, 100
42317, V, 1, 1, 1, 1, 0, 704, 100
42318, V, 1, 1, 1, 1, 0, 704, 100
42319, V, 1, 1, 1, 1, 0, 704, 100
42320, V, 1, 1, 1, 1, 0, 704, 100
42321, V, 1, 1, 1, 1, 0, 704, 100
42322, V, 1, 1, 1, 1, 0, 704, 100
42323, V, 1, 1, 1, 1, 0, 704, 99
42324, V, 1, 1, 1, 1, 0, 704, 99
42326, V, 1, 1, 1, 1, 0, 704, 99
42327, V, 1, 1, 1, 1, 0, 704, 99
42328, V, 1, 1, 1, 1, 0, 704, 99
42329, V, 1, 1, 1, 1, 0, 704, 99
42330, V, 1, 1, 1, 1, 0, 704, 99
42331, V, 1, 1, 1, 1, 0, 704, 99
42332, V, 1, 1, 1, 1, 0, 704, 99
42333, V, 1, 1, 1, 1, 0, 704, 99
42334, V, 1, 1, 1, 1, 0, 704, 99
42335, V, 1, 1, 1, 1, 0, 704, 99
42336, V, 1, 1, 1, 1, 0, 704, 99
42337, V, 1, 1, 1, 1, 0, 704, 99
42338, V, 1, 1, 1, 1, 0, 704, 99
42339, V, 1, 1, 1, 1, 0, 704, 99
42340, V, 1, 1, 1, 1, 0, 704, 99
42341, V, 1, 1, 1, 1, 0, 704, 99
42342, V, 1, 1, 1, 1, 0, 704, 99
42343, V, 1, 1, 1, 1, 0, 704, 99
42344, V, 1, 1, 1, 1, 0, 704, 99
42345, V, 1, 1, 1, 1, 0, 704, 99
42346, V, 1, 1, 1, 1, 0, 704, 99
42347, V, 1, 1, 1, 1, 0, 704, 99
42348, V, 1, 1, 1, 1, 0, 704, 99
42349, V, 1, 1, 1, 1, 0, 704, 99
42350, V, 1, 1, 1, 1, 0, 704, 99
42351, V, 1, 1, 1, 1, 0, 704, 99
42352, V, 1, 1, 1, 1, 0, 704, 99
42353, V, 1, 1, 1, 1, 0, 704, 99
42354, V, 1, 1, 1, 1, 0, 704, 99
42355, V, 1, 1, 1, 1, 0, 704, 99
42356, V, 1, 1, 1, 1, 0, 704, 99
42357, V, 1, 1, 1, 1, 0, 704, 99
42358, V, 1, 1, 1, 1, 0, 704, 99
42359, V, 1, 1, 1, 1, 0, 704, 99
42360, V, 1, 1, 1, 1, 0, 704, 99
42361, V, 1, 1, 1, 1, 0, 704, 99
42362, V, 1, 1, 1, 1, 0, 704, 99
42363, V, 1, 1, 1, 1, 0, 704, 99
42364, V, 1, 1, 1, 1, 0, 704, 99
42365, V, 1, 1, 1, 1, 0, 704, 99
42366, V, 1, 1, 1, 1, 0, 704, 99
42368, V, 1, 1, 1, 1, 0, 704, 99
42369, V, 1, 1, 1, 1, 0, 704, 99
42370, V, 1, 1, 1, 1, 0, 704, 99
42371, V, 1, 1, 1, 1, 0, 704, 99
42372, V, 1, 1, 1, 1, 0, 704, 99
42373, V, 1, 1, 1, 1, 0, 704, 99
42374, V, 1, 1, 1, 1, 0, 704, 99
42375, V, 1, 1, 1, 1, 0, 704, 99
42376, V, 1, 1, 1, 1, 0, 704, 99
42377, V, 1, 1, 1, 1, 0, 704, 99
42378, V, 1, 1, 1, 1, 0, 704, 99
42379, V, 1, 1, 1, 1, 0, 704, 99
42380, V, 1, 1, 1, 1, 0, 704, 99
42381, V, 1, 1, 1, 1, 0, 704, 99
42382, V, 1, 1, 1, 1, 0, 704, 99
42383, V, 1, 1, 1, 1, 0, 704, 99
42384, V, 1, 1, 1, 1, 0, 704, 99
42385, V, 1, 1, 1, 1, 0, 704, 99
42386, V, 1, 1, 1, 1, 0, 704, 99
42387, V, 1, 1, 1, 1, 0, 704, 99
42388, V, 1, 1, 1, 1, 0, 704, 99
42389, V, 1, 1, 1, 1, 0, 704, 99
42390, V, 1, 1, 1, 1, 0, 704, 99
42391, V, 1, 1, 1, 1, 0, 704, 99
42392, V, 1, 1, 1, 1, 0, 704, 99
42393, V, 1, 1, 1, 1, 0, 704, 99
42394, V, 1, 1, 1, 1, 0, 704, 99
42395, V, 1, 1, 1, 1, 0, 704, 99
42396, V, 1, 1, 1, 1, 0, 704, 99
42397, V, 1, 1, 1, 1, 0, 704, 99
42398, V, 1, 1, 1, 1, 0, 704, 99
42399, V, 1, 1, 1, 1, 0, 704, 99
42400, V, 1, 1, 1, 1, 0, 704, 99
42401, V, 1, 1, 1, 1, 0, 704, 99
42402, V, 1, 1, 1, 1, 0, 704, 99
42403, V, 1, 1, 1, 1, 0, 704, 99
42404, V, 1, 1, 1, 1, 0, 704, 99
42405, V, 1, 1, 1, 1, 0, 704, 99
42406, V, 1, 1, 1, 1, 0, 704, 99
42407, V, 1, 1, 1, 1, 0, 704, 99
42408, V, 1, 1, 1, 1, 0, 704, 99
42409, V, 1, 1, 1, 1, 0, 704, 99
42411, V, 1, 1, 1, 1, 0, 704, 99
42412, V, 1, 1, 1, 1, 0, 704, 99
42413, V, 1, 1, 1, 1, 0, 704, 99
42414, V, 1, 1, 1, 1, 0, 704, 99
42415, V, 1, 1, 1, 1, 0, 704, 99
42416, V, 1, 1, 1, 1, 0, 704, 99
42417, V, 1, 1, 1, 1, 0, 704, 99
42418, V, 1, 1, 1, 1, 0, 704, 99
42419, V, 1, 1, 1, 1, 0, 704, 99
42420, V, 1, 1, 1, 1, 0, 704, 99
42421, V, 1, 1, 1, 1, 0, 704, 99
42422, V, 1, 1, 1, 1, 0, 704, 99
42423, V, 1, 1, 1, 1, 0, 704, 99
42424, V, 1, 1, 1, 1, 0, 704, 99
42425, V, 1, 1, 1, 1, 0, 704, 99
42426, V, 1, 1, 1, 1, 0, 704, 99
42427, V, 1, 1, 1, 1, 0, 704, 99
42428, V, 1, 1, 1, 1, 0, 704, 99
42429, V, 1, 1, 1, 1, 0, 704, 99
42430, V, 1, 1, 1, 1, 0, 704, 99
42431, V, 1, 1, 1, 1, 0, 704, 99
42432, V, 1, 1, 1, 1, 0, 704, 99
42433, V, 1, 1, 1, 1, 0, 704, 99
42434, V, 1, 1, 1, 1, 0, 704, 99
42435, V, 1, 1, 1, 1, 0, 704, 99
42436, V, 1, 1, 1, 1, 0, 704, 99
42437, V, 1, 1, 1, 1, 0, 704, 99
42438, V, 1, 1, 1, 1, 0, 704, 99
42439, V, 1, 1, 1, 1, 0, 704, 99
42440, V, 1, 1, 1, 1, 0, 704, 99
42441, V, 1, 1, 1, 1, 0, 704, 99
42442, V, 1, 1, 1, 1, 0, 704, 99
42443, V, 1, 1, 1, 1, 0, 704, 99
42444, V, 1, 1, 1, 1, 0, 704, 99
42445, V, 1, 1, 1, 1, 0, 704, 99
42446, V, 1, 1, 1, 1, 0, 704, 99
42447, V, 1, 1, 1, 1, 0, 704, 99
42448, V, 1, 1, 1, 1, 0, 704, 99
42449, V, 1, 1, 1, 1, 0, 704, 99
42450, V, 1, 1, 1, 1, 0, 704, 99
42451, V, 1, 1, 1, 1, 0, 704, 99
42452, V, 1, 1, 1, 1, 0, 704, 99
42454, V, 1, 1, 1, 1, 0, 704, 99
42455, V, 1, 1, 1, 1, 0, 704, 99
42456, V, 1, 1, 1, 1, 0, 704, 99
42457, V, 1, 1, 1, 1, 0, 704, 99
42458, V, 1, 1, 1, 1, 0, 704, 99
42459, V, 1, 1, 1, 1, 0, 704, 99
42460, V, 1, 1, 1, 1, 0, 704, 99
42461, V, 1, 1, 1, 1, 0, 704, 99
42462, V, 1, 1, 1, 1, 0, 704, 99
42463, V, 1, 1, 1, 1, 0, 704, 99
42464, V, 1, 1, 1, 1, 0, 704, 99
42465, V, 1, 1, 1, 1, 0, 704, 99
42466, V, 1, 1, 1, 1, 0, 704, 99
42467, V, 1, 1, 1, 1, 0, 704, 99
42468, V, 1, 1, 1, 1, 0, 704, 99
42469, V, 1, 1, 1, 1, 0, 704, 99
42470, V, 1, 1, 1, 1, 0, 704, 99
42471, V, 1, 1, 1, 1, 0, 704, 99
42472, V, 1, 1, 1, 1, 0, 704, 99
42473, V, 1, 1, 1, 1, 0, 704, 99
42474, V, 1, 1, 1, 1, 0, 704, 99
42475, V, 1, 1, 1, 1, 0, 704, 99
42476, V, 1, 1, 1, 1, 0, 704, 99
42477, V, 1, 1, 1, 1, 0, 704, 99
42478, V, 1, 1, 1, 1, 0, 704, 99
42479, V, 1, 1, 1, 1, 0, 704, 99
42480, V, 1, 1, 1, 1, 0, 704, 99
42481, V, 1, 1, 1, 1, 0, 704, 99
42482, V, 1, 1, 1, 1, 0, 704, 99
42483, V, 1, 1, 1, 1, 0, 704, 99
42484, V, 1, 1, 1, 1, 0, 704, 99
42485, V, 1, 1, 1, 1, 0, 704, 99
42486, V, 1, 1, 1, 1, 0, 704, 99
42487, V, 1, 1, 1, 1, 0, 704, 99
42488, V, 1, 1, 1, 1, 0, 704, 99
42489, V, 1, 1, 1, 1, 0, 704, 99
42490, V, 1, 1, 1, 1, 0, 704, 99
42491, V, 1, 1, 1, 1, 0, 704, 99
42492, V, 1, 1, 1, 1, 0, 704, 99
42493, V, 1, 1, 1, 1, 0, 704, 99
42494, V, 1, 1, 1, 1, 0, 704, 99
42496, V, 1, 1, 1, 1, 0, 704, 99
42497, V, 1, 1, 1, 1, 0, 704, 99
42498, V, 1, 1, 1, 1, 0, 704, 99
42499, V, 1, 1, 1, 1, 0, 704, 99
42500, V, 1, 1, 1, 1, 0, 704, 99
42501, V, 1, 1, 1, 1, 0, 704, 99
42502, V, 1, 1, 1, 1, 0, 704, 99
42503, V, 1, 1, 1, 1, 0, 704, 99
42504, V, 1, 1, 1, 1, 0, 704, 99
42505, V, 1, 1, 1, 1, 0, 704, 99
42506, V, 1, 1, 1, 1, 0, 704, 99
42507, V, 1, 1, 1, 1, 0, 704, 99
42508, V, 1, 1, 1, 1, 0, 704, 99
42509, V, 1, 1, 1, 1, 0, 704, 99
42510, V, 1, 1, 1, 1, 0, 704, 99
42511, V, 1, 1, 1, 1, 0, 704, 99
42512, V, 1, 1, 1, 1, 0, 704, 99
42513, V, 1, 1, 1, 1, 0, 704, 99
42514, V, 1, 1, 1, 1, 0, 704, 99
42515, V, 1, 1, 1, 1, 0, 704, 99
42516, V, 1, 1, 1, 1, 0, 704, 99
42517, V, 1, 1, 1, 1, 0, 704, 99
42518, V, 1, 1, 1, 1, 0, 704, 99
42519, V, 1, 1, 1, 1, 0, 704, 99
42520, V, 1, 1, 1, 1, 0, 704, 99
42521, V, 1, 1, 1, 1, 0, 704, 99
42522, V, 1, 1, 1, 1, 0, 704, 99
42523, V, 1, 1, 1, 1, 0, 704, 99
42524, V, 1, 1, 1, 1, 0, 704, 99
42525, V, 1, 1, 1, 1, 0, 704, 99
42526, V, 1, 1, 1, 1, 0, 704, 99
42527, V, 1, 1, 1, 1, 0, 704, 99
42528, V, 1, 1, 1, 1, 0, 704, 99
42529, V, 1, 1, 1, 1, 0, 704, 99
42530, V, 1, 1, 1, 1, 0, 704, 99
42531, V, 1, 1, 1, 1, 0, 704, 99
42532, V, 1, 1, 1, 1, 0, 704, 99
42533, V, 1, 1, 1, 1, 0, 704, 99
42534, V, 1, 1, 1, 1, 0, 704, 99
42535, V, 1, 1, 1, 1, 0, 704, 99
42536, V, 1, 1, 1, 1, 0, 704, 99
42537, V, 1, 1, 1, 1, 0, 704, 99
42539, V, 1, 1, 1, 1, 0, 704, 99
42540, V, 1, 1, 1, 1, 0, 704, 99
42541, V, 1, 1, 1, 1, 0, 704, 99
42542, V, 1, 1, 1, 1, 0, 704, 99
42543, V, 1, 1, 1, 1, 0, 704, 99
42544, V, 1, 1, 1, 1, 0, 704, 99
42545, V, 1, 1, 1, 1, 0, 704, 99
42546, V, 1, 1, 1, 1, 0, 704, 99
42547, V, 1, 1, 1, 1, 0, 704, 99
42548, V, 1, 1, 1, 1, 0, 704, 99
42549, V, 1, 1, 1, 1, 0, 704, 99
42550, V, 1, 1, 1, 1, 0, 704, 99
42551, V, 1, 1, 1, 1, 0, 704, 99
42552, V, 1, 1, 1, 1, 0, 704, 99
42553, V, 1, 1, 1, 1, 0, 704, 99
42554, V, 1, 1, 1, 1, 0, 704, 99
42555, V, 1, 1, 1, 1, 0, 704, 99
42556, V, 1, 1, 1, 1, 0, 704, 99
42557, V, 1, 1, 1, 1, 0, 704, 99
42558, V, 1, 1, 1, 1, 0, 704, 99
42559, V, 1, 1, 1, 1, 0, 704, 99
42560, V, 1, 1, 1, 1, 0, 704, 99
42561, V, 1, 1, 1, 1, 0, 704, 99
42562, V, 1, 1, 1, 1, 0, 704, 99
42563, V, 1, 1, 1, 1, 0, 704, 99
42564, V, 1, 1, 1, 1, 0, 704, 99
42565, V, 1, 1, 1, 1, 0, 704, 99
42566, V, 1, 1, 1, 1, 0, 704, 99
42567, V, 1, 1, 1, 1, 0, 704, 99
42568, V, 1, 1, 1, 1, 0, 704, 99
42569, V, 1, 1, 1, 1, 0, 704, 99
42570, V, 1, 1, 1, 1, 0, 704, 99
42571, V, 1, 1, 1, 1, 0, 704, 99
42572, V, 1, 1, 1, 1, 0, 704, 99
42573, V, 1, 1, 1, 1, 0, 704, 99
42574, V, 1, 1, 1, 1, 0, 704, 99
42575, V, 1, 1, 1, 1, 0, 704, 99
42576, V, 1, 1, 1, 1, 0, 704, 99
42577, V, 1, 1, 1, 1, 0, 704, 99
42578, V, 1, 1, 1, 1, 0, 704, 99
42579, V, 1, 1, 1, 1, 0, 704, 99
42580, V, 1, 1, 1, 1, 0, 704, 99
42582, V, 1, 1, 1, 1, 0, 704, 99
42583, V, 1, 1, 1, 1, 0, 704, 99
42584, V, 1, 1, 1, 1, 0, 704, 99
42585, V, 1, 1, 1, 1, 0, 704, 99
42586, V, 1, 1, 1, 1, 0, 704, 99
42587, V, 1, 1, 1, 1, 0, 704, 99
42588, V, 1, 1, 1, 1, 0, 704, 99
42589, V, 1, 1, 1, 1, 0, 704, 99
42590, V, 1, 1, 1, 1, 0, 704, 99
42591, V, 1, 1, 1, 1, 0, 704, 99
42592, V, 1, 1, 1, 1, 0, 704, 99
42593, V, 1, 1, 1, 1, 0, 704, 99
42594, V, 1, 1, 1, 1, 0, 704, 99
42595, V, 1, 1, 1, 1, 0, 704, 99
42596, V, 1, 1, 1, 1, 0, 704, 99
42597, V, 1, 1, 1, 1, 0, 704, 99
42598, V, 1, 1, 1, 1, 0, 704, 99
42599, V, 1, 1, 1, 1, 0, 704, 99
42600, V, 1, 1, 1, 1, 0, 704, 99
42601, V, 1, 1, 1, 1, 0, 704, 99
42602, V, 1, 1, 1, 1, 0, 704, 99
42603, V, 1, 1, 1, 1, 0, 704, 99
42604, V, 1, 1, 1, 1, 0, 704, 99
42605, V, 1, 1, 1, 1, 0, 704, 99
42606, V, 1, 1, 1, 1, 0, 704, 99
42607, V, 1, 1, 1, 1, 0, 704, 99
42608, V, 1, 1, 1, 1, 0, 704, 99
42609, V, 1, 1, 1, 1, 0, 704, 99
42610, V, 1, 1, 1, 1, 0, 704, 99
42611, V, 1, 1, 1, 1, 0, 704, 99
42612, V, 1, 1, 1, 1, 0, 704, 99
42613, V, 1, 1, 1, 1, 0, 704, 99
42614, V, 1, 1, 1, 1, 0, 704, 99
42615, V, 1, 1, 1, 1, 0, 704, 99
42616, V, 1, 1, 1, 1, 0, 704, 99
42617, V, 1, 1, 1, 1, 0, 704, 99
42618, V, 1, 1, 1, 1, 0, 704, 99
42619, V, 1, 1, 1, 1, 0, 704, 99
42620, V, 1, 1, 1, 1, 0, 704, 99
42621, V, 1, 1, 1, 1, 0, 704, 99
42622, V, 1, 1, 1, 1, 0, 704, 99
42624, V, 1, 1, 1, 1, 0, 704, 99
42625, V, 1, 1, 1, 1, 0, 704, 99
42626, V, 1, 1, 1, 1, 0, 704, 99
42627, V, 1, 1, 1, 1, 0, 704, 99
42628, V, 1, 1, 1, 1, 0, 704, 99
42629, V, 1, 1, 1, 1, 0, 704, 99
42630, V, 1, 1, 1, 1, 0, 704, 99
42631, V, 1, 1, 1, 1, 0, 704, 99
42632, V, 1, 1, 1, 1, 0, 704, 99
42633, V, 1, 1, 1, 1, 0, 704, 99
42634, V, 1, 1, 1, 1, 0, 704, 99
42635, V, 1, 1, 1, 1, 0, 704, 99
42636, V, 1, 1, 1, 1, 0, 704, 99
42637, V, 1, 1, 1, 1, 0, 704, 99
42638, V, 1, 1, 1, 1, 0, 704, 99
42639, V, 1, 1, 1, 1, 0, 704, 99
42640, V, 1, 1, 1, 1, 0, 704, 99
42641, V, 1, 1, 1, 1, 0, 704, 99
42642, V, 1, 1, 1, 1, 0, 704, 99
42643, V, 1, 1, 1, 1, 0, 704, 99
42644, V, 1, 1, 1, 1, 0, 704, 99
42645, V, 1, 1, 1, 1, 0, 704, 99
42646, V, 1, 1, 1, 1, 0, 704, 99
42647, V, 1, 1, 1, 1, 0, 704, 99
42648, V, 1, 1, 1, 1, 0, 704, 99
42649, V, 1, 1, 1, 1, 0, 704, 99
42650, V, 1, 1, 1, 1, 0, 704, 99
42651, V, 1, 1, 1, 1, 0, 704, 99
42652, V, 1, 1, 1, 1, 0, 704, 99
42653, V, 1, 1, 1, 1, 0, 704, 99
42654, V, 1, 1, 1, 1, 0, 704, 99
42655, V, 1, 1, 1, 1, 0, 704, 99
42656, V, 1, 1, 1, 1, 0, 704, 99
42657, V, 1, 1, 1, 1, 0, 704, 99
42658, V, 1, 1, 1, 1, 0, 704, 99
42659, V, 1, 1, 1, 1, 0, 704, 99
42660, V, 1, 1, 1, 1, 0, 704, 99
42661, V, 1, 1, 1, 1, 0, 704, 99
42662, V, 1, 1, 1, 1, 0, 704, 99
42663, V, 1, 1, 1, 1, 0, 704, 99
42664, V, 1, 1, 1, 1, 0, 704, 99
42665, V, 1, 1, 1, 1, 0, 704, 99
42667, V, 1, 1, 1, 1, 0, 704, 99
42668, V, 1, 1, 1, 1, 0, 704, 99
42669, V, 1, 1, 1, 1, 0, 704, 99
42670, V, 1, 1, 1, 1, 0, 704, 99
42671, V, 1, 1, 1, 1, 0, 704, 99
42672, V, 1, 1, 1, 1, 0, 704, 99
42673, V, 1, 1, 1, 1, 0, 704, 99
42674, V, 1, 1, 1, 1, 0, 704, 99
42675, V, 1, 1, 1, 1, 0, 704, 99
42676, V, 1, 1, 1, 1, 0, 704, 99
42677, V, 1, 1, 1, 1, 0, 704, 99
42678, V, 1, 1, 1, 1, 0, 704, 99
42679, V, 1, 1, 1, 1, 0, 704, 99
42680, V, 1, 1, 1, 1, 0, 704, 99
42681, V, 1, 1, 1, 1, 0, 704, 99
42682, V, 1, 1, 1, 1, 0, 704, 99
42683, V, 1, 1, 1, 1, 0, 704, 99
42684, V, 1, 1, 1, 1, 0, 704, 99
42685, V, 1, 1, 1, 1, 0, 704, 99
42686, V, 1, 1, 1, 1, 0, 704, 99
42687, V, 1, 1, 1, 1, 0, 704, 99
42688, V, 1, 1, 1, 1, 0, 704, 99
42689, V, 1, 1, 1, 1, 0, 704, 99
42690, V, 1, 1, 1, 1, 0, 704, 99
42691, V, 1, 1, 1, 1, 0, 704, 99
42692, V, 1, 1, 1, 1, 0, 704, 99
42693, V, 1, 1, 1, 1, 0, 704, 99
42694, V, 1, 1, 1, 1, 0, 704, 99
42695, V, 1, 1, 1, 1, 0, 704, 99
42696, V, 1, 1, 1, 1, 0, 704, 99
42697, V, 1, 1, 1, 1, 0, 704, 99
42698, V, 1, 1, 1, 1, 0, 704, 99
42699, V, 1, 1, 1, 1, 0, 704, 99
42700, V, 1, 1, 1, 1, 0, 704, 99
42701, V, 1, 1, 1, 1, 0, 704, 99
42702, V, 1, 1, 1, 1, 0, 704, 99
42703, V, 1, 1, 1, 1, 0, 704, 99
42704, V, 1, 1, 1, 1, 0, 704, 99
42705, V, 1, 1, 1, 1, 0, 704, 99
42706, V, 1, 1, 1, 1, 0, 704, 99
42707, V, 1, 1, 1, 1, 0, 704, 99
42708, V, 1, 1, 1, 1, 0, 704, 99
42710, V, 1, 1, 1, 1, 0, 704, 99
42711, V, 1, 1, 1, 1, 0, 704, 99
42712, V, 1, 1, 1, 1, 0, 704, 99
42713, V, 1, 1, 1, 1, 0, 704, 99
42714, V, 1, 1, 1, 1, 0, 704, 99
42715, V, 1, 1, 1, 1, 0, 704, 99
42716, V, 1, 1, 1, 1, 0, 704, 99
42717, V, 1, 1, 1, 1, 0, 704, 99
42718, V, 1, 1, 1, 1, 0, 704, 99
42719, V, 1, 1, 1, 1, 0, 704, 99
42720, V, 1, 1, 1, 1, 0, 704, 99
42721, V, 1, 1, 1, 1, 0, 704, 99
42722, V, 1, 1, 1, 1, 0, 704, 99
42723, V, 1, 1, 1, 1, 0, 704, 99
42724, V, 1, 1, 1, 1, 0, 704, 99
42725, V, 1, 1, 1, 1, 0, 704, 99
42726, V, 1, 1, 1, 1, 0, 704, 99
42727, V, 1, 1, 1, 1, 0, 704, 99
42728, V, 1, 1, 1, 1, 0, 704, 99
42729, V, 1, 1, 1, 1, 0, 704, 99
42730, V, 1, 1, 1, 1, 0, 704, 99
42731, V, 1, 1, 1, 1, 0, 704, 99
42732, V, 1, 1, 1, 1, 0, 704, 99
42733, V, 1, 1, 1, 1, 0, 704, 99
42734, V, 1, 1, 1, 1, 0, 704, 99
42735, V, 1, 1, 1, 1, 0, 704, 99
42736, V, 1, 1, 1, 1, 0, 704, 99
42737, V, 1, 1, 1, 1, 0, 704, 99
42738, V, 1, 1, 1, 1, 0, 704, 99
42739, V, 1, 1, 1, 1, 0, 704, 99
42740, V, 1, 1, 1, 1, 0, 704, 99
42741, V, 1, 1, 1, 1, 0, 704, 99
42742, V, 1, 1, 1, 1, 0, 704, 99
42743, V, 1, 1, 1, 1, 0, 704, 99
42744, V, 1, 1, 1, 1, 0, 704, 99
42745, V, 1, 1, 1, 1, 0, 704, 99
42746, V, 1, 1, 1, 1, 0, 704, 99
42747, V, 1, 1, 1, 1, 0, 704, 99
42748, V, 1, 1, 1, 1, 0, 704, 99
42749, V, 1, 1, 1, 1, 0, 704, 99
42750, V, 1, 1, 1, 1, 0, 704, 99
42752, V, 1, 1, 1, 1, 0, 704, 99
42753, V, 1, 1, 1, 1, 0, 704, 99
42754, V, 1, 1, 1, 1, 0, 704, 99
42755, V, 1, 1, 1, 1, 0, 704, 99
42756, V, 1, 1, 1, 1, 0, 704, 99
42757, V, 1, 1, 1, 1, 0, 704, 99
42758, V, 1, 1, 1, 1, 0, 704, 99
42759, V, 1, 1, 1, 1, 0, 704, 99
42760, V, 1, 1, 1, 1, 0, 704, 99
42761, V, 1, 1, 1, 1, 0, 704, 99
42762, V, 1, 1, 1, 1, 0, 704, 99
42763, V, 1, 1, 1, 1, 0, 704, 99
42764, V, 1, 1, 1, 1, 0, 704, 99
42765, V, 1, 1, 1, 1, 0, 704, 99
42766, V, 1, 1, 1, 1, 0, 704, 99
42767, V, 1, 1, 1, 1, 0, 704, 99
42768, V, 1, 1, 1, 1, 0, 704, 99
42769, V, 1, 1, 1, 1, 0, 704, 99
42770, V, 1, 1, 1, 1, 0, 704, 99
42771, V, 1, 1, 1, 1, 0, 704, 99
42772, V, 1, 1, 1, 1, 0, 704, 99
42773, V, 1, 1, 1, 1, 0, 704, 99
42774, V, 1, 1, 1, 1, 0, 704, 99
42775, V, 1, 1, 1, 1, 0, 704, 99
42776, V, 1, 1, 1, 1, 0, 704, 99
42777, V, 1, 1, 1, 1, 0, 704, 99
42778, V, 1, 1, 1, 1, 0, 704, 99
42779, V, 1, 1, 1, 1, 0, 704, 99
42780, V, 1, 1, 1, 1, 0, 704, 99
42781, V, 1, 1, 1, 1, 0, 704, 99
42782, V, 1, 1, 1, 1, 0, 704, 99
42783, V, 1, 1, 1, 1, 0, 704, 99
42784, V, 1, 1, 1, 1, 0, 704, 99
42785, V, 1, 1, 1, 1, 0, 704, 99
42786, V, 1, 1, 1, 1, 0, 704, 99
42787, V, 1, 1, 1, 1, 0, 704, 99
42788, V, 1, 1, 1, 1, 0, 704, 99
42789, V, 1, 1, 1, 1, 0, 704, 99
42790, V, 1, 1, 1, 1, 0, 704, 99
42791, V, 1, 1, 1, 1, 0, 704, 99
42792, V, 1, 1, 1, 1, 0, 704, 99
42793, V, 1, 1, 1, 1, 0, 704, 99
42795, V, 1, 1, 1, 1, 0, 704, 99
42796, V, 1, 1, 1, 1, 0, 704, 99
42797, V, 1, 1, 1, 1, 0, 704, 99
42798, V, 1, 1, 1, 1, 0, 704, 99
42799, V, 1, 1, 1, 1, 0, 704, 99
42800, V, 1, 1, 1, 1, 0, 704, 99
42801, V, 1, 1, 1, 1, 0, 704, 99
42802, V, 1, 1, 1, 1, 0, 704, 99
42803, V, 1, 1, 1, 1, 0, 704, 99
42804, V, 1, 1, 1, 1, 0, 704, 99
42805, V, 1, 1, 1, 1, 0, 704, 99
42806, V, 1, 1, 1, 1, 0, 704, 99
42807, V, 1, 1, 1, 1, 0, 704, 99
42808, V, 1, 1, 1, 1, 0, 704, 99
42809, V, 1, 1, 1, 1, 0, 704, 99
42810, V, 1, 1, 1, 1, 0, 704, 99
42811, V, 1, 1, 1, 1, 0, 704, 99
42812, V, 1, 1, 1, 1, 0, 704, 99
42813, V, 1, 1, 1, 1, 0, 704, 99
42814, V, 1, 1, 1, 1, 0, 704, 99
42815, V, 1, 1, 1, 1, 0, 704, 99
42816, V, 1, 1, 1, 1, 0, 704, 99
42817, V, 1, 1, 1, 1, 0, 704, 99
42818, V, 1, 1, 1, 1, 0, 704, 99
42819, V, 1, 1, 1, 1, 0, 704, 99
42820, V, 1, 1, 1, 1, 0, 704, 99
42821, V, 1, 1, 1, 1, 0, 704, 99
42822, V, 1, 1, 1, 1, 0, 704, 99
42823, V, 1, 1, 1, 1, 0, 704, 99
42824, V, 1, 1, 1, 1, 0, 704, 99
42825, V, 1, 1, 1, 1, 0, 704, 99
42826, V, 1, 1, 1, 1, 0, 704, 99
42827, V, 1, 1, 1, 1, 0, 704, 99
42828, V, 1, 1, 1, 1, 0, 704, 99
42829, V, 1, 1, 1, 1, 0, 704, 99
42830, V, 1, 1, 1, 1, 0, 704, 99
42831, V, 1, 1, 1, 1, 0, 704, 99
42832, V, 1, 1, 1, 1, 0, 704, 99
42833, V, 1, 1, 1, 1, 0, 704, 99
42834, V, 1, 1, 1, 1, 0, 704, 99
42835, V, 1, 1, 1, 1, 0, 704, 99
42836, V, 1, 1, 1, 1, 0, 704, 99
42838, V, 1, 1, 1, 1, 0, 704, 99
42839, V, 1, 1, 1, 1, 0, 704, 99
42840, V, 1, 1, 1, 1, 0, 704, 99
42841, V, 1, 1, 1, 1, 0, 704, 99
42842, V, 1, 1, 1, 1, 0, 704, 99
42843, V, 1, 1, 1, 1, 0, 704, 99
42844, V, 1, 1, 1, 1, 0, 704, 99
42845, V, 1, 1, 1, 1, 0, 704, 99
42846, V, 1, 1, 1, 1, 0, 704, 99
42847, V, 1, 1, 1, 1, 0, 704, 99
42848, V, 1, 1, 1, 1, 0, 704, 99
42849, V, 1, 1, 1, 1, 0, 704, 99
42850, V, 1, 1, 1, 1, 0, 704, 99
42851, V, 1, 1, 1, 1, 0, 704, 99
42852, V, 1, 1, 1, 1, 0, 704, 99
42853, V, 1, 1, 1, 1, 0, 704, 99
42854, V, 1, 1, 1, 1, 0, 704, 99
42855, V, 1, 1, 1, 1, 0, 704, 99
42856, V, 1, 1, 1, 1, 0, 704, 99
42857, V, 1, 1, 1, 1, 0, 704, 99
42858, V, 1, 1, 1, 1, 0, 704, 99
42859, V, 1, 1, 1, 1, 0, 704, 99
42860, V, 1, 1, 1, 1, 0, 704, 99
42861, V, 1, 1, 1, 1, 0, 704, 99
42862, V, 1, 1, 1, 1, 0, 704, 99
42863, V, 1, 1, 1, 1, 0, 704, 99
42864, V, 1, 1, 1, 1, 0, 704, 99
42865, V, 1, 1, 1, 1, 0, 704, 99
42866, V, 1, 1, 1, 1, 0, 704, 99
42867, V, 1, 1, 1, 1, 0, 704, 99
42868, V, 1, 1, 1, 1, 0, 704, 99
42869, V, 1, 1, 1, 1, 0, 704, 99
42870, V, 1, 1, 1, 1, 0, 704, 99
42871, V, 1, 1, 1, 1, 0, 704, 99
42872, V, 1, 1, 1, 1, 0, 704, 99
42873, V, 1, 1, 1, 1, 0, 704, 99
42874, V, 1, 1, 1, 1, 0, 704, 99
42875, V, 1, 1, 1, 1, 0, 704, 99
42876, V, 1, 1, 1, 1, 0, 704, 99
42877, V, 1, 1, 1, 1, 0, 704, 99
42878, V, 1, 1, 1, 1, 0, 704, 99
42880, V, 1, 1, 1, 1, 0, 704, 99
42881, V, 1, 1, 1, 1, 0, 704, 99
42882, V, 1, 1, 1, 1, 0, 704, 99
42883, V, 1, 1, 1, 1, 0, 704, 99
42884, V, 1, 1, 1, 1, 0, 704, 99
42885, V, 1, 1, 1, 1, 0, 704, 99
42886, V, 1, 1, 1, 1, 0, 704, 99
42887, V, 1, 1, 1, 1, 0, 704, 99
42888, V, 1, 1, 1, 1, 0, 704, 99
42889, V, 1, 1, 1, 1, 0, 704, 99
42890, V, 1, 1, 1, 1, 0, 704, 99
42891, V, 1, 1, 1, 1, 0, 704, 99
42892, V, 1, 1, 1, 1, 0, 704, 99
42893, V, 1, 1, 1, 1, 0, 704, 99
42894, V, 1, 1, 1, 1, 0, 704, 99
42895, V, 1, 1, 1, 1, 0, 704, 99
42896, V, 1, 1, 1, 1, 0, 704, 99
42897, V, 1, 1, 1, 1, 0, 704, 99
42898, V, 1, 1, 1, 1, 0, 704, 99
42899, V, 1, 1, 1, 1, 0, 704, 99
42900, V, 1, 1, 1, 1, 0, 704, 99
42901, V, 1, 1, 1, 1, 0, 704, 99
42902, V, 1, 1, 1, 1, 0, 704, 99
42903, V, 1, 1, 1, 1, 0, 704, 99
42904, V, 1, 1, 1, 1, 0, 704, 99
42905, V, 1, 1, 1, 1, 0, 704, 99
42906, V, 1, 1, 1, 1, 0, 704, 99
42907, V, 1, 1, 1, 1, 0, 704, 99
42908, V, 1, 1, 1, 1, 0, 704, 99
42909, V, 1, 1, 1, 1, 0, 704, 99
42910, V, 1, 1, 1, 1, 0, 704, 99
42911, V, 1, 1, 1, 1, 0, 704, 99
42912, V, 1, 1, 1, 1, 0, 704, 99
42913, V, 1, 1, 1, 1, 0, 704, 99
42914, V, 1, 1, 1, 1, 0, 704, 99
42915, V, 1, 1, 1, 1, 0, 704, 99
42916, V, 1, 1, 1, 1, 0, 704, 99
42917, V, 1, 1, 1, 1, 0, 704, 99
42918, V, 1, 1, 1, 1, 0, 704, 99
42919, V, 1, 1, 1, 1, 0, 704, 99
42920, V, 1, 1, 1, 1, 0, 704, 99
42921, V, 1, 1, 1, 1, 0, 704, 99
42923, V, 1, 1, 1, 1, 0, 704, 99
42924, V, 1, 1, 1, 1, 0, 704, 99
42925, V, 1, 1, 1, 1, 0, 704, 99
42926, V, 1, 1, 1, 1, 0, 704, 99
42927, V, 1, 1, 1, 1, 0, 704, 99
42928, V, 1, 1, 1, 1, 0, 704, 99
42929, V, 1, 1, 1, 1, 0, 704, 99
42930, V, 1, 1, 1, 1, 0, 704, 99
42931, V, 1, 1, 1, 1, 0, 704, 99
42932, V, 1, 1, 1, 1, 0, 704, 99
42933, V, 1, 1, 1, 1, 0, 704, 99
42934, V, 1, 1, 1, 1, 0, 704, 99
42935, V, 1, 1, 1, 1, 0, 704, 99
42936, V, 1, 1, 1, 1, 0, 704, 99
42937, V, 1, 1, 1, 1, 0, 704, 99
42938, V, 1, 1, 1, 1, 0, 704, 99
42939, V, 1, 1, 1, 1, 0, 704, 99
42940, V, 1, 1, 1, 1, 0, 704, 99
42941, V, 1, 1, 1, 1, 0, 704, 99
42942, V, 1, 1, 1, 1, 0, 704, 99
42943, V, 1, 1, 1, 1, 0, 704, 99
42944, V, 1, 1, 1, 1, 0, 704, 99
42945, V, 1, 1, 1, 1, 0, 704, 99
42946, V, 1, 1, 1, 1, 0, 704, 99
42947, V, 1, 1, 1, 1, 0, 704, 99
42948, V, 1, 1, 1, 1, 0, 704, 99
42949, V, 1, 1, 1, 1, 0, 704, 99
42950, V, 1, 1, 1, 1, 0, 704, 99
42951, V, 1, 1, 1, 1, 0, 704, 99
42952, V, 1, 1, 1, 1, 0, 704, 99
42953, V, 1, 1, 1, 1, 0, 704, 99
42954, V, 1, 1, 1, 1, 0, 704, 99
42955, V, 1, 1, 1, 1, 0, 704, 99
42956, V, 1, 1, 1, 1, 0, 704, 99
42957, V, 1, 1, 1, 1, 0, 704, 99
42958, V, 1, 1, 1, 1, 0, 704, 99
42959, V, 1, 1, 1, 1, 0, 704, 99
42960, V, 1, 1, 1, 1, 0, 704, 99
42961, V, 1, 1, 1, 1, 0, 704, 99
42962, V, 1, 1, 1, 1, 0, 704, 99
42963, V, 1, 1, 1, 1, 0, 704, 99
42964, V, 1, 1, 1, 1, 0, 704, 99
42966, V, 1, 1, 1, 1, 0, 704, 99
42967, V, 1, 1, 1, 1, 0, 704, 99
42968, V, 1, 1, 1, 1, 0, 704, 99
42969, V, 1, 1, 1, 1, 0, 704, 99
42970, V, 1, 1, 1, 1, 0, 704, 99
42971, V, 1, 1, 1, 1, 0, 704, 99
42972, V, 1, 1, 1, 1, 0, 704, 99
42973, V, 1, 1, 1, 1, 0, 704, 99
42974, V, 1, 1, 1, 1, 0, 704, 99
42975, V, 1, 1, 1, 1, 0, 704, 99
42976, V, 1, 1, 1, 1, 0, 704, 99
42977, V, 1, 1, 1, 1, 0, 704, 99
42978, V, 1, 1, 1, 1, 0, 704, 99
42979, V, 1, 1, 1, 1, 0, 704, 99
42980, V, 1, 1, 1, 1, 0, 704, 99
42981, V, 1, 1, 1, 1, 0, 704, 99
42982, V, 1, 1, 1, 1, 0, 704, 99
42983, V, 1, 1, 1, 1, 0, 704, 99
42984, V, 1, 1, 1, 1, 0, 704, 99
42985, V, 1, 1, 1, 1, 0, 704, 99
42986, V, 1, 1, 1, 1, 0, 704, 99
42987, V, 1, 1, 1, 1, 0, 704, 99
42988, V, 1, 1, 1, 1, 0, 704, 99
42989, V, 1, 1, 1, 1, 0, 704, 99
42990, V, 1, 1, 1, 1, 0, 704, 99
42991, V, 1, 1, 1, 1, 0, 704, 99
42992, V, 1, 1, 1, 1, 0, 704, 99
42993, V, 1, 1, 1, 1, 0, 704, 99
42994, V, 1, 1, 1, 1, 0, 704, 99
42995, V, 1, 1, 1, 1, 0, 704, 99
42996, V, 1, 1, 1, 1, 0, 704, 99
42997, V, 1, 1, 1, 1, 0, 704, 99
42998, V, 1, 1, 1, 1, 0, 704, 99
42999, V, 1, 1, 1, 1, 0, 704, 99
43000, V, 1, 1, 1, 1, 0, 704, 99
43001, V, 1, 1, 1, 1, 0, 704, 99
43002, V, 1, 1, 1, 1, 0, 704, 99
43003, V, 1, 1, 1, 1, 0, 704, 99
43004, V, 1, 1, 1, 1, 0, 704, 99
43005, V, 1, 1, 1, 1, 0, 704, 99
43006, V, 1, 1, 1, 1, 0, 704, 99
43008, V, 1, 1, 1, 1, 0, 704, 99
43009, V, 1, 1, 1, 1, 0, 704, 99
43010, V, 1, 1, 1, 1, 0, 704, 99
43011, V, 1, 1, 1, 1, 0, 704, 99
43012, V, 1, 1, 1, 1, 0, 704, 99
43013, V, 1, 1, 1, 1, 0, 704, 99
43014, V, 1, 1, 1, 1, 0, 704, 99
43015, V, 1, 1, 1, 1, 0, 704, 99
43016, V, 1, 1, 1, 1, 0, 704, 99
43017, V, 1, 1, 1, 1, 0, 704, 99
43018, V, 1, 1, 1, 1, 0, 704, 99
43019, V, 1, 1, 1, 1, 0, 704, 99
43020, V, 1, 1, 1, 1, 0, 704, 99
43021, V, 1, 1, 1, 1, 0, 704, 99
43022, V, 1, 1, 1, 1, 0, 704, 99
43023, V, 1, 1, 1, 1, 0, 704, 99
43024, V, 1, 1, 1, 1, 0, 704, 99
43025, V, 1, 1, 1, 1, 0, 704, 99
43026, V, 1, 1, 1, 1, 0, 704, 99
43027, V, 1, 1, 1, 1, 0, 704, 99
43028, V, 1, 1, 1, 1, 0, 704, 99
43029, V, 1, 1, 1, 1, 0, 704, 99
43030, V, 1, 1, 1, 1, 0, 704, 99
43031, V, 1, 1, 1, 1, 0, 704, 99
43032, V, 1, 1, 1, 1, 0, 704, 99
43033, V, 1, 1, 1, 1, 0, 704, 99
43034, V, 1, 1, 1, 1, 0, 704, 99
43035, V, 1, 1, 1, 1, 0, 704, 99
43036, V, 1, 1, 1, 1, 0, 704, 99
43037, V, 1, 1, 1, 1, 0, 704, 99
43038, V, 1, 1, 1, 1, 0, 704, 99
43039, V, 1, 1, 1, 1, 0, 704, 99
43040, V, 1, 1, 1, 1, 0, 704, 99
43041, V, 1, 1, 1, 1, 0, 704, 99
43042, V, 1, 1, 1, 1, 0, 704, 99
43043, V, 1, 1, 1, 1, 0, 704, 99
43044, V, 1, 1, 1, 1, 0, 704, 99
43045, V, 1, 1, 1, 1, 0, 704, 99
43046, V, 1, 1, 1, 1, 0, 704, 99
43047, V, 1, 1, 1, 1, 0, 704, 99
43048, V, 1, 1, 1, 1, 0, 704, 99
43049, V, 1, 1, 1, 1, 0, 704, 99
43051, V, 1, 1, 1, 1, 0, 704, 99
43052, V, 1, 1, 1, 1, 0, 704, 99
43053, V, 1, 1, 1, 1, 0, 704, 99
43054, V, 1, 1, 1, 1, 0, 704, 99
43055, V, 1, 1, 1, 1, 0, 704, 99
43056, V, 1, 1, 1, 1, 0, 704, 99
43057, V, 1, 1, 1, 1, 0, 704, 99
43058, V, 1, 1, 1, 1, 0, 704, 99
43059, V, 1, 1, 1, 1, 0, 704, 99
43060, V, 1, 1, 1, 1, 0, 704, 99
43061, V, 1, 1, 1, 1, 0, 704, 99
43062, V, 1, 1, 1, 1, 0, 704, 99
43063, V, 1, 1, 1, 1, 0, 704, 99
43064, V, 1, 1, 1, 1, 0, 704, 99
43065, V, 1, 1, 1, 1, 0, 704, 99
43066, V, 1, 1, 1, 1, 0, 704, 99
43067, V, 1, 1, 1, 1, 0, 704, 99
43068, V, 1, 1, 1, 1, 0, 704, 99
43069, V, 1, 1, 1, 1, 0, 704, 99
43070, V, 1, 1, 1, 1, 0, 704, 99
43071, V, 1, 1, 1, 1, 0, 704, 99
43072, V, 1, 1, 1, 1, 0, 704, 99
43073, V, 1, 1, 1, 1, 0, 704, 99
43074, V, 1, 1, 1, 1, 0, 704, 99
43075, V, 1, 1, 1, 1, 0, 704, 99
43076, V, 1, 1, 1, 1, 0, 704, 99
43077, V, 1, 1, 1, 1, 0, 704, 99
43078, V, 1, 1, 1, 1, 0, 704, 99
43079, V, 1, 1, 1, 1, 0, 704, 99
43080, V, 1, 1, 1, 1, 0, 704, 99
43081, V, 1, 1, 1, 1, 0, 704, 99
43082, V, 1, 1, 1, 1, 0, 704, 99
43083, V, 1, 1, 1, 1, 0, 704, 99
43084, V, 1, 1, 1, 1, 0, 704, 99
43085, V, 1, 1, 1, 1, 0, 704, 99
43086, V, 1, 1, 1, 1, 0, 704, 99
43087, V, 1, 1, 1, 1, 0, 704, 99
43088, V, 1, 1, 1, 1, 0, 704, 99
43089, V, 1, 1, 1, 1, 0, 704, 99
43090, V, 1, 1, 1, 1, 0, 704, 99
43091, V, 1, 1, 1, 1, 0, 704, 99
43092, V, 1, 1, 1, 1, 0, 704, 99
43094, V, 1, 1, 1, 1, 0, 704, 99
43095, V, 1, 1, 1, 1, 0, 704, 99
43096, V, 1, 1, 1, 1, 0, 704, 99
43097, V, 1, 1, 1, 1, 0, 704, 99
43098, V, 1, 1, 1, 1, 0, 704, 99
43099, V, 1, 1, 1, 1, 0, 704, 99
43100, V, 1, 1, 1, 1, 0, 704, 99
43101, V, 1, 1, 1, 1, 0, 704, 99
43102, V, 1, 1, 1, 1, 0, 704, 99
43103, V, 1, 1, 1, 1, 0, 704, 99
43104, V, 1, 1, 1, 1, 0, 704, 99
43105, V, 1, 1, 1, 1, 0, 704, 99
43106, V, 1, 1, 1, 1, 0, 704, 99
43107, V, 1, 1, 1, 1, 0, 704, 99
43108, V, 1, 1, 1, 1, 0, 704, 99
43109, V, 1, 1, 1, 1, 0, 704, 99
43110, V, 1, 1, 1, 1, 0, 704, 99
43111, V, 1, 1, 1, 1, 0, 704, 99
43112, V, 1, 1, 1, 1, 0, 704, 99
43113, V, 1, 1, 1, 1, 0, 704, 99
43114, V, 1, 1, 1, 1, 0, 704, 99
43115, V, 1, 1, 1, 1, 0, 704, 99
43116, V, 1, 1, 1, 1, 0, 704, 99
43117, V, 1, 1, 1, 1, 0, 704, 99
43118, V, 1, 1, 1, 1, 0, 704, 99
43119, V, 1, 1, 1, 1, 0, 704, 99
43120, V, 1, 1, 1, 1, 0, 704, 99
43121, V, 1, 1, 1, 1, 0, 704, 99
43122, V, 1, 1, 1, 1, 0, 704, 99
43123, V, 1, 1, 1, 1, 0, 704, 99
43124, V, 1, 1, 1, 1, 0, 704, 99
43125, V, 1, 1, 1, 1, 0, 704, 99
43126, V, 1, 1, 1, 1, 0, 704, 99
43127, V, 1, 1, 1, 1, 0, 704, 99
43128, V, 1, 1, 1, 1, 0, 704, 99
43129, V, 1, 1, 1, 1, 0, 704, 99
43130, V, 1, 1, 1, 1, 0, 704, 99
43131, V, 1, 1, 1, 1, 0, 704, 99
43132, V, 1, 1, 1, 1, 0, 704, 99
43133, V, 1, 1, 1, 1, 0, 704, 99
43134, V, 1, 1, 1, 1, 0, 704, 99
43136, V, 1, 1, 1, 1, 0, 704, 99
43137, V, 1, 1, 1, 1, 0, 704, 99
43138, V, 1, 1, 1, 1, 0, 704, 99
43139, V, 1, 1, 1, 1, 0, 704, 99
43140, V, 1, 1, 1, 1, 0, 704, 99
43141, V, 1, 1, 1, 1, 0, 704, 99
43142, V, 1, 1, 1, 1, 0, 704, 99
43143, V, 1, 1, 1, 1, 0, 704, 99
43144, V, 1, 1, 1, 1, 0, 704, 99
43145, V, 1, 1, 1, 1, 0, 704, 99
43146, V, 1, 1, 1, 1, 0, 704, 99
43147, V, 1, 1, 1, 1, 0, 704, 99
43148, V, 1, 1, 1, 1, 0, 704, 99
43149, V, 1, 1, 1, 1, 0, 704, 99
43150, V, 1, 1, 1, 1, 0, 704, 99
43151, V, 1, 1, 1, 1, 0, 704, 99
43152, V, 1, 1, 1, 1, 0, 704, 99
43153, V, 1, 1, 1, 1, 0, 704, 99
43154, V, 1, 1, 1, 1, 0, 704, 99
43155, V, 1, 1, 1, 1, 0, 704, 99
43156, V, 1, 1, 1, 1, 0, 704, 99
43157, V, 1, 1, 1, 1, 0, 704, 99
43158, V, 1, 1, 1, 1, 0, 704, 99
43159, V, 1, 1, 1, 1, 0, 704, 99
43160, V, 1, 1, 1, 1, 0, 704, 99
43161, V, 1, 1, 1, 1, 0, 704, 99
43162, V, 1, 1, 1, 1, 0, 704, 99
43163, V, 1, 1, 1, 1, 0, 704, 99
43164, V, 1, 1, 1, 1, 0, 704, 99
43165, V, 1, 1, 1, 1, 0, 704, 99
43166, V, 1, 1, 1, 1, 0, 704, 99
43167, V, 1, 1, 1, 1, 0, 704, 99
43168, V, 1, 1, 1, 1, 0, 704, 99
43169, V, 1, 1, 1, 1, 0, 704, 99
43170, V, 1, 1, 1, 1, 0, 704, 99
43171, V, 1, 1, 1, 1, 0, 704, 99
43172, V, 1, 1, 1, 1, 0, 704, 99
43173, V, 1, 1, 1, 1, 0, 704, 99
43174, V, 1, 1, 1, 1, 0, 704, 99
43175, V, 1, 1, 1, 1, 0, 704, 99
43176, V, 1, 1, 1, 1, 0, 704, 99
43177, V, 1, 1, 1, 1, 0, 704, 99
43179, V, 1, 1, 1, 1, 0, 704, 99
43180, V, 1, 1, 1, 1, 0, 704, 99
43181, V, 1, 1, 1, 1, 0, 704, 99
43182, V, 1, 1, 1, 1, 0, 704, 99
43183, V, 1, 1, 1, 1, 0, 704, 99
43184, V, 1, 1, 1, 1, 0, 704, 99
43185, V, 1, 1, 1, 1, 0, 704, 99
43186, V, 1, 1, 1, 1, 0, 704, 99
43187, V, 1, 1, 1, 1, 0, 704, 99
43188, V, 1, 1, 1, 1, 0, 704, 99
43189, V, 1, 1, 1, 1, 0, 704, 99
43190, V, 1, 1, 1, 1, 0, 704, 99
43191, V, 1, 1, 1, 1, 0, 704, 99
43192, V, 1, 1, 1, 1, 0, 704, 99
43193, V, 1, 1, 1, 1, 0, 704, 99
43194, V, 1, 1, 1, 1, 0, 704, 99
43195, V, 1, 1, 1, 1, 0, 704, 99
43196, V, 1, 1, 1, 1, 0, 704, 99
43197, V, 1, 1, 1, 1, 0, 704, 99
43198, V, 1, 1, 1, 1, 0, 704, 99
43199, V, 1, 1, 1, 1, 0, 704, 99
43200, V, 1, 1, 1, 1, 0, 704, 99
43201, V, 1, 1, 1, 1, 0, 704, 99
43202, V, 1, 1, 1, 1, 0, 704, 99
43203, V, 1, 1, 1, 1, 0, 704, 99
43204, V, 1, 1, 1, 1, 0, 704, 99
43205, V, 1, 1, 1, 1, 0, 704, 99
43206, V, 1, 1, 1, 1, 0, 704, 99
43207, V, 1, 1, 1, 1, 0, 704, 99
43208, V, 1, 1, 1, 1, 0, 704, 99
43209, V, 1, 1, 1, 1, 0, 704, 99
43210, V, 1, 1, 1, 1, 0, 704, 99
43211, V, 1, 1, 1, 1, 0, 704, 99
43212, V, 1, 1, 1, 1, 0, 704, 99
43213, V, 1, 1, 1, 1, 0, 704, 99
43214, V, 1, 1, 1, 1, 0, 704, 99
43215, V, 1, 1, 1, 1, 0, 704, 99
43216, V, 1, 1, 1, 1, 0, 704, 99
43217, V, 1, 1, 1, 1, 0, 704, 99
43218, V, 1, 1, 1, 1, 0, 704, 99
43219, V, 1, 1, 1, 1, 0, 704, 99
43220, V, 1, 1, 1, 1, 0, 704, 99
43222, V, 1, 1, 1, 1, 0, 704, 99
43223, V, 1, 1, 1, 1, 0, 704, 99
43224, V, 1, 1, 1, 1, 0, 704, 99
43225, V, 1, 1, 1, 1, 0, 704, 99
43226, V, 1, 1, 1, 1, 0, 704, 99
43227, V, 1, 1, 1, 1, 0, 704, 99
43228, V, 1, 1, 1, 1, 0, 704, 99
43229, V, 1, 1, 1, 1, 0, 704, 99
43230, V, 1, 1, 1, 1, 0, 704, 99
43231, V, 1, 1, 1, 1, 0, 704, 99
43232, V, 1, 1, 1, 1, 0, 704, 99
43233, V, 1, 1, 1, 1, 0, 704, 99
43234, V, 1, 1, 1, 1, 0, 704, 99
43235, V, 1, 1, 1, 1, 0, 704, 99
43236, V, 1, 1, 1, 1, 0, 704, 99
43237, V, 1, 1, 1, 1, 0, 704, 99
43238, V, 1, 1, 1, 1, 0, 704, 99
43239, V, 1, 1, 1, 1, 0, 704, 99
43240, V, 1, 1, 1, 1, 0, 704, 99
43241, V, 1, 1, 1, 1, 0, 704, 99
43242, V, 1, 1, 1, 1, 0, 704, 99
43243, V, 1, 1, 1, 1, 0, 704, 99
43244, V, 1, 1, 1, 1, 0, 704, 99
43245, V, 1, 1, 1, 1, 0, 704, 99
43246, V, 1, 1, 1, 1, 0, 704, 99
43247, V, 1, 1, 1, 1, 0, 704, 99
43248, V, 1, 1, 1, 1, 0, 704, 99
43249, V, 1, 1, 1, 1, 0, 704, 99
43250, V, 1, 1, 1, 1, 0, 704, 99
43251, V, 1, 1, 1, 1, 0, 704, 99
43252, V, 1, 1, 1, 1, 0, 704, 99
43253, V, 1, 1, 1, 1, 0, 704, 99
43254, V, 1, 1, 1, 1, 0, 704, 99
43255, V, 1, 1, 1, 1, 0, 704, 99
43256, V, 1, 1, 1, 1, 0, 704, 99
43257, V, 1, 1, 1, 1, 0, 704, 99
43258, V, 1, 1, 1, 1, 0, 704, 99
43259, V, 1, 1, 1, 1, 0, 704, 99
43260, V, 1, 1, 1, 1, 0, 704, 99
43261, V, 1, 1, 1, 1, 0, 704, 99
43262, V, 1, 1, 1, 1, 0, 704, 99
43264, V, 1, 1, 1, 1, 0, 704, 99
43265, V, 1, 1, 1, 1, 0, 704, 99
43266, V, 1, 1, 1, 1, 0, 704, 99
43267, V, 1, 1, 1, 1, 0, 704, 99
43268, V, 1, 1, 1, 1, 0, 704, 99
43269, V, 1, 1, 1, 1, 0, 704, 99
43270, V, 1, 1, 1, 1, 0, 704, 99
43271, V, 1, 1, 1, 1, 0, 704, 99
43272, V, 1, 1, 1, 1, 0, 704, 99
43273, V, 1, 1, 1, 1, 0, 704, 99
43274, V, 1, 1, 1, 1, 0, 704, 99
43275, V, 1, 1, 1, 1, 0, 704, 99
43276, V, 1, 1, 1, 1, 0, 704, 99
43277, V, 1, 1, 1, 1, 0, 704, 99
43278, V, 1, 1, 1, 1, 0, 704, 99
43279, V, 1, 1, 1, 1, 0, 704, 99
43280, V, 1, 1, 1, 1, 0, 704, 99
43281, V, 1, 1, 1, 1, 0, 704, 99
43282, V, 1, 1, 1, 1, 0, 704, 99
43283, V, 1, 1, 1, 1, 0, 704, 99
43284, V, 1, 1, 1, 1, 0, 704, 99
43285, V, 1, 1, 1, 1, 0, 704, 99
43286, V, 1, 1, 1, 1, 0, 704, 99
43287, V, 1, 1, 1, 1, 0, 704, 99
43288, V, 1, 1, 1, 1, 0, 704, 99
43289, V, 1, 1, 1, 1, 0, 704, 99
43290, V, 1, 1, 1, 1, 0, 704, 99
43291, V, 1, 1, 1, 1, 0, 704, 99
43292, V, 1, 1, 1, 1, 0, 704, 99
43293, V, 1, 1, 1, 1, 0, 704, 99
43294, V, 1, 1, 1, 1, 0, 704, 99
43295, V, 1, 1, 1, 1, 0, 704, 99
43296, V, 1, 1, 1, 1, 0, 704, 99
43297, V, 1, 1, 1, 1, 0, 704, 99
43298, V, 1, 1, 1, 1, 0, 704, 99
43299, V, 1, 1, 1, 1, 0, 704, 99
43300, V, 1, 1, 1, 1, 0, 704, 99
43301, V, 1, 1, 1, 1, 0, 704, 99
43302, V, 1, 1, 1, 1, 0, 704, 99
43303, V, 1, 1, 1, 1, 0, 704, 99
43304, V, 1, 1, 1, 1, 0, 704, 99
43305, V, 1, 1, 1, 1, 0, 704, 99
43307, V, 1, 1, 1, 1, 0, 704, 99
43308, V, 1, 1, 1, 1, 0, 704, 99
43309, V, 1, 1, 1, 1, 0, 704, 99
43310, V, 1, 1, 1, 1, 0, 704, 99
43311, V, 1, 1, 1, 1, 0, 704, 99
43312, V, 1, 1, 1, 1, 0, 704, 99
43313, V, 1, 1, 1, 1, 0, 704, 99
43314, V, 1, 1, 1, 1, 0, 704, 99
43315, V, 1, 1, 1, 1, 0, 704, 99
43316, V, 1, 1, 1, 1, 0, 704, 99
43317, V, 1, 1, 1, 1, 0, 704, 99
43318, V, 1, 1, 1, 1, 0, 704, 99
43319, V, 1, 1, 1, 1, 0, 704, 99
43320, V, 1, 1, 1, 1, 0, 704, 99
43321, V, 1, 1, 1, 1, 0, 704, 99
43322, V, 1, 1, 1, 1, 0, 704, 99
43323, V, 1, 1, 1, 1, 0, 704, 99
43324, V, 1, 1, 1, 1, 0, 704, 99
43325, V, 1, 1, 1, 1, 0, 704, 99
43326, V, 1, 1, 1, 1, 0, 704, 99
43327, V, 1, 1, 1, 1, 0, 704, 99
43328, V, 1, 1, 1, 1, 0, 704, 99
43329, V, 1, 1, 1, 1, 0, 704, 99
43330, V, 1, 1, 1, 1, 0, 704, 99
43331, V, 1, 1, 1, 1, 0, 704, 99
43332, V, 1, 1, 1, 1, 0, 704, 99
43333, V, 1, 1, 1, 1, 0, 704, 99
43334, V, 1, 1, 1, 1, 0, 704, 99
43335, V, 1, 1, 1, 1, 0, 704, 99
43336, V, 1, 1, 1, 1, 0, 704, 99
43337, V, 1, 1, 1, 1, 0, 704, 99
43338, V, 1, 1, 1, 1, 0, 704, 99
43339, V, 1, 1, 1, 1, 0, 704, 99
43340, V, 1, 1, 1, 1, 0, 704, 99
43341, V, 1, 1, 1, 1, 0, 704, 99
43342, V, 1, 1, 1, 1, 0, 704, 99
43343, V, 1, 1, 1, 1, 0, 704, 99
43344, V, 1, 1, 1, 1, 0, 704, 99
43345, V, 1, 1, 1, 1, 0, 704, 99
43346, V, 1, 1, 1, 1, 0, 704, 99
43347, V, 1, 1, 1, 1, 0, 704, 99
43348, V, 1, 1, 1, 1, 0, 704, 99
43350, V, 1, 1, 1, 1, 0, 704, 99
43351, V, 1, 1, 1, 1, 0, 704, 99
43352, V, 1, 1, 1, 1, 0, 704, 99
43353, V, 1, 1, 1, 1, 0, 704, 99
43354, V, 1, 1, 1, 1, 0, 704, 99
43355, V, 1, 1, 1, 1, 0, 704, 99
43356, V, 1, 1, 1, 1, 0, 704, 99
43357, V, 1, 1, 1, 1, 0, 704, 99
43358, V, 1, 1, 1, 1, 0, 704, 99
43359, V, 1, 1, 1, 1, 0, 704, 99
43360, V, 1, 1, 1, 1, 0, 704, 99
43361, V, 1, 1, 1, 1, 0, 704, 99
43362, V, 1, 1, 1, 1, 0, 704, 99
43363, V, 1, 1, 1, 1, 0, 704, 99
43364, V, 1, 1, 1, 1, 0, 704, 99
43365, V, 1, 1, 1, 1, 0, 704, 99
43366, V, 1, 1, 1, 1, 0, 704, 99
43367, V, 1, 1, 1, 1, 0, 704, 99
43368, V, 1, 1, 1, 1, 0, 704, 99
43369, V, 1, 1, 1, 1, 0, 704, 99
43370, V, 1, 1, 1, 1, 0, 704, 99
43371, V, 1, 1, 1, 1, 0, 704, 99
43372, V, 1, 1, 1, 1, 0, 704, 99
43373, V, 1, 1, 1, 1, 0, 704, 99
43374, V, 1, 1, 1, 1, 0, 704, 99
43375, V, 1, 1, 1, 1, 0, 704, 99
43376, V, 1, 1, 1, 1, 0, 704, 99
43377, V, 1, 1, 1, 1, 0, 704, 99
43378, V, 1, 1, 1, 1, 0, 704, 99
43379, V, 1, 1, 1, 1, 0, 704, 99
43380, V, 1, 1, 1, 1, 0, 704, 99
43381, V, 1, 1, 1, 1, 0, 704, 99
43382, V, 1, 1, 1, 1, 0, 704, 99
43383, V, 1, 1, 1, 1, 0, 704, 99
43384, V, 1, 1, 1, 1, 0, 704, 99
43385, V, 1, 1, 1, 1, 0, 704, 99
43386, V, 1, 1, 1, 1, 0, 704, 99
43387, V, 1, 1, 1, 1, 0, 704, 99
43388, V, 1, 1, 1, 1, 0, 704, 99
43389, V, 1, 1, 1, 1, 0, 704, 99
43390, V, 1, 1, 1, 1, 0, 704, 99
43392, V, 1, 1, 1, 1, 0, 704, 99
43393, V, 1, 1, 1, 1, 0, 704, 99
43394, V, 1, 1, 1, 1, 0, 704, 99
43395, V, 1, 1, 1, 1, 0, 704, 99
43396, V, 1, 1, 1, 1, 0, 704, 99
43397, V, 1, 1, 1, 1, 0, 704, 99
43398, V, 1, 1, 1, 1, 0, 704, 99
43399, V, 1, 1, 1, 1, 0, 704, 99
43400, V, 1, 1, 1, 1, 0, 704, 99
43401, V, 1, 1, 1, 1, 0, 704, 99
43402, V, 1, 1, 1, 1, 0, 704, 99
43403, V, 1, 1, 1, 1, 0, 704, 99
43404, V, 1, 1, 1, 1, 0, 704, 99
43405, V, 1, 1, 1, 1, 0, 704, 99
43406, V, 1, 1, 1, 1, 0, 704, 99
43407, V, 1, 1, 1, 1, 0, 704, 99
43408, V, 1, 1, 1, 1, 0, 704, 99
43409, V, 1, 1, 1, 1, 0, 704, 99
43410, V, 1, 1, 1, 1, 0, 704, 99
43411, V, 1, 1, 1, 1, 0, 704, 99
43412, V, 1, 1, 1, 1, 0, 704, 99
43413, V, 1, 1, 1, 1, 0, 704, 99
43414, V, 1, 1, 1, 1, 0, 704, 99
43415, V, 1, 1, 1, 1, 0, 704, 99
43416, V, 1, 1, 1, 1, 0, 704, 99
43417, V, 1, 1, 1, 1, 0, 704, 99
43418, V, 1, 1, 1, 1, 0, 704, 99
43419, V, 1, 1, 1, 1, 0, 704, 99
43420, V, 1, 1, 1, 1, 0, 704, 99
43421, V, 1, 1, 1, 1, 0, 704, 99
43422, V, 1, 1, 1, 1, 0, 704, 99
43423, V, 1, 1, 1, 1, 0, 704, 99
43424, V, 1, 1, 1, 1, 0, 704, 99
43425, V, 1, 1, 1, 1, 0, 704, 99
43426, V, 1, 1, 1, 1, 0, 704, 99
43427, V, 1, 1, 1, 1, 0, 704, 99
43428, V, 1, 1, 1, 1, 0, 704, 99
43429, V, 1, 1, 1, 1, 0, 704, 99
43430, V, 1, 1, 1, 1, 0, 704, 99
43431, V, 1, 1, 1, 1, 0, 704, 99
43432, V, 1, 1, 1, 1, 0, 704, 99
43433, V, 1, 1, 1, 1, 0, 704, 98
43435, V, 1, 1, 1, 1, 0, 704, 99
43436, V, 1, 1, 1, 1, 0, 704, 99
43437, V, 1, 1, 1, 1, 0, 704, 99
43438, V, 1, 1, 1, 1, 0, 704, 98
43439, V, 1, 1, 1, 1, 0, 704, 98
43440, V, 1, 1, 1, 1, 0, 704, 98
43441, V, 1, 1, 1, 1, 0, 704, 98
43442, V, 1, 1, 1, 1, 0, 704, 99
43443, V, 1, 1, 1, 1, 0, 704, 98
43444, V, 1, 1, 1, 1, 0, 704, 98
43445, V, 1, 1, 1, 1, 0, 704, 98
43446, V, 1, 1, 1, 1, 0, 704, 98
43447, V, 1, 1, 1, 1, 0, 704, 99
43448, V, 1, 1, 1, 1, 0, 704, 98
43449, V, 1, 1, 1, 1, 0, 704, 99
43450, V, 1, 1, 1, 1, 0, 704, 98
43451, V, 1, 1, 1, 1, 0, 704, 98
43452, V, 1, 1, 1, 1, 0, 704, 99
43453, V, 1, 1, 1, 1, 0, 704, 98
43454, V, 1, 1, 1, 1, 0, 704, 99
43455, V, 1, 1, 1, 1, 0, 704, 98
43456, V, 1, 1, 1, 1, 0, 704, 98
43457, V, 1, 1, 1, 1, 0, 704, 98
43458, V, 1, 1, 1, 1, 0, 704, 98
43459, V, 1, 1, 1, 1, 0, 704, 99
43460, V, 1, 1, 1, 1, 0, 704, 98
43461, V, 1, 1, 1, 1, 0, 704, 99
43462, V, 1, 1, 1, 1, 0, 704, 98
43463, V, 1, 1, 1, 1, 0, 704, 99
43464, V, 1, 1, 1, 1, 0, 704, 99
43465, V, 1, 1, 1, 1, 0, 704, 99
43466, V, 1, 1, 1, 1, 0, 704, 99
43467, V, 1, 1, 1, 1, 0, 704, 99
43468, V, 1, 1, 1, 1, 0, 704, 99
43469, V, 1, 1, 1, 1, 0, 704, 99
43470, V, 1, 1, 1, 1, 0, 704, 99
43471, V, 1, 1, 1, 1, 0, 704, 99
43472, V, 1, 1, 1, 1, 0, 704, 99
43473, V, 1, 1, 1, 1, 0, 704, 99
43474, V, 1, 1, 1, 1, 0, 704, 99
43475, V, 1, 1, 1, 1, 0, 704, 99
43476, V, 1, 1, 1, 1, 0, 704, 99
43478, V, 1, 1, 1, 1, 0, 704, 99
43479, V, 1, 1, 1, 1, 0, 704, 98
43480, V, 1, 1, 1, 1, 0, 704, 99
43481, V, 1, 1, 1, 1, 0, 704, 98
43482, V, 1, 1, 1, 1, 0, 704, 99
43483, V, 1, 1, 1, 1, 0, 704, 99
43484, V, 1, 1, 1, 1, 0, 704, 99
43485, V, 1, 1, 1, 1, 0, 704, 99
43486, V, 1, 1, 1, 1, 0, 704, 99
43487, V, 1, 1, 1, 1, 0, 704, 99
43488, V, 1, 1, 1, 1, 0, 704, 99
43489, V, 1, 1, 1, 1, 0, 704, 99
43490, V, 1, 1, 1, 1, 0, 704, 99
43491, V, 1, 1, 1, 1, 0, 704, 99
43492, V, 1, 1, 1, 1, 0, 704, 98
43493, V, 1, 1, 1, 1, 0, 704, 98
43494, V, 1, 1, 1, 1, 0, 704, 99
43495, V, 1, 1, 1, 1, 0, 704, 99
43496, V, 1, 1, 1, 1, 0, 704, 98
43497, V, 1, 1, 1, 1, 0, 704, 99
43498, V, 1, 1, 1, 1, 0, 704, 99
43499, V, 1, 1, 1, 1, 0, 704, 99
43500, V, 1, 1, 1, 1, 0, 704, 99
43501, V, 1, 1, 1, 1, 0, 704, 98
43502, V, 1, 1, 1, 1, 0, 704, 98
43503, V, 1, 1, 1, 1, 0, 704, 99
43504, V, 1, 1, 1, 1, 0, 704, 99
43505, V, 1, 1, 1, 1, 0, 704, 99
43506, V, 1, 1, 1, 1, 0, 704, 98
43507, V, 1, 1, 1, 1, 0, 704, 99
43508, V, 1, 1, 1, 1, 0, 704, 98
43509, V, 1, 1, 1, 1, 0, 704, 99
43510, V, 1, 1, 1, 1, 0, 704, 98
43511, V, 1, 1, 1, 1, 0, 704, 98
43512, V, 1, 1, 1, 1, 0, 704, 99
43513, V, 1, 1, 1, 1, 0, 704, 98
43514, V, 1, 1, 1, 1, 0, 704, 98
43515, V, 1, 1, 1, 1, 0, 704, 98
43516, V, 1, 1, 1, 1, 0, 704, 98
43517, V, 1, 1, 1, 1, 0, 704, 98
43518, V, 1, 1, 1, 1, 0, 704, 99
43520, V, 1, 1, 1, 1, 0, 704, 98
43521, V, 1, 1, 1, 1, 0, 704, 98
43522, V, 1, 1, 1, 1, 0, 704, 98
43523, V, 1, 1, 1, 1, 0, 704, 98
43524, V, 1, 1, 1, 1, 0, 704, 98
43525, V, 1, 1, 1, 1, 0, 704, 99
43526, V, 1, 1, 1, 1, 0, 704, 98
43527, V, 1, 1, 1, 1, 0, 704, 98
43528, V, 1, 1, 1, 1, 0, 704, 99
43529, V, 1, 1, 1, 1, 0, 704, 98
43530, V, 1, 1, 1, 1, 0, 704, 98
43531, V, 1, 1, 1, 1, 0, 704, 99
43532, V, 1, 1, 1, 1, 0, 704, 99
43533, V, 1, 1, 1, 1, 0, 704, 99
43534, V, 1, 1, 1, 1, 0, 704, 99
43535, V, 1, 1, 1, 1, 0, 704, 98
43536, V, 1, 1, 1, 1, 0, 704, 98
43537, V, 1, 1, 1, 1, 0, 704, 98
43538, V, 1, 1, 1, 1, 0, 704, 99
43539, V, 1, 1, 1, 1, 0, 704, 99
43540, V, 1, 1, 1, 1, 0, 704, 99
43541, V, 1, 1, 1, 1, 0, 704, 99
43542, V, 1, 1, 1, 1, 0, 704, 99
43543, V, 1, 1, 1, 1, 0, 704, 99
43544, V, 1, 1, 1, 1, 0, 704, 99
43545, V, 1, 1, 1, 1, 0, 704, 99
43546, V, 1, 1, 1, 1, 0, 704, 99
43547, V, 1, 1, 1, 1, 0, 704, 99
43548, V, 1, 1, 1, 1, 0, 704, 99
43549, V, 1, 1, 1, 1, 0, 704, 99
43550, V, 1, 1, 1, 1, 0, 704, 99
43551, V, 1, 1, 1, 1, 0, 704, 99
43552, V, 1, 1, 1, 1, 0, 704, 99
43553, V, 1, 1, 1, 1, 0, 704, 99
43554, V, 1, 1, 1, 1, 0, 704, 99
43555, V, 1, 1, 1, 1, 0, 704, 99
43556, V, 1, 1, 1, 1, 0, 704, 99
43557, V, 1, 1, 1, 1, 0, 704, 99
43558, V, 1, 1, 1, 1, 0, 704, 99
43559, V, 1, 1, 1, 1, 0, 704, 99
43560, V, 1, 1, 1, 1, 0, 704, 99
43561, V, 1, 1, 1, 1, 0, 704, 99
43563, V, 1, 1, 1, 1, 0, 704, 99
43564, V, 1, 1, 1, 1, 0, 704, 99
43565, V, 1, 1, 1, 1, 0, 704, 99
43566, V, 1, 1, 1, 1, 0, 704, 99
43567, V, 1, 1, 1, 1, 0, 704, 99
43568, V, 1, 1, 1, 1, 0, 704, 99
43569, V, 1, 1, 1, 1, 0, 704, 99
43570, V, 1, 1, 1, 1, 0, 704, 99
43571, V, 1, 1, 1, 1, 0, 704, 99
43572, V, 1, 1, 1, 1, 0, 704, 99
43573, V, 1, 1, 1, 1, 0, 704, 99
43574, V, 1, 1, 1, 1, 0, 704, 99
43575, V, 1, 1, 1, 1, 0, 704, 99
43576, V, 1, 1, 1, 1, 0, 704, 99
43577, V, 1, 1, 1, 1, 0, 704, 99
43578, V, 1, 1, 1, 1, 0, 704, 99
43579, V, 1, 1, 1, 1, 0, 704, 99
43580, V, 1, 1, 1, 1, 0, 704, 99
43581, V, 1, 1, 1, 1, 0, 704, 99
43582, V, 1, 1, 1, 1, 0, 704, 99
43583, V, 1, 1, 1, 1, 0, 704, 99
43584, V, 1, 1, 1, 1, 0, 704, 98
43585, V, 1, 1, 1, 1, 0, 704, 99
43586, V, 1, 1, 1, 1, 0, 704, 99
43587, V, 1, 1, 1, 1, 0, 704, 99
43588, V, 1, 1, 1, 1, 0, 704, 99
43589, V, 1, 1, 1, 1, 0, 704, 98
43590, V, 1, 1, 1, 1, 0, 704, 98
43591, V, 1, 1, 1, 1, 0, 704, 98
43592, V, 1, 1, 1, 1, 0, 704, 98
43593, V, 1, 1, 1, 1, 0, 704, 98
43594, V, 1, 1, 1, 1, 0, 704, 98
43595, V, 1, 1, 1, 1, 0, 704, 98
43596, V, 1, 1, 1, 1, 0, 704, 98
43597, V, 1, 1, 1, 1, 0, 704, 98
43598, V, 1, 1, 1, 1, 0, 704, 98
43599, V, 1, 1, 1, 1, 0, 704, 98
43600, V, 1, 1, 1, 1, 0, 704, 98
43601, V, 1, 1, 1, 1, 0, 704, 98
43602, V, 1, 1, 1, 1, 0, 704, 98
43603, V, 1, 1, 1, 1, 0, 704, 98
43604, V, 1, 1, 1, 1, 0, 704, 98
43606, V, 1, 1, 1, 1, 0, 704, 98
43607, V, 1, 1, 1, 1, 0, 704, 98
43608, V, 1, 1, 1, 1, 0, 704, 98
43609, V, 1, 1, 1, 1, 0, 704, 98
43610, V, 1, 1, 1, 1, 0, 704, 98
43611, V, 1, 1, 1, 1, 0, 704, 98
43612, V, 1, 1, 1, 1, 0, 704, 98
43613, V, 1, 1, 1, 1, 0, 704, 98
43614, V, 1, 1, 1, 1, 0, 704, 98
43615, V, 1, 1, 1, 1, 0, 704, 98
43616, V, 1, 1, 1, 1, 0, 704, 98
43617, V, 1, 1, 1, 1, 0, 704, 98
43618, V, 1, 1, 1, 1, 0, 704, 98
43619, V, 1, 1, 1, 1, 0, 704, 99
43620, V, 1, 1, 1, 1, 0, 704, 98
43621, V, 1, 1, 1, 1, 0, 704, 99
43622, V, 1, 1, 1, 1, 0, 704, 99
43623, V, 1, 1, 1, 1, 0, 704, 99
43624, V, 1, 1, 1, 1, 0, 704, 99
43625, V, 1, 1, 1, 1, 0, 704, 99
43626, V, 1, 1, 1, 1, 0, 704, 99
43627, V, 1, 1, 1, 1, 0, 704, 99
43628, V, 1, 1, 1, 1, 0, 704, 99
43629, V, 1, 1, 1, 1, 0, 704, 99
43630, V, 1, 1, 1, 1, 0, 704, 99
43631, V, 1, 1, 1, 1, 0, 704, 99
43632, V, 1, 1, 1, 1, 0, 704, 98
43633, V, 1, 1, 1, 1, 0, 704, 98
43634, V, 1, 1, 1, 1, 0, 704, 99
43635, V, 1, 1, 1, 1, 0, 704, 99
43636, V, 1, 1, 1, 1, 0, 704, 99
43637, V, 1, 1, 1, 1, 0, 704, 99
43638, V, 1, 1, 1, 1, 0, 704, 99
43639, V, 1, 1, 1, 1, 0, 704, 99
43640, V, 1, 1, 1, 1, 0, 704, 99
43641, V, 1, 1, 1, 1, 0, 704, 99
43642, V, 1, 1, 1, 1, 0, 704, 98
43643, V, 1, 1, 1, 1, 0, 704, 99
43644, V, 1, 1, 1, 1, 0, 704, 99
43645, V, 1, 1, 1, 1, 0, 704, 98
43646, V, 1, 1, 1, 1, 0, 704, 99
43648, V, 1, 1, 1, 1, 0, 704, 99
43649, V, 1, 1, 1, 1, 0, 704, 99
43650, V, 1, 1, 1, 1, 0, 704, 98
43651, V, 1, 1, 1, 1, 0, 704, 98
43652, V, 1, 1, 1, 1, 0, 704, 99
43653, V, 1, 1, 1, 1, 0, 704, 98
43654, V, 1, 1, 1, 1, 0, 704, 98
43655, V, 1, 1, 1, 1, 0, 704, 98
43656, V, 1, 1, 1, 1, 0, 704, 98
43657, V, 1, 1, 1, 1, 0, 704, 98
43658, V, 1, 1, 1, 1, 0, 704, 98
43659, V, 1, 1, 1, 1, 0, 704, 98
43660, V, 1, 1, 1, 1, 0, 704, 98
43661, V, 1, 1, 1, 1, 0, 704, 98
43662, V, 1, 1, 1, 1, 0, 704, 98
43663, V, 1, 1, 1, 1, 0, 704, 98
43664, V, 1, 1, 1, 1, 0, 704, 98
43665, V, 1, 1, 1, 1, 0, 704, 98
43666, V, 1, 1, 1, 1, 0, 704, 98
43667, V, 1, 1, 1, 1, 0, 704, 98
43668, V, 1, 1, 1, 1, 0, 704, 98
43669, V, 1, 1, 1, 1, 0, 704, 98
43670, V, 1, 1, 1, 1, 0, 704, 98
43671, V, 1, 1, 1, 1, 0, 704, 98
43672, V, 1, 1, 1, 1, 0, 704, 98
43673, V, 1, 1, 1, 1, 0, 704, 98
43674, V, 1, 1, 1, 1, 0, 704, 98
43675, V, 1, 1, 1, 1, 0, 704, 98
43676, V, 1, 1, 1, 1, 0, 704, 98
43677, V, 1, 1, 1, 1, 0, 704, 98
43678, V, 1, 1, 1, 1, 0, 704, 98
43679, V, 1, 1, 1, 1, 0, 704, 98
43680, V, 1, 1, 1, 1, 0, 704, 98
43681, V, 1, 1, 1, 1, 0, 704, 98
43682, V, 1, 1, 1, 1, 0, 704, 98
43683, V, 1, 1, 1, 1, 0, 704, 98
43684, V, 1, 1, 1, 1, 0, 704, 98
43685, V, 1, 1, 1, 1, 0, 704, 99
43686, V, 1, 1, 1, 1, 0, 704, 99
43687, V, 1, 1, 1, 1, 0, 704, 98
43688, V, 1, 1, 1, 1, 0, 704, 98
43689, V, 1, 1, 1, 1, 0, 704, 99
43691, V, 1, 1, 1, 1, 0, 704, 98
43692, V, 1, 1, 1, 1, 0, 704, 99
43693, V, 1, 1, 1, 1, 0, 704, 98
43694, V, 1, 1, 1, 1, 0, 704, 98
43695, V, 1, 1, 1, 1, 0, 704, 99
43696, V, 1, 1, 1, 1, 0, 704, 99
43697, V, 1, 1, 1, 1, 0, 704, 99
43698, V, 1, 1, 1, 1, 0, 704, 99
43699, V, 1, 1, 1, 1, 0, 704, 99
43700, V, 1, 1, 1, 1, 0, 704, 99
43701, V, 1, 1, 1, 1, 0, 704, 99
43702, V, 1, 1, 1, 1, 0, 704, 99
43703, V, 1, 1, 1, 1, 0, 704, 99
43704, V, 1, 1, 1, 1, 0, 704, 99
43705, V, 1, 1, 1, 1, 0, 704, 99
43706, V, 1, 1, 1, 1, 0, 704, 99
43707, V, 1, 1, 1, 1, 0, 704, 99
43708, V, 1, 1, 1, 1, 0, 704, 99
43709, V, 1, 1, 1, 1, 0, 704, 99
43710, V, 1, 1, 1, 1, 0, 704, 99
43711, V, 1, 1, 1, 1, 0, 704, 99
43712, V, 1, 1, 1, 1, 0, 704, 99
43713, V, 1, 1, 1, 1, 0, 704, 99
43714, V, 1, 1, 1, 1, 0, 704, 99
43715, V, 1, 1, 1, 1, 0, 704, 99
43716, V, 1, 1, 1, 1, 0, 704, 99
43717, V, 1, 1, 1, 1, 0, 704, 99
43718, V, 1, 1, 1, 1, 0, 704, 99
43719, V, 1, 1, 1, 1, 0, 704, 99
43720, V, 1, 1, 1, 1, 0, 704, 99
43721, V, 1, 1, 1, 1, 0, 704, 99
43722, V, 1, 1, 1, 1, 0, 704, 99
43723, V, 1, 1, 1, 1, 0, 704, 99
43724, V, 1, 1, 1, 1, 0, 704, 99
43725, V, 1, 1, 1, 1, 0, 704, 99
43726, V, 1, 1, 1, 1, 0, 704, 99
43727, V, 1, 1, 1, 1, 0, 704, 99
43728, V, 1, 1, 1, 1, 0, 704, 99
43729, V, 1, 1, 1, 1, 0, 704, 99
43730, V, 1, 1, 1, 1, 0, 704, 99
43731, V, 1, 1, 1, 1, 0, 704, 99
43732, V, 1, 1, 1, 1, 0, 704, 99
43734, V, 1, 1, 1, 1, 0, 704, 99
43735, V, 1, 1, 1, 1, 0, 704, 99
43736, V, 1, 1, 1, 1, 0, 704, 99
43737, V, 1, 1, 1, 1, 0, 704, 98
43738, V, 1, 1, 1, 1, 0, 704, 99
43739, V, 1, 1, 1, 1, 0, 704, 98
43740, V, 1, 1, 1, 1, 0, 704, 98
43741, V, 1, 1, 1, 1, 0, 704, 98
43742, V, 1, 1, 1, 1, 0, 704, 99
43743, V, 1, 1, 1, 1, 0, 704, 98
43744, V, 1, 1, 1, 1, 0, 704, 98
43745, V, 1, 1, 1, 1, 0, 704, 98
43746, V, 1, 1, 1, 1, 0, 704, 99
43747, V, 1, 1, 1, 1, 0, 704, 98
43748, V, 1, 1, 1, 1, 0, 704, 98
43749, V, 1, 1, 1, 1, 0, 704, 98
43750, V, 1, 1, 1, 1, 0, 704, 98
43751, V, 1, 1, 1, 1, 0, 704, 98
43752, V, 1, 1, 1, 1, 0, 704, 98
43753, V, 1, 1, 1, 1, 0, 704, 98
43754, V, 1, 1, 1, 1, 0, 704, 98
43755, V, 1, 1, 1, 1, 0, 704, 98
43756, V, 1, 1, 1, 1, 0, 704, 98
43757, V, 1, 1, 1, 1, 0, 704, 98
43758, V, 1, 1, 1, 1, 0, 704, 98
43759, V, 1, 1, 1, 1, 0, 704, 98
43760, V, 1, 1, 1, 1, 0, 704, 98
43761, V, 1, 1, 1, 1, 0, 704, 98
43762, V, 1, 1, 1, 1, 0, 704, 98
43763, V, 1, 1, 1, 1, 0, 704, 98
43764, V, 1, 1, 1, 1, 0, 704, 98
43765, V, 1, 1, 1, 1, 0, 704, 98
43766, V, 1, 1, 1, 1, 0, 704, 98
43767, V, 1, 1, 1, 1, 0, 704, 98
43768, V, 1, 1, 1, 1, 0, 704, 99
43769, V, 1, 1, 1, 1, 0, 704, 98
43770, V, 1, 1, 1, 1, 0, 704, 99
43771, V, 1, 1, 1, 1, 0, 704, 99
43772, V, 1, 1, 1, 1, 0, 704, 98
43773, V, 1, 1, 1, 1, 0, 704, 98
43774, V, 1, 1, 1, 1, 0, 704, 99
43776, V, 1, 1, 1, 1, 0, 704, 99
43777, V, 1, 1, 1, 1, 0, 704, 99
43778, V, 1, 1, 1, 1, 0, 704, 99
43779, V, 1, 1, 1, 1, 0, 704, 99
43780, V, 1, 1, 1, 1, 0, 704, 99
43781, V, 1, 1, 1, 1, 0, 704, 99
43782, V, 1, 1, 1, 1, 0, 704, 99
43783, V, 1, 1, 1, 1, 0, 704, 99
43784, V, 1, 1, 1, 1, 0, 704, 98
43785, V, 1, 1, 1, 1, 0, 704, 98
43786, V, 1, 1, 1, 1, 0, 704, 99
43787, V, 1, 1, 1, 1, 0, 704, 98
43788, V, 1, 1, 1, 1, 0, 704, 99
43789, V, 1, 1, 1, 1, 0, 704, 99
43790, V, 1, 1, 1, 1, 0, 704, 98
43791, V, 1, 1, 1, 1, 0, 704, 98
43792, V, 1, 1, 1, 1, 0, 704, 98
43793, V, 1, 1, 1, 1, 0, 704, 99
43794, V, 1, 1, 1, 1, 0, 704, 98
43795, V, 1, 1, 1, 1, 0, 704, 98
43796, V, 1, 1, 1, 1, 0, 704, 99
43797, V, 1, 1, 1, 1, 0, 704, 99
43798, V, 1, 1, 1, 1, 0, 704, 99
43799, V, 1, 1, 1, 1, 0, 704, 98
43800, V, 1, 1, 1, 1, 0, 704, 98
43801, V, 1, 1, 1, 1, 0, 704, 98
43802, V, 1, 1, 1, 1, 0, 704, 98
43803, V, 1, 1, 1, 1, 0, 704, 98
43804, V, 1, 1, 1, 1, 0, 704, 99
43805, V, 1, 1, 1, 1, 0, 704, 98
43806, V, 1, 1, 1, 1, 0, 704, 98
43807, V, 1, 1, 1, 1, 0, 704, 98
43808, V, 1, 1, 1, 1, 0, 704, 98
43809, V, 1, 1, 1, 1, 0, 704, 98
43810, V, 1, 1, 1, 1, 0, 704, 98
43811, V, 1, 1, 1, 1, 0, 704, 98
43812, V, 1, 1, 1, 1, 0, 704, 98
43813, V, 1, 1, 1, 1, 0, 704, 98
43814, V, 1, 1, 1, 1, 0, 704, 98
43815, V, 1, 1, 1, 1, 0, 704, 98
43816, V, 1, 1, 1, 1, 0, 704, 98
43817, V, 1, 1, 1, 1, 0, 704, 98
43819, V, 1, 1, 1, 1, 0, 704, 98
43820, V, 1, 1, 1, 1, 0, 704, 98
43821, V, 1, 1, 1, 1, 0, 704, 98
43822, V, 1, 1, 1, 1, 0, 704, 98
43823, V, 1, 1, 1, 1, 0, 704, 98
43824, V, 1, 1, 1, 1, 0, 704, 98
43825, V, 1, 1, 1, 1, 0, 704, 98
43826, V, 1, 1, 1, 1, 0, 704, 98
43827, V, 1, 1, 1, 1, 0, 704, 98
43828, V, 1, 1, 1, 1, 0, 704, 98
43829, V, 1, 1, 1, 1, 0, 704, 98
43830, V, 1, 1, 1, 1, 0, 704, 98
43831, V, 1, 1, 1, 1, 0, 704, 98
43832, V, 1, 1, 1, 1, 0, 704, 98
43833, V, 1, 1, 1, 1, 0, 704, 98
43834, V, 1, 1, 1, 1, 0, 704, 98
43835, V, 1, 1, 1, 1, 0, 704, 98
43836, V, 1, 1, 1, 1, 0, 704, 99
43837, V, 1, 1, 1, 1, 0, 704, 98
43838, V, 1, 1, 1, 1, 0, 704, 98
43839, V, 1, 1, 1, 1, 0, 704, 99
43840, V, 1, 1, 1, 1, 0, 704, 99
43841, V, 1, 1, 1, 1, 0, 704, 99
43842, V, 1, 1, 1, 1, 0, 704, 98
43843, V, 1, 1, 1, 1, 0, 704, 98
43844, V, 1, 1, 1, 1, 0, 704, 99
43845, V, 1, 1, 1, 1, 0, 704, 99
43846, V, 1, 1, 1, 1, 0, 704, 99
43847, V, 1, 1, 1, 1, 0, 704, 98
43848, V, 1, 1, 1, 1, 0, 704, 98
43849, V, 1, 1, 1, 1, 0, 704, 99
43850, V, 1, 1, 1, 1, 0, 704, 98
43851, V, 1, 1, 1, 1, 0, 704, 99
43852, V, 1, 1, 1, 1, 0, 704, 99
43853, V, 1, 1, 1, 1, 0, 704, 99
43854, V, 1, 1, 1, 1, 0, 704, 99
43855, V, 1, 1, 1, 1, 0, 704, 99
43856, V, 1, 1, 1, 1, 0, 704, 99
43857, V, 1, 1, 1, 1, 0, 704, 99
43858, V, 1, 1, 1, 1, 0, 704, 99
43859, V, 1, 1, 1, 1, 0, 704, 99
43860, V, 1, 1, 1, 1, 0, 704, 99
43862, V, 1, 1, 1, 1, 0, 704, 99
43863, V, 1, 1, 1, 1, 0, 704, 99
43864, V, 1, 1, 1, 1, 0, 704, 99
43865, V, 1, 1, 1, 1, 0, 704, 99
43866, V, 1, 1, 1, 1, 0, 704, 99
43867, V, 1, 1, 1, 1, 0, 704, 99
43868, V, 1, 1, 1, 1, 0, 704, 99
43869, V, 1, 1, 1, 1, 0, 704, 99
43870, V, 1, 1, 1, 1, 0, 704, 99
43871, V, 1, 1, 1, 1, 0, 704, 99
43872, V, 1, 1, 1, 1, 0, 704, 99
43873, V, 1, 1, 1, 1, 0, 704, 99
43874, V, 1, 1, 1, 1, 0, 704, 99
43875, V, 1, 1, 1, 1, 0, 704, 99
43876, V, 1, 1, 1, 1, 0, 704, 98
43877, V, 1, 1, 1, 1, 0, 704, 99
43878, V, 1, 1, 1, 1, 0, 704, 99
43879, V, 1, 1, 1, 1, 0, 704, 99
43880, V, 1, 1, 1, 1, 0, 704, 99
43881, V, 1, 1, 1, 1, 0, 704, 99
43882, V, 1, 1, 1, 1, 0, 704, 98
43883, V, 1, 1, 1, 1, 0, 704, 99
43884, V, 1, 1, 1, 1, 0, 704, 99
43885, V, 1, 1, 1, 1, 0, 704, 99
43886, V, 1, 1, 1, 1, 0, 704, 99
43887, V, 1, 1, 1, 1, 0, 704, 99
43888, V, 1, 1, 1, 1, 0, 704, 98
43889, V, 1, 1, 1, 1, 0, 704, 99
43890, V, 1, 1, 1, 1, 0, 704, 98
43891, V, 1, 1, 1, 1, 0, 704, 98
43892, V, 1, 1, 1, 1, 0, 704, 98
43893, V, 1, 1, 1, 1, 0, 704, 98
43894, V, 1, 1, 1, 1, 0, 704, 98
43895, V, 1, 1, 1, 1, 0, 704, 98
43896, V, 1, 1, 1, 1, 0, 704, 98
43897, V, 1, 1, 1, 1, 0, 704, 98
43898, V, 1, 1, 1, 1, 0, 704, 98
43899, V, 1, 1, 1, 1, 0, 704, 98
43900, V, 1, 1, 1, 1, 0, 704, 98
43901, V, 1, 1, 1, 1, 0, 704, 98
43902, V, 1, 1, 1, 1, 0, 704, 98
43904, V, 1, 1, 1, 1, 0, 704, 98
43905, V, 1, 1, 1, 1, 0, 704, 99
43906, V, 1, 1, 1, 1, 0, 704, 98
43907, V, 1, 1, 1, 1, 0, 704, 98
43908, V, 1, 1, 1, 1, 0, 704, 98
43909, V, 1, 1, 1, 1, 0, 704, 98
43910, V, 1, 1, 1, 1, 0, 704, 98
43911, V, 1, 1, 1, 1, 0, 704, 98
43912, V, 1, 1, 1, 1, 0, 704, 98
43913, V, 1, 1, 1, 1, 0, 704, 98
43914, V, 1, 1, 1, 1, 0, 704, 98
43915, V, 1, 1, 1, 1, 0, 704, 98
43916, V, 1, 1, 1, 1, 0, 704, 98
43917, V, 1, 1, 1, 1, 0, 704, 98
43918, V, 1, 1, 1, 1, 0, 704, 98
43919, V, 1, 1, 1, 1, 0, 704, 98
43920, V, 1, 1, 1, 1, 0, 704, 98
43921, V, 1, 1, 1, 1, 0, 704, 98
43922, V, 1, 1, 1, 1, 0, 704, 99
43923, V, 1, 1, 1, 1, 0, 704, 98
43924, V, 1, 1, 1, 1, 0, 704, 98
43925, V, 1, 1, 1, 1, 0, 704, 99
43926, V, 1, 1, 1, 1, 0, 704, 99
43927, V, 1, 1, 1, 1, 0, 704, 99
43928, V, 1, 1, 1, 1, 0, 704, 99
43929, V, 1, 1, 1, 1, 0, 704, 99
43930, V, 1, 1, 1, 1, 0, 704, 99
43931, V, 1, 1, 1, 1, 0, 704, 99
43932, V, 1, 1, 1, 1, 0, 704, 99
43933, V, 1, 1, 1, 1, 0, 704, 99
43934, V, 1, 1, 1, 1, 0, 704, 99
43935, V, 1, 1, 1, 1, 0, 704, 99
43936, V, 1, 1, 1, 1, 0, 704, 99
43937, V, 1, 1, 1, 1, 0, 704, 99
43938, V, 1, 1, 1, 1, 0, 704, 99
43939, V, 1, 1, 1, 1, 0, 704, 99
43940, V, 1, 1, 1, 1, 0, 704, 99
43941, V, 1, 1, 1, 1, 0, 704, 99
43942, V, 1, 1, 1, 1, 0, 704, 99
43943, V, 1, 1, 1, 1, 0, 704, 99
43944, V, 1, 1, 1, 1, 0, 704, 99
43945, V, 1, 1, 1, 1, 0, 704, 99
43947, V, 1, 1, 1, 1, 0, 704, 99
43948, V, 1, 1, 1, 1, 0, 704, 99
43949, V, 1, 1, 1, 1, 0, 704, 99
43950, V, 1, 1, 1, 1, 0, 704, 99
43951, V, 1, 1, 1, 1, 0, 704, 99
43952, V, 1, 1, 1, 1, 0, 704, 99
43953, V, 1, 1, 1, 1, 0, 704, 99
43954, V, 1, 1, 1, 1, 0, 704, 99
43955, V, 1, 1, 1, 1, 0, 704, 99
43956, V, 1, 1, 1, 1, 0, 704, 98
43957, V, 1, 1, 1, 1, 0, 704, 98
43958, V, 1, 1, 1, 1, 0, 704, 99
43959, V, 1, 1, 1, 1, 0, 704, 99
43960, V, 1, 1, 1, 1, 0, 704, 99
43961, V, 1, 1, 1, 1, 0, 704, 99
43962, V, 1, 1, 1, 1, 0, 704, 99
43963, V, 1, 1, 1, 1, 0, 704, 99
43964, V, 1, 1, 1, 1, 0, 704, 99
43965, V, 1, 1, 1, 1, 0, 704, 99
43966, V, 1, 1, 1, 1, 0, 704, 98
43967, V, 1, 1, 1, 1, 0, 704, 98
43968, V, 1, 1, 1, 1, 0, 704, 99
43969, V, 1, 1, 1, 1, 0, 704, 98
43970, V, 1, 1, 1, 1, 0, 704, 98
43971, V, 1, 1, 1, 1, 0, 704, 98
43972, V, 1, 1, 1, 1, 0, 704, 98
43973, V, 1, 1, 1, 1, 0, 704, 98
43974, V, 1, 1, 1, 1, 0, 704, 98
43975, V, 1, 1, 1, 1, 0, 704, 98
43976, V, 1, 1, 1, 1, 0, 704, 98
43977, V, 1, 1, 1, 1, 0, 704, 98
43978, V, 1, 1, 1, 1, 0, 704, 98
43979, V, 1, 1, 1, 1, 0, 704, 98
43980, V, 1, 1, 1, 1, 0, 704, 98
43981, V, 1, 1, 1, 1, 0, 704, 98
43982, V, 1, 1, 1, 1, 0, 704, 98
43983, V, 1, 1, 1, 1, 0, 704, 99
43984, V, 1, 1, 1, 1, 0, 704, 98
43985, V, 1, 1, 1, 1, 0, 704, 99
43986, V, 1, 1, 1, 1, 0, 704, 99
43987, V, 1, 1, 1, 1, 0, 704, 98
43988, V, 1, 1, 1, 1, 0, 704, 98
43990, V, 1, 1, 1, 1, 0, 704, 98
43991, V, 1, 1, 1, 1, 0, 704, 98
43992, V, 1, 1, 1, 1, 0, 704, 98
43993, V, 1, 1, 1, 1, 0, 704, 98
43994, V, 1, 1, 1, 1, 0, 704, 98
43995, V, 1, 1, 1, 1, 0, 704, 98
43996, V, 1, 1, 1, 1, 0, 704, 98
43997, V, 1, 1, 1, 1, 0, 704, 98
43998, V, 1, 1, 1, 1, 0, 704, 99
43999, V, 1, 1, 1, 1, 0, 704, 98
44000, V, 1, 1, 1, 1, 0, 704, 98
44001, V, 1, 1, 1, 1, 0, 704, 98
44002, V, 1, 1, 1, 1, 0, 704, 99
44003, V, 1, 1, 1, 1, 0, 704, 99
44004, V, 1, 1, 1, 1, 0, 704, 99
44005, V, 1, 1, 1, 1, 0, 704, 99
44006, V, 1, 1, 1, 1, 0, 704, 99
44007, V, 1, 1, 1, 1, 0, 704, 99
44008, V, 1, 1, 1, 1, 0, 704, 99
44009, V, 1, 1, 1, 1, 0, 704, 99
44010, V, 1, 1, 1, 1, 0, 704, 98
44011, V, 1, 1, 1, 1, 0, 704, 98
44012, V, 1, 1, 1, 1, 0, 704, 98
44013, V, 1, 1, 1, 1, 0, 704, 99
44014, V, 1, 1, 1, 1, 0, 704, 99
44015, V, 1, 1, 1, 1, 0, 704, 99
44016, V, 1, 1, 1, 1, 0, 704, 99
44017, V, 1, 1, 1, 1, 0, 704, 99
44018, V, 1, 1, 1, 1, 0, 704, 99
44019, V, 1, 1, 1, 1, 0, 704, 98
44020, V, 1, 1, 1, 1, 0, 704, 98
44021, V, 1, 1, 1, 1, 0, 704, 99
44022, V, 1, 1, 1, 1, 0, 704, 98
44023, V, 1, 1, 1, 1, 0, 704, 99
44024, V, 1, 1, 1, 1, 0, 704, 99
44025, V, 1, 1, 1, 1, 0, 704, 99
44026, V, 1, 1, 1, 1, 0, 704, 99
44027, V, 1, 1, 1, 1, 0, 704, 98
44028, V, 1, 1, 1, 1, 0, 704, 99
44029, V, 1, 1, 1, 1, 0, 704, 98
44030, V, 1, 1, 1, 1, 0, 704, 98
44032, V, 1, 1, 1, 1, 0, 704, 98
44033, V, 1, 1, 1, 1, 0, 704, 99
44034, V, 1, 1, 1, 1, 0, 704, 98
44035, V, 1, 1, 1, 1, 0, 704, 98
44036, V, 1, 1, 1, 1, 0, 704, 98
44037, V, 1, 1, 1, 1, 0, 704, 98
44038, V, 1, 1, 1, 1, 0, 704, 98
44039, V, 1, 1, 1, 1, 0, 704, 98
44040, V, 1, 1, 1, 1, 0, 704, 98
44041, V, 1, 1, 1, 1, 0, 704, 98
44042, V, 1, 1, 1, 1, 0, 704, 98
44043, V, 1, 1, 1, 1, 0, 704, 98
44044, V, 1, 1, 1, 1, 0, 704, 98
44045, V, 1, 1, 1, 1, 0, 704, 98
44046, V, 1, 1, 1, 1, 0, 704, 98
44047, V, 1, 1, 1, 1, 0, 704, 98
44048, V, 1, 1, 1, 1, 0, 704, 98
44049, V, 1, 1, 1, 1, 0, 704, 98
44050, V, 1, 1, 1, 1, 0, 704, 98
44051, V, 1, 1, 1, 1, 0, 704, 98
44052, V, 1, 1, 1, 1, 0, 704, 98
44053, V, 1, 1, 1, 1, 0, 704, 98
44054, V, 1, 1, 1, 1, 0, 704, 98
44055, V, 1, 1, 1, 1, 0, 704, 98
44056, V, 1, 1, 1, 1, 0, 704, 98
44057, V, 1, 1, 1, 1, 0, 704, 98
44058, V, 1, 1, 1, 1, 0, 704, 98
44059, V, 1, 1, 1, 1, 0, 704, 98
44060, V, 1, 1, 1, 1, 0, 704, 98
44061, V, 1, 1, 1, 1, 0, 704, 98
44062, V, 1, 1, 1, 1, 0, 704, 98
44063, V, 1, 1, 1, 1, 0, 704, 98
44064, V, 1, 1, 1, 1, 0, 704, 98
44065, V, 1, 1, 1, 1, 0, 704, 98
44066, V, 1, 1, 1, 1, 0, 704, 98
44067, V, 1, 1, 1, 1, 0, 704, 98
44068, V, 1, 1, 1, 1, 0, 704, 98
44069, V, 1, 1, 1, 1, 0, 704, 98
44070, V, 1, 1, 1, 1, 0, 704, 98
44071, V, 1, 1, 1, 1, 0, 704, 98
44072, V, 1, 1, 1, 1, 0, 704, 98
44073, V, 1, 1, 1, 1, 0, 704, 98
44075, V, 1, 1, 1, 1, 0, 704, 98
44076, V, 1, 1, 1, 1, 0, 704, 98
44077, V, 1, 1, 1, 1, 0, 704, 98
44078, V, 1, 1, 1, 1, 0, 704, 98
44079, V, 1, 1, 1, 1, 0, 704, 99
44080, V, 1, 1, 1, 1, 0, 704, 98
44081, V, 1, 1, 1, 1, 0, 704, 99
44082, V, 1, 1, 1, 1, 0, 704, 98
44083, V, 1, 1, 1, 1, 0, 704, 98
44084, V, 1, 1, 1, 1, 0, 704, 99
44085, V, 1, 1, 1, 1, 0, 704, 98
44086, V, 1, 1, 1, 1, 0, 704, 99
44087, V, 1, 1, 1, 1, 0, 704, 99
44088, V, 1, 1, 1, 1, 0, 704, 98
44089, V, 1, 1, 1, 1, 0, 704, 98
44090, V, 1, 1, 1, 1, 0, 704, 98
44091, V, 1, 1, 1, 1, 0, 704, 98
44092, V, 1, 1, 1, 1, 0, 704, 99
44093, V, 1, 1, 1, 1, 0, 704, 98
44094, V, 1, 1, 1, 1, 0, 704, 98
44095, V, 1, 1, 1, 1, 0, 704, 98
44096, V, 1, 1, 1, 1, 0, 704, 98
44097, V, 1, 1, 1, 1, 0, 704, 98
44098, V, 1, 1, 1, 1, 0, 704, 98
44099, V, 1, 1, 1, 1, 0, 704, 98
44100, V, 1, 1, 1, 1, 0, 704, 98
44101, V, 1, 1, 1, 1, 0, 704, 98
44102, V, 1, 1, 1, 1, 0, 704, 99
44103, V, 1, 1, 1, 1, 0, 704, 98
44104, V, 1, 1, 1, 1, 0, 704, 98
44105, V, 1, 1, 1, 1, 0, 704, 98
44106, V, 1, 1, 1, 1, 0, 704, 98
44107, V, 1, 1, 1, 1, 0, 704, 98
44108, V, 1, 1, 1, 1, 0, 704, 98
44109, V, 1, 1, 1, 1, 0, 704, 98
44110, V, 1, 1, 1, 1, 0, 704, 98
44111, V, 1, 1, 1, 1, 0, 704, 98
44112, V, 1, 1, 1, 1, 0, 704, 98
44113, V, 1, 1, 1, 1, 0, 704, 98
44114, V, 1, 1, 1, 1, 0, 704, 98
44115, V, 1, 1, 1, 1, 0, 704, 98
44116, V, 1, 1, 1, 1, 0, 704, 98
44118, V, 1, 1, 1, 1, 0, 704, 98
44119, V, 1, 1, 1, 1, 0, 704, 98
44120, V, 1, 1, 1, 1, 0, 704, 98
44121, V, 1, 1, 1, 1, 0, 704, 98
44122, V, 1, 1, 1, 1, 0, 704, 98
44123, V, 1, 1, 1, 1, 0, 704, 98
44124, V, 1, 1, 1, 1, 0, 704, 98
44125, V, 1, 1, 1, 1, 0, 704, 98
44126, V, 1, 1, 1, 1, 0, 704, 98
44127, V, 1, 1, 1, 1, 0, 704, 98
44128, V, 1, 1, 1, 1, 0, 704, 98
44129, V, 1, 1, 1, 1, 0, 704, 98
44130, V, 1, 1, 1, 1, 0, 704, 98
44131, V, 1, 1, 1, 1, 0, 704, 98
44132, V, 1, 1, 1, 1, 0, 704, 98
44133, V, 1, 1, 1, 1, 0, 704, 98
44134, V, 1, 1, 1, 1, 0, 704, 98
44135, V, 1, 1, 1, 1, 0, 704, 98
44136, V, 1, 1, 1, 1, 0, 704, 98
44137, V, 1, 1, 1, 1, 0, 704, 98
44138, V, 1, 1, 1, 1, 0, 704, 98
44139, V, 1, 1, 1, 1, 0, 704, 98
44140, V, 1, 1, 1, 1, 0, 704, 98
44141, V, 1, 1, 1, 1, 0, 704, 98
44142, V, 1, 1, 1, 1, 0, 704, 98
44143, V, 1, 1, 1, 1, 0, 704, 98
44144, V, 1, 1, 1, 1, 0, 704, 98
44145, V, 1, 1, 1, 1, 0, 704, 98
44146, V, 1, 1, 1, 1, 0, 704, 98
44147, V, 1, 1, 1, 1, 0, 704, 98
44148, V, 1, 1, 1, 1, 0, 704, 98
44149, V, 1, 1, 1, 1, 0, 704, 98
44150, V, 1, 1, 1, 1, 0, 704, 98
44151, V, 1, 1, 1, 1, 0, 704, 98
44152, V, 1, 1, 1, 1, 0, 704, 98
44153, V, 1, 1, 1, 1, 0, 704, 98
44154, V, 1, 1, 1, 1, 0, 704, 98
44155, V, 1, 1, 1, 1, 0, 704, 99
44156, V, 1, 1, 1, 1, 0, 704, 98
44157, V, 1, 1, 1, 1, 0, 704, 98
44158, V, 1, 1, 1, 1, 0, 704, 98
44160, V, 1, 1, 1, 1, 0, 704, 98
44161, V, 1, 1, 1, 1, 0, 704, 98
44162, V, 1, 1, 1, 1, 0, 704, 99
44163, V, 1, 1, 1, 1, 0, 704, 99
44164, V, 1, 1, 1, 1, 0, 704, 99
44165, V, 1, 1, 1, 1, 0, 704, 98
44166, V, 1, 1, 1, 1, 0, 704, 99
44167, V, 1, 1, 1, 1, 0, 704, 98
44168, V, 1, 1, 1, 1, 0, 704, 99
44169, V, 1, 1, 1, 1, 0, 704, 98
44170, V, 1, 1, 1, 1, 0, 704, 98
44171, V, 1, 1, 1, 1, 0, 704, 98
44172, V, 1, 1, 1, 1, 0, 704, 98
44173, V, 1, 1, 1, 1, 0, 704, 98
44174, V, 1, 1, 1, 1, 0, 704, 99
44175, V, 1, 1, 1, 1, 0, 704, 99
44176, V, 1, 1, 1, 1, 0, 704, 98
44177, V, 1, 1, 1, 1, 0, 704, 98
44178, V, 1, 1, 1, 1, 0, 704, 99
44179, V, 1, 1, 1, 1, 0, 704, 98
44180, V, 1, 1, 1, 1, 0, 704, 99
44181, V, 1, 1, 1, 1, 0, 704, 98
44182, V, 1, 1, 1, 1, 0, 704, 98
44183, V, 1, 1, 1, 1, 0, 704, 99
44184, V, 1, 1, 1, 1, 0, 704, 98
44185, V, 1, 1, 1, 1, 0, 704, 99
44186, V, 1, 1, 1, 1, 0, 704, 98
44187, V, 1, 1, 1, 1, 0, 704, 98
44188, V, 1, 1, 1, 1, 0, 704, 99
44189, V, 1, 1, 1, 1, 0, 704, 98
44190, V, 1, 1, 1, 1, 0, 704, 98
44191, V, 1, 1, 1, 1, 0, 704, 98
44192, V, 1, 1, 1, 1, 0, 704, 98
44193, V, 1, 1, 1, 1, 0, 704, 99
44194, V, 1, 1, 1, 1, 0, 704, 99
44195, V, 1, 1, 1, 1, 0, 704, 99
44196, V, 1, 1, 1, 1, 0, 704, 99
44197, V, 1, 1, 1, 1, 0, 704, 99
44198, V, 1, 1, 1, 1, 0, 704, 99
44199, V, 1, 1, 1, 1, 0, 704, 99
44200, V, 1, 1, 1, 1, 0, 704, 99
44201, V, 1, 1, 1, 1, 0, 704, 99
44203, V, 1, 1, 1, 1, 0, 704, 99
44204, V, 1, 1, 1, 1, 0, 704, 99
44205, V, 1, 1, 1, 1, 0, 704, 99
44206, V, 1, 1, 1, 1, 0, 704, 99
44207, V, 1, 1, 1, 1, 0, 704, 99
44208, V, 1, 1, 1, 1, 0, 704, 99
44209, V, 1, 1, 1, 1, 0, 704, 98
44210, V, 1, 1, 1, 1, 0, 704, 99
44211, V, 1, 1, 1, 1, 0, 704, 99
44212, V, 1, 1, 1, 1, 0, 704, 98
44213, V, 1, 1, 1, 1, 0, 704, 98
44214, V, 1, 1, 1, 1, 0, 704, 98
44215, V, 1, 1, 1, 1, 0, 704, 98
44216, V, 1, 1, 1, 1, 0, 704, 98
44217, V, 1, 1, 1, 1, 0, 704, 98
44218, V, 1, 1, 1, 1, 0, 704, 98
44219, V, 1, 1, 1, 1, 0, 704, 99
44220, V, 1, 1, 1, 1, 0, 704, 98
44221, V, 1, 1, 1, 1, 0, 704, 98
44222, V, 1, 1, 1, 1, 0, 704, 98
44223, V, 1, 1, 1, 1, 0, 704, 98
44224, V, 1, 1, 1, 1, 0, 704, 98
44225, V, 1, 1, 1, 1, 0, 704, 98
44226, V, 1, 1, 1, 1, 0, 704, 98
44227, V, 1, 1, 1, 1, 0, 704, 98
44228, V, 1, 1, 1, 1, 0, 704, 98
44229, V, 1, 1, 1, 1, 0, 704, 98
44230, V, 1, 1, 1, 1, 0, 704, 98
44231, V, 1, 1, 1, 1, 0, 704, 98
44232, V, 1, 1, 1, 1, 0, 704, 98
44233, V, 1, 1, 1, 1, 0, 704, 98
44234, V, 1, 1, 1, 1, 0, 704, 98
44235, V, 1, 1, 1, 1, 0, 704, 98
44236, V, 1, 1, 1, 1, 0, 704, 98
44237, V, 1, 1, 1, 1, 0, 704, 98
44238, V, 1, 1, 1, 1, 0, 704, 98
44239, V, 1, 1, 1, 1, 0, 704, 98
44240, V, 1, 1, 1, 1, 0, 704, 98
44241, V, 1, 1, 1, 1, 0, 704, 98
44242, V, 1, 1, 1, 1, 0, 704, 98
44243, V, 1, 1, 1, 1, 0, 704, 98
44244, V, 1, 1, 1, 1, 0, 704, 98
44246, V, 1, 1, 1, 1, 0, 704, 98
44247, V, 1, 1, 1, 1, 0, 704, 98
44248, V, 1, 1, 1, 1, 0, 704, 98
44249, V, 1, 1, 1, 1, 0, 704, 99
44250, V, 1, 1, 1, 1, 0, 704, 98
44251, V, 1, 1, 1, 1, 0, 704, 98
44252, V, 1, 1, 1, 1, 0, 704, 98
44253, V, 1, 1, 1, 1, 0, 704, 98
44254, V, 1, 1, 1, 1, 0, 704, 98
44255, V, 1, 1, 1, 1, 0, 704, 98
44256, V, 1, 1, 1, 1, 0, 704, 98
44257, V, 1, 1, 1, 1, 0, 704, 98
44258, V, 1, 1, 1, 1, 0, 704, 98
44259, V, 1, 1, 1, 1, 0, 704, 98
44260, V, 1, 1, 1, 1, 0, 704, 98
44261, V, 1, 1, 1, 1, 0, 704, 98
44262, V, 1, 1, 1, 1, 0, 704, 98
44263, V, 1, 1, 1, 1, 0, 704, 98
44264, V, 1, 1, 1, 1, 0, 704, 98
44265, V, 1, 1, 1, 1, 0, 704, 98
44266, V, 1, 1, 1, 1, 0, 704, 98
44267, V, 1, 1, 1, 1, 0, 704, 98
44268, V, 1, 1, 1, 1, 0, 704, 98
44269, V, 1, 1, 1, 1, 0, 704, 98
44270, V, 1, 1, 1, 1, 0, 704, 98
44271, V, 1, 1, 1, 1, 0, 704, 98
44272, V, 1, 1, 1, 1, 0, 704, 98
44273, V, 1, 1, 1, 1, 0, 704, 98
44274, V, 1, 1, 1, 1, 0, 704, 98
44275, V, 1, 1, 1, 1, 0, 704, 98
44276, V, 1, 1, 1, 1, 0, 704, 98
44277, V, 1, 1, 1, 1, 0, 704, 98
44278, V, 1, 1, 1, 1, 0, 704, 98
44279, V, 1, 1, 1, 1, 0, 704, 98
44280, V, 1, 1, 1, 1, 0, 704, 98
44281, V, 1, 1, 1, 1, 0, 704, 98
44282, V, 1, 1, 1, 1, 0, 704, 98
44283, V, 1, 1, 1, 1, 0, 704, 98
44284, V, 1, 1, 1, 1, 0, 704, 98
44285, V, 1, 1, 1, 1, 0, 704, 98
44286, V, 1, 1, 1, 1, 0, 704, 98
44288, V, 1, 1, 1, 1, 0, 704, 98
44289, V, 1, 1, 1, 1, 0, 704, 98
44290, V, 1, 1, 1, 1, 0, 704, 98
44291, V, 1, 1, 1, 1, 0, 704, 98
44292, V, 1, 1, 1, 1, 0, 704, 98
44293, V, 1, 1, 1, 1, 0, 704, 98
44294, V, 1, 1, 1, 1, 0, 704, 98
44295, V, 1, 1, 1, 1, 0, 704, 98
44296, V, 1, 1, 1, 1, 0, 704, 98
44297, V, 1, 1, 1, 1, 0, 704, 98
44298, V, 1, 1, 1, 1, 0, 704, 98
44299, V, 1, 1, 1, 1, 0, 704, 98
44300, V, 1, 1, 1, 1, 0, 704, 98
44301, V, 1, 1, 1, 1, 0, 704, 98
44302, V, 1, 1, 1, 1, 0, 704, 98
44303, V, 1, 1, 1, 1, 0, 704, 98
44304, V, 1, 1, 1, 1, 0, 704, 98
44305, V, 1, 1, 1, 1, 0, 704, 98
44306, V, 1, 1, 1, 1, 0, 704, 98
44307, V, 1, 1, 1, 1, 0, 704, 98
44308, V, 1, 1, 1, 1, 0, 704, 98
44309, V, 1, 1, 1, 1, 0, 704, 98
44310, V, 1, 1, 1, 1, 0, 704, 98
44311, V, 1, 1, 1, 1, 0, 704, 98
44312, V, 1, 1, 1, 1, 0, 704, 98
44313, V, 1, 1, 1, 1, 0, 704, 98
44314, V, 1, 1, 1, 1, 0, 704, 98
44315, V, 1, 1, 1, 1, 0, 704, 98
44316, V, 1, 1, 1, 1, 0, 704, 98
44317, V, 1, 1, 1, 1, 0, 704, 98
44318, V, 1, 1, 1, 1, 0, 704, 98
44319, V, 1, 1, 1, 1, 0, 704, 98
44320, V, 1, 1, 1, 1, 0, 704, 98
44321, V, 1, 1, 1, 1, 0, 704, 98
44322, V, 1, 1, 1, 1, 0, 704, 98
44323, V, 1, 1, 1, 1, 0, 704, 98
44324, V, 1, 1, 1, 1, 0, 704, 98
44325, V, 1, 1, 1, 1, 0, 704, 98
44326, V, 1, 1, 1, 1, 0, 704, 98
44327, V, 1, 1, 1, 1, 0, 704, 98
44328, V, 1, 1, 1, 1, 0, 704, 98
44329, V, 1, 1, 1, 1, 0, 704, 98
44331, V, 1, 1, 1, 1, 0, 704, 98
44332, V, 1, 1, 1, 1, 0, 704, 98
44333, V, 1, 1, 1, 1, 0, 704, 98
44334, V, 1, 1, 1, 1, 0, 704, 98
44335, V, 1, 1, 1, 1, 0, 704, 98
44336, V, 1, 1, 1, 1, 0, 704, 98
44337, V, 1, 1, 1, 1, 0, 704, 98
44338, V, 1, 1, 1, 1, 0, 704, 98
44339, V, 1, 1, 1, 1, 0, 704, 98
44340, V, 1, 1, 1, 1, 0, 704, 98
44341, V, 1, 1, 1, 1, 0, 704, 98
44342, V, 1, 1, 1, 1, 0, 704, 98
44343, V, 1, 1, 1, 1, 0, 704, 98
44344, V, 1, 1, 1, 1, 0, 704, 98
44345, V, 1, 1, 1, 1, 0, 704, 98
44346, V, 1, 1, 1, 1, 0, 704, 98
44347, V, 1, 1, 1, 1, 0, 704, 98
44348, V, 1, 1, 1, 1, 0, 704, 98
44349, V, 1, 1, 1, 1, 0, 704, 98
44350, V, 1, 1, 1, 1, 0, 704, 98
44351, V, 1, 1, 1, 1, 0, 704, 98
44352, V, 1, 1, 1, 1, 0, 704, 98
44353, V, 1, 1, 1, 1, 0, 704, 98
44354, V, 1, 1, 1, 1, 0, 704, 98
44355, V, 1, 1, 1, 1, 0, 704, 98
44356, V, 1, 1, 1, 1, 0, 704, 98
44357, V, 1, 1, 1, 1, 0, 704, 98
44358, V, 1, 1, 1, 1, 0, 704, 98
44359, V, 1, 1, 1, 1, 0, 704, 98
44360, V, 1, 1, 1, 1, 0, 704, 98
44361, V, 1, 1, 1, 1, 0, 704, 98
44362, V, 1, 1, 1, 1, 0, 704, 98
44363, V, 1, 1, 1, 1, 0, 704, 98
44364, V, 1, 1, 1, 1, 0, 704, 98
44365, V, 1, 1, 1, 1, 0, 704, 98
44366, V, 1, 1, 1, 1, 0, 704, 98
44367, V, 1, 1, 1, 1, 0, 704, 98
44368, V, 1, 1, 1, 1, 0, 704, 98
44369, V, 1, 1, 1, 1, 0, 704, 98
44370, V, 1, 1, 1, 1, 0, 704, 98
44371, V, 1, 1, 1, 1, 0, 704, 98
44372, V, 1, 1, 1, 1, 0, 704, 98
44374, V, 1, 1, 1, 1, 0, 704, 98
44375, V, 1, 1, 1, 1, 0, 704, 98
44376, V, 1, 1, 1, 1, 0, 704, 98
44377, V, 1, 1, 1, 1, 0, 704, 98
44378, V, 1, 1, 1, 1, 0, 704, 98
44379, V, 1, 1, 1, 1, 0, 704, 98
44380, V, 1, 1, 1, 1, 0, 704, 98
44381, V, 1, 1, 1, 1, 0, 704, 98
44382, V, 1, 1, 1, 1, 0, 704, 98
44383, V, 1, 1, 1, 1, 0, 704, 98
44384, V, 1, 1, 1, 1, 0, 704, 98
44385, V, 1, 1, 1, 1, 0, 704, 98
44386, V, 1, 1, 1, 1, 0, 704, 98
44387, V, 1, 1, 1, 1, 0, 704, 98
44388, V, 1, 1, 1, 1, 0, 704, 98
44389, V, 1, 1, 1, 1, 0, 704, 98
44390, V, 1, 1, 1, 1, 0, 704, 98
44391, V, 1, 1, 1, 1, 0, 704, 98
44392, V, 1, 1, 1, 1, 0, 704, 98
44393, V, 1, 1, 1, 1, 0, 704, 98
44394, V, 1, 1, 1, 1, 0, 704, 98
44395, V, 1, 1, 1, 1, 0, 704, 98
44396, V, 1, 1, 1, 1, 0, 704, 98
44397, V, 1, 1, 1, 1, 0, 704, 98
44398, V, 1, 1, 1, 1, 0, 704, 98
44399, V, 1, 1, 1, 1, 0, 704, 98
44400, V, 1, 1, 1, 1, 0, 704, 98
44401, V, 1, 1, 1, 1, 0, 704, 98
44402, V, 1, 1, 1, 1, 0, 704, 98
44403, V, 1, 1, 1, 1, 0, 704, 98
44404, V, 1, 1, 1, 1, 0, 704, 98
44405, V, 1, 1, 1, 1, 0, 704, 98
44406, V, 1, 1, 1, 1, 0, 704, 98
44407, V, 1, 1, 1, 1, 0, 704, 98
44408, V, 1, 1, 1, 1, 0, 704, 98
44409, V, 1, 1, 1, 1, 0, 704, 98
44410, V, 1, 1, 1, 1, 0, 704, 98
44411, V, 1, 1, 1, 1, 0, 704, 98
44412, V, 1, 1, 1, 1, 0, 704, 98
44413, V, 1, 1, 1, 1, 0, 704, 98
44414, V, 1, 1, 1, 1, 0, 704, 98
44416, V, 1, 1, 1, 1, 0, 704, 98
44417, V, 1, 1, 1, 1, 0, 704, 98
44418, V, 1, 1, 1, 1, 0, 704, 98
44419, V, 1, 1, 1, 1, 0, 704, 98
44420, V, 1, 1, 1, 1, 0, 704, 98
44421, V, 1, 1, 1, 1, 0, 704, 98
44422, V, 1, 1, 1, 1, 0, 704, 98
44423, V, 1, 1, 1, 1, 0, 704, 98
44424, V, 1, 1, 1, 1, 0, 704, 98
44425, V, 1, 1, 1, 1, 0, 704, 98
44426, V, 1, 1, 1, 1, 0, 704, 98
44427, V, 1, 1, 1, 1, 0, 704, 98
44428, V, 1, 1, 1, 1, 0, 704, 98
44429, V, 1, 1, 1, 1, 0, 704, 98
44430, V, 1, 1, 1, 1, 0, 704, 98
44431, V, 1, 1, 1, 1, 0, 704, 98
44432, V, 1, 1, 1, 1, 0, 704, 98
44433, V, 1, 1, 1, 1, 0, 704, 98
44434, V, 1, 1, 1, 1, 0, 704, 98
44435, V, 1, 1, 1, 1, 0, 704, 98
44436, V, 1, 1, 1, 1, 0, 704, 98
44437, V, 1, 1, 1, 1, 0, 704, 98
44438, V, 1, 1, 1, 1, 0, 704, 98
44439, V, 1, 1, 1, 1, 0, 704, 98
44440, V, 1, 1, 1, 1, 0, 704, 98
44441, V, 1, 1, 1, 1, 0, 704, 98
44442, V, 1, 1, 1, 1, 0, 704, 98
44443, V, 1, 1, 1, 1, 0, 704, 98
44444, V, 1, 1, 1, 1, 0, 704, 98
44445, V, 1, 1, 1, 1, 0, 704, 98
44446, V, 1, 1, 1, 1, 0, 704, 98
44447, V, 1, 1, 1, 1, 0, 704, 98
44448, V, 1, 1, 1, 1, 0, 704, 98
44449, V, 1, 1, 1, 1, 0, 704, 98
44450, V, 1, 1, 1, 1, 0, 704, 98
44451, V, 1, 1, 1, 1, 0, 704, 98
44452, V, 1, 1, 1, 1, 0, 704, 98
44453, V, 1, 1, 1, 1, 0, 704, 98
44454, V, 1, 1, 1, 1, 0, 704, 98
44455, V, 1, 1, 1, 1, 0, 704, 98
44456, V, 1, 1, 1, 1, 0, 704, 98
44457, V, 1, 1, 1, 1, 0, 704, 98
44459, V, 1, 1, 1, 1, 0, 704, 98
44460, V, 1, 1, 1, 1, 0, 704, 98
44461, V, 1, 1, 1, 1, 0, 704, 98
44462, V, 1, 1, 1, 1, 0, 704, 98
44463, V, 1, 1, 1, 1, 0, 704, 98
44464, V, 1, 1, 1, 1, 0, 704, 98
44465, V, 1, 1, 1, 1, 0, 704, 98
44466, V, 1, 1, 1, 1, 0, 704, 99
44467, V, 1, 1, 1, 1, 0, 704, 98
44468, V, 1, 1, 1, 1, 0, 704, 99
44469, V, 1, 1, 1, 1, 0, 704, 98
44470, V, 1, 1, 1, 1, 0, 704, 98
44471, V, 1, 1, 1, 1, 0, 704, 98
44472, V, 1, 1, 1, 1, 0, 704, 98
44473, V, 1, 1, 1, 1, 0, 704, 98
44474, V, 1, 1, 1, 1, 0, 704, 98
44475, V, 1, 1, 1, 1, 0, 704, 98
44476, V, 1, 1, 1, 1, 0, 704, 98
44477, V, 1, 1, 1, 1, 0, 704, 98
44478, V, 1, 1, 1, 1, 0, 704, 98
44479, V, 1, 1, 1, 1, 0, 704, 98
44480, V, 1, 1, 1, 1, 0, 704, 99
44481, V, 1, 1, 1, 1, 0, 704, 98
44482, V, 1, 1, 1, 1, 0, 704, 98
44483, V, 1, 1, 1, 1, 0, 704, 98
44484, V, 1, 1, 1, 1, 0, 704, 98
44485, V, 1, 1, 1, 1, 0, 704, 98
44486, V, 1, 1, 1, 1, 0, 704, 98
44487, V, 1, 1, 1, 1, 0, 704, 98
44488, V, 1, 1, 1, 1, 0, 704, 98
44489, V, 1, 1, 1, 1, 0, 704, 98
44490, V, 1, 1, 1, 1, 0, 704, 98
44491, V, 1, 1, 1, 1, 0, 704, 99
44492, V, 1, 1, 1, 1, 0, 704, 98
44493, V, 1, 1, 1, 1, 0, 704, 98
44494, V, 1, 1, 1, 1, 0, 704, 98
44495, V, 1, 1, 1, 1, 0, 704, 98
44496, V, 1, 1, 1, 1, 0, 704, 98
44497, V, 1, 1, 1, 1, 0, 704, 98
44498, V, 1, 1, 1, 1, 0, 704, 98
44499, V, 1, 1, 1, 1, 0, 704, 98
44500, V, 1, 1, 1, 1, 0, 704, 98
44502, V, 1, 1, 1, 1, 0, 704, 98
44503, V, 1, 1, 1, 1, 0, 704, 98
44504, V, 1, 1, 1, 1, 0, 704, 98
44505, V, 1, 1, 1, 1, 0, 704, 98
44506, V, 1, 1, 1, 1, 0, 704, 98
44507, V, 1, 1, 1, 1, 0, 704, 98
44508, V, 1, 1, 1, 1, 0, 704, 98
44509, V, 1, 1, 1, 1, 0, 704, 98
44510, V, 1, 1, 1, 1, 0, 704, 98
44511, V, 1, 1, 1, 1, 0, 704, 98
44512, V, 1, 1, 1, 1, 0, 704, 98
44513, V, 1, 1, 1, 1, 0, 704, 98
44514, V, 1, 1, 1, 1, 0, 704, 98
44515, V, 1, 1, 1, 1, 0, 704, 98
44516, V, 1, 1, 1, 1, 0, 704, 98
44517, V, 1, 1, 1, 1, 0, 704, 98
44518, V, 1, 1, 1, 1, 0, 704, 98
44519, V, 1, 1, 1, 1, 0, 704, 98
44520, V, 1, 1, 1, 1, 0, 704, 98
44521, V, 1, 1, 1, 1, 0, 704, 98
44522, V, 1, 1, 1, 1, 0, 704, 98
44523, V, 1, 1, 1, 1, 0, 704, 98
44524, V, 1, 1, 1, 1, 0, 704, 98
44525, V, 1, 1, 1, 1, 0, 704, 98
44526, V, 1, 1, 1, 1, 0, 704, 98
44527, V, 1, 1, 1, 1, 0, 704, 98
44528, V, 1, 1, 1, 1, 0, 704, 98
44529, V, 1, 1, 1, 1, 0, 704, 98
44530, V, 1, 1, 1, 1, 0, 704, 98
44531, V, 1, 1, 1, 1, 0, 704, 98
44532, V, 1, 1, 1, 1, 0, 704, 98
44533, V, 1, 1, 1, 1, 0, 704, 98
44534, V, 1, 1, 1, 1, 0, 704, 98
44535, V, 1, 1, 1, 1, 0, 704, 98
44536, V, 1, 1, 1, 1, 0, 704, 98
44537, V, 1, 1, 1, 1, 0, 704, 98
44538, V, 1, 1, 1, 1, 0, 704, 98
44539, V, 1, 1, 1, 1, 0, 704, 98
44540, V, 1, 1, 1, 1, 0, 704, 98
44541, V, 1, 1, 1, 1, 0, 704, 98
44542, V, 1, 1, 1, 1, 0, 704, 98
44544, V, 1, 1, 1, 1, 0, 704, 98
44545, V, 1, 1, 1, 1, 0, 704, 98
44546, V, 1, 1, 1, 1, 0, 704, 98
44547, V, 1, 1, 1, 1, 0, 704, 98
44548, V, 1, 1, 1, 1, 0, 704, 98
44549, V, 1, 1, 1, 1, 0, 704, 98
44550, V, 1, 1, 1, 1, 0, 704, 98
44551, V, 1, 1, 1, 1, 0, 704, 98
44552, V, 1, 1, 1, 1, 0, 704, 98
44553, V, 1, 1, 1, 1, 0, 704, 98
44554, V, 1, 1, 1, 1, 0, 704, 98
44555, V, 1, 1, 1, 1, 0, 704, 98
44556, V, 1, 1, 1, 1, 0, 704, 98
44557, V, 1, 1, 1, 1, 0, 704, 98
44558, V, 1, 1, 1, 1, 0, 704, 98
44559, V, 1, 1, 1, 1, 0, 704, 98
44560, V, 1, 1, 1, 1, 0, 704, 98
44561, V, 1, 1, 1, 1, 0, 704, 98
44562, V, 1, 1, 1, 1, 0, 704, 98
44563, V, 1, 1, 1, 1, 0, 704, 98
44564, V, 1, 1, 1, 1, 0, 704, 98
44565, V, 1, 1, 1, 1, 0, 704, 98
44566, V, 1, 1, 1, 1, 0, 704, 98
44567, V, 1, 1, 1, 1, 0, 704, 98
44568, V, 1, 1, 1, 1, 0, 704, 98
44569, V, 1, 1, 1, 1, 0, 704, 98
44570, V, 1, 1, 1, 1, 0, 704, 98
44571, V, 1, 1, 1, 1, 0, 704, 98
44572, V, 1, 1, 1, 1, 0, 704, 98
44573, V, 1, 1, 1, 1, 0, 704, 98
44574, V, 1, 1, 1, 1, 0, 704, 98
44575, V, 1, 1, 1, 1, 0, 704, 98
44576, V, 1, 1, 1, 1, 0, 704, 98
44577, V, 1, 1, 1, 1, 0, 704, 98
44578, V, 1, 1, 1, 1, 0, 704, 98
44579, V, 1, 1, 1, 1, 0, 704, 98
44580, V, 1, 1, 1, 1, 0, 704, 98
44581, V, 1, 1, 1, 1, 0, 704, 98
44582, V, 1, 1, 1, 1, 0, 704, 98
44583, V, 1, 1, 1, 1, 0, 704, 98
44584, V, 1, 1, 1, 1, 0, 704, 98
44585, V, 1, 1, 1, 1, 0, 704, 98
44587, V, 1, 1, 1, 1, 0, 704, 98
44588, V, 1, 1, 1, 1, 0, 704, 98
44589, V, 1, 1, 1, 1, 0, 704, 98
44590, V, 1, 1, 1, 1, 0, 704, 98
44591, V, 1, 1, 1, 1, 0, 704, 98
44592, V, 1, 1, 1, 1, 0, 704, 98
44593, V, 1, 1, 1, 1, 0, 704, 98
44594, V, 1, 1, 1, 1, 0, 704, 98
44595, V, 1, 1, 1, 1, 0, 704, 98
44596, V, 1, 1, 1, 1, 0, 704, 98
44597, V, 1, 1, 1, 1, 0, 704, 98
44598, V, 1, 1, 1, 1, 0, 704, 98
44599, V, 1, 1, 1, 1, 0, 704, 98
44600, V, 1, 1, 1, 1, 0, 704, 98
44601, V, 1, 1, 1, 1, 0, 704, 98
44602, V, 1, 1, 1, 1, 0, 704, 98
44603, V, 1, 1, 1, 1, 0, 704, 98
44604, V, 1, 1, 1, 1, 0, 704, 98
44605, V, 1, 1, 1, 1, 0, 704, 98
44606, V, 1, 1, 1, 1, 0, 704, 98
44607, V, 1, 1, 1, 1, 0, 704, 98
44608, V, 1, 1, 1, 1, 0, 704, 98
44609, V, 1, 1, 1, 1, 0, 704, 98
44610, V, 1, 1, 1, 1, 0, 704, 98
44611, V, 1, 1, 1, 1, 0, 704, 98
44612, V, 1, 1, 1, 1, 0, 704, 98
44613, V, 1, 1, 1, 1, 0, 704, 98
44614, V, 1, 1, 1, 1, 0, 704, 98
44615, V, 1, 1, 1, 1, 0, 704, 98
44616, V, 1, 1, 1, 1, 0, 704, 98
44617, V, 1, 1, 1, 1, 0, 704, 98
44618, V, 1, 1, 1, 1, 0, 704, 98
44619, V, 1, 1, 1, 1, 0, 704, 98
44620, V, 1, 1, 1, 1, 0, 704, 98
44621, V, 1, 1, 1, 1, 0, 704, 98
44622, V, 1, 1, 1, 1, 0, 704, 98
44623, V, 1, 1, 1, 1, 0, 704, 98
44624, V, 1, 1, 1, 1, 0, 704, 98
44625, V, 1, 1, 1, 1, 0, 704, 99
44626, V, 1, 1, 1, 1, 0, 704, 98
44627, V, 1, 1, 1, 1, 0, 704, 98
44628, V, 1, 1, 1, 1, 0, 704, 98
44630, V, 1, 1, 1, 1, 0, 704, 98
44631, V, 1, 1, 1, 1, 0, 704, 98
44632, V, 1, 1, 1, 1, 0, 704, 98
44633, V, 1, 1, 1, 1, 0, 704, 98
44634, V, 1, 1, 1, 1, 0, 704, 98
44635, V, 1, 1, 1, 1, 0, 704, 98
44636, V, 1, 1, 1, 1, 0, 704, 98
44637, V, 1, 1, 1, 1, 0, 704, 98
44638, V, 1, 1, 1, 1, 0, 704, 98
44639, V, 1, 1, 1, 1, 0, 704, 98
44640, V, 1, 1, 1, 1, 0, 704, 98
44641, V, 1, 1, 1, 1, 0, 704, 98
44642, V, 1, 1, 1, 1, 0, 704, 98
44643, V, 1, 1, 1, 1, 0, 704, 98
44644, V, 1, 1, 1, 1, 0, 704, 98
44645, V, 1, 1, 1, 1, 0, 704, 98
44646, V, 1, 1, 1, 1, 0, 704, 98
44647, V, 1, 1, 1, 1, 0, 704, 98
44648, V, 1, 1, 1, 1, 0, 704, 98
44649, V, 1, 1, 1, 1, 0, 704, 98
44650, V, 1, 1, 1, 1, 0, 704, 98
44651, V, 1, 1, 1, 1, 0, 704, 98
44652, V, 1, 1, 1, 1, 0, 704, 98
44653, V, 1, 1, 1, 1, 0, 704, 98
44654, V, 1, 1, 1, 1, 0, 704, 98
44655, V, 1, 1, 1, 1, 0, 704, 98
44656, V, 1, 1, 1, 1, 0, 704, 98
44657, V, 1, 1, 1, 1, 0, 704, 98
44658, V, 1, 1, 1, 1, 0, 704, 98
44659, V, 1, 1, 1, 1, 0, 704, 98
44660, V, 1, 1, 1, 1, 0, 704, 98
44661, V, 1, 1, 1, 1, 0, 704, 98
44662, V, 1, 1, 1, 1, 0, 704, 98
44663, V, 1, 1, 1, 1, 0, 704, 98
44664, V, 1, 1, 1, 1, 0, 704, 98
44665, V, 1, 1, 1, 1, 0, 704, 98
44666, V, 1, 1, 1, 1, 0, 704, 98
44667, V, 1, 1, 1, 1, 0, 704, 98
44668, V, 1, 1, 1, 1, 0, 704, 98
44669, V, 1, 1, 1, 1, 0, 704, 98
44670, V, 1, 1, 1, 1, 0, 704, 98
44672, V, 1, 1, 1, 1, 0, 704, 98
44673, V, 1, 1, 1, 1, 0, 704, 98
44674, V, 1, 1, 1, 1, 0, 704, 98
44675, V, 1, 1, 1, 1, 0, 704, 98
44676, V, 1, 1, 1, 1, 0, 704, 98
44677, V, 1, 1, 1, 1, 0, 704, 98
44678, V, 1, 1, 1, 1, 0, 704, 98
44679, V, 1, 1, 1, 1, 0, 704, 98
44680, V, 1, 1, 1, 1, 0, 704, 98
44681, V, 1, 1, 1, 1, 0, 704, 98
44682, V, 1, 1, 1, 1, 0, 704, 98
44683, V, 1, 1, 1, 1, 0, 704, 98
44684, V, 1, 1, 1, 1, 0, 704, 98
44685, V, 1, 1, 1, 1, 0, 704, 98
44686, V, 1, 1, 1, 1, 0, 704, 98
44687, V, 1, 1, 1, 1, 0, 704, 98
44688, V, 1, 1, 1, 1, 0, 704, 98
44689, V, 1, 1, 1, 1, 0, 704, 98
44690, V, 1, 1, 1, 1, 0, 704, 98
44691, V, 1, 1, 1, 1, 0, 704, 98
44692, V, 1, 1, 1, 1, 0, 704, 98
44693, V, 1, 1, 1, 1, 0, 704, 98
44694, V, 1, 1, 1, 1, 0, 704, 98
44695, V, 1, 1, 1, 1, 0, 704, 98
44696, V, 1, 1, 1, 1, 0, 704, 98
44697, V, 1, 1, 1, 1, 0, 704, 98
44698, V, 1, 1, 1, 1, 0, 704, 98
44699, V, 1, 1, 1, 1, 0, 704, 98
44700, V, 1, 1, 1, 1, 0, 704, 98
44701, V, 1, 1, 1, 1, 0, 704, 98
44702, V, 1, 1, 1, 1, 0, 704, 98
44703, V, 1, 1, 1, 1, 0, 704, 98
44704, V, 1, 1, 1, 1, 0, 704, 98
44705, V, 1, 1, 1, 1, 0, 704, 98
44706, V, 1, 1, 1, 1, 0, 704, 98
44707, V, 1, 1, 1, 1, 0, 704, 98
44708, V, 1, 1, 1, 1, 0, 704, 98
44709, V, 1, 1, 1, 1, 0, 704, 98
44710, V, 1, 1, 1, 1, 0, 704, 98
44711, V, 1, 1, 1, 1, 0, 704, 98
44712, V, 1, 1, 1, 1, 0, 704, 98
44713, V, 1, 1, 1, 1, 0, 704, 98
44715, V, 1, 1, 1, 1, 0, 704, 98
44716, V, 1, 1, 1, 1, 0, 704, 98
44717, V, 1, 1, 1, 1, 0, 704, 98
44718, V, 1, 1, 1, 1, 0, 704, 98
44719, V, 1, 1, 1, 1, 0, 704, 98
44720, V, 1, 1, 1, 1, 0, 704, 98
44721, V, 1, 1, 1, 1, 0, 704, 98
44722, V, 1, 1, 1, 1, 0, 704, 98
44723, V, 1, 1, 1, 1, 0, 704, 98
44724, V, 1, 1, 1, 1, 0, 704, 98
44725, V, 1, 1, 1, 1, 0, 704, 98
44726, V, 1, 1, 1, 1, 0, 704, 98
44727, V, 1, 1, 1, 1, 0, 704, 98
44728, V, 1, 1, 1, 1, 0, 704, 98
44729, V, 1, 1, 1, 1, 0, 704, 98
44730, V, 1, 1, 1, 1, 0, 704, 98
44731, V, 1, 1, 1, 1, 0, 704, 98
44732, V, 1, 1, 1, 1, 0, 704, 98
44733, V, 1, 1, 1, 1, 0, 704, 98
44734, V, 1, 1, 1, 1, 0, 704, 98
44735, V, 1, 1, 1, 1, 0, 704, 98
44736, V, 1, 1, 1, 1, 0, 704, 98
44737, V, 1, 1, 1, 1, 0, 704, 98
44738, V, 1, 1, 1, 1, 0, 704, 98
44739, V, 1, 1, 1, 1, 0, 704, 98
44740, V, 1, 1, 1, 1, 0, 704, 98
44741, V, 1, 1, 1, 1, 0, 704, 98
44742, V, 1, 1, 1, 1, 0, 704, 98
44743, V, 1, 1, 1, 1, 0, 704, 98
44744, V, 1, 1, 1, 1, 0, 704, 98
44745, V, 1, 1, 1, 1, 0, 704, 98
44746, V, 1, 1, 1, 1, 0, 704, 98
44747, V, 1, 1, 1, 1, 0, 704, 98
44748, V, 1, 1, 1, 1, 0, 704, 98
44749, V, 1, 1, 1, 1, 0, 704, 98
44750, V, 1, 1, 1, 1, 0, 704, 98
44751, V, 1, 1, 1, 1, 0, 704, 98
44752, V, 1, 1, 1, 1, 0, 704, 98
44753, V, 1, 1, 1, 1, 0, 704, 98
44754, V, 1, 1, 1, 1, 0, 704, 98
44755, V, 1, 1, 1, 1, 0, 704, 98
44756, V, 1, 1, 1, 1, 0, 704, 98
44758, V, 1, 1, 1, 1, 0, 704, 98
44759, V, 1, 1, 1, 1, 0, 704, 98
44760, V, 1, 1, 1, 1, 0, 704, 98
44761, V, 1, 1, 1, 1, 0, 704, 98
44762, V, 1, 1, 1, 1, 0, 704, 98
44763, V, 1, 1, 1, 1, 0, 704, 98
44764, V, 1, 1, 1, 1, 0, 704, 98
44765, V, 1, 1, 1, 1, 0, 704, 98
44766, V, 1, 1, 1, 1, 0, 704, 98
44767, V, 1, 1, 1, 1, 0, 704, 98
44768, V, 1, 1, 1, 1, 0, 704, 98
44769, V, 1, 1, 1, 1, 0, 704, 98
44770, V, 1, 1, 1, 1, 0, 704, 98
44771, V, 1, 1, 1, 1, 0, 704, 98
44772, V, 1, 1, 1, 1, 0, 704, 98
44773, V, 1, 1, 1, 1, 0, 704, 98
44774, V, 1, 1, 1, 1, 0, 704, 98
44775, V, 1, 1, 1, 1, 0, 704, 98
44776, V, 1, 1, 1, 1, 0, 704, 98
44777, V, 1, 1, 1, 1, 0, 704, 98
44778, V, 1, 1, 1, 1, 0, 704, 98
44779, V, 1, 1, 1, 1, 0, 704, 98
44780, V, 1, 1, 1, 1, 0, 704, 98
44781, V, 1, 1, 1, 1, 0, 704, 98
44782, V, 1, 1, 1, 1, 0, 704, 98
44783, V, 1, 1, 1, 1, 0, 704, 98
44784, V, 1, 1, 1, 1, 0, 704, 98
44785, V, 1, 1, 1, 1, 0, 704, 98
44786, V, 1, 1, 1, 1, 0, 704, 98
44787, V, 1, 1, 1, 1, 0, 704, 98
44788, V, 1, 1, 1, 1, 0, 704, 98
44789, V, 1, 1, 1, 1, 0, 704, 98
44790, V, 1, 1, 1, 1, 0, 704, 98
44791, V, 1, 1, 1, 1, 0, 704, 98
44792, V, 1, 1, 1, 1, 0, 704, 98
44793, V, 1, 1, 1, 1, 0, 704, 98
44794, V, 1, 1, 1, 1, 0, 704, 98
44795, V, 1, 1, 1, 1, 0, 704, 98
44796, V, 1, 1, 1, 1, 0, 704, 98
44797, V, 1, 1, 1, 1, 0, 704, 98
44798, V, 1, 1, 1, 1, 0, 704, 98
44800, V, 1, 1, 1, 1, 0, 704, 98
44801, V, 1, 1, 1, 1, 0, 704, 98
44802, V, 1, 1, 1, 1, 0, 704, 98
44803, V, 1, 1, 1, 1, 0, 704, 98
44804, V, 1, 1, 1, 1, 0, 704, 98
44805, V, 1, 1, 1, 1, 0, 704, 98
44806, V, 1, 1, 1, 1, 0, 704, 98
44807, V, 1, 1, 1, 1, 0, 704, 98
44808, V, 1, 1, 1, 1, 0, 704, 98
44809, V, 1, 1, 1, 1, 0, 704, 98
44810, V, 1, 1, 1, 1, 0, 704, 98
44811, V, 1, 1, 1, 1, 0, 704, 98
44812, V, 1, 1, 1, 1, 0, 704, 98
44813, V, 1, 1, 1, 1, 0, 704, 98
44814, V, 1, 1, 1, 1, 0, 704, 98
44815, V, 1, 1, 1, 1, 0, 704, 98
44816, V, 1, 1, 1, 1, 0, 704, 98
44817, V, 1, 1, 1, 1, 0, 704, 98
44818, V, 1, 1, 1, 1, 0, 704, 98
44819, V, 1, 1, 1, 1, 0, 704, 98
44820, V, 1, 1, 1, 1, 0, 704, 98
44821, V, 1, 1, 1, 1, 0, 704, 98
44822, V, 1, 1, 1, 1, 0, 704, 98
44823, V, 1, 1, 1, 1, 0, 704, 98
44824, V, 1, 1, 1, 1, 0, 704, 98
44825, V, 1, 1, 1, 1, 0, 704, 98
44826, V, 1, 1, 1, 1, 0, 704, 98
44827, V, 1, 1, 1, 1, 0, 704, 98
44828, V, 1, 1, 1, 1, 0, 704, 98
44829, V, 1, 1, 1, 1, 0, 704, 98
44830, V, 1, 1, 1, 1, 0, 704, 98
44831, V, 1, 1, 1, 1, 0, 704, 98
44832, V, 1, 1, 1, 1, 0, 704, 98
44833, V, 1, 1, 1, 1, 0, 704, 98
44834, V, 1, 1, 1, 1, 0, 704, 98
44835, V, 1, 1, 1, 1, 0, 704, 98
44836, V, 1, 1, 1, 1, 0, 704, 98
44837, V, 1, 1, 1, 1, 0, 704, 98
44838, V, 1, 1, 1, 1, 0, 704, 98
44839, V, 1, 1, 1, 1, 0, 704, 98
44840, V, 1, 1, 1, 1, 0, 704, 98
44841, V, 1, 1, 1, 1, 0, 704, 98
44843, V, 1, 1, 1, 1, 0, 704, 98
44844, V, 1, 1, 1, 1, 0, 704, 98
44845, V, 1, 1, 1, 1, 0, 704, 98
44846, V, 1, 1, 1, 1, 0, 704, 98
44847, V, 1, 1, 1, 1, 0, 704, 98
44848, V, 1, 1, 1, 1, 0, 704, 98
44849, V, 1, 1, 1, 1, 0, 704, 98
44850, V, 1, 1, 1, 1, 0, 704, 98
44851, V, 1, 1, 1, 1, 0, 704, 98
44852, V, 1, 1, 1, 1, 0, 704, 98
44853, V, 1, 1, 1, 1, 0, 704, 98
44854, V, 1, 1, 1, 1, 0, 704, 98
44855, V, 1, 1, 1, 1, 0, 704, 98
44856, V, 1, 1, 1, 1, 0, 704, 98
44857, V, 1, 1, 1, 1, 0, 704, 98
44858, V, 1, 1, 1, 1, 0, 704, 98
44859, V, 1, 1, 1, 1, 0, 704, 98
44860, V, 1, 1, 1, 1, 0, 704, 98
44861, V, 1, 1, 1, 1, 0, 704, 98
44862, V, 1, 1, 1, 1, 0, 704, 98
44863, V, 1, 1, 1, 1, 0, 704, 98
44864, V, 1, 1, 1, 1, 0, 704, 98
44865, V, 1, 1, 1, 1, 0, 704, 98
44866, V, 1, 1, 1, 1, 0, 704, 98
44867, V, 1, 1, 1, 1, 0, 704, 98
44868, V, 1, 1, 1, 1, 0, 704, 98
44869, V, 1, 1, 1, 1, 0, 704, 98
44870, V, 1, 1, 1, 1, 0, 704, 98
44871, V, 1, 1, 1, 1, 0, 704, 98
44872, V, 1, 1, 1, 1, 0, 704, 98
44873, V, 1, 1, 1, 1, 0, 704, 98
44874, V, 1, 1, 1, 1, 0, 704, 98
44875, V, 1, 1, 1, 1, 0, 704, 98
44876, V, 1, 1, 1, 1, 0, 704, 98
44877, V, 1, 1, 1, 1, 0, 704, 98
44878, V, 1, 1, 1, 1, 0, 704, 98
44879, V, 1, 1, 1, 1, 0, 704, 98
44880, V, 1, 1, 1, 1, 0, 704, 98
44881, V, 1, 1, 1, 1, 0, 704, 98
44882, V, 1, 1, 1, 1, 0, 704, 98
44883, V, 1, 1, 1, 1, 0, 704, 98
44884, V, 1, 1, 1, 1, 0, 704, 98
44886, V, 1, 1, 1, 1, 0, 704, 98
44887, V, 1, 1, 1, 1, 0, 704, 98
44888, V, 1, 1, 1, 1, 0, 704, 98
44889, V, 1, 1, 1, 1, 0, 704, 98
44890, V, 1, 1, 1, 1, 0, 704, 98
44891, V, 1, 1, 1, 1, 0, 704, 98
44892, V, 1, 1, 1, 1, 0, 704, 98
44893, V, 1, 1, 1, 1, 0, 704, 98
44894, V, 1, 1, 1, 1, 0, 704, 98
44895, V, 1, 1, 1, 1, 0, 704, 98
44896, V, 1, 1, 1, 1, 0, 704, 98
44897, V, 1, 1, 1, 1, 0, 704, 98
44898, V, 1, 1, 1, 1, 0, 704, 98
44899, V, 1, 1, 1, 1, 0, 704, 98
44900, V, 1, 1, 1, 1, 0, 704, 98
44901, V, 1, 1, 1, 1, 0, 704, 98
44902, V, 1, 1, 1, 1, 0, 704, 98
44903, V, 1, 1, 1, 1, 0, 704, 98
44904, V, 1, 1, 1, 1, 0, 704, 98
44905, V, 1, 1, 1, 1, 0, 704, 98
44906, V, 1, 1, 1, 1, 0, 704, 98
44907, V, 1, 1, 1, 1, 0, 704, 98
44908, V, 1, 1, 1, 1, 0, 704, 98
44909, V, 1, 1, 1, 1, 0, 704, 98
44910, V, 1, 1, 1, 1, 0, 704, 98
44911, V, 1, 1, 1, 1, 0, 704, 98
44912, V, 1, 1, 1, 1, 0, 704, 98
44913, V, 1, 1, 1, 1, 0, 704, 98
44914, V, 1, 1, 1, 1, 0, 704, 98
44915, V, 1, 1, 1, 1, 0, 704, 98
44916, V, 1, 1, 1, 1, 0, 704, 98
44917, V, 1, 1, 1, 1, 0, 704, 98
44918, V, 1, 1, 1, 1, 0, 704, 98
44919, V, 1, 1, 1, 1, 0, 704, 98
44920, V, 1, 1, 1, 1, 0, 704, 98
44921, V, 1, 1, 1, 1, 0, 704, 98
44922, V, 1, 1, 1, 1, 0, 704, 98
44923, V, 1, 1, 1, 1, 0, 704, 98
44924, V, 1, 1, 1, 1, 0, 704, 98
44925, V, 1, 1, 1, 1, 0, 704, 98
44926, V, 1, 1, 1, 1, 0, 704, 98
44928, V, 1, 1, 1, 1, 0, 704, 98
44929, V, 1, 1, 1, 1, 0, 704, 98
44930, V, 1, 1, 1, 1, 0, 704, 98
44931, V, 1, 1, 1, 1, 0, 704, 98
44932, V, 1, 1, 1, 1, 0, 704, 98
44933, V, 1, 1, 1, 1, 0, 704, 98
44934, V, 1, 1, 1, 1, 0, 704, 98
44935, V, 1, 1, 1, 1, 0, 704, 98
44936, V, 1, 1, 1, 1, 0, 704, 98
44937, V, 1, 1, 1, 1, 0, 704, 98
44938, V, 1, 1, 1, 1, 0, 704, 98
44939, V, 1, 1, 1, 1, 0, 704, 98
44940, V, 1, 1, 1, 1, 0, 704, 98
44941, V, 1, 1, 1, 1, 0, 704, 98
44942, V, 1, 1, 1, 1, 0, 704, 98
44943, V, 1, 1, 1, 1, 0, 704, 98
44944, V, 1, 1, 1, 1, 0, 704, 98
44945, V, 1, 1, 1, 1, 0, 704, 98
44946, V, 1, 1, 1, 1, 0, 704, 98
44947, V, 1, 1, 1, 1, 0, 704, 98
44948, V, 1, 1, 1, 1, 0, 704, 98
44949, V, 1, 1, 1, 1, 0, 704, 98
44950, V, 1, 1, 1, 1, 0, 704, 98
44951, V, 1, 1, 1, 1, 0, 704, 98
44952, V, 1, 1, 1, 1, 0, 704, 98
44953, V, 1, 1, 1, 1, 0, 704, 98
44954, V, 1, 1, 1, 1, 0, 704, 98
44955, V, 1, 1, 1, 1, 0, 704, 98
44956, V, 1, 1, 1, 1, 0, 704, 98
44957, V, 1, 1, 1, 1, 0, 704, 98
44958, V, 1, 1, 1, 1, 0, 704, 98
44959, V, 1, 1, 1, 1, 0, 704, 98
44960, V, 1, 1, 1, 1, 0, 704, 98
44961, V, 1, 1, 1, 1, 0, 704, 98
44962, V, 1, 1, 1, 1, 0, 704, 98
44963, V, 1, 1, 1, 1, 0, 704, 98
44964, V, 1, 1, 1, 1, 0, 704, 98
44965, V, 1, 1, 1, 1, 0, 704, 98
44966, V, 1, 1, 1, 1, 0, 704, 98
44967, V, 1, 1, 1, 1, 0, 704, 98
44968, V, 1, 1, 1, 1, 0, 704, 98
44969, V, 1, 1, 1, 1, 0, 704, 98
44971, V, 1, 1, 1, 1, 0, 704, 98
44972, V, 1, 1, 1, 1, 0, 704, 98
44973, V, 1, 1, 1, 1, 0, 704, 98
44974, V, 1, 1, 1, 1, 0, 704, 98
44975, V, 1, 1, 1, 1, 0, 704, 98
44976, V, 1, 1, 1, 1, 0, 704, 98
44977, V, 1, 1, 1, 1, 0, 704, 98
44978, V, 1, 1, 1, 1, 0, 704, 98
44979, V, 1, 1, 1, 1, 0, 704, 98
44980, V, 1, 1, 1, 1, 0, 704, 98
44981, V, 1, 1, 1, 1, 0, 704, 98
44982, V, 1, 1, 1, 1, 0, 704, 98
44983, V, 1, 1, 1, 1, 0, 704, 98
44984, V, 1, 1, 1, 1, 0, 704, 98
44985, V, 1, 1, 1, 1, 0, 704, 98
44986, V, 1, 1, 1, 1, 0, 704, 98
44987, V, 1, 1, 1, 1, 0, 704, 98
44988, V, 1, 1, 1, 1, 0, 704, 98
44989, V, 1, 1, 1, 1, 0, 704, 98
44990, V, 1, 1, 1, 1, 0, 704, 98
44991, V, 1, 1, 1, 1, 0, 704, 98
44992, V, 1, 1, 1, 1, 0, 704, 98
44993, V, 1, 1, 1, 1, 0, 704, 98
44994, V, 1, 1, 1, 1, 0, 704, 98
44995, V, 1, 1, 1, 1, 0, 704, 98
44996, V, 1, 1, 1, 1, 0, 704, 98
44997, V, 1, 1, 1, 1, 0, 704, 98
44998, V, 1, 1, 1, 1, 0, 704, 98
44999, V, 1, 1, 1, 1, 0, 704, 98
45000, V, 1, 1, 1, 1, 0, 704, 98
45001, V, 1, 1, 1, 1, 0, 704, 98
45002, V, 1, 1, 1, 1, 0, 704, 98
45003, V, 1, 1, 1, 1, 0, 704, 98
45004, V, 1, 1, 1, 1, 0, 704, 98
45005, V, 1, 1, 1, 1, 0, 704, 98
45006, V, 1, 1, 1, 1, 0, 704, 98
45007, V, 1, 1, 1, 1, 0, 704, 98
45008, V, 1, 1, 1, 1, 0, 704, 98
45009, V, 1, 1, 1, 1, 0, 704, 98
45010, V, 1, 1, 1, 1, 0, 704, 98
45011, V, 1, 1, 1, 1, 0, 704, 98
45012, V, 1, 1, 1, 1, 0, 704, 98
45014, V, 1, 1, 1, 1, 0, 704, 98
45015, V, 1, 1, 1, 1, 0, 704, 98
45016, V, 1, 1, 1, 1, 0, 704, 98
45017, V, 1, 1, 1, 1, 0, 704, 98
45018, V, 1, 1, 1, 1, 0, 704, 98
45019, V, 1, 1, 1, 1, 0, 704, 98
45020, V, 1, 1, 1, 1, 0, 704, 98
45021, V, 1, 1, 1, 1, 0, 704, 98
45022, V, 1, 1, 1, 1, 0, 704, 98
45023, V, 1, 1, 1, 1, 0, 704, 98
45024, V, 1, 1, 1, 1, 0, 704, 98
45025, V, 1, 1, 1, 1, 0, 704, 98
45026, V, 1, 1, 1, 1, 0, 704, 98
45027, V, 1, 1, 1, 1, 0, 704, 98
45028, V, 1, 1, 1, 1, 0, 704, 98
45029, V, 1, 1, 1, 1, 0, 704, 98
45030, V, 1, 1, 1, 1, 0, 704, 98
45031, V, 1, 1, 1, 1, 0, 704, 98
45032, V, 1, 1, 1, 1, 0, 704, 98
45033, V, 1, 1, 1, 1, 0, 704, 98
45034, V, 1, 1, 1, 1, 0, 704, 98
45035, V, 1, 1, 1, 1, 0, 704, 98
45036, V, 1, 1, 1, 1, 0, 704, 98
45037, V, 1, 1, 1, 1, 0, 704, 98
45038, V, 1, 1, 1, 1, 0, 704, 98
45039, V, 1, 1, 1, 1, 0, 704, 98
45040, V, 1, 1, 1, 1, 0, 704, 98
45041, V, 1, 1, 1, 1, 0, 704, 98
45042, V, 1, 1, 1, 1, 0, 704, 98
45043, V, 1, 1, 1, 1, 0, 704, 98
45044, V, 1, 1, 1, 1, 0, 704, 98
45045, V, 1, 1, 1, 1, 0, 704, 98
45046, V, 1, 1, 1, 1, 0, 704, 98
45047, V, 1, 1, 1, 1, 0, 704, 98
45048, V, 1, 1, 1, 1, 0, 704, 98
45049, V, 1, 1, 1, 1, 0, 704, 98
45050, V, 1, 1, 1, 1, 0, 704, 98
45051, V, 1, 1, 1, 1, 0, 704, 98
45052, V, 1, 1, 1, 1, 0, 704, 98
45053, V, 1, 1, 1, 1, 0, 704, 98
45054, V, 1, 1, 1, 1, 0, 704, 98
45056, V, 1, 1, 1, 1, 0, 704, 98
45057, V, 1, 1, 1, 1, 0, 704, 98
45058, V, 1, 1, 1, 1, 0, 704, 98
45059, V, 1, 1, 1, 1, 0, 704, 98
45060, V, 1, 1, 1, 1, 0, 704, 98
45061, V, 1, 1, 1, 1, 0, 704, 98
45062, V, 1, 1, 1, 1, 0, 704, 98
45063, V, 1, 1, 1, 1, 0, 704, 98
45064, V, 1, 1, 1, 1, 0, 704, 98
45065, V, 1, 1, 1, 1, 0, 704, 98
45066, V, 1, 1, 1, 1, 0, 704, 98
45067, V, 1, 1, 1, 1, 0, 704, 98
45068, V, 1, 1, 1, 1, 0, 704, 98
45069, V, 1, 1, 1, 1, 0, 704, 98
45070, V, 1, 1, 1, 1, 0, 704, 98
45071, V, 1, 1, 1, 1, 0, 704, 98
45072, V, 1, 1, 1, 1, 0, 704, 98
45073, V, 1, 1, 1, 1, 0, 704, 98
45074, V, 1, 1, 1, 1, 0, 704, 98
45075, V, 1, 1, 1, 1, 0, 704, 98
45076, V, 1, 1, 1, 1, 0, 704, 98
45077, V, 1, 1, 1, 1, 0, 704, 98
45078, V, 1, 1, 1, 1, 0, 704, 98
45079, V, 1, 1, 1, 1, 0, 704, 98
45080, V, 1, 1, 1, 1, 0, 704, 98
45081, V, 1, 1, 1, 1, 0, 704, 99
45082, V, 1, 1, 1, 1, 0, 704, 98
45083, V, 1, 1, 1, 1, 0, 704, 98
45084, V, 1, 1, 1, 1, 0, 704, 98
45085, V, 1, 1, 1, 1, 0, 704, 98
45086, V, 1, 1, 1, 1, 0, 704, 98
45087, V, 1, 1, 1, 1, 0, 704, 98
45088, V, 1, 1, 1, 1, 0, 704, 98
45089, V, 1, 1, 1, 1, 0, 704, 98
45090, V, 1, 1, 1, 1, 0, 704, 98
45091, V, 1, 1, 1, 1, 0, 704, 98
45092, V, 1, 1, 1, 1, 0, 704, 98
45093, V, 1, 1, 1, 1, 0, 704, 98
45094, V, 1, 1, 1, 1, 0, 704, 98
45095, V, 1, 1, 1, 1, 0, 704, 98
45096, V, 1, 1, 1, 1, 0, 704, 98
45097, V, 1, 1, 1, 1, 0, 704, 98
45099, V, 1, 1, 1, 1, 0, 704, 98
45100, V, 1, 1, 1, 1, 0, 704, 98
45101, V, 1, 1, 1, 1, 0, 704, 98
45102, V, 1, 1, 1, 1, 0, 704, 98
45103, V, 1, 1, 1, 1, 0, 704, 98
45104, V, 1, 1, 1, 1, 0, 704, 98
45105, V, 1, 1, 1, 1, 0, 704, 98
45106, V, 1, 1, 1, 1, 0, 704, 98
45107, V, 1, 1, 1, 1, 0, 704, 98
45108, V, 1, 1, 1, 1, 0, 704, 98
45109, V, 1, 1, 1, 1, 0, 704, 98
45110, V, 1, 1, 1, 1, 0, 704, 98
45111, V, 1, 1, 1, 1, 0, 704, 98
45112, V, 1, 1, 1, 1, 0, 704, 98
45113, V, 1, 1, 1, 1, 0, 704, 98
45114, V, 1, 1, 1, 1, 0, 704, 98
45115, V, 1, 1, 1, 1, 0, 704, 98
45116, V, 1, 1, 1, 1, 0, 704, 98
45117, V, 1, 1, 1, 1, 0, 704, 98
45118, V, 1, 1, 1, 1, 0, 704, 98
45119, V, 1, 1, 1, 1, 0, 704, 98
45120, V, 1, 1, 1, 1, 0, 704, 98
45121, V, 1, 1, 1, 1, 0, 704, 98
45122, V, 1, 1, 1, 1, 0, 704, 98
45123, V, 1, 1, 1, 1, 0, 704, 98
45124, V, 1, 1, 1, 1, 0, 704, 98
45125, V, 1, 1, 1, 1, 0, 704, 98
45126, V, 1, 1, 1, 1, 0, 704, 98
45127, V, 1, 1, 1, 1, 0, 704, 98
45128, V, 1, 1, 1, 1, 0, 704, 98
45129, V, 1, 1, 1, 1, 0, 704, 98
45130, V, 1, 1, 1, 1, 0, 704, 98
45131, V, 1, 1, 1, 1, 0, 704, 98
45132, V, 1, 1, 1, 1, 0, 704, 98
45133, V, 1, 1, 1, 1, 0, 704, 98
45134, V, 1, 1, 1, 1, 0, 704, 98
45135, V, 1, 1, 1, 1, 0, 704, 98
45136, V, 1, 1, 1, 1, 0, 704, 98
45137, V, 1, 1, 1, 1, 0, 704, 98
45138, V, 1, 1, 1, 1, 0, 704, 98
45139, V, 1, 1, 1, 1, 0, 704, 98
45140, V, 1, 1, 1, 1, 0, 704, 98
45142, V, 1, 1, 1, 1, 0, 704, 98
45143, V, 1, 1, 1, 1, 0, 704, 98
45144, V, 1, 1, 1, 1, 0, 704, 98
45145, V, 1, 1, 1, 1, 0, 704, 98
45146, V, 1, 1, 1, 1, 0, 704, 98
45147, V, 1, 1, 1, 1, 0, 704, 98
45148, V, 1, 1, 1, 1, 0, 704, 98
45149, V, 1, 1, 1, 1, 0, 704, 98
45150, V, 1, 1, 1, 1, 0, 704, 98
45151, V, 1, 1, 1, 1, 0, 704, 98
45152, V, 1, 1, 1, 1, 0, 704, 98
45153, V, 1, 1, 1, 1, 0, 704, 98
45154, V, 1, 1, 1, 1, 0, 704, 98
45155, V, 1, 1, 1, 1, 0, 704, 98
45156, V, 1, 1, 1, 1, 0, 704, 98
45157, V, 1, 1, 1, 1, 0, 704, 98
45158, V, 1, 1, 1, 1, 0, 704, 98
45159, V, 1, 1, 1, 1, 0, 704, 98
45160, V, 1, 1, 1, 1, 0, 704, 98
45161, V, 1, 1, 1, 1, 0, 704, 98
45162, V, 1, 1, 1, 1, 0, 704, 98
45163, V, 1, 1, 1, 1, 0, 704, 98
45164, V, 1, 1, 1, 1, 0, 704, 98
45165, V, 1, 1, 1, 1, 0, 704, 98
45166, V, 1, 1, 1, 1, 0, 704, 98
45167, V, 1, 1, 1, 1, 0, 704, 98
45168, V, 1, 1, 1, 1, 0, 704, 98
45169, V, 1, 1, 1, 1, 0, 704, 98
45170, V, 1, 1, 1, 1, 0, 704, 98
45171, V, 1, 1, 1, 1, 0, 704, 98
45172, V, 1, 1, 1, 1, 0, 704, 98
45173, V, 1, 1, 1, 1, 0, 704, 98
45174, V, 1, 1, 1, 1, 0, 704, 98
45175, V, 1, 1, 1, 1, 0, 704, 98
45176, V, 1, 1, 1, 1, 0, 704, 98
45177, V, 1, 1, 1, 1, 0, 704, 98
45178, V, 1, 1, 1, 1, 0, 704, 98
45179, V, 1, 1, 1, 1, 0, 704, 98
45180, V, 1, 1, 1, 1, 0, 704, 98
45181, V, 1, 1, 1, 1, 0, 704, 98
45182, V, 1, 1, 1, 1, 0, 704, 98
45184, V, 1, 1, 1, 1, 0, 704, 98
45185, V, 1, 1, 1, 1, 0, 704, 98
45186, V, 1, 1, 1, 1, 0, 704, 98
45187, V, 1, 1, 1, 1, 0, 704, 98
45188, V, 1, 1, 1, 1, 0, 704, 98
45189, V, 1, 1, 1, 1, 0, 704, 98
45190, V, 1, 1, 1, 1, 0, 704, 98
45191, V, 1, 1, 1, 1, 0, 704, 98
45192, V, 1, 1, 1, 1, 0, 704, 98
45193, V, 1, 1, 1, 1, 0, 704, 98
45194, V, 1, 1, 1, 1, 0, 704, 98
45195, V, 1, 1, 1, 1, 0, 704, 98
45196, V, 1, 1, 1, 1, 0, 704, 98
45197, V, 1, 1, 1, 1, 0, 704, 98
45198, V, 1, 1, 1, 1, 0, 704, 98
45199, V, 1, 1, 1, 1, 0, 704, 98
45200, V, 1, 1, 1, 1, 0, 704, 98
45201, V, 1, 1, 1, 1, 0, 704, 98
45202, V, 1, 1, 1, 1, 0, 704, 98
45203, V, 1, 1, 1, 1, 0, 704, 98
45204, V, 1, 1, 1, 1, 0, 704, 98
45205, V, 1, 1, 1, 1, 0, 704, 98
45206, V, 1, 1, 1, 1, 0, 704, 98
45207, V, 1, 1, 1, 1, 0, 704, 98
45208, V, 1, 1, 1, 1, 0, 704, 98
45209, V, 1, 1, 1, 1, 0, 704, 98
45210, V, 1, 1, 1, 1, 0, 704, 98
45211, V, 1, 1, 1, 1, 0, 704, 98
45212, V, 1, 1, 1, 1, 0, 704, 98
45213, V, 1, 1, 1, 1, 0, 704, 98
45214, V, 1, 1, 1, 1, 0, 704, 98
45215, V, 1, 1, 1, 1, 0, 704, 98
45216, V, 1, 1, 1, 1, 0, 704, 98
45217, V, 1, 1, 1, 1, 0, 704, 98
45218, V, 1, 1, 1, 1, 0, 704, 98
45219, V, 1, 1, 1, 1, 0, 704, 98
45220, V, 1, 1, 1, 1, 0, 704, 98
45221, V, 1, 1, 1, 1, 0, 704, 98
45222, V, 1, 1, 1, 1, 0, 704, 98
45223, V, 1, 1, 1, 1, 0, 704, 98
45224, V, 1, 1, 1, 1, 0, 704, 98
45225, V, 1, 1, 1, 1, 0, 704, 98
45227, V, 1, 1, 1, 1, 0, 704, 98
45228, V, 1, 1, 1, 1, 0, 704, 98
45229, V, 1, 1, 1, 1, 0, 704, 98
45230, V, 1, 1, 1, 1, 0, 704, 98
45231, V, 1, 1, 1, 1, 0, 704, 98
45232, V, 1, 1, 1, 1, 0, 704, 98
45233, V, 1, 1, 1, 1, 0, 704, 99
45234, V, 1, 1, 1, 1, 0, 704, 98
45235, V, 1, 1, 1, 1, 0, 704, 98
45236, V, 1, 1, 1, 1, 0, 704, 98
45237, V, 1, 1, 1, 1, 0, 704, 98
45238, V, 1, 1, 1, 1, 0, 704, 98
45239, V, 1, 1, 1, 1, 0, 704, 98
45240, V, 1, 1, 1, 1, 0, 704, 98
45241, V, 1, 1, 1, 1, 0, 704, 98
45242, V, 1, 1, 1, 1, 0, 704, 98
45243, V, 1, 1, 1, 1, 0, 704, 98
45244, V, 1, 1, 1, 1, 0, 704, 98
45245, V, 1, 1, 1, 1, 0, 704, 98
45246, V, 1, 1, 1, 1, 0, 704, 98
45247, V, 1, 1, 1, 1, 0, 704, 99
45248, V, 1, 1, 1, 1, 0, 704, 98
45249, V, 1, 1, 1, 1, 0, 704, 98
45250, V, 1, 1, 1, 1, 0, 704, 98
45251, V, 1, 1, 1, 1, 0, 704, 98
45252, V, 1, 1, 1, 1, 0, 704, 98
45253, V, 1, 1, 1, 1, 0, 704, 98
45254, V, 1, 1, 1, 1, 0, 704, 98
45255, V, 1, 1, 1, 1, 0, 704, 98
45256, V, 1, 1, 1, 1, 0, 704, 98
45257, V, 1, 1, 1, 1, 0, 704, 98
45258, V, 1, 1, 1, 1, 0, 704, 98
45259, V, 1, 1, 1, 1, 0, 704, 98
45260, V, 1, 1, 1, 1, 0, 704, 98
45261, V, 1, 1, 1, 1, 0, 704, 98
45262, V, 1, 1, 1, 1, 0, 704, 98
45263, V, 1, 1, 1, 1, 0, 704, 98
45264, V, 1, 1, 1, 1, 0, 704, 98
45265, V, 1, 1, 1, 1, 0, 704, 98
45266, V, 1, 1, 1, 1, 0, 704, 98
45267, V, 1, 1, 1, 1, 0, 704, 98
45268, V, 1, 1, 1, 1, 0, 704, 98
45270, V, 1, 1, 1, 1, 0, 704, 98
45271, V, 1, 1, 1, 1, 0, 704, 98
45272, V, 1, 1, 1, 1, 0, 704, 98
45273, V, 1, 1, 1, 1, 0, 704, 98
45274, V, 1, 1, 1, 1, 0, 704, 98
45275, V, 1, 1, 1, 1, 0, 704, 98
45276, V, 1, 1, 1, 1, 0, 704, 98
45277, V, 1, 1, 1, 1, 0, 704, 98
45278, V, 1, 1, 1, 1, 0, 704, 98
45279, V, 1, 1, 1, 1, 0, 704, 98
45280, V, 1, 1, 1, 1, 0, 704, 98
45281, V, 1, 1, 1, 1, 0, 704, 98
45282, V, 1, 1, 1, 1, 0, 704, 98
45283, V, 1, 1, 1, 1, 0, 704, 98
45284, V, 1, 1, 1, 1, 0, 704, 98
45285, V, 1, 1, 1, 1, 0, 704, 98
45286, V, 1, 1, 1, 1, 0, 704, 98
45287, V, 1, 1, 1, 1, 0, 704, 98
45288, V, 1, 1, 1, 1, 0, 704, 98
45289, V, 1, 1, 1, 1, 0, 704, 98
45290, V, 1, 1, 1, 1, 0, 704, 98
45291, V, 1, 1, 1, 1, 0, 704, 98
45292, V, 1, 1, 1, 1, 0, 704, 98
45293, V, 1, 1, 1, 1, 0, 704, 98
45294, V, 1, 1, 1, 1, 0, 704, 98
45295, V, 1, 1, 1, 1, 0, 704, 98
45296, V, 1, 1, 1, 1, 0, 704, 98
45297, V, 1, 1, 1, 1, 0, 704, 98
45298, V, 1, 1, 1, 1, 0, 704, 98
45299, V, 1, 1, 1, 1, 0, 704, 98
45300, V, 1, 1, 1, 1, 0, 704, 98
45301, V, 1, 1, 1, 1, 0, 704, 98
45302, V, 1, 1, 1, 1, 0, 704, 98
45303, V, 1, 1, 1, 1, 0, 704, 98
45304, V, 1, 1, 1, 1, 0, 704, 98
45305, V, 1, 1, 1, 1, 0, 704, 98
45306, V, 1, 1, 1, 1, 0, 704, 98
45307, V, 1, 1, 1, 1, 0, 704, 98
45308, V, 1, 1, 1, 1, 0, 704, 98
45309, V, 1, 1, 1, 1, 0, 704, 98
45310, V, 1, 1, 1, 1, 0, 704, 98
45312, V, 1, 1, 1, 1, 0, 704, 98
45313, V, 1, 1, 1, 1, 0, 704, 98
45314, V, 1, 1, 1, 1, 0, 704, 98
45315, V, 1, 1, 1, 1, 0, 704, 98
45316, V, 1, 1, 1, 1, 0, 704, 98
45317, V, 1, 1, 1, 1, 0, 704, 98
45318, V, 1, 1, 1, 1, 0, 704, 98
45319, V, 1, 1, 1, 1, 0, 704, 98
45320, V, 1, 1, 1, 1, 0, 704, 98
45321, V, 1, 1, 1, 1, 0, 704, 98
45322, V, 1, 1, 1, 1, 0, 704, 98
45323, V, 1, 1, 1, 1, 0, 704, 98
45324, V, 1, 1, 1, 1, 0, 704, 98
45325, V, 1, 1, 1, 1, 0, 704, 98
45326, V, 1, 1, 1, 1, 0, 704, 98
45327, V, 1, 1, 1, 1, 0, 704, 98
45328, V, 1, 1, 1, 1, 0, 704, 98
45329, V, 1, 1, 1, 1, 0, 704, 98
45330, V, 1, 1, 1, 1, 0, 704, 98
45331, V, 1, 1, 1, 1, 0, 704, 98
45332, V, 1, 1, 1, 1, 0, 704, 98
45333, V, 1, 1, 1, 1, 0, 704, 98
45334, V, 1, 1, 1, 1, 0, 704, 98
45335, V, 1, 1, 1, 1, 0, 704, 98
45336, V, 1, 1, 1, 1, 0, 704, 98
45337, V, 1, 1, 1, 1, 0, 704, 98
45338, V, 1, 1, 1, 1, 0, 704, 98
45339, V, 1, 1, 1, 1, 0, 704, 98
45340, V, 1, 1, 1, 1, 0, 704, 98
45341, V, 1, 1, 1, 1, 0, 704, 98
45342, V, 1, 1, 1, 1, 0, 704, 98
45343, V, 1, 1, 1, 1, 0, 704, 98
45344, V, 1, 1, 1, 1, 0, 704, 98
45345, V, 1, 1, 1, 1, 0, 704, 98
45346, V, 1, 1, 1, 1, 0, 704, 98
45347, V, 1, 1, 1, 1, 0, 704, 98
45348, V, 1, 1, 1, 1, 0, 704, 98
45349, V, 1, 1, 1, 1, 0, 704, 98
45350, V, 1, 1, 1, 1, 0, 704, 98
45351, V, 1, 1, 1, 1, 0, 704, 98
45352, V, 1, 1, 1, 1, 0, 704, 98
45353, V, 1, 1, 1, 1, 0, 704, 98
45355, V, 1, 1, 1, 1, 0, 704, 98
45356, V, 1, 1, 1, 1, 0, 704, 98
45357, V, 1, 1, 1, 1, 0, 704, 98
45358, V, 1, 1, 1, 1, 0, 704, 98
45359, V, 1, 1, 1, 1, 0, 704, 98
45360, V, 1, 1, 1, 1, 0, 704, 98
45361, V, 1, 1, 1, 1, 0, 704, 98
45362, V, 1, 1, 1, 1, 0, 704, 98
45363, V, 1, 1, 1, 1, 0, 704, 98
45364, V, 1, 1, 1, 1, 0, 704, 98
45365, V, 1, 1, 1, 1, 0, 704, 98
45366, V, 1, 1, 1, 1, 0, 704, 98
45367, V, 1, 1, 1, 1, 0, 704, 98
45368, V, 1, 1, 1, 1, 0, 704, 98
45369, V, 1, 1, 1, 1, 0, 704, 98
45370, V, 1, 1, 1, 1, 0, 704, 98
45371, V, 1, 1, 1, 1, 0, 704, 98
45372, V, 1, 1, 1, 1, 0, 704, 98
45373, V, 1, 1, 1, 1, 0, 704, 98
45374, V, 1, 1, 1, 1, 0, 704, 98
45375, V, 1, 1, 1, 1, 0, 704, 98
45376, V, 1, 1, 1, 1, 0, 704, 98
45377, V, 1, 1, 1, 1, 0, 704, 98
45378, V, 1, 1, 1, 1, 0, 704, 98
45379, V, 1, 1, 1, 1, 0, 704, 98
45380, V, 1, 1, 1, 1, 0, 704, 98
45381, V, 1, 1, 1, 1, 0, 704, 98
45382, V, 1, 1, 1, 1, 0, 704, 98
45383, V, 1, 1, 1, 1, 0, 704, 98
45384, V, 1, 1, 1, 1, 0, 704, 98
45385, V, 1, 1, 1, 1, 0, 704, 98
45386, V, 1, 1, 1, 1, 0, 704, 98
45387, V, 1, 1, 1, 1, 0, 704, 98
45388, V, 1, 1, 1, 1, 0, 704, 98
45389, V, 1, 1, 1, 1, 0, 704, 98
45390, V, 1, 1, 1, 1, 0, 704, 98
45391, V, 1, 1, 1, 1, 0, 704, 98
45392, V, 1, 1, 1, 1, 0, 704, 98
45393, V, 1, 1, 1, 1, 0, 704, 98
45394, V, 1, 1, 1, 1, 0, 704, 98
45395, V, 1, 1, 1, 1, 0, 704, 98
45396, V, 1, 1, 1, 1, 0, 704, 98
45398, V, 1, 1, 1, 1, 0, 704, 98
45399, V, 1, 1, 1, 1, 0, 704, 98
45400, V, 1, 1, 1, 1, 0, 704, 98
45401, V, 1, 1, 1, 1, 0, 704, 98
45402, V, 1, 1, 1, 1, 0, 704, 98
45403, V, 1, 1, 1, 1, 0, 704, 98
45404, V, 1, 1, 1, 1, 0, 704, 98
45405, V, 1, 1, 1, 1, 0, 704, 98
45406, V, 1, 1, 1, 1, 0, 704, 98
45407, V, 1, 1, 1, 1, 0, 704, 98
45408, V, 1, 1, 1, 1, 0, 704, 98
45409, V, 1, 1, 1, 1, 0, 704, 98
45410, V, 1, 1, 1, 1, 0, 704, 98
45411, V, 1, 1, 1, 1, 0, 704, 98
45412, V, 1, 1, 1, 1, 0, 704, 98
45413, V, 1, 1, 1, 1, 0, 704, 98
45414, V, 1, 1, 1, 1, 0, 704, 98
45415, V, 1, 1, 1, 1, 0, 704, 98
45416, V, 1, 1, 1, 1, 0, 704, 98
45417, V, 1, 1, 1, 1, 0, 704, 98
45418, V, 1, 1, 1, 1, 0, 704, 98
45419, V, 1, 1, 1, 1, 0, 704, 98
45420, V, 1, 1, 1, 1, 0, 704, 98
45421, V, 1, 1, 1, 1, 0, 704, 98
45422, V, 1, 1, 1, 1, 0, 704, 98
45423, V, 1, 1, 1, 1, 0, 704, 98
45424, V, 1, 1, 1, 1, 0, 704, 98
45425, V, 1, 1, 1, 1, 0, 704, 98
45426, V, 1, 1, 1, 1, 0, 704, 98
45427, V, 1, 1, 1, 1, 0, 704, 98
45428, V, 1, 1, 1, 1, 0, 704, 98
45429, V, 1, 1, 1, 1, 0, 704, 98
45430, V, 1, 1, 1, 1, 0, 704, 98
45431, V, 1, 1, 1, 1, 0, 704, 98
45432, V, 1, 1, 1, 1, 0, 704, 98
45433, V, 1, 1, 1, 1, 0, 704, 98
45434, V, 1, 1, 1, 1, 0, 704, 98
45435, V, 1, 1, 1, 1, 0, 704, 98
45436, V, 1, 1, 1, 1, 0, 704, 98
45437, V, 1, 1, 1, 1, 0, 704, 98
45438, V, 1, 1, 1, 1, 0, 704, 98
45440, V, 1, 1, 1, 1, 0, 704, 98
45441, V, 1, 1, 1, 1, 0, 704, 98
45442, V, 1, 1, 1, 1, 0, 704, 98
45443, V, 1, 1, 1, 1, 0, 704, 98
45444, V, 1, 1, 1, 1, 0, 704, 98
45445, V, 1, 1, 1, 1, 0, 704, 98
45446, V, 1, 1, 1, 1, 0, 704, 98
45447, V, 1, 1, 1, 1, 0, 704, 98
45448, V, 1, 1, 1, 1, 0, 704, 98
45449, V, 1, 1, 1, 1, 0, 704, 98
45450, V, 1, 1, 1, 1, 0, 704, 98
45451, V, 1, 1, 1, 1, 0, 704, 98
45452, V, 1, 1, 1, 1, 0, 704, 98
45453, V, 1, 1, 1, 1, 0, 704, 98
45454, V, 1, 1, 1, 1, 0, 704, 98
45455, V, 1, 1, 1, 1, 0, 704, 98
45456, V, 1, 1, 1, 1, 0, 704, 98
45457, V, 1, 1, 1, 1, 0, 704, 98
45458, V, 1, 1, 1, 1, 0, 704, 98
45459, V, 1, 1, 1, 1, 0, 704, 98
45460, V, 1, 1, 1, 1, 0, 704, 98
45461, V, 1, 1, 1, 1, 0, 704, 98
45462, V, 1, 1, 1, 1, 0, 704, 98
45463, V, 1, 1, 1, 1, 0, 704, 98
45464, V, 1, 1, 1, 1, 0, 704, 98
45465, V, 1, 1, 1, 1, 0, 704, 98
45466, V, 1, 1, 1, 1, 0, 704, 98
45467, V, 1, 1, 1, 1, 0, 704, 98
45468, V, 1, 1, 1, 1, 0, 704, 98
45469, V, 1, 1, 1, 1, 0, 704, 98
45470, V, 1, 1, 1, 1, 0, 704, 98
45471, V, 1, 1, 1, 1, 0, 704, 98
45472, V, 1, 1, 1, 1, 0, 704, 98
45473, V, 1, 1, 1, 1, 0, 704, 98
45474, V, 1, 1, 1, 1, 0, 704, 98
45475, V, 1, 1, 1, 1, 0, 704, 98
45476, V, 1, 1, 1, 1, 0, 704, 98
45477, V, 1, 1, 1, 1, 0, 704, 98
45478, V, 1, 1, 1, 1, 0, 704, 98
45479, V, 1, 1, 1, 1, 0, 704, 98
45480, V, 1, 1, 1, 1, 0, 704, 98
45481, V, 1, 1, 1, 1, 0, 704, 98
45483, V, 1, 1, 1, 1, 0, 704, 98
45484, V, 1, 1, 1, 1, 0, 704, 98
45485, V, 1, 1, 1, 1, 0, 704, 98
45486, V, 1, 1, 1, 1, 0, 704, 98
45487, V, 1, 1, 1, 1, 0, 704, 98
45488, V, 1, 1, 1, 1, 0, 704, 98
45489, V, 1, 1, 1, 1, 0, 704, 98
45490, V, 1, 1, 1, 1, 0, 704, 98
45491, V, 1, 1, 1, 1, 0, 704, 98
45492, V, 1, 1, 1, 1, 0, 704, 98
45493, V, 1, 1, 1, 1, 0, 704, 98
45494, V, 1, 1, 1, 1, 0, 704, 98
45495, V, 1, 1, 1, 1, 0, 704, 98
45496, V, 1, 1, 1, 1, 0, 704, 98
45497, V, 1, 1, 1, 1, 0, 704, 98
45498, V, 1, 1, 1, 1, 0, 704, 98
45499, V, 1, 1, 1, 1, 0, 704, 98
45500, V, 1, 1, 1, 1, 0, 704, 98
45501, V, 1, 1, 1, 1, 0, 704, 98
45502, V, 1, 1, 1, 1, 0, 704, 98
45503, V, 1, 1, 1, 1, 0, 704, 98
45504, V, 1, 1, 1, 1, 0, 704, 98
45505, V, 1, 1, 1, 1, 0, 704, 98
45506, V, 1, 1, 1, 1, 0, 704, 98
45507, V, 1, 1, 1, 1, 0, 704, 98
45508, V, 1, 1, 1, 1, 0, 704, 98
45509, V, 1, 1, 1, 1, 0, 704, 98
45510, V, 1, 1, 1, 1, 0, 704, 98
45511, V, 1, 1, 1, 1, 0, 704, 98
45512, V, 1, 1, 1, 1, 0, 704, 98
45513, V, 1, 1, 1, 1, 0, 704, 98
45514, V, 1, 1, 1, 1, 0, 704, 98
45515, V, 1, 1, 1, 1, 0, 704, 98
45516, V, 1, 1, 1, 1, 0, 704, 98
45517, V, 1, 1, 1, 1, 0, 704, 98
45518, V, 1, 1, 1, 1, 0, 704, 98
45519, V, 1, 1, 1, 1, 0, 704, 98
45520, V, 1, 1, 1, 1, 0, 704, 98
45521, V, 1, 1, 1, 1, 0, 704, 98
45522, V, 1, 1, 1, 1, 0, 704, 98
45523, V, 1, 1, 1, 1, 0, 704, 98
45524, V, 1, 1, 1, 1, 0, 704, 98
45526, V, 1, 1, 1, 1, 0, 704, 98
45527, V, 1, 1, 1, 1, 0, 704, 98
45528, V, 1, 1, 1, 1, 0, 704, 98
45529, V, 1, 1, 1, 1, 0, 704, 98
45530, V, 1, 1, 1, 1, 0, 704, 98
45531, V, 1, 1, 1, 1, 0, 704, 98
45532, V, 1, 1, 1, 1, 0, 704, 98
45533, V, 1, 1, 1, 1, 0, 704, 98
45534, V, 1, 1, 1, 1, 0, 704, 98
45535, V, 1, 1, 1, 1, 0, 704, 98
45536, V, 1, 1, 1, 1, 0, 704, 98
45537, V, 1, 1, 1, 1, 0, 704, 98
45538, V, 1, 1, 1, 1, 0, 704, 98
45539, V, 1, 1, 1, 1, 0, 704, 98
45540, V, 1, 1, 1, 1, 0, 704, 98
45541, V, 1, 1, 1, 1, 0, 704, 98
45542, V, 1, 1, 1, 1, 0, 704, 98
45543, V, 1, 1, 1, 1, 0, 704, 98
45544, V, 1, 1, 1, 1, 0, 704, 98
45545, V, 1, 1, 1, 1, 0, 704, 98
45546, V, 1, 1, 1, 1, 0, 704, 98
45547, V, 1, 1, 1, 1, 0, 704, 98
45548, V, 1, 1, 1, 1, 0, 704, 98
45549, V, 1, 1, 1, 1, 0, 704, 98
45550, V, 1, 1, 1, 1, 0, 704, 98
45551, V, 1, 1, 1, 1, 0, 704, 98
45552, V, 1, 1, 1, 1, 0, 704, 98
45553, V, 1, 1, 1, 1, 0, 704, 98
45554, V, 1, 1, 1, 1, 0, 704, 98
45555, V, 1, 1, 1, 1, 0, 704, 98
45556, V, 1, 1, 1, 1, 0, 704, 98
45557, V, 1, 1, 1, 1, 0, 704, 98
45558, V, 1, 1, 1, 1, 0, 704, 98
45559, V, 1, 1, 1, 1, 0, 704, 98
45560, V, 1, 1, 1, 1, 0, 704, 98
45561, V, 1, 1, 1, 1, 0, 704, 98
45562, V, 1, 1, 1, 1, 0, 704, 98
45563, V, 1, 1, 1, 1, 0, 704, 98
45564, V, 1, 1, 1, 1, 0, 704, 98
45565, V, 1, 1, 1, 1, 0, 704, 98
45566, V, 1, 1, 1, 1, 0, 704, 98
45568, V, 1, 1, 1, 1, 0, 704, 98
45569, V, 1, 1, 1, 1, 0, 704, 98
45570, V, 1, 1, 1, 1, 0, 704, 98
45571, V, 1, 1, 1, 1, 0, 704, 98
45572, V, 1, 1, 1, 1, 0, 704, 98
45573, V, 1, 1, 1, 1, 0, 704, 98
45574, V, 1, 1, 1, 1, 0, 704, 98
45575, V, 1, 1, 1, 1, 0, 704, 98
45576, V, 1, 1, 1, 1, 0, 704, 98
45577, V, 1, 1, 1, 1, 0, 704, 98
45578, V, 1, 1, 1, 1, 0, 704, 98
45579, V, 1, 1, 1, 1, 0, 704, 98
45580, V, 1, 1, 1, 1, 0, 704, 98
45581, V, 1, 1, 1, 1, 0, 704, 98
45582, V, 1, 1, 1, 1, 0, 704, 98
45583, V, 1, 1, 1, 1, 0, 704, 98
45584, V, 1, 1, 1, 1, 0, 704, 98
45585, V, 1, 1, 1, 1, 0, 704, 98
45586, V, 1, 1, 1, 1, 0, 704, 98
45587, V, 1, 1, 1, 1, 0, 704, 98
45588, V, 1, 1, 1, 1, 0, 704, 98
45589, V, 1, 1, 1, 1, 0, 704, 98
45590, V, 1, 1, 1, 1, 0, 704, 98
45591, V, 1, 1, 1, 1, 0, 704, 98
45592, V, 1, 1, 1, 1, 0, 704, 98
45593, V, 1, 1, 1, 1, 0, 704, 98
45594, V, 1, 1, 1, 1, 0, 704, 98
45595, V, 1, 1, 1, 1, 0, 704, 98
45596, V, 1, 1, 1, 1, 0, 704, 98
45597, V, 1, 1, 1, 1, 0, 704, 98
45598, V, 1, 1, 1, 1, 0, 704, 98
45599, V, 1, 1, 1, 1, 0, 704, 98
45600, V, 1, 1, 1, 1, 0, 704, 98
45601, V, 1, 1, 1, 1, 0, 704, 98
45602, V, 1, 1, 1, 1, 0, 704, 98
45603, V, 1, 1, 1, 1, 0, 704, 98
45604, V, 1, 1, 1, 1, 0, 704, 98
45605, V, 1, 1, 1, 1, 0, 704, 98
45606, V, 1, 1, 1, 1, 0, 704, 98
45607, V, 1, 1, 1, 1, 0, 704, 98
45608, V, 1, 1, 1, 1, 0, 704, 98
45609, V, 1, 1, 1, 1, 0, 704, 98
45611, V, 1, 1, 1, 1, 0, 704, 98
45612, V, 1, 1, 1, 1, 0, 704, 98
45613, V, 1, 1, 1, 1, 0, 704, 98
45614, V, 1, 1, 1, 1, 0, 704, 98
45615, V, 1, 1, 1, 1, 0, 704, 98
45616, V, 1, 1, 1, 1, 0, 704, 98
45617, V, 1, 1, 1, 1, 0, 704, 98
45618, V, 1, 1, 1, 1, 0, 704, 98
45619, V, 1, 1, 1, 1, 0, 704, 98
45620, V, 1, 1, 1, 1, 0, 704, 98
45621, V, 1, 1, 1, 1, 0, 704, 98
45622, V, 1, 1, 1, 1, 0, 704, 98
45623, V, 1, 1, 1, 1, 0, 704, 98
45624, V, 1, 1, 1, 1, 0, 704, 98
45625, V, 1, 1, 1, 1, 0, 704, 98
45626, V, 1, 1, 1, 1, 0, 704, 98
45627, V, 1, 1, 1, 1, 0, 704, 98
45628, V, 1, 1, 1, 1, 0, 704, 98
45629, V, 1, 1, 1, 1, 0, 704, 98
45630, V, 1, 1, 1, 1, 0, 704, 98
45631, V, 1, 1, 1, 1, 0, 704, 98
45632, V, 1, 1, 1, 1, 0, 704, 98
45633, V, 1, 1, 1, 1, 0, 704, 98
45634, V, 1, 1, 1, 1, 0, 704, 98
45635, V, 1, 1, 1, 1, 0, 704, 98
45636, V, 1, 1, 1, 1, 0, 704, 98
45637, V, 1, 1, 1, 1, 0, 704, 98
45638, V, 1, 1, 1, 1, 0, 704, 98
45639, V, 1, 1, 1, 1, 0, 704, 98
45640, V, 1, 1, 1, 1, 0, 704, 98
45641, V, 1, 1, 1, 1, 0, 704, 98
45642, V, 1, 1, 1, 1, 0, 704, 98
45643, V, 1, 1, 1, 1, 0, 704, 98
45644, V, 1, 1, 1, 1, 0, 704, 98
45645, V, 1, 1, 1, 1, 0, 704, 98
45646, V, 1, 1, 1, 1, 0, 704, 98
45647, V, 1, 1, 1, 1, 0, 704, 98
45648, V, 1, 1, 1, 1, 0, 704, 98
45649, V, 1, 1, 1, 1, 0, 704, 98
45650, V, 1, 1, 1, 1, 0, 704, 98
45651, V, 1, 1, 1, 1, 0, 704, 98
45652, V, 1, 1, 1, 1, 0, 704, 98
45654, V, 1, 1, 1, 1, 0, 704, 98
45655, V, 1, 1, 1, 1, 0, 704, 98
45656, V, 1, 1, 1, 1, 0, 704, 98
45657, V, 1, 1, 1, 1, 0, 704, 98
45658, V, 1, 1, 1, 1, 0, 704, 98
45659, V, 1, 1, 1, 1, 0, 704, 98
45660, V, 1, 1, 1, 1, 0, 704, 98
45661, V, 1, 1, 1, 1, 0, 704, 98
45662, V, 1, 1, 1, 1, 0, 704, 98
45663, V, 1, 1, 1, 1, 0, 704, 98
45664, V, 1, 1, 1, 1, 0, 704, 98
45665, V, 1, 1, 1, 1, 0, 704, 98
45666, V, 1, 1, 1, 1, 0, 704, 98
45667, V, 1, 1, 1, 1, 0, 704, 98
45668, V, 1, 1, 1, 1, 0, 704, 98
45669, V, 1, 1, 1, 1, 0, 704, 98
45670, V, 1, 1, 1, 1, 0, 704, 98
45671, V, 1, 1, 1, 1, 0, 704, 98
45672, V, 1, 1, 1, 1, 0, 704, 98
45673, V, 1, 1, 1, 1, 0, 704, 98
45674, V, 1, 1, 1, 1, 0, 704, 98
45675, V, 1, 1, 1, 1, 0, 704, 98
45676, V, 1, 1, 1, 1, 0, 704, 98
45677, V, 1, 1, 1, 1, 0, 704, 98
45678, V, 1, 1, 1, 1, 0, 704, 98
45679, V, 1, 1, 1, 1, 0, 704, 98
45680, V, 1, 1, 1, 1, 0, 704, 98
45681, V, 1, 1, 1, 1, 0, 704, 98
45682, V, 1, 1, 1, 1, 0, 704, 98
45683, V, 1, 1, 1, 1, 0, 704, 98
45684, V, 1, 1, 1, 1, 0, 704, 98
45685, V, 1, 1, 1, 1, 0, 704, 98
45686, V, 1, 1, 1, 1, 0, 704, 98
45687, V, 1, 1, 1, 1, 0, 704, 98
45688, V, 1, 1, 1, 1, 0, 704, 98
45689, V, 1, 1, 1, 1, 0, 704, 98
45690, V, 1, 1, 1, 1, 0, 704, 98
45691, V, 1, 1, 1, 1, 0, 704, 98
45692, V, 1, 1, 1, 1, 0, 704, 98
45693, V, 1, 1, 1, 1, 0, 704, 98
45694, V, 1, 1, 1, 1, 0, 704, 98
45696, V, 1, 1, 1, 1, 0, 704, 98
45697, V, 1, 1, 1, 1, 0, 704, 98
45698, V, 1, 1, 1, 1, 0, 704, 98
45699, V, 1, 1, 1, 1, 0, 704, 98
45700, V, 1, 1, 1, 1, 0, 704, 98
45701, V, 1, 1, 1, 1, 0, 704, 98
45702, V, 1, 1, 1, 1, 0, 704, 98
45703, V, 1, 1, 1, 1, 0, 704, 98
45704, V, 1, 1, 1, 1, 0, 704, 98
45705, V, 1, 1, 1, 1, 0, 704, 98
45706, V, 1, 1, 1, 1, 0, 704, 98
45707, V, 1, 1, 1, 1, 0, 704, 98
45708, V, 1, 1, 1, 1, 0, 704, 98
45709, V, 1, 1, 1, 1, 0, 704, 98
45710, V, 1, 1, 1, 1, 0, 704, 98
45711, V, 1, 1, 1, 1, 0, 704, 98
45712, V, 1, 1, 1, 1, 0, 704, 98
45713, V, 1, 1, 1, 1, 0, 704, 98
45714, V, 1, 1, 1, 1, 0, 704, 98
45715, V, 1, 1, 1, 1, 0, 704, 98
45716, V, 1, 1, 1, 1, 0, 704, 98
45717, V, 1, 1, 1, 1, 0, 704, 98
45718, V, 1, 1, 1, 1, 0, 704, 98
45719, V, 1, 1, 1, 1, 0, 704, 98
45720, V, 1, 1, 1, 1, 0, 704, 98
45721, V, 1, 1, 1, 1, 0, 704, 98
45722, V, 1, 1, 1, 1, 0, 704, 98
45723, V, 1, 1, 1, 1, 0, 704, 98
45724, V, 1, 1, 1, 1, 0, 704, 98
45725, V, 1, 1, 1, 1, 0, 704, 98
45726, V, 1, 1, 1, 1, 0, 704, 98
45727, V, 1, 1, 1, 1, 0, 704, 98
45728, V, 1, 1, 1, 1, 0, 704, 98
45729, V, 1, 1, 1, 1, 0, 704, 98
45730, V, 1, 1, 1, 1, 0, 704, 98
45731, V, 1, 1, 1, 1, 0, 704, 98
45732, V, 1, 1, 1, 1, 0, 704, 98
45733, V, 1, 1, 1, 1, 0, 704, 98
45734, V, 1, 1, 1, 1, 0, 704, 98
45735, V, 1, 1, 1, 1, 0, 704, 98
45736, V, 1, 1, 1, 1, 0, 704, 98
45737, V, 1, 1, 1, 1, 0, 704, 98
45739, V, 1, 1, 1, 1, 0, 704, 98
45740, V, 1, 1, 1, 1, 0, 704, 98
45741, V, 1, 1, 1, 1, 0, 704, 98
45742, V, 1, 1, 1, 1, 0, 704, 98
45743, V, 1, 1, 1, 1, 0, 704, 98
45744, V, 1, 1, 1, 1, 0, 704, 98
45745, V, 1, 1, 1, 1, 0, 704, 98
45746, V, 1, 1, 1, 1, 0, 704, 98
45747, V, 1, 1, 1, 1, 0, 704, 98
45748, V, 1, 1, 1, 1, 0, 704, 98
45749, V, 1, 1, 1, 1, 0, 704, 98
45750, V, 1, 1, 1, 1, 0, 704, 98
45751, V, 1, 1, 1, 1, 0, 704, 98
45752, V, 1, 1, 1, 1, 0, 704, 98
45753, V, 1, 1, 1, 1, 0, 704, 98
45754, V, 1, 1, 1, 1, 0, 704, 98
45755, V, 1, 1, 1, 1, 0, 704, 98
45756, V, 1, 1, 1, 1, 0, 704, 98
45757, V, 1, 1, 1, 1, 0, 704, 98
45758, V, 1, 1, 1, 1, 0, 704, 98
45759, V, 1, 1, 1, 1, 0, 704, 98
45760, V, 1, 1, 1, 1, 0, 704, 98
45761, V, 1, 1, 1, 1, 0, 704, 98
45762, V, 1, 1, 1, 1, 0, 704, 98
45763, V, 1, 1, 1, 1, 0, 704, 98
45764, V, 1, 1, 1, 1, 0, 704, 98
45765, V, 1, 1, 1, 1, 0, 704, 98
45766, V, 1, 1, 1, 1, 0, 704, 98
45767, V, 1, 1, 1, 1, 0, 704, 98
45768, V, 1, 1, 1, 1, 0, 704, 98
45769, V, 1, 1, 1, 1, 0, 704, 98
45770, V, 1, 1, 1, 1, 0, 704, 98
45771, V, 1, 1, 1, 1, 0, 704, 98
45772, V, 1, 1, 1, 1, 0, 704, 98
45773, V, 1, 1, 1, 1, 0, 704, 98
45774, V, 1, 1, 1, 1, 0, 704, 98
45775, V, 1, 1, 1, 1, 0, 704, 98
45776, V, 1, 1, 1, 1, 0, 704, 98
45777, V, 1, 1, 1, 1, 0, 704, 98
45778, V, 1, 1, 1, 1, 0, 704, 98
45779, V, 1, 1, 1, 1, 0, 704, 98
45780, V, 1, 1, 1, 1, 0, 704, 98
45782, V, 1, 1, 1, 1, 0, 704, 98
45783, V, 1, 1, 1, 1, 0, 704, 98
45784, V, 1, 1, 1, 1, 0, 704, 98
45785, V, 1, 1, 1, 1, 0, 704, 98
45786, V, 1, 1, 1, 1, 0, 704, 98
45787, V, 1, 1, 1, 1, 0, 704, 98
45788, V, 1, 1, 1, 1, 0, 704, 98
45789, V, 1, 1, 1, 1, 0, 704, 98
45790, V, 1, 1, 1, 1, 0, 704, 98
45791, V, 1, 1, 1, 1, 0, 704, 98
45792, V, 1, 1, 1, 1, 0, 704, 98
45793, V, 1, 1, 1, 1, 0, 704, 98
45794, V, 1, 1, 1, 1, 0, 704, 98
45795, V, 1, 1, 1, 1, 0, 704, 98
45796, V, 1, 1, 1, 1, 0, 704, 98
45797, V, 1, 1, 1, 1, 0, 704, 98
45798, V, 1, 1, 1, 1, 0, 704, 98
45799, V, 1, 1, 1, 1, 0, 704, 98
45800, V, 1, 1, 1, 1, 0, 704, 98
45801, V, 1, 1, 1, 1, 0, 704, 98
45802, V, 1, 1, 1, 1, 0, 704, 98
45803, V, 1, 1, 1, 1, 0, 704, 98
45804, V, 1, 1, 1, 1, 0, 704, 98
45805, V, 1, 1, 1, 1, 0, 704, 98
45806, V, 1, 1, 1, 1, 0, 704, 98
45807, V, 1, 1, 1, 1, 0, 704, 98
45808, V, 1, 1, 1, 1, 0, 704, 98
45809, V, 1, 1, 1, 1, 0, 704, 98
45810, V, 1, 1, 1, 1, 0, 704, 98
45811, V, 1, 1, 1, 1, 0, 704, 98
45812, V, 1, 1, 1, 1, 0, 704, 98
45813, V, 1, 1, 1, 1, 0, 704, 98
45814, V, 1, 1, 1, 1, 0, 704, 98
45815, V, 1, 1, 1, 1, 0, 704, 98
45816, V, 1, 1, 1, 1, 0, 704, 98
45817, V, 1, 1, 1, 1, 0, 704, 98
45818, V, 1, 1, 1, 1, 0, 704, 98
45819, V, 1, 1, 1, 1, 0, 704, 98
45820, V, 1, 1, 1, 1, 0, 704, 98
45821, V, 1, 1, 1, 1, 0, 704, 98
45822, V, 1, 1, 1, 1, 0, 704, 98
45824, V, 1, 1, 1, 1, 0, 704, 98
45825, V, 1, 1, 1, 1, 0, 704, 98
45826, V, 1, 1, 1, 1, 0, 704, 98
45827, V, 1, 1, 1, 1, 0, 704, 98
45828, V, 1, 1, 1, 1, 0, 704, 98
45829, V, 1, 1, 1, 1, 0, 704, 98
45830, V, 1, 1, 1, 1, 0, 704, 98
45831, V, 1, 1, 1, 1, 0, 704, 98
45832, V, 1, 1, 1, 1, 0, 704, 98
45833, V, 1, 1, 1, 1, 0, 704, 98
45834, V, 1, 1, 1, 1, 0, 704, 98
45835, V, 1, 1, 1, 1, 0, 704, 98
45836, V, 1, 1, 1, 1, 0, 704, 98
45837, V, 1, 1, 1, 1, 0, 704, 98
45838, V, 1, 1, 1, 1, 0, 704, 98
45839, V, 1, 1, 1, 1, 0, 704, 98
45840, V, 1, 1, 1, 1, 0, 704, 98
45841, V, 1, 1, 1, 1, 0, 704, 98
45842, V, 1, 1, 1, 1, 0, 704, 98
45843, V, 1, 1, 1, 1, 0, 704, 98
45844, V, 1, 1, 1, 1, 0, 704, 98
45845, V, 1, 1, 1, 1, 0, 704, 98
45846, V, 1, 1, 1, 1, 0, 704, 98
45847, V, 1, 1, 1, 1, 0, 704, 98
45848, V, 1, 1, 1, 1, 0, 704, 98
45849, V, 1, 1, 1, 1, 0, 704, 98
45850, V, 1, 1, 1, 1, 0, 704, 98
45851, V, 1, 1, 1, 1, 0, 704, 98
45852, V, 1, 1, 1, 1, 0, 704, 98
45853, V, 1, 1, 1, 1, 0, 704, 98
45854, V, 1, 1, 1, 1, 0, 704, 98
45855, V, 1, 1, 1, 1, 0, 704, 98
45856, V, 1, 1, 1, 1, 0, 704, 98
45857, V, 1, 1, 1, 1, 0, 704, 98
45858, V, 1, 1, 1, 1, 0, 704, 98
45859, V, 1, 1, 1, 1, 0, 704, 98
45860, V, 1, 1, 1, 1, 0, 704, 98
45861, V, 1, 1, 1, 1, 0, 704, 98
45862, V, 1, 1, 1, 1, 0, 704, 98
45863, V, 1, 1, 1, 1, 0, 704, 98
45864, V, 1, 1, 1, 1, 0, 704, 98
45865, V, 1, 1, 1, 1, 0, 704, 98
45867, V, 1, 1, 1, 1, 0, 704, 98
45868, V, 1, 1, 1, 1, 0, 704, 98
45869, V, 1, 1, 1, 1, 0, 704, 98
45870, V, 1, 1, 1, 1, 0, 704, 98
45871, V, 1, 1, 1, 1, 0, 704, 98
45872, V, 1, 1, 1, 1, 0, 704, 98
45873, V, 1, 1, 1, 1, 0, 704, 98
45874, V, 1, 1, 1, 1, 0, 704, 98
45875, V, 1, 1, 1, 1, 0, 704, 98
45876, V, 1, 1, 1, 1, 0, 704, 98
45877, V, 1, 1, 1, 1, 0, 704, 98
45878, V, 1, 1, 1, 1, 0, 704, 98
45879, V, 1, 1, 1, 1, 0, 704, 98
45880, V, 1, 1, 1, 1, 0, 704, 98
45881, V, 1, 1, 1, 1, 0, 704, 98
45882, V, 1, 1, 1, 1, 0, 704, 98
45883, V, 1, 1, 1, 1, 0, 704, 98
45884, V, 1, 1, 1, 1, 0, 704, 98
45885, V, 1, 1, 1, 1, 0, 704, 98
45886, V, 1, 1, 1, 1, 0, 704, 98
45887, V, 1, 1, 1, 1, 0, 704, 98
45888, V, 1, 1, 1, 1, 0, 704, 98
45889, V, 1, 1, 1, 1, 0, 704, 98
45890, V, 1, 1, 1, 1, 0, 704, 98
45891, V, 1, 1, 1, 1, 0, 704, 98
45892, V, 1, 1, 1, 1, 0, 704, 98
45893, V, 1, 1, 1, 1, 0, 704, 98
45894, V, 1, 1, 1, 1, 0, 704, 98
45895, V, 1, 1, 1, 1, 0, 704, 98
45896, V, 1, 1, 1, 1, 0, 704, 98
45897, V, 1, 1, 1, 1, 0, 704, 98
45898, V, 1, 1, 1, 1, 0, 704, 98
45899, V, 1, 1, 1, 1, 0, 704, 98
45900, V, 1, 1, 1, 1, 0, 704, 98
45901, V, 1, 1, 1, 1, 0, 704, 98
45902, V, 1, 1, 1, 1, 0, 704, 98
45903, V, 1, 1, 1, 1, 0, 704, 98
45904, V, 1, 1, 1, 1, 0, 704, 98
45905, V, 1, 1, 1, 1, 0, 704, 98
45906, V, 1, 1, 1, 1, 0, 704, 98
45907, V, 1, 1, 1, 1, 0, 704, 98
45908, V, 1, 1, 1, 1, 0, 704, 98
45910, V, 1, 1, 1, 1, 0, 704, 98
45911, V, 1, 1, 1, 1, 0, 704, 98
45912, V, 1, 1, 1, 1, 0, 704, 98
45913, V, 1, 1, 1, 1, 0, 704, 98
45914, V, 1, 1, 1, 1, 0, 704, 98
45915, V, 1, 1, 1, 1, 0, 704, 98
45916, V, 1, 1, 1, 1, 0, 704, 98
45917, V, 1, 1, 1, 1, 0, 704, 98
45918, V, 1, 1, 1, 1, 0, 704, 98
45919, V, 1, 1, 1, 1, 0, 704, 98
45920, V, 1, 1, 1, 1, 0, 704, 98
45921, V, 1, 1, 1, 1, 0, 704, 98
45922, V, 1, 1, 1, 1, 0, 704, 98
45923, V, 1, 1, 1, 1, 0, 704, 98
45924, V, 1, 1, 1, 1, 0, 704, 98
45925, V, 1, 1, 1, 1, 0, 704, 98
45926, V, 1, 1, 1, 1, 0, 704, 99
45927, V, 1, 1, 1, 1, 0, 704, 98
45928, V, 1, 1, 1, 1, 0, 704, 98
45929, V, 1, 1, 1, 1, 0, 704, 98
45930, V, 1, 1, 1, 1, 0, 704, 98
45931, V, 1, 1, 1, 1, 0, 704, 98
45932, V, 1, 1, 1, 1, 0, 704, 98
45933, V, 1, 1, 1, 1, 0, 704, 98
45934, V, 1, 1, 1, 1, 0, 704, 98
45935, V, 1, 1, 1, 1, 0, 704, 98
45936, V, 1, 1, 1, 1, 0, 704, 98
45937, V, 1, 1, 1, 1, 0, 704, 98
45938, V, 1, 1, 1, 1, 0, 704, 98
45939, V, 1, 1, 1, 1, 0, 704, 98
45940, V, 1, 1, 1, 1, 0, 704, 98
45941, V, 1, 1, 1, 1, 0, 704, 98
45942, V, 1, 1, 1, 1, 0, 704, 98
45943, V, 1, 1, 1, 1, 0, 704, 98
45944, V, 1, 1, 1, 1, 0, 704, 98
45945, V, 1, 1, 1, 1, 0, 704, 98
45946, V, 1, 1, 1, 1, 0, 704, 98
45947, V, 1, 1, 1, 1, 0, 704, 98
45948, V, 1, 1, 1, 1, 0, 704, 98
45949, V, 1, 1, 1, 1, 0, 704, 98
45950, V, 1, 1, 1, 1, 0, 704, 98
45952, V, 1, 1, 1, 1, 0, 704, 98
45953, V, 1, 1, 1, 1, 0, 704, 98
45954, V, 1, 1, 1, 1, 0, 704, 98
45955, V, 1, 1, 1, 1, 0, 704, 98
45956, V, 1, 1, 1, 1, 0, 704, 98
45957, V, 1, 1, 1, 1, 0, 704, 98
45958, V, 1, 1, 1, 1, 0, 704, 98
45959, V, 1, 1, 1, 1, 0, 704, 98
45960, V, 1, 1, 1, 1, 0, 704, 98
45961, V, 1, 1, 1, 1, 0, 704, 98
45962, V, 1, 1, 1, 1, 0, 704, 98
45963, V, 1, 1, 1, 1, 0, 704, 98
45964, V, 1, 1, 1, 1, 0, 704, 98
45965, V, 1, 1, 1, 1, 0, 704, 98
45966, V, 1, 1, 1, 1, 0, 704, 98
45967, V, 1, 1, 1, 1, 0, 704, 98
45968, V, 1, 1, 1, 1, 0, 704, 98
45969, V, 1, 1, 1, 1, 0, 704, 98
45970, V, 1, 1, 1, 1, 0, 704, 98
45971, V, 1, 1, 1, 1, 0, 704, 98
45972, V, 1, 1, 1, 1, 0, 704, 98
45973, V, 1, 1, 1, 1, 0, 704, 98
45974, V, 1, 1, 1, 1, 0, 704, 98
45975, V, 1, 1, 1, 1, 0, 704, 98
45976, V, 1, 1, 1, 1, 0, 704, 98
45977, V, 1, 1, 1, 1, 0, 704, 98
45978, V, 1, 1, 1, 1, 0, 704, 98
45979, V, 1, 1, 1, 1, 0, 704, 98
45980, V, 1, 1, 1, 1, 0, 704, 98
45981, V, 1, 1, 1, 1, 0, 704, 98
45982, V, 1, 1, 1, 1, 0, 704, 98
45983, V, 1, 1, 1, 1, 0, 704, 98
45984, V, 1, 1, 1, 1, 0, 704, 98
45985, V, 1, 1, 1, 1, 0, 704, 98
45986, V, 1, 1, 1, 1, 0, 704, 98
45987, V, 1, 1, 1, 1, 0, 704, 98
45988, V, 1, 1, 1, 1, 0, 704, 98
45989, V, 1, 1, 1, 1, 0, 704, 98
45990, V, 1, 1, 1, 1, 0, 704, 98
45991, V, 1, 1, 1, 1, 0, 704, 98
45992, V, 1, 1, 1, 1, 0, 704, 98
45993, V, 1, 1, 1, 1, 0, 704, 98
45995, V, 1, 1, 1, 1, 0, 704, 99
45996, V, 1, 1, 1, 1, 0, 704, 98
45997, V, 1, 1, 1, 1, 0, 704, 98
45998, V, 1, 1, 1, 1, 0, 704, 98
45999, V, 1, 1, 1, 1, 0, 704, 98
46000, V, 1, 1, 1, 1, 0, 704, 98
46001, V, 1, 1, 1, 1, 0, 704, 98
46002, V, 1, 1, 1, 1, 0, 704, 99
46003, V, 1, 1, 1, 1, 0, 704, 99
46004, V, 1, 1, 1, 1, 0, 704, 99
46005, V, 1, 1, 1, 1, 0, 704, 98
46006, V, 1, 1, 1, 1, 0, 704, 99
46007, V, 1, 1, 1, 1, 0, 704, 98
46008, V, 1, 1, 1, 1, 0, 704, 99
46009, V, 1, 1, 1, 1, 0, 704, 99
46010, V, 1, 1, 1, 1, 0, 704, 98
46011, V, 1, 1, 1, 1, 0, 704, 98
46012, V, 1, 1, 1, 1, 0, 704, 99
46013, V, 1, 1, 1, 1, 0, 704, 98
46014, V, 1, 1, 1, 1, 0, 704, 99
46015, V, 1, 1, 1, 1, 0, 704, 98
46016, V, 1, 1, 1, 1, 0, 704, 98
46017, V, 1, 1, 1, 1, 0, 704, 98
46018, V, 1, 1, 1, 1, 0, 704, 98
46019, V, 1, 1, 1, 1, 0, 704, 98
46020, V, 1, 1, 1, 1, 0, 704, 98
46021, V, 1, 1, 1, 1, 0, 704, 98
46022, V, 1, 1, 1, 1, 0, 704, 98
46023, V, 1, 1, 1, 1, 0, 704, 98
46024, V, 1, 1, 1, 1, 0, 704, 99
46025, V, 1, 1, 1, 1, 0, 704, 98
46026, V, 1, 1, 1, 1, 0, 704, 98
46027, V, 1, 1, 1, 1, 0, 704, 98
46028, V, 1, 1, 1, 1, 0, 704, 98
46029, V, 1, 1, 1, 1, 0, 704, 98
46030, V, 1, 1, 1, 1, 0, 704, 98
46031, V, 1, 1, 1, 1, 0, 704, 98
46032, V, 1, 1, 1, 1, 0, 704, 98
46033, V, 1, 1, 1, 1, 0, 704, 98
46034, V, 1, 1, 1, 1, 0, 704, 98
46035, V, 1, 1, 1, 1, 0, 704, 98
46036, V, 1, 1, 1, 1, 0, 704, 98
46038, V, 1, 1, 1, 1, 0, 704, 98
46039, V, 1, 1, 1, 1, 0, 704, 98
46040, V, 1, 1, 1, 1, 0, 704, 98
46041, V, 1, 1, 1, 1, 0, 704, 98
46042, V, 1, 1, 1, 1, 0, 704, 98
46043, V, 1, 1, 1, 1, 0, 704, 98
46044, V, 1, 1, 1, 1, 0, 704, 98
46045, V, 1, 1, 1, 1, 0, 704, 98
46046, V, 1, 1, 1, 1, 0, 704, 98
46047, V, 1, 1, 1, 1, 0, 704, 98
46048, V, 1, 1, 1, 1, 0, 704, 98
46049, V, 1, 1, 1, 1, 0, 704, 98
46050, V, 1, 1, 1, 1, 0, 704, 98
46051, V, 1, 1, 1, 1, 0, 704, 98
46052, V, 1, 1, 1, 1, 0, 704, 98
46053, V, 1, 1, 1, 1, 0, 704, 98
46054, V, 1, 1, 1, 1, 0, 704, 98
46055, V, 1, 1, 1, 1, 0, 704, 98
46056, V, 1, 1, 1, 1, 0, 704, 98
46057, V, 1, 1, 1, 1, 0, 704, 98
46058, V, 1, 1, 1, 1, 0, 704, 98
46059, V, 1, 1, 1, 1, 0, 704, 98
46060, V, 1, 1, 1, 1, 0, 704, 98
46061, V, 1, 1, 1, 1, 0, 704, 98
46062, V, 1, 1, 1, 1, 0, 704, 98
46063, V, 1, 1, 1, 1, 0, 704, 98
46064, V, 1, 1, 1, 1, 0, 704, 98
46065, V, 1, 1, 1, 1, 0, 704, 98
46066, V, 1, 1, 1, 1, 0, 704, 98
46067, V, 1, 1, 1, 1, 0, 704, 98
46068, V, 1, 1, 1, 1, 0, 704, 98
46069, V, 1, 1, 1, 1, 0, 704, 98
46070, V, 1, 1, 1, 1, 0, 704, 98
46071, V, 1, 1, 1, 1, 0, 704, 98
46072, V, 1, 1, 1, 1, 0, 704, 98
46073, V, 1, 1, 1, 1, 0, 704, 98
46074, V, 1, 1, 1, 1, 0, 704, 98
46075, V, 1, 1, 1, 1, 0, 704, 98
46076, V, 1, 1, 1, 1, 0, 704, 98
46077, V, 1, 1, 1, 1, 0, 704, 98
46078, V, 1, 1, 1, 1, 0, 704, 98
46080, V, 1, 1, 1, 1, 0, 704, 98
46081, V, 1, 1, 1, 1, 0, 704, 98
46082, V, 1, 1, 1, 1, 0, 704, 98
46083, V, 1, 1, 1, 1, 0, 704, 98
46084, V, 1, 1, 1, 1, 0, 704, 98
46085, V, 1, 1, 1, 1, 0, 704, 98
46086, V, 1, 1, 1, 1, 0, 704, 98
46087, V, 1, 1, 1, 1, 0, 704, 98
46088, V, 1, 1, 1, 1, 0, 704, 98
46089, V, 1, 1, 1, 1, 0, 704, 98
46090, V, 1, 1, 1, 1, 0, 704, 98
46091, V, 1, 1, 1, 1, 0, 704, 98
46092, V, 1, 1, 1, 1, 0, 704, 98
46093, V, 1, 1, 1, 1, 0, 704, 98
46094, V, 1, 1, 1, 1, 0, 704, 98
46095, V, 1, 1, 1, 1, 0, 704, 98
46096, V, 1, 1, 1, 1, 0, 704, 98
46097, V, 1, 1, 1, 1, 0, 704, 98
46098, V, 1, 1, 1, 1, 0, 704, 98
46099, V, 1, 1, 1, 1, 0, 704, 98
46100, V, 1, 1, 1, 1, 0, 704, 98
46101, V, 1, 1, 1, 1, 0, 704, 98
46102, V, 1, 1, 1, 1, 0, 704, 98
46103, V, 1, 1, 1, 1, 0, 704, 98
46104, V, 1, 1, 1, 1, 0, 704, 98
46105, V, 1, 1, 1, 1, 0, 704, 98
46106, V, 1, 1, 1, 1, 0, 704, 98
46107, V, 1, 1, 1, 1, 0, 704, 98
46108, V, 1, 1, 1, 1, 0, 704, 98
46109, V, 1, 1, 1, 1, 0, 704, 98
46110, V, 1, 1, 1, 1, 0, 704, 98
46111, V, 1, 1, 1, 1, 0, 704, 98
46112, V, 1, 1, 1, 1, 0, 704, 98
46113, V, 1, 1, 1, 1, 0, 704, 98
46114, V, 1, 1, 1, 1, 0, 704, 98
46115, V, 1, 1, 1, 1, 0, 704, 98
46116, V, 1, 1, 1, 1, 0, 704, 98
46117, V, 1, 1, 1, 1, 0, 704, 98
46118, V, 1, 1, 1, 1, 0, 704, 98
46119, V, 1, 1, 1, 1, 0, 704, 98
46120, V, 1, 1, 1, 1, 0, 704, 98
46121, V, 1, 1, 1, 1, 0, 704, 98
46123, V, 1, 1, 1, 1, 0, 704, 98
46124, V, 1, 1, 1, 1, 0, 704, 98
46125, V, 1, 1, 1, 1, 0, 704, 98
46126, V, 1, 1, 1, 1, 0, 704, 98
46127, V, 1, 1, 1, 1, 0, 704, 98
46128, V, 1, 1, 1, 1, 0, 704, 98
46129, V, 1, 1, 1, 1, 0, 704, 98
46130, V, 1, 1, 1, 1, 0, 704, 98
46131, V, 1, 1, 1, 1, 0, 704, 98
46132, V, 1, 1, 1, 1, 0, 704, 98
46133, V, 1, 1, 1, 1, 0, 704, 98
46134, V, 1, 1, 1, 1, 0, 704, 98
46135, V, 1, 1, 1, 1, 0, 704, 98
46136, V, 1, 1, 1, 1, 0, 704, 98
46137, V, 1, 1, 1, 1, 0, 704, 98
46138, V, 1, 1, 1, 1, 0, 704, 98
46139, V, 1, 1, 1, 1, 0, 704, 98
46140, V, 1, 1, 1, 1, 0, 704, 98
46141, V, 1, 1, 1, 1, 0, 704, 98
46142, V, 1, 1, 1, 1, 0, 704, 98
46143, V, 1, 1, 1, 1, 0, 704, 98
46144, V, 1, 1, 1, 1, 0, 704, 98
46145, V, 1, 1, 1, 1, 0, 704, 98
46146, V, 1, 1, 1, 1, 0, 704, 98
46147, V, 1, 1, 1, 1, 0, 704, 98
46148, V, 1, 1, 1, 1, 0, 704, 98
46149, V, 1, 1, 1, 1, 0, 704, 98
46150, V, 1, 1, 1, 1, 0, 704, 98
46151, V, 1, 1, 1, 1, 0, 704, 98
46152, V, 1, 1, 1, 1, 0, 704, 98
46153, V, 1, 1, 1, 1, 0, 704, 98
46154, V, 1, 1, 1, 1, 0, 704, 98
46155, V, 1, 1, 1, 1, 0, 704, 98
46156, V, 1, 1, 1, 1, 0, 704, 98
46157, V, 1, 1, 1, 1, 0, 704, 98
46158, V, 1, 1, 1, 1, 0, 704, 98
46159, V, 1, 1, 1, 1, 0, 704, 98
46160, V, 1, 1, 1, 1, 0, 704, 98
46161, V, 1, 1, 1, 1, 0, 704, 98
46162, V, 1, 1, 1, 1, 0, 704, 98
46163, V, 1, 1, 1, 1, 0, 704, 98
46164, V, 1, 1, 1, 1, 0, 704, 98
46166, V, 1, 1, 1, 1, 0, 704, 98
46167, V, 1, 1, 1, 1, 0, 704, 98
46168, V, 1, 1, 1, 1, 0, 704, 98
46169, V, 1, 1, 1, 1, 0, 704, 98
46170, V, 1, 1, 1, 1, 0, 704, 98
46171, V, 1, 1, 1, 1, 0, 704, 98
46172, V, 1, 1, 1, 1, 0, 704, 98
46173, V, 1, 1, 1, 1, 0, 704, 98
46174, V, 1, 1, 1, 1, 0, 704, 98
46175, V, 1, 1, 1, 1, 0, 704, 98
46176, V, 1, 1, 1, 1, 0, 704, 98
46177, V, 1, 1, 1, 1, 0, 704, 98
46178, V, 1, 1, 1, 1, 0, 704, 98
46179, V, 1, 1, 1, 1, 0, 704, 98
46180, V, 1, 1, 1, 1, 0, 704, 98
46181, V, 1, 1, 1, 1, 0, 704, 98
46182, V, 1, 1, 1, 1, 0, 704, 98
46183, V, 1, 1, 1, 1, 0, 704, 98
46184, V, 1, 1, 1, 1, 0, 704, 98
46185, V, 1, 1, 1, 1, 0, 704, 98
46186, V, 1, 1, 1, 1, 0, 704, 98
46187, V, 1, 1, 1, 1, 0, 704, 98
46188, V, 1, 1, 1, 1, 0, 704, 98
46189, V, 1, 1, 1, 1, 0, 704, 98
46190, V, 1, 1, 1, 1, 0, 704, 98
46191, V, 1, 1, 1, 1, 0, 704, 98
46192, V, 1, 1, 1, 1, 0, 704, 98
46193, V, 1, 1, 1, 1, 0, 704, 98
46194, V, 1, 1, 1, 1, 0, 704, 98
46195, V, 1, 1, 1, 1, 0, 704, 98
46196, V, 1, 1, 1, 1, 0, 704, 98
46197, V, 1, 1, 1, 1, 0, 704, 98
46198, V, 1, 1, 1, 1, 0, 704, 98
46199, V, 1, 1, 1, 1, 0, 704, 98
46200, V, 1, 1, 1, 1, 0, 704, 98
46201, V, 1, 1, 1, 1, 0, 704, 98
46202, V, 1, 1, 1, 1, 0, 704, 98
46203, V, 1, 1, 1, 1, 0, 704, 98
46204, V, 1, 1, 1, 1, 0, 704, 98
46205, V, 1, 1, 1, 1, 0, 704, 98
46206, V, 1, 1, 1, 1, 0, 704, 98
46208, V, 1, 1, 1, 1, 0, 704, 98
46209, V, 1, 1, 1, 1, 0, 704, 98
46210, V, 1, 1, 1, 1, 0, 704, 98
46211, V, 1, 1, 1, 1, 0, 704, 98
46212, V, 1, 1, 1, 1, 0, 704, 98
46213, V, 1, 1, 1, 1, 0, 704, 98
46214, V, 1, 1, 1, 1, 0, 704, 98
46215, V, 1, 1, 1, 1, 0, 704, 98
46216, V, 1, 1, 1, 1, 0, 704, 98
46217, V, 1, 1, 1, 1, 0, 704, 98
46218, V, 1, 1, 1, 1, 0, 704, 98
46219, V, 1, 1, 1, 1, 0, 704, 98
46220, V, 1, 1, 1, 1, 0, 704, 98
46221, V, 1, 1, 1, 1, 0, 704, 98
46222, V, 1, 1, 1, 1, 0, 704, 98
46223, V, 1, 1, 1, 1, 0, 704, 98
46224, V, 1, 1, 1, 1, 0, 704, 98
46225, V, 1, 1, 1, 1, 0, 704, 98
46226, V, 1, 1, 1, 1, 0, 704, 98
46227, V, 1, 1, 1, 1, 0, 704, 98
46228, V, 1, 1, 1, 1, 0, 704, 98
46229, V, 1, 1, 1, 1, 0, 704, 98
46230, V, 1, 1, 1, 1, 0, 704, 98
46231, V, 1, 1, 1, 1, 0, 704, 98
46232, V, 1, 1, 1, 1, 0, 704, 98
46233, V, 1, 1, 1, 1, 0, 704, 98
46234, V, 1, 1, 1, 1, 0, 704, 98
46235, V, 1, 1, 1, 1, 0, 704, 98
46236, V, 1, 1, 1, 1, 0, 704, 98
46237, V, 1, 1, 1, 1, 0, 704, 98
46238, V, 1, 1, 1, 1, 0, 704, 98
46239, V, 1, 1, 1, 1, 0, 704, 98
46240, V, 1, 1, 1, 1, 0, 704, 98
46241, V, 1, 1, 1, 1, 0, 704, 98
46242, V, 1, 1, 1, 1, 0, 704, 98
46243, V, 1, 1, 1, 1, 0, 704, 98
46244, V, 1, 1, 1, 1, 0, 704, 98
46245, V, 1, 1, 1, 1, 0, 704, 98
46246, V, 1, 1, 1, 1, 0, 704, 98
46247, V, 1, 1, 1, 1, 0, 704, 98
46248, V, 1, 1, 1, 1, 0, 704, 98
46249, V, 1, 1, 1, 1, 0, 704, 98
46251, V, 1, 1, 1, 1, 0, 704, 98
46252, V, 1, 1, 1, 1, 0, 704, 98
46253, V, 1, 1, 1, 1, 0, 704, 98
46254, V, 1, 1, 1, 1, 0, 704, 98
46255, V, 1, 1, 1, 1, 0, 704, 98
46256, V, 1, 1, 1, 1, 0, 704, 98
46257, V, 1, 1, 1, 1, 0, 704, 98
46258, V, 1, 1, 1, 1, 0, 704, 98
46259, V, 1, 1, 1, 1, 0, 704, 98
46260, V, 1, 1, 1, 1, 0, 704, 98
46261, V, 1, 1, 1, 1, 0, 704, 98
46262, V, 1, 1, 1, 1, 0, 704, 98
46263, V, 1, 1, 1, 1, 0, 704, 98
46264, V, 1, 1, 1, 1, 0, 704, 98
46265, V, 1, 1, 1, 1, 0, 704, 98
46266, V, 1, 1, 1, 1, 0, 704, 98
46267, V, 1, 1, 1, 1, 0, 704, 98
46268, V, 1, 1, 1, 1, 0, 704, 98
46269, V, 1, 1, 1, 1, 0, 704, 98
46270, V, 1, 1, 1, 1, 0, 704, 98
46271, V, 1, 1, 1, 1, 0, 704, 98
46272, V, 1, 1, 1, 1, 0, 704, 98
46273, V, 1, 1, 1, 1, 0, 704, 98
46274, V, 1, 1, 1, 1, 0, 704, 98
46275, V, 1, 1, 1, 1, 0, 704, 98
46276, V, 1, 1, 1, 1, 0, 704, 98
46277, V, 1, 1, 1, 1, 0, 704, 98
46278, V, 1, 1, 1, 1, 0, 704, 98
46279, V, 1, 1, 1, 1, 0, 704, 98
46280, V, 1, 1, 1, 1, 0, 704, 98
46281, V, 1, 1, 1, 1, 0, 704, 98
46282, V, 1, 1, 1, 1, 0, 704, 98
46283, V, 1, 1, 1, 1, 0, 704, 98
46284, V, 1, 1, 1, 1, 0, 704, 98
46285, V, 1, 1, 1, 1, 0, 704, 98
46286, V, 1, 1, 1, 1, 0, 704, 98
46287, V, 1, 1, 1, 1, 0, 704, 98
46288, V, 1, 1, 1, 1, 0, 704, 98
46289, V, 1, 1, 1, 1, 0, 704, 98
46290, V, 1, 1, 1, 1, 0, 704, 98
46291, V, 1, 1, 1, 1, 0, 704, 98
46292, V, 1, 1, 1, 1, 0, 704, 98
46294, V, 1, 1, 1, 1, 0, 704, 98
46295, V, 1, 1, 1, 1, 0, 704, 98
46296, V, 1, 1, 1, 1, 0, 704, 98
46297, V, 1, 1, 1, 1, 0, 704, 98
46298, V, 1, 1, 1, 1, 0, 704, 98
46299, V, 1, 1, 1, 1, 0, 704, 98
46300, V, 1, 1, 1, 1, 0, 704, 98
46301, V, 1, 1, 1, 1, 0, 704, 98
46302, V, 1, 1, 1, 1, 0, 704, 98
46303, V, 1, 1, 1, 1, 0, 704, 99
46304, V, 1, 1, 1, 1, 0, 704, 98
46305, V, 1, 1, 1, 1, 0, 704, 99
46306, V, 1, 1, 1, 1, 0, 704, 98
46307, V, 1, 1, 1, 1, 0, 704, 98
46308, V, 1, 1, 1, 1, 0, 704, 98
46309, V, 1, 1, 1, 1, 0, 704, 98
46310, V, 1, 1, 1, 1, 0, 704, 98
46311, V, 1, 1, 1, 1, 0, 704, 98
46312, V, 1, 1, 1, 1, 0, 704, 98
46313, V, 1, 1, 1, 1, 0, 704, 98
46314, V, 1, 1, 1, 1, 0, 704, 99
46315, V, 1, 1, 1, 1, 0, 704, 98
46316, V, 1, 1, 1, 1, 0, 704, 98
46317, V, 1, 1, 1, 1, 0, 704, 98
46318, V, 1, 1, 1, 1, 0, 704, 98
46319, V, 1, 1, 1, 1, 0, 704, 98
46320, V, 1, 1, 1, 1, 0, 704, 98
46321, V, 1, 1, 1, 1, 0, 704, 98
46322, V, 1, 1, 1, 1, 0, 704, 98
46323, V, 1, 1, 1, 1, 0, 704, 99
46324, V, 1, 1, 1, 1, 0, 704, 98
46325, V, 1, 1, 1, 1, 0, 704, 99
46326, V, 1, 1, 1, 1, 0, 704, 98
46327, V, 1, 1, 1, 1, 0, 704, 98
46328, V, 1, 1, 1, 1, 0, 704, 98
46329, V, 1, 1, 1, 1, 0, 704, 98
46330, V, 1, 1, 1, 1, 0, 704, 98
46331, V, 1, 1, 1, 1, 0, 704, 98
46332, V, 1, 1, 1, 1, 0, 704, 98
46333, V, 1, 1, 1, 1, 0, 704, 98
46334, V, 1, 1, 1, 1, 0, 704, 98
46336, V, 1, 1, 1, 1, 0, 704, 98
46337, V, 1, 1, 1, 1, 0, 704, 98
46338, V, 1, 1, 1, 1, 0, 704, 98
46339, V, 1, 1, 1, 1, 0, 704, 98
46340, V, 1, 1, 1, 1, 0, 704, 98
46341, V, 1, 1, 1, 1, 0, 704, 98
46342, V, 1, 1, 1, 1, 0, 704, 98
46343, V, 1, 1, 1, 1, 0, 704, 98
46344, V, 1, 1, 1, 1, 0, 704, 98
46345, V, 1, 1, 1, 1, 0, 704, 98
46346, V, 1, 1, 1, 1, 0, 704, 98
46347, V, 1, 1, 1, 1, 0, 704, 98
46348, V, 1, 1, 1, 1, 0, 704, 98
46349, V, 1, 1, 1, 1, 0, 704, 98
46350, V, 1, 1, 1, 1, 0, 704, 98
46351, V, 1, 1, 1, 1, 0, 704, 98
46352, V, 1, 1, 1, 1, 0, 704, 98
46353, V, 1, 1, 1, 1, 0, 704, 98
46354, V, 1, 1, 1, 1, 0, 704, 98
46355, V, 1, 1, 1, 1, 0, 704, 98
46356, V, 1, 1, 1, 1, 0, 704, 98
46357, V, 1, 1, 1, 1, 0, 704, 98
46358, V, 1, 1, 1, 1, 0, 704, 98
46359, V, 1, 1, 1, 1, 0, 704, 98
46360, V, 1, 1, 1, 1, 0, 704, 98
46361, V, 1, 1, 1, 1, 0, 704, 98
46362, V, 1, 1, 1, 1, 0, 704, 98
46363, V, 1, 1, 1, 1, 0, 704, 98
46364, V, 1, 1, 1, 1, 0, 704, 98
46365, V, 1, 1, 1, 1, 0, 704, 98
46366, V, 1, 1, 1, 1, 0, 704, 98
46367, V, 1, 1, 1, 1, 0, 704, 98
46368, V, 1, 1, 1, 1, 0, 704, 98
46369, V, 1, 1, 1, 1, 0, 704, 98
46370, V, 1, 1, 1, 1, 0, 704, 98
46371, V, 1, 1, 1, 1, 0, 704, 98
46372, V, 1, 1, 1, 1, 0, 704, 98
46373, V, 1, 1, 1, 1, 0, 704, 98
46374, V, 1, 1, 1, 1, 0, 704, 98
46375, V, 1, 1, 1, 1, 0, 704, 98
46376, V, 1, 1, 1, 1, 0, 704, 98
46377, V, 1, 1, 1, 1, 0, 704, 98
46379, V, 1, 1, 1, 1, 0, 704, 98
46380, V, 1, 1, 1, 1, 0, 704, 98
46381, V, 1, 1, 1, 1, 0, 704, 98
46382, V, 1, 1, 1, 1, 0, 704, 98
46383, V, 1, 1, 1, 1, 0, 704, 98
46384, V, 1, 1, 1, 1, 0, 704, 98
46385, V, 1, 1, 1, 1, 0, 704, 98
46386, V, 1, 1, 1, 1, 0, 704, 98
46387, V, 1, 1, 1, 1, 0, 704, 98
46388, V, 1, 1, 1, 1, 0, 704, 98
46389, V, 1, 1, 1, 1, 0, 704, 98
46390, V, 1, 1, 1, 1, 0, 704, 98
46391, V, 1, 1, 1, 1, 0, 704, 98
46392, V, 1, 1, 1, 1, 0, 704, 98
46393, V, 1, 1, 1, 1, 0, 704, 98
46394, V, 1, 1, 1, 1, 0, 704, 98
46395, V, 1, 1, 1, 1, 0, 704, 98
46396, V, 1, 1, 1, 1, 0, 704, 98
46397, V, 1, 1, 1, 1, 0, 704, 98
46398, V, 1, 1, 1, 1, 0, 704, 98
46399, V, 1, 1, 1, 1, 0, 704, 98
46400, V, 1, 1, 1, 1, 0, 704, 98
46401, V, 1, 1, 1, 1, 0, 704, 98
46402, V, 1, 1, 1, 1, 0, 704, 98
46403, V, 1, 1, 1, 1, 0, 704, 98
46404, V, 1, 1, 1, 1, 0, 704, 98
46405, V, 1, 1, 1, 1, 0, 704, 98
46406, V, 1, 1, 1, 1, 0, 704, 98
46407, V, 1, 1, 1, 1, 0, 704, 98
46408, V, 1, 1, 1, 1, 0, 704, 98
46409, V, 1, 1, 1, 1, 0, 704, 98
46410, V, 1, 1, 1, 1, 0, 704, 98
46411, V, 1, 1, 1, 1, 0, 704, 98
46412, V, 1, 1, 1, 1, 0, 704, 98
46413, V, 1, 1, 1, 1, 0, 704, 98
46414, V, 1, 1, 1, 1, 0, 704, 98
46415, V, 1, 1, 1, 1, 0, 704, 98
46416, V, 1, 1, 1, 1, 0, 704, 98
46417, V, 1, 1, 1, 1, 0, 704, 98
46418, V, 1, 1, 1, 1, 0, 704, 98
46419, V, 1, 1, 1, 1, 0, 704, 98
46420, V, 1, 1, 1, 1, 0, 704, 98
46422, V, 1, 1, 1, 1, 0, 704, 98
46423, V, 1, 1, 1, 1, 0, 704, 98
46424, V, 1, 1, 1, 1, 0, 704, 98
46425, V, 1, 1, 1, 1, 0, 704, 98
46426, V, 1, 1, 1, 1, 0, 704, 98
46427, V, 1, 1, 1, 1, 0, 704, 98
46428, V, 1, 1, 1, 1, 0, 704, 98
46429, V, 1, 1, 1, 1, 0, 704, 98
46430, V, 1, 1, 1, 1, 0, 704, 98
46431, V, 1, 1, 1, 1, 0, 704, 98
46432, V, 1, 1, 1, 1, 0, 704, 98
46433, V, 1, 1, 1, 1, 0, 704, 98
46434, V, 1, 1, 1, 1, 0, 704, 98
46435, V, 1, 1, 1, 1, 0, 704, 98
46436, V, 1, 1, 1, 1, 0, 704, 98
46437, V, 1, 1, 1, 1, 0, 704, 98
46438, V, 1, 1, 1, 1, 0, 704, 98
46439, V, 1, 1, 1, 1, 0, 704, 98
46440, V, 1, 1, 1, 1, 0, 704, 98
46441, V, 1, 1, 1, 1, 0, 704, 98
46442, V, 1, 1, 1, 1, 0, 704, 98
46443, V, 1, 1, 1, 1, 0, 704, 98
46444, V, 1, 1, 1, 1, 0, 704, 98
46445, V, 1, 1, 1, 1, 0, 704, 98
46446, V, 1, 1, 1, 1, 0, 704, 98
46447, V, 1, 1, 1, 1, 0, 704, 98
46448, V, 1, 1, 1, 1, 0, 704, 98
46449, V, 1, 1, 1, 1, 0, 704, 98
46450, V, 1, 1, 1, 1, 0, 704, 98
46451, V, 1, 1, 1, 1, 0, 704, 98
46452, V, 1, 1, 1, 1, 0, 704, 98
46453, V, 1, 1, 1, 1, 0, 704, 98
46454, V, 1, 1, 1, 1, 0, 704, 98
46455, V, 1, 1, 1, 1, 0, 704, 98
46456, V, 1, 1, 1, 1, 0, 704, 98
46457, V, 1, 1, 1, 1, 0, 704, 98
46458, V, 1, 1, 1, 1, 0, 704, 98
46459, V, 1, 1, 1, 1, 0, 704, 98
46460, V, 1, 1, 1, 1, 0, 704, 98
46461, V, 1, 1, 1, 1, 0, 704, 98
46462, V, 1, 1, 1, 1, 0, 704, 98
46464, V, 1, 1, 1, 1, 0, 704, 98
46465, V, 1, 1, 1, 1, 0, 704, 98
46466, V, 1, 1, 1, 1, 0, 704, 98
46467, V, 1, 1, 1, 1, 0, 704, 98
46468, V, 1, 1, 1, 1, 0, 704, 98
46469, V, 1, 1, 1, 1, 0, 704, 98
46470, V, 1, 1, 1, 1, 0, 704, 98
46471, V, 1, 1, 1, 1, 0, 704, 98
46472, V, 1, 1, 1, 1, 0, 704, 98
46473, V, 1, 1, 1, 1, 0, 704, 98
46474, V, 1, 1, 1, 1, 0, 704, 98
46475, V, 1, 1, 1, 1, 0, 704, 98
46476, V, 1, 1, 1, 1, 0, 704, 98
46477, V, 1, 1, 1, 1, 0, 704, 98
46478, V, 1, 1, 1, 1, 0, 704, 98
46479, V, 1, 1, 1, 1, 0, 704, 98
46480, V, 1, 1, 1, 1, 0, 704, 98
46481, V, 1, 1, 1, 1, 0, 704, 98
46482, V, 1, 1, 1, 1, 0, 704, 98
46483, V, 1, 1, 1, 1, 0, 704, 98
46484, V, 1, 1, 1, 1, 0, 704, 98
46485, V, 1, 1, 1, 1, 0, 704, 99
46486, V, 1, 1, 1, 1, 0, 704, 98
46487, V, 1, 1, 1, 1, 0, 704, 98
46488, V, 1, 1, 1, 1, 0, 704, 98
46489, V, 1, 1, 1, 1, 0, 704, 98
46490, V, 1, 1, 1, 1, 0, 704, 98
46491, V, 1, 1, 1, 1, 0, 704, 98
46492, V, 1, 1, 1, 1, 0, 704, 98
46493, V, 1, 1, 1, 1, 0, 704, 98
46494, V, 1, 1, 1, 1, 0, 704, 98
46495, V, 1, 1, 1, 1, 0, 704, 98
46496, V, 1, 1, 1, 1, 0, 704, 98
46497, V, 1, 1, 1, 1, 0, 704, 98
46498, V, 1, 1, 1, 1, 0, 704, 98
46499, V, 1, 1, 1, 1, 0, 704, 98
46500, V, 1, 1, 1, 1, 0, 704, 98
46501, V, 1, 1, 1, 1, 0, 704, 98
46502, V, 1, 1, 1, 1, 0, 704, 98
46503, V, 1, 1, 1, 1, 0, 704, 98
46504, V, 1, 1, 1, 1, 0, 704, 98
46505, V, 1, 1, 1, 1, 0, 704, 98
46507, V, 1, 1, 1, 1, 0, 704, 98
46508, V, 1, 1, 1, 1, 0, 704, 98
46509, V, 1, 1, 1, 1, 0, 704, 98
46510, V, 1, 1, 1, 1, 0, 704, 98
46511, V, 1, 1, 1, 1, 0, 704, 98
46512, V, 1, 1, 1, 1, 0, 704, 98
46513, V, 1, 1, 1, 1, 0, 704, 98
46514, V, 1, 1, 1, 1, 0, 704, 98
46515, V, 1, 1, 1, 1, 0, 704, 98
46516, V, 1, 1, 1, 1, 0, 704, 98
46517, V, 1, 1, 1, 1, 0, 704, 98
46518, V, 1, 1, 1, 1, 0, 704, 98
46519, V, 1, 1, 1, 1, 0, 704, 98
46520, V, 1, 1, 1, 1, 0, 704, 98
46521, V, 1, 1, 1, 1, 0, 704, 98
46522, V, 1, 1, 1, 1, 0, 704, 98
46523, V, 1, 1, 1, 1, 0, 704, 98
46524, V, 1, 1, 1, 1, 0, 704, 98
46525, V, 1, 1, 1, 1, 0, 704, 98
46526, V, 1, 1, 1, 1, 0, 704, 98
46527, V, 1, 1, 1, 1, 0, 704, 98
46528, V, 1, 1, 1, 1, 0, 704, 98
46529, V, 1, 1, 1, 1, 0, 704, 98
46530, V, 1, 1, 1, 1, 0, 704, 98
46531, V, 1, 1, 1, 1, 0, 704, 98
46532, V, 1, 1, 1, 1, 0, 704, 98
46533, V, 1, 1, 1, 1, 0, 704, 98
46534, V, 1, 1, 1, 1, 0, 704, 98
46535, V, 1, 1, 1, 1, 0, 704, 98
46536, V, 1, 1, 1, 1, 0, 704, 98
46537, V, 1, 1, 1, 1, 0, 704, 98
46538, V, 1, 1, 1, 1, 0, 704, 98
46539, V, 1, 1, 1, 1, 0, 704, 98
46540, V, 1, 1, 1, 1, 0, 704, 98
46541, V, 1, 1, 1, 1, 0, 704, 98
46542, V, 1, 1, 1, 1, 0, 704, 98
46543, V, 1, 1, 1, 1, 0, 704, 98
46544, V, 1, 1, 1, 1, 0, 704, 98
46545, V, 1, 1, 1, 1, 0, 704, 98
46546, V, 1, 1, 1, 1, 0, 704, 98
46547, V, 1, 1, 1, 1, 0, 704, 98
46548, V, 1, 1, 1, 1, 0, 704, 98
46550, V, 1, 1, 1, 1, 0, 704, 98
46551, V, 1, 1, 1, 1, 0, 704, 98
46552, V, 1, 1, 1, 1, 0, 704, 98
46553, V, 1, 1, 1, 1, 0, 704, 98
46554, V, 1, 1, 1, 1, 0, 704, 98
46555, V, 1, 1, 1, 1, 0, 704, 98
46556, V, 1, 1, 1, 1, 0, 704, 98
46557, V, 1, 1, 1, 1, 0, 704, 98
46558, V, 1, 1, 1, 1, 0, 704, 98
46559, V, 1, 1, 1, 1, 0, 704, 98
46560, V, 1, 1, 1, 1, 0, 704, 98
46561, V, 1, 1, 1, 1, 0, 704, 98
46562, V, 1, 1, 1, 1, 0, 704, 98
46563, V, 1, 1, 1, 1, 0, 704, 98
46564, V, 1, 1, 1, 1, 0, 704, 98
46565, V, 1, 1, 1, 1, 0, 704, 98
46566, V, 1, 1, 1, 1, 0, 704, 98
46567, V, 1, 1, 1, 1, 0, 704, 98
46568, V, 1, 1, 1, 1, 0, 704, 98
46569, V, 1, 1, 1, 1, 0, 704, 98
46570, V, 1, 1, 1, 1, 0, 704, 98
46571, V, 1, 1, 1, 1, 0, 704, 98
46572, V, 1, 1, 1, 1, 0, 704, 98
46573, V, 1, 1, 1, 1, 0, 704, 98
46574, V, 1, 1, 1, 1, 0, 704, 98
46575, V, 1, 1, 1, 1, 0, 704, 98
46576, V, 1, 1, 1, 1, 0, 704, 98
46577, V, 1, 1, 1, 1, 0, 704, 98
46578, V, 1, 1, 1, 1, 0, 704, 98
46579, V, 1, 1, 1, 1, 0, 704, 98
46580, V, 1, 1, 1, 1, 0, 704, 98
46581, V, 1, 1, 1, 1, 0, 704, 98
46582, V, 1, 1, 1, 1, 0, 704, 98
46583, V, 1, 1, 1, 1, 0, 704, 98
46584, V, 1, 1, 1, 1, 0, 704, 98
46585, V, 1, 1, 1, 1, 0, 704, 98
46586, V, 1, 1, 1, 1, 0, 704, 98
46587, V, 1, 1, 1, 1, 0, 704, 98
46588, V, 1, 1, 1, 1, 0, 704, 98
46589, V, 1, 1, 1, 1, 0, 704, 98
46590, V, 1, 1, 1, 1, 0, 704, 98
46592, V, 1, 1, 1, 1, 0, 704, 98
46593, V, 1, 1, 1, 1, 0, 704, 98
46594, V, 1, 1, 1, 1, 0, 704, 98
46595, V, 1, 1, 1, 1, 0, 704, 98
46596, V, 1, 1, 1, 1, 0, 704, 98
46597, V, 1, 1, 1, 1, 0, 704, 98
46598, V, 1, 1, 1, 1, 0, 704, 98
46599, V, 1, 1, 1, 1, 0, 704, 98
46600, V, 1, 1, 1, 1, 0, 704, 98
46601, V, 1, 1, 1, 1, 0, 704, 98
46602, V, 1, 1, 1, 1, 0, 704, 98
46603, V, 1, 1, 1, 1, 0, 704, 98
46604, V, 1, 1, 1, 1, 0, 704, 98
46605, V, 1, 1, 1, 1, 0, 704, 98
46606, V, 1, 1, 1, 1, 0, 704, 98
46607, V, 1, 1, 1, 1, 0, 704, 98
46608, V, 1, 1, 1, 1, 0, 704, 98
46609, V, 1, 1, 1, 1, 0, 704, 98
46610, V, 1, 1, 1, 1, 0, 704, 98
46611, V, 1, 1, 1, 1, 0, 704, 98
46612, V, 1, 1, 1, 1, 0, 704, 98
46613, V, 1, 1, 1, 1, 0, 704, 98
46614, V, 1, 1, 1, 1, 0, 704, 98
46615, V, 1, 1, 1, 1, 0, 704, 98
46616, V, 1, 1, 1, 1, 0, 704, 98
46617, V, 1, 1, 1, 1, 0, 704, 98
46618, V, 1, 1, 1, 1, 0, 704, 98
46619, V, 1, 1, 1, 1, 0, 704, 98
46620, V, 1, 1, 1, 1, 0, 704, 98
46621, V, 1, 1, 1, 1, 0, 704, 98
46622, V, 1, 1, 1, 1, 0, 704, 98
46623, V, 1, 1, 1, 1, 0, 704, 98
46624, V, 1, 1, 1, 1, 0, 704, 98
46625, V, 1, 1, 1, 1, 0, 704, 98
46626, V, 1, 1, 1, 1, 0, 704, 98
46627, V, 1, 1, 1, 1, 0, 704, 98
46628, V, 1, 1, 1, 1, 0, 704, 98
46629, V, 1, 1, 1, 1, 0, 704, 98
46630, V, 1, 1, 1, 1, 0, 704, 98
46631, V, 1, 1, 1, 1, 0, 704, 98
46632, V, 1, 1, 1, 1, 0, 704, 98
46633, V, 1, 1, 1, 1, 0, 704, 98
46635, V, 1, 1, 1, 1, 0, 704, 98
46636, V, 1, 1, 1, 1, 0, 704, 98
46637, V, 1, 1, 1, 1, 0, 704, 98
46638, V, 1, 1, 1, 1, 0, 704, 98
46639, V, 1, 1, 1, 1, 0, 704, 98
46640, V, 1, 1, 1, 1, 0, 704, 98
46641, V, 1, 1, 1, 1, 0, 704, 98
46642, V, 1, 1, 1, 1, 0, 704, 98
46643, V, 1, 1, 1, 1, 0, 704, 98
46644, V, 1, 1, 1, 1, 0, 704, 98
46645, V, 1, 1, 1, 1, 0, 704, 98
46646, V, 1, 1, 1, 1, 0, 704, 98
46647, V, 1, 1, 1, 1, 0, 704, 98
46648, V, 1, 1, 1, 1, 0, 704, 98
46649, V, 1, 1, 1, 1, 0, 704, 98
46650, V, 1, 1, 1, 1, 0, 704, 98
46651, V, 1, 1, 1, 1, 0, 704, 98
46652, V, 1, 1, 1, 1, 0, 704, 98
46653, V, 1, 1, 1, 1, 0, 704, 98
46654, V, 1, 1, 1, 1, 0, 704, 98
46655, V, 1, 1, 1, 1, 0, 704, 98
46656, V, 1, 1, 1, 1, 0, 704, 98
46657, V, 1, 1, 1, 1, 0, 704, 98
46658, V, 1, 1, 1, 1, 0, 704, 98
46659, V, 1, 1, 1, 1, 0, 704, 98
46660, V, 1, 1, 1, 1, 0, 704, 98
46661, V, 1, 1, 1, 1, 0, 704, 98
46662, V, 1, 1, 1, 1, 0, 704, 98
46663, V, 1, 1, 1, 1, 0, 704, 98
46664, V, 1, 1, 1, 1, 0, 704, 98
46665, V, 1, 1, 1, 1, 0, 704, 98
46666, V, 1, 1, 1, 1, 0, 704, 98
46667, V, 1, 1, 1, 1, 0, 704, 98
46668, V, 1, 1, 1, 1, 0, 704, 98
46669, V, 1, 1, 1, 1, 0, 704, 98
46670, V, 1, 1, 1, 1, 0, 704, 98
46671, V, 1, 1, 1, 1, 0, 704, 98
46672, V, 1, 1, 1, 1, 0, 704, 98
46673, V, 1, 1, 1, 1, 0, 704, 98
46674, V, 1, 1, 1, 1, 0, 704, 98
46675, V, 1, 1, 1, 1, 0, 704, 98
46676, V, 1, 1, 1, 1, 0, 704, 98
46678, V, 1, 1, 1, 1, 0, 704, 98
46679, V, 1, 1, 1, 1, 0, 704, 98
46680, V, 1, 1, 1, 1, 0, 704, 98
46681, V, 1, 1, 1, 1, 0, 704, 98
46682, V, 1, 1, 1, 1, 0, 704, 98
46683, V, 1, 1, 1, 1, 0, 704, 98
46684, V, 1, 1, 1, 1, 0, 704, 98
46685, V, 1, 1, 1, 1, 0, 704, 98
46686, V, 1, 1, 1, 1, 0, 704, 98
46687, V, 1, 1, 1, 1, 0, 704, 98
46688, V, 1, 1, 1, 1, 0, 704, 98
46689, V, 1, 1, 1, 1, 0, 704, 98
46690, V, 1, 1, 1, 1, 0, 704, 98
46691, V, 1, 1, 1, 1, 0, 704, 98
46692, V, 1, 1, 1, 1, 0, 704, 98
46693, V, 1, 1, 1, 1, 0, 704, 98
46694, V, 1, 1, 1, 1, 0, 704, 98
46695, V, 1, 1, 1, 1, 0, 704, 98
46696, V, 1, 1, 1, 1, 0, 704, 98
46697, V, 1, 1, 1, 1, 0, 704, 98
46698, V, 1, 1, 1, 1, 0, 704, 98
46699, V, 1, 1, 1, 1, 0, 704, 98
46700, V, 1, 1, 1, 1, 0, 704, 98
46701, V, 1, 1, 1, 1, 0, 704, 98
46702, V, 1, 1, 1, 1, 0, 704, 98
46703, V, 1, 1, 1, 1, 0, 704, 98
46704, V, 1, 1, 1, 1, 0, 704, 98
46705, V, 1, 1, 1, 1, 0, 704, 98
46706, V, 1, 1, 1, 1, 0, 704, 98
46707, V, 1, 1, 1, 1, 0, 704, 98
46708, V, 1, 1, 1, 1, 0, 704, 98
46709, V, 1, 1, 1, 1, 0, 704, 98
46710, V, 1, 1, 1, 1, 0, 704, 98
46711, V, 1, 1, 1, 1, 0, 704, 98
46712, V, 1, 1, 1, 1, 0, 704, 98
46713, V, 1, 1, 1, 1, 0, 704, 98
46714, V, 1, 1, 1, 1, 0, 704, 98
46715, V, 1, 1, 1, 1, 0, 704, 98
46716, V, 1, 1, 1, 1, 0, 704, 98
46717, V, 1, 1, 1, 1, 0, 704, 98
46718, V, 1, 1, 1, 1, 0, 704, 98
46720, V, 1, 1, 1, 1, 0, 704, 98
46721, V, 1, 1, 1, 1, 0, 704, 98
46722, V, 1, 1, 1, 1, 0, 704, 98
46723, V, 1, 1, 1, 1, 0, 704, 98
46724, V, 1, 1, 1, 1, 0, 704, 98
46725, V, 1, 1, 1, 1, 0, 704, 98
46726, V, 1, 1, 1, 1, 0, 704, 98
46727, V, 1, 1, 1, 1, 0, 704, 98
46728, V, 1, 1, 1, 1, 0, 704, 98
46729, V, 1, 1, 1, 1, 0, 704, 98
46730, V, 1, 1, 1, 1, 0, 704, 98
46731, V, 1, 1, 1, 1, 0, 704, 98
46732, V, 1, 1, 1, 1, 0, 704, 98
46733, V, 1, 1, 1, 1, 0, 704, 98
46734, V, 1, 1, 1, 1, 0, 704, 98
46735, V, 1, 1, 1, 1, 0, 704, 99
46736, V, 1, 1, 1, 1, 0, 704, 98
46737, V, 1, 1, 1, 1, 0, 704, 99
46738, V, 1, 1, 1, 1, 0, 704, 99
46739, V, 1, 1, 1, 1, 0, 704, 99
46740, V, 1, 1, 1, 1, 0, 704, 99
46741, V, 1, 1, 1, 1, 0, 704, 99
46742, V, 1, 1, 1, 1, 0, 704, 99
46743, V, 1, 1, 1, 1, 0, 704, 99
46744, V, 1, 1, 1, 1, 0, 704, 99
46745, V, 1, 1, 1, 1, 0, 704, 99
46746, V, 1, 1, 1, 1, 0, 704, 99
46747, V, 1, 1, 1, 1, 0, 704, 99
46748, V, 1, 1, 1, 1, 0, 704, 99
46749, V, 1, 1, 1, 1, 0, 704, 99
46750, V, 1, 1, 1, 1, 0, 704, 99
46751, V, 1, 1, 1, 1, 0, 704, 99
46752, V, 1, 1, 1, 1, 0, 704, 99
46753, V, 1, 1, 1, 1, 0, 704, 99
46754, V, 1, 1, 1, 1, 0, 704, 99
46755, V, 1, 1, 1, 1, 0, 704, 99
46756, V, 1, 1, 1, 1, 0, 704, 99
46757, V, 1, 1, 1, 1, 0, 704, 99
46758, V, 1, 1, 1, 1, 0, 704, 99
46759, V, 1, 1, 1, 1, 0, 704, 99
46760, V, 1, 1, 1, 1, 0, 704, 99
46761, V, 1, 1, 1, 1, 0, 704, 99
46763, V, 1, 1, 1, 1, 0, 704, 99
46764, V, 1, 1, 1, 1, 0, 704, 99
46765, V, 1, 1, 1, 1, 0, 704, 99
46766, V, 1, 1, 1, 1, 0, 704, 99
46767, V, 1, 1, 1, 1, 0, 704, 99
46768, V, 1, 1, 1, 1, 0, 704, 99
46769, V, 1, 1, 1, 1, 0, 704, 99
46770, V, 1, 1, 1, 1, 0, 704, 99
46771, V, 1, 1, 1, 1, 0, 704, 99
46772, V, 1, 1, 1, 1, 0, 704, 99
46773, V, 1, 1, 1, 1, 0, 704, 99
46774, V, 1, 1, 1, 1, 0, 704, 99
46775, V, 1, 1, 1, 1, 0, 704, 99
46776, V, 1, 1, 1, 1, 0, 704, 99
46777, V, 1, 1, 1, 1, 0, 704, 99
46778, V, 1, 1, 1, 1, 0, 704, 99
46779, V, 1, 1, 1, 1, 0, 704, 99
46780, V, 1, 1, 1, 1, 0, 704, 99
46781, V, 1, 1, 1, 1, 0, 704, 99
46782, V, 1, 1, 1, 1, 0, 704, 99
46783, V, 1, 1, 1, 1, 0, 704, 99
46784, V, 1, 1, 1, 1, 0, 704, 99
46785, V, 1, 1, 1, 1, 0, 704, 99
46786, V, 1, 1, 1, 1, 0, 704, 99
46787, V, 1, 1, 1, 1, 0, 704, 99
46788, V, 1, 1, 1, 1, 0, 704, 99
46789, V, 1, 1, 1, 1, 0, 704, 99
46790, V, 1, 1, 1, 1, 0, 704, 99
46791, V, 1, 1, 1, 1, 0, 704, 99
46792, V, 1, 1, 1, 1, 0, 704, 99
46793, V, 1, 1, 1, 1, 0, 704, 99
46794, V, 1, 1, 1, 1, 0, 704, 99
46795, V, 1, 1, 1, 1, 0, 704, 99
46796, V, 1, 1, 1, 1, 0, 704, 99
46797, V, 1, 1, 1, 1, 0, 704, 99
46798, V, 1, 1, 1, 1, 0, 704, 99
46799, V, 1, 1, 1, 1, 0, 704, 99
46800, V, 1, 1, 1, 1, 0, 704, 99
46801, V, 1, 1, 1, 1, 0, 704, 99
46802, V, 1, 1, 1, 1, 0, 704, 99
46803, V, 1, 1, 1, 1, 0, 704, 99
46804, V, 1, 1, 1, 1, 0, 704, 99
46806, V, 1, 1, 1, 1, 0, 704, 99
46807, V, 1, 1, 1, 1, 0, 704, 99
46808, V, 1, 1, 1, 1, 0, 704, 99
46809, V, 1, 1, 1, 1, 0, 704, 99
46810, V, 1, 1, 1, 1, 0, 704, 99
46811, V, 1, 1, 1, 1, 0, 704, 99
46812, V, 1, 1, 1, 1, 0, 704, 99
46813, V, 1, 1, 1, 1, 0, 704, 99
46814, V, 1, 1, 1, 1, 0, 704, 99
46815, V, 1, 1, 1, 1, 0, 704, 99
46816, V, 1, 1, 1, 1, 0, 704, 99
46817, V, 1, 1, 1, 1, 0, 704, 99
46818, V, 1, 1, 1, 1, 0, 704, 99
46819, V, 1, 1, 1, 1, 0, 704, 99
46820, V, 1, 1, 1, 1, 0, 704, 99
46821, V, 1, 1, 1, 1, 0, 704, 99
46822, V, 1, 1, 1, 1, 0, 704, 99
46823, V, 1, 1, 1, 1, 0, 704, 99
46824, V, 1, 1, 1, 1, 0, 704, 99
46825, V, 1, 1, 1, 1, 0, 704, 99
46826, V, 1, 1, 1, 1, 0, 704, 99
46827, V, 1, 1, 1, 1, 0, 704, 99
46828, V, 1, 1, 1, 1, 0, 704, 99
46829, V, 1, 1, 1, 1, 0, 704, 99
46830, V, 1, 1, 1, 1, 0, 704, 99
46831, V, 1, 1, 1, 1, 0, 704, 99
46832, V, 1, 1, 1, 1, 0, 704, 99
46833, V, 1, 1, 1, 1, 0, 704, 99
46834, V, 1, 1, 1, 1, 0, 704, 99
46835, V, 1, 1, 1, 1, 0, 704, 99
46836, V, 1, 1, 1, 1, 0, 704, 99
46837, V, 1, 1, 1, 1, 0, 704, 99
46838, V, 1, 1, 1, 1, 0, 704, 99
46839, V, 1, 1, 1, 1, 0, 704, 99
46840, V, 1, 1, 1, 1, 0, 704, 99
46841, V, 1, 1, 1, 1, 0, 704, 99
46842, V, 1, 1, 1, 1, 0, 704, 99
46843, V, 1, 1, 1, 1, 0, 704, 99
46844, V, 1, 1, 1, 1, 0, 704, 99
46845, V, 1, 1, 1, 1, 0, 704, 99
46846, V, 1, 1, 1, 1, 0, 704, 99
46848, V, 1, 1, 1, 1, 0, 704, 99
46849, V, 1, 1, 1, 1, 0, 704, 99
46850, V, 1, 1, 1, 1, 0, 704, 99
46851, V, 1, 1, 1, 1, 0, 704, 99
46852, V, 1, 1, 1, 1, 0, 704, 99
46853, V, 1, 1, 1, 1, 0, 704, 99
46854, V, 1, 1, 1, 1, 0, 704, 99
46855, V, 1, 1, 1, 1, 0, 704, 99
46856, V, 1, 1, 1, 1, 0, 704, 99
46857, V, 1, 1, 1, 1, 0, 704, 99
46858, V, 1, 1, 1, 1, 0, 704, 99
46859, V, 1, 1, 1, 1, 0, 704, 99
46860, V, 1, 1, 1, 1, 0, 704, 99
46861, V, 1, 1, 1, 1, 0, 704, 99
46862, V, 1, 1, 1, 1, 0, 704, 99
46863, V, 1, 1, 1, 1, 0, 704, 99
46864, V, 1, 1, 1, 1, 0, 704, 99
46865, V, 1, 1, 1, 1, 0, 704, 99
46866, V, 1, 1, 1, 1, 0, 704, 99
46867, V, 1, 1, 1, 1, 0, 704, 99
46868, V, 1, 1, 1, 1, 0, 704, 99
46869, V, 1, 1, 1, 1, 0, 704, 99
46870, V, 1, 1, 1, 1, 0, 704, 99
46871, V, 1, 1, 1, 1, 0, 704, 99
46872, V, 1, 1, 1, 1, 0, 704, 99
46873, V, 1, 1, 1, 1, 0, 704, 99
46874, V, 1, 1, 1, 1, 0, 704, 99
46875, V, 1, 1, 1, 1, 0, 704, 99
46876, V, 1, 1, 1, 1, 0, 704, 99
46877, V, 1, 1, 1, 1, 0, 704, 99
46878, V, 1, 1, 1, 1, 0, 704, 99
46879, V, 1, 1, 1, 1, 0, 704, 99
46880, V, 1, 1, 1, 1, 0, 704, 99
46881, V, 1, 1, 1, 1, 0, 704, 99
46882, V, 1, 1, 1, 1, 0, 704, 99
46883, V, 1, 1, 1, 1, 0, 704, 99
46884, V, 1, 0, 0, 1, 0, 704, 99
46884, V, 1, 0, 0, 0, 0, 704, 99
46885, V, 1, 1, 0, 0, 0, 704, 99
46885, V, 1, 1, 0, 0, 0, 704, 99
46886, V, 1, 1, 1, 1, 0, 704, 99
46887, V, 1, 1, 1, 1, 0, 704, 99
46888, V, 1, 1, 1, 1, 0, 704, 99
46889, V, 1, 1, 1, 1, 0, 704, 99
46891, V, 1, 1, 1, 1, 0, 704, 99
46892, V, 1, 1, 1, 1, 0, 704, 99
46893, V, 1, 1, 1, 1, 0, 704, 99
46894, V, 1, 1, 1, 1, 0, 704, 99
46895, V, 1, 1, 1, 1, 0, 704, 99
46896, V, 1, 1, 1, 1, 0, 704, 99
46897, V, 1, 1, 1, 1, 0, 704, 99
46898, V, 1, 1, 1, 1, 0, 704, 99
46899, V, 1, 1, 1, 1, 0, 704, 99
46900, V, 1, 1, 1, 1, 0, 704, 99
46901, V, 1, 1, 1, 1, 0, 704, 99
46902, V, 1, 1, 1, 1, 0, 704, 99
46903, V, 1, 1, 1, 1, 0, 704, 99
46904, V, 1, 1, 1, 1, 0, 704, 99
46905, V, 1, 1, 1, 1, 0, 704, 99
46906, V, 1, 1, 1, 1, 0, 704, 99
46907, V, 1, 1, 1, 1, 0, 704, 99
46908, V, 1, 1, 1, 1, 0, 704, 99
46909, V, 1, 1, 1, 1, 0, 704, 99
46910, V, 1, 1, 1, 1, 0, 704, 99
46911, V, 1, 1, 1, 1, 0, 704, 99
46912, V, 1, 1, 1, 1, 0, 704, 99
46913, V, 1, 1, 1, 1, 0, 704, 99
46914, V, 1, 1, 1, 1, 0, 704, 99
46915, V, 1, 1, 1, 1, 0, 704, 99
46916, V, 1, 1, 1, 1, 0, 704, 99
46917, V, 1, 1, 1, 1, 0, 704, 99
46918, V, 1, 1, 1, 1, 0, 704, 99
46919, V, 1, 1, 1, 1, 0, 704, 99
46920, V, 1, 1, 1, 1, 0, 704, 99
46921, V, 1, 1, 1, 1, 0, 704, 99
46922, V, 1, 1, 1, 1, 0, 704, 99
46923, V, 1, 1, 1, 1, 0, 704, 99
46924, V, 1, 1, 1, 1, 0, 704, 99
46925, V, 1, 1, 1, 1, 0, 704, 99
46926, V, 1, 1, 1, 1, 0, 704, 99
46927, V, 1, 1, 1, 1, 0, 704, 99
46928, V, 1, 1, 1, 1, 0, 704, 99
46929, V, 1, 1, 1, 1, 0, 704, 99
46930, V, 1, 1, 1, 1, 0, 704, 99
46931, V, 1, 1, 1, 1, 0, 704, 99
46932, V, 1, 1, 1, 1, 0, 704, 99
46934, V, 1, 1, 1, 1, 0, 704, 99
46935, V, 1, 1, 1, 1, 0, 704, 99
46936, V, 1, 1, 1, 1, 0, 704, 99
46937, V, 1, 1, 1, 1, 0, 704, 99
46938, V, 1, 1, 1, 1, 0, 704, 99
46939, V, 1, 1, 1, 1, 0, 704, 99
46940, V, 1, 1, 1, 1, 0, 704, 99
46941, V, 1, 1, 1, 1, 0, 704, 99
46942, V, 1, 1, 1, 1, 0, 704, 99
46943, V, 1, 1, 1, 1, 0, 704, 99
46944, V, 1, 1, 1, 1, 0, 704, 99
46945, V, 1, 1, 1, 1, 0, 704, 99
46946, V, 1, 1, 1, 1, 0, 704, 99
46947, V, 1, 1, 1, 1, 0, 704, 99
46948, V, 1, 1, 1, 1, 0, 704, 99
46949, V, 1, 1, 1, 1, 0, 704, 99
46950, V, 1, 1, 1, 1, 0, 704, 99
46951, V, 1, 1, 1, 1, 0, 704, 99
46952, V, 1, 1, 1, 1, 0, 704, 99
46953, V, 1, 1, 1, 1, 0, 704, 99
46954, V, 1, 1, 1, 1, 0, 704, 99
46955, V, 1, 1, 1, 1, 0, 704, 99
46956, V, 1, 1, 1, 1, 0, 704, 99
46957, V, 1, 1, 1, 1, 0, 704, 99
46958, V, 1, 1, 1, 1, 0, 704, 99
46959, V, 1, 1, 1, 1, 0, 704, 99
46960, V, 1, 1, 1, 1, 0, 704, 99
46961, V, 1, 1, 1, 1, 0, 704, 99
46962, V, 1, 1, 1, 1, 0, 704, 99
46963, V, 1, 1, 1, 1, 0, 704, 99
46964, V, 1, 1, 1, 1, 0, 704, 99
46965, V, 1, 1, 1, 1, 0, 704, 99
46966, V, 1, 1, 1, 1, 0, 704, 99
46967, V, 1, 1, 1, 1, 0, 704, 99
46968, V, 1, 1, 1, 1, 0, 704, 99
46969, V, 1, 1, 1, 1, 0, 704, 99
46970, V, 1, 1, 1, 1, 0, 704, 99
46971, V, 1, 1, 1, 1, 0, 704, 99
46972, V, 1, 1, 1, 1, 0, 704, 99
46973, V, 1, 1, 1, 1, 0, 704, 99
46974, V, 1, 1, 1, 1, 0, 704, 99
46976, V, 1, 1, 1, 1, 0, 704, 99
46977, V, 1, 1, 1, 1, 0, 704, 99
46978, V, 1, 1, 1, 1, 0, 704, 99
46979, V, 1, 1, 1, 1, 0, 704, 99
46980, V, 1, 1, 1, 1, 0, 704, 99
46981, V, 1, 1, 1, 1, 0, 704, 99
46982, V, 1, 1, 1, 1, 0, 704, 99
46983, V, 1, 1, 1, 1, 0, 704, 99
46984, V, 1, 1, 1, 1, 0, 704, 99
46985, V, 1, 1, 1, 1, 0, 704, 99
46986, V, 1, 1, 1, 1, 0, 704, 99
46987, V, 1, 1, 1, 1, 0, 704, 99
46988, V, 1, 1, 1, 1, 0, 704, 99
46989, V, 1, 1, 1, 1, 0, 704, 99
46990, V, 1, 1, 1, 1, 0, 704, 99
46991, V, 1, 1, 1, 1, 0, 704, 99
46992, V, 1, 1, 1, 1, 0, 704, 99
46993, V, 1, 1, 1, 1, 0, 704, 99
46994, V, 1, 1, 1, 1, 0, 704, 99
46995, V, 1, 1, 1, 1, 0, 704, 99
46996, V, 1, 1, 1, 1, 0, 704, 99
46997, V, 1, 1, 1, 1, 0, 704, 99
46998, V, 1, 1, 1, 1, 0, 704, 99
46999, V, 1, 1, 1, 1, 0, 704, 99
47000, V, 1, 1, 1, 1, 0, 704, 99
47001, V, 1, 1, 1, 1, 0, 704, 99
47002, V, 1, 1, 1, 1, 0, 704, 99
47003, V, 1, 1, 1, 1, 0, 704, 99
47004, V, 1, 1, 1, 1, 0, 704, 99
47005, V, 1, 1, 1, 1, 0, 704, 99
47006, V, 1, 1, 1, 1, 0, 704, 99
47007, V, 1, 1, 1, 1, 0, 704, 99
47008, V, 1, 1, 1, 1, 0, 704, 99
47009, V, 1, 1, 1, 1, 0, 704, 99
47010, V, 1, 1, 1, 1, 0, 704, 99
47011, V, 1, 1, 1, 1, 0, 704, 99
47012, V, 1, 1, 1, 1, 0, 704, 99
47013, V, 1, 1, 1, 1, 0, 704, 99
47014, V, 1, 1, 1, 1, 0, 704, 99
47015, V, 1, 1, 1, 1, 0, 704, 99
47016, V, 1, 1, 1, 1, 0, 704, 99
47017, V, 1, 1, 1, 1, 0, 704, 99
47019, V, 1, 1, 1, 1, 0, 704, 99
47020, V, 1, 1, 1, 1, 0, 704, 99
47021, V, 1, 1, 1, 1, 0, 704, 99
47022, V, 1, 1, 1, 1, 0, 704, 99
47023, V, 1, 1, 1, 1, 0, 704, 99
47024, V, 1, 1, 1, 1, 0, 704, 99
47025, V, 1, 1, 1, 1, 0, 704, 99
47026, V, 1, 1, 1, 1, 0, 704, 99
47027, V, 1, 1, 1, 1, 0, 704, 99
47028, V, 1, 1, 1, 1, 0, 704, 99
47029, V, 1, 1, 1, 1, 0, 704, 99
47030, V, 1, 1, 1, 1, 0, 704, 99
47031, V, 1, 1, 1, 1, 0, 704, 99
47032, V, 1, 1, 1, 1, 0, 704, 99
47033, V, 1, 1, 1, 1, 0, 704, 99
47034, V, 1, 1, 1, 1, 0, 704, 99
47035, V, 1, 1, 1, 1, 0, 704, 99
47036, V, 1, 1, 1, 1, 0, 704, 99
47037, V, 1, 1, 1, 1, 0, 704, 99
47038, V, 1, 1, 1, 1, 0, 704, 99
47039, V, 1, 1, 1, 1, 0, 704, 99
47040, V, 1, 1, 1, 1, 0, 704, 99
47041, V, 1, 1, 1, 1, 0, 704, 99
47042, V, 1, 1, 1, 1, 0, 704, 99
47043, V, 1, 1, 1, 1, 0, 704, 99
47044, V, 1, 1, 1, 1, 0, 704, 99
47045, V, 1, 1, 1, 1, 0, 704, 99
47046, V, 1, 1, 1, 1, 0, 704, 99
47047, V, 1, 1, 1, 1, 0, 704, 99
47048, V, 1, 1, 1, 1, 0, 704, 99
47049, V, 1, 1, 1, 1, 0, 704, 99
47050, V, 1, 1, 1, 1, 0, 704, 99
47051, V, 1, 1, 1, 1, 0, 704, 99
47052, V, 1, 1, 1, 1, 0, 704, 99
47053, V, 1, 1, 1, 1, 0, 704, 99
47054, V, 1, 1, 1, 1, 0, 704, 99
47055, V, 1, 1, 1, 1, 0, 704, 99
47056, V, 1, 1, 1, 1, 0, 704, 99
47057, V, 1, 1, 1, 1, 0, 704, 99
47058, V, 1, 1, 1, 1, 0, 704, 99
47059, V, 1, 1, 1, 1, 0, 704, 99
47060, V, 1, 1, 1, 1, 0, 704, 99
47062, V, 1, 1, 1, 1, 0, 704, 99
47063, V, 1, 1, 1, 1, 0, 704, 99
47064, V, 1, 1, 1, 1, 0, 704, 99
47065, V, 1, 1, 1, 1, 0, 704, 99
47066, V, 1, 1, 1, 1, 0, 704, 99
47067, V, 1, 1, 1, 1, 0, 704, 99
47068, V, 1, 1, 1, 1, 0, 704, 99
47069, V, 1, 1, 1, 1, 0, 704, 99
47070, V, 1, 1, 1, 1, 0, 704, 99
47071, V, 1, 1, 1, 1, 0, 704, 99
47072, V, 1, 1, 1, 1, 0, 704, 99
47073, V, 1, 1, 1, 1, 0, 704, 99
47074, V, 1, 1, 1, 1, 0, 704, 99
47075, V, 1, 1, 1, 1, 0, 704, 99
47076, V, 1, 1, 1, 1, 0, 704, 99
47077, V, 1, 1, 1, 1, 0, 704, 99
47078, V, 1, 1, 1, 1, 0, 704, 99
47079, V, 1, 1, 1, 1, 0, 704, 99
47080, V, 1, 1, 1, 1, 0, 704, 99
47081, V, 1, 1, 1, 1, 0, 704, 99
47082, V, 1, 1, 1, 1, 0, 704, 99
47083, V, 1, 1, 1, 1, 0, 704, 99
47084, V, 1, 1, 1, 1, 0, 704, 99
47085, V, 1, 1, 1, 1, 0, 704, 99
47086, V, 1, 1, 1, 1, 0, 704, 99
47087, V, 1, 1, 1, 1, 0, 704, 99
47088, V, 1, 1, 1, 1, 0, 704, 99
47089, V, 1, 1, 1, 1, 0, 704, 99
47090, V, 1, 1, 1, 1, 0, 704, 99
47091, V, 1, 1, 1, 1, 0, 704, 99
47092, V, 1, 1, 1, 1, 0, 704, 99
47093, V, 1, 1, 1, 1, 0, 704, 99
47094, V, 1, 1, 1, 1, 0, 704, 99
47095, V, 1, 1, 1, 1, 0, 704, 99
47096, V, 1, 1, 1, 1, 0, 704, 99
47097, V, 1, 1, 1, 1, 0, 704, 99
47098, V, 1, 1, 1, 1, 0, 704, 99
47099, V, 1, 1, 1, 1, 0, 704, 99
47100, V, 1, 1, 1, 1, 0, 704, 99
47101, V, 1, 1, 1, 1, 0, 704, 99
47102, V, 1, 1, 1, 1, 0, 704, 99
47104, V, 1, 1, 1, 1, 0, 704, 99
47105, V, 1, 1, 1, 1, 0, 704, 99
47106, V, 1, 1, 1, 1, 0, 704, 99
47107, V, 1, 1, 1, 1, 0, 704, 99
47108, V, 1, 1, 1, 1, 0, 704, 99
47109, V, 1, 1, 1, 1, 0, 704, 99
47110, V, 1, 1, 1, 1, 0, 704, 99
47111, V, 1, 1, 1, 1, 0, 704, 99
47112, V, 1, 1, 1, 1, 0, 704, 99
47113, V, 1, 1, 1, 1, 0, 704, 99
47114, V, 1, 1, 1, 1, 0, 704, 99
47115, V, 1, 1, 1, 1, 0, 704, 99
47116, V, 1, 1, 1, 1, 0, 704, 99
47117, V, 1, 1, 1, 1, 0, 704, 99
47118, V, 1, 1, 1, 1, 0, 704, 99
47119, V, 1, 1, 1, 1, 0, 704, 99
47120, V, 1, 1, 1, 1, 0, 704, 99
47121, V, 1, 1, 1, 1, 0, 704, 99
47122, V, 1, 1, 1, 1, 0, 704, 99
47123, V, 1, 1, 1, 1, 0, 704, 99
47124, V, 1, 1, 1, 1, 0, 704, 99
47125, V, 1, 1, 1, 1, 0, 704, 99
47126, V, 1, 1, 1, 1, 0, 704, 99
47127, V, 1, 1, 1, 1, 0, 704, 99
47128, V, 1, 1, 1, 1, 0, 704, 99
47129, V, 1, 1, 1, 1, 0, 704, 99
47130, V, 1, 1, 1, 1, 0, 704, 99
47131, V, 1, 1, 1, 1, 0, 704, 99
47132, V, 1, 1, 1, 1, 0, 704, 99
47133, V, 1, 1, 1, 1, 0, 704, 99
47134, V, 1, 1, 1, 1, 0, 704, 99
47135, V, 1, 1, 1, 1, 0, 704, 99
47136, V, 1, 1, 1, 1, 0, 704, 99
47137, V, 1, 1, 1, 1, 0, 704, 99
47138, V, 1, 1, 1, 1, 0, 704, 99
47139, V, 1, 1, 1, 1, 0, 704, 99
47140, V, 1, 1, 1, 1, 0, 704, 99
47141, V, 1, 1, 1, 1, 0, 704, 99
47142, V, 1, 1, 1, 1, 0, 704, 99
47143, V, 1, 1, 1, 1, 0, 704, 99
47144, V, 1, 1, 1, 1, 0, 704, 99
47145, V, 1, 1, 1, 1, 0, 704, 99
47147, V, 1, 1, 1, 1, 0, 704, 99
47148, V, 1, 1, 1, 1, 0, 704, 99
47149, V, 1, 1, 1, 1, 0, 704, 99
47150, V, 1, 1, 1, 1, 0, 704, 99
47151, V, 1, 1, 1, 1, 0, 704, 99
47152, V, 1, 1, 1, 1, 0, 704, 99
47153, V, 1, 1, 1, 1, 0, 704, 99
47154, V, 1, 1, 1, 1, 0, 704, 99
47155, V, 1, 1, 1, 1, 0, 704, 99
47156, V, 1, 1, 1, 1, 0, 704, 99
47157, V, 1, 1, 1, 1, 0, 704, 99
47158, V, 1, 1, 1, 1, 0, 704, 99
47159, V, 1, 1, 1, 1, 0, 704, 99
47160, V, 1, 1, 1, 1, 0, 704, 99
47161, V, 1, 1, 1, 1, 0, 704, 99
47162, V, 1, 1, 1, 1, 0, 704, 99
47163, V, 1, 1, 1, 1, 0, 704, 99
47164, V, 1, 1, 1, 1, 0, 704, 99
47165, V, 1, 1, 1, 1, 0, 704, 99
47166, V, 1, 1, 1, 1, 0, 704, 99
47167, V, 1, 1, 1, 1, 0, 704, 99
47168, V, 1, 1, 1, 1, 0, 704, 99
47169, V, 1, 1, 1, 1, 0, 704, 99
47170, V, 1, 1, 1, 1, 0, 704, 99
47171, V, 1, 1, 1, 1, 0, 704, 99
47172, V, 1, 1, 1, 1, 0, 704, 99
47173, V, 1, 1, 1, 1, 0, 704, 99
47174, V, 1, 1, 1, 1, 0, 704, 99
47175, V, 1, 1, 1, 1, 0, 704, 99
47176, V, 1, 1, 1, 1, 0, 704, 99
47177, V, 1, 1, 1, 1, 0, 704, 99
47178, V, 1, 1, 1, 1, 0, 704, 99
47179, V, 1, 1, 1, 1, 0, 704, 99
47180, V, 1, 1, 1, 1, 0, 704, 99
47181, V, 1, 1, 1, 1, 0, 704, 99
47182, V, 1, 1, 1, 1, 0, 704, 99
47183, V, 1, 1, 1, 1, 0, 704, 99
47184, V, 1, 1, 1, 1, 0, 704, 99
47185, V, 1, 1, 1, 1, 0, 704, 99
47186, V, 1, 1, 1, 1, 0, 704, 99
47187, V, 1, 1, 1, 1, 0, 704, 99
47188, V, 1, 1, 1, 1, 0, 704, 99
47190, V, 1, 1, 1, 1, 0, 704, 99
47191, V, 1, 1, 1, 1, 0, 704, 99
47192, V, 1, 1, 1, 1, 0, 704, 99
47193, V, 1, 1, 1, 1, 0, 704, 99
47194, V, 1, 1, 1, 1, 0, 704, 99
47195, V, 1, 1, 1, 1, 0, 704, 99
47196, V, 1, 1, 1, 1, 0, 704, 99
47197, V, 1, 1, 1, 1, 0, 704, 99
47198, V, 1, 1, 1, 1, 0, 704, 99
47199, V, 1, 1, 1, 1, 0, 704, 99
47200, V, 1, 1, 1, 1, 0, 704, 99
47201, V, 1, 1, 1, 1, 0, 704, 99
47202, V, 1, 1, 1, 1, 0, 704, 99
47203, V, 1, 1, 1, 1, 0, 704, 99
47204, V, 1, 1, 1, 1, 0, 704, 99
47205, V, 1, 1, 1, 1, 0, 704, 99
47206, V, 1, 1, 1, 1, 0, 704, 99
47207, V, 1, 1, 1, 1, 0, 704, 99
47208, V, 1, 1, 1, 1, 0, 704, 99
47209, V, 1, 1, 1, 1, 0, 704, 99
47210, V, 1, 1, 1, 1, 0, 704, 99
47211, V, 1, 1, 1, 1, 0, 704, 99
47212, V, 1, 1, 1, 1, 0, 704, 99
47213, V, 1, 1, 1, 1, 0, 704, 99
47214, V, 1, 1, 1, 1, 0, 704, 99
47215, V, 1, 1, 1, 1, 0, 704, 99
47216, V, 1, 1, 1, 1, 0, 704, 99
47217, V, 1, 1, 1, 1, 0, 704, 99
47218, V, 1, 1, 1, 1, 0, 704, 99
47219, V, 1, 1, 1, 1, 0, 704, 99
47220, V, 1, 1, 1, 1, 0, 704, 99
47221, V, 1, 1, 1, 1, 0, 704, 99
47222, V, 1, 1, 1, 1, 0, 704, 99
47223, V, 1, 1, 1, 1, 0, 704, 99
47224, V, 1, 1, 1, 1, 0, 704, 99
47225, V, 1, 1, 1, 1, 0, 704, 99
47226, V, 1, 1, 1, 1, 0, 704, 99
47227, V, 1, 1, 1, 1, 0, 704, 99
47228, V, 1, 1, 1, 1, 0, 704, 99
47229, V, 1, 1, 1, 1, 0, 704, 99
47230, V, 1, 1, 1, 1, 0, 704, 99
47232, V, 1, 1, 1, 1, 0, 704, 99
47233, V, 1, 1, 1, 1, 0, 704, 99
47234, V, 1, 1, 1, 1, 0, 704, 99
47235, V, 1, 1, 1, 1, 0, 704, 99
47236, V, 1, 1, 1, 1, 0, 704, 99
47237, V, 1, 1, 1, 1, 0, 704, 99
47238, V, 1, 1, 1, 1, 0, 704, 99
47239, V, 1, 1, 1, 1, 0, 704, 99
47240, V, 1, 1, 1, 1, 0, 704, 99
47241, V, 1, 1, 1, 1, 0, 704, 99
47242, V, 1, 1, 1, 1, 0, 704, 99
47243, V, 1, 1, 1, 1, 0, 704, 99
47244, V, 1, 1, 1, 1, 0, 704, 99
47245, V, 1, 1, 1, 1, 0, 704, 99
47246, V, 1, 1, 1, 1, 0, 704, 99
47247, V, 1, 1, 1, 1, 0, 704, 99
47248, V, 1, 1, 1, 1, 0, 704, 99
47249, V, 1, 1, 1, 1, 0, 704, 99
47250, V, 1, 1, 1, 1, 0, 704, 99
47251, V, 1, 1, 1, 1, 0, 704, 99
47252, V, 1, 1, 1, 1, 0, 704, 99
47253, V, 1, 1, 1, 1, 0, 704, 99
47254, V, 1, 1, 1, 1, 0, 704, 99
47255, V, 1, 1, 1, 1, 0, 704, 99
47256, V, 1, 1, 1, 1, 0, 704, 99
47257, V, 1, 1, 1, 1, 0, 704, 99
47258, V, 1, 1, 1, 1, 0, 704, 99
47259, V, 1, 1, 1, 1, 0, 704, 99
47260, V, 1, 1, 1, 1, 0, 704, 99
47261, V, 1, 1, 1, 1, 0, 704, 99
47262, V, 1, 1, 1, 1, 0, 704, 99
47263, V, 1, 1, 1, 1, 0, 704, 99
47264, V, 1, 1, 1, 1, 0, 704, 99
47265, V, 1, 1, 1, 1, 0, 704, 99
47266, V, 1, 1, 1, 1, 0, 704, 99
47267, V, 1, 1, 1, 1, 0, 704, 99
47268, V, 1, 1, 1, 1, 0, 704, 99
47269, V, 1, 1, 1, 1, 0, 704, 99
47270, V, 1, 1, 1, 1, 0, 704, 99
47271, V, 1, 1, 1, 1, 0, 704, 99
47272, V, 1, 1, 1, 1, 0, 704, 99
47273, V, 1, 1, 1, 1, 0, 704, 99
47275, V, 1, 1, 1, 1, 0, 704, 99
47276, V, 1, 1, 1, 1, 0, 704, 99
47277, V, 1, 1, 1, 1, 0, 704, 99
47278, V, 1, 1, 1, 1, 0, 704, 99
47279, V, 1, 1, 1, 1, 0, 704, 99
47280, V, 1, 1, 1, 1, 0, 704, 99
47281, V, 1, 1, 1, 1, 0, 704, 99
47282, V, 1, 1, 1, 1, 0, 704, 99
47283, V, 1, 1, 1, 1, 0, 704, 99
47284, V, 1, 1, 1, 1, 0, 704, 99
47285, V, 1, 1, 1, 1, 0, 704, 99
47286, V, 1, 1, 1, 1, 0, 704, 99
47287, V, 1, 1, 1, 1, 0, 704, 99
47288, V, 1, 1, 1, 1, 0, 704, 99
47289, V, 1, 1, 1, 1, 0, 704, 99
47290, V, 1, 1, 1, 1, 0, 704, 99
47291, V, 1, 1, 1, 1, 0, 704, 99
47292, V, 1, 1, 1, 1, 0, 704, 99
47293, V, 1, 1, 1, 1, 0, 704, 99
47294, V, 1, 1, 1, 1, 0, 704, 99
47295, V, 1, 1, 1, 1, 0, 704, 99
47296, V, 1, 1, 1, 1, 0, 704, 99
47297, V, 1, 1, 1, 1, 0, 704, 99
47298, V, 1, 1, 1, 1, 0, 704, 99
47299, V, 1, 1, 1, 1, 0, 704, 99
47300, V, 1, 1, 1, 1, 0, 704, 99
47301, V, 1, 1, 1, 1, 0, 704, 99
47302, V, 1, 1, 1, 1, 0, 704, 99
47303, V, 1, 1, 1, 1, 0, 704, 99
47304, V, 1, 1, 1, 1, 0, 704, 99
47305, V, 1, 1, 1, 1, 0, 704, 99
47306, V, 1, 1, 1, 1, 0, 704, 99
47307, V, 1, 1, 1, 1, 0, 704, 99
47308, V, 1, 1, 1, 1, 0, 704, 99
47309, V, 1, 1, 1, 1, 0, 704, 99
47310, V, 1, 1, 1, 1, 0, 704, 99
47311, V, 1, 1, 1, 1, 0, 704, 99
47312, V, 1, 1, 1, 1, 0, 704, 99
47313, V, 1, 1, 1, 1, 0, 704, 99
47314, V, 1, 1, 1, 1, 0, 704, 99
47315, V, 1, 1, 1, 1, 0, 704, 99
47316, V, 1, 1, 1, 1, 0, 704, 99
47318, V, 1, 1, 1, 1, 0, 704, 99
47319, V, 1, 1, 1, 1, 0, 704, 99
47320, V, 1, 1, 1, 1, 0, 704, 99
47321, V, 1, 1, 1, 1, 0, 704, 99
47322, V, 1, 1, 1, 1, 0, 704, 99
47323, V, 1, 1, 1, 1, 0, 704, 99
47324, V, 1, 1, 1, 1, 0, 704, 99
47325, V, 1, 1, 1, 1, 0, 704, 99
47326, V, 1, 1, 1, 1, 0, 704, 99
47327, V, 1, 1, 1, 1, 0, 704, 99
47328, V, 1, 1, 1, 1, 0, 704, 99
47329, V, 1, 1, 1, 1, 0, 704, 99
47330, V, 1, 1, 1, 1, 0, 704, 99
47331, V, 1, 1, 1, 1, 0, 704, 99
47332, V, 1, 1, 1, 1, 0, 704, 99
47333, V, 1, 1, 1, 1, 0, 704, 99
47334, V, 1, 1, 1, 1, 0, 704, 99
47335, V, 1, 1, 1, 1, 0, 704, 99
47336, V, 1, 1, 1, 1, 0, 704, 99
47337, V, 1, 1, 1, 1, 0, 704, 99
47338, V, 1, 1, 1, 1, 0, 704, 99
47339, V, 1, 1, 1, 1, 0, 704, 99
47340, V, 1, 1, 1, 1, 0, 704, 99
47341, V, 1, 1, 1, 1, 0, 704, 99
47342, V, 1, 1, 1, 1, 0, 704, 99
47343, V, 1, 1, 1, 1, 0, 704, 99
47344, V, 1, 1, 1, 1, 0, 704, 99
47345, V, 1, 1, 1, 1, 0, 704, 99
47346, V, 1, 1, 1, 1, 0, 704, 99
47347, V, 1, 1, 1, 1, 0, 704, 99
47348, V, 1, 1, 1, 1, 0, 704, 99
47349, V, 1, 1, 1, 1, 0, 704, 99
47350, V, 1, 1, 1, 1, 0, 704, 99
47351, V, 1, 1, 1, 1, 0, 704, 99
47352, V, 1, 1, 1, 1, 0, 704, 99
47353, V, 1, 1, 1, 1, 0, 704, 99
47354, V, 1, 1, 1, 1, 0, 704, 99
47355, V, 1, 1, 1, 1, 0, 704, 99
47356, V, 1, 1, 1, 1, 0, 704, 99
47357, V, 1, 1, 1, 1, 0, 704, 99
47358, V, 1, 1, 1, 1, 0, 704, 99
47360, V, 1, 1, 1, 1, 0, 704, 99
47361, V, 1, 1, 1, 1, 0, 704, 99
47362, V, 1, 1, 1, 1, 0, 704, 99
47363, V, 1, 1, 1, 1, 0, 704, 99
47364, V, 1, 1, 1, 1, 0, 704, 99
47365, V, 1, 1, 1, 1, 0, 704, 99
47366, V, 1, 1, 1, 1, 0, 704, 99
47367, V, 1, 1, 1, 1, 0, 704, 99
47368, V, 1, 1, 1, 1, 0, 704, 99
47369, V, 1, 1, 1, 1, 0, 704, 99
47370, V, 1, 1, 1, 1, 0, 704, 99
47371, V, 1, 1, 1, 1, 0, 704, 99
47372, V, 1, 1, 1, 1, 0, 704, 99
47373, V, 1, 1, 1, 1, 0, 704, 99
47374, V, 1, 1, 1, 1, 0, 704, 99
47375, V, 1, 1, 1, 1, 0, 704, 99
47376, V, 1, 1, 1, 1, 0, 704, 99
47377, V, 1, 1, 1, 1, 0, 704, 99
47378, V, 1, 1, 1, 1, 0, 704, 99
47379, V, 1, 1, 1, 1, 0, 704, 99
47380, V, 1, 1, 1, 1, 0, 704, 99
47381, V, 1, 1, 1, 1, 0, 704, 99
47382, V, 1, 1, 1, 1, 0, 704, 99
47383, V, 1, 1, 1, 1, 0, 704, 99
47384, V, 1, 1, 1, 1, 0, 704, 99
47385, V, 1, 1, 1, 1, 0, 704, 99
47386, V, 1, 1, 1, 1, 0, 704, 99
47387, V, 1, 1, 1, 1, 0, 704, 99
47388, V, 1, 1, 1, 1, 0, 704, 99
47389, V, 1, 1, 1, 1, 0, 704, 99
47390, V, 1, 1, 1, 1, 0, 704, 99
47391, V, 1, 1, 1, 1, 0, 704, 99
47392, V, 1, 1, 1, 1, 0, 704, 99
47393, V, 1, 1, 1, 1, 0, 704, 99
47394, V, 1, 1, 1, 1, 0, 704, 99
47395, V, 1, 1, 1, 1, 0, 704, 99
47396, V, 1, 1, 1, 1, 0, 704, 99
47397, V, 1, 1, 1, 1, 0, 704, 99
47398, V, 1, 1, 1, 1, 0, 704, 99
47399, V, 1, 1, 1, 1, 0, 704, 99
47400, V, 1, 1, 1, 1, 0, 704, 99
47401, V, 1, 1, 1, 1, 0, 704, 99
47403, V, 1, 1, 1, 1, 0, 704, 99
47404, V, 1, 1, 1, 1, 0, 704, 99
47405, V, 1, 1, 1, 1, 0, 704, 99
47406, V, 1, 1, 1, 1, 0, 704, 99
47407, V, 1, 1, 1, 1, 0, 704, 99
47408, V, 1, 1, 1, 1, 0, 704, 99
47409, V, 1, 1, 1, 1, 0, 704, 99
47410, V, 1, 1, 1, 1, 0, 704, 99
47411, V, 1, 1, 1, 1, 0, 704, 99
47412, V, 1, 1, 1, 1, 0, 704, 99
47413, V, 1, 1, 1, 1, 0, 704, 99
47414, V, 1, 1, 1, 1, 0, 704, 99
47415, V, 1, 1, 1, 1, 0, 704, 99
47416, V, 1, 1, 1, 1, 0, 704, 99
47417, V, 1, 1, 1, 1, 0, 704, 99
47418, V, 1, 1, 1, 1, 0, 704, 99
47419, V, 1, 1, 1, 1, 0, 704, 99
47420, V, 1, 1, 1, 1, 0, 704, 99
47421, V, 1, 1, 1, 1, 0, 704, 99
47422, V, 1, 1, 1, 1, 0, 704, 99
47423, V, 1, 1, 1, 1, 0, 704, 99
47424, V, 1, 1, 1, 1, 0, 704, 99
47425, V, 1, 1, 1, 1, 0, 704, 99
47426, V, 1, 1, 1, 1, 0, 704, 99
47427, V, 1, 1, 1, 1, 0, 704, 99
47428, V, 1, 1, 1, 1, 0, 704, 99
47429, V, 1, 1, 1, 1, 0, 704, 99
47430, V, 1, 1, 1, 1, 0, 704, 99
47431, V, 1, 1, 1, 1, 0, 704, 99
47432, V, 1, 1, 1, 1, 0, 704, 99
47433, V, 1, 1, 1, 1, 0, 704, 99
47434, V, 1, 1, 1, 1, 0, 704, 99
47435, V, 1, 1, 1, 1, 0, 704, 99
47436, V, 1, 1, 1, 1, 0, 704, 99
47437, V, 1, 1, 1, 1, 0, 704, 99
47438, V, 1, 1, 1, 1, 0, 704, 99
47439, V, 1, 1, 1, 1, 0, 704, 99
47440, V, 1, 1, 1, 1, 0, 704, 99
47441, V, 1, 1, 1, 1, 0, 704, 99
47442, V, 1, 1, 1, 1, 0, 704, 99
47443, V, 1, 1, 1, 1, 0, 704, 99
47444, V, 1, 1, 1, 1, 0, 704, 99
47446, V, 1, 1, 1, 1, 0, 704, 99
47447, V, 1, 1, 1, 1, 0, 704, 99
47448, V, 1, 1, 1, 1, 0, 704, 99
47449, V, 1, 1, 1, 1, 0, 704, 99
47450, V, 1, 1, 1, 1, 0, 704, 99
47451, V, 1, 1, 1, 1, 0, 704, 99
47452, V, 1, 1, 1, 1, 0, 704, 99
47453, V, 1, 1, 1, 1, 0, 704, 99
47454, V, 1, 1, 1, 1, 0, 704, 99
47455, V, 1, 1, 1, 1, 0, 704, 99
47456, V, 1, 1, 1, 1, 0, 704, 99
47457, V, 1, 1, 1, 1, 0, 704, 99
47458, V, 1, 1, 1, 1, 0, 704, 99
47459, V, 1, 1, 1, 1, 0, 704, 99
47460, V, 1, 1, 1, 1, 0, 704, 99
47461, V, 1, 1, 1, 1, 0, 704, 99
47462, V, 1, 1, 1, 1, 0, 704, 99
47463, V, 1, 1, 1, 1, 0, 704, 99
47464, V, 1, 1, 1, 1, 0, 704, 99
47465, V, 1, 1, 1, 1, 0, 704, 99
47466, V, 1, 1, 1, 1, 0, 704, 99
47467, V, 1, 1, 1, 1, 0, 704, 99
47468, V, 1, 1, 1, 1, 0, 704, 99
47469, V, 1, 1, 1, 1, 0, 704, 99
47470, V, 1, 1, 1, 1, 0, 704, 99
47471, V, 1, 1, 1, 1, 0, 704, 99
47472, V, 1, 1, 1, 1, 0, 704, 99
47473, V, 1, 1, 1, 1, 0, 704, 99
47474, V, 1, 1, 1, 1, 0, 704, 99
47475, V, 1, 1, 1, 1, 0, 704, 99
47476, V, 1, 1, 1, 1, 0, 704, 99
47477, V, 1, 1, 1, 1, 0, 704, 99
47478, V, 1, 1, 1, 1, 0, 704, 99
47479, V, 1, 1, 1, 1, 0, 704, 99
47480, V, 1, 1, 1, 1, 0, 704, 99
47481, V, 1, 1, 1, 1, 0, 704, 99
47482, V, 1, 1, 1, 1, 0, 704, 99
47483, V, 1, 1, 1, 1, 0, 704, 99
47484, V, 1, 1, 1, 1, 0, 704, 99
47485, V, 1, 1, 1, 1, 0, 704, 99
47486, V, 1, 1, 1, 1, 0, 704, 99
47488, V, 1, 1, 1, 1, 0, 704, 99
47489, V, 1, 1, 1, 1, 0, 704, 99
47490, V, 1, 1, 1, 1, 0, 704, 99
47491, V, 1, 1, 1, 1, 0, 704, 99
47492, V, 1, 1, 1, 1, 0, 704, 99
47493, V, 1, 1, 1, 1, 0, 704, 99
47494, V, 1, 1, 1, 1, 0, 704, 99
47495, V, 1, 1, 1, 1, 0, 704, 99
47496, V, 1, 1, 1, 1, 0, 704, 99
47497, V, 1, 1, 1, 1, 0, 704, 99
47498, V, 1, 1, 1, 1, 0, 704, 99
47499, V, 1, 1, 1, 1, 0, 704, 99
47500, V, 1, 1, 1, 1, 0, 704, 99
47501, V, 1, 1, 1, 1, 0, 704, 99
47502, V, 1, 1, 1, 1, 0, 704, 99
47503, V, 1, 1, 1, 1, 0, 704, 99
47504, V, 1, 1, 1, 1, 0, 704, 99
47505, V, 1, 1, 1, 1, 0, 704, 99
47506, V, 1, 1, 1, 1, 0, 704, 99
47507, V, 1, 1, 1, 1, 0, 704, 99
47508, V, 1, 1, 1, 1, 0, 704, 99
47509, V, 1, 1, 1, 1, 0, 704, 99
47510, V, 1, 1, 1, 1, 0, 704, 99
47511, V, 1, 1, 1, 1, 0, 704, 99
47512, V, 1, 1, 1, 1, 0, 704, 99
47513, V, 1, 1, 1, 1, 0, 704, 99
47514, V, 1, 1, 1, 1, 0, 704, 99
47515, V, 1, 1, 1, 1, 0, 704, 99
47516, V, 1, 1, 1, 1, 0, 704, 99
47517, V, 1, 1, 1, 1, 0, 704, 99
47518, V, 1, 1, 1, 1, 0, 704, 99
47519, V, 1, 1, 1, 1, 0, 704, 99
47520, V, 1, 1, 1, 1, 0, 704, 99
47521, V, 1, 1, 1, 1, 0, 704, 99
47522, V, 1, 1, 1, 1, 0, 704, 99
47523, V, 1, 1, 1, 1, 0, 704, 99
47524, V, 1, 1, 1, 1, 0, 704, 99
47525, V, 1, 1, 1, 1, 0, 704, 99
47526, V, 1, 1, 1, 1, 0, 704, 99
47527, V, 1, 1, 1, 1, 0, 704, 99
47528, V, 1, 1, 1, 1, 0, 704, 99
47529, V, 1, 1, 1, 1, 0, 704, 99
47531, V, 1, 1, 1, 1, 0, 704, 99
47532, V, 1, 1, 1, 1, 0, 704, 99
47533, V, 1, 1, 1, 1, 0, 704, 99
47534, V, 1, 1, 1, 1, 0, 704, 99
47535, V, 1, 1, 1, 1, 0, 704, 99
47536, V, 1, 1, 1, 1, 0, 704, 99
47537, V, 1, 1, 1, 1, 0, 704, 99
47538, V, 1, 1, 1, 1, 0, 704, 99
47539, V, 1, 1, 1, 1, 0, 704, 99
47540, V, 1, 1, 1, 1, 0, 704, 99
47541, V, 1, 1, 1, 1, 0, 704, 99
47542, V, 1, 1, 1, 1, 0, 704, 99
47543, V, 1, 1, 1, 1, 0, 704, 99
47544, V, 1, 1, 1, 1, 0, 704, 99
47545, V, 1, 1, 1, 1, 0, 704, 99
47546, V, 1, 1, 1, 1, 0, 704, 99
47547, V, 1, 1, 1, 1, 0, 704, 99
47548, V, 1, 1, 1, 1, 0, 704, 99
47549, V, 1, 1, 1, 1, 0, 704, 99
47550, V, 1, 1, 1, 1, 0, 704, 99
47551, V, 1, 1, 1, 1, 0, 704, 99
47552, V, 1, 1, 1, 1, 0, 704, 99
47553, V, 1, 1, 1, 1, 0, 704, 99
47554, V, 1, 1, 1, 1, 0, 704, 99
47555, V, 1, 1, 1, 1, 0, 704, 99
47556, V, 1, 1, 1, 1, 0, 704, 99
47557, V, 1, 1, 1, 1, 0, 704, 99
47558, V, 1, 1, 1, 1, 0, 704, 99
47559, V, 1, 1, 1, 1, 0, 704, 99
47560, V, 1, 1, 1, 1, 0, 704, 99
47561, V, 1, 1, 1, 1, 0, 704, 99
47562, V, 1, 1, 1, 1, 0, 704, 99
47563, V, 1, 1, 1, 1, 0, 704, 99
47564, V, 1, 1, 1, 1, 0, 704, 99
47565, V, 1, 1, 1, 1, 0, 704, 99
47566, V, 1, 1, 1, 1, 0, 704, 99
47567, V, 1, 1, 1, 1, 0, 704, 99
47568, V, 1, 1, 1, 1, 0, 704, 99
47569, V, 1, 1, 1, 1, 0, 704, 99
47570, V, 1, 1, 1, 1, 0, 704, 99
47571, V, 1, 1, 1, 1, 0, 704, 99
47572, V, 1, 1, 1, 1, 0, 704, 99
47574, V, 1, 1, 1, 1, 0, 704, 99
47575, V, 1, 1, 1, 1, 0, 704, 99
47576, V, 1, 1, 1, 1, 0, 704, 99
47577, V, 1, 1, 1, 1, 0, 704, 99
47578, V, 1, 1, 1, 1, 0, 704, 99
47579, V, 1, 1, 1, 1, 0, 704, 99
47580, V, 1, 1, 1, 1, 0, 704, 99
47581, V, 1, 1, 1, 1, 0, 704, 99
47582, V, 1, 1, 1, 1, 0, 704, 99
47583, V, 1, 1, 1, 1, 0, 704, 99
47584, V, 1, 1, 1, 1, 0, 704, 99
47585, V, 1, 1, 1, 1, 0, 704, 99
47586, V, 1, 1, 1, 1, 0, 704, 99
47587, V, 1, 1, 1, 1, 0, 704, 99
47588, V, 1, 1, 1, 1, 0, 704, 99
47589, V, 1, 1, 1, 1, 0, 704, 99
47590, V, 1, 1, 1, 1, 0, 704, 99
47591, V, 1, 1, 1, 1, 0, 704, 99
47592, V, 1, 1, 1, 1, 0, 704, 99
47593, V, 1, 1, 1, 1, 0, 704, 99
47594, V, 1, 1, 1, 1, 0, 704, 99
47595, V, 1, 1, 1, 1, 0, 704, 99
47596, V, 1, 1, 1, 1, 0, 704, 99
47597, V, 1, 1, 1, 1, 0, 704, 99
47598, V, 1, 1, 1, 1, 0, 704, 99
47599, V, 1, 1, 1, 1, 0, 704, 99
47600, V, 1, 1, 1, 1, 0, 704, 99
47601, V, 1, 1, 1, 1, 0, 704, 99
47602, V, 1, 1, 1, 1, 0, 704, 99
47603, V, 1, 1, 1, 1, 0, 704, 99
47604, V, 1, 1, 1, 1, 0, 704, 99
47605, V, 1, 1, 1, 1, 0, 704, 99
47606, V, 1, 1, 1, 1, 0, 704, 99
47607, V, 1, 1, 1, 1, 0, 704, 99
47608, V, 1, 1, 1, 1, 0, 704, 99
47609, V, 1, 1, 1, 1, 0, 704, 99
47610, V, 1, 1, 1, 1, 0, 704, 99
47611, V, 1, 1, 1, 1, 0, 704, 99
47612, V, 1, 1, 1, 1, 0, 704, 99
47613, V, 1, 1, 1, 1, 0, 704, 99
47614, V, 1, 1, 1, 1, 0, 704, 99
47616, V, 1, 1, 1, 1, 0, 704, 99
47617, V, 1, 1, 1, 1, 0, 704, 99
47618, V, 1, 1, 1, 1, 0, 704, 99
47619, V, 1, 1, 1, 1, 0, 704, 99
47620, V, 1, 1, 1, 1, 0, 704, 99
47621, V, 1, 1, 1, 1, 0, 704, 99
47622, V, 1, 1, 1, 1, 0, 704, 99
47623, V, 1, 1, 1, 1, 0, 704, 99
47624, V, 1, 1, 1, 1, 0, 704, 99
47625, V, 1, 1, 1, 1, 0, 704, 99
47626, V, 1, 1, 1, 1, 0, 704, 99
47627, V, 1, 1, 1, 1, 0, 704, 99
47628, V, 1, 1, 1, 1, 0, 704, 99
47629, V, 1, 1, 1, 1, 0, 704, 99
47630, V, 1, 1, 1, 1, 0, 704, 99
47631, V, 1, 1, 1, 1, 0, 704, 99
47632, V, 1, 1, 1, 1, 0, 704, 99
47633, V, 1, 1, 1, 1, 0, 704, 99
47634, V, 1, 1, 1, 1, 0, 704, 99
47635, V, 1, 1, 1, 1, 0, 704, 99
47636, V, 1, 1, 1, 1, 0, 704, 99
47637, V, 1, 1, 1, 1, 0, 704, 99
47638, V, 1, 1, 1, 1, 0, 704, 99
47639, V, 1, 1, 1, 1, 0, 704, 99
47640, V, 1, 1, 1, 1, 0, 704, 99
47641, V, 1, 1, 1, 1, 0, 704, 99
47642, V, 1, 1, 1, 1, 0, 704, 99
47643, V, 1, 1, 1, 1, 0, 704, 99
47644, V, 1, 1, 1, 1, 0, 704, 99
47645, V, 1, 1, 1, 1, 0, 704, 99
47646, V, 1, 1, 1, 1, 0, 704, 99
47647, V, 1, 1, 1, 1, 0, 704, 99
47648, V, 1, 1, 1, 1, 0, 704, 99
47649, V, 1, 1, 1, 1, 0, 704, 99
47650, V, 1, 1, 1, 1, 0, 704, 99
47651, V, 1, 1, 1, 1, 0, 704, 99
47652, V, 1, 1, 1, 1, 0, 704, 99
47653, V, 1, 1, 1, 1, 0, 704, 99
47654, V, 1, 1, 1, 1, 0, 704, 99
47655, V, 1, 1, 1, 1, 0, 704, 99
47656, V, 1, 1, 1, 1, 0, 704, 99
47657, V, 1, 1, 1, 1, 0, 704, 99
47659, V, 1, 1, 1, 1, 0, 704, 99
47660, V, 1, 1, 1, 1, 0, 704, 99
47661, V, 1, 1, 1, 1, 0, 704, 99
47662, V, 1, 1, 1, 1, 0, 704, 99
47663, V, 1, 1, 1, 1, 0, 704, 99
47664, V, 1, 1, 1, 1, 0, 704, 99
47665, V, 1, 1, 1, 1, 0, 704, 99
47666, V, 1, 1, 1, 1, 0, 704, 99
47667, V, 1, 1, 1, 1, 0, 704, 99
47668, V, 1, 1, 1, 1, 0, 704, 99
47669, V, 1, 1, 1, 1, 0, 704, 99
47670, V, 1, 1, 1, 1, 0, 704, 99
47671, V, 1, 1, 1, 1, 0, 704, 99
47672, V, 1, 1, 1, 1, 0, 704, 99
47673, V, 1, 1, 1, 1, 0, 704, 99
47674, V, 1, 1, 1, 1, 0, 704, 99
47675, V, 1, 1, 1, 1, 0, 704, 99
47676, V, 1, 1, 1, 1, 0, 704, 99
47677, V, 1, 1, 1, 1, 0, 704, 99
47678, V, 1, 1, 1, 1, 0, 704, 99
47679, V, 1, 1, 1, 1, 0, 704, 99
47680, V, 1, 1, 1, 1, 0, 704, 99
47681, V, 1, 1, 1, 1, 0, 704, 99
47682, V, 1, 1, 1, 1, 0, 704, 99
47683, V, 1, 1, 1, 1, 0, 704, 99
47684, V, 1, 1, 1, 1, 0, 704, 99
47685, V, 1, 1, 1, 1, 0, 704, 99
47686, V, 1, 1, 1, 1, 0, 704, 99
47687, V, 1, 1, 1, 1, 0, 704, 99
47688, V, 1, 1, 1, 1, 0, 704, 99
47689, V, 1, 1, 1, 1, 0, 704, 99
47690, V, 1, 1, 1, 1, 0, 704, 99
47691, V, 1, 1, 1, 1, 0, 704, 99
47692, V, 1, 1, 1, 1, 0, 704, 99
47693, V, 1, 1, 1, 1, 0, 704, 99
47694, V, 1, 1, 1, 1, 0, 704, 99
47695, V, 1, 1, 1, 1, 0, 704, 99
47696, V, 1, 1, 1, 1, 0, 704, 99
47697, V, 1, 1, 1, 1, 0, 704, 99
47698, V, 1, 1, 1, 1, 0, 704, 99
47699, V, 1, 1, 1, 1, 0, 704, 99
47700, V, 1, 1, 1, 1, 0, 704, 99
47702, V, 1, 1, 1, 1, 0, 704, 99
47703, V, 1, 1, 1, 1, 0, 704, 99
47704, V, 1, 1, 1, 1, 0, 704, 99
47705, V, 1, 1, 1, 1, 0, 704, 99
47706, V, 1, 1, 1, 1, 0, 704, 99
47707, V, 1, 1, 1, 1, 0, 704, 99
47708, V, 1, 1, 1, 1, 0, 704, 99
47709, V, 1, 1, 1, 1, 0, 704, 99
47710, V, 1, 1, 1, 1, 0, 704, 99
47711, V, 1, 1, 1, 1, 0, 704, 99
47712, V, 1, 1, 1, 1, 0, 704, 99
47713, V, 1, 1, 1, 1, 0, 704, 99
47714, V, 1, 1, 1, 1, 0, 704, 99
47715, V, 1, 1, 1, 1, 0, 704, 99
47716, V, 1, 1, 1, 1, 0, 704, 99
47717, V, 1, 1, 1, 1, 0, 704, 99
47718, V, 1, 1, 1, 1, 0, 704, 99
47719, V, 1, 1, 1, 1, 0, 704, 99
47720, V, 1, 1, 1, 1, 0, 704, 99
47721, V, 1, 1, 1, 1, 0, 704, 99
47722, V, 1, 1, 1, 1, 0, 704, 99
47723, V, 1, 1, 1, 1, 0, 704, 99
47724, V, 1, 1, 1, 1, 0, 704, 99
47725, V, 1, 1, 1, 1, 0, 704, 99
47726, V, 1, 1, 1, 1, 0, 704, 99
47727, V, 1, 1, 1, 1, 0, 704, 99
47728, V, 1, 1, 1, 1, 0, 704, 99
47729, V, 1, 1, 1, 1, 0, 704, 99
47730, V, 1, 1, 1, 1, 0, 704, 99
47731, V, 1, 1, 1, 1, 0, 704, 99
47732, V, 1, 1, 1, 1, 0, 704, 99
47733, V, 1, 1, 1, 1, 0, 704, 99
47734, V, 1, 1, 1, 1, 0, 704, 99
47735, V, 1, 1, 1, 1, 0, 704, 99
47736, V, 1, 1, 1, 1, 0, 704, 99
47737, V, 1, 1, 1, 1, 0, 704, 99
47738, V, 1, 1, 1, 1, 0, 704, 99
47739, V, 1, 1, 1, 1, 0, 704, 99
47740, V, 1, 1, 1, 1, 0, 704, 99
47741, V, 1, 1, 1, 1, 0, 704, 99
47742, V, 1, 1, 1, 1, 0, 704, 99
47744, V, 1, 1, 1, 1, 0, 704, 99
47745, V, 1, 1, 1, 1, 0, 704, 99
47746, V, 1, 1, 1, 1, 0, 704, 99
47747, V, 1, 1, 1, 1, 0, 704, 99
47748, V, 1, 1, 1, 1, 0, 704, 99
47749, V, 1, 1, 1, 1, 0, 704, 99
47750, V, 1, 1, 1, 1, 0, 704, 99
47751, V, 1, 1, 1, 1, 0, 704, 99
47752, V, 1, 1, 1, 1, 0, 704, 99
47753, V, 1, 1, 1, 1, 0, 704, 99
47754, V, 1, 1, 1, 1, 0, 704, 99
47755, V, 1, 1, 1, 1, 0, 704, 99
47756, V, 1, 1, 1, 1, 0, 704, 99
47757, V, 1, 1, 1, 1, 0, 704, 99
47758, V, 1, 1, 1, 1, 0, 704, 99
47759, V, 1, 1, 1, 1, 0, 704, 99
47760, V, 1, 1, 1, 1, 0, 704, 99
47761, V, 1, 1, 1, 1, 0, 704, 99
47762, V, 1, 1, 1, 1, 0, 704, 99
47763, V, 1, 1, 1, 1, 0, 704, 99
47764, V, 1, 1, 1, 1, 0, 704, 99
47765, V, 1, 1, 1, 1, 0, 704, 99
47766, V, 1, 1, 1, 1, 0, 704, 99
47767, V, 1, 1, 1, 1, 0, 704, 99
47768, V, 1, 1, 1, 1, 0, 704, 99
47769, V, 1, 1, 1, 1, 0, 704, 99
47770, V, 1, 1, 1, 1, 0, 704, 99
47771, V, 1, 1, 1, 1, 0, 704, 99
47772, V, 1, 1, 1, 1, 0, 704, 99
47773, V, 1, 1, 1, 1, 0, 704, 99
47774, V, 1, 1, 1, 1, 0, 704, 99
47775, V, 1, 1, 1, 1, 0, 704, 99
47776, V, 1, 1, 1, 1, 0, 704, 99
47777, V, 1, 1, 1, 1, 0, 704, 99
47778, V, 1, 1, 1, 1, 0, 704, 99
47779, V, 1, 1, 1, 1, 0, 704, 99
47780, V, 1, 1, 1, 1, 0, 704, 99
47781, V, 1, 1, 1, 1, 0, 704, 99
47782, V, 1, 1, 1, 1, 0, 704, 99
47783, V, 1, 1, 1, 1, 0, 704, 99
47784, V, 1, 1, 1, 1, 0, 704, 99
47785, V, 1, 1, 1, 1, 0, 704, 99
47787, V, 1, 1, 1, 1, 0, 704, 99
47788, V, 1, 1, 1, 1, 0, 704, 99
47789, V, 1, 1, 1, 1, 0, 704, 99
47790, V, 1, 1, 1, 1, 0, 704, 99
47791, V, 1, 1, 1, 1, 0, 704, 99
47792, V, 1, 1, 1, 1, 0, 704, 99
47793, V, 1, 1, 1, 1, 0, 704, 99
47794, V, 1, 1, 1, 1, 0, 704, 99
47795, V, 1, 1, 1, 1, 0, 704, 99
47796, V, 1, 1, 1, 1, 0, 704, 99
47797, V, 1, 1, 1, 1, 0, 704, 99
47798, V, 1, 1, 1, 1, 0, 704, 99
47799, V, 1, 1, 1, 1, 0, 704, 99
47800, V, 1, 1, 1, 1, 0, 704, 99
47801, V, 1, 1, 1, 1, 0, 704, 99
47802, V, 1, 1, 1, 1, 0, 704, 99
47803, V, 1, 1, 1, 1, 0, 704, 99
47804, V, 1, 1, 1, 1, 0, 704, 99
47805, V, 1, 1, 1, 1, 0, 704, 99
47806, V, 1, 1, 1, 1, 0, 704, 99
47807, V, 1, 1, 1, 1, 0, 704, 99
47808, V, 1, 1, 1, 1, 0, 704, 99
47809, V, 1, 1, 1, 1, 0, 704, 99
47810, V, 1, 1, 1, 1, 0, 704, 99
47811, V, 1, 1, 1, 1, 0, 704, 99
47812, V, 1, 1, 1, 1, 0, 704, 99
47813, V, 1, 1, 1, 1, 0, 704, 99
47814, V, 1, 1, 1, 1, 0, 704, 99
47815, V, 1, 1, 1, 1, 0, 704, 99
47816, V, 1, 1, 1, 1, 0, 704, 99
47817, V, 1, 1, 1, 1, 0, 704, 99
47818, V, 1, 1, 1, 1, 0, 704, 99
47819, V, 1, 1, 1, 1, 0, 704, 99
47820, V, 1, 1, 1, 1, 0, 704, 99
47821, V, 1, 1, 1, 1, 0, 704, 99
47822, V, 1, 1, 1, 1, 0, 704, 99
47823, V, 1, 1, 1, 1, 0, 704, 99
47824, V, 1, 1, 1, 1, 0, 704, 99
47825, V, 1, 1, 1, 1, 0, 704, 99
47826, V, 1, 1, 1, 1, 0, 704, 99
47827, V, 1, 1, 1, 1, 0, 704, 99
47828, V, 1, 1, 1, 1, 0, 704, 99
47830, V, 1, 1, 1, 1, 0, 704, 99
47831, V, 1, 1, 1, 1, 0, 704, 99
47832, V, 1, 1, 1, 1, 0, 704, 99
47833, V, 1, 1, 1, 1, 0, 704, 99
47834, V, 1, 1, 1, 1, 0, 704, 99
47835, V, 1, 1, 1, 1, 0, 704, 99
47836, V, 1, 1, 1, 1, 0, 704, 99
47837, V, 1, 1, 1, 1, 0, 704, 99
47838, V, 1, 1, 1, 1, 0, 704, 99
47839, V, 1, 1, 1, 1, 0, 704, 99
47840, V, 1, 1, 1, 1, 0, 704, 99
47841, V, 1, 1, 1, 1, 0, 704, 99
47842, V, 1, 1, 1, 1, 0, 704, 99
47843, V, 1, 1, 1, 1, 0, 704, 99
47844, V, 1, 1, 1, 1, 0, 704, 99
47845, V, 1, 1, 1, 1, 0, 704, 99
47846, V, 1, 1, 1, 1, 0, 704, 99
47847, V, 1, 1, 1, 1, 0, 704, 99
47848, V, 1, 1, 1, 1, 0, 704, 99
47849, V, 1, 1, 1, 1, 0, 704, 99
47850, V, 1, 1, 1, 1, 0, 704, 99
47851, V, 1, 1, 1, 1, 0, 704, 99
47852, V, 1, 1, 1, 1, 0, 704, 99
47853, V, 1, 1, 1, 1, 0, 704, 99
47854, V, 1, 1, 1, 1, 0, 704, 99
47855, V, 1, 1, 1, 1, 0, 704, 99
47856, V, 1, 1, 1, 1, 0, 704, 99
47857, V, 1, 1, 1, 1, 0, 704, 99
47858, V, 1, 1, 1, 1, 0, 704, 99
47859, V, 1, 1, 1, 1, 0, 704, 99
47860, V, 1, 1, 1, 1, 0, 704, 99
47861, V, 1, 1, 1, 1, 0, 704, 99
47862, V, 1, 1, 1, 1, 0, 704, 99
47863, V, 1, 1, 1, 1, 0, 704, 99
47864, V, 1, 1, 1, 1, 0, 704, 99
47865, V, 1, 1, 1, 1, 0, 704, 99
47866, V, 1, 1, 1, 1, 0, 704, 99
47867, V, 1, 1, 1, 1, 0, 704, 99
47868, V, 1, 1, 1, 1, 0, 704, 99
47869, V, 1, 1, 1, 1, 0, 704, 99
47870, V, 1, 1, 1, 1, 0, 704, 99
47872, V, 1, 1, 1, 1, 0, 704, 99
47873, V, 1, 1, 1, 1, 0, 704, 99
47874, V, 1, 1, 1, 1, 0, 704, 99
47875, V, 1, 1, 1, 1, 0, 704, 99
47876, V, 1, 1, 1, 1, 0, 704, 99
47877, V, 1, 1, 1, 1, 0, 704, 99
47878, V, 1, 1, 1, 1, 0, 704, 99
47879, V, 1, 1, 1, 1, 0, 704, 99
47880, V, 1, 1, 1, 1, 0, 704, 99
47881, V, 1, 1, 1, 1, 0, 704, 99
47882, V, 1, 1, 1, 1, 0, 704, 99
47883, V, 1, 1, 1, 1, 0, 704, 99
47884, V, 1, 1, 1, 1, 0, 704, 99
47885, V, 1, 1, 1, 1, 0, 704, 99
47886, V, 1, 1, 1, 1, 0, 704, 99
47887, V, 1, 1, 1, 1, 0, 704, 99
47888, V, 1, 1, 1, 1, 0, 704, 99
47889, V, 1, 1, 1, 1, 0, 704, 99
47890, V, 1, 1, 1, 1, 0, 704, 99
47891, V, 1, 1, 1, 1, 0, 704, 99
47892, V, 1, 1, 1, 1, 0, 704, 99
47893, V, 1, 1, 1, 1, 0, 704, 99
47894, V, 1, 1, 1, 1, 0, 704, 99
47895, V, 1, 1, 1, 1, 0, 704, 99
47896, V, 1, 1, 1, 1, 0, 704, 99
47897, V, 1, 1, 1, 1, 0, 704, 99
47898, V, 1, 1, 1, 1, 0, 704, 99
47899, V, 1, 1, 1, 1, 0, 704, 99
47900, V, 1, 1, 1, 1, 0, 704, 99
47901, V, 1, 1, 1, 1, 0, 704, 99
47902, V, 1, 1, 1, 1, 0, 704, 99
47903, V, 1, 1, 1, 1, 0, 704, 99
47904, V, 1, 1, 1, 1, 0, 704, 99
47905, V, 1, 1, 1, 1, 0, 704, 99
47906, V, 1, 1, 1, 1, 0, 704, 99
47907, V, 1, 1, 1, 1, 0, 704, 99
47908, V, 1, 1, 1, 1, 0, 704, 99
47909, V, 1, 1, 1, 1, 0, 704, 99
47910, V, 1, 1, 1, 1, 0, 704, 99
47911, V, 1, 1, 1, 1, 0, 704, 99
47912, V, 1, 1, 1, 1, 0, 704, 99
47913, V, 1, 1, 1, 1, 0, 704, 99
47915, V, 1, 1, 1, 1, 0, 704, 99
47916, V, 1, 1, 1, 1, 0, 704, 99
47917, V, 1, 1, 1, 1, 0, 704, 99
47918, V, 1, 1, 1, 1, 0, 704, 99
47919, V, 1, 1, 1, 1, 0, 704, 99
47920, V, 1, 1, 1, 1, 0, 704, 99
47921, V, 1, 1, 1, 1, 0, 704, 99
47922, V, 1, 1, 1, 1, 0, 704, 99
47923, V, 1, 1, 1, 1, 0, 704, 99
47924, V, 1, 1, 1, 1, 0, 704, 99
47925, V, 1, 1, 1, 1, 0, 704, 99
47926, V, 1, 1, 1, 1, 0, 704, 99
47927, V, 1, 1, 1, 1, 0, 704, 99
47928, V, 1, 1, 1, 1, 0, 704, 99
47929, V, 1, 1, 1, 1, 0, 704, 99
47930, V, 1, 1, 1, 1, 0, 704, 99
47931, V, 1, 1, 1, 1, 0, 704, 99
47932, V, 1, 1, 1, 1, 0, 704, 99
47933, V, 1, 1, 1, 1, 0, 704, 99
47934, V, 1, 1, 1, 1, 0, 704, 99
47935, V, 1, 1, 1, 1, 0, 704, 99
47936, V, 1, 1, 1, 1, 0, 704, 99
47937, V, 1, 1, 1, 1, 0, 704, 99
47938, V, 1, 1, 1, 1, 0, 704, 99
47939, V, 1, 1, 1, 1, 0, 704, 99
47940, V, 1, 1, 1, 1, 0, 704, 99
47941, V, 1, 1, 1, 1, 0, 704, 99
47942, V, 1, 1, 1, 1, 0, 704, 99
47943, V, 1, 1, 1, 1, 0, 704, 99
47944, V, 1, 1, 1, 1, 0, 704, 99
47945, V, 1, 1, 1, 1, 0, 704, 99
47946, V, 1, 1, 1, 1, 0, 704, 99
47947, V, 1, 1, 1, 1, 0, 704, 99
47948, V, 1, 1, 1, 1, 0, 704, 99
47949, V, 1, 1, 1, 1, 0, 704, 99
47950, V, 1, 1, 1, 1, 0, 704, 99
47951, V, 1, 1, 1, 1, 0, 704, 99
47952, V, 1, 1, 1, 1, 0, 704, 99
47953, V, 1, 1, 1, 1, 0, 704, 99
47954, V, 1, 1, 1, 1, 0, 704, 99
47955, V, 1, 1, 1, 1, 0, 704, 99
47956, V, 1, 1, 1, 1, 0, 704, 99
47958, V, 1, 1, 1, 1, 0, 704, 99
47959, V, 1, 1, 1, 1, 0, 704, 99
47960, V, 1, 1, 1, 1, 0, 704, 99
47961, V, 1, 1, 1, 1, 0, 704, 99
47962, V, 1, 1, 1, 1, 0, 704, 99
47963, V, 1, 1, 1, 1, 0, 704, 99
47964, V, 1, 1, 1, 1, 0, 704, 99
47965, V, 1, 1, 1, 1, 0, 704, 99
47966, V, 1, 1, 1, 1, 0, 704, 99
47967, V, 1, 1, 1, 1, 0, 704, 99
47968, V, 1, 1, 1, 1, 0, 704, 99
47969, V, 1, 1, 1, 1, 0, 704, 99
47970, V, 1, 1, 1, 1, 0, 704, 99
47971, V, 1, 1, 1, 1, 0, 704, 99
47972, V, 1, 1, 1, 1, 0, 704, 99
47973, V, 1, 1, 1, 1, 0, 704, 99
47974, V, 1, 1, 1, 1, 0, 704, 99
47975, V, 1, 1, 1, 1, 0, 704, 99
47976, V, 1, 1, 1, 1, 0, 704, 99
47977, V, 1, 1, 1, 1, 0, 704, 99
47978, V, 1, 1, 1, 1, 0, 704, 99
47979, V, 1, 1, 1, 1, 0, 704, 99
47980, V, 1, 1, 1, 1, 0, 704, 99
47981, V, 1, 1, 1, 1, 0, 704, 99
47982, V, 1, 1, 1, 1, 0, 704, 99
47983, V, 1, 1, 1, 1, 0, 704, 99
47984, V, 1, 1, 1, 1, 0, 704, 99
47985, V, 1, 1, 1, 1, 0, 704, 99
47986, V, 1, 1, 1, 1, 0, 704, 99
47987, V, 1, 1, 1, 1, 0, 704, 99
47988, V, 1, 1, 1, 1, 0, 704, 99
47989, V, 1, 1, 1, 1, 0, 704, 99
47990, V, 1, 1, 1, 1, 0, 704, 99
47991, V, 1, 1, 1, 1, 0, 704, 99
47992, V, 1, 1, 1, 1, 0, 704, 99
47993, V, 1, 1, 1, 1, 0, 704, 99
47994, V, 1, 1, 1, 1, 0, 704, 99
47995, V, 1, 1, 1, 1, 0, 704, 99
47996, V, 1, 1, 1, 1, 0, 704, 99
47997, V, 1, 1, 1, 1, 0, 704, 99
47998, V, 1, 1, 1, 1, 0, 704, 99
48000, V, 1, 1, 1, 1, 0, 704, 99
48001, V, 1, 1, 1, 1, 0, 704, 99
48002, V, 1, 1, 1, 1, 0, 704, 99
48003, V, 1, 1, 1, 1, 0, 704, 99
48004, V, 1, 1, 1, 1, 0, 704, 99
48005, V, 1, 1, 1, 1, 0, 704, 99
48006, V, 1, 1, 1, 1, 0, 704, 99
48007, V, 1, 1, 1, 1, 0, 704, 99
48008, V, 1, 1, 1, 1, 0, 704, 99
48009, V, 1, 1, 1, 1, 0, 704, 99
48010, V, 1, 1, 1, 1, 0, 704, 99
48011, V, 1, 1, 1, 1, 0, 704, 99
48012, V, 1, 1, 1, 1, 0, 704, 99
48013, V, 1, 1, 1, 1, 0, 704, 99
48014, V, 1, 1, 1, 1, 0, 704, 99
48015, V, 1, 1, 1, 1, 0, 704, 99
48016, V, 1, 1, 1, 1, 0, 704, 99
48017, V, 1, 1, 1, 1, 0, 704, 99
48018, V, 1, 1, 1, 1, 0, 704, 99
48019, V, 1, 1, 1, 1, 0, 704, 99
48020, V, 1, 1, 1, 1, 0, 704, 99
48021, V, 1, 1, 1, 1, 0, 704, 99
48022, V, 1, 1, 1, 1, 0, 704, 99
48023, V, 1, 1, 1, 1, 0, 704, 99
48024, V, 1, 1, 1, 1, 0, 704, 99
48025, V, 1, 1, 1, 1, 0, 704, 99
48026, V, 1, 1, 1, 1, 0, 704, 99
48027, V, 1, 1, 1, 1, 0, 704, 99
48028, V, 1, 1, 1, 1, 0, 704, 99
48029, V, 1, 1, 1, 1, 0, 704, 99
48030, V, 1, 1, 1, 1, 0, 704, 99
48031, V, 1, 1, 1, 1, 0, 704, 99
48032, V, 1, 1, 1, 1, 0, 704, 99
48033, V, 1, 1, 1, 1, 0, 704, 99
48034, V, 1, 1, 1, 1, 0, 704, 99
48035, V, 1, 1, 1, 1, 0, 704, 99
48036, V, 1, 1, 1, 1, 0, 704, 99
48037, V, 1, 1, 1, 1, 0, 704, 99
48038, V, 1, 1, 1, 1, 0, 704, 99
48039, V, 1, 1, 1, 1, 0, 704, 99
48040, V, 1, 1, 1, 1, 0, 704, 99
48041, V, 1, 1, 1, 1, 0, 704, 99
48043, V, 1, 1, 1, 1, 0, 704, 99
48044, V, 1, 1, 1, 1, 0, 704, 99
48045, V, 1, 1, 1, 1, 0, 704, 99
48046, V, 1, 1, 1, 1, 0, 704, 99
48047, V, 1, 1, 1, 1, 0, 704, 99
48048, V, 1, 1, 1, 1, 0, 704, 99
48049, V, 1, 1, 1, 1, 0, 704, 99
48050, V, 1, 1, 1, 1, 0, 704, 99
48051, V, 1, 1, 1, 1, 0, 704, 99
48052, V, 1, 1, 1, 1, 0, 704, 99
48053, V, 1, 1, 1, 1, 0, 704, 99
48054, V, 1, 1, 1, 1, 0, 704, 99
48055, V, 1, 1, 1, 1, 0, 704, 99
48056, V, 1, 1, 1, 1, 0, 704, 99
48057, V, 1, 1, 1, 1, 0, 704, 99
48058, V, 1, 1, 1, 1, 0, 704, 99
48059, V, 1, 1, 1, 1, 0, 704, 99
48060, V, 1, 1, 1, 1, 0, 704, 99
48061, V, 1, 1, 1, 1, 0, 704, 99
48062, V, 1, 1, 1, 1, 0, 704, 99
48063, V, 1, 1, 1, 1, 0, 704, 99
48064, V, 1, 1, 1, 1, 0, 704, 99
48065, V, 1, 1, 1, 1, 0, 704, 99
48066, V, 1, 1, 1, 1, 0, 704, 99
48067, V, 1, 1, 1, 1, 0, 704, 99
48068, V, 1, 1, 1, 1, 0, 704, 99
48069, V, 1, 1, 1, 1, 0, 704, 99
48070, V, 1, 1, 1, 1, 0, 704, 99
48071, V, 1, 1, 1, 1, 0, 704, 99
48072, V, 1, 1, 1, 1, 0, 704, 99
48073, V, 1, 1, 1, 1, 0, 704, 99
48074, V, 1, 1, 1, 1, 0, 704, 99
48075, V, 1, 1, 1, 1, 0, 704, 99
48076, V, 1, 1, 1, 1, 0, 704, 99
48077, V, 1, 1, 1, 1, 0, 704, 99
48078, V, 1, 1, 1, 1, 0, 704, 99
48079, V, 1, 1, 1, 1, 0, 704, 99
48080, V, 1, 1, 1, 1, 0, 704, 99
48081, V, 1, 1, 1, 1, 0, 704, 99
48082, V, 1, 1, 1, 1, 0, 704, 99
48083, V, 1, 1, 1, 1, 0, 704, 99
48084, V, 1, 1, 1, 1, 0, 704, 99
48086, V, 1, 1, 1, 1, 0, 704, 99
48087, V, 1, 1, 1, 1, 0, 704, 99
48088, V, 1, 1, 1, 1, 0, 704, 99
48089, V, 1, 1, 1, 1, 0, 704, 99
48090, V, 1, 1, 1, 1, 0, 704, 99
48091, V, 1, 1, 1, 1, 0, 704, 99
48092, V, 1, 1, 1, 1, 0, 704, 99
48093, V, 1, 1, 1, 1, 0, 704, 99
48094, V, 1, 1, 1, 1, 0, 704, 99
48095, V, 1, 1, 1, 1, 0, 704, 99
48096, V, 1, 1, 1, 1, 0, 704, 99
48097, V, 1, 1, 1, 1, 0, 704, 99
48098, V, 1, 1, 1, 1, 0, 704, 99
48099, V, 1, 1, 1, 1, 0, 704, 99
48100, V, 1, 1, 1, 1, 0, 704, 99
48101, V, 1, 1, 1, 1, 0, 704, 99
48102, V, 1, 1, 1, 1, 0, 704, 99
48103, V, 1, 1, 1, 1, 0, 704, 99
48104, V, 1, 1, 1, 1, 0, 704, 99
48105, V, 1, 1, 1, 1, 0, 704, 99
48106, V, 1, 1, 1, 1, 0, 704, 99
48107, V, 1, 1, 1, 1, 0, 704, 99
48108, V, 1, 1, 1, 1, 0, 704, 99
48109, V, 1, 1, 1, 1, 0, 704, 99
48110, V, 1, 1, 1, 1, 0, 704, 99
48111, V, 1, 1, 1, 1, 0, 704, 99
48112, V, 1, 1, 1, 1, 0, 704, 99
48113, V, 1, 1, 1, 1, 0, 704, 99
48114, V, 1, 1, 1, 1, 0, 704, 99
48115, V, 1, 1, 1, 1, 0, 704, 99
48116, V, 1, 1, 1, 1, 0, 704, 99
48117, V, 1, 1, 1, 1, 0, 704, 99
48118, V, 1, 1, 1, 1, 0, 704, 99
48119, V, 1, 1, 1, 1, 0, 704, 99
48120, V, 1, 1, 1, 1, 0, 704, 99
48121, V, 1, 1, 1, 1, 0, 704, 99
48122, V, 1, 1, 1, 1, 0, 704, 99
48123, V, 1, 1, 1, 1, 0, 704, 99
48124, V, 1, 1, 1, 1, 0, 704, 99
48125, V, 1, 1, 1, 1, 0, 704, 99
48126, V, 1, 1, 1, 1, 0, 704, 99
48128, V, 1, 1, 1, 1, 0, 704, 99
48129, V, 1, 1, 1, 1, 0, 704, 99
48130, V, 1, 1, 1, 1, 0, 704, 99
48131, V, 1, 1, 1, 1, 0, 704, 99
48132, V, 1, 1, 1, 1, 0, 704, 99
48133, V, 1, 1, 1, 1, 0, 704, 99
48134, V, 1, 1, 1, 1, 0, 704, 99
48135, V, 1, 1, 1, 1, 0, 704, 99
48136, V, 1, 1, 1, 1, 0, 704, 99
48137, V, 1, 1, 1, 1, 0, 704, 99
48138, V, 1, 1, 1, 1, 0, 704, 99
48139, V, 1, 1, 1, 1, 0, 704, 99
48140, V, 1, 1, 1, 1, 0, 704, 99
48141, V, 1, 1, 1, 1, 0, 704, 99
48142, V, 1, 1, 1, 1, 0, 704, 99
48143, V, 1, 1, 1, 1, 0, 704, 99
48144, V, 1, 1, 1, 1, 0, 704, 99
48145, V, 1, 1, 1, 1, 0, 704, 99
48146, V, 1, 1, 1, 1, 0, 704, 99
48147, V, 1, 1, 1, 1, 0, 704, 99
48148, V, 1, 1, 1, 1, 0, 704, 99
48149, V, 1, 1, 1, 1, 0, 704, 99
48150, V, 1, 1, 1, 1, 0, 704, 99
48151, V, 1, 1, 1, 1, 0, 704, 99
48152, V, 1, 1, 1, 1, 0, 704, 99
48153, V, 1, 1, 1, 1, 0, 704, 99
48154, V, 1, 1, 1, 1, 0, 704, 99
48155, V, 1, 1, 1, 1, 0, 704, 99
48156, V, 1, 1, 1, 1, 0, 704, 99
48157, V, 1, 1, 1, 1, 0, 704, 99
48158, V, 1, 1, 1, 1, 0, 704, 99
48159, V, 1, 1, 1, 1, 0, 704, 99
48160, V, 1, 1, 1, 1, 0, 704, 99
48161, V, 1, 1, 1, 1, 0, 704, 99
48162, V, 1, 1, 1, 1, 0, 704, 99
48163, V, 1, 1, 1, 1, 0, 704, 99
48164, V, 1, 1, 1, 1, 0, 704, 99
48165, V, 1, 1, 1, 1, 0, 704, 99
48166, V, 1, 1, 1, 1, 0, 704, 99
48167, V, 1, 1, 1, 1, 0, 704, 99
48168, V, 1, 1, 1, 1, 0, 704, 99
48169, V, 1, 1, 1, 1, 0, 704, 99
48171, V, 1, 1, 1, 1, 0, 704, 99
48172, V, 1, 1, 1, 1, 0, 704, 99
48173, V, 1, 1, 1, 1, 0, 704, 99
48174, V, 1, 1, 1, 1, 0, 704, 99
48175, V, 1, 1, 1, 1, 0, 704, 99
48176, V, 1, 1, 1, 1, 0, 704, 99
48177, V, 1, 1, 1, 1, 0, 704, 99
48178, V, 1, 1, 1, 1, 0, 704, 99
48179, V, 1, 1, 1, 1, 0, 704, 99
48180, V, 1, 1, 1, 1, 0, 704, 99
48181, V, 1, 1, 1, 1, 0, 704, 99
48182, V, 1, 1, 1, 1, 0, 704, 99
48183, V, 1, 1, 1, 1, 0, 704, 99
48184, V, 1, 1, 1, 1, 0, 704, 99
48185, V, 1, 1, 1, 1, 0, 704, 99
48186, V, 1, 1, 1, 1, 0, 704, 99
48187, V, 1, 1, 1, 1, 0, 704, 99
48188, V, 1, 1, 1, 1, 0, 704, 99
48189, V, 1, 1, 1, 1, 0, 704, 99
48190, V, 1, 1, 1, 1, 0, 704, 99
48191, V, 1, 1, 1, 1, 0, 704, 99
48192, V, 1, 1, 1, 1, 0, 704, 99
48193, V, 1, 1, 1, 1, 0, 704, 99
48194, V, 1, 1, 1, 1, 0, 704, 99
48195, V, 1, 1, 1, 1, 0, 704, 99
48196, V, 1, 1, 1, 1, 0, 704, 99
48197, V, 1, 1, 1, 1, 0, 704, 99
48198, V, 1, 1, 1, 1, 0, 704, 99
48199, V, 1, 1, 1, 1, 0, 704, 99
48200, V, 1, 1, 1, 1, 0, 704, 99
48201, V, 1, 1, 1, 1, 0, 704, 99
48202, V, 1, 1, 1, 1, 0, 704, 99
48203, V, 1, 1, 1, 1, 0, 704, 99
48204, V, 1, 1, 1, 1, 0, 704, 99
48205, V, 1, 1, 1, 1, 0, 704, 99
48206, V, 1, 1, 1, 1, 0, 704, 99
48207, V, 1, 1, 1, 1, 0, 704, 99
48208, V, 1, 1, 1, 1, 0, 704, 99
48209, V, 1, 1, 1, 1, 0, 704, 99
48210, V, 1, 1, 1, 1, 0, 704, 99
48211, V, 1, 1, 1, 1, 0, 704, 99
48212, V, 1, 1, 1, 1, 0, 704, 99
48214, V, 1, 1, 1, 1, 0, 704, 99
48215, V, 1, 1, 1, 1, 0, 704, 99
48216, V, 1, 1, 1, 1, 0, 704, 99
48217, V, 1, 1, 1, 1, 0, 704, 99
48218, V, 1, 1, 1, 1, 0, 704, 99
48219, V, 1, 1, 1, 1, 0, 704, 99
48220, V, 1, 1, 1, 1, 0, 704, 99
48221, V, 1, 1, 1, 1, 0, 704, 99
48222, V, 1, 1, 1, 1, 0, 704, 99
48223, V, 1, 1, 1, 1, 0, 704, 99
48224, V, 1, 1, 1, 1, 0, 704, 99
48225, V, 1, 1, 1, 1, 0, 704, 99
48226, V, 1, 1, 1, 1, 0, 704, 99
48227, V, 1, 1, 1, 1, 0, 704, 99
48228, V, 1, 1, 1, 1, 0, 704, 99
48229, V, 1, 1, 1, 1, 0, 704, 99
48230, V, 1, 1, 1, 1, 0, 704, 99
48231, V, 1, 1, 1, 1, 0, 704, 99
48232, V, 1, 1, 1, 1, 0, 704, 99
48233, V, 1, 1, 1, 1, 0, 704, 99
48234, V, 1, 1, 1, 1, 0, 704, 99
48235, V, 1, 1, 1, 1, 0, 704, 99
48236, V, 1, 1, 1, 1, 0, 704, 99
48237, V, 1, 1, 1, 1, 0, 704, 99
48238, V, 1, 1, 1, 1, 0, 704, 99
48239, V, 1, 1, 1, 1, 0, 704, 99
48240, V, 1, 1, 1, 1, 0, 704, 99
48241, V, 1, 1, 1, 1, 0, 704, 99
48242, V, 1, 1, 1, 1, 0, 704, 99
48243, V, 1, 1, 1, 1, 0, 704, 99
48244, V, 1, 1, 1, 1, 0, 704, 99
48245, V, 1, 1, 1, 1, 0, 704, 99
48246, V, 1, 1, 1, 1, 0, 704, 99
48247, V, 1, 1, 1, 1, 0, 704, 99
48248, V, 1, 1, 1, 1, 0, 704, 99
48249, V, 1, 1, 1, 1, 0, 704, 99
48250, V, 1, 1, 1, 1, 0, 704, 99
48251, V, 1, 1, 1, 1, 0, 704, 99
48252, V, 1, 1, 1, 1, 0, 704, 99
48253, V, 1, 1, 1, 1, 0, 704, 99
48254, V, 1, 1, 1, 1, 0, 704, 99
48256, V, 1, 1, 1, 1, 0, 704, 99
48257, V, 1, 1, 1, 1, 0, 704, 99
48258, V, 1, 1, 1, 1, 0, 704, 99
48259, V, 1, 1, 1, 1, 0, 704, 99
48260, V, 1, 1, 1, 1, 0, 704, 99
48261, V, 1, 1, 1, 1, 0, 704, 99
48262, V, 1, 1, 1, 1, 0, 704, 99
48263, V, 1, 1, 1, 1, 0, 704, 99
48264, V, 1, 1, 1, 1, 0, 704, 99
48265, V, 1, 1, 1, 1, 0, 704, 99
48266, V, 1, 1, 1, 1, 0, 704, 99
48267, V, 1, 1, 1, 1, 0, 704, 99
48268, V, 1, 1, 1, 1, 0, 704, 99
48269, V, 1, 1, 1, 1, 0, 704, 99
48270, V, 1, 1, 1, 1, 0, 704, 99
48271, V, 1, 1, 1, 1, 0, 704, 99
48272, V, 1, 1, 1, 1, 0, 704, 99
48273, V, 1, 1, 1, 1, 0, 704, 99
48274, V, 1, 1, 1, 1, 0, 704, 99
48275, V, 1, 1, 1, 1, 0, 704, 99
48276, V, 1, 1, 1, 1, 0, 704, 99
48277, V, 1, 1, 1, 1, 0, 704, 99
48278, V, 1, 1, 1, 1, 0, 704, 99
48279, V, 1, 1, 1, 1, 0, 704, 99
48280, V, 1, 1, 1, 1, 0, 704, 99
48281, V, 1, 1, 1, 1, 0, 704, 99
48282, V, 1, 1, 1, 1, 0, 704, 99
48283, V, 1, 1, 1, 1, 0, 704, 99
48284, V, 1, 1, 1, 1, 0, 704, 99
48285, V, 1, 1, 1, 1, 0, 704, 99
48286, V, 1, 1, 1, 1, 0, 704, 99
48287, V, 1, 1, 1, 1, 0, 704, 99
48288, V, 1, 1, 1, 1, 0, 704, 99
48289, V, 1, 1, 1, 1, 0, 704, 99
48290, V, 1, 1, 1, 1, 0, 704, 99
48291, V, 1, 1, 1, 1, 0, 704, 99
48292, V, 1, 1, 1, 1, 0, 704, 99
48293, V, 1, 1, 1, 1, 0, 704, 99
48294, V, 1, 1, 1, 1, 0, 704, 99
48295, V, 1, 1, 1, 1, 0, 704, 99
48296, V, 1, 1, 1, 1, 0, 704, 99
48297, V, 1, 1, 1, 1, 0, 704, 99
48299, V, 1, 1, 1, 1, 0, 704, 99
48300, V, 1, 1, 1, 1, 0, 704, 99
48301, V, 1, 1, 1, 1, 0, 704, 99
48302, V, 1, 1, 1, 1, 0, 704, 99
48303, V, 1, 1, 1, 1, 0, 704, 99
48304, V, 1, 1, 1, 1, 0, 704, 99
48305, V, 1, 1, 1, 1, 0, 704, 99
48306, V, 1, 1, 1, 1, 0, 704, 99
48307, V, 1, 1, 1, 1, 0, 704, 99
48308, V, 1, 1, 1, 1, 0, 704, 99
48309, V, 1, 1, 1, 1, 0, 704, 99
48310, V, 1, 1, 1, 1, 0, 704, 99
48311, V, 1, 1, 1, 1, 0, 704, 99
48312, V, 1, 1, 1, 1, 0, 704, 99
48313, V, 1, 1, 1, 1, 0, 704, 99
48314, V, 1, 1, 1, 1, 0, 704, 99
48315, V, 1, 1, 1, 1, 0, 704, 99
48316, V, 1, 1, 1, 1, 0, 704, 99
48317, V, 1, 1, 1, 1, 0, 704, 99
48318, V, 1, 1, 1, 1, 0, 704, 99
48319, V, 1, 1, 1, 1, 0, 704, 99
48320, V, 1, 1, 1, 1, 0, 704, 99
48321, V, 1, 1, 1, 1, 0, 704, 99
48322, V, 1, 1, 1, 1, 0, 704, 99
48323, V, 1, 1, 1, 1, 0, 704, 99
48324, V, 1, 1, 1, 1, 0, 704, 99
48325, V, 1, 1, 1, 1, 0, 704, 99
48326, V, 1, 1, 1, 1, 0, 704, 99
48327, V, 1, 1, 1, 1, 0, 704, 99
48328, V, 1, 1, 1, 1, 0, 704, 99
48329, V, 1, 1, 1, 1, 0, 704, 99
48330, V, 1, 1, 1, 1, 0, 704, 99
48331, V, 1, 1, 1, 1, 0, 704, 99
48332, V, 1, 1, 1, 1, 0, 704, 99
48333, V, 1, 1, 1, 1, 0, 704, 99
48334, V, 1, 1, 1, 1, 0, 704, 99
48335, V, 1, 1, 1, 1, 0, 704, 99
48336, V, 1, 1, 1, 1, 0, 704, 99
48337, V, 1, 1, 1, 1, 0, 704, 99
48338, V, 1, 1, 1, 1, 0, 704, 99
48339, V, 1, 1, 1, 1, 0, 704, 99
48340, V, 1, 1, 1, 1, 0, 704, 99
48342, V, 1, 1, 1, 1, 0, 704, 99
48343, V, 1, 1, 1, 1, 0, 704, 99
48344, V, 1, 1, 1, 1, 0, 704, 99
48345, V, 1, 1, 1, 1, 0, 704, 99
48346, V, 1, 1, 1, 1, 0, 704, 99
48347, V, 1, 1, 1, 1, 0, 704, 99
48348, V, 1, 1, 1, 1, 0, 704, 99
48349, V, 1, 1, 1, 1, 0, 704, 99
48350, V, 1, 1, 1, 1, 0, 704, 99
48351, V, 1, 1, 1, 1, 0, 704, 99
48352, V, 1, 1, 1, 1, 0, 704, 99
48353, V, 1, 1, 1, 1, 0, 704, 99
48354, V, 1, 1, 1, 1, 0, 704, 99
48355, V, 1, 1, 1, 1, 0, 704, 99
48356, V, 1, 1, 1, 1, 0, 704, 99
48357, V, 1, 1, 1, 1, 0, 704, 99
48358, V, 1, 1, 1, 1, 0, 704, 99
48359, V, 1, 1, 1, 1, 0, 704, 99
48360, V, 1, 1, 1, 1, 0, 704, 99
48361, V, 1, 1, 1, 1, 0, 704, 99
48362, V, 1, 1, 1, 1, 0, 704, 99
48363, V, 1, 1, 1, 1, 0, 704, 99
48364, V, 1, 1, 1, 1, 0, 704, 99
48365, V, 1, 1, 1, 1, 0, 704, 99
48366, V, 1, 1, 1, 1, 0, 704, 99
48367, V, 1, 1, 1, 1, 0, 704, 99
48368, V, 1, 1, 1, 1, 0, 704, 99
48369, V, 1, 1, 1, 1, 0, 704, 99
48370, V, 1, 1, 1, 1, 0, 704, 99
48371, V, 1, 1, 1, 1, 0, 704, 99
48372, V, 1, 1, 1, 1, 0, 704, 99
48373, V, 1, 1, 1, 1, 0, 704, 99
48374, V, 1, 1, 1, 1, 0, 704, 99
48375, V, 1, 1, 1, 1, 0, 704, 99
48376, V, 1, 1, 1, 1, 0, 704, 99
48377, V, 1, 1, 1, 1, 0, 704, 99
48378, V, 1, 1, 1, 1, 0, 704, 99
48379, V, 1, 1, 1, 1, 0, 704, 99
48380, V, 1, 1, 1, 1, 0, 704, 99
48381, V, 1, 1, 1, 1, 0, 704, 99
48382, V, 1, 1, 1, 1, 0, 704, 99
48384, V, 1, 1, 1, 1, 0, 704, 99
48385, V, 1, 1, 1, 1, 0, 704, 99
48386, V, 1, 1, 1, 1, 0, 704, 99
48387, V, 1, 1, 1, 1, 0, 704, 99
48388, V, 1, 1, 1, 1, 0, 704, 99
48389, V, 1, 1, 1, 1, 0, 704, 99
48390, V, 1, 1, 1, 1, 0, 704, 99
48391, V, 1, 1, 1, 1, 0, 704, 99
48392, V, 1, 1, 1, 1, 0, 704, 99
48393, V, 1, 1, 1, 1, 0, 704, 99
48394, V, 1, 1, 1, 1, 0, 704, 99
48395, V, 1, 1, 1, 1, 0, 704, 99
48396, V, 1, 1, 1, 1, 0, 704, 99
48397, V, 1, 1, 1, 1, 0, 704, 99
48398, V, 1, 1, 1, 1, 0, 704, 99
48399, V, 1, 1, 1, 1, 0, 704, 99
48400, V, 1, 1, 1, 1, 0, 704, 99
48401, V, 1, 1, 1, 1, 0, 704, 99
48402, V, 1, 1, 1, 1, 0, 704, 99
48403, V, 1, 1, 1, 1, 0, 704, 99
48404, V, 1, 1, 1, 1, 0, 704, 99
48405, V, 1, 1, 1, 1, 0, 704, 99
48406, V, 1, 1, 1, 1, 0, 704, 99
48407, V, 1, 1, 1, 1, 0, 704, 99
48408, V, 1, 1, 1, 1, 0, 704, 99
48409, V, 1, 1, 1, 1, 0, 704, 99
48410, V, 1, 1, 1, 1, 0, 704, 99
48411, V, 1, 1, 1, 1, 0, 704, 99
48412, V, 1, 1, 1, 1, 0, 704, 99
48413, V, 1, 1, 1, 1, 0, 704, 99
48414, V, 1, 1, 1, 1, 0, 704, 99
48415, V, 1, 1, 1, 1, 0, 704, 99
48416, V, 1, 1, 1, 1, 0, 704, 99
48417, V, 1, 1, 1, 1, 0, 704, 99
48418, V, 1, 1, 1, 1, 0, 704, 99
48419, V, 1, 1, 1, 1, 0, 704, 99
48420, V, 1, 1, 1, 1, 0, 704, 99
48421, V, 1, 1, 1, 1, 0, 704, 99
48422, V, 1, 1, 1, 1, 0, 704, 99
48423, V, 1, 1, 1, 1, 0, 704, 99
48424, V, 1, 1, 1, 1, 0, 704, 99
48425, V, 1, 1, 1, 1, 0, 704, 99
48427, V, 1, 1, 1, 1, 0, 704, 99
48428, V, 1, 1, 1, 1, 0, 704, 99
48429, V, 1, 1, 1, 1, 0, 704, 99
48430, V, 1, 1, 1, 1, 0, 704, 99
48431, V, 1, 1, 1, 1, 0, 704, 99
48432, V, 1, 1, 1, 1, 0, 704, 99
48433, V, 1, 1, 1, 1, 0, 704, 99
48434, V, 1, 1, 1, 1, 0, 704, 99
48435, V, 1, 1, 1, 1, 0, 704, 99
48436, V, 1, 1, 1, 1, 0, 704, 99
48437, V, 1, 1, 1, 1, 0, 704, 99
48438, V, 1, 1, 1, 1, 0, 704, 99
48439, V, 1, 1, 1, 1, 0, 704, 99
48440, V, 1, 1, 1, 1, 0, 704, 99
48441, V, 1, 1, 1, 1, 0, 704, 99
48442, V, 1, 1, 1, 1, 0, 704, 99
48443, V, 1, 1, 1, 1, 0, 704, 99
48444, V, 1, 1, 1, 1, 0, 704, 99
48445, V, 1, 1, 1, 1, 0, 704, 99
48446, V, 1, 1, 1, 1, 0, 704, 99
48447, V, 1, 1, 1, 1, 0, 704, 99
48448, V, 1, 1, 1, 1, 0, 704, 99
48449, V, 1, 1, 1, 1, 0, 704, 99
48450, V, 1, 1, 1, 1, 0, 704, 99
48451, V, 1, 1, 1, 1, 0, 704, 99
48452, V, 1, 1, 1, 1, 0, 704, 99
48453, V, 1, 1, 1, 1, 0, 704, 99
48454, V, 1, 1, 1, 1, 0, 704, 99
48455, V, 1, 1, 1, 1, 0, 704, 99
48456, V, 1, 1, 1, 1, 0, 704, 99
48457, V, 1, 1, 1, 1, 0, 704, 99
48458, V, 1, 1, 1, 1, 0, 704, 99
48459, V, 1, 1, 1, 1, 0, 704, 99
48460, V, 1, 1, 1, 1, 0, 704, 99
48461, V, 1, 1, 1, 1, 0, 704, 99
48462, V, 1, 1, 1, 1, 0, 704, 99
48463, V, 1, 1, 1, 1, 0, 704, 99
48464, V, 1, 1, 1, 1, 0, 704, 99
48465, V, 1, 1, 1, 1, 0, 704, 99
48466, V, 1, 1, 1, 1, 0, 704, 99
48467, V, 1, 1, 1, 1, 0, 704, 99
48468, V, 1, 1, 1, 1, 0, 704, 99
48470, V, 1, 1, 1, 1, 0, 704, 99
48471, V, 1, 1, 1, 1, 0, 704, 99
48472, V, 1, 1, 1, 1, 0, 704, 99
48473, V, 1, 1, 1, 1, 0, 704, 99
48474, V, 1, 1, 1, 1, 0, 704, 99
48475, V, 1, 1, 1, 1, 0, 704, 99
48476, V, 1, 1, 1, 1, 0, 704, 99
48477, V, 1, 1, 1, 1, 0, 704, 99
48478, V, 1, 1, 1, 1, 0, 704, 99
48479, V, 1, 1, 1, 1, 0, 704, 99
48480, V, 1, 1, 1, 1, 0, 704, 99
48481, V, 1, 1, 1, 1, 0, 704, 99
48482, V, 1, 1, 1, 1, 0, 704, 99
48483, V, 1, 1, 1, 1, 0, 704, 99
48484, V, 1, 1, 1, 1, 0, 704, 99
48485, V, 1, 1, 1, 1, 0, 704, 99
48486, V, 1, 1, 1, 1, 0, 704, 99
48487, V, 1, 1, 1, 1, 0, 704, 99
48488, V, 1, 1, 1, 1, 0, 704, 99
48489, V, 1, 1, 1, 1, 0, 704, 99
48490, V, 1, 1, 1, 1, 0, 704, 99
48491, V, 1, 1, 1, 1, 0, 704, 99
48492, V, 1, 1, 1, 1, 0, 704, 99
48493, V, 1, 1, 1, 1, 0, 704, 99
48494, V, 1, 1, 1, 1, 0, 704, 99
48495, V, 1, 1, 1, 1, 0, 704, 99
48496, V, 1, 1, 1, 1, 0, 704, 99
48497, V, 1, 1, 1, 1, 0, 704, 99
48498, V, 1, 1, 1, 1, 0, 704, 99
48499, V, 1, 1, 1, 1, 0, 704, 99
48500, V, 1, 1, 1, 1, 0, 704, 99
48501, V, 1, 1, 1, 1, 0, 704, 99
48502, V, 1, 1, 1, 1, 0, 704, 99
48503, V, 1, 1, 1, 1, 0, 704, 99
48504, V, 1, 1, 1, 1, 0, 704, 99
48505, V, 1, 1, 1, 1, 0, 704, 99
48506, V, 1, 1, 1, 1, 0, 704, 99
48507, V, 1, 1, 1, 1, 0, 704, 99
48508, V, 1, 1, 1, 1, 0, 704, 99
48509, V, 1, 1, 1, 1, 0, 704, 99
48510, V, 1, 1, 1, 1, 0, 704, 99
48512, V, 1, 1, 1, 1, 0, 704, 99
48513, V, 1, 1, 1, 1, 0, 704, 99
48514, V, 1, 1, 1, 1, 0, 704, 99
48515, V, 1, 1, 1, 1, 0, 704, 99
48516, V, 1, 1, 1, 1, 0, 704, 99
48517, V, 1, 1, 1, 1, 0, 704, 99
48518, V, 1, 1, 1, 1, 0, 704, 99
48519, V, 1, 1, 1, 1, 0, 704, 99
48520, V, 1, 1, 1, 1, 0, 704, 99
48521, V, 1, 1, 1, 1, 0, 704, 99
48522, V, 1, 1, 1, 1, 0, 704, 99
48523, V, 1, 1, 1, 1, 0, 704, 99
48524, V, 1, 1, 1, 1, 0, 704, 99
48525, V, 1, 1, 1, 1, 0, 704, 99
48526, V, 1, 1, 1, 1, 0, 704, 99
48527, V, 1, 1, 1, 1, 0, 704, 99
48528, V, 1, 1, 1, 1, 0, 704, 99
48529, V, 1, 1, 1, 1, 0, 704, 99
48530, V, 1, 1, 1, 1, 0, 704, 99
48531, V, 1, 1, 1, 1, 0, 704, 99
48532, V, 1, 1, 1, 1, 0, 704, 99
48533, V, 1, 1, 1, 1, 0, 704, 99
48534, V, 1, 1, 1, 1, 0, 704, 99
48535, V, 1, 1, 1, 1, 0, 704, 99
48536, V, 1, 1, 1, 1, 0, 704, 99
48537, V, 1, 1, 1, 1, 0, 704, 99
48538, V, 1, 1, 1, 1, 0, 704, 99
48539, V, 1, 1, 1, 1, 0, 704, 99
48540, V, 1, 1, 1, 1, 0, 704, 99
48541, V, 1, 1, 1, 1, 0, 704, 99
48542, V, 1, 1, 1, 1, 0, 704, 99
48543, V, 1, 1, 1, 1, 0, 704, 99
48544, V, 1, 1, 1, 1, 0, 704, 99
48545, V, 1, 1, 1, 1, 0, 704, 99
48546, V, 1, 1, 1, 1, 0, 704, 99
48547, V, 1, 1, 1, 1, 0, 704, 99
48548, V, 1, 1, 1, 1, 0, 704, 99
48549, V, 1, 1, 1, 1, 0, 704, 99
48550, V, 1, 1, 1, 1, 0, 704, 99
48551, V, 1, 1, 1, 1, 0, 704, 99
48552, V, 1, 1, 1, 1, 0, 704, 99
48553, V, 1, 1, 1, 1, 0, 704, 99
48555, V, 1, 1, 1, 1, 0, 704, 99
48556, V, 1, 1, 1, 1, 0, 704, 99
48557, V, 1, 1, 1, 1, 0, 704, 99
48558, V, 1, 1, 1, 1, 0, 704, 99
48559, V, 1, 1, 1, 1, 0, 704, 99
48560, V, 1, 1, 1, 1, 0, 704, 99
48561, V, 1, 1, 1, 1, 0, 704, 99
48562, V, 1, 1, 1, 1, 0, 704, 99
48563, V, 1, 1, 1, 1, 0, 704, 99
48564, V, 1, 1, 1, 1, 0, 704, 99
48565, V, 1, 1, 1, 1, 0, 704, 99
48566, V, 1, 1, 1, 1, 0, 704, 99
48567, V, 1, 1, 1, 1, 0, 704, 99
48568, V, 1, 1, 1, 1, 0, 704, 99
48569, V, 1, 1, 1, 1, 0, 704, 99
48570, V, 1, 1, 1, 1, 0, 704, 99
48571, V, 1, 1, 1, 1, 0, 704, 99
48572, V, 1, 1, 1, 1, 0, 704, 99
48573, V, 1, 1, 1, 1, 0, 704, 99
48574, V, 1, 1, 1, 1, 0, 704, 99
48575, V, 1, 1, 1, 1, 0, 704, 99
48576, V, 1, 1, 1, 1, 0, 704, 99
48577, V, 1, 1, 1, 1, 0, 704, 99
48578, V, 1, 1, 1, 1, 0, 704, 99
48579, V, 1, 1, 1, 1, 0, 704, 99
48580, V, 1, 1, 1, 1, 0, 704, 99
48581, V, 1, 1, 1, 1, 0, 704, 99
48582, V, 1, 1, 1, 1, 0, 704, 99
48583, V, 1, 1, 1, 1, 0, 704, 99
48584, V, 1, 1, 1, 1, 0, 704, 99
48585, V, 1, 1, 1, 1, 0, 704, 99
48586, V, 1, 1, 1, 1, 0, 704, 99
48587, V, 1, 1, 1, 1, 0, 704, 99
48588, V, 1, 1, 1, 1, 0, 704, 99
48589, V, 1, 1, 1, 1, 0, 704, 99
48590, V, 1, 1, 1, 1, 0, 704, 99
48591, V, 1, 1, 1, 1, 0, 704, 99
48592, V, 1, 1, 1, 1, 0, 704, 99
48593, V, 1, 1, 1, 1, 0, 704, 99
48594, V, 1, 1, 1, 1, 0, 704, 99
48595, V, 1, 1, 1, 1, 0, 704, 99
48596, V, 1, 1, 1, 1, 0, 704, 99
48598, V, 1, 1, 1, 1, 0, 704, 99
48599, V, 1, 1, 1, 1, 0, 704, 99
48600, V, 1, 1, 1, 1, 0, 704, 99
48601, V, 1, 1, 1, 1, 0, 704, 99
48602, V, 1, 1, 1, 1, 0, 704, 99
48603, V, 1, 1, 1, 1, 0, 704, 99
48604, V, 1, 1, 1, 1, 0, 704, 99
48605, V, 1, 1, 1, 1, 0, 704, 99
48606, V, 1, 1, 1, 1, 0, 704, 99
48607, V, 1, 1, 1, 1, 0, 704, 99
48608, V, 1, 1, 1, 1, 0, 704, 99
48609, V, 1, 1, 1, 1, 0, 704, 99
48610, V, 1, 1, 1, 1, 0, 704, 99
48611, V, 1, 1, 1, 1, 0, 704, 99
48612, V, 1, 1, 1, 1, 0, 704, 99
48613, V, 1, 1, 1, 1, 0, 704, 99
48614, V, 1, 1, 1, 1, 0, 704, 99
48615, V, 1, 1, 1, 1, 0, 704, 99
48616, V, 1, 1, 1, 1, 0, 704, 99
48617, V, 1, 1, 1, 1, 0, 704, 99
48618, V, 1, 1, 1, 1, 0, 704, 99
48619, V, 1, 1, 1, 1, 0, 704, 99
48620, V, 1, 1, 1, 1, 0, 704, 99
48621, V, 1, 1, 1, 1, 0, 704, 99
48622, V, 1, 1, 1, 1, 0, 704, 99
48623, V, 1, 1, 1, 1, 0, 704, 99
48624, V, 1, 1, 1, 1, 0, 704, 99
48625, V, 1, 1, 1, 1, 0, 704, 99
48626, V, 1, 1, 1, 1, 0, 704, 99
48627, V, 1, 1, 1, 1, 0, 704, 99
48628, V, 1, 1, 1, 1, 0, 704, 99
48629, V, 1, 1, 1, 1, 0, 704, 99
48630, V, 1, 1, 1, 1, 0, 704, 99
48631, V, 1, 1, 1, 1, 0, 704, 99
48632, V, 1, 1, 1, 1, 0, 704, 99
48633, V, 1, 1, 1, 1, 0, 704, 99
48634, V, 1, 1, 1, 1, 0, 704, 99
48635, V, 1, 1, 1, 1, 0, 704, 99
48636, V, 1, 1, 1, 1, 0, 704, 99
48637, V, 1, 1, 1, 1, 0, 704, 99
48638, V, 1, 1, 1, 1, 0, 704, 99
48640, V, 1, 1, 1, 1, 0, 704, 99
48641, V, 1, 1, 1, 1, 0, 704, 99
48642, V, 1, 1, 1, 1, 0, 704, 99
48643, V, 1, 1, 1, 1, 0, 704, 99
48644, V, 1, 1, 1, 1, 0, 704, 99
48645, V, 1, 1, 1, 1, 0, 704, 99
48646, V, 1, 1, 1, 1, 0, 704, 99
48647, V, 1, 1, 1, 1, 0, 704, 99
48648, V, 1, 1, 1, 1, 0, 704, 99
48649, V, 1, 1, 1, 1, 0, 704, 99
48650, V, 1, 1, 1, 1, 0, 704, 99
48651, V, 1, 1, 1, 1, 0, 704, 99
48652, V, 1, 1, 1, 1, 0, 704, 99
48653, V, 1, 1, 1, 1, 0, 704, 99
48654, V, 1, 1, 1, 1, 0, 704, 99
48655, V, 1, 1, 1, 1, 0, 704, 99
48656, V, 1, 1, 1, 1, 0, 704, 99
48657, V, 1, 1, 1, 1, 0, 704, 99
48658, V, 1, 1, 1, 1, 0, 704, 99
48659, V, 1, 1, 1, 1, 0, 704, 99
48660, V, 1, 1, 1, 1, 0, 704, 99
48661, V, 1, 1, 1, 1, 0, 704, 99
48662, V, 1, 1, 1, 1, 0, 704, 99
48663, V, 1, 1, 1, 1, 0, 704, 99
48664, V, 1, 1, 1, 1, 0, 704, 99
48665, V, 1, 1, 1, 1, 0, 704, 99
48666, V, 1, 1, 1, 1, 0, 704, 99
48667, V, 1, 1, 1, 1, 0, 704, 99
48668, V, 1, 1, 1, 1, 0, 704, 99
48669, V, 1, 1, 1, 1, 0, 704, 99
48670, V, 1, 1, 1, 1, 0, 704, 99
48671, V, 1, 1, 1, 1, 0, 704, 99
48672, V, 1, 1, 1, 1, 0, 704, 99
48673, V, 1, 1, 1, 1, 0, 704, 99
48674, V, 1, 1, 1, 1, 0, 704, 99
48675, V, 1, 1, 1, 1, 0, 704, 99
48676, V, 1, 1, 1, 1, 0, 704, 99
48677, V, 1, 1, 1, 1, 0, 704, 99
48678, V, 1, 1, 1, 1, 0, 704, 99
48679, V, 1, 1, 1, 1, 0, 704, 99
48680, V, 1, 1, 1, 1, 0, 704, 99
48681, V, 1, 1, 1, 1, 0, 704, 99
48683, V, 1, 1, 1, 1, 0, 704, 99
48684, V, 1, 1, 1, 1, 0, 704, 99
48685, V, 1, 1, 1, 1, 0, 704, 99
48686, V, 1, 1, 1, 1, 0, 704, 99
48687, V, 1, 1, 1, 1, 0, 704, 99
48688, V, 1, 1, 1, 1, 0, 704, 99
48689, V, 1, 1, 1, 1, 0, 704, 99
48690, V, 1, 1, 1, 1, 0, 704, 99
48691, V, 1, 1, 1, 1, 0, 704, 99
48692, V, 1, 1, 1, 1, 0, 704, 99
48693, V, 1, 1, 1, 1, 0, 704, 99
48694, V, 1, 1, 1, 1, 0, 704, 99
48695, V, 1, 1, 1, 1, 0, 704, 99
48696, V, 1, 1, 1, 1, 0, 704, 99
48697, V, 1, 1, 1, 1, 0, 704, 99
48698, V, 1, 1, 1, 1, 0, 704, 99
48699, V, 1, 1, 1, 1, 0, 704, 99
48700, V, 1, 1, 1, 1, 0, 704, 99
48701, V, 1, 1, 1, 1, 0, 704, 99
48702, V, 1, 1, 1, 1, 0, 704, 99
48703, V, 1, 1, 1, 1, 0, 704, 99
48704, V, 1, 1, 1, 1, 0, 704, 99
48705, V, 1, 1, 1, 1, 0, 704, 99
48706, V, 1, 1, 1, 1, 0, 704, 99
48707, V, 1, 1, 1, 1, 0, 704, 99
48708, V, 1, 1, 1, 1, 0, 704, 99
48709, V, 1, 1, 1, 1, 0, 704, 99
48710, V, 1, 1, 1, 1, 0, 704, 99
48711, V, 1, 1, 1, 1, 0, 704, 99
48712, V, 1, 1, 1, 1, 0, 704, 99
48713, V, 1, 1, 1, 1, 0, 704, 99
48714, V, 1, 1, 1, 1, 0, 704, 99
48715, V, 1, 1, 1, 1, 0, 704, 99
48716, V, 1, 1, 1, 1, 0, 704, 99
48717, V, 1, 1, 1, 1, 0, 704, 99
48718, V, 1, 1, 1, 1, 0, 704, 99
48719, V, 1, 1, 1, 1, 0, 704, 99
48720, V, 1, 1, 1, 1, 0, 704, 99
48721, V, 1, 1, 1, 1, 0, 704, 99
48722, V, 1, 1, 1, 1, 0, 704, 99
48723, V, 1, 1, 1, 1, 0, 704, 99
48724, V, 1, 1, 1, 1, 0, 704, 99
48726, V, 1, 1, 1, 1, 0, 704, 99
48727, V, 1, 1, 1, 1, 0, 704, 99
48728, V, 1, 1, 1, 1, 0, 704, 99
48729, V, 1, 1, 1, 1, 0, 704, 99
48730, V, 1, 1, 1, 1, 0, 704, 99
48731, V, 1, 1, 1, 1, 0, 704, 99
48732, V, 1, 1, 1, 1, 0, 704, 99
48733, V, 1, 1, 1, 1, 0, 704, 99
48734, V, 1, 1, 1, 1, 0, 704, 99
48735, V, 1, 1, 1, 1, 0, 704, 99
48736, V, 1, 1, 1, 1, 0, 704, 99
48737, V, 1, 1, 1, 1, 0, 704, 99
48738, V, 1, 1, 1, 1, 0, 704, 99
48739, V, 1, 1, 1, 1, 0, 704, 99
48740, V, 1, 1, 1, 1, 0, 704, 99
48741, V, 1, 1, 1, 1, 0, 704, 99
48742, V, 1, 1, 1, 1, 0, 704, 99
48743, V, 1, 1, 1, 1, 0, 704, 99
48744, V, 1, 1, 1, 1, 0, 704, 99
48745, V, 1, 1, 1, 1, 0, 704, 99
48746, V, 1, 1, 1, 1, 0, 704, 99
48747, V, 1, 1, 1, 1, 0, 704, 99
48748, V, 1, 1, 1, 1, 0, 704, 99
48749, V, 1, 1, 1, 1, 0, 704, 99
48750, V, 1, 1, 1, 1, 0, 704, 99
48751, V, 1, 1, 1, 1, 0, 704, 99
48752, V, 1, 1, 1, 1, 0, 704, 99
48753, V, 1, 1, 1, 1, 0, 704, 99
48754, V, 1, 1, 1, 1, 0, 704, 99
48755, V, 1, 1, 1, 1, 0, 704, 99
48756, V, 1, 1, 1, 1, 0, 704, 99
48757, V, 1, 1, 1, 1, 0, 704, 99
48758, V, 1, 1, 1, 1, 0, 704, 99
48759, V, 1, 1, 1, 1, 0, 704, 99
48760, V, 1, 1, 1, 1, 0, 704, 99
48761, V, 1, 1, 1, 1, 0, 704, 99
48762, V, 1, 1, 1, 1, 0, 704, 99
48763, V, 1, 1, 1, 1, 0, 704, 99
48764, V, 1, 1, 1, 1, 0, 704, 99
48765, V, 1, 1, 1, 1, 0, 704, 99
48766, V, 1, 1, 1, 1, 0, 704, 99
48768, V, 1, 1, 1, 1, 0, 704, 99
48769, V, 1, 1, 1, 1, 0, 704, 99
48770, V, 1, 1, 1, 1, 0, 704, 99
48771, V, 1, 1, 1, 1, 0, 704, 99
48772, V, 1, 1, 1, 1, 0, 704, 99
48773, V, 1, 1, 1, 1, 0, 704, 99
48774, V, 1, 1, 1, 1, 0, 704, 99
48775, V, 1, 1, 1, 1, 0, 704, 99
48776, V, 1, 1, 1, 1, 0, 704, 99
48777, V, 1, 1, 1, 1, 0, 704, 99
48778, V, 1, 1, 1, 1, 0, 704, 99
48779, V, 1, 1, 1, 1, 0, 704, 99
48780, V, 1, 1, 1, 1, 0, 704, 99
48781, V, 1, 1, 1, 1, 0, 704, 99
48782, V, 1, 1, 1, 1, 0, 704, 99
48783, V, 1, 1, 1, 1, 0, 704, 99
48784, V, 1, 1, 1, 1, 0, 704, 99
48785, V, 1, 1, 1, 1, 0, 704, 99
48786, V, 1, 1, 1, 1, 0, 704, 99
48787, V, 1, 1, 1, 1, 0, 704, 99
48788, V, 1, 1, 1, 1, 0, 704, 99
48789, V, 1, 1, 1, 1, 0, 704, 99
48790, V, 1, 1, 1, 1, 0, 704, 99
48791, V, 1, 1, 1, 1, 0, 704, 99
48792, V, 1, 1, 1, 1, 0, 704, 99
48793, V, 1, 1, 1, 1, 0, 704, 99
48794, V, 1, 1, 1, 1, 0, 704, 99
48795, V, 1, 1, 1, 1, 0, 704, 99
48796, V, 1, 1, 1, 1, 0, 704, 99
48797, V, 1, 1, 1, 1, 0, 704, 99
48798, V, 1, 1, 1, 1, 0, 704, 99
48799, V, 1, 1, 1, 1, 0, 704, 99
48800, V, 1, 1, 1, 1, 0, 704, 99
48801, V, 1, 1, 1, 1, 0, 704, 99
48802, V, 1, 1, 1, 1, 0, 704, 99
48803, V, 1, 1, 1, 1, 0, 704, 99
48804, V, 1, 1, 1, 1, 0, 704, 99
48805, V, 1, 1, 1, 1, 0, 704, 99
48806, V, 1, 1, 1, 1, 0, 704, 99
48807, V, 1, 1, 1, 1, 0, 704, 99
48808, V, 1, 1, 1, 1, 0, 704, 99
48809, V, 1, 1, 1, 1, 0, 704, 99
48811, V, 1, 1, 1, 1, 0, 704, 99
48812, V, 1, 1, 1, 1, 0, 704, 99
48813, V, 1, 1, 1, 1, 0, 704, 99
48814, V, 1, 1, 1, 1, 0, 704, 99
48815, V, 1, 1, 1, 1, 0, 704, 99
48816, V, 1, 1, 1, 1, 0, 704, 99
48817, V, 1, 1, 1, 1, 0, 704, 99
48818, V, 1, 1, 1, 1, 0, 704, 99
48819, V, 1, 1, 1, 1, 0, 704, 99
48820, V, 1, 1, 1, 1, 0, 704, 99
48821, V, 1, 1, 1, 1, 0, 704, 99
48822, V, 1, 1, 1, 1, 0, 704, 99
48823, V, 1, 1, 1, 1, 0, 704, 99
48824, V, 1, 1, 1, 1, 0, 704, 99
48825, V, 1, 1, 1, 1, 0, 704, 99
48826, V, 1, 1, 1, 1, 0, 704, 99
48827, V, 1, 1, 1, 1, 0, 704, 99
48828, V, 1, 1, 1, 1, 0, 704, 99
48829, V, 1, 1, 1, 1, 0, 704, 99
48830, V, 1, 1, 1, 1, 0, 704, 99
48831, V, 1, 1, 1, 1, 0, 704, 99
48832, V, 1, 1, 1, 1, 0, 704, 99
48833, V, 1, 1, 1, 1, 0, 704, 99
48834, V, 1, 1, 1, 1, 0, 704, 99
48835, V, 1, 1, 1, 1, 0, 704, 99
48836, V, 1, 1, 1, 1, 0, 704, 99
48837, V, 1, 1, 1, 1, 0, 704, 99
48838, V, 1, 1, 1, 1, 0, 704, 99
48839, V, 1, 1, 1, 1, 0, 704, 99
48840, V, 1, 1, 1, 1, 0, 704, 99
48841, V, 1, 1, 1, 1, 0, 704, 99
48842, V, 1, 1, 1, 1, 0, 704, 99
48843, V, 1, 1, 1, 1, 0, 704, 99
48844, V, 1, 1, 1, 1, 0, 704, 99
48845, V, 1, 1, 1, 1, 0, 704, 99
48846, V, 1, 1, 1, 1, 0, 704, 99
48847, V, 1, 1, 1, 1, 0, 704, 99
48848, V, 1, 1, 1, 1, 0, 704, 99
48849, V, 1, 1, 1, 1, 0, 704, 99
48850, V, 1, 1, 1, 1, 0, 704, 99
48851, V, 1, 1, 1, 1, 0, 704, 99
48852, V, 1, 1, 1, 1, 0, 704, 99
48854, V, 1, 1, 1, 1, 0, 704, 99
48855, V, 1, 1, 1, 1, 0, 704, 99
48856, V, 1, 1, 1, 1, 0, 704, 99
48857, V, 1, 1, 1, 1, 0, 704, 99
48858, V, 1, 1, 1, 1, 0, 704, 99
48859, V, 1, 1, 1, 1, 0, 704, 99
48860, V, 1, 1, 1, 1, 0, 704, 99
48861, V, 1, 1, 1, 1, 0, 704, 99
48862, V, 1, 1, 1, 1, 0, 704, 99
48863, V, 1, 1, 1, 1, 0, 704, 99
48864, V, 1, 1, 1, 1, 0, 704, 99
48865, V, 1, 1, 1, 1, 0, 704, 99
48866, V, 1, 1, 1, 1, 0, 704, 99
48867, V, 1, 1, 1, 1, 0, 704, 99
48868, V, 1, 1, 1, 1, 0, 704, 99
48869, V, 1, 1, 1, 1, 0, 704, 99
48870, V, 1, 1, 1, 1, 0, 704, 99
48871, V, 1, 1, 1, 1, 0, 704, 99
48872, V, 1, 1, 1, 1, 0, 704, 99
48873, V, 1, 1, 1, 1, 0, 704, 99
48874, V, 1, 1, 1, 1, 0, 704, 99
48875, V, 1, 1, 1, 1, 0, 704, 99
48876, V, 1, 1, 1, 1, 0, 704, 99
48877, V, 1, 1, 1, 1, 0, 704, 99
48878, V, 1, 1, 1, 1, 0, 704, 99
48879, V, 1, 1, 1, 1, 0, 704, 99
48880, V, 1, 1, 1, 1, 0, 704, 99
48881, V, 1, 1, 1, 1, 0, 704, 99
48882, V, 1, 1, 1, 1, 0, 704, 99
48883, V, 1, 1, 1, 1, 0, 704, 99
48884, V, 1, 1, 1, 1, 0, 704, 99
48885, V, 1, 1, 1, 1, 0, 704, 99
48886, V, 1, 1, 1, 1, 0, 704, 99
48887, V, 1, 1, 1, 1, 0, 704, 99
48888, V, 1, 1, 1, 1, 0, 704, 99
48889, V, 1, 1, 1, 1, 0, 704, 99
48890, V, 1, 1, 1, 1, 0, 704, 99
48891, V, 1, 1, 1, 1, 0, 704, 99
48892, V, 1, 1, 1, 1, 0, 704, 99
48893, V, 1, 1, 1, 1, 0, 704, 99
48894, V, 1, 1, 1, 1, 0, 704, 99
48896, V, 1, 1, 1, 1, 0, 704, 99
48897, V, 1, 1, 1, 1, 0, 704, 99
48898, V, 1, 1, 1, 1, 0, 704, 99
48899, V, 1, 1, 1, 1, 0, 704, 99
48900, V, 1, 1, 1, 1, 0, 704, 99
48901, V, 1, 1, 1, 1, 0, 704, 99
48902, V, 1, 1, 1, 1, 0, 704, 99
48903, V, 1, 1, 1, 1, 0, 704, 99
48904, V, 1, 1, 1, 1, 0, 704, 99
48905, V, 1, 1, 1, 1, 0, 704, 99
48906, V, 1, 1, 1, 1, 0, 704, 99
48907, V, 1, 1, 1, 1, 0, 704, 99
48908, V, 1, 1, 1, 1, 0, 704, 99
48909, V, 1, 1, 1, 1, 0, 704, 99
48910, V, 1, 1, 1, 1, 0, 704, 99
48911, V, 1, 1, 1, 1, 0, 704, 99
48912, V, 1, 1, 1, 1, 0, 704, 99
48913, V, 1, 1, 1, 1, 0, 704, 99
48914, V, 1, 1, 1, 1, 0, 704, 99
48915, V, 1, 1, 1, 1, 0, 704, 99
48916, V, 1, 1, 1, 1, 0, 704, 99
48917, V, 1, 1, 1, 1, 0, 704, 99
48918, V, 1, 1, 1, 1, 0, 704, 99
48919, V, 1, 1, 1, 1, 0, 704, 99
48920, V, 1, 1, 1, 1, 0, 704, 99
48921, V, 1, 1, 1, 1, 0, 704, 99
48922, V, 1, 1, 1, 1, 0, 704, 99
48923, V, 1, 1, 1, 1, 0, 704, 99
48924, V, 1, 1, 1, 1, 0, 704, 99
48925, V, 1, 1, 1, 1, 0, 704, 99
48926, V, 1, 1, 1, 1, 0, 704, 99
48927, V, 1, 1, 1, 1, 0, 704, 99
48928, V, 1, 1, 1, 1, 0, 704, 99
48929, V, 1, 1, 1, 1, 0, 704, 99
48930, V, 1, 1, 1, 1, 0, 704, 99
48931, V, 1, 1, 1, 1, 0, 704, 99
48932, V, 1, 1, 1, 1, 0, 704, 99
48933, V, 1, 1, 1, 1, 0, 704, 99
48934, V, 1, 1, 1, 1, 0, 704, 99
48935, V, 1, 1, 1, 1, 0, 704, 99
48936, V, 1, 1, 1, 1, 0, 704, 99
48937, V, 1, 1, 1, 1, 0, 704, 99
48939, V, 1, 1, 1, 1, 0, 704, 99
48940, V, 1, 1, 1, 1, 0, 704, 99
48941, V, 1, 1, 1, 1, 0, 704, 99
48942, V, 1, 1, 1, 1, 0, 704, 99
48943, V, 1, 1, 1, 1, 0, 704, 99
48944, V, 1, 1, 1, 1, 0, 704, 99
48945, V, 1, 1, 1, 1, 0, 704, 99
48946, V, 1, 1, 1, 1, 0, 704, 99
48947, V, 1, 1, 1, 1, 0, 704, 99
48948, V, 1, 1, 1, 1, 0, 704, 99
48949, V, 1, 1, 1, 1, 0, 704, 99
48950, V, 1, 1, 1, 1, 0, 704, 99
48951, V, 1, 1, 1, 1, 0, 704, 99
48952, V, 1, 1, 1, 1, 0, 704, 99
48953, V, 1, 1, 1, 1, 0, 704, 99
48954, V, 1, 1, 1, 1, 0, 704, 99
48955, V, 1, 1, 1, 1, 0, 704, 99
48956, V, 1, 1, 1, 1, 0, 704, 99
48957, V, 1, 1, 1, 1, 0, 704, 99
48958, V, 1, 1, 1, 1, 0, 704, 99
48959, V, 1, 1, 1, 1, 0, 704, 99
48960, V, 1, 1, 1, 1, 0, 704, 99
48961, V, 1, 1, 1, 1, 0, 704, 99
48962, V, 1, 1, 1, 1, 0, 704, 99
48963, V, 1, 1, 1, 1, 0, 704, 99
48964, V, 1, 1, 1, 1, 0, 704, 99
48965, V, 1, 1, 1, 1, 0, 704, 99
48966, V, 1, 1, 1, 1, 0, 704, 99
48967, V, 1, 1, 1, 1, 0, 704, 99
48968, V, 1, 1, 1, 1, 0, 704, 99
48969, V, 1, 1, 1, 1, 0, 704, 99
48970, V, 1, 1, 1, 1, 0, 704, 99
48971, V, 1, 1, 1, 1, 0, 704, 99
48972, V, 1, 1, 1, 1, 0, 704, 99
48973, V, 1, 1, 1, 1, 0, 704, 99
48974, V, 1, 1, 1, 1, 0, 704, 99
48975, V, 1, 1, 1, 1, 0, 704, 99
48976, V, 1, 1, 1, 1, 0, 704, 99
48977, V, 1, 1, 1, 1, 0, 704, 99
48978, V, 1, 1, 1, 1, 0, 704, 99
48979, V, 1, 1, 1, 1, 0, 704, 99
48980, V, 1, 1, 1, 1, 0, 704, 99
48982, V, 1, 1, 1, 1, 0, 704, 99
48983, V, 1, 1, 1, 1, 0, 704, 99
48984, V, 1, 1, 1, 1, 0, 704, 99
48985, V, 1, 1, 1, 1, 0, 704, 99
48986, V, 1, 1, 1, 1, 0, 704, 99
48987, V, 1, 1, 1, 1, 0, 704, 99
48988, V, 1, 1, 1, 1, 0, 704, 99
48989, V, 1, 1, 1, 1, 0, 704, 99
48990, V, 1, 1, 1, 1, 0, 704, 99
48991, V, 1, 1, 1, 1, 0, 704, 99
48992, V, 1, 1, 1, 1, 0, 704, 99
48993, V, 1, 1, 1, 1, 0, 704, 99
48994, V, 1, 1, 1, 1, 0, 704, 99
48995, V, 1, 1, 1, 1, 0, 704, 99
48996, V, 1, 1, 1, 1, 0, 704, 99
48997, V, 1, 1, 1, 1, 0, 704, 99
48998, V, 1, 1, 1, 1, 0, 704, 99
48999, V, 1, 1, 1, 1, 0, 704, 99
49000, V, 1, 1, 1, 1, 0, 704, 99
49001, V, 1, 1, 1, 1, 0, 704, 99
49002, V, 1, 1, 1, 1, 0, 704, 99
49003, V, 1, 1, 1, 1, 0, 704, 99
49004, V, 1, 1, 1, 1, 0, 704, 99
49005, V, 1, 1, 1, 1, 0, 704, 99
49006, V, 1, 1, 1, 1, 0, 704, 99
49007, V, 1, 1, 1, 1, 0, 704, 99
49008, V, 1, 1, 1, 1, 0, 704, 99
49009, V, 1, 1, 1, 1, 0, 704, 99
49010, V, 1, 1, 1, 1, 0, 704, 99
49011, V, 1, 1, 1, 1, 0, 704, 99
49012, V, 1, 1, 1, 1, 0, 704, 99
49013, V, 1, 1, 1, 1, 0, 704, 99
49014, V, 1, 1, 1, 1, 0, 704, 99
49015, V, 1, 1, 1, 1, 0, 704, 99
49016, V, 1, 1, 1, 1, 0, 704, 99
49017, V, 1, 1, 1, 1, 0, 704, 99
49018, V, 1, 1, 1, 1, 0, 704, 99
49019, V, 1, 1, 1, 1, 0, 704, 99
49020, V, 1, 1, 1, 1, 0, 704, 99
49021, V, 1, 1, 1, 1, 0, 704, 99
49022, V, 1, 1, 1, 1, 0, 704, 99
49024, V, 1, 1, 1, 1, 0, 704, 99
49025, V, 1, 1, 1, 1, 0, 704, 99
49026, V, 1, 1, 1, 1, 0, 704, 99
49027, V, 1, 1, 1, 1, 0, 704, 99
49028, V, 1, 1, 1, 1, 0, 704, 99
49029, V, 1, 1, 1, 1, 0, 704, 99
49030, V, 1, 1, 1, 1, 0, 704, 99
49031, V, 1, 1, 1, 1, 0, 704, 99
49032, V, 1, 1, 1, 1, 0, 704, 99
49033, V, 1, 1, 1, 1, 0, 704, 99
49034, V, 1, 1, 1, 1, 0, 704, 99
49035, V, 1, 1, 1, 1, 0, 704, 99
49036, V, 1, 1, 1, 1, 0, 704, 99
49037, V, 1, 1, 1, 1, 0, 704, 99
49038, V, 1, 1, 1, 1, 0, 704, 99
49039, V, 1, 1, 1, 1, 0, 704, 99
49040, V, 1, 1, 1, 1, 0, 704, 99
49041, V, 1, 1, 1, 1, 0, 704, 99
49042, V, 1, 1, 1, 1, 0, 704, 99
49043, V, 1, 1, 1, 1, 0, 704, 99
49044, V, 1, 1, 1, 1, 0, 704, 99
49045, V, 1, 1, 1, 1, 0, 704, 99
49046, V, 1, 1, 1, 1, 0, 704, 99
49047, V, 1, 1, 1, 1, 0, 704, 99
49048, V, 1, 1, 1, 1, 0, 704, 99
49049, V, 1, 1, 1, 1, 0, 704, 99
49050, V, 1, 1, 1, 1, 0, 704, 99
49051, V, 1, 1, 1, 1, 0, 704, 99
49052, V, 1, 1, 1, 1, 0, 704, 99
49053, V, 1, 1, 1, 1, 0, 704, 99
49054, V, 1, 1, 1, 1, 0, 704, 99
49055, V, 1, 1, 1, 1, 0, 704, 99
49056, V, 1, 1, 1, 1, 0, 704, 99
49057, V, 1, 1, 1, 1, 0, 704, 99
49058, V, 1, 1, 1, 1, 0, 704, 99
49059, V, 1, 1, 1, 1, 0, 704, 99
49060, V, 1, 1, 1, 1, 0, 704, 99
49061, V, 1, 1, 1, 1, 0, 704, 99
49062, V, 1, 1, 1, 1, 0, 704, 99
49063, V, 1, 1, 1, 1, 0, 704, 99
49064, V, 1, 1, 1, 1, 0, 704, 99
49065, V, 1, 1, 1, 1, 0, 704, 99
49067, V, 1, 1, 1, 1, 0, 704, 99
49068, V, 1, 1, 1, 1, 0, 704, 99
49069, V, 1, 1, 1, 1, 0, 704, 99
49070, V, 1, 1, 1, 1, 0, 704, 99
49071, V, 1, 1, 1, 1, 0, 704, 99
49072, V, 1, 1, 1, 1, 0, 704, 99
49073, V, 1, 1, 1, 1, 0, 704, 99
49074, V, 1, 1, 1, 1, 0, 704, 99
49075, V, 1, 1, 1, 1, 0, 704, 99
49076, V, 1, 1, 1, 1, 0, 704, 99
49077, V, 1, 1, 1, 1, 0, 704, 99
49078, V, 1, 1, 1, 1, 0, 704, 99
49079, V, 1, 1, 1, 1, 0, 704, 99
49080, V, 1, 1, 1, 1, 0, 704, 99
49081, V, 1, 1, 1, 1, 0, 704, 99
49082, V, 1, 1, 1, 1, 0, 704, 99
49083, V, 1, 1, 1, 1, 0, 704, 99
49084, V, 1, 1, 1, 1, 0, 704, 99
49085, V, 1, 1, 1, 1, 0, 704, 99
49086, V, 1, 1, 1, 1, 0, 704, 99
49087, V, 1, 1, 1, 1, 0, 704, 99
49088, V, 1, 1, 1, 1, 0, 704, 99
49089, V, 1, 1, 1, 1, 0, 704, 99
49090, V, 1, 1, 1, 1, 0, 704, 99
49091, V, 1, 1, 1, 1, 0, 704, 99
49092, V, 1, 1, 1, 1, 0, 704, 99
49093, V, 1, 1, 1, 1, 0, 704, 99
49094, V, 1, 1, 1, 1, 0, 704, 99
49095, V, 1, 1, 1, 1, 0, 704, 99
49096, V, 1, 1, 1, 1, 0, 704, 99
49097, V, 1, 1, 1, 1, 0, 704, 99
49098, V, 1, 1, 1, 1, 0, 704, 99
49099, V, 1, 1, 1, 1, 0, 704, 99
49100, V, 1, 1, 1, 1, 0, 704, 99
49101, V, 1, 1, 1, 1, 0, 704, 99
49102, V, 1, 1, 1, 1, 0, 704, 99
49103, V, 1, 1, 1, 1, 0, 704, 99
49104, V, 1, 1, 1, 1, 0, 704, 99
49105, V, 1, 1, 1, 1, 0, 704, 99
49106, V, 1, 1, 1, 1, 0, 704, 99
49107, V, 1, 1, 1, 1, 0, 704, 99
49108, V, 1, 1, 1, 1, 0, 704, 99
49110, V, 1, 1, 1, 1, 0, 704, 99
49111, V, 1, 1, 1, 1, 0, 704, 99
49112, V, 1, 1, 1, 1, 0, 704, 99
49113, V, 1, 1, 1, 1, 0, 704, 99
49114, V, 1, 1, 1, 1, 0, 704, 99
49115, V, 1, 1, 1, 1, 0, 704, 99
49116, V, 1, 1, 1, 1, 0, 704, 99
49117, V, 1, 1, 1, 1, 0, 704, 99
49118, V, 1, 1, 1, 1, 0, 704, 99
49119, V, 1, 1, 1, 1, 0, 704, 99
49120, V, 1, 1, 1, 1, 0, 704, 99
49121, V, 1, 1, 1, 1, 0, 704, 99
49122, V, 1, 1, 1, 1, 0, 704, 99
49123, V, 1, 1, 1, 1, 0, 704, 99
49124, V, 1, 1, 1, 1, 0, 704, 99
49125, V, 1, 1, 1, 1, 0, 704, 99
49126, V, 1, 1, 1, 1, 0, 704, 99
49127, V, 1, 1, 1, 1, 0, 704, 99
49128, V, 1, 1, 1, 1, 0, 704, 99
49129, V, 1, 1, 1, 1, 0, 704, 99
49130, V, 1, 1, 1, 1, 0, 704, 99
49131, V, 1, 1, 1, 1, 0, 704, 99
49132, V, 1, 1, 1, 1, 0, 704, 99
49133, V, 1, 1, 1, 1, 0, 704, 99
49134, V, 1, 1, 1, 1, 0, 704, 99
49135, V, 1, 1, 1, 1, 0, 704, 99
49136, V, 1, 1, 1, 1, 0, 704, 99
49137, V, 1, 1, 1, 1, 0, 704, 99
49138, V, 1, 1, 1, 1, 0, 704, 99
49139, V, 1, 1, 1, 1, 0, 704, 99
49140, V, 1, 1, 1, 1, 0, 704, 99
49141, V, 1, 1, 1, 1, 0, 704, 99
49142, V, 1, 1, 1, 1, 0, 704, 99
49143, V, 1, 1, 1, 1, 0, 704, 99
49144, V, 1, 1, 1, 1, 0, 704, 99
49145, V, 1, 1, 1, 1, 0, 704, 99
49146, V, 1, 1, 1, 1, 0, 704, 99
49147, V, 1, 1, 1, 1, 0, 704, 99
49148, V, 1, 1, 1, 1, 0, 704, 99
49149, V, 1, 1, 1, 1, 0, 704, 99
49150, V, 1, 1, 1, 1, 0, 704, 99
49152, V, 1, 1, 1, 1, 0, 704, 99
49153, V, 1, 1, 1, 1, 0, 704, 99
49154, V, 1, 1, 1, 1, 0, 704, 99
49155, V, 1, 1, 1, 1, 0, 704, 99
49156, V, 1, 1, 1, 1, 0, 704, 99
49157, V, 1, 1, 1, 1, 0, 704, 99
49158, V, 1, 1, 1, 1, 0, 704, 99
49159, V, 1, 1, 1, 1, 0, 704, 99
49160, V, 1, 1, 1, 1, 0, 704, 99
49161, V, 1, 1, 1, 1, 0, 704, 99
49162, V, 1, 1, 1, 1, 0, 704, 99
49163, V, 1, 1, 1, 1, 0, 704, 99
49164, V, 1, 1, 1, 1, 0, 704, 99
49165, V, 1, 1, 1, 1, 0, 704, 99
49166, V, 1, 1, 1, 1, 0, 704, 99
49167, V, 1, 1, 1, 1, 0, 704, 99
49168, V, 1, 1, 1, 1, 0, 704, 99
49169, V, 1, 1, 1, 1, 0, 704, 99
49170, V, 1, 1, 1, 1, 0, 704, 99
49171, V, 1, 1, 1, 1, 0, 704, 99
49172, V, 1, 1, 1, 1, 0, 704, 99
49173, V, 1, 1, 1, 1, 0, 704, 99
49174, V, 1, 1, 1, 1, 0, 704, 99
49175, V, 1, 1, 1, 1, 0, 704, 99
49176, V, 1, 1, 1, 1, 0, 704, 99
49177, V, 1, 1, 1, 1, 0, 704, 99
49178, V, 1, 1, 1, 1, 0, 704, 99
49179, V, 1, 1, 1, 1, 0, 704, 99
49180, V, 1, 1, 1, 1, 0, 704, 99
49181, V, 1, 1, 1, 1, 0, 704, 99
49182, V, 1, 1, 1, 1, 0, 704, 99
49183, V, 1, 1, 1, 1, 0, 704, 99
49184, V, 1, 1, 1, 1, 0, 704, 99
49185, V, 1, 1, 1, 1, 0, 704, 99
49186, V, 1, 1, 1, 1, 0, 704, 99
49187, V, 1, 1, 1, 1, 0, 704, 99
49188, V, 1, 1, 1, 1, 0, 704, 99
49189, V, 1, 1, 1, 1, 0, 704, 99
49190, V, 1, 1, 1, 1, 0, 704, 99
49191, V, 1, 1, 1, 1, 0, 704, 99
49192, V, 1, 1, 1, 1, 0, 704, 99
49193, V, 1, 1, 1, 1, 0, 704, 99
49195, V, 1, 1, 1, 1, 0, 704, 99
49196, V, 1, 1, 1, 1, 0, 704, 99
49197, V, 1, 1, 1, 1, 0, 704, 99
49198, V, 1, 1, 1, 1, 0, 704, 99
49199, V, 1, 1, 1, 1, 0, 704, 99
49200, V, 1, 1, 1, 1, 0, 704, 99
49201, V, 1, 1, 1, 1, 0, 704, 99
49202, V, 1, 1, 1, 1, 0, 704, 99
49203, V, 1, 1, 1, 1, 0, 704, 99
49204, V, 1, 1, 1, 1, 0, 704, 99
49205, V, 1, 1, 1, 1, 0, 704, 99
49206, V, 1, 1, 1, 1, 0, 704, 99
49207, V, 1, 1, 1, 1, 0, 704, 99
49208, V, 1, 1, 1, 1, 0, 704, 99
49209, V, 1, 1, 1, 1, 0, 704, 99
49210, V, 1, 1, 1, 1, 0, 704, 99
49211, V, 1, 1, 1, 1, 0, 704, 99
49212, V, 1, 1, 1, 1, 0, 704, 99
49213, V, 1, 1, 1, 1, 0, 704, 99
49214, V, 1, 1, 1, 1, 0, 704, 99
49215, V, 1, 1, 1, 1, 0, 704, 99
49216, V, 1, 1, 1, 1, 0, 704, 99
49217, V, 1, 1, 1, 1, 0, 704, 99
49218, V, 1, 1, 1, 1, 0, 704, 99
49219, V, 1, 1, 1, 1, 0, 704, 99
49220, V, 1, 1, 1, 1, 0, 704, 99
49221, V, 1, 1, 1, 1, 0, 704, 99
49222, V, 1, 1, 1, 1, 0, 704, 99
49223, V, 1, 1, 1, 1, 0, 704, 99
49224, V, 1, 1, 1, 1, 0, 704, 99
49225, V, 1, 1, 1, 1, 0, 704, 99
49226, V, 1, 1, 1, 1, 0, 704, 99
49227, V, 1, 1, 1, 1, 0, 704, 99
49228, V, 1, 1, 1, 1, 0, 704, 99
49229, V, 1, 1, 1, 1, 0, 704, 99
49230, V, 1, 1, 1, 1, 0, 704, 99
49231, V, 1, 1, 1, 1, 0, 704, 99
49232, V, 1, 1, 1, 1, 0, 704, 99
49233, V, 1, 1, 1, 1, 0, 704, 99
49234, V, 1, 1, 1, 1, 0, 704, 99
49235, V, 1, 1, 1, 1, 0, 704, 99
49236, V, 1, 1, 1, 1, 0, 704, 99
49238, V, 1, 1, 1, 1, 0, 704, 99
49239, V, 1, 1, 1, 1, 0, 704, 99
49240, V, 1, 1, 1, 1, 0, 704, 99
49241, V, 1, 1, 1, 1, 0, 704, 99
49242, V, 1, 1, 1, 1, 0, 704, 99
49243, V, 1, 1, 1, 1, 0, 704, 99
49244, V, 1, 1, 1, 1, 0, 704, 99
49245, V, 1, 1, 1, 1, 0, 704, 99
49246, V, 1, 1, 1, 1, 0, 704, 99
49247, V, 1, 1, 1, 1, 0, 704, 99
49248, V, 1, 1, 1, 1, 0, 704, 99
49249, V, 1, 1, 1, 1, 0, 704, 99
49250, V, 1, 1, 1, 1, 0, 704, 99
49251, V, 1, 1, 1, 1, 0, 704, 99
49252, V, 1, 1, 1, 1, 0, 704, 99
49253, V, 1, 1, 1, 1, 0, 704, 99
49254, V, 1, 1, 1, 1, 0, 704, 99
49255, V, 1, 1, 1, 1, 0, 704, 99
49256, V, 1, 1, 1, 1, 0, 704, 99
49257, V, 1, 1, 1, 1, 0, 704, 99
49258, V, 1, 1, 1, 1, 0, 704, 99
49259, V, 1, 1, 1, 1, 0, 704, 99
49260, V, 1, 1, 1, 1, 0, 704, 99
49261, V, 1, 1, 1, 1, 0, 704, 99
49262, V, 1, 1, 1, 1, 0, 704, 99
49263, V, 1, 1, 1, 1, 0, 704, 99
49264, V, 1, 1, 1, 1, 0, 704, 99
49265, V, 1, 1, 1, 1, 0, 704, 99
49266, V, 1, 1, 1, 1, 0, 704, 99
49267, V, 1, 1, 1, 1, 0, 704, 99
49268, V, 1, 1, 1, 1, 0, 704, 99
49269, V, 1, 1, 1, 1, 0, 704, 99
49270, V, 1, 1, 1, 1, 0, 704, 99
49271, V, 1, 1, 1, 1, 0, 704, 99
49272, V, 1, 1, 1, 1, 0, 704, 99
49273, V, 1, 1, 1, 1, 0, 704, 99
49274, V, 1, 1, 1, 1, 0, 704, 99
49275, V, 1, 1, 1, 1, 0, 704, 99
49276, V, 1, 1, 1, 1, 0, 704, 99
49277, V, 1, 1, 1, 1, 0, 704, 99
49278, V, 1, 1, 1, 1, 0, 704, 99
49280, V, 1, 1, 1, 1, 0, 704, 99
49281, V, 1, 1, 1, 1, 0, 704, 99
49282, V, 1, 1, 1, 1, 0, 704, 99
49283, V, 1, 1, 1, 1, 0, 704, 99
49284, V, 1, 1, 1, 1, 0, 704, 99
49285, V, 1, 1, 1, 1, 0, 704, 99
49286, V, 1, 1, 1, 1, 0, 704, 99
49287, V, 1, 1, 1, 1, 0, 704, 99
49288, V, 1, 1, 1, 1, 0, 704, 99
49289, V, 1, 1, 1, 1, 0, 704, 99
49290, V, 1, 1, 1, 1, 0, 704, 99
49291, V, 1, 1, 1, 1, 0, 704, 99
49292, V, 1, 1, 1, 1, 0, 704, 99
49293, V, 1, 1, 1, 1, 0, 704, 99
49294, V, 1, 1, 1, 1, 0, 704, 99
49295, V, 1, 1, 1, 1, 0, 704, 99
49296, V, 1, 1, 1, 1, 0, 704, 99
49297, V, 1, 1, 1, 1, 0, 704, 99
49298, V, 1, 1, 1, 1, 0, 704, 99
49299, V, 1, 1, 1, 1, 0, 704, 99
49300, V, 1, 1, 1, 1, 0, 704, 99
49301, V, 1, 1, 1, 1, 0, 704, 99
49302, V, 1, 1, 1, 1, 0, 704, 99
49303, V, 1, 1, 1, 1, 0, 704, 99
49304, V, 1, 1, 1, 1, 0, 704, 99
49305, V, 1, 1, 1, 1, 0, 704, 99
49306, V, 1, 1, 1, 1, 0, 704, 99
49307, V, 1, 1, 1, 1, 0, 704, 99
49308, V, 1, 1, 1, 1, 0, 704, 99
49309, V, 1, 1, 1, 1, 0, 704, 99
49310, V, 1, 1, 1, 1, 0, 704, 99
49311, V, 1, 1, 1, 1, 0, 704, 99
49312, V, 1, 1, 1, 1, 0, 704, 99
49313, V, 1, 1, 1, 1, 0, 704, 99
49314, V, 1, 1, 1, 1, 0, 704, 99
49315, V, 1, 1, 1, 1, 0, 704, 99
49316, V, 1, 1, 1, 1, 0, 704, 99
49317, V, 1, 1, 1, 1, 0, 704, 99
49318, V, 1, 1, 1, 1, 0, 704, 99
49319, V, 1, 1, 1, 1, 0, 704, 99
49320, V, 1, 1, 1, 1, 0, 704, 99
49321, V, 1, 1, 1, 1, 0, 704, 99
49323, V, 1, 1, 1, 1, 0, 704, 99
49324, V, 1, 1, 1, 1, 0, 704, 99
49325, V, 1, 1, 1, 1, 0, 704, 99
49326, V, 1, 1, 1, 1, 0, 704, 99
49327, V, 1, 1, 1, 1, 0, 704, 99
49328, V, 1, 1, 1, 1, 0, 704, 99
49329, V, 1, 1, 1, 1, 0, 704, 99
49330, V, 1, 1, 1, 1, 0, 704, 99
49331, V, 1, 1, 1, 1, 0, 704, 99
49332, V, 1, 1, 1, 1, 0, 704, 99
49333, V, 1, 1, 1, 1, 0, 704, 99
49334, V, 1, 1, 1, 1, 0, 704, 99
49335, V, 1, 1, 1, 1, 0, 704, 99
49336, V, 1, 1, 1, 1, 0, 704, 99
49337, V, 1, 1, 1, 1, 0, 704, 99
49338, V, 1, 1, 1, 1, 0, 704, 99
49339, V, 1, 1, 1, 1, 0, 704, 99
49340, V, 1, 1, 1, 1, 0, 704, 99
49341, V, 1, 1, 1, 1, 0, 704, 99
49342, V, 1, 1, 1, 1, 0, 704, 99
49343, V, 1, 1, 1, 1, 0, 704, 99
49344, V, 1, 1, 1, 1, 0, 704, 99
49345, V, 1, 1, 1, 1, 0, 704, 99
49346, V, 1, 1, 1, 1, 0, 704, 99
49347, V, 1, 1, 1, 1, 0, 704, 99
49348, V, 1, 1, 1, 1, 0, 704, 99
49349, V, 1, 1, 1, 1, 0, 704, 99
49350, V, 1, 1, 1, 1, 0, 704, 99
49351, V, 1, 1, 1, 1, 0, 704, 99
49352, V, 1, 1, 1, 1, 0, 704, 99
49353, V, 1, 1, 1, 1, 0, 704, 99
49354, V, 1, 1, 1, 1, 0, 704, 99
49355, V, 1, 1, 1, 1, 0, 704, 99
49356, V, 1, 1, 1, 1, 0, 704, 99
49357, V, 1, 1, 1, 1, 0, 704, 99
49358, V, 1, 1, 1, 1, 0, 704, 99
49359, V, 1, 1, 1, 1, 0, 704, 99
49360, V, 1, 1, 1, 1, 0, 704, 99
49361, V, 1, 1, 1, 1, 0, 704, 99
49362, V, 1, 1, 1, 1, 0, 704, 99
49363, V, 1, 1, 1, 1, 0, 704, 99
49364, V, 1, 1, 1, 1, 0, 704, 99
49366, V, 1, 1, 1, 1, 0, 704, 99
49367, V, 1, 1, 1, 1, 0, 704, 99
49368, V, 1, 1, 1, 1, 0, 704, 99
49369, V, 1, 1, 1, 1, 0, 704, 99
49370, V, 1, 1, 1, 1, 0, 704, 99
49371, V, 1, 1, 1, 1, 0, 704, 99
49372, V, 1, 1, 1, 1, 0, 704, 99
49373, V, 1, 1, 1, 1, 0, 704, 99
49374, V, 1, 1, 1, 1, 0, 704, 99
49375, V, 1, 1, 1, 1, 0, 704, 99
49376, V, 1, 1, 1, 1, 0, 704, 99
49377, V, 1, 1, 1, 1, 0, 704, 99
49378, V, 1, 1, 1, 1, 0, 704, 99
49379, V, 1, 1, 1, 1, 0, 704, 99
49380, V, 1, 1, 1, 1, 0, 704, 99
49381, V, 1, 1, 1, 1, 0, 704, 99
49382, V, 1, 1, 1, 1, 0, 704, 99
49383, V, 1, 1, 1, 1, 0, 704, 99
49384, V, 1, 1, 1, 1, 0, 704, 99
49385, V, 1, 1, 1, 1, 0, 704, 99
49386, V, 1, 1, 1, 1, 0, 704, 99
49387, V, 1, 1, 1, 1, 0, 704, 99
49388, V, 1, 1, 1, 1, 0, 704, 99
49389, V, 1, 1, 1, 1, 0, 704, 99
49390, V, 1, 1, 1, 1, 0, 704, 99
49391, V, 1, 1, 1, 1, 0, 704, 99
49392, V, 1, 1, 1, 1, 0, 704, 99
49393, V, 1, 1, 1, 1, 0, 704, 99
49394, V, 1, 1, 1, 1, 0, 704, 99
49395, V, 1, 1, 1, 1, 0, 704, 99
49396, V, 1, 1, 1, 1, 0, 704, 99
49397, V, 1, 1, 1, 1, 0, 704, 99
49398, V, 1, 1, 1, 1, 0, 704, 99
49399, V, 1, 1, 1, 1, 0, 704, 99
49400, V, 1, 1, 1, 1, 0, 704, 99
49401, V, 1, 1, 1, 1, 0, 704, 99
49402, V, 1, 1, 1, 1, 0, 704, 99
49403, V, 1, 1, 1, 1, 0, 704, 99
49404, V, 1, 1, 1, 1, 0, 704, 99
49405, V, 1, 1, 1, 1, 0, 704, 99
49406, V, 1, 1, 1, 1, 0, 704, 99
49408, V, 1, 1, 1, 1, 0, 704, 99
49409, V, 1, 1, 1, 1, 0, 704, 99
49410, V, 1, 1, 1, 1, 0, 704, 99
49411, V, 1, 1, 1, 1, 0, 704, 99
49412, V, 1, 1, 1, 1, 0, 704, 99
49413, V, 1, 1, 1, 1, 0, 704, 99
49414, V, 1, 1, 1, 1, 0, 704, 99
49415, V, 1, 1, 1, 1, 0, 704, 99
49416, V, 1, 1, 1, 1, 0, 704, 99
49417, V, 1, 1, 1, 1, 0, 704, 99
49418, V, 1, 1, 1, 1, 0, 704, 99
49419, V, 1, 1, 1, 1, 0, 704, 99
49420, V, 1, 1, 1, 1, 0, 704, 99
49421, V, 1, 1, 1, 1, 0, 704, 99
49422, V, 1, 1, 1, 1, 0, 704, 99
49423, V, 1, 1, 1, 1, 0, 704, 99
49424, V, 1, 1, 1, 1, 0, 704, 99
49425, V, 1, 1, 1, 1, 0, 704, 99
49426, V, 1, 1, 1, 1, 0, 704, 99
49427, V, 1, 1, 1, 1, 0, 704, 99
49428, V, 1, 1, 1, 1, 0, 704, 99
49429, V, 1, 1, 1, 1, 0, 704, 99
49430, V, 1, 1, 1, 1, 0, 704, 99
49431, V, 1, 1, 1, 1, 0, 704, 99
49432, V, 1, 1, 1, 1, 0, 704, 99
49433, V, 1, 1, 1, 1, 0, 704, 99
49434, V, 1, 1, 1, 1, 0, 704, 99
49435, V, 1, 1, 1, 1, 0, 704, 99
49436, V, 1, 1, 1, 1, 0, 704, 99
49437, V, 1, 1, 1, 1, 0, 704, 99
49438, V, 1, 1, 1, 1, 0, 704, 99
49439, V, 1, 1, 1, 1, 0, 704, 99
49440, V, 1, 1, 1, 1, 0, 704, 99
49441, V, 1, 1, 1, 1, 0, 704, 99
49442, V, 1, 1, 1, 1, 0, 704, 99
49443, V, 1, 1, 1, 1, 0, 704, 99
49444, V, 1, 1, 1, 1, 0, 704, 99
49445, V, 1, 1, 1, 1, 0, 704, 99
49446, V, 1, 1, 1, 1, 0, 704, 99
49447, V, 1, 1, 1, 1, 0, 704, 99
49448, V, 1, 1, 1, 1, 0, 704, 99
49449, V, 1, 1, 1, 1, 0, 704, 99
49451, V, 1, 1, 1, 1, 0, 704, 99
49452, V, 1, 1, 1, 1, 0, 704, 99
49453, V, 1, 1, 1, 1, 0, 704, 99
49454, V, 1, 1, 1, 1, 0, 704, 99
49455, V, 1, 1, 1, 1, 0, 704, 99
49456, V, 1, 1, 1, 1, 0, 704, 99
49457, V, 1, 1, 1, 1, 0, 704, 99
49458, V, 1, 1, 1, 1, 0, 704, 99
49459, V, 1, 1, 1, 1, 0, 704, 99
49460, V, 1, 1, 1, 1, 0, 704, 99
49461, V, 1, 1, 1, 1, 0, 704, 99
49462, V, 1, 1, 1, 1, 0, 704, 99
49463, V, 1, 1, 1, 1, 0, 704, 99
49464, V, 1, 1, 1, 1, 0, 704, 99
49465, V, 1, 1, 1, 1, 0, 704, 99
49466, V, 1, 1, 1, 1, 0, 704, 99
49467, V, 1, 1, 1, 1, 0, 704, 99
49468, V, 1, 1, 1, 1, 0, 704, 99
49469, V, 1, 1, 1, 1, 0, 704, 99
49470, V, 1, 1, 1, 1, 0, 704, 99
49471, V, 1, 1, 1, 1, 0, 704, 99
49472, V, 1, 1, 1, 1, 0, 704, 99
49473, V, 1, 1, 1, 1, 0, 704, 99
49474, V, 1, 1, 1, 1, 0, 704, 99
49475, V, 1, 1, 1, 1, 0, 704, 99
49476, V, 1, 1, 1, 1, 0, 704, 99
49477, V, 1, 1, 1, 1, 0, 704, 99
49478, V, 1, 1, 1, 1, 0, 704, 99
49479, V, 1, 1, 1, 1, 0, 704, 99
49480, V, 1, 1, 1, 1, 0, 704, 99
49481, V, 1, 1, 1, 1, 0, 704, 99
49482, V, 1, 1, 1, 1, 0, 704, 99
49483, V, 1, 1, 1, 1, 0, 704, 99
49484, V, 1, 1, 1, 1, 0, 704, 99
49485, V, 1, 1, 1, 1, 0, 704, 99
49486, V, 1, 1, 1, 1, 0, 704, 99
49487, V, 1, 1, 1, 1, 0, 704, 99
49488, V, 1, 1, 1, 1, 0, 704, 99
49489, V, 1, 1, 1, 1, 0, 704, 99
49490, V, 1, 1, 1, 1, 0, 704, 99
49491, V, 1, 1, 1, 1, 0, 704, 99
49492, V, 1, 1, 1, 1, 0, 704, 99
49494, V, 1, 1, 1, 1, 0, 704, 99
49495, V, 1, 1, 1, 1, 0, 704, 99
49496, V, 1, 1, 1, 1, 0, 704, 99
49497, V, 1, 1, 1, 1, 0, 704, 99
49498, V, 1, 1, 1, 1, 0, 704, 99
49499, V, 1, 1, 1, 1, 0, 704, 99
49500, V, 1, 1, 1, 1, 0, 704, 99
49501, V, 1, 1, 1, 1, 0, 704, 99
49502, V, 1, 1, 1, 1, 0, 704, 99
49503, V, 1, 1, 1, 1, 0, 704, 99
49504, V, 1, 1, 1, 1, 0, 704, 99
49505, V, 1, 1, 1, 1, 0, 704, 99
49506, V, 1, 1, 1, 1, 0, 704, 99
49507, V, 1, 1, 1, 1, 0, 704, 99
49508, V, 1, 1, 1, 1, 0, 704, 99
49509, V, 1, 1, 1, 1, 0, 704, 99
49510, V, 1, 1, 1, 1, 0, 704, 99
49511, V, 1, 1, 1, 1, 0, 704, 99
49512, V, 1, 1, 1, 1, 0, 704, 99
49513, V, 1, 1, 1, 1, 0, 704, 99
49514, V, 1, 1, 1, 1, 0, 704, 99
49515, V, 1, 1, 1, 1, 0, 704, 99
49516, V, 1, 1, 1, 1, 0, 704, 99
49517, V, 1, 1, 1, 1, 0, 704, 99
49518, V, 1, 1, 1, 1, 0, 704, 99
49519, V, 1, 1, 1, 1, 0, 704, 99
49520, V, 1, 1, 1, 1, 0, 704, 99
49521, V, 1, 1, 1, 1, 0, 704, 99
49522, V, 1, 1, 1, 1, 0, 704, 99
49523, V, 1, 1, 1, 1, 0, 704, 99
49524, V, 1, 1, 1, 1, 0, 704, 99
49525, V, 1, 1, 1, 1, 0, 704, 99
49526, V, 1, 1, 1, 1, 0, 704, 99
49527, V, 1, 1, 1, 1, 0, 704, 99
49528, V, 1, 1, 1, 1, 0, 704, 99
49529, V, 1, 1, 1, 1, 0, 704, 99
49530, V, 1, 1, 1, 1, 0, 704, 99
49531, V, 1, 1, 1, 1, 0, 704, 99
49532, V, 1, 1, 1, 1, 0, 704, 99
49533, V, 1, 1, 1, 1, 0, 704, 99
49534, V, 1, 1, 1, 1, 0, 704, 99
49536, V, 1, 1, 1, 1, 0, 704, 99
49537, V, 1, 1, 1, 1, 0, 704, 99
49538, V, 1, 1, 1, 1, 0, 704, 99
49539, V, 1, 1, 1, 1, 0, 704, 99
49540, V, 1, 1, 1, 1, 0, 704, 99
49541, V, 1, 1, 1, 1, 0, 704, 99
49542, V, 1, 1, 1, 1, 0, 704, 99
49543, V, 1, 1, 1, 1, 0, 704, 99
49544, V, 1, 1, 1, 1, 0, 704, 100
49545, V, 1, 1, 1, 1, 0, 704, 99
49546, V, 1, 1, 1, 1, 0, 704, 99
49547, V, 1, 1, 1, 1, 0, 704, 99
49548, V, 1, 1, 1, 1, 0, 704, 99
49549, V, 1, 1, 1, 1, 0, 704, 99
49550, V, 1, 1, 1, 1, 0, 704, 99
49551, V, 1, 1, 1, 1, 0, 704, 99
49552, V, 1, 1, 1, 1, 0, 704, 99
49553, V, 1, 1, 1, 1, 0, 704, 99
49554, V, 1, 1, 1, 1, 0, 704, 99
49555, V, 1, 1, 1, 1, 0, 704, 99
49556, V, 1, 1, 1, 1, 0, 704, 100
49557, V, 1, 1, 1, 1, 0, 704, 99
49558, V, 1, 1, 1, 1, 0, 704, 100
49559, V, 1, 1, 1, 1, 0, 704, 100
49560, V, 1, 1, 1, 1, 0, 704, 100
49561, V, 1, 1, 1, 1, 0, 704, 100
49562, V, 1, 1, 1, 1, 0, 704, 100
49563, V, 1, 1, 1, 1, 0, 704, 100
49564, V, 1, 1, 1, 1, 0, 704, 100
49565, V, 1, 1, 1, 1, 0, 704, 100
49566, V, 1, 1, 1, 1, 0, 704, 100
49567, V, 1, 1, 1, 1, 0, 704, 100
49568, V, 1, 1, 1, 1, 0, 704, 100
49569, V, 1, 1, 1, 1, 0, 704, 100
49570, V, 1, 1, 1, 1, 0, 704, 100
49571, V, 1, 1, 1, 1, 0, 704, 100
49572, V, 1, 1, 1, 1, 0, 704, 100
49573, V, 1, 1, 1, 1, 0, 704, 100
49574, V, 1, 1, 1, 1, 0, 704, 100
49575, V, 1, 1, 1, 1, 0, 704, 100
49576, V, 1, 1, 1, 1, 0, 704, 100
49577, V, 1, 1, 1, 1, 0, 704, 100
49579, V, 1, 1, 1, 1, 0, 704, 100
49580, V, 1, 1, 1, 1, 0, 704, 100
49581, V, 1, 1, 1, 1, 0, 704, 100
49582, V, 1, 1, 1, 1, 0, 704, 100
49583, V, 1, 1, 1, 1, 0, 704, 100
49584, V, 1, 1, 1, 1, 0, 704, 100
49585, V, 1, 1, 1, 1, 0, 704, 100
49586, V, 1, 1, 1, 1, 0, 704, 100
49587, V, 1, 1, 1, 1, 0, 704, 100
49588, V, 1, 1, 1, 1, 0, 704, 100
49589, V, 1, 1, 1, 1, 0, 704, 100
49590, V, 1, 1, 1, 1, 0, 704, 100
49591, V, 1, 1, 1, 1, 0, 704, 100
49592, V, 1, 1, 1, 1, 0, 704, 100
49593, V, 1, 1, 1, 1, 0, 704, 100
49594, V, 1, 1, 1, 1, 0, 704, 100
49595, V, 1, 1, 1, 1, 0, 704, 100
49596, V, 1, 1, 1, 1, 0, 704, 100
49597, V, 1, 1, 1, 1, 0, 704, 100
49598, V, 1, 1, 1, 1, 0, 704, 100
49599, V, 1, 1, 1, 1, 0, 704, 100
49600, V, 1, 1, 1, 1, 0, 704, 100
49601, V, 1, 1, 1, 1, 0, 704, 100
49602, V, 1, 1, 1, 1, 0, 704, 100
49603, V, 1, 1, 1, 1, 0, 704, 100
49604, V, 1, 1, 1, 1, 0, 704, 100
49605, V, 1, 1, 1, 1, 0, 704, 100
49606, V, 1, 1, 1, 1, 0, 704, 100
49607, V, 1, 1, 1, 1, 0, 704, 100
49608, V, 1, 1, 1, 1, 0, 704, 100
49609, V, 1, 1, 1, 1, 0, 704, 100
49610, V, 1, 1, 1, 1, 0, 704, 100
49611, V, 1, 1, 1, 1, 0, 704, 100
49612, V, 1, 1, 1, 1, 0, 704, 100
49613, V, 1, 1, 1, 1, 0, 704, 100
49614, V, 1, 1, 1, 1, 0, 704, 100
49615, V, 1, 1, 1, 1, 0, 704, 100
49616, V, 1, 1, 1, 1, 0, 704, 100
49617, V, 1, 1, 1, 1, 0, 704, 100
49618, V, 1, 1, 1, 1, 0, 704, 100
49619, V, 1, 1, 1, 1, 0, 704, 100
49620, V, 1, 1, 1, 1, 0, 704, 100
49622, V, 1, 1, 1, 1, 0, 704, 100
49623, V, 1, 1, 1, 1, 0, 704, 100
49624, V, 1, 1, 1, 1, 0, 704, 100
49625, V, 1, 1, 1, 1, 0, 704, 100
49626, V, 1, 1, 1, 1, 0, 704, 100
49627, V, 1, 1, 1, 1, 0, 704, 100
49628, V, 1, 1, 1, 1, 0, 704, 100
49629, V, 1, 1, 1, 1, 0, 704, 100
49630, V, 1, 1, 1, 1, 0, 704, 100
49631, V, 1, 1, 1, 1, 0, 704, 100
49632, V, 1, 1, 1, 1, 0, 704, 100
49633, V, 1, 1, 1, 1, 0, 704, 100
49634, V, 1, 1, 1, 1, 0, 704, 100
49635, V, 1, 1, 1, 1, 0, 704, 100
49636, V, 1, 1, 1, 1, 0, 704, 100
49637, V, 1, 1, 1, 1, 0, 704, 100
49638, V, 1, 1, 1, 1, 0, 704, 100
49639, V, 1, 1, 1, 1, 0, 704, 100
49640, V, 1, 1, 1, 1, 0, 704, 100
49641, V, 1, 1, 1, 1, 0, 704, 100
49642, V, 1, 1, 1, 1, 0, 704, 100
49643, V, 1, 1, 1, 1, 0, 704, 100
49644, V, 1, 1, 1, 1, 0, 704, 100
49645, V, 1, 1, 1, 1, 0, 704, 100
49646, V, 1, 1, 1, 1, 0, 704, 100
49647, V, 1, 1, 1, 1, 0, 704, 100
49648, V, 1, 1, 1, 1, 0, 704, 100
49649, V, 1, 1, 1, 1, 0, 704, 100
49650, V, 1, 1, 1, 1, 0, 704, 100
49651, V, 1, 1, 1, 1, 0, 704, 100
49652, V, 1, 1, 1, 1, 0, 704, 100
49653, V, 1, 1, 1, 1, 0, 704, 100
49654, V, 1, 1, 1, 1, 0, 704, 100
49655, V, 1, 1, 1, 1, 0, 704, 100
49656, V, 0, 1, 0, 0, 0, 704, 100
49682, V, 0, 0, 0, 0, 0, 704, 97
49744, V, 0, 0, 0, 0, 0, 704, 64
49744, V, 0, 0, 0, 0, 0, 704, 64
50001, V, 0, 0, 0, 0, 0, 704, 51
50001, V, 0, 0, 0, 0, 0, 704, 51
50258, V, 0, 0, 0, 0, 0, 704, 51
50258, V, 0, 0, 0, 0, 0, 704, 51
50515, V, 0, 0, 0, 0, 0, 704, 51
50515, V, 0, 0, 0, 0, 0, 704, 51
50772, V, 0, 0, 0, 0, 0, 704, 51
50772, V, 0, 0, 0, 0, 0, 704, 51
51030, V, 0, 0, 0, 0, 0, 704, 51
51030, V, 0, 0, 0, 0, 0, 704, 51
51287, V, 0, 0, 0, 0, 0, 704, 51
51287, V, 0, 0, 0, 0, 0, 704, 51
51544, V, 0, 0, 0, 0, 0, 704, 51
51544, V, 0, 0, 0, 0, 0, 704, 51
51801, V, 0, 0, 0, 0, 0, 704, 51
51801, V, 0, 0, 0, 0, 0, 704, 51
52058, V, 0, 0, 0, 0, 0, 704, 52
52058, V, 0, 0, 0, 0, 0, 704, 52
52315, V, 0, 0, 0, 0, 0, 704, 52
52315, V, 0, 0, 0, 0, 0, 704, 52
52572, V, 0, 0, 0, 0, 0, 704, 51
52572, V, 0, 0, 0, 0, 0, 704, 51
52829, V, 0, 0, 0, 0, 0, 704, 51
52829, V, 0, 0, 0, 0, 0, 704, 51
53086, V, 0, 0, 0, 0, 0, 704, 51
53086, V, 0, 0, 0, 0, 0, 704, 51
53343, V, 0, 0, 0, 0, 0, 704, 52
53343, V, 0, 0, 0, 0, 0, 704, 52
53600, V, 0, 0, 0, 0, 0, 704, 52
53600, V, 0, 0, 0, 0, 0, 704, 52
53857, V, 0, 0, 0, 0, 0, 704, 52
53857, V, 0, 0, 0, 0, 0, 704, 52
54114, V, 0, 0, 0, 0, 0, 704, 52
54114, V, 0, 0, 0, 0, 0, 704, 52
54371, V, 0, 0, 0, 0, 0, 704, 52
54371, V, 0, 0, 0, 0, 0, 704, 52
54628, V, 0, 0, 0, 0, 0, 704, 52
54628, V, 0, 0, 0, 0, 0, 704, 52
54885, V, 0, 0, 0, 0, 0, 704, 52
54885, V, 0, 0, 0, 0, 0, 704, 52
55142, V, 0, 0, 0, 0, 0, 704, 52
55142, V, 0, 0, 0, 0, 0, 704, 52
55399, V, 0, 0, 0, 0, 0, 704, 52
55399, V, 0, 0, 0, 0, 0, 704, 52
55656, V, 0, 0, 0, 0, 0, 704, 52
55656, V, 0, 0, 0, 0, 0, 704, 52
55913, V, 0, 0, 0, 0, 0, 704, 52
55913, V, 0, 0, 0, 0, 0, 704, 52
56170, V, 0, 0, 0, 0, 0, 704, 52
56170, V, 0, 0, 0, 0, 0, 704, 52
56427, V, 0, 0, 0, 0, 0, 704, 52
56427, V, 0, 0, 0, 0, 0, 704, 52
56684, V, 0, 0, 0, 0, 0, 704, 52
56684, V, 0, 0, 0, 0, 0, 704, 52
56941, V, 0, 0, 0, 0, 0, 704, 52
56941, V, 0, 0, 0, 0, 0, 704, 52
57198, V, 0, 0, 0, 0, 0, 704, 52
57198, V, 0, 0, 0, 0, 0, 704, 52
57455, V, 0, 0, 0, 0, 0, 704, 52
57455, V, 0, 0, 0, 0, 0, 704, 52
57712, V, 0, 0, 0, 0, 0, 704, 52
57712, V, 0, 0, 0, 0, 0, 704, 52
57969, V, 0, 0, 0, 0, 0, 704, 52
57969, V, 0, 0, 0, 0, 0, 704, 52
58226, V, 0, 0, 0, 0, 0, 704, 52
58226, V, 0, 0, 0, 0, 0, 704, 52
58483, V, 0, 0, 0, 0, 0, 704, 52
58483, V, 0, 0, 0, 0, 0, 704, 52
58740, V, 0, 0, 0, 0, 0, 704, 52
58740, V, 0, 0, 0, 0, 0, 704, 52
58997, V, 0, 0, 0, 0, 0, 704, 52
58997, V, 0, 0, 0, 0, 0, 704, 52
59254, V, 0, 0, 0, 0, 0, 704, 52
59254, V, 0, 0, 0, 0, 0, 704, 52
59511, V, 0, 0, 0, 0, 0, 704, 52
59511, V, 0, 0, 0, 0, 0, 704, 52
59768, V, 0, 0, 0, 0, 0, 704, 52
59768, V, 0, 0, 0, 0, 0, 704, 52
60025, V, 0, 0, 0, 0, 0, 704, 52
60025, V, 0, 0, 0, 0, 0, 704, 52
60282, V, 0, 0, 0, 0, 0, 704, 52
60282, V, 0, 0, 0, 0, 0, 704, 52
60539, V, 0, 0, 0, 0, 0, 704, 52
60539, V, 0, 0, 0, 0, 0, 704, 52
60796, V, 0, 0, 0, 0, 0, 704, 51
60796, V, 0, 0, 0, 0, 0, 704, 51
61053, V, 0, 0, 0, 0, 0, 704, 51
61053, V, 0, 0, 0, 0, 0, 704, 51
61310, V, 0, 0, 0, 0, 0, 704, 51
61310, V, 0, 0, 0, 0, 0, 704, 51
61568, V, 0, 0, 0, 0, 0, 704, 51
61568, V, 0, 0, 0, 0, 0, 704, 51
61825, V, 0, 0, 0, 0, 0, 704, 51
61825, V, 0, 0, 0, 0, 0, 704, 51
62082, V, 0, 0, 0, 0, 0, 704, 51
62082, V, 0, 0, 0, 0, 0, 704, 51
62339, V, 0, 0, 0, 0, 0, 704, 51
62339, V, 0, 0, 0, 0, 0, 704, 51
62596, V, 0, 0, 0, 0, 0, 704, 52
62596, V, 0, 0, 0, 0, 0, 704, 52
62853, V, 0, 0, 0, 0, 0, 704, 52
62853, V, 0, 0, 0, 0, 0, 704, 52
63110, V, 0, 0, 0, 0, 0, 704, 52
63110, V, 0, 0, 0, 0, 0, 704, 52
63367, V, 0, 0, 0, 0, 0, 704, 52
63367, V, 0, 0, 0, 0, 0, 704, 52
63624, V, 0, 0, 0, 0, 0, 704, 52
63624, V, 0, 0, 0, 0, 0, 704, 52
63881, V, 0, 0, 0, 0, 0, 704, 52
63881, V, 0, 0, 0, 0, 0, 704, 52
64138, V, 0, 0, 0, 0, 0, 704, 52
64138, V, 0, 0, 0, 0, 0, 704, 52
64395, V, 0, 0, 0, 0, 0, 704, 52
64395, V, 0, 0, 0, 0, 0, 704, 52
64652, V, 0, 0, 0, 0, 0, 704, 52
64652, V, 0, 0, 0, 0, 0, 704, 52
64909, V, 0, 0, 0, 0, 0, 704, 52
64909, V, 0, 0, 0, 0, 0, 704, 52
65166, V, 0, 0, 0, 0, 0, 704, 52
65166, V, 0, 0, 0, 0, 0, 704, 52
65423, V, 0, 0, 0, 0, 0, 704, 52
65423, V, 0, 0, 0, 0, 0, 704, 52
144, V, 0, 0, 0, 0, 0, 704, 52
144, V, 0, 0, 0, 0, 0, 704, 52
401, V, 0, 0, 0, 0, 0, 704, 52
401, V, 0, 0, 0, 0, 0, 704, 52
658, V, 0, 0, 0, 0, 0, 704, 52
658, V, 0, 0, 0, 0, 0, 704, 52
915, V, 0, 0, 0, 0, 0, 704, 52
915, V, 0, 0, 0, 0, 0, 704, 52
1172, V, 0, 0, 0, 0, 0, 704, 52
1172, V, 0, 0, 0, 0, 0, 704, 52
1429, V, 0, 0, 0, 0, 0, 704, 52
1429, V, 0, 0, 0, 0, 0, 704, 52
1686, V, 0, 0, 0, 0, 0, 704, 52
1686, V, 0, 0, 0, 0, 0, 704, 52
1943, V, 0, 0, 0, 0, 0, 704, 52
1943, V, 0, 0, 0, 0, 0, 704, 52
2200, V, 0, 0, 0, 0, 0, 704, 52
2200, V, 0, 0, 0, 0, 0, 704, 52
2457, V, 0, 0, 0, 0, 0, 704, 52
2457, V, 0, 0, 0, 0, 0, 704, 52
2714, V, 0, 0, 0, 0, 0, 704, 52
2714, V, 0, 0, 0, 0, 0, 704, 52
2971, V, 0, 0, 0, 0, 0, 704, 52
2971, V, 0, 0, 0, 0, 0, 704, 52
3228, V, 0, 0, 0, 0, 0, 704, 52
3228, V, 0, 0, 0, 0, 0, 704, 52
3485, V, 0, 0, 0, 0, 0, 704, 52
3485, V, 0, 0, 0, 0, 0, 704, 52
3742, V, 0, 0, 0, 0, 0, 704, 52
3742, V, 0, 0, 0, 0, 0, 704, 52
3999, V, 0, 0, 0, 0, 0, 704, 52
3999, V, 0, 0, 0, 0, 0, 704, 52
4256, V, 0, 0, 0, 0, 0, 704, 52
4256, V, 0, 0, 0, 0, 0, 704, 52
4513, V, 0, 0, 0, 0, 0, 704, 52
4513, V, 0, 0, 0, 0, 0, 704, 52
4770, V, 0, 0, 0, 0, 0, 704, 52
4770, V, 0, 0, 0, 0, 0, 704, 52
5027, V, 0, 0, 0, 0, 0, 704, 52
5027, V, 0, 0, 0, 0, 0, 704, 52
5284, V, 0, 0, 0, 0, 0, 704, 52
5284, V, 0, 0, 0, 0, 0, 704, 52
5541, V, 0, 0, 0, 0, 0, 704, 52
5541, V, 0, 0, 0, 0, 0, 704, 52
5798, V, 0, 0, 0, 0, 0, 704, 52
5798, V, 0, 0, 0, 0, 0, 704, 52
6055, V, 0, 0, 0, 0, 0, 704, 52
6055, V, 0, 0, 0, 0, 0, 704, 52
6312, V, 0, 0, 0, 0, 0, 704, 52
6312, V, 0, 0, 0, 0, 0, 704, 52
6569, V, 0, 0, 0, 0, 0, 704, 52
6569, V, 0, 0, 0, 0, 0, 704, 52
6827, V, 0, 0, 0, 0, 0, 704, 52
6827, V, 0, 0, 0, 0, 0, 704, 52
7084, V, 0, 0, 0, 0, 0, 704, 52
7084, V, 0, 0, 0, 0, 0, 704, 52
7341, V, 0, 0, 0, 0, 0, 704, 52
7341, V, 0, 0, 0, 0, 0, 704, 52
7598, V, 0, 0, 0, 0, 0, 704, 52
7598, V, 0, 0, 0, 0, 0, 704, 52
7855, V, 0, 0, 0, 0, 0, 704, 52
7855, V, 0, 0, 0, 0, 0, 704, 52
8112, V, 0, 0, 0, 0, 0, 704, 52
8112, V, 0, 0, 0, 0, 0, 704, 52
8369, V, 0, 0, 0, 0, 0, 704, 52
8369, V, 0, 0, 0, 0, 0, 704, 52
8626, V, 0, 0, 0, 0, 0, 704, 52
8626, V, 0, 0, 0, 0, 0, 704, 52
8883, V, 0, 0, 0, 0, 0, 704, 52
8883, V, 0, 0, 0, 0, 0, 704, 52
9140, V, 0, 0, 0, 0, 0, 704, 52
9140, V, 0, 0, 0, 0, 0, 704, 52
9397, V, 0, 0, 0, 0, 0, 704, 52
9397, V, 0, 0, 0, 0, 0, 704, 52
9654, V, 0, 0, 0, 0, 0, 704, 52
9654, V, 0, 0, 0, 0, 0, 704, 52
9911, V, 0, 0, 0, 0, 0, 704, 52
9911, V, 0, 0, 0, 0, 0, 704, 52
10168, V, 0, 0, 0, 0, 0, 704, 52
10168, V, 0, 0, 0, 0, 0, 704, 52
10425, V, 0, 0, 0, 0, 0, 704, 52
10425, V, 0, 0, 0, 0, 0, 704, 52
10682, V, 0, 0, 0, 0, 0, 704, 52
10682, V, 0, 0, 0, 0, 0, 704, 52
10939, V, 0, 0, 0, 0, 0, 704, 52
10939, V, 0, 0, 0, 0, 0, 704, 52
11196, V, 0, 0, 0, 0, 0, 704, 52
11196, V, 0, 0, 0, 0, 0, 704, 52
11453, V, 0, 0, 0, 0, 0, 704, 52
11453, V, 0, 0, 0, 0, 0, 704, 52
11710, V, 0, 0, 0, 0, 0, 704, 52
11710, V, 0, 0, 0, 0, 0, 704, 52
11967, V, 0, 0, 0, 0, 0, 704, 52
11967, V, 0, 0, 0, 0, 0, 704, 52
12224, V, 0, 0, 0, 0, 0, 704, 52
12224, V, 0, 0, 0, 0, 0, 704, 52
12481, V, 0, 0, 0, 0, 0, 704, 52
12481, V, 0, 0, 0, 0, 0, 704, 52
12738, V, 0, 0, 0, 0, 0, 704, 52
12738, V, 0, 0, 0, 0, 0, 704, 52
12995, V, 0, 0, 0, 0, 0, 704, 52
12995, V, 0, 0, 0, 0, 0, 704, 52
13252, V, 0, 0, 0, 0, 0, 704, 52
13252, V, 0, 0, 0, 0, 0, 704, 52
13509, V, 0, 0, 0, 0, 0, 704, 52
13509, V, 0, 0, 0, 0, 0, 704, 52
13766, V, 0, 0, 0, 0, 0, 704, 52
13766, V, 0, 0, 0, 0, 0, 704, 52
14023, V, 0, 0, 0, 0, 0, 704, 52
14023, V, 0, 0, 0, 0, 0, 704, 52
14326, V, 0, 0, 0, 0, 0, 704, 52
14326, V, 0, 0, 0, 0, 0, 704, 52
14583, V, 0, 0, 0, 0, 0, 704, 52
14583, V, 0, 0, 0, 0, 0, 704, 52
14840, V, 0, 0, 0, 0, 0, 704, 52
14840, V, 0, 0, 0, 0, 0, 704, 52
15097, V, 0, 0, 0, 0, 0, 704, 52
15097, V, 0, 0, 0, 0, 0, 704, 52
15354, V, 0, 0, 0, 0, 0, 704, 52
15354, V, 0, 0, 0, 0, 0, 704, 52
15611, V, 0, 0, 0, 0, 0, 704, 52
15611, V, 0, 0, 0, 0, 0, 704, 52
15868, V, 0, 0, 0, 0, 0, 704, 52
15868, V, 0, 0, 0, 0, 0, 704, 52
16125, V, 0, 0, 0, 0, 0, 704, 52
16125, V, 0, 0, 0, 0, 0, 704, 52
16382, V, 0, 0, 0, 0, 0, 704, 52
16382, V, 0, 0, 0, 0, 0, 704, 52
16640, V, 0, 0, 0, 0, 0, 704, 52
16640, V, 0, 0, 0, 0, 0, 704, 52
16897, V, 0, 0, 0, 0, 0, 704, 52
16897, V, 0, 0, 0, 0, 0, 704, 52
17154, V, 0, 0, 0, 0, 0, 704, 52
17154, V, 0, 0, 0, 0, 0, 704, 52
17411, V, 0, 0, 0, 0, 0, 704, 52
17411, V, 0, 0, 0, 0, 0, 704, 52
17668, V, 0, 0, 0, 0, 0, 704, 52
17668, V, 0, 0, 0, 0, 0, 704, 52
17925, V, 0, 0, 0, 0, 0, 704, 52
17925, V, 0, 0, 0, 0, 0, 704, 52
18182, V, 0, 0, 0, 0, 0, 704, 52
18182, V, 0, 0, 0, 0, 0, 704, 52
18439, V, 0, 0, 0, 0, 0, 704, 52
18439, V, 0, 0, 0, 0, 0, 704, 52
18696, V, 0, 0, 0, 0, 0, 704, 52
18696, V, 0, 0, 0, 0, 0, 704, 52
18953, V, 0, 0, 0, 0, 0, 704, 52
18953, V, 0, 0, 0, 0, 0, 704, 52
19210, V, 0, 0, 0, 0, 0, 704, 52
19210, V, 0, 0, 0, 0, 0, 704, 52
19467, V, 0, 0, 0, 0, 0, 704, 52
19467, V, 0, 0, 0, 0, 0, 704, 52
19724, V, 0, 0, 0, 0, 0, 704, 52
19724, V, 0, 0, 0, 0, 0, 704, 52
19981, V, 0, 0, 0, 0, 0, 704, 52
19981, V, 0, 0, 0, 0, 0, 704, 52
20238, V, 0, 0, 0, 0, 0, 704, 52
20238, V, 0, 0, 0, 0, 0, 704, 52
20495, V, 0, 0, 0, 0, 0, 704, 52
20495, V, 0, 0, 0, 0, 0, 704, 52
20752, V, 0, 0, 0, 0, 0, 704, 52
20752, V, 0, 0, 0, 0, 0, 704, 52
21009, V, 0, 0, 0, 0, 0, 704, 52
21009, V, 0, 0, 0, 0, 0, 704, 52
21266, V, 0, 0, 0, 0, 0, 704, 52
21266, V, 0, 0, 0, 0, 0, 704, 52
21523, V, 0, 0, 0, 0, 0, 704, 52
21523, V, 0, 0, 0, 0, 0, 704, 52
21780, V, 0, 0, 0, 0, 0, 704, 52
21780, V, 0, 0, 0, 0, 0, 704, 52
22037, V, 0, 0, 0, 0, 0, 704, 52
22037, V, 0, 0, 0, 0, 0, 704, 52
22294, V, 0, 0, 0, 0, 0, 704, 52
22294, V, 0, 0, 0, 0, 0, 704, 52
22551, V, 0, 0, 0, 0, 0, 704, 52
22551, V, 0, 0, 0, 0, 0, 704, 52
22808, V, 0, 0, 0, 0, 0, 704, 52
22808, V, 0, 0, 0, 0, 0, 704, 52
23065, V, 0, 0, 0, 0, 0, 704, 52
23065, V, 0, 0, 0, 0, 0, 704, 52
23322, V, 0, 0, 0, 0, 0, 704, 52
23322, V, 0, 0, 0, 0, 0, 704, 52
23579, V, 0, 0, 0, 0, 0, 704, 52
23579, V, 0, 0, 0, 0, 0, 704, 52
23836, V, 0, 0, 0, 0, 0, 704, 52
23836, V, 0, 0, 0, 0, 0, 704, 52
24093, V, 0, 0, 0, 0, 0, 704, 52
24093, V, 0, 0, 0, 0, 0, 704, 52
24350, V, 0, 0, 0, 0, 0, 704, 52
24350, V, 0, 0, 0, 0, 0, 704, 52
24607, V, 0, 0, 0, 0, 0, 704, 52
24607, V, 0, 0, 0, 0, 0, 704, 52
24864, V, 0, 0, 0, 0, 0, 704, 52
24864, V, 0, 0, 0, 0, 0, 704, 52
25121, V, 0, 0, 0, 0, 0, 704, 52
25121, V, 0, 0, 0, 0, 0, 704, 52
25378, V, 0, 0, 0, 0, 0, 704, 52
25378, V, 0, 0, 0, 0, 0, 704, 52
25635, V, 0, 0, 0, 0, 0, 704, 52
25635, V, 0, 0, 0, 0, 0, 704, 52
25892, V, 0, 0, 0, 0, 0, 704, 52
25892, V, 0, 0, 0, 0, 0, 704, 52
26149, V, 0, 0, 0, 0, 0, 704, 52
26149, V, 0, 0, 0, 0, 0, 704, 52
26406, V, 0, 0, 0, 0, 0, 704, 52
26406, V, 0, 0, 0, 0, 0, 704, 52
26663, V, 0, 0, 0, 0, 0, 704, 52
26663, V, 0, 0, 0, 0, 0, 704, 52
26920, V, 0, 0, 0, 0, 0, 704, 52
26920, V, 0, 0, 0, 0, 0, 704, 52
27177, V, 0, 0, 0, 0, 0, 704, 52
27177, V, 0, 0, 0, 0, 0, 704, 52
27435, V, 0, 0, 0, 0, 0, 704, 52
27435, V, 0, 0, 0, 0, 0, 704, 52
27692, V, 0, 0, 0, 0, 0, 704, 52
27692, V, 0, 0, 0, 0, 0, 704, 52
27949, V, 0, 0, 0, 0, 0, 704, 52
27949, V, 0, 0, 0, 0, 0, 704, 52
28206, V, 0, 0, 0, 0, 0, 704, 52
28206, V, 0, 0, 0, 0, 0, 704, 52
28463, V, 0, 0, 0, 0, 0, 704, 52
28463, V, 0, 0, 0, 0, 0, 704, 52
28720, V, 0, 0, 0, 0, 0, 704, 52
28720, V, 0, 0, 0, 0, 0, 704, 52
28977, V, 0, 0, 0, 0, 0, 704, 52
28977, V, 0, 0, 0, 0, 0, 704, 52
29234, V, 0, 0, 0, 0, 0, 704, 52
29234, V, 0, 0, 0, 0, 0, 704, 52
29491, V, 0, 0, 0, 0, 0, 704, 52
29491, V, 0, 0, 0, 0, 0, 704, 52
29748, V, 0, 0, 0, 0, 0, 704, 52
29748, V, 0, 0, 0, 0, 0, 704, 52
30005, V, 0, 0, 0, 0, 0, 704, 52
30005, V, 0, 0, 0, 0, 0, 704, 52
30262, V, 0, 0, 0, 0, 0, 704, 52
30262, V, 0, 0, 0, 0, 0, 704, 52
30519, V, 0, 0, 0, 0, 0, 704, 52
30519, V, 0, 0, 0, 0, 0, 704, 52
30776, V, 0, 0, 0, 0, 0, 704, 52
30776, V, 0, 0, 0, 0, 0, 704, 52
31033, V, 0, 0, 0, 0, 0, 704, 52
31033, V, 0, 0, 0, 0, 0, 704, 52
31290, V, 0, 0, 0, 0, 0, 704, 52
31290, V, 0, 0, 0, 0, 0, 704, 52
31547, V, 0, 0, 0, 0, 0, 704, 52
31547, V, 0, 0, 0, 0, 0, 704, 52
31804, V, 0, 0, 0, 0, 0, 704, 52
31804, V, 0, 0, 0, 0, 0, 704, 52
32061, V, 0, 0, 0, 0, 0, 704, 52
32061, V, 0, 0, 0, 0, 0, 704, 52
32318, V, 0, 0, 0, 0, 0, 704, 52
32318, V, 0, 0, 0, 0, 0, 704, 52
32575, V, 0, 0, 0, 0, 0, 704, 52
32575, V, 0, 0, 0, 0, 0, 704, 52
32832, V, 0, 0, 0, 0, 0, 704, 52
32832, V, 0, 0, 0, 0, 0, 704, 52
33089, V, 0, 0, 0, 0, 0, 704, 52
33089, V, 0, 0, 0, 0, 0, 704, 52
33346, V, 0, 0, 0, 0, 0, 704, 52
33346, V, 0, 0, 0, 0, 0, 704, 52
33603, V, 0, 0, 0, 0, 0, 704, 52
33603, V, 0, 0, 0, 0, 0, 704, 52
33860, V, 0, 0, 0, 0, 0, 704, 52
33860, V, 0, 0, 0, 0, 0, 704, 52
34117, V, 0, 0, 0, 0, 0, 704, 52
34117, V, 0, 0, 0, 0, 0, 704, 52
34374, V, 0, 0, 0, 0, 0, 704, 52
34374, V, 0, 0, 0, 0, 0, 704, 52
34631, V, 0, 0, 0, 0, 0, 704, 52
34631, V, 0, 0, 0, 0, 0, 704, 52
34888, V, 0, 0, 0, 0, 0, 704, 52
34888, V, 0, 0, 0, 0, 0, 704, 52
35145, V, 0, 0, 0, 0, 0, 704, 52
35145, V, 0, 0, 0, 0, 0, 704, 52
35402, V, 0, 0, 0, 0, 0, 704, 52
35402, V, 0, 0, 0, 0, 0, 704, 52
35659, V, 0, 0, 0, 0, 0, 704, 52
35659, V, 0, 0, 0, 0, 0, 704, 52
35916, V, 0, 0, 0, 0, 0, 704, 52
35916, V, 0, 0, 0, 0, 0, 704, 52
36173, V, 0, 0, 0, 0, 0, 704, 52
36173, V, 0, 0, 0, 0, 0, 704, 52
36430, V, 0, 0, 0, 0, 0, 704, 52
36430, V, 0, 0, 0, 0, 0, 704, 52
36687, V, 0, 0, 0, 0, 0, 704, 52
36687, V, 0, 0, 0, 0, 0, 704, 52
36944, V, 0, 0, 0, 0, 0, 704, 52
36944, V, 0, 0, 0, 0, 0, 704, 52
37201, V, 0, 0, 0, 0, 0, 704, 52
37201, V, 0, 0, 0, 0, 0, 704, 52
37458, V, 0, 0, 0, 0, 0, 704, 52
37458, V, 0, 0, 0, 0, 0, 704, 52
37715, V, 0, 0, 0, 0, 0, 704, 52
37715, V, 0, 0, 0, 0, 0, 704, 52
37972, V, 0, 0, 0, 0, 0, 704, 52
37972, V, 0, 0, 0, 0, 0, 704, 52
38230, V, 0, 0, 0, 0, 0, 704, 52
38230, V, 0, 0, 0, 0, 0, 704, 52
38487, V, 0, 0, 0, 0, 0, 704, 52
38487, V, 0, 0, 0, 0, 0, 704, 52
38744, V, 0, 0, 0, 0, 0, 704, 52
38744, V, 0, 0, 0, 0, 0, 704, 52
39001, V, 0, 0, 0, 0, 0, 704, 52
39001, V, 0, 0, 0, 0, 0, 704, 52
39258, V, 0, 0, 0, 0, 0, 704, 52
39258, V, 0, 0, 0, 0, 0, 704, 52
39515, V, 0, 0, 0, 0, 0, 704, 52
39515, V, 0, 0, 0, 0, 0, 704, 52
39772, V, 0, 0, 0, 0, 0, 704, 52
39772, V, 0, 0, 0, 0, 0, 704, 52
40029, V, 0, 0, 0, 0, 0, 704, 52
40029, V, 0, 0, 0, 0, 0, 704, 52
40286, V, 0, 0, 0, 0, 0, 704, 52
40286, V, 0, 0, 0, 0, 0, 704, 52
40543, V, 0, 0, 0, 0, 0, 704, 52
40543, V, 0, 0, 0, 0, 0, 704, 52
40800, V, 0, 0, 0, 0, 0, 704, 52
40800, V, 0, 0, 0, 0, 0, 704, 52
41057, V, 0, 0, 0, 0, 0, 704, 52
41057, V, 0, 0, 0, 0, 0, 704, 52
41314, V, 0, 0, 0, 0, 0, 704, 52
41314, V, 0, 0, 0, 0, 0, 704, 52
41571, V, 0, 0, 0, 0, 0, 704, 52
41571, V, 0, 0, 0, 0, 0, 704, 52
41828, V, 0, 0, 0, 0, 0, 704, 52
41828, V, 0, 0, 0, 0, 0, 704, 52
42085, V, 0, 0, 0, 0, 0, 704, 52
42085, V, 0, 0, 0, 0, 0, 704, 52
42342, V, 0, 0, 0, 0, 0, 704, 52
42342, V, 0, 0, 0, 0, 0, 704, 52
42599, V, 0, 0, 0, 0, 0, 704, 52
42599, V, 0, 0, 0, 0, 0, 704, 52
42856, V, 0, 0, 0, 0, 0, 704, 52
42856, V, 0, 0, 0, 0, 0, 704, 52
43113, V, 0, 0, 0, 0, 0, 704, 52
43113, V, 0, 0, 0, 0, 0, 704, 52
43370, V, 0, 0, 0, 0, 0, 704, 52
43370, V, 0, 0, 0, 0, 0, 704, 52
43627, V, 0, 0, 0, 0, 0, 704, 52
43627, V, 0, 0, 0, 0, 0, 704, 52
43884, V, 0, 0, 0, 0, 0, 704, 52
43884, V, 0, 0, 0, 0, 0, 704, 52
44141, V, 0, 0, 0, 0, 0, 704, 52
44141, V, 0, 0, 0, 0, 0, 704, 52
44398, V, 0, 0, 0, 0, 0, 704, 52
44398, V, 0, 0, 0, 0, 0, 704, 52
44655, V, 0, 0, 0, 0, 0, 704, 52
44655, V, 0, 0, 0, 0, 0, 704, 52
44912, V, 0, 0, 0, 0, 0, 704, 52
44912, V, 0, 0, 0, 0, 0, 704, 52
45169, V, 0, 0, 0, 0, 0, 704, 52
45169, V, 0, 0, 0, 0, 0, 704, 52
45426, V, 0, 0, 0, 0, 0, 704, 52
45426, V, 0, 0, 0, 0, 0, 704, 52
45683, V, 0, 0, 0, 0, 0, 704, 52
45683, V, 0, 0, 0, 0, 0, 704, 52
45940, V, 0, 0, 0, 0, 0, 704, 52
45940, V, 0, 0, 0, 0, 0, 704, 52
46197, V, 0, 0, 0, 0, 0, 704, 52
46197, V, 0, 0, 0, 0, 0, 704, 52
46454, V, 0, 0, 0, 0, 0, 704, 52
46454, V, 0, 0, 0, 0, 0, 704, 52
46711, V, 0, 0, 0, 0, 0, 704, 52
46711, V, 0, 0, 0, 0, 0, 704, 52
46968, V, 0, 0, 0, 0, 0, 704, 52
46968, V, 0, 0, 0, 0, 0, 704, 52
47225, V, 0, 0, 0, 0, 0, 704, 52
47225, V, 0, 0, 0, 0, 0, 704, 52
47482, V, 0, 0, 0, 0, 0, 704, 52
47482, V, 0, 0, 0, 0, 0, 704, 52
47739, V, 0, 0, 0, 0, 0, 704, 52
47739, V, 0, 0, 0, 0, 0, 704, 52
47996, V, 0, 0, 0, 0, 0, 704, 52
47996, V, 0, 0, 0, 0, 0, 704, 52
48253, V, 0, 0, 0, 0, 0, 704, 52
48253, V, 0, 0, 0, 0, 0, 704, 52
48510, V, 0, 0, 0, 0, 0, 704, 52
48510, V, 0, 0, 0, 0, 0, 704, 52
48768, V, 0, 0, 0, 0, 0, 704, 52
48768, V, 0, 0, 0, 0, 0, 704, 52
49025, V, 0, 0, 0, 0, 0, 704, 52
49025, V, 0, 0, 0, 0, 0, 704, 52
49282, V, 0, 0, 0, 0, 0, 704, 52
49282, V, 0, 0, 0, 0, 0, 704, 52
49539, V, 0, 0, 0, 0, 0, 704, 52
49539, V, 0, 0, 0, 0, 0, 704, 52
49796, V, 0, 0, 0, 0, 0, 704, 52
49796, V, 0, 0, 0, 0, 0, 704, 52
50053, V, 0, 0, 0, 0, 0, 704, 52
50053, V, 0, 0, 0, 0, 0, 704, 52
50310, V, 0, 0, 0, 0, 0, 704, 52
50310, V, 0, 0, 0, 0, 0, 704, 52
50567, V, 0, 0, 0, 0, 0, 704, 52
50567, V, 0, 0, 0, 0, 0, 704, 52
50824, V, 0, 0, 0, 0, 0, 704, 52
50824, V, 0, 0, 0, 0, 0, 704, 52
51081, V, 0, 0, 0, 0, 0, 704, 52
51081, V, 0, 0, 0, 0, 0, 704, 52
51338, V, 0, 0, 0, 0, 0, 704, 52
51338, V, 0, 0, 0, 0, 0, 704, 52
51595, V, 0, 0, 0, 0, 0, 704, 52
51595, V, 0, 0, 0, 0, 0, 704, 52
51852, V, 0, 0, 0, 0, 0, 704, 52
51852, V, 0, 0, 0, 0, 0, 704, 52
52109, V, 0, 0, 0, 0, 0, 704, 52
52109, V, 0, 0, 0, 0, 0, 704, 52
52366, V, 0, 0, 0, 0, 0, 704, 52
52366, V, 0, 0, 0, 0, 0, 704, 52
52623, V, 0, 0, 0, 0, 0, 704, 52
52623, V, 0, 0, 0, 0, 0, 704, 52
52880, V, 0, 0, 0, 0, 0, 704, 52
52880, V, 0, 0, 0, 0, 0, 704, 52
53137, V, 0, 0, 0, 0, 0, 704, 52
53137, V, 0, 0, 0, 0, 0, 704, 52
53394, V, 0, 0, 0, 0, 0, 704, 52
53394, V, 0, 0, 0, 0, 0, 704, 52
53651, V, 0, 0, 0, 0, 0, 704, 52
53651, V, 0, 0, 0, 0, 0, 704, 52
53908, V, 0, 0, 0, 0, 0, 704, 52
53908, V, 0, 0, 0, 0, 0, 704, 52
54165, V, 0, 0, 0, 0, 0, 704, 52
54165, V, 0, 0, 0, 0, 0, 704, 52
54422, V, 0, 0, 0, 0, 0, 704, 52
54422, V, 0, 0, 0, 0, 0, 704, 52
54679, V, 0, 0, 0, 0, 0, 704, 52
54679, V, 0, 0, 0, 0, 0, 704, 52
54936, V, 0, 0, 0, 0, 0, 704, 52
54936, V, 0, 0, 0, 0, 0, 704, 52
55193, V, 0, 0, 0, 0, 0, 704, 52
55193, V, 0, 0, 0, 0, 0, 704, 52
55450, V, 0, 0, 0, 0, 0, 704, 52
55450, V, 0, 0, 0, 0, 0, 704, 52
55707, V, 0, 0, 0, 0, 0, 704, 52
55707, V, 0, 0, 0, 0, 0, 704, 52
55964, V, 0, 0, 0, 0, 0, 704, 52
55964, V, 0, 0, 0, 0, 0, 704, 52
56221, V, 0, 0, 0, 0, 0, 704, 52
56221, V, 0, 0, 0, 0, 0, 704, 52
56478, V, 0, 0, 0, 0, 0, 704, 52
56478, V, 0, 0, 0, 0, 0, 704, 52
56735, V, 0, 0, 0, 0, 0, 704, 52
56735, V, 0, 0, 0, 0, 0, 704, 52
56992, V, 0, 0, 0, 0, 0, 704, 52
56992, V, 0, 0, 0, 0, 0, 704, 52
57249, V, 0, 0, 0, 0, 0, 704, 52
57249, V, 0, 0, 0, 0, 0, 704, 52
57506, V, 0, 0, 0, 0, 0, 704, 52
57506, V, 0, 0, 0, 0, 0, 704, 52
57763, V, 0, 0, 0, 0, 0, 704, 52
57763, V, 0, 0, 0, 0, 0, 704, 52
58020, V, 0, 0, 0, 0, 0, 704, 52
58020, V, 0, 0, 0, 0, 0, 704, 52
58277, V, 0, 0, 0, 0, 0, 704, 52
58277, V, 0, 0, 0, 0, 0, 704, 52
58534, V, 0, 0, 0, 0, 0, 704, 52
58534, V, 0, 0, 0, 0, 0, 704, 52
58791, V, 0, 0, 0, 0, 0, 704, 52
58791, V, 0, 0, 0, 0, 0, 704, 52
59048, V, 0, 0, 0, 0, 0, 704, 52
59048, V, 0, 0, 0, 0, 0, 704, 52
59305, V, 0, 0, 0, 0, 0, 704, 52
59305, V, 0, 0, 0, 0, 0, 704, 52
59563, V, 0, 0, 0, 0, 0, 704, 52
59563, V, 0, 0, 0, 0, 0, 704, 52
59820, V, 0, 0, 0, 0, 0, 704, 52
59820, V, 0, 0, 0, 0, 0, 704, 52
60077, V, 0, 0, 0, 0, 0, 704, 52
60077, V, 0, 0, 0, 0, 0, 704, 52
60334, V, 0, 0, 0, 0, 0, 704, 52
60334, V, 0, 0, 0, 0, 0, 704, 52
60591, V, 0, 0, 0, 0, 0, 704, 52
60591, V, 0, 0, 0, 0, 0, 704, 52
60848, V, 0, 0, 0, 0, 0, 704, 52
60848, V, 0, 0, 0, 0, 0, 704, 52
61105, V, 0, 0, 0, 0, 0, 704, 52
61105, V, 0, 0, 0, 0, 0, 704, 52
61362, V, 0, 0, 0, 0, 0, 704, 52
61362, V, 0, 0, 0, 0, 0, 704, 52
61619, V, 0, 0, 0, 0, 0, 704, 52
61619, V, 0, 0, 0, 0, 0, 704, 52
61876, V, 0, 0, 0, 0, 0, 704, 52
61876, V, 0, 0, 0, 0, 0, 704, 52
62133, V, 0, 0, 0, 0, 0, 704, 52
62133, V, 0, 0, 0, 0, 0, 704, 52
62390, V, 0, 0, 0, 0, 0, 704, 52
62390, V, 0, 0, 0, 0, 0, 704, 52
62647, V, 0, 0, 0, 0, 0, 704, 52
62647, V, 0, 0, 0, 0, 0, 704, 52
62904, V, 0, 0, 0, 0, 0, 704, 52
62904, V, 0, 0, 0, 0, 0, 704, 52
63161, V, 0, 0, 0, 0, 0, 704, 52
63161, V, 0, 0, 0, 0, 0, 704, 52
63418, V, 0, 0, 0, 0, 0, 704, 52
63418, V, 0, 0, 0, 0, 0, 704, 52
63675, V, 0, 0, 0, 0, 0, 704, 52
63675, V, 0, 0, 0, 0, 0, 704, 52
63932, V, 0, 0, 0, 0, 0, 704, 52
63932, V, 0, 0, 0, 0, 0, 704, 52
64189, V, 0, 0, 0, 0, 0, 704, 52
64189, V, 0, 0, 0, 0, 0, 704, 52
64446, V, 0, 0, 0, 0, 0, 704, 52
64446, V, 0, 0, 0, 0, 0, 704, 52
64703, V, 0, 0, 0, 0, 0, 704, 52
64703, V, 0, 0, 0, 0, 0, 704, 52
64960, V, 0, 0, 0, 0, 0, 704, 52
64960, V, 0, 0, 0, 0, 0, 704, 52
65217, V, 0, 0, 0, 0, 0, 704, 52
65217, V, 0, 0, 0, 0, 0, 704, 52
65474, V, 0, 0, 0, 0, 0, 704, 52
65474, V, 0, 0, 0, 0, 0, 704, 52
195, V, 0, 0, 0, 0, 0, 704, 52
195, V, 0, 0, 0, 0, 0, 704, 52
452, V, 0, 0, 0, 0, 0, 704, 52
452, V, 0, 0, 0, 0, 0, 704, 52
709, V, 0, 0, 0, 0, 0, 704, 52
709, V, 0, 0, 0, 0, 0, 704, 52
966, V, 0, 0, 0, 0, 0, 704, 52
966, V, 0, 0, 0, 0, 0, 704, 52
1223, V, 0, 0, 0, 0, 0, 704, 52
1223, V, 0, 0, 0, 0, 0, 704, 52
1480, V, 0, 0, 0, 0, 0, 704, 52
1480, V, 0, 0, 0, 0, 0, 704, 52
1737, V, 0, 0, 0, 0, 0, 704, 52
1737, V, 0, 0, 0, 0, 0, 704, 52
1994, V, 0, 0, 0, 0, 0, 704, 52
1994, V, 0, 0, 0, 0, 0, 704, 52
2251, V, 0, 0, 0, 0, 0, 704, 52
2251, V, 0, 0, 0, 0, 0, 704, 52
2508, V, 0, 0, 0, 0, 0, 704, 52
2508, V, 0, 0, 0, 0, 0, 704, 52
2765, V, 0, 0, 0, 0, 0, 704, 52
2765, V, 0, 0, 0, 0, 0, 704, 52
3022, V, 0, 0, 0, 0, 0, 704, 52
3022, V, 0, 0, 0, 0, 0, 704, 52
3279, V, 0, 0, 0, 0, 0, 704, 52
3279, V, 0, 0, 0, 0, 0, 704, 52
3536, V, 0, 0, 0, 0, 0, 704, 52
3536, V, 0, 0, 0, 0, 0, 704, 52
3793, V, 0, 0, 0, 0, 0, 704, 52
3793, V, 0, 0, 0, 0, 0, 704, 52
4050, V, 0, 0, 0, 0, 0, 704, 52
4050, V, 0, 0, 0, 0, 0, 704, 52
4307, V, 0, 0, 0, 0, 0, 704, 52
4307, V, 0, 0, 0, 0, 0, 704, 52
4564, V, 0, 0, 0, 0, 0, 704, 52
4564, V, 0, 0, 0, 0, 0, 704, 52
4822, V, 0, 0, 0, 0, 0, 704, 52
4822, V, 0, 0, 0, 0, 0, 704, 52
5079, V, 0, 0, 0, 0, 0, 704, 52
5079, V, 0, 0, 0, 0, 0, 704, 52
5336, V, 0, 0, 0, 0, 0, 704, 52
5336, V, 0, 0, 0, 0, 0, 704, 52
5593, V, 0, 0, 0, 0, 0, 704, 52
5593, V, 0, 0, 0, 0, 0, 704, 52
5850, V, 0, 0, 0, 0, 0, 704, 52
5850, V, 0, 0, 0, 0, 0, 704, 52
6107, V, 0, 0, 0, 0, 0, 704, 52
6107, V, 0, 0, 0, 0, 0, 704, 52
6364, V, 0, 0, 0, 0, 0, 704, 52
6364, V, 0, 0, 0, 0, 0, 704, 52
6621, V, 0, 0, 0, 0, 0, 704, 52
6621, V, 0, 0, 0, 0, 0, 704, 52
6878, V, 0, 0, 0, 0, 0, 704, 52
6878, V, 0, 0, 0, 0, 0, 704, 52
7135, V, 0, 0, 0, 0, 0, 704, 52
7135, V, 0, 0, 0, 0, 0, 704, 52
7392, V, 0, 0, 0, 0, 0, 704, 52
7392, V, 0, 0, 0, 0, 0, 704, 52
7649, V, 0, 0, 0, 0, 0, 704, 52
7649, V, 0, 0, 0, 0, 0, 704, 52
7906, V, 0, 0, 0, 0, 0, 704, 52
7906, V, 0, 0, 0, 0, 0, 704, 52
8163, V, 0, 0, 0, 0, 0, 704, 52
8163, V, 0, 0, 0, 0, 0, 704, 52
8420, V, 0, 0, 0, 0, 0, 704, 52
8420, V, 0, 0, 0, 0, 0, 704, 52
8677, V, 0, 0, 0, 0, 0, 704, 52
8677, V, 0, 0, 0, 0, 0, 704, 52
8934, V, 0, 0, 0, 0, 0, 704, 52
8934, V, 0, 0, 0, 0, 0, 704, 52
9191, V, 0, 0, 0, 0, 0, 704, 52
9191, V, 0, 0, 0, 0, 0, 704, 52
9448, V, 0, 0, 0, 0, 0, 704, 52
9448, V, 0, 0, 0, 0, 0, 704, 52
9705, V, 0, 0, 0, 0, 0, 704, 52
9705, V, 0, 0, 0, 0, 0, 704, 52
9962, V, 0, 0, 0, 0, 0, 704, 52
9962, V, 0, 0, 0, 0, 0, 704, 52
10219, V, 0, 0, 0, 0, 0, 704, 52
10219, V, 0, 0, 0, 0, 0, 704, 52
10476, V, 0, 0, 0, 0, 0, 704, 52
10476, V, 0, 0, 0, 0, 0, 704, 52
10733, V, 0, 0, 0, 0, 0, 704, 52
10733, V, 0, 0, 0, 0, 0, 704, 52
10990, V, 0, 0, 0, 0, 0, 704, 52
10990, V, 0, 0, 0, 0, 0, 704, 52
11247, V, 0, 0, 0, 0, 0, 704, 52
11247, V, 0, 0, 0, 0, 0, 704, 52
11504, V, 0, 0, 0, 0, 0, 704, 52
11504, V, 0, 0, 0, 0, 0, 704, 52
11761, V, 0, 0, 0, 0, 0, 704, 52
11761, V, 0, 0, 0, 0, 0, 704, 52
12018, V, 0, 0, 0, 0, 0, 704, 52
12018, V, 0, 0, 0, 0, 0, 704, 52
12275, V, 0, 0, 0, 0, 0, 704, 52
12275, V, 0, 0, 0, 0, 0, 704, 52
12532, V, 0, 0, 0, 0, 0, 704, 52
12532, V, 0, 0, 0, 0, 0, 704, 52
12789, V, 0, 0, 0, 0, 0, 704, 52
12789, V, 0, 0, 0, 0, 0, 704, 52
13046, V, 0, 0, 0, 0, 0, 704, 52
13046, V, 0, 0, 0, 0, 0, 704, 52
13303, V, 0, 0, 0, 0, 0, 704, 52
13303, V, 0, 0, 0, 0, 0, 704, 52
13560, V, 0, 0, 0, 0, 0, 704, 52
13560, V, 0, 0, 0, 0, 0, 704, 52
13817, V, 0, 0, 0, 0, 0, 704, 52
13817, V, 0, 0, 0, 0, 0, 704, 52
14074, V, 0, 0, 0, 0, 0, 704, 52
14074, V, 0, 0, 0, 0, 0, 704, 52
14331, V, 0, 0, 0, 0, 0, 704, 52
14331, V, 0, 0, 0, 0, 0, 704, 52
14588, V, 0, 0, 0, 0, 0, 704, 52
14588, V, 0, 0, 0, 0, 0, 704, 52
14845, V, 0, 0, 0, 0, 0, 704, 52
14845, V, 0, 0, 0, 0, 0, 704, 52
15102, V, 0, 0, 0, 0, 0, 704, 52
15102, V, 0, 0, 0, 0, 0, 704, 52
15360, V, 0, 0, 0, 0, 0, 704, 52
15360, V, 0, 0, 0, 0, 0, 704, 52
15617, V, 0, 0, 0, 0, 0, 704, 52
15617, V, 0, 0, 0, 0, 0, 704, 52
15874, V, 0, 0, 0, 0, 0, 704, 52
15874, V, 0, 0, 0, 0, 0, 704, 52
16131, V, 0, 0, 0, 0, 0, 704, 52
16131, V, 0, 0, 0, 0, 0, 704, 52
16388, V, 0, 0, 0, 0, 0, 704, 52
16388, V, 0, 0, 0, 0, 0, 704, 52
16645, V, 0, 0, 0, 0, 0, 704, 52
16645, V, 0, 0, 0, 0, 0, 704, 52
16902, V, 0, 0, 0, 0, 0, 704, 52
16902, V, 0, 0, 0, 0, 0, 704, 52
17159, V, 0, 0, 0, 0, 0, 704, 52
17159, V, 0, 0, 0, 0, 0, 704, 52
17416, V, 0, 0, 0, 0, 0, 704, 52
17416, V, 0, 0, 0, 0, 0, 704, 52
17673, V, 0, 0, 0, 0, 0, 704, 52
17673, V, 0, 0, 0, 0, 0, 704, 52
17930, V, 0, 0, 0, 0, 0, 704, 52
17930, V, 0, 0, 0, 0, 0, 704, 52
18187, V, 0, 0, 0, 0, 0, 704, 52
18187, V, 0, 0, 0, 0, 0, 704, 52
18444, V, 0, 0, 0, 0, 0, 704, 52
18444, V, 0, 0, 0, 0, 0, 704, 52
18701, V, 0, 0, 0, 0, 0, 704, 52
18701, V, 0, 0, 0, 0, 0, 704, 52
18958, V, 0, 0, 0, 0, 0, 704, 52
18958, V, 0, 0, 0, 0, 0, 704, 52
19215, V, 0, 0, 0, 0, 0, 704, 52
19215, V, 0, 0, 0, 0, 0, 704, 52
19472, V, 0, 0, 0, 0, 0, 704, 52
19472, V, 0, 0, 0, 0, 0, 704, 52
19729, V, 0, 0, 0, 0, 0, 704, 52
19729, V, 0, 0, 0, 0, 0, 704, 52
19986, V, 0, 0, 0, 0, 0, 704, 52
19986, V, 0, 0, 0, 0, 0, 704, 52
20243, V, 0, 0, 0, 0, 0, 704, 52
20243, V, 0, 0, 0, 0, 0, 704, 52
20500, V, 0, 0, 0, 0, 0, 704, 52
20500, V, 0, 0, 0, 0, 0, 704, 52
20757, V, 0, 0, 0, 0, 0, 704, 52
20757, V, 0, 0, 0, 0, 0, 704, 52
21014, V, 0, 0, 0, 0, 0, 704, 52
21014, V, 0, 0, 0, 0, 0, 704, 52
21271, V, 0, 0, 0, 0, 0, 704, 52
21271, V, 0, 0, 0, 0, 0, 704, 52
21528, V, 0, 0, 0, 0, 0, 704, 52
21528, V, 0, 0, 0, 0, 0, 704, 52
21785, V, 0, 0, 0, 0, 0, 704, 52
21785, V, 0, 0, 0, 0, 0, 704, 52
22042, V, 0, 0, 0, 0, 0, 704, 52
22042, V, 0, 0, 0, 0, 0, 704, 52
22299, V, 0, 0, 0, 0, 0, 704, 52
22299, V, 0, 0, 0, 0, 0, 704, 52
22556, V, 0, 0, 0, 0, 0, 704, 52
22556, V, 0, 0, 0, 0, 0, 704, 52
22813, V, 0, 0, 0, 0, 0, 704, 52
22813, V, 0, 0, 0, 0, 0, 704, 52
23070, V, 0, 0, 0, 0, 0, 704, 52
23070, V, 0, 0, 0, 0, 0, 704, 52
23327, V, 0, 0, 0, 0, 0, 704, 52
23327, V, 0, 0, 0, 0, 0, 704, 52
23584, V, 0, 0, 0, 0, 0, 704, 52
23584, V, 0, 0, 0, 0, 0, 704, 52
23841, V, 0, 0, 0, 0, 0, 704, 52
23841, V, 0, 0, 0, 0, 0, 704, 52
24098, V, 0, 0, 0, 0, 0, 704, 52
24098, V, 0, 0, 0, 0, 0, 704, 52
24355, V, 0, 0, 0, 0, 0, 704, 52
24355, V, 0, 0, 0, 0, 0, 704, 52
24612, V, 0, 0, 0, 0, 0, 704, 52
24612, V, 0, 0, 0, 0, 0, 704, 52
24869, V, 0, 0, 0, 0, 0, 704, 52
24869, V, 0, 0, 0, 0, 0, 704, 52
25126, V, 0, 0, 0, 0, 0, 704, 52
25126, V, 0, 0, 0, 0, 0, 704, 52
25383, V, 0, 0, 0, 0, 0, 704, 52
25383, V, 0, 0, 0, 0, 0, 704, 52
25640, V, 0, 0, 0, 0, 0, 704, 52
25640, V, 0, 0, 0, 0, 0, 704, 52
25897, V, 0, 0, 0, 0, 0, 704, 52
25897, V, 0, 0, 0, 0, 0, 704, 52
26155, V, 0, 0, 0, 0, 0, 704, 52
26155, V, 0, 0, 0, 0, 0, 704, 52
26412, V, 0, 0, 0, 0, 0, 704, 52
26412, V, 0, 0, 0, 0, 0, 704, 52
26669, V, 0, 0, 0, 0, 0, 704, 52
26669, V, 0, 0, 0, 0, 0, 704, 52
26926, V, 0, 0, 0, 0, 0, 704, 52
26926, V, 0, 0, 0, 0, 0, 704, 52
27183, V, 0, 0, 0, 0, 0, 704, 52
27183, V, 0, 0, 0, 0, 0, 704, 52
27440, V, 0, 0, 0, 0, 0, 704, 52
27440, V, 0, 0, 0, 0, 0, 704, 52
27697, V, 0, 0, 0, 0, 0, 704, 52
27697, V, 0, 0, 0, 0, 0, 704, 52
27954, V, 0, 0, 0, 0, 0, 704, 52
27954, V, 0, 0, 0, 0, 0, 704, 52
28211, V, 0, 0, 0, 0, 0, 704, 52
28211, V, 0, 0, 0, 0, 0, 704, 52
28468, V, 0, 0, 0, 0, 0, 704, 52
28468, V, 0, 0, 0, 0, 0, 704, 52
28725, V, 0, 0, 0, 0, 0, 704, 52
28725, V, 0, 0, 0, 0, 0, 704, 52
28982, V, 0, 0, 0, 0, 0, 704, 52
28982, V, 0, 0, 0, 0, 0, 704, 52
29239, V, 0, 0, 0, 0, 0, 704, 52
29239, V, 0, 0, 0, 0, 0, 704, 52
29496, V, 0, 0, 0, 0, 0, 704, 52
29496, V, 0, 0, 0, 0, 0, 704, 52
29753, V, 0, 0, 0, 0, 0, 704, 52
29753, V, 0, 0, 0, 0, 0, 704, 52
30010, V, 0, 0, 0, 0, 0, 704, 52
30010, V, 0, 0, 0, 0, 0, 704, 52
30267, V, 0, 0, 0, 0, 0, 704, 52
30267, V, 0, 0, 0, 0, 0, 704, 52
30524, V, 0, 0, 0, 0, 0, 704, 52
30524, V, 0, 0, 0, 0, 0, 704, 52
30781, V, 0, 0, 0, 0, 0, 704, 52
30781, V, 0, 0, 0, 0, 0, 704, 52
31038, V, 0, 0, 0, 0, 0, 704, 52
31038, V, 0, 0, 0, 0, 0, 704, 52
31295, V, 0, 0, 0, 0, 0, 704, 52
31295, V, 0, 0, 0, 0, 0, 704, 52
31552, V, 0, 0, 0, 0, 0, 704, 52
31552, V, 0, 0, 0, 0, 0, 704, 52
31809, V, 0, 0, 0, 0, 0, 704, 52
31809, V, 0, 0, 0, 0, 0, 704, 52
32066, V, 0, 0, 0, 0, 0, 704, 52
32066, V, 0, 0, 0, 0, 0, 704, 52
32323, V, 0, 0, 0, 0, 0, 704, 52
32323, V, 0, 0, 0, 0, 0, 704, 52
32580, V, 0, 0, 0, 0, 0, 704, 52
32580, V, 0, 0, 0, 0, 0, 704, 52
32837, V, 0, 0, 0, 0, 0, 704, 52
32837, V, 0, 0, 0, 0, 0, 704, 52
33094, V, 0, 0, 0, 0, 0, 704, 52
33094, V, 0, 0, 0, 0, 0, 704, 52
33351, V, 0, 0, 0, 0, 0, 704, 52
33351, V, 0, 0, 0, 0, 0, 704, 52
33608, V, 0, 0, 0, 0, 0, 704, 52
33608, V, 0, 0, 0, 0, 0, 704, 52
33865, V, 0, 0, 0, 0, 0, 704, 52
33865, V, 0, 0, 0, 0, 0, 704, 52
34122, V, 0, 0, 0, 0, 0, 704, 52
34122, V, 0, 0, 0, 0, 0, 704, 52
34379, V, 0, 0, 0, 0, 0, 704, 52
34379, V, 0, 0, 0, 0, 0, 704, 52
34636, V, 0, 0, 0, 0, 0, 704, 52
34636, V, 0, 0, 0, 0, 0, 704, 52
34893, V, 0, 0, 0, 0, 0, 704, 52
34893, V, 0, 0, 0, 0, 0, 704, 52
35150, V, 0, 0, 0, 0, 0, 704, 52
35150, V, 0, 0, 0, 0, 0, 704, 52
35407, V, 0, 0, 0, 0, 0, 704, 52
35407, V, 0, 0, 0, 0, 0, 704, 52
35664, V, 0, 0, 0, 0, 0, 704, 52
35664, V, 0, 0, 0, 0, 0, 704, 52
35921, V, 0, 0, 0, 0, 0, 704, 52
35921, V, 0, 0, 0, 0, 0, 704, 52
36178, V, 0, 0, 0, 0, 0, 704, 52
36178, V, 0, 0, 0, 0, 0, 704, 52
36435, V, 0, 0, 0, 0, 0, 704, 52
36435, V, 0, 0, 0, 0, 0, 704, 52
36692, V, 0, 0, 0, 0, 0, 704, 52
36692, V, 0, 0, 0, 0, 0, 704, 52
36950, V, 0, 0, 0, 0, 0, 704, 52
36950, V, 0, 0, 0, 0, 0, 704, 52
37207, V, 0, 0, 0, 0, 0, 704, 52
37207, V, 0, 0, 0, 0, 0, 704, 52
37464, V, 0, 0, 0, 0, 0, 704, 52
37464, V, 0, 0, 0, 0, 0, 704, 52
37721, V, 0, 0, 0, 0, 0, 704, 52
37721, V, 0, 0, 0, 0, 0, 704, 52
37978, V, 0, 0, 0, 0, 0, 704, 52
37978, V, 0, 0, 0, 0, 0, 704, 52
38235, V, 0, 0, 0, 0, 0, 704, 52
38235, V, 0, 0, 0, 0, 0, 704, 52
38492, V, 0, 0, 0, 0, 0, 704, 52
38492, V, 0, 0, 0, 0, 0, 704, 52
38749, V, 0, 0, 0, 0, 0, 704, 52
38749, V, 0, 0, 0, 0, 0, 704, 52
39006, V, 0, 0, 0, 0, 0, 704, 52
39006, V, 0, 0, 0, 0, 0, 704, 52
39263, V, 0, 0, 0, 0, 0, 704, 52
39263, V, 0, 0, 0, 0, 0, 704, 52
39520, V, 0, 0, 0, 0, 0, 704, 52
39520, V, 0, 0, 0, 0, 0, 704, 52
39777, V, 0, 0, 0, 0, 0, 704, 52
39777, V, 0, 0, 0, 0, 0, 704, 52
40034, V, 0, 0, 0, 0, 0, 704, 52
40034, V, 0, 0, 0, 0, 0, 704, 52
40291, V, 0, 0, 0, 0, 0, 704, 52
40291, V, 0, 0, 0, 0, 0, 704, 52
40548, V, 0, 0, 0, 0, 0, 704, 52
40548, V, 0, 0, 0, 0, 0, 704, 52
40805, V, 0, 0, 0, 0, 0, 704, 52
40805, V, 0, 0, 0, 0, 0, 704, 52
41062, V, 0, 0, 0, 0, 0, 704, 52
41062, V, 0, 0, 0, 0, 0, 704, 52
41319, V, 0, 0, 0, 0, 0, 704, 52
41319, V, 0, 0, 0, 0, 0, 704, 52
41576, V, 0, 0, 0, 0, 0, 704, 52
41576, V, 0, 0, 0, 0, 0, 704, 52
41833, V, 0, 0, 0, 0, 0, 704, 52
41833, V, 0, 0, 0, 0, 0, 704, 52
42090, V, 0, 0, 0, 0, 0, 704, 52
42090, V, 0, 0, 0, 0, 0, 704, 52
42347, V, 0, 0, 0, 0, 0, 704, 52
42347, V, 0, 0, 0, 0, 0, 704, 52
42604, V, 0, 0, 0, 0, 0, 704, 52
42604, V, 0, 0, 0, 0, 0, 704, 52
42861, V, 0, 0, 0, 0, 0, 704, 52
42861, V, 0, 0, 0, 0, 0, 704, 52
43118, V, 0, 0, 0, 0, 0, 704, 52
43118, V, 0, 0, 0, 0, 0, 704, 52
43375, V, 0, 0, 0, 0, 0, 704, 52
43375, V, 0, 0, 0, 0, 0, 704, 52
43632, V, 0, 0, 0, 0, 0, 704, 52
43632, V, 0, 0, 0, 0, 0, 704, 52
43889, V, 0, 0, 0, 0, 0, 704, 52
43889, V, 0, 0, 0, 0, 0, 704, 52
44146, V, 0, 0, 0, 0, 0, 704, 52
44146, V, 0, 0, 0, 0, 0, 704, 52
44403, V, 0, 0, 0, 0, 0, 704, 52
44403, V, 0, 0, 0, 0, 0, 704, 52
44660, V, 0, 0, 0, 0, 0, 704, 52
44660, V, 0, 0, 0, 0, 0, 704, 52
44917, V, 0, 0, 0, 0, 0, 704, 52
44917, V, 0, 0, 0, 0, 0, 704, 52
45174, V, 0, 0, 0, 0, 0, 704, 52
45174, V, 0, 0, 0, 0, 0, 704, 52
45431, V, 0, 0, 0, 0, 0, 704, 52
45431, V, 0, 0, 0, 0, 0, 704, 52
45688, V, 0, 0, 0, 0, 0, 704, 52
45688, V, 0, 0, 0, 0, 0, 704, 52
45945, V, 0, 0, 0, 0, 0, 704, 52
45945, V, 0, 0, 0, 0, 0, 704, 52
46202, V, 0, 0, 0, 0, 0, 704, 52
46202, V, 0, 0, 0, 0, 0, 704, 52
46459, V, 0, 0, 0, 0, 0, 704, 52
46459, V, 0, 0, 0, 0, 0, 704, 52
46716, V, 0, 0, 0, 0, 0, 704, 52
46716, V, 0, 0, 0, 0, 0, 704, 52
46973, V, 0, 0, 0, 0, 0, 704, 52
46973, V, 0, 0, 0, 0, 0, 704, 52
47230, V, 0, 0, 0, 0, 0, 704, 52
47230, V, 0, 0, 0, 0, 0, 704, 52
47488, V, 0, 0, 0, 0, 0, 704, 52
47488, V, 0, 0, 0, 0, 0, 704, 52
47745, V, 0, 0, 0, 0, 0, 704, 52
47745, V, 0, 0, 0, 0, 0, 704, 52
48002, V, 0, 0, 0, 0, 0, 704, 52
48002, V, 0, 0, 0, 0, 0, 704, 52
48259, V, 0, 0, 0, 0, 0, 704, 52
48259, V, 0, 0, 0, 0, 0, 704, 52
48516, V, 0, 0, 0, 0, 0, 704, 52
48516, V, 0, 0, 0, 0, 0, 704, 52
48773, V, 0, 0, 0, 0, 0, 704, 52
48773, V, 0, 0, 0, 0, 0, 704, 52
49030, V, 0, 0, 0, 0, 0, 704, 52
49030, V, 0, 0, 0, 0, 0, 704, 52
49287, V, 0, 0, 0, 0, 0, 704, 52
49287, V, 0, 0, 0, 0, 0, 704, 52
49544, V, 0, 0, 0, 0, 0, 704, 52
49544, V, 0, 0, 0, 0, 0, 704, 52
49801, V, 0, 0, 0, 0, 0, 704, 52
49801, V, 0, 0, 0, 0, 0, 704, 52
50058, V, 0, 0, 0, 0, 0, 704, 52
50058, V, 0, 0, 0, 0, 0, 704, 52
50315, V, 0, 0, 0, 0, 0, 704, 52
50315, V, 0, 0, 0, 0, 0, 704, 52
50572, V, 0, 0, 0, 0, 0, 704, 52
50572, V, 0, 0, 0, 0, 0, 704, 52
50829, V, 0, 0, 0, 0, 0, 704, 52
50829, V, 0, 0, 0, 0, 0, 704, 52
51086, V, 0, 0, 0, 0, 0, 704, 52
51086, V, 0, 0, 0, 0, 0, 704, 52
51343, V, 0, 0, 0, 0, 0, 704, 52
51343, V, 0, 0, 0, 0, 0, 704, 52
51600, V, 0, 0, 0, 0, 0, 704, 52
51600, V, 0, 0, 0, 0, 0, 704, 52
51857, V, 0, 0, 0, 0, 0, 704, 52
51857, V, 0, 0, 0, 0, 0, 704, 52
52114, V, 0, 0, 0, 0, 0, 704, 52
52114, V, 0, 0, 0, 0, 0, 704, 52
52371, V, 0, 0, 0, 0, 0, 704, 52
52371, V, 0, 0, 0, 0, 0, 704, 52
52628, V, 0, 0, 0, 0, 0, 704, 52
52628, V, 0, 0, 0, 0, 0, 704, 52
52885, V, 0, 0, 0, 0, 0, 704, 52
52885, V, 0, 0, 0, 0, 0, 704, 52
53142, V, 0, 0, 0, 0, 0, 704, 52
53142, V, 0, 0, 0, 0, 0, 704, 52
53399, V, 0, 0, 0, 0, 0, 704, 52
53399, V, 0, 0, 0, 0, 0, 704, 52
53656, V, 0, 0, 0, 0, 0, 704, 52
53656, V, 0, 0, 0, 0, 0, 704, 52
53913, V, 0, 0, 0, 0, 0, 704, 52
53913, V, 0, 0, 0, 0, 0, 704, 52
54170, V, 0, 0, 0, 0, 0, 704, 52
54170, V, 0, 0, 0, 0, 0, 704, 52
54427, V, 0, 0, 0, 0, 0, 704, 52
54427, V, 0, 0, 0, 0, 0, 704, 52
54684, V, 0, 0, 0, 0, 0, 704, 52
54684, V, 0, 0, 0, 0, 0, 704, 52
54941, V, 0, 0, 0, 0, 0, 704, 52
54941, V, 0, 0, 0, 0, 0, 704, 52
55198, V, 0, 0, 0, 0, 0, 704, 52
55198, V, 0, 0, 0, 0, 0, 704, 52
55455, V, 0, 0, 0, 0, 0, 704, 52
55455, V, 0, 0, 0, 0, 0, 704, 52
55712, V, 0, 0, 0, 0, 0, 704, 52
55712, V, 0, 0, 0, 0, 0, 704, 52
55969, V, 0, 0, 0, 0, 0, 704, 52
55969, V, 0, 0, 0, 0, 0, 704, 52
56226, V, 0, 0, 0, 0, 0, 704, 52
56226, V, 0, 0, 0, 0, 0, 704, 52
56483, V, 0, 0, 0, 0, 0, 704, 52
56483, V, 0, 0, 0, 0, 0, 704, 52
56740, V, 0, 0, 0, 0, 0, 704, 52
56740, V, 0, 0, 0, 0, 0, 704, 52
56997, V, 0, 0, 0, 0, 0, 704, 52
56997, V, 0, 0, 0, 0, 0, 704, 52
57254, V, 0, 0, 0, 0, 0, 704, 52
57254, V, 0, 0, 0, 0, 0, 704, 52
57511, V, 0, 0, 0, 0, 0, 704, 52
57511, V, 0, 0, 0, 0, 0, 704, 52
57768, V, 0, 0, 0, 0, 0, 704, 52
57768, V, 0, 0, 0, 0, 0, 704, 52
58025, V, 0, 0, 0, 0, 0, 704, 52
58025, V, 0, 0, 0, 0, 0, 704, 52
58283, V, 0, 0, 0, 0, 0, 704, 52
58283, V, 0, 0, 0, 0, 0, 704, 52
58540, V, 0, 0, 0, 0, 0, 704, 52
58540, V, 0, 0, 0, 0, 0, 704, 52
58797, V, 0, 0, 0, 0, 0, 704, 52
58797, V, 0, 0, 0, 0, 0, 704, 52
59054, V, 0, 0, 0, 0, 0, 704, 52
59054, V, 0, 0, 0, 0, 0, 704, 52
59311, V, 0, 0, 0, 0, 0, 704, 52
59311, V, 0, 0, 0, 0, 0, 704, 52
59568, V, 0, 0, 0, 0, 0, 704, 52
59568, V, 0, 0, 0, 0, 0, 704, 52
59825, V, 0, 0, 0, 0, 0, 704, 52
59825, V, 0, 0, 0, 0, 0, 704, 52
60082, V, 0, 0, 0, 0, 0, 704, 52
60082, V, 0, 0, 0, 0, 0, 704, 52
60339, V, 0, 0, 0, 0, 0, 704, 52
60339, V, 0, 0, 0, 0, 0, 704, 52
60596, V, 0, 0, 0, 0, 0, 704, 52
60596, V, 0, 0, 0, 0, 0, 704, 52
60853, V, 0, 0, 0, 0, 0, 704, 52
60853, V, 0, 0, 0, 0, 0, 704, 52
61110, V, 0, 0, 0, 0, 0, 704, 52
61110, V, 0, 0, 0, 0, 0, 704, 52
61367, V, 0, 0, 0, 0, 0, 704, 52
61367, V, 0, 0, 0, 0, 0, 704, 52
61624, V, 0, 0, 0, 0, 0, 704, 52
61624, V, 0, 0, 0, 0, 0, 704, 52
61881, V, 0, 0, 0, 0, 0, 704, 52
61881, V, 0, 0, 0, 0, 0, 704, 52
62138, V, 0, 0, 0, 0, 0, 704, 52
62138, V, 0, 0, 0, 0, 0, 704, 52
62395, V, 0, 0, 0, 0, 0, 704, 52
62395, V, 0, 0, 0, 0, 0, 704, 52
62652, V, 0, 0, 0, 0, 0, 704, 52
62652, V, 0, 0, 0, 0, 0, 704, 52
62909, V, 0, 0, 0, 0, 0, 704, 52
62909, V, 0, 0, 0, 0, 0, 704, 52
63166, V, 0, 0, 0, 0, 0, 704, 52
63166, V, 0, 0, 0, 0, 0, 704, 52
63423, V, 0, 0, 0, 0, 0, 704, 52
63423, V, 0, 0, 0, 0, 0, 704, 52
63680, V, 0, 0, 0, 0, 0, 704, 52
63680, V, 0, 0, 0, 0, 0, 704, 52
63937, V, 0, 0, 0, 0, 0, 704, 52
63937, V, 0, 0, 0, 0, 0, 704, 52
64194, V, 0, 0, 0, 0, 0, 704, 52
64194, V, 0, 0, 0, 0, 0, 704, 52
64451, V, 0, 0, 0, 0, 0, 704, 52
64451, V, 0, 0, 0, 0, 0, 704, 52
64708, V, 0, 0, 0, 0, 0, 704, 52
64708, V, 0, 0, 0, 0, 0, 704, 52
64965, V, 0, 0, 0, 0, 0, 704, 52
64965, V, 0, 0, 0, 0, 0, 704, 52
65222, V, 0, 0, 0, 0, 0, 704, 52
65222, V, 0, 0, 0, 0, 0, 704, 52
65479, V, 0, 0, 0, 0, 0, 704, 52
65479, V, 0, 0, 0, 0, 0, 704, 52
200, V, 0, 0, 0, 0, 0, 704, 52
200, V, 0, 0, 0, 0, 0, 704, 52
457, V, 0, 0, 0, 0, 0, 704, 52
457, V, 0, 0, 0, 0, 0, 704, 52
714, V, 0, 0, 0, 0, 0, 704, 52
714, V, 0, 0, 0, 0, 0, 704, 52
971, V, 0, 0, 0, 0, 0, 704, 52
971, V, 0, 0, 0, 0, 0, 704, 52
1228, V, 0, 0, 0, 0, 0, 704, 52
1228, V, 0, 0, 0, 0, 0, 704, 52
1485, V, 0, 0, 0, 0, 0, 704, 52
1485, V, 0, 0, 0, 0, 0, 704, 52
1742, V, 0, 0, 0, 0, 0, 704, 52
1742, V, 0, 0, 0, 0, 0, 704, 52
1999, V, 0, 0, 0, 0, 0, 704, 52
1999, V, 0, 0, 0, 0, 0, 704, 52
2256, V, 0, 0, 0, 0, 0, 704, 52
2256, V, 0, 0, 0, 0, 0, 704, 52
2513, V, 0, 0, 0, 0, 0, 704, 52
2513, V, 0, 0, 0, 0, 0, 704, 52
2770, V, 0, 0, 0, 0, 0, 704, 52
2770, V, 0, 0, 0, 0, 0, 704, 52
3027, V, 0, 0, 0, 0, 0, 704, 52
3027, V, 0, 0, 0, 0, 0, 704, 52
3284, V, 0, 0, 0, 0, 0, 704, 52
3284, V, 0, 0, 0, 0, 0, 704, 52
3542, V, 0, 0, 0, 0, 0, 704, 52
3542, V, 0, 0, 0, 0, 0, 704, 52
3799, V, 0, 0, 0, 0, 0, 704, 52
3799, V, 0, 0, 0, 0, 0, 704, 52
4056, V, 0, 0, 0, 0, 0, 704, 52
4056, V, 0, 0, 0, 0, 0, 704, 52
4313, V, 0, 0, 0, 0, 0, 704, 52
4313, V, 0, 0, 0, 0, 0, 704, 52
4570, V, 0, 0, 0, 0, 0, 704, 52
4570, V, 0, 0, 0, 0, 0, 704, 52
4827, V, 0, 0, 0, 0, 0, 704, 52
4827, V, 0, 0, 0, 0, 0, 704, 52
5084, V, 0, 0, 0, 0, 0, 704, 52
5084, V, 0, 0, 0, 0, 0, 704, 52
5341, V, 0, 0, 0, 0, 0, 704, 52
5341, V, 0, 0, 0, 0, 0, 704, 52
5598, V, 0, 0, 0, 0, 0, 704, 52
5598, V, 0, 0, 0, 0, 0, 704, 52
5855, V, 0, 0, 0, 0, 0, 704, 52
5855, V, 0, 0, 0, 0, 0, 704, 52
6112, V, 0, 0, 0, 0, 0, 704, 52
6112, V, 0, 0, 0, 0, 0, 704, 52
6369, V, 0, 0, 0, 0, 0, 704, 52
6369, V, 0, 0, 0, 0, 0, 704, 52
6626, V, 0, 0, 0, 0, 0, 704, 52
6626, V, 0, 0, 0, 0, 0, 704, 52
6883, V, 0, 0, 0, 0, 0, 704, 52
6883, V, 0, 0, 0, 0, 0, 704, 52
7140, V, 0, 0, 0, 0, 0, 704, 52
7140, V, 0, 0, 0, 0, 0, 704, 52
7397, V, 0, 0, 0, 0, 0, 704, 52
7397, V, 0, 0, 0, 0, 0, 704, 52
7654, V, 0, 0, 0, 0, 0, 704, 52
7654, V, 0, 0, 0, 0, 0, 704, 52
7911, V, 0, 0, 0, 0, 0, 704, 52
7911, V, 0, 0, 0, 0, 0, 704, 52
8168, V, 0, 0, 0, 0, 0, 704, 52
8168, V, 0, 0, 0, 0, 0, 704, 52
8425, V, 0, 0, 0, 0, 0, 704, 52
8425, V, 0, 0, 0, 0, 0, 704, 52
8682, V, 0, 0, 0, 0, 0, 704, 52
8682, V, 0, 0, 0, 0, 0, 704, 52
8939, V, 0, 0, 0, 0, 0, 704, 52
8939, V, 0, 0, 0, 0, 0, 704, 52
9196, V, 0, 0, 0, 0, 0, 704, 52
9196, V, 0, 0, 0, 0, 0, 704, 52
9453, V, 0, 0, 0, 0, 0, 704, 52
9453, V, 0, 0, 0, 0, 0, 704, 52
9710, V, 0, 0, 0, 0, 0, 704, 52
9710, V, 0, 0, 0, 0, 0, 704, 52
9967, V, 0, 0, 0, 0, 0, 704, 52
9967, V, 0, 0, 0, 0, 0, 704, 52
10224, V, 0, 0, 0, 0, 0, 704, 52
10224, V, 0, 0, 0, 0, 0, 704, 52
10481, V, 0, 0, 0, 0, 0, 704, 52
10481, V, 0, 0, 0, 0, 0, 704, 52
10738, V, 0, 0, 0, 0, 0, 704, 52
10738, V, 0, 0, 0, 0, 0, 704, 52
10995, V, 0, 0, 0, 0, 0, 704, 52
10995, V, 0, 0, 0, 0, 0, 704, 52
11252, V, 0, 0, 0, 0, 0, 704, 52
11252, V, 0, 0, 0, 0, 0, 704, 52
11509, V, 0, 0, 0, 0, 0, 704, 52
11509, V, 0, 0, 0, 0, 0, 704, 52
11766, V, 0, 0, 0, 0, 0, 704, 52
11766, V, 0, 0, 0, 0, 0, 704, 52
12023, V, 0, 0, 0, 0, 0, 704, 52
12023, V, 0, 0, 0, 0, 0, 704, 52
12280, V, 0, 0, 0, 0, 0, 704, 52
12280, V, 0, 0, 0, 0, 0, 704, 52
12537, V, 0, 0, 0, 0, 0, 704, 52
12537, V, 0, 0, 0, 0, 0, 704, 52
12794, V, 0, 0, 0, 0, 0, 704, 52
12794, V, 0, 0, 0, 0, 0, 704, 52
13051, V, 0, 0, 0, 0, 0, 704, 52
13051, V, 0, 0, 0, 0, 0, 704, 52
13308, V, 0, 0, 0, 0, 0, 704, 52
13308, V, 0, 0, 0, 0, 0, 704, 52